Light emitting device and method for manufacturing the same
The light emitting device addresses thermal expansion issues by using a notched resin substrate and thicker wiring electrodes to balance stress, reducing warpage and improving yield.
Patent Information
- Application Number
- JP2021072385
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-04-22
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2041-04-22
AI Technical Summary
The existing side-emitting surface-mounted light emitting diodes face issues due to thermal expansion differences between the manufacturing substrate and sealing resin, leading to warpage and potential cracks during heat treatment, which affect manufacturing yield.
A light emitting device design with a resin substrate featuring notches and through holes, thicker wiring electrodes on the lower surface, and a light-reflective resin body to balance thermal expansion, reducing warpage by equalizing stress distribution.
The design effectively minimizes warpage and improves manufacturing yield by balancing thermal expansion, preventing cracks and enhancing the reliability of the light emitting device.
Smart Images

Figure 0007581116000001 
Figure 0007581116000002 
Figure 0007581116000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a light emitting device and a method for manufacturing a light emitting device. [Background technology]
[0002] 2. Description of the Related Art A light-emitting device that uses a light-emitting element such as a light-emitting diode (LED) as a light source and is made up of a flat mounting substrate, a light-emitting element disposed on the mounting substrate, and a sealing resin disposed to cover the light-emitting element is known as a small light-emitting device.
[0003] Further, a side emission type (hereinafter also referred to as a side view type) light emitting device is known in which an external electrode is formed on one side surface of the light emitting device, and the one side surface serves as a mounting surface.
[0004] For example, Patent Document 1 discloses a side-emitting surface-mounted light-emitting diode in which a light-emitting diode element is disposed on a flat production substrate having a rectangular upper surface shape made of a glass epoxy insulating base material, a thin metal plate, and copper foil, and a sealing resin part made of a light-transmitting resin is formed on the production substrate so as to cover the light-emitting diode element. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2003-188424 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, in the side-emitting surface-mount light-emitting diode disclosed in Patent Document 1, the amount of warping of the manufacturing substrate may change between high temperatures and room temperatures due to the difference in thermal expansion coefficient between the manufacturing substrate and the encapsulating resin portion when the light-emitting element is mounted on the mounting substrate. This change in the amount of warping of the manufacturing substrate may cause problems such as cracks in the solder or cracks in the mounted light-emitting diode element.
[0007] The present invention has been made in consideration of the above points, and aims to provide a light-emitting device and a manufacturing method thereof that can improve manufacturing yields by reducing the change in the amount of warping of the mounting substrate between high temperatures and room temperature during heating treatment etc. during manufacturing. [Means for solving the problem]
[0008] The light emitting device according to the present invention includes a flat resin substrate having a planar shape in which a first region including a vertex at one end of one long side of a rectangle and a second region including a vertex at the other end are cut out, and having a first through hole and a second through hole penetrating from a first main surface to a second main surface, a first wiring electrode made of metal having an electrode portion filling the first through hole, and a wiring portion extending from the electrode portion on the second main surface side through a side surface of the resin substrate facing the first region to the first main surface and exposing a region along the other long side of the rectangle of the resin substrate on the first main surface and the second main surface, and an electrode portion filling the second through hole, and a wiring portion extending from the electrode portion on the second main surface side through a side surface of the resin substrate facing the second region to the first main surface and exposing a region along the other long side of the rectangle of the resin substrate on the first main surface and the second main surface. the second wiring electrode made of a metal having a main surface and a wiring portion exposing a region along the other long side of the rectangle of the resin substrate on the second main surface; a light-emitting element mounted on the electrode portion of the first wiring electrode and the second wiring electrode on the first main surface side of the resin substrate; and a light-reflective resin body covering the first main surface of the resin substrate, covering the wiring portions of the first wiring electrode and the second wiring electrode on the first main surface and forming a frame body surrounding the light-emitting element, and covering the region exposed from the first wiring electrode and the second wiring electrode on the second main surface of the resin substrate, wherein the first wiring electrode and the second wiring electrode have a thickness greater on the second main surface than on the first main surface.
[0009] Furthermore, a method for manufacturing a light emitting device according to the present invention includes a resin substrate preparation step of preparing a resin substrate having a first main surface on which a plurality of element mounting regions are defined in a rectangular shape by grid-like parting lines; a copper foil attachment step of attaching a first copper foil onto the first main surface of the resin substrate and attaching a second copper foil having a thickness greater than that of the first copper foil onto a second main surface of the resin substrate opposite to the first main surface; a substrate shape formation step of forming a cutout portion that cuts out a first region including a vertex at one end of one long side of the rectangle and a second region including a vertex at the other end, and forming a first through hole and a second through hole by penetrating two regions of the element mounting region from the first copper foil to the second main surface; the first copper foil, the second copper foil, and the metal layer on the first main surface and the second main surface being patterned into the shapes of a first wiring electrode and a second wiring electrode; a resin body forming process for forming a light-reflective resin body on the first main surface to form a frame body surrounding the element mounting area and covering the areas of the second main surface that are exposed from the first wiring electrode and the second wiring electrode; and an element bonding process for mounting a light-emitting element on the first main surface side on the upper surfaces of the first wiring electrode and the second wiring electrode. [Brief description of the drawings]
[0010] [Figure 1] 1 is a perspective view of a light emitting device according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a perspective view of a resin substrate of the light emitting device according to the embodiment of the present invention. [Diagram 3] 2 is a perspective view of a resin substrate and wiring electrodes of a light emitting device according to an embodiment of the present invention. FIG. [Figure 4] 2 is a top view of a resin substrate and wiring electrodes of a light emitting device according to an embodiment of the present invention. FIG. [Diagram 5] FIG. 2 is a top view of a light emitting device according to an embodiment of the present invention. [Figure 6]1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention. [Figure 7] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention. [Figure 8] 5A to 5C are diagrams illustrating a manufacturing flow of the light emitting device according to the embodiment of the present invention. [Figure 9] 5A to 5C are diagrams illustrating a manufacturing flow of the light emitting device according to the embodiment of the present invention. [Figure 10] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 11] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 12] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 13] 1 is a top view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 14] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 15] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 16] 1 is a top view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 17] 1 is a top view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 18] 1 is a top view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 19] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 20] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 21] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 22] 1 is a cross-sectional view of a light emitting device according to an embodiment of the present invention at one step during manufacturing. [Figure 23]FIG. 13 is a top view of a light emitting device according to a modified example of the present invention. [Figure 24] 13 is a top view of a resin substrate and wiring electrodes according to a modified example of the present invention. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS EXAMPLES
[0011] An embodiment of the present invention will be described in detail with reference to Figures 1 to 7. In the following description and the accompanying drawings, substantially the same or equivalent parts are given the same reference symbols. In the following description, the term "material 1 / material 2" refers to a laminated structure in which material 2 is laminated on material 1. Furthermore, the term "material 1-material 2" refers to an alloy of materials 1 and 2.
[0012] FIG. 1 shows a perspective view of the light emitting device 100. FIG. 2 shows a perspective view of the resin substrate 10. FIG. 3 shows a perspective view of the resin substrate 10, the first wiring electrode 20, and the second wiring electrode 30. FIG. 4 shows a top view of the resin substrate 10, the first wiring electrode 20, and the second wiring electrode 30. FIG. 5 shows a top view of the light emitting device 100. FIG. 6 shows a cross-sectional view of the light emitting device 100 of FIG. 5 taken along line AA. FIG. 7 shows a cross-sectional view of the light emitting device 100 of FIG. 5 taken along line BB.
[0013] The light emitting device 100 includes a resin substrate 10, a first wiring electrode 20 and a second wiring electrode 30 formed on the resin substrate 10, a resin body 50 formed to have a cavity on the resin substrate 10, a light emitting element 60 disposed on the resin substrate 10, and a sealing resin 70 filled in the cavity of the resin body 50 so as to cover the light emitting element 60. Note that in Fig. 5, the sealing resin 70 is omitted in order to show the structure inside the cavity of the resin body 50.
[0014] The resin substrate 10 is, for example, a flat-plate-shaped substrate made of an insulating base material and having an upper surface 10S1 as a first main surface and a lower surface 10S2 as a second main surface. The resin substrate 10 is, for example, a plate-shaped insulating substrate made of glass epoxy obtained by impregnating glass fiber with epoxy resin and subjecting it to a heat curing treatment.
[0015] As shown in FIG. 2, the resin substrate 10 has a first through hole 11 and a second through hole 12 that are spaced apart from each other and pass through the substrate 10 from the upper surface 10S1 to the lower surface 10S2.
[0016] 2, the resin substrate 10 has a cutout portion 13 formed by cutting out a first region NT1 including a vertex at one end of a first long side 10E, which is one of the long sides, from the top surface shape of the rectangle 10R. Also, the resin substrate 10 has a cutout portion 14 formed by cutting out a second region NT2 including a vertex at the other end of the first long side 10E from the top surface shape of the rectangle 10R, as shown in FIG.
[0017] In other words, the light emitting device 100 has a flat resin substrate 10 having a planar shape in which cutout portions 13 and 14 are formed by cutting out a first region NT1 including a vertex at one end of a first long side 10E, which is one of the long sides of the rectangle 10R, and a second region NT2 including a vertex at the other end, and having a first through hole 11 and a second through hole 12 that penetrate from the upper surface 10S1 to the lower surface 10S2.
[0018] The resin substrate 10 has cutouts 13, 14 at both ends of the first long side 10E, but no cutout is formed at the end of the second long side opposite the first long side 10E, and the end of the second long side is formed at a right angle with the adjacent short side.
[0019] Further, the resin substrate 10 has a third through hole 15 and a fourth through hole 16, each of which has a semicircular or semi-elliptical shape and penetrates from the upper surface 10S1 to the lower surface 10S2 so as to contact the side surface of the short side and the cutout portions 13 and 14, respectively, of the rectangle 10R. In addition, in Fig. 4, the area defined by the two-dot chain line indicates the area in which the through holes are formed and the cutout area in the resin substrate 10. That is, the area defined by the two-dot chain line indicates each end of the first through hole 11, the second through hole 12, the cutout portion 13, and the cutout portion 14, that is, the end of the resin substrate 10.
[0020] The resin substrate 10 has a first wiring electrode 20 and a second wiring electrode 30, which are a pair of wiring electrodes formed apart from each other. Each of the first wiring electrode 20 and the second wiring electrode 30 has a first electrode portion 21 and a second electrode portion 31 as electrode portions filling the first through hole 11 and the second through hole 12 of the resin substrate 10. Each of the first wiring electrode 20 and the second wiring electrode 30 has a first wiring portion 22 and a second wiring portion 32 as wiring portions extending from each of the first electrode portion 21 and the second electrode portion 31 on the lower surface 10S2 side of the resin substrate 10 through each side surface of the cutout portions 13 and 14 to the upper surface 10S1.
[0021] In other words, the light emitting device 100 has a first wiring electrode 20 made of a metal having a first electrode portion 21 filling the first through hole 11 and a first wiring portion 22 which is a wiring portion extending from the first electrode portion 21 on the lower surface 10S2 side through a side surface facing the notch portion 13 of the resin substrate 10 to the upper surface 10S1. The light emitting device 100 also has a second wiring electrode 30 made of a metal having a second electrode portion 31 filling the second through hole 12 and a second wiring portion 32 which extends from the second electrode portion 31 on the lower surface 10S2 side through a side surface facing the notch portion 14 of the resin substrate 10 to the upper surface 10S1. The first wiring electrode 20 and the second wiring electrode 30 are made of copper.
[0022] In addition, in Fig. 4, the regions defined by solid lines so as to surround each of the first through holes 11 and the second through holes 12 indicate the ends of the first electrode portion 21 and the second electrode portion 31 formed on the upper surface 10S1 side of the resin substrate 10, respectively, in a top view. In addition, in Fig. 4, the first wiring portion 22 and the second wiring portion 32 indicated by dashed lines indicate the ends of the first wiring portion 22 and the second wiring portion 32 formed on the lower surface 10S2 side of the resin substrate 10, respectively, in a top view. In addition, in Fig. 4, the first wiring portion 22 and the second wiring portion 32 indicated by dashed lines indicate the ends of the first wiring portion 22 and the second wiring portion 32 formed on the upper surface 10S1 side of the resin substrate 10, respectively, in a top view.
[0023] Each of the first wiring electrode 20 and the second wiring electrode 30 is a metal electrode made of, for example, copper. Each of the first wiring electrode 20 and the second wiring electrode 30 is made of, for example, copper foil formed on the upper surface 10S1 and the lower surface 10S2 of the resin substrate 10 by a manufacturing method described later, and copper formed by plating on the exposed surface of the copper foil.
[0024] As shown in Figs. 3, 4 and 6, the first electrode portion 21 is formed to fill the first through hole 11 of the resin substrate 10. The second electrode portion 31 is formed to fill the second through hole 12 of the resin substrate 10. The first electrode portion 21 and the second electrode portion 31 are formed to protrude upward from the upper surface 10S1 of the resin substrate 10. The upper surfaces of the first electrode portion 21 and the second electrode portion 31 are formed to be at approximately the same height from the upper surface 10S1 of the resin substrate 10.
[0025] A light emitting element is mounted on the first electrode portion 21 and the second electrode portion 31 via an element bonding layer, and the first electrode portion 21 and the second electrode portion 31 are electrically connected to the electrodes of the light emitting element.
[0026] As shown in Figures 4, 6 and 7, each of the first wiring portion 22 and the second wiring portion 32 is formed on the lower surface 10S2 of the resin substrate 10 so as to cover each of the first electrode portion 21 and the second electrode portion 31 formed in the first through hole 11 and the second through hole 12, respectively.
[0027] Furthermore, the first wiring portion 22 and the second wiring portion 32 are each formed on the lower surface 10S2 of the resin substrate 10 so as to extend from the first electrode portion 21 and the second electrode portion 31 to a side surface along the first long side 10E.
[0028] Moreover, each of the first wiring portion 22 and the second wiring portion 32 is formed so as to fill each of the cutout portions 13 and 14 of the resin substrate 10 and extend to the upper surface 10S1 through the cutout portions 13 and 14. Moreover, each of the upper surfaces of the first wiring portion 22 and the second wiring portion 32 is formed so that the height from the upper surface 10S1 of the resin substrate 10 is substantially the same as the height of each of the upper surfaces of the first electrode portion 21 and the second electrode portion 31.
[0029] As shown in FIG. 2 and FIG. 3, each of the first wiring portion 22 and the second wiring portion 32 is formed in a region along the side surface of each of the third through hole 15 and the fourth through hole 16 on the short side of the rectangle 10R of the resin substrate 10. Also, each of the first wiring portion 22 and the second wiring portion 32 is formed on the short side of the rectangle 10R of the resin substrate 10 from the region where each of the third through hole 15 and the fourth through hole 16 is formed to the region along the first long side 10E. Also, each of the first wiring portion 22 and the second wiring portion 32 is formed so as to expose a region along the second long side opposite to the first long side 10E on the lower surface 10S2 of the resin substrate 10. In other words, the first wiring electrode 20 and the second wiring electrode 30 expose a region along the second long side of the rectangle 10R of the resin substrate 10 on the upper surface 10S1 and the lower surface 10S2.
[0030] The first wiring portion 22 and the second wiring portion 32 are exposed on the mounting surface of the light emitting device 100 to form a terminal electrode surface. The first wiring portion 22 and the second wiring portion 32 are also exposed on a side surface adjacent to the mounting surface of the light emitting device 100 to form a vertical corner. This vertical corner is formed without metal burrs by a method to be described later, and therefore the mounting accuracy of the light emitting device 100 can be improved.
[0031] Further, each of the first wiring portion 22 and the second wiring portion 32 is covered with resist RE on the upper surface 10S1 of the resin substrate 10 except for the side surfaces along the side surfaces of the rectangle 10R of the resin substrate 10 and the side surfaces along the side surfaces of the third through hole 15 and the fourth through hole 16. In other words, each of the first and second wiring portions 22 and 32 of the first wiring electrode 20 and the second wiring electrode 30 is covered with resist RE on the upper surface 10S1 except for the side surfaces along the side surfaces of the resin substrate 10.
[0032] Therefore, the surfaces of the first wiring portion 22 and the second wiring portion 32 that are on the upper surface 10S1 of the resin substrate 10 and that are parallel to the upper surface 10S1 are covered with the resin body 50 via the resist RE.
[0033] In this embodiment, the resist RE is formed in an area that covers the upper and side surfaces of the portions of the first wiring electrode 20 and the second wiring electrode 30 that are formed on the upper surface 10S1 of the resin substrate 10 and reaches the upper surface 10S1 of the resin substrate 10.
[0034] The resist RE is formed on the upper surface 10S1 of the resin substrate 10 to a region that is approximately 100 μm or more from the ends of the first wiring electrode 20 and the second wiring electrode 30. That is, as shown in Fig. 4, the resist RE on the resin substrate 10 is formed in a region that extends from the ends, in a top view, of the first wiring portion 22 and the second wiring portion indicated by the dashed lines to the upper surface 10S1 of the resin substrate 10.
[0035] In addition, on each of the first wiring electrode 20 and the second wiring electrode 30, a metal film made of nickel (Ni) / gold (Au) (not shown) is formed in order from the surface of the first wiring electrode 20 and the second wiring electrode 30 on each surface except for the side surface along the side surface of the rectangle 10R of the resin substrate 10, the side surface along the side surface of each of the third through hole 15 and the fourth through hole 16, and the surface covered with the resist RE. That is, the metal film made of nickel (Ni) / gold (Au) is not formed on the cut surface by dicing, the area covered with the resist RE, and the side surface area along the inner wall surface of the third through hole 15 and the fourth through hole in the first wiring part 22 and the second wiring part 32, which will be described later. Note that a metal film made of gold (Au) can be formed arbitrarily on the cut surface by dicing. In other words, the first and second electrode portions 21 and 31 of the first wiring electrode 20 and the second wiring electrode 30 have metal layers in which nickel and gold are laminated in this order on their surfaces exposed from the resin substrate 10. That is, a metal film made of nickel (Ni) / gold (Au) is formed on the upper and side surfaces of the portions of the first electrode portion 21 and the second electrode portion 31 that protrude above the upper surface 10S1 of the resin substrate 10.
[0036] The first wiring portion 22 and the second wiring portion 32 on the upper surface 10S1 of the resin substrate 10 are not provided with a metal film made of nickel (Ni) / gold (Au), but are made of copper foil and copper plating film. In other words, the resist RE is formed on the copper plating film.
[0037] The Ni / Au metal film formed as the metal film, particularly the Au on the outermost surface, has low adhesion to the resist RE and resin materials such as the resin body 50 described below. Therefore, by forming the resist RE on a surface composed of copper foil and copper plating, and by contacting the resist RE with the resin body 50, it is possible to suppress peeling between the resin body 50 and the first wiring portion 22 and the second wiring portion 32. In addition, the side regions along the inner wall surfaces of the third through hole 15 and the fourth through hole in the first wiring portion 22 and the second wiring portion 32 are composed of copper foil and copper plating and are in direct contact with the resin body 50, so that it is possible to suppress peeling between the resin body and the first wiring portion 22 and the second wiring portion 32.
[0038] As shown in Figs. 1 and 5 to 7, the resin body 50 is formed on the upper surface 10S1 of the resin substrate 10 so as to have a concave cavity on the upper surface. The resin body 50 is formed so as to fill the third through hole 15 and the fourth through hole 16, and to cover the entire area of the lower surface 10S2 of the resin substrate 10 except for the area where the first wiring portion 22 and the second wiring portion 32 are formed. The resin body 50 is made of, for example, titanium oxide (TiO 2 The white resin is made of particles having light scattering properties such as ruthenium oxide, etc., and a thermosetting resin material such as a silicone resin in which the particles are dispersed.
[0039] The resin body 50 is formed on the upper surface 10S1 of the substrate 10 so as to cover the resist RE. The resin body 50 is formed so as to expose the upper surfaces of the first electrode portion 21 and the second electrode portion 31 at the bottom surface of the concave cavity. The resin body 50 is formed on the lower surface 10S2 of the substrate 10 so as to expose the lower surfaces of the first wiring portion 22 and the second wiring portion 32 and the side surfaces along the side surfaces of the rectangle 10R of the substrate 10. The resin body 50 is formed on the lower surface 10S2 of the substrate 10 so as to fill the gap between the first wiring portion 22 and the second wiring portion 32 with a thickness such that the bottom surface of the resin body 50 and the lower surfaces of the first wiring portion 22 and the second wiring portion 32 are on the same plane.
[0040] That is, the resin body 50 forms a frame surrounding a light-emitting element 60 described below on the upper surface 10S1 of the resin substrate 10. In other words, the light-emitting device 100 has a light-reflective resin body 50 that covers the upper surface 10S1 of the resin substrate 10, covers the first and second wiring portions 22 and 32 of the first wiring electrode 20 and the second wiring electrode 30 on the upper surface 10S1, forms a frame surrounding the light-emitting element 60, and covers the areas of the lower surface 10S2 of the resin substrate 10 that are exposed from the first wiring electrode 20 and the second wiring electrode 30.
[0041] The resin body 50 is formed so as to sandwich the resin substrate 10, in particular so as to continuously sandwich the second long side opposite to the first long side 10E of the resin substrate 10. The resin body 50 is formed so as to sandwich a corner portion formed by the second long side of the resin substrate 10 and the adjacent short side.
[0042] The resin body 50 is formed by filling the third through hole 15 and the fourth through hole 16 adjacent to the cutout portions 13, 14. Therefore, the resin body 50 is formed so as to contact the inner surfaces exposed in the third through hole 15 and the fourth through hole 16 of the first wiring portion 22 and the second wiring portion 32, respectively.
[0043] The side of the resin body 50 is a cut surface formed by the singulation process of the light-emitting device 100 described later, and is formed on the same plane as the side of the resin substrate 10, the side of the resist RE, the first wiring section 22, and the second wiring section 32, as shown in FIG. 1, to constitute the side of the light-emitting device 100.
[0044] In this embodiment, the first wiring portion 22 and the second wiring portion 32 exposed on the side surface along the first long side 10E of the resin substrate 10 function as terminal electrode surfaces when the light emitting device 100 is mounted on a mounting substrate. That is, the light emitting device 100 is a side-view type light emitting device in which the side surface along the first long side 10E of the resin substrate 10 functions as a mounting surface.
[0045] Moreover, the resin body 50 is formed in the cavity so that each of the inner surfaces formed on the short side of the rectangle 10R of the resin substrate 10 has an incline. The inclined inner surface guides and collects light emitted from the light emitting element 60 and the sealing resin 70 described below toward the upper surface of the light emitting device 100 (the cavity opening direction).
[0046] As shown in FIG. 6, the light emitting element 60 is mounted on each of the first electrode portion 21 and the second electrode portion 31 via an element bonding layer 61. The light emitting element 60 is a semiconductor light emitting element that emits blue light and has a gallium nitride semiconductor layer formed on one main surface of a light-transmitting growth substrate such as sapphire. The semiconductor layer is formed, for example, in the order of an n-type gallium nitride layer (n-GaN), an indium gallium nitride (InGaN) quantum well type light emitting layer, and a p-type gallium nitride layer (p-GaN) from the growth substrate side. In addition, electrodes electrically connected to each of the n-GaN layer and the p-GaN layer are provided on the surface of the light emitting element 60 on which the semiconductor layer is formed, and the electrode provided on the n-GaN layer functions as a cathode electrode of the light emitting element 60, and the electrode provided on the p-GaN functions as an anode electrode. The light emitting element 60 is mounted over the upper surfaces of the first electrode portion 21 and the second electrode portion 31 with the semiconductor layer as the lower surface. That is, the surface of the light emitting element 60 on which the electrodes are formed and the upper surfaces of the first electrode portion 21 and the second electrode portion 31 are bonded via the element bonding layer 61. In other words, the light emitting device 100 has the light emitting element 60 mounted on the first and second electrode portions 21 and 31 of the first wiring electrode 20 and the second wiring electrode 30 on the upper surface 10S1 side of the resin substrate 10.
[0047] The light emitting element 60 is bonded to the upper surfaces of the first electrode portion 21 and the second electrode portion 31 in a flip-chip manner in which light emitted from the semiconductor layer is transmitted through the growth substrate and emitted upward. That is, the light emitting element 60 functions as a light extraction surface in which a semiconductor layer including a light emitting layer is formed on the lower surface side and light is emitted from the upper surface side. In this embodiment, the light emitting element 60 is a light emitting element in a flip-chip manner, but the manner of the light emitting element 60 is not limited to this. Specifically, a light emitting element may be mounted having a conductive support substrate and a semiconductor layer including a light emitting layer and an electrode pad formed on the upper surface of the support substrate. In this case, the light emitting element is placed on one of the first electrode portion 21 or the second electrode portion 31, and the electrode pad of the light emitting element and the other of the first electrode portion 21 or the second electrode portion 31 are connected by a conductive wire.
[0048] The element bonding layer 61 is, for example, a conductive adhesive of the same material. The element bonding layer 61 is made of, for example, a paste containing a mixture of gold (Au)-tin (Sn) alloy particles. The paste is applied to the upper surface of each of the first electrode portion 21 and the second electrode portion 31, and the electrodes of the light emitting element 60 are placed on the paste so as to contact each other, and then heated. As a result, the Au-Sn particles contained in the paste melt and undergo a eutectic reaction with the Au layer on the surface of each of the first electrode portion 21 and the second electrode portion 31, and each electrode of the light emitting element 60 is eutectic-bonded to each of the first electrode portion 21 and the second electrode portion 31. The material of the element bonding layer 61 is not limited to the Au-Sn paste, and materials such as solder paste and silver paste may be used.
[0049] The sealing resin 70 is a resin layer that is filled in the cavity of the resin body 50 and formed so as to cover the light emitting elements 60. The sealing resin 70 may contain a wavelength conversion material, a light scattering material, and the like. In this embodiment, the sealing resin 70 is a wavelength conversion body in which phosphor particles that perform wavelength conversion on the light emitted from each of the light emitting elements 60 are dispersed in a thermosetting resin material such as a light-transmitting silicone resin. The phosphor particles are, for example, yttrium aluminum garnet (YAG:Y) doped with cerium (Ce). 3 Al 5 O12 In this embodiment, the sealing resin 70 is a wavelength converter that converts the wavelength of part of the blue light emitted by the light emitting element 60 and emits white light.
[0050] In this embodiment, the light emitting device 100 is manufactured by forming a plurality of light emitting devices 100 in a matrix on a flat resin substrate 10 and dividing the light emitting device 100 by dicing. That is, each side surface of the light emitting device 100 in a direction perpendicular to the upper surface 10S1 of the resin substrate 10 is a cut surface by dicing. Each of the first wiring electrode 20, the second wiring electrode 30, and the resist RE formed in the region along each side of the rectangle 10R of the resin substrate 10 is exposed on the side surface of the light emitting device 100 corresponding to the region. In addition, the cut surfaces of the first wiring electrode 20 and the second wiring electrode 30 exposed on the side surface of the light emitting device 100 are plated with a metal layer of Au after dicing.
[0051] The resin substrate 10 is a plate-shaped substrate made of glass epoxy obtained by impregnating glass fiber with epoxy resin and subjecting it to a heat curing treatment, and has a thermal expansion coefficient of about 10 to 20 ppm / K. Each of the first wiring electrode 20 and the second wiring electrode 30 is a metal mainly made of copper, and has a thermal expansion coefficient of about 16.8 ppm / K. The resin substrate 10 contains glass fiber, and therefore the thermal expansion coefficients of the resin substrate 10 and the first wiring electrode 20 and the second wiring electrode 30 can be made close to each other. On the other hand, the resin body 50 is a resin mainly made of silicone resin, and has a thermal expansion coefficient of about 200 to 300 ppm / K. In other words, the resin body 50 has a higher thermal expansion coefficient than the resin substrate 10, the first wiring electrode 20, and the second wiring electrode 30.
[0052] Due to the difference in thermal expansion coefficient between the resin substrate 10, the first wiring electrode 20, the second wiring electrode 30, and the resin body 50, the warping behavior may vary between the time of heat treatment and the time of room temperature. For example, when cooled after the heat treatment for eutectic bonding of the light emitting element 60 on the first wiring electrode 20 and the second wiring electrode 30, the resin body 50 shrinks more than the resin substrate 10 and each wiring electrode. As a result, the resin substrate 10, the first wiring electrode 20, the second wiring electrode 30, and the resin body 50 exhibit upward concave warping behavior. In addition, the warping is prominent in the direction along the long side direction of the substrate 10. In addition, the concave warping may cause manufacturing defects such as cracks in the light emitting element 60 mounted on the first wiring electrode 20 and the second wiring electrode 30.
[0053] In this embodiment, as shown in FIG. 4, on the underside 10S2 of the substrate 10, each of the first wiring portion 22 and the second wiring portion 32 is formed so as to expose an area along a second long side opposite to the first long side 10E of the rectangle 10R of the substrate 10.
[0054] In this embodiment, the first wiring portion 22 and the second wiring portion 32 are arranged such that the resin body 50 is formed on both ends of the region along the second long side of the rectangle 10R of the substrate 10 on the lower surface 10S2 of the substrate 10. That is, the resin body 50 can be formed on the lower surface 10S2 of the substrate 10 along both ends of the direction along the second long side facing the mounting surface of the light emitting device 100.
[0055] If each of the first wiring portion 22 and the second wiring portion 32 is formed up to a region along the second long side opposite to the first long side 10E of the rectangle 10R of the substrate 10, the resin body 50 arranged on the lower surface 10S2 side of the substrate 10 is interrupted in the direction along the long side of the light emitting device 100. In this case, stress caused by shrinkage of the resin body 50 arranged on the upper surface 10S1 of the substrate 10 after heat treatment is concentrated in the interrupted region of the resin body 50 on the lower surface of the substrate 10, which may cause warping.
[0056] In this embodiment, by forming the resin body 50 on the lower surface 10S2 of the substrate 10 in a direction along the long side, it is possible to suppress the concentration of stress when the resin body 50 arranged on the upper surface 10S1 of the substrate 10 shrinks after heat treatment.
[0057] In this embodiment, the thickness of the first wiring portion 22 and the second wiring portion 32 on the lower surface side of the substrate 10 is formed to be larger than the thickness of the upper surface 10S1 side of the substrate 10. More preferably, the thickness of the first wiring portion 22 and the second wiring portion 32 on the lower surface side of the substrate 10 is formed to be larger than the sum of the thickness of the upper surface 10S1 side of the substrate 10 and the thickness of the resin substrate 10. In other words, the first wiring electrode 20 and the second wiring electrode 30 are thicker on the lower surface 10S2 than on the upper surface 10S1. Also, the thickness of each of the first wiring electrode 20 and the second wiring electrode 30 on the lower surface 10S2 is larger than the sum of the thickness of the resin substrate 10 and the thickness on the upper surface 10S1.
[0058] By forming each of the first wiring portion 22 and the second wiring portion 32 to the above-mentioned thickness, the resin body 50 arranged on the upper surface 10S1 side of the substrate 10 and the resin body 50 arranged on the lower surface 10S2 side of the substrate 10 can be made to have similar volumes.
[0059] By approximating the volume of the resin body 50 arranged on the upper surface 10S1 and the lower surface 10S2 of the substrate 10, the light emitting device 100 can equalize the balance of stress acting on the upper surface 10S1 side and the lower surface 10S2 side of the resin body 50 when the resin body 50 shrinks after heating.
[0060] With the above-described configuration, the light emitting device 100 can reduce the change in the amount of warping of the mounting substrate between high temperatures during heat treatment or the like in the manufacturing process and room temperature.
[0061] The resin substrate 10 is formed to a thickness of, for example, about 100 μm. Furthermore, the resin substrate 10 is formed to have a long side dimension of about 1.7 mm and a short side dimension of about 0.4 mm in the upper surface shape of the rectangle 10R before the formation of the cutout portions 13 and 14 and the through holes.
[0062] As described above, the first wiring electrode 20 and the second wiring electrode 30 are made of copper foil formed on the upper surface 10S1 and the lower surface 10S2 of the resin substrate 10, and copper formed by plating on the exposed surfaces of the copper foil.
[0063] Specifically, a copper foil having a thickness of about 150 μm is attached to the lower surface 10S2 of the resin substrate 10 over the formation regions of the first wiring portion 22 and the second wiring portion 32. The copper foil attached to the lower surface 10S2 of the resin substrate 10 is attached so as to cover the through holes and notches in the formation regions of the first wiring portion 22 and the second wiring portion 32.
[0064] Furthermore, copper foil having a thickness of about 20 μm is attached to the upper surface 10S1 of the resin substrate 10 in the formation regions of the first electrode portion 21 and the second electrode portion 31 and in the formation regions of the first wiring portion 22 and the second wiring portion 32. The copper foil attached to the upper surface 10S1 of the resin substrate 10 is attached to the regions excluding the through holes and notches of the formation regions of the first electrode portion 21 and the second electrode portion 31.
[0065] Copper plating is applied to the exposed surfaces of the copper foil attached to the lower surface 10S2 of the resin substrate 10 and the copper foil attached to the upper surface 10S1 of the resin substrate 10, filling the through holes 11 and 12 and the cutouts 13 and 14. Furthermore, a metal layer of Ni / Au is applied to the lower surface of the resin substrate 10 and the copper plating. The copper plating / Ni plating / Au plating is laminated to a thickness of about 30 μm on the lower surface of the copper foil attached to the lower surface 10S2 of the resin substrate 10 and on the upper surface of the copper foil attached to the upper surface 10S1 of the resin substrate 10.
[0066] That is, the electrodes 21 and 31 and the wiring portions 22 and 32 formed on the upper surface 10S1 side of the resin substrate 10 are formed to a thickness of about 50 μm from the upper surface 10S1. The wiring portions 22 and 32 formed on the lower surface 10S2 side of the resin substrate 10 are formed to a thickness of about 180 μm from the lower surface 10S2.
[0067] That is, the thickness of the first wiring electrode 20 and the second wiring electrode 30 on the lower surface 10S2 is 180 μm, which is greater than the thickness of 50 μm on the upper surface 10S1 of the first wiring electrode 20 and the second wiring electrode 30. The thickness of the first wiring electrode 20 and the second wiring electrode 30 on the lower surface 10S2 is 180 μm, which is greater than the thickness of the resin substrate 10, 100 μm, and is greater than the total thickness of the resin substrate 10 and the thickness of the first wiring electrode 20 and the second wiring electrode 30 on the upper surface 10S1, 150 μm.
[0068] The resin body 50 is formed with a thickness of about 300 μm from the upper surface of each of the electrode parts 21 and 31 formed on the upper surface 10S1 of the substrate 10. The resin body 50 is formed with a cavity opening formed on the upper surface with a long side dimension of about 1.5 mm and a short side dimension of about 0.3 mm. That is, the cavity inner wall of the resin body 50 in the direction along the long side of the resin substrate 10 is formed with a thickness of about 50 μm. By reducing the thickness of the cavity inner wall of the resin body 50 in the direction along the long side of the resin substrate 10, it is possible to reduce the warpage in the long side direction of the resin substrate 10, particularly the change in the amount of warpage in the longitudinal direction of the substrate 10.
[0069] Next, an example of a manufacturing procedure for the light emitting device 100 will be described with reference to FIGS.
[0070] Fig. 8 and Fig. 9 are diagrams showing a manufacturing flow of the light emitting device 100 according to an embodiment of the present invention. Fig. 10 to Fig. 12, Fig. 14 to Fig. 15, and Fig. 19 to Fig. 22 show cross-sectional views of the light emitting device 100 at each step of the manufacturing procedure shown in Fig. 8 or Fig. 9. Note that Fig. 10 to Fig. 12, Fig. 14 to Fig. 15, and Fig. 19 to Fig. 22 show cross-sectional views taken along line AA of the light emitting device 100 in Fig. 5. Fig. 13, Fig. 16 to Fig. 18 show top views of the light emitting device 100 at each step of the manufacturing procedure shown in Fig. 8 or Fig. 9.
[0071] First, a resin substrate preparation step is performed in which a flat resin substrate 10 is prepared (step S11, resin substrate preparation step).
[0072] Next, as shown in Fig. 10, a copper foil attaching step is performed in which a first copper foil F1 is attached to the upper surface 10S1 side of the resin substrate 10 and a second copper foil F2 is attached to the lower surface 10S2 side (step S12, copper foil attaching step). The resin substrate 10, the first copper foil F1, and the second copper foil F2 are laminated from below in the order of the second copper foil F2, the resin substrate 10, and the first copper foil F1, and then pressed from above and below while heating at about 180°C. The first copper foil F1 is a copper foil having a thickness of about 18 µm, and the second copper foil F2 is a copper foil having a thickness of about 150 µm.
[0073] As described above, a plurality of light emitting devices 100 are manufactured in a matrix on the resin substrate 10. The light emitting devices 100 are manufactured in a matrix on each of the rectangular regions 10R defined by the cut lines CL of the resin substrate 10. The plurality of light emitting devices 100 formed on the resin substrate 10 are continuously formed in the direction along the long side of the light emitting device 100, and continuously formed through the waste region in the direction along the short side. In other words, the manufacturing method of the light emitting device 100 includes a resin substrate preparation step of preparing a resin substrate 10 having a plurality of element mounting regions defined in the shape of a rectangle 10R by lattice-shaped division lines on the upper surface 10S1 of the resin substrate 10, and a copper foil attachment step of attaching a first copper foil F1 to the upper surface 10S1 of the resin substrate 10 and attaching a second copper foil F2 having a thickness larger than that of the first copper foil F1 to the lower surface 10S2 opposite to the upper surface 10S1 of the resin substrate 10.
[0074] Next, the first copper foil F1 is patterned from above to open the first copper foil F1 in the regions where the first and second through holes 11 and 12 and the notches 13 and 14 of the resin substrate 10 are to be formed (step S13, first pattern forming step). The upper surface 10S1 of the resin substrate 10 is exposed in the openings of the first copper foil F1. In this step, for example, a mask is applied to the upper surface of the first copper foil F1, and etching is performed from above to open the first copper foil F1.
[0075] 12, the resin substrate 10 at the opening portion of the first copper foil F1 is removed so as to penetrate to the upper surface of the second copper foil F2, thereby forming the first and second through holes 11 and 12, and the cutout portions 13 and 14 (step S14, first through hole forming step). In this step, a laser is irradiated from above to the opening portion of the first copper foil F1, and the resin substrate 10 at the opening portion is removed so as to penetrate to the upper surface of the second copper foil F2.
[0076] 13, in this step, the first through hole 11 and the second through hole 12 are formed in a rectangular region 10R defined by the cut line CL of the resin substrate 10. In this step, the notches 13 and 14 are formed collectively in a region including each end of the first long side 10E of each of the substrates 10 adjacent to each other in the long side direction of the resin substrate 10. That is, the opening of the resin substrate 10 formed as the notch 13 or 14 is formed such that one side of the cut line CL is the notch 13 and the other side is the notch 14. In this step, the opening of the resin substrate 10 formed as the notch 13 or 14 is formed so as to extend to the adjacent waste region in the short side direction.
[0077] The laser irradiated to the resin substrate 10 is, for example, a laser beam of Yttrium Aluminum Garnet (YAG). The exposed portion of the resin substrate 10 is irradiated with the laser to evaporate the glass epoxy of the resin substrate 10, thereby forming the first and second through holes 11 and 12, and the notches 13 and 14. The first copper foils F1 and F2 are not removed by the laser. The type of laser that evaporates the glass epoxy is not limited to YAG. Specifically, the type of laser used may be any laser that can decompose the bond between the epoxy resin and the glass fiber of the glass epoxy and has irradiation energy that does not destroy the metal bond of the first copper foils F1 and F2.
[0078] The above-mentioned steps S13 and S14 are processed as a substrate shape forming step for forming the shape of the resin substrate 10. In other words, the manufacturing method of the light emitting device 100 includes a substrate shape forming step for forming cutout portions 13 and 14 that cut out a first region NT1 including a vertex at one end of a first long side 10E of the rectangle 10R and a second region NT2 including a vertex at the other end, and for forming a first through hole 11 and a second through hole 12 that penetrate two regions of the element mounting region from the first copper foil F1 to the lower surface 10S2.
[0079] Next, as shown in Fig. 14, a copper plating step is performed to fill the first and second through holes 11 and 12 and the notches 13 and 14 and to form a copper plating layer so as to cover the upper surface of the first copper foil F1 and the lower surface of the second copper foil F2 (step S15, first plating step). In this step, the portion consisting of the first copper foil F1 and the copper plating layer is defined as the metal part M1, and the portion consisting of the second copper foil F2 and the copper plating layer is defined as the metal part M2. In other words, the manufacturing method of the light emitting device 100 includes a copper plating step of forming a metal layer consisting of copper so as to fill the notches 13 and 14, the first through hole 11 and the second through hole 12 and to cover the upper surface of the first copper foil F1 and the lower surface of the second copper foil F2.
[0080] In this step, the copper plating layer is formed on the upper surface of the first copper foil F1 and the lower surface of the second copper foil F2 to a thickness of about 12 μm. The copper plating used in this step is filling plating that fills the openings in the resin board 10 and plated so that the upper surface of the metal part M1 is flat.
[0081] Next, as shown in FIG. 15, a wiring electrode forming step is performed in which the metal parts M1 and M2 are patterned into the shapes of the first wiring electrode 20 and the second wiring electrode 30 (step S16, second pattern forming step). On the side of the upper surface 10S1 of the resin substrate 10, for example, a mask patterned with the shapes of the first and second electrode parts 21 and 31, and the first wiring part 22 and the second wiring part 32 on the upper surface 10S1 of the resin substrate 10 is applied to the upper surface of the first copper foil F1. Also, on the side of the lower surface 10S2 of the resin substrate 10, for example, a mask patterned with the shapes of the first wiring part 22 and the second wiring part 32 on the lower surface 10S2 of the resin substrate 10 is applied to the lower surface of the second copper foil F2. Thereafter, etching is performed from above and below, and the first wiring electrode 20 and the second wiring electrode 30 are patterned on the upper surface 10S1 and the lower surface 10S2 of the resin substrate 10. In other words, the manufacturing method of the light emitting device 100 includes a wiring electrode formation process of patterning a metal part M1 consisting of a first copper foil F1 and a copper plating layer, and a metal part M2 consisting of a second copper foil F2 and a copper plating layer on the upper surface 10S1 and the lower surface 10S2 into the shapes of the first wiring electrode 20 and the second wiring electrode 30.
[0082] 16, in this step, the first and second wiring parts 22 and 32 of each of the substrates 10 adjacent to each other in the long side direction of the resin substrate 10 are formed at the same time. That is, the first and second wiring parts 22 and 32 formed on the resin substrate 10 are arranged such that one of them is the first wiring part 22 and the other is the second wiring part 32, sandwiching the cut line CL. In this step, each of the first and second wiring parts 22 and 32 is formed so as to extend to a discard area adjacent to the side of the cut line CL corresponding to the first long side 10E of the resin substrate 10. As described above, the first wiring part 22 and the second wiring part 32 are formed so as to expose the lower surface 10S2 of the resin substrate 10 in the area along the cut line CL corresponding to the second long side opposite to the first long side 10E of the resin substrate 10. In other words, in the manufacturing method for the light emitting device 100, in the wiring electrode formation process, the first wiring electrode 20 and the second wiring electrode 30 are formed so as to expose the area along the second long side opposite to the first long side of the rectangle 10R on the lower surface 10S2 side.
[0083] 17, a resist RE is formed so as to cover each of the first and second wiring portions 22 and 32 formed on the upper surface 10S1 side of the resin substrate 10 (step S17, resist formation step). In this step, the resist RE is formed on the upper surface 10S1 of the resin substrate 10 to a region about 100 μm or more from the ends of the first and second wiring portions 22 and 32.
[0084] Next, a metal layer of Ni / Au is formed by plating so as to cover the surfaces of the first wiring electrode 20 and the second wiring electrode 30 except for the surfaces covered with the resist RE (step S18, second plating step). In this embodiment, the metal layer of Ni / Au is formed by using electric field plating. Therefore, the metal layer of Ni / Au is not formed on the exposed surface of the resin substrate 10 and the surface of the resist RE.
[0085] Next, as shown in FIG. 18, a third through hole 15 and a fourth through hole 16 penetrating the resist film, the first and second wiring parts 22 and 32, and the resin substrate 10 are formed on each of the short sides of the rectangular region 10R defined by the cut line CL of the resin substrate 10 (step S19, second through hole forming step). In this step, a through hole having a circular or elliptical shape is formed on each of the short sides of the rectangular region 10R defined by the cut line CL of the resin substrate 10. In this embodiment, the through hole is formed by a drill or the like. Note that the through hole formed in the resin substrate 10 is the third through hole 15 on one side of the cut line CL, and the fourth through hole 16 on the other side.
[0086] In this way, by performing the step of forming the third through hole 15 and the fourth through hole 16 (step S19) after the step of forming the Ni / Au metal layer by plating, it is possible to form the side surfaces of the first wiring portion 22 and the second wiring portion 32 in a shape that conforms to the inner walls of the third through hole 15 and the fourth through hole 16. In addition, the side surfaces of the first wiring portion 22 and the second wiring portion 32 formed so as to conform to the inner walls of the third through hole 15 and the fourth through hole 16 can be formed as side surfaces composed of copper foil, copper plating, and resist RE, and can be formed as side surfaces that have high adhesion to the resin body 50.
[0087] Next, as shown in FIG. 19, a resin body forming step is performed to form a resin body 50 on the upper surface 10S1 and the lower surface 10S2 of the resin substrate 10 (step S20, resin frame forming step). In this step, the resin substrate 10 is set in a mold of an injection molding device, and the resin as the raw material of the resin body 50 is poured in by a transfer molding method to mold the resin body 50. At this time, a lower mold of a flat mold is set on the lower surface 10S2 side of the resin substrate 10, and the lower mold is set so as to contact the lower surfaces of the first and second wiring parts 22 and 32. In addition, an upper mold of a mold having a convex part having a shape similar to the shape of the inner surface of the cavity of the resin body 50 is set on the upper surface 10S1 side of the resin substrate 10, and the lower surface of the upper mold is set so as to contact the upper surfaces of the first and second electrode parts 21 and 31.
[0088] In this state, the raw resin of the resin body 50 is poured into the mold, the raw resin is filled in the mold, and the raw resin is heated to harden the raw resin to form the resin body 50. The raw resin is poured from one side of the upper surface 10S1 or the lower surface 10S2 of the resin substrate 10, and flows into the other side through the third through hole 15 and the fourth through hole 16 to fill the mold. In addition, the resin is filled so that the lower mold of the mold and the lower surfaces of the first and second wiring parts 22 and 32 are in contact with each other and the lower surface of the upper mold of the mold and the upper surfaces of the first and second electrode parts 21 and 31 are in contact with each other. Therefore, the upper surfaces of the first and second electrode parts 21 and 31 and the lower surfaces of the first and second wiring parts 22 and 32 are exposed from the resin body 50. In other words, the manufacturing method of the light emitting device 100 includes a resin body formation step of forming a light reflective resin body 50 to form a frame body surrounding the element mounting area on the upper surface 10S1 and to cover the area exposed from the first wiring electrode 20 and the second wiring electrode 30 on the lower surface 10S2.
[0089] Moreover, the bottom surface of the cavity of the resin body 50 is preferably formed at a height equal to or lower than the upper surfaces of the first and second electrode portions 21 and 31. By forming the bottom surface of the cavity of the resin body 50 at a height equal to or lower than the upper surfaces of the first and second electrode portions 21 and 31, it is possible to prevent the light emitting element 60 from being misaligned during the element bonding process.
[0090] Next, as shown in FIG. 20, an element bonding process is performed in which the light emitting element 60 is mounted and bonded on the upper surfaces of the first and second electrode parts 21 and 31 (step S21, element bonding process). In this step, a paste containing Au-Sn alloy particles, which is the raw material of the element bonding layer 61, is first applied to the upper surfaces of the first and second electrode parts 21 and 31 using a dispenser. Then, the cathode and anode electrode surfaces of the light emitting element 60 are placed on each paste so that they come into contact with each other. The resin substrate 10 in this state is heated at about 280° C. to melt the Au-Sn particles and cause a eutectic reaction with the Au layer of the metal layer formed on the upper surfaces of the first and second electrode parts 21 and 31, thereby eutectic bonding is performed between each electrode of the light emitting element 60 and each electrode part 21 and 31. In other words, the manufacturing method of the light emitting device 100 includes an element bonding process in which the light emitting element 60 is mounted on the upper surfaces of the first and second electrode portions 21 and 31 of the first wiring electrode 20 and the second wiring electrode 30 on the upper surface 10S1 side.
[0091] 21, sealing resin 70 is filled into each cavity of resin body 50 (step S22, sealing resin filling step). In this step, a dispenser is used to fill the cavity so as to cover light emitting element 60, and seal it. As a result, a plurality of light emitting devices 100 are formed in a matrix on resin substrate 10.
[0092] Next, as shown in Fig. 22, dicing is performed along cut lines CL to separate the light emitting devices 100 (step S23, dicing step). In this step, dicing is first performed in the direction of the long sides of the light emitting devices 100. Next, in the direction of the short sides, dicing is performed from the side of the first long side 10E of the resin substrate 10 on which the first and second wiring portions 22 and 32 are formed to the side of the second long side opposite the first long side. This makes it possible to suppress metal burrs from being generated on the exposed surfaces of the first and second wiring portions 22 and 32 exposed on the side surfaces of the light emitting device 100 during dicing.
[0093] Metal burrs are likely to occur due to the thermal expansion of the metal part caused by heat generated during dicing. In addition, if the metal part is arranged at an end part in a direction perpendicular to the dicing direction, such that the metal part is followed by a space such as air in that order, the metal part thermally expands in the dicing direction, and metal burrs are likely to occur.
[0094] In this embodiment, as described above, after dicing in the long side direction of the light emitting device 100, dicing is performed in the short side direction from the side of the first long side 10E where the first and second wiring portions 22 and 32 of the light emitting device 100 are arranged. That is, by performing dicing in a direction in which there is no space for the thermal expansion of the first and second wiring portions 22 and 32, it is possible to suppress the occurrence of metal burrs.
[0095] Next, Au plating is applied to the exposed surfaces of the first and second wiring portions 22 and 32 of the individualized light emitting devices 100 (step S24, third plating step). Note that the plating with Au in step S24 can be applied arbitrarily.
[0096] By carrying out the above processes, the light emitting device 100 is manufactured.
[0097] According to this embodiment, the thickness of the first wiring electrode 20 and the second wiring electrode 30 formed on the lower surface 10S2 of the resin substrate 10 is made larger than the total thickness of the resin substrate 10 and the portion formed on the upper surface 10S1. Moreover, on the lower surface 10S2 side of the resin substrate 10, the resin body 50 is formed in a direction along the long side of the light emitting device 100 across both ends of the light emitting device 100. Moreover, on the upper surface 10S1 of the resin substrate 10, the thickness of the inner wall of the cavity of the resin body 50 in the direction along the long side of the resin substrate 10 is made smaller.
[0098] As a result, the light emitting device 100 can make the resin body 50 arranged on the upper surface 10S1 side of the substrate 10 and the resin body 50 arranged on the lower surface 10S2 side of the substrate 10 have similar volumes. Furthermore, the light emitting device 100 can suppress the concentration of stress when the resin body 50 arranged on the upper surface 10S1 of the substrate 10 shrinks after heat treatment by forming the resin body 50 on the lower surface 10S2 of the substrate 10 in the direction along the long side of the substrate 10 from both ends. Therefore, the light emitting device 100 can improve the manufacturing yield by reducing the change in the amount of warping of the mounting substrate between high temperature and normal temperature during heat treatment or the like during manufacturing.
[0099] In this embodiment, a case has been described in which one cavity is provided on the light extraction surface of the light emitting device 100 and one light emitting element 60 is mounted in the cavity. However, the number of cavities provided in the light emitting device 100 and the number of light emitting elements 60 mounted therein are not limited to this.
[0100] Fig. 23 is a top view of a light emitting device 100A according to a modified example of this embodiment. Fig. 24 is a top view of a resin substrate 10A and wiring electrodes formed thereon of the light emitting device 100A according to a modified example of this embodiment. Note that in Fig. 23, the sealing resin 70 is omitted in order to show the structure inside the cavity of the resin body 50A.
[0101] The light emitting device 100A has a basically similar configuration to the light emitting device 100 of the embodiment. In this embodiment, the light emitting device 100A differs from the embodiment in that two cavities are formed on the upper surface of the resin body 50A, and a light emitting element 60 is mounted in each cavity.
[0102] As shown in FIG. 24, resin substrate 10A of light emitting device 100A has cutout portion 17 formed by cutting out a central region of first long side 10AE, which is one of the long sides, from the top surface shape of rectangle 10R.
[0103] Furthermore, the resin substrate 10A has a fifth through hole 18 having a circular or elliptical shape penetrating from the upper surface to the lower surface so as to contact the cutout portion 17 in the central region of the upper surface of the resin substrate 10A.
[0104] Furthermore, resin substrate 10A has a pair of through holes, a first through hole 11A and a second through hole 12A, and a first through hole 11B and a second through hole 12B, which are spaced apart from each other and extend from the top surface to the bottom surface in each of the regions between notch 17 and notch 13 and between notch 17 and notch 14.
[0105] In addition, the resin substrate 10A is formed with the first electrode portions 21A and 21B and the second electrode portions 31A and 31B, which fill the through holes 11A, 11B, 12A, and 12B and are formed up to the region of the upper surface of the resin substrate 10A. In addition, the resin substrate 10A has a first wiring electrode 20A consisting of a first wiring portion 22A extending from the portion of the first electrode portion 21A to the upper surface through the side of the notch portion 13 on the lower surface of the resin substrate 10A. In addition, the resin substrate 10A has a second wiring electrode 30A consisting of a second wiring portion 32A extending from the portion of the second electrode portion 31B to the upper surface through the side of the notch portion 14 on the lower surface of the resin substrate 10A. In addition, the resin substrate 10A has a third wiring electrode 80 consisting of a third wiring portion 33 extending from each of the portion of the second electrode portion 31A and the portion of the first electrode portion 21B to the upper surface through the side of the notch portion 17 on the lower surface of the resin substrate 10A. That is, the second electrode portion 31A and the first electrode portion 21B are electrically connected via the third wiring portion 33. Moreover, the resin substrate 10A of this modified example has a shape in which the resin substrate 10 of the embodiment and each wiring electrode are connected in a direction along the long side.
[0106] The light emitting element 60 is mounted on each of the first electrode portion 21A and the second electrode portion 31A, and the first electrode portion 21B and the second electrode portion 31B. That is, one electrode of each of the light emitting elements 60 mounted on each of the first electrode portion 21A and the second electrode portion 31A, and the first electrode portion 21B and the second electrode portion 31B is electrically connected to each other.
[0107] At this time, the light emitting elements 60 may be arranged such that the cathode electrodes or the anode electrodes are electrically connected to each other, or the anode electrode of one light emitting element 60 and the cathode electrode of the other light emitting element 60 may be electrically connected to each other. Specifically, when the cathode electrodes or the anode electrodes of the light emitting elements 60 are electrically connected to each other, the light emitting elements 60 can be driven in parallel connection by applying a voltage to each of the first wiring electrode 20A and the second wiring electrode 30A with the third wiring electrode 80 at a ground potential. Also, when the anode electrode of one light emitting element 60 and the cathode electrode of the other light emitting element 60 are electrically connected to each other, the light emitting elements 60 can be driven in series connection by applying a voltage between the first wiring electrode 20A and the second wiring electrode 30A with the third wiring electrode 80 at an intermediate potential.
[0108] In this modified example, the light emitting device 100A has two cavities and is equipped with two light emitting elements 60, but it may have three or more cavities and light emitting elements 60. Also, it may have a plurality of light emitting elements 60 mounted in a cavity.
[0109] Also in the light emitting device 100A of this modification, similarly to the embodiment, the thickness of the portions of the first, second and third wiring electrodes 20A, 30A and 80 formed on the lower surface of the resin substrate 10A is made larger than the total thickness of the portions of the resin substrate 10 and the upper surface. Also, on the lower surface side of the resin substrate 10A, a resin body 50A is formed in a direction along the long side of the light emitting device 100A across both ends of the light emitting device 100A.
[0110] Therefore, also in the light emitting device 100A of this modification, it is possible to improve the manufacturing yield by reducing the change in the amount of warping of the mounting substrate between high temperatures during heat treatment or the like in the manufacturing process and room temperature. [Explanation of symbols]
[0111] 100 Light emitting device 10 Resin substrate 11 First through hole 12 Second through hole 13, 14, 17 Notch 15 Third Through Hole 16 Fourth Through Hole 17 Fifth Through Hole 20 First wiring electrode 21 First electrode part 22 First wiring section 30 Second wiring electrode 31 Second electrode part 32 Second wiring section 50 Resin body 60 Light emitting element 61 Element bonding layer 70 Sealing resin 80 Third wiring electrode
Claims
1. a flat resin substrate having a planar shape in which a first region including a vertex at one end of one long side of a rectangle and a second region including a vertex at the other end are cut out, the flat resin substrate having a first through hole and a second through hole penetrating from the first main surface to the second main surface; a first wiring electrode made of metal, the first wiring electrode having an electrode portion filling the first through hole and a wiring portion extending from the electrode portion on the second main surface side through a side surface facing the first region of the resin substrate to the first main surface and exposing a region along the other long side of the rectangle of the resin substrate on the first main surface and the second main surface; a second wiring electrode made of metal having an electrode portion filling the second through hole and a wiring portion extending from the electrode portion on the second main surface side through a side surface facing the second region of the resin substrate to the first main surface and exposing a region along the other long side of the rectangle of the resin substrate on the first main surface and the second main surface; a light emitting element mounted on the electrode portion of the first wiring electrode and the second wiring electrode on the first main surface side of the resin substrate; a light-reflecting resin body covering the first main surface of the resin substrate, covering the wiring portions of the first wiring electrode and the second wiring electrode on the first main surface, forming a frame surrounding the light-emitting element, and covering an area of the second main surface of the resin substrate that is exposed from the first wiring electrode and the second wiring electrode; A light emitting device, wherein the first wiring electrode and the second wiring electrode have a thickness greater on the second main surface than on the first main surface.
2. 2. The light-emitting device according to claim 1, wherein the thickness of each of the first wiring electrode and the second wiring electrode on the second main surface is greater than the total thickness of the thickness of the resin substrate and the thickness on the first main surface.
3. The light-emitting device according to claim 1 or 2, characterized in that each of the first wiring electrode and the second wiring electrode extends from the respective electrode portion on the second main surface to a region along one long side of the rectangle of the resin substrate.
4. 4. The light emitting device according to claim 1, wherein the resin body has a thermal expansion coefficient higher than those of the resin substrate, the first wiring electrode, and the second wiring electrode.
5. 5. The light emitting device according to claim 1, wherein the resin substrate is made of an epoxy resin containing glass fiber.
6. the first wiring electrode and the second wiring electrode are made of copper, The light-emitting device according to any one of claims 1 to 5, characterized in that each surface of the electrode portion of the first wiring electrode and the second wiring electrode exposed from the resin substrate has a metal layer in which nickel and gold are laminated in order.
7. The light-emitting device according to any one of claims 1 to 6, characterized in that the wiring portions of each of the first wiring electrode and the second wiring electrode are covered with the resin body via a resist on a surface parallel to the first main surface on the first main surface of the resin substrate.
8. A method for manufacturing a light emitting device, comprising the steps of: a resin substrate preparation step of preparing a resin substrate having a first main surface, the first main surface being provided with a plurality of element mounting regions defined into rectangular shapes by grid-like division lines; a copper foil attaching step of attaching a first copper foil onto the first main surface of the resin substrate and attaching a second copper foil having a thickness greater than that of the first copper foil onto a second main surface of the resin substrate opposite to the first main surface; a substrate shape forming step of forming a notch portion by cutting out a first region including a vertex at one end of one long side of the rectangle and a second region including a vertex at the other end, and forming a first through hole and a second through hole penetrating two regions of the element mounting region from the first copper foil to the second main surface; a copper plating process for forming a metal layer made of copper so as to fill the notch portion, the first through hole, and the second through hole and to cover the upper surface of the first copper foil and the lower surface of the second copper foil; a wiring electrode forming process of patterning the first copper foil, the second copper foil, and the metal layer on the first main surface and the second main surface into a shape of a first wiring electrode and a second wiring electrode; a resin body forming step of forming a light-reflective resin body so as to form a frame body surrounding each of the plurality of element mounting regions on the first main surface and to cover a region of the second main surface exposed from the first wiring electrode and the second wiring electrode; an element bonding step of mounting a light emitting element on the upper surface of each of the first wiring electrode and the second wiring electrode on the first main surface side, A method for manufacturing a light emitting device, characterized in that in the wiring electrode formation process, the first wiring electrode and the second wiring electrode are formed on the second main surface side so as to expose an area along the other long side of the rectangle.
9. A sealing resin filling process in which a sealing resin is filled into cavities defined by the frame body formed by the resin body formed in the resin body forming process and each cavity accommodates the light-emitting element, to cover the light-emitting element provided in the element bonding process; 9. The method for manufacturing a light emitting device according to claim 8, further comprising: a dicing step of, after the sealing resin filling step, dicing along the parting lines to separate the plurality of light emitting devices.
Citation Information
Patent Citations
Surface-mounted light-emitting diode
JP2003188424A
Light-emitting diode package
JP2009177187A
Semiconductor device
JP2010073734A
LED module
JP2012169326A
LED module
JP2017212354A