Coating device and coating method
The coating device addresses the challenge of selectively applying coating films on specific parts of a base material by using a block configuration with exposure ports, ensuring precise application and uniform coating without increasing device complexity.
Patent Information
- Application Number
- JP2020114273
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-07-01
- Publication Date
- 2024-11-11
- Estimated Expiration
- 2040-07-01
AI Technical Summary
Existing coating devices complicate the process and increase size when attempting to selectively form a coating film on specific parts of a sheet-like base material by adjusting substrate orientation and conveyance direction, making it difficult to apply coating liquid to both sides of a specific area while avoiding other areas.
A coating device with a pair of blocks facing each other in the thickness direction, featuring a liquid reservoir with an inlet and outlet aligned with the conveyance direction, and exposure ports on the side surfaces, allowing selective application of coating liquid to specific portions of the base material by protruding them through exposure openings.
Enables the selective formation of a coating film on specific portions of the base material while preventing application on non-specific areas, reducing apparatus complexity and size, and improving coating uniformity and coverage.
Smart Images

Figure 0007580030000001 
Figure 0007580030000002 
Figure 0007580030000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a coating device and a coating method. [Background technology]
[0002] For example, various techniques have been disclosed regarding coating devices for forming coating films on both sides of a sheet-like substrate transported by a roll-to-roll method.
[0003] For example, in the coating device disclosed in Patent Document 1, first, a continuously conveyed long sheet-like substrate is immersed in an immersion tank in which the coating liquid is stored, so that the coating liquid is applied to both sides of the substrate. Then, while the substrate is raised vertically, a pair of scraping rolls scrapes off excess coating liquid on both sides of the substrate. This forms a coating film of a certain thickness on both sides of the substrate. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 64-7965 Summary of the Invention [Problem to be solved by the invention]
[0005] However, there are cases where it is desired to selectively form a coating film on both sides of a specific portion in the width direction of a substrate. In this case, it is necessary to apply a coating liquid to both sides of the specific portion in the width direction of the substrate, while not applying the coating liquid to portions other than the specific portion.
[0006] However, when attempting to selectively form a coating film on both sides of a specific portion of a substrate in the width direction using the coating device of Patent Document 1, it is necessary to adjust the orientation of the substrate itself and the conveying direction of the substrate so that only the specific portion of the substrate is immersed in the immersion tank, which poses the problem of complicating the coating process and requiring an increased size of the coating device.
[0007] The present disclosure has been made in consideration of these points, and its main objective is to make it possible to selectively form a coating film on both sides of a specific portion in the width direction of a substrate being transported. [Means for solving the problem]
[0008] A coating device according to the present disclosure is a coating device that applies a coating liquid to both sides of a sheet-like substrate being transported, and includes a pair of blocks facing each other in the thickness direction of the substrate, and a liquid pool portion formed so that the coating liquid pools in the gap between the pair of blocks and through which the substrate passes, the liquid pool portion including an inlet opening upstream in the transport direction of the substrate and through which the substrate is introduced, an outlet opening downstream in the transport direction and through which the substrate is discharged, and side portions located on both sides in a width direction intersecting the transport direction, the side portion on at least one side in the width direction including an exposed opening that opens from the inlet to the outlet, and a portion of the substrate in the width direction can protrude from the exposed opening to the outside of the liquid pool portion.
[0009] The coating method according to the present disclosure uses the coating device to apply the coating liquid to both sides of a specific portion of the substrate in the width direction by passing the substrate through the coating device while causing a portion of the substrate in the width direction to protrude from the exposed opening to the outside of the liquid reservoir. Effect of the Invention
[0010] According to the present disclosure, it is possible to selectively form a coating film on both sides of a specific portion in the width direction of a substrate being transported. [Brief description of the drawings]
[0011] [Figure 1] FIG. 1 is a diagram illustrating a coating system including a coating device according to a first embodiment of the present disclosure. [Diagram 2] FIG. 2 is a front view of the coating device according to the first embodiment. [Diagram 3]FIG. 3 is a plan view of the coating device according to the first embodiment. [Figure 4] FIG. 4 is a side view of the coating device according to the first embodiment. [Diagram 5] FIG. 5 is an enlarged front view showing the vicinity of the discharge port of the coating device according to the first embodiment. [Figure 6] FIG. 6 is a side view of a coating device according to the second embodiment. [Figure 7] FIG. 7 is a side view of a coating device according to the third embodiment. [Figure 8] FIG. 8 is a front view of a coating device according to the fourth embodiment. [Figure 9] FIG. 9 is a plan sectional view of a coating device according to the fourth embodiment. [Figure 10] FIG. 10 is a plan sectional view of a coating device according to the fifth embodiment. [Figure 11] FIG. 11 is a front view of a coating device according to the sixth embodiment. [Figure 12] FIG. 12 is a front view of a coating device according to the seventh embodiment. [Figure 13] FIG. 13 is a front view of a coating device according to the eighth embodiment. [Figure 14] FIG. 14 is a plan view of a coating device according to a ninth embodiment. [Figure 15] FIG. 15 is a plan view of a coating device according to a tenth embodiment. [Figure 16] FIG. 16 is a side view of a coating device according to an eleventh embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, the embodiments of the present disclosure will be described in detail with reference to the drawings. The following description of the preferred embodiments is merely illustrative in nature and is not intended to limit the present disclosure, its application, or its uses.
[0013] <First embodiment> (Basic configuration) 1 is a schematic diagram of a coating system 1 according to a first embodiment of the present disclosure. The coating system 1 is for continuously forming a coating film F on both sides of a substrate 2. The coating system 1 is composed of a substrate supplying device 10, a coating device 20, and a coating fluid supplying device 40.
[0014] The substrate 2 is formed in a long sheet shape. Examples of the substrate 2 include metal foil, resin film, woven fabric, nonwoven fabric, paper, etc. The thickness dimension t (see FIG. 5) of the substrate 2 not including the coating film F is, for example, 1 mm or less.
[0015] The base material supplying device 10 continuously transports the base material 2 by a roll-to-roll method with its longitudinal direction being the transport direction (indicated by X). Specifically, the base material supplying device 10 continuously transports the base material 2 by unwinding the base material 2 with an unwinder 11 and winding it with a winder 12. The transported base material 2 passes through a first roll 13 and a second roll 14 along the way.
[0016] A coating device 20 is disposed between the first roll 13 and the second roll 14 in the transport direction of the substrate 2. The coating device 20, which will be described in detail later, applies a coating liquid C to both sides of the sheet-like substrate 2 that is continuously transported, to form a coating film F on both sides of the substrate 2. The substrate 2 with the coating film F formed on both sides by the coating device 20 is dried in a drying furnace (not shown) to remove volatile components contained in the coating film F, and then taken up by a winder 12.
[0017] The configuration of the coating device 20 will be described in detail. Figures 2 to 5 show the coating device 20 according to this embodiment, with Figure 2 being a front cross-sectional view (viewed in the direction of arrow II), Figure 3 being a side view (viewed in the direction of arrow III), Figure 4 being a plan view (viewed in the direction of arrow IV), and Figure 5 being an enlarged front view of the vicinity of a discharge port 25 described later.
[0018] In this embodiment, the conveying direction (longitudinal direction) of the substrate 2 is approximately the same as the horizontal direction perpendicular to the vertical direction. The thickness direction (indicated by Z) of the substrate 2 is approximately the same as the vertical direction. The width direction (indicated by Y) of the substrate 2 is approximately the same as the horizontal direction intersecting the conveying direction of the substrate 2, specifically, the horizontal direction perpendicular to the conveying direction.
[0019] 2, the coating device 20 includes a pair of blocks, specifically a first block 21 and a second block 22. The first block 21 and the second block 22 are disposed at a predetermined interval from each other in the thickness direction of the substrate 2 and face each other in the thickness direction of the substrate 2. Each of the blocks 21, 22 is formed in a substantially rectangular parallelepiped shape and disposed such that its longitudinal direction is aligned with the transport direction of the substrate 2.
[0020] 3 and 4, L1 is the length dimension of each of the blocks 21 and 22. L2 is the width dimension of each of the blocks 21 and 22. L3 is the thickness dimension of each of the blocks 21 and 22.
[0021] It is preferable that the length dimension L1 of each of the blocks 21, 22 is sufficiently larger than the thickness dimension t (see FIG. 5) of the base material 2. Specifically, it is preferable that the length dimension L1 of each of the blocks 21, 22 is 100 times or more, and more preferably 500 times or more, the thickness dimension t of the base material 2.
[0022] As shown in FIG. 4, in this embodiment, the width dimension L2 of each of the blocks 21 and 22 is smaller than the width dimension B of the base material 2.
[0023] 2, in the gap 23 between a pair of blocks, i.e., the gap 23 between the first block 21 and the second block 22, a liquid pool is formed so that the coating liquid C can pool (hereinafter, referred to as the "liquid pool 23"). When the substrate 2 passes through the liquid pool 23, the coating liquid C is applied to both sides of the substrate 2, and a coating film F is formed on both sides of the substrate 2.
[0024] The coating liquid C is preferably in the form of a paste or a slurry, and for example, a coating liquid C having a viscosity η of 1 mPa·s or more can be applied to both sides of the substrate 2. Furthermore, for example, when a coating liquid C having a viscosity η of 1 Pa·s to 1000 Pa·s is used, it is preferable because this allows a smooth coating film F to be formed on both sides of the substrate 2.
[0025] Coating liquid C can be made of, for example, insulating materials containing metal oxide particles such as silica, low-melting glass, alumina, titanium oxide, etc.; metal particles such as solder, copper, silver, metal-coated particles, etc.; conductive materials containing lithium nickel oxide, lithium manganate, lithium cobalt oxide, carbon, etc.; dyes, etc.
[0026] H indicates the gap dimension between the first block 21 and the second block 22. In this embodiment, the gap dimension H is uniform across the conveyance direction and the width direction. The gap dimension H is larger than the thickness dimension t (e.g., 0.1 mm or less) of the substrate 2 so that the substrate 2 can pass through. It is preferable that the gap dimension H is as small as possible. Specifically, the gap dimension H is preferably 0.1 mm or more and 1 mm or less.
[0027] The liquid reservoir 23 includes an inlet 24 that opens to the upstream side (left side in FIG. 2) in the conveying direction of the substrate 2, and an outlet 25 that opens to the downstream side (right side in FIG. 2) in the conveying direction of the substrate 2. The inlet 24 and the outlet 25 face each other in the conveying direction. The substrate 2 is introduced from the inlet 24, passes through the liquid reservoir 23, and is discharged from the outlet 25.
[0028] 3 and 4, the liquid reservoir 23 includes side portions 26 located on both sides in the width direction of the substrate 2. The side portion 26 is composed of a first side portion 26a on one side in the width direction and a second side portion 26b on the other side in the width direction. The first side portion 26a and the second side portion 26b face each other in the width direction.
[0029] At least one side surface portion 26 in the width direction includes an exposed opening 29. In this embodiment, as shown in Fig. 4, the exposed opening 29 is included in each of the side surface portions 26 on both sides in the width direction, i.e., the first side surface portion 26a and the second side surface portion 26b. Each exposed opening 29 is open from the inlet 24 side (upstream side) to the outlet 25 side (downstream side) in each of the first side surface portion 26a and the second side surface portion 26b (see Fig. 2). That is, the first side surface portion 26a and the second side surface portion 26b are open.
[0030] As shown in FIG. 4, a part of the base material 2 in the width direction can protrude from the exposure opening 29 to the outside of the liquid reservoir .
[0031] A coating liquid supply port 30 for supplying the coating liquid C to the liquid reservoir 23 is provided on the surface of the first block 21 facing the liquid reservoir 23. In this embodiment, a plurality of (e.g., three) coating liquid supply ports 30 are provided in the widthwise center of the first block 21, lined up in the transport direction. It is noted that the number of coating liquid supply ports 30 may be one.
[0032] Here, the coating liquid supply device 40 (see FIG. 1) is a device for supplying the coating liquid C to the coating device 20, and is composed of a supply pump 41 and a supply path 42. The coating liquid supply port 30 is in communication with the supply pump 41 via the supply path 42. The coating liquid C pumped by the supply pump 41 is supplied from the coating liquid supply port 30 to the liquid pool 23 through the supply path 42. This allows the coating liquid C to pool in the liquid pool 23. The cross-sectional shape of the coating liquid supply port 30 is, for example, circular or elliptical. The diameter of the coating liquid supply port 30 is preferably, for example, 1 mm or more. In addition, it is preferable that the supply speed of the coating liquid C by the supply pump 41 is approximately equal to the discharge speed of the coating liquid C discharged from the discharge port 25.
[0033] Although not shown, the coating device 20 may include a coating fluid discharge mechanism. The coating fluid discharge mechanism removes the coating fluid C accumulated in the fluid reservoir 23 when coating is stopped.
[0034] (Coating aspect) An embodiment (coating embodiment) in which a coating liquid C is applied to both sides of a substrate 2 by a coating device 20 to form coating films F on both sides of the substrate 2 will be described.
[0035] 3, a region in the width direction of the substrate 2 to which the coating liquid C is to be applied is specified, and this is designated as a specific region P. Moreover, a region in the width direction other than the specific region P is designated as a non-specific region Q to which the coating liquid C is not to be applied.
[0036] In this embodiment, the widthwise intermediate portion 2b of the base material 2 is defined as a specific portion P. On the other hand, both widthwise end portions 2a of the base material 2 other than the specific portion P (widthwise intermediate portion 2b) are defined as non-specific portions Q.
[0037] 3 and 4, the widthwise position of the substrate 2 is adjusted so that the specific portion P of the substrate 2 passes through the liquid pool 23, while each non-specific portion Q of the substrate 2 does not pass through the liquid pool 23. Specifically, each non-specific portion Q (each of both widthwise ends 2a) of the substrate 2 passing through the coating device 20 is caused to protrude from each exposed opening 29 to the outside of the liquid pool 23.
[0038] As the substrate 2 passes through the coating device 20, the coating liquid C is applied to both sides of the specific region P of the substrate 2, and a coating film F is formed on both sides of the specific region P of the substrate 2. On the other hand, the coating liquid C is not applied to both sides of each non-specific region Q of the substrate 2, and therefore no coating film F is formed thereon.
[0039] When the substrate 2 is discharged from the discharge port 25, a strong shear force is applied to the coating liquid C applied to both sides of the specific portion P of the substrate 2 in the vicinity of the discharge port 25. For this reason, as shown in Fig. 5, the thickness dimension T of the substrate 2 including the coating film F becomes slightly smaller than the gap dimension H of the discharge port 25 (liquid pool portion 23). This smoothes the surface of the coating film F, resulting in a good appearance.
[0040] (Action and effect) According to this embodiment, an exposure opening 29 is included in at least one side portion 26 in the width direction, so that a portion of the substrate 2 passing through the coating device 20 in the width direction can be protruded from the exposure opening 29 to the outside of the liquid reservoir portion 23.
[0041] That is, in the width direction of the substrate 2, the portion to which the coating liquid C is applied is defined as a specific portion P, and the portion other than the specific portion P to which the coating liquid C is not applied is defined as a non-specific portion Q. Then, the substrate 2 is passed through the coating device 20 while the non-specific portion Q of the substrate 2 is protruding from the exposure opening 29 to the outside of the liquid pool portion 23. This makes it possible to apply the coating liquid C to both sides of the specific portion P of the substrate 2 without applying the coating liquid C to both sides of the non-specific portion Q of the substrate 2.
[0042] Therefore, the coating film F can be selectively formed on both sides of the specific portion P in the width direction of the substrate 2 being transported.
[0043] In addition, in this embodiment, the exposed openings 29 are included in the first side portion 26a and the second side portion 26b on both sides in the width direction, so that when the width dimension B of the substrate 2 is larger than the width dimension L2 of each block 21, 22 (the width dimension of the liquid reservoir portion 23), both of the width direction end portions 2a of the substrate 2 can protrude from each exposed opening 29 to the outside of the liquid reservoir portion 23.
[0044] By reducing the gap dimension H to, for example, 0.1 mm to 1 mm, the ratio ρ [kg / (m 2 s)×10 3 Increasing the ratio ρ (preferably to 75 or more) is advantageous in preventing the coating liquid C from leaking out of the liquid reservoir 23. Note that the ratio ρ can also be increased by increasing the viscosity η of the coating liquid C.
[0045] By setting the viscosity η of the coating liquid C to, for example, 1 Pa·s to 1000 Pa·s, it is possible to prevent the coating liquid C from leaking out of the liquid reservoir 23, improve the surface roughness of the coating film F, reduce the pressure loss of the coating liquid C in the supply path 42, and so on.
[0046] Since the transport direction of the substrate 2 is substantially the same as the horizontal direction, the coating liquid C stored in the liquid reservoir 23 is supported by the first block 21 located below it in the vertical direction (thickness direction). This is more advantageous in preventing the coating liquid C from leaking out of the liquid reservoir 23.
[0047] By making the length dimension L1 of each block 21, 22 sufficiently large relative to the thickness dimension t of the substrate 2, it is possible to prevent coating voids on both sides of the specific portion P of the substrate 2 and to increase the coverage rate.
[0048] By increasing the diameter of the coating liquid supply port 30 to, for example, 1 mm or more, the pressure loss of the coating liquid C supplied to the liquid reservoir 23 can be reduced.
[0049] For example, in the dip coating method, the substrate is introduced into the immersion tank from an upper inlet, passed through the immersion tank, and discharged from an upper outlet. This requires changing the conveying direction of the substrate 2 many times, making the device large and complicated. In addition, it is necessary to store a large amount of coating liquid C in the immersion tank, which is disadvantageous in terms of cost, especially when expensive coating liquid C is used. According to this embodiment, the inlet 24 and the outlet 25 are opposed to each other in the conveying direction of the substrate 2, so that the device can be made smaller and simpler than the dip coating method, and the amount of coating liquid C can be reduced to reduce costs.
[0050] <Second embodiment> A coating device 20 according to a second embodiment will be described with reference to Fig. 6. In the following description, the same components as those in the above embodiment are given the same reference numerals, and detailed description thereof may be omitted.
[0051] In this embodiment, one width direction side 2c of the base material 2 is a specific portion P. On the other hand, the other width direction side 2d of the base material 2 is a non-specific portion Q.
[0052] In this embodiment, the coating liquid C is also applied to the side surface 2e on one side in the width direction of the substrate 2 to form a coating film F. Here, by making the length dimension L1 of each of the blocks 21, 22 sufficiently larger than the thickness dimension t of the substrate 2, the coating liquid C can be sufficiently applied to the side surface 2e on one side in the width direction of the substrate 2.
[0053] For example, in a coating method using a slit die, it is difficult to apply the coating liquid C to the side surface 2e of the substrate 2. Therefore, the coating device 20 according to the present embodiment is advantageous over a slit die in that it is possible to apply the coating liquid C to the side surface 2e of the substrate 2.
[0054] <Third embodiment> A coating device 20 according to a third embodiment will be described with reference to Fig. 7. In the following description, the same components as those in the above embodiment are denoted by the same reference numerals, and detailed description thereof may be omitted.
[0055] In this embodiment, the width dimension B of the substrate 2 is smaller than the width dimension L2 (width dimension of the liquid reservoir 23) of each of the blocks 21, 22. Moreover, the entire width direction of the substrate 2 is designated as a specific region P, and no non-specific region Q is provided. In other words, the coating liquid C is applied to both sides of the substrate 2 in the entire width direction to form a coating film F (full-surface coating).
[0056] In this way, it is not necessary to make a portion of the base material 2 in the width direction protrude from the exposure opening 29 to the outside of the liquid reservoir portion 23 .
[0057] In this embodiment, the coating liquid C is also applied to the side surfaces 2e on both sides of the substrate 2 in the width direction, so that a coating film F is formed.
[0058] <Fourth embodiment> A coating device 20 according to a fourth embodiment will be described with reference to Figures 8 and 9. In the following description, the same components as those in the above embodiment are given the same reference numerals, and detailed description may be omitted. Note that Figure 9 is a cross-sectional view taken along line IX-IX in Figure 8.
[0059] In this embodiment, the first block 21 and the second block 22 are each provided with a plurality of coating liquid supply ports 30 on the surface facing the liquid reservoir 23. Each coating liquid supply port 30 is for supplying the coating liquid C to the liquid reservoir 23, and is connected to a supply pump 41 via a supply path 42.
[0060] In this embodiment, each coating fluid supply port 30 is a circular hole. The number of coating fluid supply ports 30 provided in each block 21 is equal to the number of coating fluid supply ports 30 provided in each block 22. The coating fluid supply ports 30 face each other in the thickness direction, with the liquid reservoir portion 23 between them.
[0061] According to this embodiment, the coating liquid C is supplied from the first block 21 and the second block 22 to the liquid reservoir 23 so as to face each other in the thickness direction of the substrate 2, and the liquid pressure at this time can restrict the substrate 2 to the vicinity of the center in the thickness direction of the liquid reservoir 23. This allows the coating liquid C to be applied stably and uniformly to both sides of the substrate 2, and a high-quality coating film F can be formed on both sides of the substrate 2. Furthermore, restricting the substrate 2 to the vicinity of the center in the thickness direction of the liquid reservoir 23 can prevent the substrate 2 from coming into contact with the blocks 21, 22, and prevent damage to the coating film F formed on both sides of the substrate 2.
[0062] <Fifth embodiment> A coating device 20 according to a fifth embodiment will be described with reference to Fig. 10. In the following description, the same components as those in the above embodiment are denoted by the same reference numerals, and detailed description thereof may be omitted.
[0063] In this embodiment, each coating fluid supply port 30 is an elliptical long hole extending in the longitudinal direction (the transport direction of the substrate 2) of each block 21, 22. The width of each coating fluid supply port (long hole) 30 is preferably, for example, 1 mm or more. The other configurations are the same as those of the fourth embodiment.
[0064] Sixth embodiment A coating device 20 according to a sixth embodiment will be described with reference to Fig. 11. In the following description, the same components as those in the above embodiment are denoted by the same reference numerals, and detailed description thereof may be omitted.
[0065] In this embodiment, the opening edge portion 31 of the discharge port 25 in the first block 21 and the second block 22 has a thickness smaller than other portions of each block 21, 22 in the transport direction, and a wetting spread suppression portion M is formed to suppress the wetting and spreading of the coating liquid C.
[0066] That is, the wetting spread suppression portion M is formed by making the thickness dimension L3' of the opening edge portion 31 of the discharge port 25 in each block 21, 22 smaller than the thickness dimension L3 of other portions in the conveying direction of each block 21, 22. The thickness dimension L3' is preferably as small as possible, for example, preferably 5 mm or less, and more preferably 1 mm or less.
[0067] When the substrate 2 is discharged from the discharge port 25, the coating liquid C applied to both sides of the substrate 2 may spread over the surfaces of the blocks 21 and 22 on the discharge port 25 side. Therefore, according to the present embodiment, the thickness dimension L3' of the opening edge portion 31 of the discharge port 25 of each block 21 and 22 is reduced to reduce the area of the surface onto which the coating liquid C spreads. This makes it possible to prevent the coating liquid C from spreading over the surfaces of the blocks 21 and 22 on the discharge port 25 side, and to form a coating film F stably and uniformly on both sides of the substrate 2.
[0068] <Seventh embodiment> A coating device 20 according to the seventh embodiment will be described with reference to Fig. 12. In the following description, the same components as those in the above embodiment are denoted by the same reference numerals, and detailed description thereof may be omitted.
[0069] In this embodiment, the gap (liquid reservoir) 23 between the first block 21 and the second block 22 is wider on the inlet 24 side than on the outlet 25 side.
[0070] According to this embodiment, by increasing the gap dimension H1 at the inlet 24, it is possible to suppress contact between the substrate 2 and each of the blocks 21 and 22 at the inlet 24. In addition, by setting the gap dimension H2 at the outlet 25 to a predetermined value, it is possible to determine the thickness of the coating film F formed on both sides of the substrate 2.
[0071] <Eighth embodiment> A coating device 20 according to an eighth embodiment will be described with reference to Fig. 13. In the following description, the same components as those in the above embodiment are denoted by the same reference numerals, and detailed description thereof may be omitted.
[0072] In this embodiment, in addition to the seventh embodiment, the gap (liquid pool) 23 between the first block 21 and the second block 22 narrows from the inlet 24 side toward the outlet 25 side in the transport direction of the substrate 2. That is, the gap (liquid pool) 23 between the first block 21 and the second block 22 is formed in a tapered shape.
[0073] According to this embodiment, in addition to the effects of the seventh embodiment, retention of the coating liquid C in the liquid pool (gap) 23 can be suppressed.
[0074] <Ninth embodiment> A coating device 20 according to a ninth embodiment will be described with reference to Fig. 14. In the following description, the same components as those in the above embodiment are denoted by the same reference numerals, and detailed description thereof may be omitted.
[0075] In this embodiment, a plurality of punch holes 3 are formed in the base material 2. The other configurations are the same as those in the first embodiment.
[0076] According to this embodiment, the coating liquid C is also applied to the inner circumferential surfaces of the punched holes 3 formed in the substrate 2 to form a coating film F. Here, by making the length dimension L1 of each of the blocks 21, 22 sufficiently larger than the thickness dimension t of the substrate 2, the coating liquid C can be sufficiently introduced around the inner circumferential surfaces of the punched holes 3.
[0077] <Tenth embodiment> A coating device 20 according to a tenth embodiment will be described with reference to Fig. 15. In the following description, the same components as those in the above embodiment are denoted by the same reference numerals, and detailed description thereof may be omitted.
[0078] In this embodiment, both side surfaces in the width direction of the base material 2 are formed in a sawtooth shape and are provided with a plurality of teeth 4. The other configurations are the same as those of the third embodiment.
[0079] According to this embodiment, the coating liquid C is also applied to both side surfaces of each tooth 4 in the transport direction to form a coating film F. Here, by making the length dimension L1 of each block 21, 22 sufficiently larger than the thickness dimension t of the substrate 2, the coating liquid C can be sufficiently applied to both side surfaces of each tooth 4 in the transport direction.
[0080] <Eleventh embodiment> A coating device 20 according to an eleventh embodiment will be described with reference to Fig. 16. In the following description, the same components as those in the above embodiment are denoted by the same reference numerals, and detailed description thereof may be omitted.
[0081] In this embodiment, the exposure opening 29 is included only in the side surface portion 26 on one side in the width direction. Specifically, the exposure opening 29 is included only in the second side surface portion 26b on the other side in the width direction. That is, the first side surface portion 26a on one side in the width direction is closed.
[0082] The first side surface portion 26a faces vertically downward, while the second side surface portion 26b faces vertically upward, that is, the exposure opening 29 opens vertically upward.
[0083] According to this embodiment, the number of exposed openings 29 is only one, which is more advantageous than the above-described embodiment in terms of preventing the coating liquid C from leaking out of the liquid pool 23.
[0084] Moreover, by opening the exposed opening 29 included in the second side surface portion 26b vertically upward, the first side surface portion 26a can be positioned vertically below the liquid reservoir portion 23. This allows the coating liquid C stored in the liquid reservoir portion 23 to be supported by the closed first side surface portion 26a.
[0085] <Other embodiments> Although the present disclosure has been described above with reference to the preferred embodiments, such description is not limiting, and various modifications are possible.
[0086] The shape of the substrate 2 may be, for example, a comb-tooth shape or a ladder shape. In the case of a comb-tooth shape, the coating liquid C is applied to both side surfaces of each comb tooth in the transport direction to form a coating film F. The distance between the comb teeth is preferably 0.1 mm or more and 1.0 mm or less. Here, by making the length dimension L1 of each block 21, 22 sufficiently larger than the thickness dimension t of the substrate 2, for example, 100 times or more, the coating liquid C can be sufficiently introduced to the side surfaces of each comb tooth in the transport direction. The case where the substrate 2 is shaped like a ladder is generally similar to the case where the substrate 2 is shaped like a comb tooth.
[0087] The substrate 2 may be made of a porous material. In this case, the coating liquid C penetrates into each pore of the porous material to form a coating film F. By making the length dimension L1 of each block 21, 22 sufficiently larger than the thickness dimension t of the substrate 2, for example, 500 times or more, the coating liquid C penetrates sufficiently into each pore.
[0088] In the above embodiment, the conveying direction of the base material 2 is substantially the same as the horizontal direction perpendicular to the vertical direction, but is not limited thereto. The base material 2 may be conveyed, for example, from above to below in the vertical direction or from below to above in the vertical direction.
[0089] Instead of providing the supply pump 41, compressed air may be introduced into the supply tank to pressure-feed the liquid.
[0090] In the fourth and fifth embodiments, the coating liquid supply ports 30 provided in the blocks 21 and 22 face each other in the thickness direction with the liquid reservoir 23 therebetween (see FIG. 8), but this is not limited to the above. The coating liquid supply ports 30 may be positioned so as to be offset from each other in the transport direction or width direction.
[0091] In the sixth embodiment, the wetting spread suppression portion M is formed by making the thickness dimension L3' of the opening edge portion 31 of the discharge port 25 in each block 21, 22 smaller than the thickness dimension L3 of the other portion in the conveying direction of each block 21, 22, but is not limited thereto. The wetting spread suppression portion M may be formed, for example, by controlling the wettability of the surface on the discharge port 25 side of each block 21, 22. Methods for controlling the wettability include a method of controlling the surface roughness, a method of forming a film using a material having low affinity with the coating liquid C, a method of using a fluorine-based resin such as PTFE, and the like.
[0092] In the above embodiment, the coating device 20 is used to apply the coating liquid C to both sides of the substrate 2 that is continuously transported by a roll-to-roll method, but is not limited thereto. The coating device 20 may be used, for example, to apply the coating liquid C to both sides of a glass substrate that is transported by a belt conveyor.
[0093] The coating method of the present disclosure uses the coating device 20 of the above embodiment, and applies coating liquid C to both sides of a specific portion P in the width direction of the substrate 2 by passing the substrate 2 through the coating device 20 while a portion of the substrate 2 in the width direction protrudes from the exposed opening 29 to the outside of the liquid reservoir 23. EXAMPLES
[0094] <Setting conditions> (Example) The substrate 2 was made of SUS304 material having a thickness of 0.1 mm.
[0095] A conductive paste with a viscosity η of approximately 100 Pa·s was used as coating liquid C. The viscosity η of coating liquid C was measured using a rotational viscometer (Thermo Scientific Mars40, manufactured by HAAKE). The measurement conditions for viscosity η were as follows: stage diameter 20 mm, probe diameter 20 mm, angle 1°, measurement gap 0.05 mm, shear rate 1 / sec, and measurement temperature 25°C.
[0096] The coating device 20 (see Figs. 1 to 5) according to the first embodiment was used. Specifically, the coating device 20 was a tabletop coating device (Minilab, manufactured by Yasui Seiki). The first block 21 and the second block 22 were made of SUS304 material. The length dimension L1 of each block 21, 22 was 40 mm, the width dimension L2 was 50 mm, and the thickness dimension L3 was 10 mm. A total of three circular supply ports with a diameter of 2 mm were provided at the center of the width of each block 21, 22, arranged at intervals of 10 mm in the conveying direction.
[0097] A mono pump (3HMC010F, manufactured by Heishin Soubi) was used as the supply pump 41. The unwinding torque and winding torque of the substrate supplying device 10 were both set to 60 N·m.
[0098] The gap dimension H between the first block 21 and the second block 22 was set arbitrarily using a shim. The coating speed (conveying speed) was set arbitrarily.
[0099] After the formation of the coating film F, it was dried for 30 minutes using a hot air drying oven (DKM-400, manufactured by Yamato Scientific) at a set temperature of 200° C. and a fan rotation speed of 500 rpm to obtain a dried film.
[0100] (Comparative Example) A conventional coating device different from that of the present disclosure was used. The conditions of the coating liquid C and the substrate 2 were the same as those of the example.
[0101] <Measurement conditions> The thickness of the coating F was measured using a micrometer (Mitutoyo). The thickness was calculated by subtracting the thickness dimension t of the substrate 2 before the coating F was formed from the thickness dimension T of the substrate 2 after the coating F was formed (see Figure 5). The average thickness was calculated from the measurements taken at 5 mm intervals in the coating direction (transport direction). The standard deviation 3σ was calculated from the measurements taken at 5 points, and the value was divided by the average thickness (expressed as a percentage) to determine the thickness variation. The surface roughness was measured as the arithmetic mean roughness using a one-shot 3D shape measuring instrument (VR-3200, Keyence).
[0102] <Measurement results> Example 1 The gap dimension H was 0.2 mm, and the coating speed (transport speed) was 0.2 m per minute. The average film thickness was 7.6 μm, the film thickness variation was 28%, and the surface roughness was 2.5 μm, which were good results.
[0103] Example 2 The gap dimension H was 0.2 mm, and the coating speed (transport speed) was 0.5 m per minute. The average film thickness was 14.8 μm, the film thickness variation was 29%, and the surface roughness was 2.0 μm, which were good results.
[0104] Example 3 The gap dimension H was 0.2 mm, and the coating speed (transport speed) was 1 m per minute. The average film thickness was 17.9 μm, the film thickness variation was 29%, and the surface roughness was 2.8 μm, which were good results.
[0105] Example 4 In contrast to Example 1, a cut was formed in the substrate 2. The other conditions were the same as those in Example 1. A coating film F was also formed on the side surface of the cut in the substrate 2.
[0106] Comparative Example 1 Roll transfer was used. The gap between the roll and the substrate 2 was 0 mm, and the coating speed (transport speed) was 1 m per minute. The average film thickness was 7.2 μm, the film thickness variation was 65%, and the surface roughness was 3.8 μm, and the film thickness variation and surface roughness were worse than those in Examples 1 to 4.
[0107] Comparative Example 2 A slit die was used. The gap between the slit die and the substrate 2 was 0.05 mm, and the coating speed (conveying speed) was 1 m per minute. The average film thickness was 15.0 μm, the film thickness variation was 31%, and the surface roughness was 3.3 μm, which were better results than those of Comparative Example 1. However, if the film thickness was reduced any further, coating defects occurred, making it difficult to form a uniform coating film.
[0108] Comparative Example 3 In Comparative Example 2, a cut was formed in the substrate 2. The other conditions were the same as those in Comparative Example 2. No coating film F was formed on the side surface of the cut in the substrate 2. [Industrial Applicability]
[0109] The present disclosure can be applied to a coating apparatus and a coating method, and is therefore extremely useful and has high industrial applicability. [Explanation of symbols]
[0110] X conveying direction Y Width direction Z thickness direction P Specific part Q Non-specific parts H Gap dimension H1 Gap dimension H2 Gap dimension C Coating liquid F Paint film M Wetting and spreading suppression part 2 Base material 20 Coating equipment 21 1st Block (Pair of Blocks) 22 2nd Block (Pair of Blocks) 23 Liquid reservoir (gap) 24 Introduction 25 Outlet 26 Side part 26a 1st side part 26b Second side part 29 Exposed mouth 30 Coating fluid supply port 31 Opening edge
Claims
1. A coating device that applies a coating liquid to both sides of a sheet-like substrate being transported, A pair of blocks facing each other in a thickness direction of the base material; a liquid pool portion formed in a gap between the pair of blocks so that the coating liquid can be pooled and through which the substrate can pass, The liquid reservoir is an inlet opening that opens to an upstream side in a conveying direction of the base material and through which the base material is introduced; a discharge port that opens on a downstream side in the conveying direction and through which the base material is discharged; and side portions located on both sides in a width direction intersecting the conveying direction, At least one of the side surfaces in the width direction includes an exposure opening extending from the inlet to the outlet, a portion of the base material in the width direction can protrude from the exposure opening to an outside of the liquid reservoir, In the coating device, each of the blocks is formed in a substantially rectangular parallelepiped shape and is arranged such that the longitudinal direction thereof is aligned with the transport direction of the base material.
2. In claim 1, The exposure opening is included in each of the side portions on both sides in the width direction.
3. In claim 1, The exposure opening is included only in one of the side surface portions in the width direction, The exposure port is open vertically upward.
4. In any one of claims 1 to 3, each of the pair of blocks is provided with a coating liquid supply port on a surface facing the liquid reservoir, the coating liquid being supplied to the liquid reservoir; The coating liquid supply ports are opposed to each other across the liquid reservoir.
5. In any one of claims 1 to 4, The gap is wider on the inlet side than on the outlet side.
6. In claim 5, The gap narrows from the inlet side to the outlet side in the conveying direction.
7. In any one of claims 1 to 6, a coating device in which an opening edge portion of the discharge port in the pair of blocks has a thickness smaller than that of other portions of the pair of blocks in the transport direction, and a wetting spread suppression portion is formed to suppress the wetting and spreading of the coating liquid.
8. In any one of claims 1 to 7, The gap is equal to or greater than 0.1 mm and equal to or less than 1 mm.
9. In any one of claims 1 to 8, The blocks are arranged symmetrically in the thickness direction of the base material.
10. 10. A coating method using the coating device according to claim 1 , wherein the coating liquid is applied to both surfaces of a specific portion of the substrate in the width direction by passing the substrate through the coating device while causing a portion of the substrate in the width direction to protrude from the exposure opening to the outside of the liquid reservoir.
Citation Information
Patent Citations
Method and device for coating high-viscosity material
JP1989007965A
Coating device and coating method
JP1999221512A
Manufacturing apparatus and method for battery electrode
JP2017147035A
Coating device and coating system
WO2019181916A1