Super Thermal Conductive Aluminum Alloy

A superthermally conductive aluminum alloy with enhanced thermal conductivity is developed, addressing poor heat dissipation in current alloys by incorporating controlled smelting and degassing, suitable for high-heat applications.

JP7579604B1Active Publication Date: 2024-11-08TOKIRYO IND CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023088560
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-05-30
Publication Date
2024-11-08
Estimated Expiration
2043-05-30

AI Technical Summary

Technical Problem

Current aluminum alloys used in radiators exhibit poor heat dissipation properties, failing to meet the high thermal conductivity requirements of precision equipment operating in harsh environments.

Method used

A superthermally conductive aluminum alloy composed of specific weight percentages of aluminum, nickel, aluminum titanium carbon, and trace elements, manufactured through a controlled smelting and degassing process to enhance thermal conductivity.

Benefits of technology

The alloy achieves thermal conductivity exceeding 230 W/mK, with high-temperature strength and electrical conductivity, suitable for applications like 3C electronic parts, 5G communication equipment, car electronics, and aerospace components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007579604000001_ABST
    Figure 0007579604000001_ABST
Patent Text Reader

Abstract

A super-thermal conductive aluminum alloy having high thermal conductivity and a manufacturing method thereof are provided. [Solution] The method for producing a super thermal conductive aluminum alloy according to the present invention includes the following steps: Preheating a crucible furnace to 500°C or higher; Adding a pure aluminum ingot and smelting; Refining and removing slag when the temperature of the molten metal reaches 720°C; Raising the temperature to 750°C after completion, adding nickel, and controlling the temperature to 750-810°C; Stirring thoroughly and then confirming completion of nickel melting; Sampling and analyzing the composition to confirm that there are no errors in the nickel composition; Adding aluminum titanium carbon, stirring, and then confirming completion of aluminum titanium carbon melting; Turning on the ventilation equipment and degassing. The degassing process takes about 5-10 minutes. Allowing to stand for about 10 minutes after completion; Sampling and determining the composition; Casting the aluminum ingot.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention is a super-thermal conductive aluminum alloy. To money In particular, it belongs to the field of industrial aluminum alloy manufacturing. [Background technology]

[0002] Aluminum alloy ingot is made of pure aluminum and recycled aluminum. It is an alloy that is formulated to improve the castability, chemical and physical deficiencies of pure aluminum by adding other elements such as silicon (Si), magnesium (Mg) and iron (Fe) according to international standards or special regulations. It is commonly used in the foundry industry.

[0003] With the rapid development of science and technology, the performance requirements and precision of equipment are also increasing. Precision equipment requires strict operating environment. Temperature control is a vital part of ensuring equipment operation. Most equipment temperature control cannot be separated from the radiator. However, in order to improve the heat dissipation performance of the radiator, in addition to changing the structure, the most fundamental thing is to improve the heat dissipation performance of the material used to make the radiator. Therefore, by developing a more reasonable manufacturing method and producing a high-quality heat dissipation material that can be molded and processed, the requirements for high heat dissipation equipment can be met, the degree of integration of various equipment can be improved, and the volume can be reduced. However, in actual production, the aluminum alloy material currently used has poor heat dissipation performance. Summary of the Invention [Problem to be solved by the invention]

[0004] The main objective of the present invention is to develop an ultra-high thermal conductive aluminum alloy. Money The ultra-high thermal conductivity aluminum alloy is used in aluminum alloy products that manufacture components under ultra-high thermal conductivity, and can meet the requirements for heat dissipation of aluminum alloy materials in special industries. [Means for solving the problem]

[0005] The super thermal conductive aluminum alloy of the present invention is mainly composed of aluminum, nickel, and aluminum titanium carbon. The weight percentages of the components other than aluminum are as follows: Nickel is 2-5%, carbon in aluminum titanium carbon is 0.1%-0.5%, titanium in aluminum titanium carbon is 0.01-0.2%, iron is less than 0.1%, silicon is less than 0.1%, The copper, zinc, manganese, magnesium, chromium, lead, and tin content is less than 0.01% each. The content of other elements is limited to 0.005% each.

[0006] Among the constituents of the super thermal conductive aluminum alloy of the present invention, the weight percentage of aluminum is more than 94%.

[0007] Reference aspect The manufacturing method of the super thermal conductive aluminum alloy includes the following steps. This process involves preheating the crucible furnace to over 500°C. This is the process in which pure aluminum ingots are fed and smelted. Once the temperature of the molten metal reaches 720°C, it is refined and slag removed. After refining and removing slag, the temperature is raised to 750°C, the smelting temperature is controlled at 750-810°C, and nickel is added and stirred. This is a process to check that the nickel has been completely dissolved. Sampling is carried out to analyze the composition and check that the nickel composition is correct. This step involves adding aluminum titanium carbon and stirring while simultaneously checking to see if the aluminum titanium carbon has completely dissolved. This is the process of turning on the ventilation equipment and degassing. The degassing process lasts for 5 to 10 minutes. After completion, the mixture is left to rest for 10 minutes. This process involves sampling, evaluating the components, and ultimately verifying that the specified conditions are met. The process of casting aluminum ingots.

[0008] The ultra-high thermal conductive aluminum alloy of the present invention Gold The advantages are as follows. The ultra-high thermal conductive aluminum alloy of the present invention has high-temperature strength and electrical conductivity, and is created to be easily molded. In addition, the thermal conductivity of unheated aluminum alloy is close to that of pure aluminum, reaching 230W / mK or more, and has a very good heat dissipation effect, and is applicable to production methods such as aluminum alloy die casting and aluminum alloy casting. The products can be applied to parts that require high heat dissipation and high thermal conductivity, such as 3C electronic parts, 5G communication equipment, automotive electronic parts, engine rotors, and aerospace / satellite communications. [Brief description of the drawings]

[0009] [Figure 1] 1 is a flowchart showing a manufacturing method according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a microstructure diagram of the metal structure of the aluminum alloy containing 2.5% nickel according to the present invention. [Diagram 3] FIG. 2 is a microstructure diagram of the metal structure of the aluminum alloy containing 2.5% nickel and aluminum titanium carbon according to the present invention. [Figure 4] FIG. 2 is a microstructure diagram of the metal structure of the aluminum alloy containing 3.3% nickel and aluminum titanium carbon according to the present invention. [Diagram 5] FIG. 2 is a microstructure diagram of the metal structure of the aluminum alloy containing 3.5% nickel and aluminum titanium carbon according to the present invention. [Figure 6] FIG. 2 is a micro-structure diagram of the metal structure of the aluminum alloy containing 5% nickel according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The technical means used to achieve the above-mentioned purposes and effects will be described in detail below with reference to preferred examples and drawings.

[0011] Please refer to FIG. 1 for the manufacturing method of the ultra-high thermal conductive aluminum alloy of the present invention. The manufacturing method is as follows. The crucible furnace is preheated to 500°C or more. Pure aluminum ingots are put in and smelted. When the temperature of the molten metal reaches 720°C, refining and slag removal are performed. After completion, the temperature is raised to 750°C. Nickel (Ni), which is the main element, is added, the temperature is controlled to 750-810°C, and after thorough stirring, the completion of nickel melting is confirmed. After sampling and analyzing the composition to confirm that there is no mistake in the nickel composition, aluminum titanium carbon (AlTiC) is added, stirred, and the completion of aluminum titanium carbon melting is confirmed. Then, degassing is performed using ventilation equipment. The degassing process takes about 5-10 minutes, and after completion, the mixture is left to stand for about 10 minutes. Next, sampling is performed to determine the composition. The final composition determination must meet the specified conditions (as shown in Table 1). Then, aluminum ingots are cast. [Table 1]

[0012] The components of the ultra-high thermal conductivity aluminum alloy of the present invention are mainly aluminum (Al), nickel (Ni), and aluminum titanium carbon (AlTiC). The weight percentages of the components are as follows: nickel is 2-5%, carbon (C) of aluminum titanium carbon is 0.1-0.5%, titanium (Ti) is 0.01-0.2%, iron (Fe) is 0.1% or less, and silicon (Si) is 0.1% or less. In addition, the content of each element such as copper (Cu), zinc (Zn), magnesium (Mn), chromium (Cr), lead (Pb), and tin (Sn) is 0.01% or less. The content of each of the other elements is limited to 0.005% or less. The rest is aluminum, which is more than 94%.

[0013] In the present invention, the metal structure formed differs depending on the ratio of nickel and aluminum titanium carbon added to the aluminum alloy. Fig. 2 is a micro-structure diagram of the metal structure observed under a microscope after adding 2.5% nickel of the present invention. Fig. 3 is a micro-structure diagram of the metal structure observed under a microscope after adding 2.5% nickel and aluminum titanium carbon of the present invention. Fig. 4 is a micro-structure diagram of the metal structure observed under a microscope after adding 3.3% nickel and aluminum titanium carbon of the present invention. Fig. 5 is a micro-structure diagram of the metal structure observed under a microscope after adding 3.5% nickel and aluminum titanium carbon of the present invention. Fig. 6 is a micro-structure diagram of the metal structure observed under a microscope after adding 5% nickel of the present invention.

[0014] The present invention has produced aluminum alloys with different amounts of nickel (Ni) added, and the thermal conductivity coefficients and tensile test results are shown in Table 2 below. [Table 2]

[0015] The ultra-high thermal conductive aluminum alloy of the present invention has electrical conductivity and thermal conductivity close to that of a pure aluminum ingot, which is advantageous for die casting / casting of aluminum alloys and allows the cast products to be easily processed.

[0016] As described above, the present invention achieves the expected purpose and effect, and is more ideal and practical than those skilled in the art. However, the above-mentioned embodiments are merely detailed descriptions of the preferred embodiments of the present invention, and the scope of the claims of the present invention is not limited thereby. All equivalent changes and modifications based on the scope of the claims of the present invention belong to the scope of the claims of the present invention.

Claims

[Claim 1] The main components are aluminum, nickel, and aluminum titanium carbon. The weight percent of aluminum is greater than 94%; The weight percentages of the components other than aluminum are: Nickel is 2-5%, carbon of the aluminum titanium carbon is 0.1%-0.5%, titanium of the aluminum titanium carbon is 0.01-0.2%, iron is 0.1% or less, silicon is 0.1% or less, The content of copper, zinc, manganese, magnesium, chromium, lead, and tin is each 0.01% or less. A super thermal conductive aluminum alloy, characterized in that the content of each of the other elements is limited to 0.005% or less.

Citation Information

Patent Citations

  • Preparation method of aluminum-nickel-titanium-carbon intermediate alloy

    CN102220524A

  • High-strength composite aluminum alloy automobile part mixed with nano titanium carbide powder and casting technology of high-strength composite aluminum alloy automobile part

    CN105177362A

  • A high thermal conductivity die-cast aluminum alloy and its preparation method

    CN114672697B

  • Casting alloy for high pressure vacuum die casting

    JP2022517830A

  • Aluminum alloy for die casting

    KR1020210038624A