Method for fracturing an electrochemical generator
The method of fracturing electrochemical generators in an ionic liquid solution with redox species addresses the inefficiencies and safety concerns of existing recycling methods by enabling safe and cost-effective lithium or sodium extraction through redox reactions.
Patent Information
- Application Number
- JP2021568071
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-05-15
- Filing Date
- 2020-05-12
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2040-05-12
AI Technical Summary
Existing methods for recycling electrochemical generators, such as lithium-ion batteries, are inefficient and unsafe due to the risk of explosive atmospheres and chemical hazards, requiring high temperatures, ultra-low temperatures, or controlled atmospheres that are difficult to industrialize and costly.
A method involving fracturing electrochemical generators in an ionic liquid solution containing a redox species to safely discharge the generators, using redox reactions to neutralize the chemical energy without consuming reagents, thus preventing explosive atmospheres.
The method allows for rapid and safe extraction of lithium or sodium from batteries without the need for controlled atmospheres, reducing costs and environmental impact while ensuring safety by avoiding hydrogen, oxygen, and heat evolution.
Smart Images

Figure 0007581242000001 
Figure 0007581242000002
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for shredding electrochemical generators, such as Li-ion, Na-ion or lithium metal accumulators or batteries, in particular with a view to their recycling and / or storage.
[0002] More specifically, the present invention relates to a method for fracturing an electrochemical generator in a solution containing an ionic liquid and a redox active species, the redox active species being used to discharge the electrochemical generator, the ionic liquid allowing this process to be carried out in complete safety, in particular by preventing the formation of an explosive atmosphere.
[0003] In this way, salvageable pieces of the electrochemical generator can be safely recycled. [Background technology]
[0004] An electrochemical generator is a power generating device that converts chemical energy into electrical energy. It may be, for example, a battery cell or an accumulator.
[0005] The market for storage batteries, in particular for lithium storage batteries of the Li-ion type, is currently expanding rapidly, on the one hand for so-called portable applications (smartphones, computers, cameras, etc.) and on the other hand for new mobility-related applications (electric and hybrid vehicles) and so-called stationary applications (connected to the power grid).
[0006] Due to the recent growth in the number of storage batteries, the issue of recycling them has become an important issue.
[0007] Traditionally, a lithium-ion battery includes an anode, a cathode, a separator, an electrolyte, and a casing.
[0008] Typically, the anode is formed of graphite mixed with a PVDF-type binder and deposited on a copper foil, and the cathode is a lithium metal intercalation material (e.g., LiCoO2, LiMnO2, LiNiO2, Li3NiMnCoO6, or LiFePO4) mixed with a binder and deposited on an aluminum foil.
[0009] The electrolyte is a mixture of a non-aqueous solvent and a lithium salt, and optional additives that slow down secondary reactions.
[0010] It works as follows: upon charging, lithium de-intercalates from the metal oxide and intercalates into graphite, which is thermodynamically unstable. Upon discharging, the process is reversed and lithium ions are intercalated into the lithium metal oxide.
[0011] As the cells are used, aging causes a loss of capacity and they must be recycled.
[0012] However, many accumulators or battery packs to be recycled are still at least partially charged, and their shattering could generate sparks and significant fires or even explosions, especially primary lithium battery cells (Li-SOCl2).
[0013] Damaged cells must also be recycled, but these cells may have lithium metal deposits on the anode, which are highly reactive when exposed to air or water.
[0014] Therefore, end-of-life and / or damaged cells to be recycled must be handled with the utmost care.
[0015] Battery recycling involves several steps: - a pre-processing step, including a dismantling step and a safeguard step; - carrying out thermal and / or hydrometallurgical treatments to recover the various materials and convertible metals contained in these battery cells and accumulators; Includes.
[0016] So far, the main difficulty lies in making these lithium-based (primary and secondary) electrochemical systems safe.
[0017] More specifically, if containment is compromised, electrolytes leak out in liquid as well as gaseous form, which are toxic, flammable, and corrosive products. The resulting vapors mixed with air can then form an explosive atmosphere (ATEX). This atmosphere can ignite when in contact with an ignition source, such as a spark or a hot surface. This leads to an explosion with both thermal and pressure effects. Furthermore, electrolyte salts such as lithium hexafluorophosphate LiPF6, lithium tetrafluoroborate LiBF4, lithium perchlorate LiClO4, and lithium hexafluoroarsenate LiAsF6 can emit particularly toxic and corrosive fumes containing phosphorus, fluorine, and / or lithium. For example, hydrofluoric acid (HF) can be formed during the thermal decomposition of Li-ion batteries.
[0018] To overcome these drawbacks, the batteries can be crushed in a chamber with a controlled atmosphere and under a controlled pressure. By way of example, the document WO 2005 / 101564 describes a method for recycling lithium anode batteries by hydrometallurgical methods at ambient temperature and inert atmosphere. The atmosphere contains argon and / or carbon dioxide. The two gases drive out the oxygen and create a protective gas space above the crushed charge. The presence of carbon dioxide causes passivation of the lithium metal by forming lithium carbonate on the surface, which slows down the reactivity of this metal. Hydrolysis of the lithium-containing crushed charge leads to the formation of hydrogen. To prevent the risk of hydrogen ignition and explosion, the lithium-containing crushed charge is added in a carefully controlled manner to an aqueous solution, creating very strong turbulence above the bath. This operation is accompanied by a lack of oxygen in the atmosphere. The water becomes rich in lithium hydroxide and lithium is recovered by adding sodium carbonate or phosphoric acid.
[0019] In the method described in US Patent No. 5,888,463, battery cells and accumulators are made safe using cryogenic methods. The battery cells and accumulators are frozen in liquid nitrogen at -196°C before being crushed. The crushed material is then immersed in water. To prevent the formation of H2S, the pH is maintained at a pH of at least 10 by adding LiOH. The lithium salts formed (Li2SO4, LiCl) are precipitated as carbonates by adding sodium carbonate.
[0020] CA 2313173 A1 describes a method for recycling lithium-ion battery cells. The battery cells are previously cut open in an anhydrous inert atmosphere. A first organic solvent (acetonitrile) is used to dissolve the electrolyte and a second organic solvent (NMP) is used to dissolve the binder. The particulate intercalation material is then separated from the solution and reduced by electrolysis.
[0021] In the document WO 2011 / 113860, so-called drying techniques are described. The temperature of the mill is kept at 40-50°C and a cyclone-like airflow is used to displace the mixture of hydrogen and oxygen released from the batteries in order to minimize the risk of combustion. The battery fragments and dust collected after sorting are cooled to ambient temperature. The extraction of lithium appears to take place by reaction with oxygen and moisture in the air, bringing with it the risks associated with the simultaneous presence of hydrogen, oxygen and heat, which may lead to combustion and explosion. Furthermore, the electrolyte is decomposed, leading to risks, losses and difficulties in handling the dust and gases.
[0022] The UmiCore VAL'EAS™ process, described in the paper by Georgi-Maschler et al. ("Development of a recycling process for Li-ion batteries", Journal of Power Sources 207 (2012) pp. 173-182), combines pyrometallurgical and hydrometallurgical processes. Dismantled batteries are fed directly into a furnace. They are inactivated using pyrometallurgical processes, the electrolyte is evaporated at approximately 300 °C, the plastic is pyrolyzed at 700 °C, and finally the remainder is melted and reduced at 1,200-1,450 °C. In this process, part of the organic material contained in the battery cells acts as reducing agents. Aluminum and lithium are lost. Iron, copper and manganese are recovered in aqueous solutions. Cobalt and nickel are recovered as LiCoO2 and Ni(OH)2 and recycled to obtain the cathode material. However, this type of heat treatment consumes a lot of energy and causes significant decomposition of the battery components.
[0023] The document EP 0 613 198 A1 describes a method for recovering materials from lithium battery cells. The battery cells are opened either under a high pressure water jet or in an inert atmosphere to prevent combustion. The lithium is then reacted with water, alcohol, or acid to obtain lithium hydroxide, lithium alkoxide, or lithium salt (e.g. LiCl), respectively. However, the sanitization of the process by opening with a high pressure water jet consumes large amounts of water and generates H2 gas in the air.
[0024] To date, the various methods mentioned above require high temperature processing, cryogenic processing, and / or processing in a controlled atmosphere, which are difficult to commercialize and / or are expensive. [Prior art documents] [Patent documents]
[0025] [Patent Document 1] International Publication No. 2005 / 101564 [Patent Document 2] U.S. Pat. No. 5,888,463 [Patent Document 3] Canadian Patent Application Publication No. 2313173 [Patent Document 4] International Publication No. 2011 / 113860 [Patent Document 5] European Patent Application Publication No. 0613198 [Non-patent literature]
[0026] [Non-Patent Document 1] Georgi-Maschler et al., “Development of a recycling process for Li-ion batteries,” Journal of Power Sources 207, 2012, pp. 173-182. Summary of the Invention [Problem to be solved by the invention]
[0027] The object of the present invention is to provide a method that overcomes the drawbacks of the prior art, in particular a method for fracturing electrochemical generators that can be easily industrialized without the need for high temperatures, ultra-low temperatures and / or controlled atmospheres. [Means for solving the problem]
[0028] This is achieved by a method of fracturing an electrochemical generator containing a lithium or sodium containing anode and cathode, comprising fracturing the electrochemical generator in an ionic liquid solution containing an ionic liquid and a so-called oxidizing redox species that can be reduced at the anode to discharge the electrochemical generator.
[0029] The present invention differs fundamentally from the prior art in that the electrochemical generator is fractured in the presence of an ionic liquid solution containing an ionic liquid and a redox species.
[0030] This fracturing method opens the battery and provides access to the lithium or sodium. The ionic liquid solution safens the electrochemical generator for fracturing and allows reactive redox species to be introduced which upon fracturing discharges the electrochemical generator via oxidation-reduction with lithium (or sodium).
[0031] The absence of water prevents the generation of hydrogen, oxygen, and / or heat, which may create an explosive atmosphere.
[0032] In the following description, where lithium is mentioned, this lithium can be replaced by sodium.
[0033] According to a first embodiment, in the case of lithium metal accumulators, the reduction reaction of so-called oxidizing redox species leads to the oxidation of lithium metal in ionic form.
[0034] According to another embodiment, in the case of lithium-ion accumulators, the reduction reactions of so-called reducing redox species result in the deintercalation and intercalation of lithium ions from the active material of the negative electrode.
[0035] The free ions extracted from the anode migrate through the ionically conductive electrolyte and are immobilized at the cathode, where they form a thermodynamically stable lithium oxide, thermodynamically stable being understood to mean an oxide that does not react violently with water and / or air.
[0036] The crushing method according to the invention allows lithium to be rapidly extracted from the negative electrode (anode) while preventing the risk of fire and / or explosion.
[0037] Advantageously, the solution contains a second so-called reducing redox species capable of being oxidized at the positive electrode, the so-called oxidizing redox species and the so-called reducing redox species forming a redox species pair.
[0038] A redox couple, also called a redox mediator, electrochemical shuttle, or redox shuttle, is understood to mean an oxidation / reduction (Ox / Red) couple in solution form, where an oxidant can be reduced at the anode (negative electrode) and a reductant can be oxidized at the cathode (positive electrode). The redox couple produces a redox reaction, thereby discharging the generator, so that the medium remains intact and the reagents are not consumed.
[0039] The redox species or species allow the electrochemical generator to be significantly or even completely discharged while lowering the chemical energy of the electrodes and thus the potential difference between the electrodes (anode and cathode), which also reduces the effect of internal short circuits.
[0040] This method is cost-effective because the redox couple in solution form simultaneously produces redox reactions at the electrodes of the electrochemical generator, resulting in zero reagent consumption, and the solution can be used to sequentially safen multiple electrochemical generators.
[0041] Advantageously, the redox species pair is preferably Mn 2+ / Mn 3+ , Co 2+ / Co 3+ , Cr 2+ / Cr 3+ , Cr 3+ / Cr 6+ , V 2+ / V 3+ , V 4+ / V 5+ , Sn 2+ / Sn 4+ , Ag + / Ag 2+ , Cu + / Cu 2+ , Ru 4+ / Ru 8+ , or Fe 2+ / Fe 3+ Metal pairs, organic molecule pairs, metallocene pairs, e.g. Fc / Fc + etc., or halogenated molecular pairs, e.g. Cl2 / Cl - Or Cl - / Cl3- It is.
[0042] Advantageously, the ionic liquid solution contains a further ionic liquid.
[0043] Advantageously, the ionic liquid solution forms a deep eutectic solvent.
[0044] Advantageously, the electrochemical generator is immersed in the ionic liquid solution.
[0045] Advantageously, the electrochemical generator is discharged at a temperature in the range 0°C to 100°C, preferably 15°C to 60°C.
[0046] Advantageously, the electrochemical generator is discharged in air.
[0047] Advantageously, the method includes a dismantling and / or sorting step prior to the step of discharging the electrochemical generator.
[0048] Advantageously, the method includes a pyrometallurgical and / or hydrometallurgical step subsequent to the step of discharging the electrochemical generator.
[0049] The crushing method according to the invention has many advantages: - The generator is secured (discharged) and unpacked in one step, which saves considerable time and investment; - no wet grinding step is performed, which avoids the problems associated with dealing with hydrogen, oxygen and heat and thus with explosive atmospheres (safety, treatment of influents, additional economic costs) and avoids the need to use large amounts of water and treat aqueous wastewater; - no thermal treatment process is carried out, which avoids the problems associated with gas emissions (e.g. emissions of greenhouse gases or any other gases that are harmful and dangerous to humans and the environment), in particular with regard to their treatment, reducing the financial and energy costs of the method; - the constraints related to the use of water are significantly reduced, since ionic liquids are non-volatile, non-flammable and chemically stable at temperatures that can exceed 200°C (e.g. between 200°C and 400°C); - there is no need to control the gas atmosphere, especially using an inert gas, when opening the battery, which makes the method simpler and more cost-effective; - the lithium is directly available, this ensures that the generator is discharged very quickly, in contrast to the prior art where the discharging process takes several hours or even days; - One redox species is used: there is no need to use a redox couple, which widens the choice and nature of the available species, since the species simply needs to have a higher electrochemical potential than lithium, while lithium is the species with the lowest electrochemical potential. Lithium can therefore be extracted by any species capable of being reduced to a potential above -3.05 V vs SHE. - Damaged generators, generators that are not discharged or insufficiently discharged, and / or generators that cannot be discharged (because their terminals are deteriorated and / or corroded) may be handled without creating safety issues when opening them.
[0050] Opening by fracturing avoids depending on the state of damage to the generator. The use of fracturing in an anhydrous and airless environment overcomes this type of problem. - there is no need to control the gas atmosphere, especially using an inert gas, when opening the battery, which makes the method simple and cost-effective; - It is quick and easy to implement.
[0051] Other characteristics and advantages of the invention will become apparent on reading the further description given below.
[0052] Of course, this further description is given merely for the purpose of illustrating the scope of the present invention and should not be construed as limiting thereto in any way.
[0053] The present invention will be better understood after reading the following description of exemplary embodiments, given for purposes of illustration only and not intended to limit the scope of the invention, and with reference to the accompanying drawings, in which: [Brief description of the drawings]
[0054] [Figure 1] 1 is a schematic cross-sectional view of an electrochemical generator according to one particular embodiment of the present invention; [Diagram 2] FIG. 1 is a schematic cross-sectional view of an electrochemical generator according to one particular embodiment of the method of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0055] In order to make the figures easier to read, the different parts shown in the figures are not necessarily represented according to a uniform scale.
[0056] It must be understood that the various possibilities (alternatives and embodiments) are not mutually exclusive and can be combined with one another.
[0057] Although in the following the description refers to a Li-ion accumulator, the invention can be replaced by any electrochemical generator, for example a battery (also called a battery pack) or a battery cell, including multiple accumulators connected in series or parallel depending on the nominal operating voltage and / or the amount of energy to be supplied.
[0058] These various electrochemical devices may be metal ion type, such as lithium ion or sodium ion, or Li metal type.
[0059] This may also be a primary system such as Li / MnO2, or a redox flow battery.
[0060] An electrochemical generator having a potential above 1.5 V is advantageously chosen.
[0061] Reference is first made to Figure 1, which shows a lithium-ion (or Li-ion) accumulator 10. A single electrochemical cell is shown, but the generator may include multiple electrochemical cells, each cell including a first electrode 20, in this case an anode, and a second electrode 30, in this case a cathode, a separator 40, and an electrolyte 50. According to another embodiment, the first electrode 20 and the second electrode 30 may be reversed.
[0062] The anode (negative electrode) 20 is preferably carbon-based, for example made of graphite, which can be mixed with a PVDF-type binder and deposited on a copper foil. It can also be lithium titanate Li4Ti5O 12 It may be a lithium mixed oxide such as (LTO) or a sodium mixed oxide such as sodium titanate for Na-ion batteries. It may also be a lithium or sodium alloy depending on the technology chosen.
[0063] The cathode (positive electrode) 30 is a lithium ion insertion material in a Li-ion accumulator. It may be a layered oxide of the LiMO2 type, a LiMPO4 phosphate with an olivine structure, or a LiMn2O4 spinel compound, where M represents a transition metal. For example, a positive electrode made of LiCoO2, LiMnO2, LiNiO2, Li3NiMnCoO6, or LiFePO4 is selected.
[0064] The cathode (positive electrode) 30 is a sodium ion insertion material in a Na-ion battery, which may be a sodium oxide type material containing at least one transition metal element, a sodium phosphate or sulfate type material containing at least one transition metal element, a sodium fluoride type material, or a sulfide type material containing at least one transition metal element.
[0065] The intercalating material can be mixed with a polyvinylidene fluoride type binder and deposited onto an aluminum foil.
[0066] The electrolyte 50 contains a lithium salt (e.g. LiPF6, LiBF4, LiClO4) or a sodium salt (e.g. N3Na) solubilized in a non-aqueous solvent mixture, depending on the battery technology selected. The solvent mixture is, for example, a binary or ternary mixture. The solvents are selected, for example, from carbonate-based solvents (ethylene carbonate, propylene carbonate, butylene carbonate), linear or branched carbonate-based solvents (dimethyl carbonate, diethyl carbonate, ethyl methyl carbonate, dimethoxyethane) in various ratios.
[0067] Alternatively, it may also be a polymer electrolyte, containing a polymer matrix made of organic and / or inorganic materials, a liquid mixture containing one or more metal salts, and an optional mechanical reinforcement material. The polymer matrix may contain one or more polymeric materials, for example selected from polyvinylidene fluoride (PVDF), polyacrylonitrile (PAN), polyvinylidene fluoride-hexafluoropropylene (PVDF-HFP), or poly(ionic liquids) of the type poly(N-vinylimidazolium) bis(trifluoromethanesulfonylamide), N,N-diethyl-N-(2-methoxyethyl)-N-methylammonium bis(trifluoromethylsulfonyl)imide (DEMM-TFSI).
[0068] The cell may be wound on itself around a winding shaft or may have a laminated structure.
[0069] A casing 60, for example a polymer pouch or a metal package made for example of steel, is used to enclose the battery.
[0070] Each electrode 20, 30 is connected to a current collector 21, 31 that passes through the casing 60 and forms a terminal 22, 32 (also called output terminal or electrical terminal or pole) respectively on the outside of the casing 60. The current collectors 21, 31 have a dual function of providing mechanical support for the active material as well as electrical continuity to the terminals of the cell. The terminals (also called electrical terminals or poles) form output terminals and are intended to be connected to a "powered device".
[0071] In some configurations, one of the terminals 22, 32 (e.g., the one connected to the negative pole) may be connected to the ground of the electrochemical generator. The ground is thus at the negative potential of the electrochemical generator, and the positive terminal is at the positive potential of the electrochemical generator. The positive potential is therefore defined as the positive pole / terminal and any metallic parts connected in electrical continuity from this pole.
[0072] An intermediate electronic device may be optionally placed between the terminal connected to earth and earth.
[0073] To make the electrochemical generator safe, the electrochemical generator is fractured in the presence of an ionic liquid solution 100 (also called a solution of ionic liquid), which contains an ionic liquid and a redox species capable of reacting with lithium to neutralize it.
[0074] This ionic liquid solution 100 prevents contact between waste (battery cell or accumulator) / water / air and at the same time ensures the discharge of the waste via electrochemical redox species present in the ionic liquid, thus making the whole process safe with respect to the combustion ternary.
[0075] Preferably, the electrochemical generator 10 is fully discharged. The free ions are immobilized in the cathode 30 where they form thermodynamically stable lithium metal oxides that do not react violently with water or air. This is done at low environmental and economic cost. Furthermore, this process does not prevent recycling (in particular the electrolyte does not decompose). The discharge time will be estimated according to the type of battery cell and accumulator as well as the charging rate.
[0076] The electrochemical generator 10 is at least partially covered in the ionic liquid solution, and preferably is completely immersed in the ionic liquid solution 100 (FIG. 2).
[0077] Ionic liquid solution 100 contains at least one ionic liquid LI1, referred to as the solvent ionic liquid, and a redox active species A.
[0078] Ionic liquids are understood to mean associations of at least one cation and one anion which give rise to a liquid with a melting point below about 100° C. These are molten salts.
[0079] Solvent ionic liquid is understood to mean an ionic liquid that is thermally and electrochemically stable, which minimizes decomposition of the medium during a discharge event.
[0080] The ionic liquid solution may further contain one or more (e.g. two or three) further ionic liquids, i.e. it may contain a mixture of several ionic liquids.
[0081] The further ionic liquid, indicated with the reference LI2, is understood to mean an ionic liquid which improves one or more properties with regard to the safeguarding and discharging processes, in particular this may concern one or more of the following properties: fire extinguishing, flame retardancy, redox shuttle, salt stabilization, viscosity, solubility, hydrophobicity and conductivity.
[0082] Advantageously, the ionic liquid, and optionally the further ionic liquid, are liquid at ambient temperature (20-25° C.).
[0083] In the solvent ionic liquid and in the one or more further ionic liquids, the cations are preferably selected from the imidazolium, pyrrolidinium, ammonium, piperidinium, and phosphonium families.
[0084] Advantageously, cations are preferably selected that have a wide cation window large enough to predict the cathodic reaction to prevent or minimize decomposition of the ionic liquid.
[0085] Advantageously, LI1 and LI2 will have the same cation to enhance the solubility of LI2 in LI1. Of the many possible systems, low-cost, low-environmental-impact (biodegradable), non-toxic media are preferred.
[0086] Advantageously, anions are used that simultaneously provide a wide electrochemical window, moderate viscosity, low melting point (liquid at ambient temperature), and good solubility by the ionic liquid and other species in solution, and that do not cause hydrolysis (decomposition) of the ionic liquid.
[0087] The TFSI anion is one example that meets the above criteria in many contexts, for example in the use of LI1:[BMIM][TFSI], or ionic liquids of the type [P66614][TFSI], the ionic liquid 1-ethyl-2,3-trimethyleneimidazolium bis(trifluoromethanesulfonyl)imide ([ETMIm][TFSI]), the ionic liquid N,N-diethyl-N-methyl-N-2-methoxyethylammonium bis(trifluoromethylsulfonyl)amide [DEME][TFSA], the ionic liquid N-methyl-N-butylpyrrolidinium bis(trifluoromethylsulfonyl)imide ([PYR14][TFSI]), or the ionic liquid N-methyl-N-propylpiperidinium bis(trifluoromethanesulfonyl)imide (PP13-TFSI). The anion may also be of the bis(fluorosulfonyl)imide (FSA or FSI) type, such as the ionic liquids N-methyl-N-propylpyrrolidinium FSI (P13-FSI), N-methyl-N-propylpiperidinium FSI (PP13-FSI), or 1-ethyl-3-methylimidazolium FSI (EMI-FSI).
[0088] The anion of the solvent ionic liquid LI1 and / or the further liquid LI2 may be a complexing anion which forms a complex with the electrochemical shuttle.
[0089] Another association is conceivable with ionic liquids, preferably with a wide anodic window, in which the cation is associated with an anion, which may be organic or inorganic.
[0090] The ionic liquid solution 100 advantageously forms a deep eutectic solvent (or DES), which has the general formula: [Cat] + .[X] - .z[Y] A mixture that is liquid at ambient temperature, obtained by forming a eutectic mixture of two salts of [Cat] + is the cation (e.g., ammonium) of the solvent ionic liquid, [X] -is a halide anion (e.g., Cl - ) and [Y] is the solvent ionic liquid X - is a Lewis or Bronsted acid capable of complexing with an anion, z is the number of molecules Y.
[0091] Eutectic products can be divided into three categories according to the nature of Y.
[0092] The first category corresponds to Type I eutectics: Y=MCl x , where, for example, M=Fe, Zn, Sn, Fe, Al, Ga The first category corresponds to type II eutectics: Y=MClx.yH2O, where, for example, M=Cr, Co, Cu, Ni, Fe The first category corresponds to type III eutectics: Y=RZ, where, for example, Z=CONH2, COOH, OH.
[0093] For example, DES is choline chloride associated with a very low toxicity H-bond donor, such as glycerol or urea, ensuring a non-toxic and very low cost DES.
[0094] According to another exemplary embodiment, choline chloride can be replaced by betaine. Although these systems have a limited electrochemical stability window, they can guarantee flooding and deactivation of any open storage battery.
[0095] Advantageously, a compound "Y" is selected that can be oxidized and / or reduced and act as an electrochemical shuttle. For example, Y is a metal salt that can dissolve in an ionic liquid solution to form metal ions. For example, Y contains iron.
[0096] As an illustration, a eutectic can be formed between chloride anion ionic liquid and metal salts FeCl2 and FeCl3 with various cations in various ratios.
[0097] This type of reaction can also be carried out by type II eutectics incorporating water molecules in the metal salt, which does not pose a risk if the water content is low, low being understood to mean typically less than 10 wt% of the solution, for example 5-10 wt% of the solution.
[0098] Type III eutectics, combining an ionic liquid and a hydrogen bond donor species (Y), can also be used with mixtures of type [LI1] / [Y], where LI1 can be a quaternary ammonium and Y can be a complexing molecule (hydrogen bond donor), such as urea, ethylene glycol, or thiourea.
[0099] Mixtures can also be made that will advantageously modify the properties of the solution for discharging the medium, in particular by combining solvent ionic liquids of the type [BMIM][NTF2], which are very stable and liquid at ambient temperature, but which slightly solubilize electrochemical shuttles (or redox mediators), such as ferric chloride.
[0100] For example, LI2 can be combined with a further ionic liquid of the type [BMIM][Cl], which will increase the solubility of metal salts in chloride form by complexing with the anions of LI2. This allows simultaneously good transport properties and good solubility of the redox mediator, thereby enhancing the discharge phenomenon.
[0101] Solution 100 contains redox species, which are species in ionic or solution form that are capable of being oxidized at the negative electrode according to A → A*, where A* is the oxidized form of species A (Figure 2). The redox species make it possible to safeguard the accumulator by extracting lithium from the negative electrode.
[0102] The proposed method renders the battery non-reactive to air.
[0103] Electrochemical couples or combinations thereof can also be used. Preferably, this is a redox couple that acts as an electrochemical shuttle (or redox mediator) by carrying out an oxidation-reduction reaction, thereby reducing the degradation of the medium.
[0104] A redox couple is understood to mean an oxidizing agent and a reducing agent in solution form that can be reduced and oxidized, respectively, at the electrodes of a battery cell. Their oxidation / reduction can advantageously regenerate the redox species that are initially present in solution form. The use of an electrochemical shuttle allows the device to be operated in a closed loop, reducing the decomposition of the medium.
[0105] The oxidizing and reducing agents may be introduced in equimolar or non-equimolar proportions.
[0106] One of the redox species may come from the generator itself, which may be cobalt, nickel, and / or manganese, among others.
[0107] The redox couple is an electrochemical metal couple or combination thereof: Mn 2+ / Mn 3+ , Co 2+ / Co 3+ , Cr 2+ / Cr 3+ , Cr 3+ / Cr 6+ , V 2+ / V 3+ , V 4+ / V 5+ , Sn 2+ / Sn 4+ , Ag + / Ag 2+ , Cu + / Cu 2+ , Ru 4+ / Ru 8+ , or Fe 2+ / Fe 3+ may be also possible.
[0108] The redox species and redox couples may also be selected from organic molecules, in particular 2,4,6-tri-t-butylphenoxyl, nitronyl nitroxide / 2,2,6,6-tetramethyl-1-piperidinyloxy (TEMPO), tetracyanoethylene, tetramethylphenylenediamine, dihydrophenazine, aromatic molecules, such as those with methoxy groups, N,N-dimethylamino groups, such as methoxybenzeneanisole, dimethoxybenzene, or those with N,N-dimethylaniline groups, such as N,N-dimethylaminobenzene, etc. Other examples include 10-methyl-phenothiazine (MPT), 2,5-di-tert-butyl-1,4-dimethoxybenzene (DDB), and 2-(pentafluorophenyl)-tetrafluoro-1,3,2-benzodioxaborole (PFPTFBDB).
[0109] This also applies to the family of metallocenes (Fc / Fc+, Fe(bpy)3(ClO4)2 and Fe(phen)3(ClO4)2 and their derivatives) or halogenated molecules (Cl2 / Cl - , Cl - / Cl 3- , Br2 / Br - , I2 / I - , I - / I3 - ) family.
[0110] In particular, bromides or chlorides are selected. It is preferably the chlorides which can easily complex with metals. For example, iron is complexed with the chloride anion, FeCl4 - which can reduce the reactivity of the negative electrode.
[0111] It may also be tetramethylphenylenediamine.
[0112] Several redox couples can be combined, the metals of the metal ions being the same or different.
[0113] For example, Fe 2+ / Fe3+ and / or Cu + / Cu 2+ is selected because the latter is soluble in two oxidation states, is non-toxic, and does not decompose the ionic liquid.
[0114] To prevent thermal runaway, especially in the event of opening the accumulator, the solution may contain a fire extinguishing agent and / or a flame retardant. This may be an alkyl phosphate, optionally fluorinated (fluorinated alkyl phosphate), such as trimethyl phosphate, triethyl phosphate, or tris(2,2,2-trifluoroethyl)phosphate. The concentration of the active species may be between 80wt% and 5wt%, preferably between 30wt% and 10wt%.
[0115] Optionally, the ionic liquid solution may contain a desiccant, and / or an agent to enhance transport of materials, and / or a protectant, e.g., a stabilizer / reducer of corrosive and toxic species selected from PF5, HF, and POF3.
[0116] Agents that improve the transport of substances are, for example, small amounts of co-solvents that can be added to reduce viscosity.
[0117] This may be a small percentage of water, such as 5% water.
[0118] Preferably, the organic solvent is selected for effective action without risk of discharge or flammability. It may be vinylene carbonate (VC), gamma-butyrolactone (γ-BL), propylene carbonate (PC), poly(ethylene glycol), or dimethyl ether. The concentration of the agent that enhances the transport of the substance is advantageously 1 wt% to 40 wt%, more advantageously 10 wt% to 40 wt%.
[0119] Protective agents capable of reducing and / or stabilizing corrosive and / or toxic elements are, for example, compounds of the butylamine type, carbodiimides (of the N,N-dicyclohexylcarbodiimide type), N,N-diethylaminotrimethyl-silane, tris(2,2,2-trifluoroethyl)phosphite (TTFP), amine-based compounds such as 1-methyl-2-pyrrolidinone, fluorinated carbamates or hexamethylphosphoramide, etc. It may also be a compound of the cyclophosphazene family, such as hexamethoxycyclotriphosphazene.
[0120] Advantageously, the ionic liquid solution contains less than 10 wt% water, preferably less than 5 wt% water.
[0121] Even more preferably, the ionic liquid solution is water-free.
[0122] The process may be carried out at a temperature ranging from 0° C. to 100° C., preferably from 20° C. to 60° C., and even more preferably at ambient temperature (20-25° C.).
[0123] The process can be carried out in air or in an inert atmosphere such as argon, carbon dioxide, nitrogen, or mixtures thereof. It can also be carried out in an atmosphere with controlled oxygen content.
[0124] If the electrochemical generator is immersed in an ionic solution, the solution may be agitated to improve reagent uptake, for example this may involve stirring at between 50 and 2,000 rpm, preferably between 200 and 800 rpm.
[0125] By way of example, the crushing step may be carried out in a recycling process, which may include the following steps: sorting, dismantling, crushing, followed by recycling of the elements to be recovered (e.g. pyrometallurgy, hydrometallurgy, etc.).
[0126] Safely open the generator and utilize its salvageable parts.
[0127] Illustrative and non-limiting examples of embodiments: In this embodiment, the discharge is carried out in a glycerin type medium (a mixture of choline chloride and glycerin).
[0128] The ionic liquid solution contained choline chloride and glycerin in a volume ratio of 1:2 and had a Cp of 2.2 Jg. -1 .K -1 is an ionic liquid mixture containing 5 wt% trimethyl phosphate as a fire extinguishing agent. After the solution is dried, the crushing area of a sealed knife mill is filled with the solution. 18650 Li-ion battery cells are then placed in the mill at ambient temperature. Rotation is at 50 rpm. This crushing method simultaneously opens the battery cells and causes a reaction of the lithium with the bath, thereby discharging and safening the battery cells. [Explanation of symbols]
[0129] 10 Lithium Ion Battery 20 First electrode 21 Current collector 22 Terminals 30 Second electrode 31 Current collector 32 terminals 40 Separator 50 electrolytes 60 Casing 100 Ionic Liquid Solution
Claims
1. A method for crushing an electrochemical generator (10) comprising a lithium or sodium containing anode (20) and a cathode (30) using a knife mill, the method comprising the step of crushing the electrochemical generator (10) using a knife mill in an ionic liquid solution (100) containing an ionic liquid and a so-called oxidizing redox species that can be reduced at the anode (20) to discharge the electrochemical generator (10), characterized in that the ionic liquid solution (100) forms a deep eutectic solvent and the crushing area of the knife mill is filled with the ionic liquid solution (100).
2. 2. The method of claim 1, characterized in that the ionic liquid solution (100) contains a second so-called reducing redox species capable of being oxidized at the positive electrode (30), the so-called oxidizing redox species and the so-called reducing redox species forming a redox species pair.
3. 3. The method according to claim 1 or 2, characterized in that the redox species pair is a metal pair, an organic molecule pair, a metallocene pair, or a halogenated molecule pair.
4. 4. The method according to claim 1, wherein the ionic liquid solution (100) contains a further ionic liquid.
5. 5. The method according to any one of claims 1 to 4, characterized in that the electrochemical generator (10) is crushed in an inert atmosphere.
6. 6. The method according to any one of claims 1 to 5, characterized in that it comprises a dismantling and / or sorting step prior to the step of crushing the electrochemical generators (10).
7. 7. The method according to any one of claims 1 to 6, characterized in that it comprises pyrometallurgical and / or hydrometallurgical steps subsequent to the step of crushing the electrochemical generator (10).
8. 8. The method according to any one of claims 1 to 7, characterized in that the electrochemical generator (10) is a lithium ion generator or a sodium ion generator.
9. The method according to claim 1, wherein the process of crushing the electrochemical generator (10) is carried out at a temperature in the range of 0°C to 100°C.
10. The method of claim 3, wherein the metal pairs are selected from Mn2+ / Mn3+, Co2+ / Co3+, Cr2+ / Cr3+, Cr3+ / Cr6+, V2+ / V3+, V4+ / V5+, Sn2+ / Sn4+, Ag+ / Ag2+, Cu+ / Cu2+, Ru4+ / Ru8+, and Fe2+ / Fe3+.
11. The method of claim 3, wherein the metallocene pair is Fc / Fc + .
12. The method according to claim 3, wherein the halogenated molecular pair is Cl 2 / Cl − or Cl − / Cl 3 − .
Citation Information
Patent Citations
Recycling of galvanic cells
CA2313173A1
Method for recycling and extracting four metal elements of cobalt, copper, aluminum and lithium from waste lithium-ion batteries by using liquid-phase reaction
CN104124487B
Method for recovering lithium cell materials
EP0613198A1
Trough type molten metal supplying method and device thereof