Vibration device and method for manufacturing the same

The vibration device addresses wiring pattern defects by using dry and wet etching with guard ring metal layers, achieving high reliability and compactness.

JP7581915B2Active Publication Date: 2024-11-13SEIKO EPSON CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021010083
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-01-26
Publication Date
2024-11-13
Estimated Expiration
2041-01-26

AI Technical Summary

Technical Problem

Wet etching in forming through electrodes leads to isotropic etching, causing side etching and unintended metal invasion, resulting in wiring pattern defects.

Method used

A vibration device with a semiconductor substrate and an annular metal layer surrounding the through electrode, using dry etching to penetrate the substrate and wet etching to penetrate the insulating layer, with metal layers acting as guard rings to restrict side etching.

Benefits of technology

This method suppresses plasma damage and wiring pattern defects, ensuring a highly reliable and compact vibration device with improved thermal stability and reduced size.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007581915000001
    Figure 0007581915000001
  • Figure 0007581915000002
    Figure 0007581915000002
  • Figure 0007581915000003
    Figure 0007581915000003
Patent Text Reader

Abstract

To provide a vibration device and a method for manufacturing a vibration device, capable of suppressing occurrence of pattern defects in wiring.SOLUTION: A vibration device includes a base and a vibration element placed on the base. The base has: a semiconductor substrate having a first surface and a second surface that are opposite to each other; an integrated circuit including a wiring layer being placed on a second surface side and including a connection pad, and an insulating layer placed between the second surface and the wiring layer; a through electrode passing through the semiconductor substrate and the insulating layer and connected to the connection pad; and an annular metal layer placed between the second surface and the wiring layer while passing through the insulating layer, the metal layer surrounding the through electrode in plan view of the semiconductor substrate.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a vibration device and a method for manufacturing a vibration device. [Background technology]

[0002] The semiconductor substrate described in Patent Document 1 includes a silicon substrate, an insulating layer formed on the silicon substrate, a conductive pad formed on the insulating layer, and a through electrode that penetrates the silicon substrate and the insulating layer and is connected to the conductive pad. The method for forming the through electrode includes a step of forming a through hole in the silicon substrate by dry etching, a step of forming a through hole in the insulating layer by wet etching, and a step of filling the through hole with a metal material. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Special Publication No. 2014-519201 Summary of the Invention [Problem to be solved by the invention]

[0004] Thus, in the method of forming a through electrode in Patent Document 1, a through hole is formed in an insulating layer by wet etching. However, wet etching is isotropic etching. Therefore, there is a problem that side etching occurs in the insulating layer, and a metal material may infiltrate into a void unintentionally generated by the side etching, which may cause a wiring pattern defect (hereinafter also referred to as "wiring pattern defect caused by side etching"). [Means for solving the problem]

[0005] The vibration device of the present invention includes a base and a vibration element disposed on the base, The base includes a semiconductor substrate having a first surface and a second surface that are opposite to each other; an integrated circuit including a wiring layer disposed on the second surface side and having a connection pad, and an insulating layer disposed between the second surface and the wiring layer; a through electrode that penetrates the semiconductor substrate and the insulating layer and is connected to the connection pad; The semiconductor substrate further includes a ring-shaped metal layer disposed between the second surface and the wiring layer, penetrating the insulating layer, and surrounding the through electrode in a plan view of the semiconductor substrate.

[0006] The method for manufacturing a resonator device of the present invention includes a base preparation step of preparing a base having a semiconductor substrate having a first surface and a second surface that are reverse to each other, an integrated circuit including a wiring layer disposed on the second surface side and having a connection pad, and an insulating layer disposed between the second surface and the wiring layer, and a ring-shaped metal layer disposed between the second surface and the wiring layer and penetrating the insulating layer; a through electrode forming step of forming a through electrode that penetrates the semiconductor substrate and the insulating layer, passes through an inner side of the metal layer, and is connected to the connection pad; The through electrode forming step includes: a through hole forming step of penetrating the semiconductor substrate by dry etching and then penetrating the insulating layer by wet etching to form a through hole that passes from the first surface through an inner side of the metal layer and faces the connection pad; and a conductive material disposing step of disposing a conductive material in the through hole to form the through electrode. [Brief description of the drawings]

[0007] [Figure 1] 1 is a vertical cross-sectional view showing a vibration device according to a first embodiment. [Diagram 2] FIG. 2 is a plan view showing the upper surface of the base. [Diagram 3] FIG. 4 is a vertical cross-sectional view showing a metal layer surrounding a through electrode. [Figure 4] FIG. 4 is a cross-sectional view showing a metal layer surrounding a through electrode. [Diagram 5] FIG. 2 is a plan view showing a vibration element. [Figure 6] 1 is a flowchart showing a manufacturing process of a vibration device. [Figure 7] 5A to 5C are longitudinal cross-sectional views illustrating a method for manufacturing the vibration device. [Figure 8] 5A to 5C are longitudinal cross-sectional views illustrating a method for manufacturing the vibration device. [Figure 9] 5A to 5C are longitudinal cross-sectional views illustrating a method for manufacturing the vibration device. [Figure 10] 5A to 5C are longitudinal cross-sectional views illustrating a method for manufacturing the vibration device. [Figure 11] 5A to 5C are longitudinal cross-sectional views illustrating a method for manufacturing the vibration device. [Figure 12] 5A to 5C are longitudinal cross-sectional views illustrating a method for manufacturing the vibration device. [Figure 13] 5A to 5C are longitudinal cross-sectional views illustrating a method for manufacturing the vibration device. [Figure 14] 5A to 5C are longitudinal cross-sectional views illustrating a method for manufacturing the vibration device. [Figure 15] FIG. 11 is a vertical cross-sectional view showing a vibration device according to a second embodiment. [Figure 16] 13 is a cross-sectional view showing a metal layer of a resonation device according to a third embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, preferred embodiments of the vibration device will be described with reference to the accompanying drawings. For convenience of explanation, the upper side of the paper in Fig. 1, Fig. 3, Fig. 7 to Fig. 15 will be referred to as "upper" and the lower side of the paper will be referred to as "lower".

[0009] First Embodiment FIG. 1 is a longitudinal sectional view showing a vibration device according to a first embodiment. FIG. 2 is a plan view showing the upper surface of a base. FIG. 3 is a longitudinal sectional view showing a metal layer surrounding a through electrode. FIG. 4 is a transverse sectional view showing a metal layer surrounding a through electrode. FIG. 5 is a plan view showing a vibration element. FIG. 6 is a flowchart showing the manufacturing process of the vibration device. FIGS. 7 to 14 are longitudinal sectional views for explaining a manufacturing method of the vibration device. FIG. 1 is a sectional view taken along line AA in FIG. 2.

[0010] 1, the vibration device 1 includes a package 10 having a housing portion S, and a vibration element 4 housed in the housing portion S. The package 10 also includes a base 2 on which the vibration element 4 is mounted, and a lid 3 that covers the vibration element 4 and is bonded to an upper surface of the base 2. The base 2 also includes a semiconductor substrate 5 and an integrated circuit 6 disposed on the semiconductor substrate 5.

[0011] The semiconductor substrate 5 is a silicon substrate, particularly a P-type silicon substrate. However, the semiconductor substrate 5 is not particularly limited and may be an N-type silicon substrate. The semiconductor substrate 5 may also be a semiconductor substrate other than silicon, such as a semiconductor substrate of Ge, GaP, GaAs, InP, etc.

[0012] The semiconductor substrate 5 is plate-shaped and has a first surface 5a and a second surface 5b that are opposite each other. The first surface 5a is the upper surface, and the second surface 5b is the lower surface. An insulating film 50 made of SiO2 (silicon oxide) is formed on the surface of the semiconductor substrate 5. However, the insulating film 50 is not particularly limited, and may be, for example, an organic insulating film.

[0013] Furthermore, an integrated circuit 6 electrically connected to the vibration element 4 is formed on the second surface 5b of the semiconductor substrate 5. By forming the integrated circuit 6 on the semiconductor substrate 5, the semiconductor substrate 5 can be effectively utilized. In particular, by forming the integrated circuit 6 on the second surface 5b, a larger space can be secured for forming the integrated circuit 6 since there is no bonding area with the lid 3 compared to the case where the integrated circuit 6 is formed on the first surface 5a.

[0014] The integrated circuit 6 includes an oscillator circuit 6A that is electrically connected to the vibration element 4 and oscillates the vibration element 4 to generate an oscillation signal such as a clock signal. The integrated circuit 6 may include circuits other than the oscillator circuit 6A. Examples of such circuits include a processing circuit that processes an output signal from the oscillator circuit 6A, and examples of such processing circuits include a PLL circuit.

[0015] On the second surface 5b side, a laminate 60 is formed in which an etching stop layer 61, an insulating layer 62, a wiring layer 63, an insulating layer 64, a wiring layer 65, an insulating layer 66, a passivation film 67, and a terminal layer 68 are laminated in this order. Then, a plurality of active elements (not shown) formed on the second surface 5b are electrically connected via the wiring layers 63 and 65 to form the integrated circuit 6. In addition, the terminal layer 68 has a plurality of mounting terminals 681. The integrated circuit 6 is electrically connected to an external device via these mounting terminals 681. The number of wiring layers included in the laminate 60 is not particularly limited, and may be one or may be three or more.

[0016] In addition, a pair of through holes 21 and 22 are formed in the base 2 from its upper surface side, penetrating the semiconductor substrate 5, the etching stop layer 61, and the insulating layer 62 in the thickness direction and facing the wiring layer 63. As will be described in the manufacturing method of the vibration device 1 described later, the through holes 21 and 22 are formed by penetrating the semiconductor substrate 5 and the etching stop layer 61 by dry etching, and then penetrating the insulating layer 62 by wet etching. According to such a forming method, the through holes 21 and 22 reach the wiring layer 63 during wet etching, so that plasma damage to the wiring layer 63 is suppressed. In addition, since the semiconductor substrate 5 is penetrated by dry etching, the through holes 21 and 22 can be formed with a high aspect ratio. Therefore, the reliability of the vibration device 1 can be improved while miniaturizing the vibration device 1.

[0017] The through holes 21 and 22 are filled with a conductive material E to form the through electrodes 210 and 220. The through electrodes 210 and 220 are electrically connected to the connection pads 631 and 632 of the wiring layer 63, respectively. That is, the through electrodes 210 and 220 are connected to the connection pads 631 and 632 of the wiring layer 63 located closest to the semiconductor substrate 5 among the multiple wiring layers 63 and 65 included in the integrated circuit 6. This allows the through electrodes 210 and 220 to be shorter than when they are connected to the connection pads included in the wiring layer 65. This makes it easier to form the through electrodes 210 and 220. However, this is not limited thereto, and for example, the through electrodes 210 and 220 may be connected to the connection pads included in the wiring layer 65.

[0018] 2, a pair of wirings 28, 29 electrically connected to the vibration element 4 via metal bumps 81, 82 are disposed on the first surface 5a side of the semiconductor substrate 5. The wiring 28 is electrically connected to the integrated circuit 6 via a through electrode 210, and the wiring 29 is electrically connected to the integrated circuit 6 via a through electrode 220.

[0019] 1 and 3, the base 2 has metal layers 691 and 692 disposed between the etching stop layer 61 and the wiring layer 63 and penetrating the insulating layer 62. As shown in FIG. 4, the metal layers 691 and 692 form rings surrounding the through electrodes 210 and 220 in a plan view of the semiconductor substrate 5. The wiring layer 63 has connection pads 631 and 632 connected to the through electrodes 210 and 220, and the metal layer 691 is included in the connection pad 631 and the metal layer 692 is included in the connection pad 632 in a plan view of the semiconductor substrate 5. Therefore, the upper ends of the metal layers 691 and 692 penetrate the insulating layer 62 and contact the lower surface of the etching stop layer 61, and the lower ends of the metal layers 691 and 692 penetrate the insulating layer 62 and contact the upper surfaces of the connection pads 631 and 632.

[0020] As will be described later in the manufacturing method of the resonator device 1, the metal layers 691 and 692 function as guard rings that are etching stop layers when the through holes 21 and 22 are formed. By providing the metal layers 691 and 692, when the through holes 21 and 22 are formed in the insulating layer 62 by wet etching, side etching outward from the metal layers 691 and 692 is restricted, and further unintended side etching can be suppressed. Therefore, wiring pattern defects caused by side etching can be suppressed, resulting in a highly reliable resonator device 1.

[0021] The lid 3 is a silicon substrate, like the semiconductor substrate 5. This makes the linear expansion coefficients of the semiconductor substrate 5 and the lid 3 equal. Therefore, the generation of thermal stress caused by thermal expansion is suppressed, and the resonator device 1 has excellent vibration characteristics. In addition, since the resonator device 1 can be formed by a semiconductor process, the resonator device 1 can be manufactured with high precision and can be made small. However, the lid 3 is not particularly limited, and a semiconductor substrate other than silicon, such as a semiconductor substrate of Ge, GaP, GaAs, InP, etc., may be used. In addition, a substrate other than a semiconductor substrate, such as a metal substrate of Kovar, a glass substrate, etc., may be used.

[0022] As shown in FIG. 1, the lid 3 has an opening on its lower surface and a bottomed recess 31 for accommodating the vibration element 4 therein. The lid 3 is bonded at its lower surface to the upper surface of the base 2 via a bonding member 7. As a result, an accommodating section S, which is a space for accommodating the vibration element 4, is formed between the lid 3 and the base 2. In this embodiment, the lid 3 and the base 2 are bonded using diffusion bonding that utilizes the diffusion between metals. However, the method for bonding the lid 3 and the base 2 is not particularly limited.

[0023] The storage section S is airtight and in a reduced pressure state, preferably in a state closer to a vacuum, which reduces viscous resistance and improves the oscillation characteristics of the vibration element 4. However, the atmosphere in the storage section S is not particularly limited, and may be, for example, an atmosphere filled with an inert gas such as nitrogen or Ar, or may be in an atmospheric pressure state or a pressurized state instead of a reduced pressure state.

[0024] As shown in FIG. 5, the vibration element 4 has a vibration substrate 41 and an electrode 42 arranged on the surface of the vibration substrate 41. The vibration substrate 41 has a thickness shear vibration mode, and is formed of an AT-cut quartz substrate in this embodiment. The AT-cut quartz substrate has a third-order frequency-temperature characteristic, and therefore the vibration element 4 has excellent temperature characteristics. The electrode 42 has an excitation electrode 421 arranged on the upper surface of the vibration substrate 41, and an excitation electrode 422 arranged on the lower surface opposite the excitation electrode 421. The electrode 42 has a pair of terminals 423 and 424 arranged on the lower surface of the vibration substrate 41, a wiring 425 that electrically connects the terminal 423 and the excitation electrode 421, and a wiring 426 that electrically connects the terminal 424 and the excitation electrode 422.

[0025] The configuration of the vibration element 4 is not limited to the above-mentioned configuration. For example, the vibration element 4 may be a mesa type in which the vibration region sandwiched between the excitation electrodes 421 and 422 protrudes from its surroundings, or conversely, may be an inverted mesa type in which the vibration region is recessed from its surroundings. In addition, bevel processing for grinding the periphery of the vibration substrate 41, or convex processing for making the upper and lower surfaces into convex curved surfaces may be performed.

[0026] The vibration element 4 is not limited to vibrating in a thickness-shear vibration mode, and may be, for example, a tuning fork type vibration element with multiple vibrating arms that perform bending vibration in an in-plane direction. In other words, the vibration substrate 41 is not limited to being formed from an AT-cut quartz substrate, and may be formed from a quartz substrate other than an AT-cut quartz substrate, for example, an X-cut quartz substrate, a Y-cut quartz substrate, a Z-cut quartz substrate, a BT-cut quartz substrate, an SC-cut quartz substrate, an ST-cut quartz substrate, or the like.

[0027] The material of the vibration substrate 41 is not limited to quartz crystal, and may be, for example, a piezoelectric single crystal such as lithium niobate, lithium tantalate, lithium tetraborate, langasite, potassium niobate, or gallium phosphate, or may be a piezoelectric single crystal other than these. Furthermore, the vibration element 4 is not limited to a piezoelectric drive type vibration piece, and may be an electrostatic drive type vibration piece using electrostatic force.

[0028] Such a vibration element 4 is located on the first surface 5a side of the semiconductor substrate 5. The vibration element 4 is joined to the base 2 by a pair of metal bumps 81, 82 and is electrically connected to the wirings 28, 29. The metal bumps 81, 82 are stud bumps, plated bumps, or the like. The method of connecting the vibration element 4 to the base 2 is not particularly limited, and for example, the vibration element 4 may be joined to the base 2 by a conductive adhesive and electrically connected to the wirings 28, 29.

[0029] The configuration of the vibration device 1 has been described above. Next, a manufacturing method of the vibration device 1 will be described. The manufacturing method of the vibration device 1 includes a base preparation step S1, a through electrode formation step S2, a vibration element arrangement step S3, and a lid arrangement step S4, as shown in Fig. 6. Furthermore, the through electrode formation step S2 includes a through hole formation step S21 and a conductive material arrangement step S22.

[0030] <Base preparation process S1> First, as shown in FIG. 7, the base 2 is prepared. At this stage, the through electrodes 210, 220 and the wirings 28, 29 are not formed in the base 2. That is, the base 2 has a semiconductor substrate 5, an integrated circuit 6 arranged on the second surface 5b side of the semiconductor substrate 5, and annular metal layers 691, 692 formed in the integrated circuit 6. The etching stop layer 61 is made of SiN (silicon nitride), and the insulating layers 62, 64 are made of SiO2 (silicon oxide). The wiring layers 63, 65, the terminal layer 68, and the metal layers 691, 692 are each made of aluminum (Al), and the passivation film 67 is made of polyimide. However, the constituent materials of these layers are not particularly limited as long as they can perform their functions.

[0031] <Through electrode formation process S2> ≪Through hole formation step S21≫ Next, as shown in FIG. 8, through holes 211 and 221 are formed penetrating the semiconductor substrate 5 in the thickness direction. The through holes 211 and 221 are formed by dry etching, particularly the Bosch method. This allows the through holes 211 and 221 to be formed with a high aspect ratio. The etching stop layer 61 functions as a stop layer for this dry etching. In particular, by forming the etching stop layer 61 from SiN (silicon nitride), the etching stop layer 61 has a high selectivity for this dry etching, and overetching can be effectively suppressed. Therefore, for example, it is possible to effectively suppress the through holes 211 and 221 from reaching the wiring layer 63 and causing plasma damage to the wiring layer 63. As a result, wiring pattern defects caused by this dry etching are suppressed, and a highly reliable resonator device 1 can be manufactured.

[0032] 9, the through holes 211, 221 are dug from their lower ends to form the through holes 212, 222 that penetrate the etching stop layer 61 in the thickness direction. The through holes 212, 222 are formed by dry etching. However, the method is not limited to this, and the through holes 212, 222 may be formed by wet etching.

[0033] Next, as shown in FIG. 10, the through holes 213, 223 are formed by digging from the lower end of the through holes 212, 222, passing through the inside of the metal layers 691, 692 and penetrating the insulating layer 62 in the thickness direction. The through holes 213, 223 are formed by wet etching. By forming the through holes 213, 223 by wet etching, plasma damage to the wiring layer 63 does not occur as occurs when the through holes 213, 223 are formed by dry etching. Therefore, it is possible to suppress wiring pattern defects caused by dry etching. Instead, side etching occurs in wet etching, and there is a risk of wiring pattern defects caused by wet etching. However, in this embodiment, since the through holes 213, 223 pass through the inside of the metal layers 691, 692, side etching further outward is restricted by the metal layers 691, 692. Therefore, unintended side etching is suppressed. As a result, wiring pattern defects caused by side etching are suppressed, and a highly reliable resonator device 1 can be manufactured.

[0034] Particularly, in this embodiment, in a plan view of the semiconductor substrate 5, the metal layers 691, 692 are contained within the connection pads 631, 632, and the lower ends of the metal layers 691, 692 are in contact with the upper surfaces of the connection pads 631, 632. Therefore, it is possible to effectively prevent the etching solution from entering outside the metal layers 691, 692, and it is possible to effectively prevent unintended side etching. As a result, it is possible to more effectively prevent wiring pattern defects caused by wet etching.

[0035] Through the above steps, the through holes 21, 22 are formed, passing from the first surface 5a through the inside of the metal layers 691, 692 and facing the connection pads 631, 632 of the wiring layer 63. According to such a method for forming the through holes 21, 22, it is possible to form the through holes 21, 22 having a high aspect ratio while suppressing plasma damage to the wiring layer 63 and wiring pattern defects caused by side etching. Therefore, it is possible to manufacture a highly reliable and small resonator device 1.

[0036] ≪Conductive material placement step S22≫ 11, an insulating film 50 is formed on the first surface 5a of the semiconductor substrate 5 and the inner surfaces of the through holes 21, 22. The method for forming the insulating film 50 is not particularly limited, and for example, CVD (chemical vapor deposition) can be used. Next, as shown in FIG. 12, the insulating film 50 formed on the bottom surfaces of the through holes 21, 22 is removed by etching to expose the connection pads 631, 632 in the through holes 21, 22.

[0037] Next, the conductive material E is disposed in a film shape on the first surface 5a and filled into the through holes 21, 22. Next, the conductive material E on the first surface 5a is patterned by etching. As a result, as shown in FIG. 13, the wirings 28, 29 and the through electrodes 210, 220 are formed at once. The conductive material E is not particularly limited, but for example, the same material as the wiring layer 63 can be used. This increases the affinity between the through electrodes 210, 220 and the wiring layer 63, and effectively suppresses poor contact between them. In addition, since the material can be shared, the manufacturing cost of the vibration device 1 can be reduced. However, the conductive material E is not particularly limited, and for example, it can be a laminated structure of titanium tungsten alloy (TiW) / copper (Cu) / gold (Au).

[0038] <Vibration element placement process S3> Next, the vibration element 4 is mounted on the wirings 28 and 29 via the metal bumps 81 and 82 .

[0039] <Lid placement process S4> Next, the lid 3 is bonded to the upper surface of the base 2. In this manner, the vibration device 1 is manufactured as shown in FIG.

[0040] The vibration device 1 and the manufacturing method of the vibration device 1 have been described in detail above. As described above, the vibration device 1 has the base 2 and the vibration element 4 arranged on the base 2. The base 2 also has an integrated circuit 6 including a semiconductor substrate 5 having a first surface 5a and a second surface 5b that are in a front-back relationship, a wiring layer 63 arranged on the second surface 5b side and having connection pads 631 and 632, and an insulating layer 62 arranged between the second surface 5b and the wiring layer 63, through electrodes 210 and 220 that penetrate the semiconductor substrate 5 and the insulating layer 62 and are connected to the connection pads 631 and 632, and annular metal layers 691 and 692 that are arranged between the second surface 5b and the wiring layer 63, penetrating the insulating layer 62, and surrounding the through electrodes 210 and 220 in a plan view of the semiconductor substrate 5. According to the resonator device 1 having such a configuration, even if the through holes 213, 223 penetrating the insulating layer 62 are formed by wet etching, the metal layers 691, 692 function as guard rings and restrict further side etching. Therefore, for example, plasma damage as in dry etching is not given to the wiring layer 63, and wiring pattern defects caused by side etching are suppressed. Therefore, the resonator device 1 has high reliability.

[0041] As described above, in a plan view of the semiconductor substrate 5, the metal layers 691, 692 are contained within the connection pads 631, 632. This makes it possible to more effectively prevent the etching solution from penetrating outside the metal layers 691, 692, and more effectively prevent wiring pattern defects caused by side etching.

[0042] As described above, the integrated circuit 6 has a plurality of wiring layers 63, 65 stacked in the thickness direction of the semiconductor substrate 5, and the through electrodes 210, 220 are connected to the connection pads 631, 632 included in the wiring layer 63 that is located closest to the semiconductor substrate 5 among the plurality of wiring layers 63, 65. This allows the through electrodes 210, 220 to be as short as possible, making it easier to form the through electrodes 210, 220.

[0043] As described above, the base 2 has the etching stop layer 61 made of SiN and disposed between the second surface 5b and the insulating layer 62. This makes it possible to suppress over-etching when the semiconductor substrate 5 is dry-etched to form the through-holes 211, 221, and effectively suppresses plasma damage to the wiring layer 63.

[0044] As described above, the wiring layer 63 and the through electrodes 210, 220 are made of the same material. This increases the affinity between the through electrodes 210, 220 and the wiring layer 63, and effectively suppresses poor contact between them. In addition, since the material can be shared, the manufacturing cost of the resonator device 1 can be reduced.

[0045] As described above, the vibration element 4 is disposed on the first surface 5a side of the semiconductor substrate 5. The vibration device 1 also has a lid 3 that houses the vibration element 4 between the base 2 and the vibration device 1. This makes it possible to protect the vibration element 4. By forming the integrated circuit 6 on the second surface 5b side, a larger space can be secured for forming the integrated circuit 6 since there is no bonding area with the lid 3 compared to the case where the integrated circuit 6 is formed on the first surface 5a.

[0046] As described above, the manufacturing method of the vibration device 1 includes a base preparation process S1 for preparing a base 2 having a semiconductor substrate 5 having a first surface 5a and a second surface 5b that are reverse to each other, an integrated circuit 6 including a wiring layer 63 arranged on the second surface 5b side and having connection pads 631, 632, and an insulating layer 62 arranged between the second surface 5b and the wiring layer 63, and annular metal layers 691, 692 arranged between the second surface 5b and the wiring layer 63 and penetrating the insulating layer 62, and a through electrode formation process S2 for forming through electrodes 210, 220 that penetrate the semiconductor substrate 5 and the insulating layer 62 and pass through the inside of the metal layers 691, 692 to be connected to the connection pads 631, 632. The through-electrode forming step S2 includes a through-hole forming step S21 in which the semiconductor substrate 5 is penetrated by dry etching, and then the insulating layer 62 is penetrated by wet etching to form the through-holes 21 and 22 that face the connection pads 631 and 632 from the first surface 5a through the inside of the metal layers 691 and 692, and a conductive material disposing step S22 in which a conductive material E is disposed in the through-holes 21 and 22 to form the through-electrodes 210 and 220. According to this method, even if the through-holes 213 and 223 that penetrate the insulating layer 62 are formed by wet etching, the metal layers 691 and 692 function as guard rings, and further side etching is restricted. Therefore, for example, plasma damage that occurs in dry etching is not given to the wiring layer 63, and pattern defects of the wiring caused by side etching are suppressed. Therefore, the resonator device 1 has high reliability.

[0047] As described above, the base 2 has the etching stop layer 61 made of SiN and disposed between the second surface 5b and the insulating layer 62. This makes it possible to suppress over-etching when the semiconductor substrate 5 is dry-etched to form the through-holes 211, 221, and effectively suppresses plasma damage to the wiring layer 63.

[0048] <Second embodiment> FIG. 15 is a vertical cross-sectional view showing the vibration device according to the second embodiment.

[0049] The vibration device 1 of this embodiment is similar to the vibration device 1 of the first embodiment described above, except for the configuration of the base 2. In the following description, the present embodiment will be described with a focus on the differences from the previous embodiment, and the description of the similarities will be omitted. In addition, in FIG. 15, the same reference numerals are used for the same configurations as the previous embodiment.

[0050] As shown in FIG. 15, the base 2 of this embodiment is upside down with respect to the first embodiment described above, and the integrated circuit 6 is formed on the upper surface side of the semiconductor substrate 5, i.e., the second surface 5b side. The vibration element 4 is disposed on the upper surface side of the semiconductor substrate 5, and the vibration element 4 and the integrated circuit 6 are joined via a pair of metal bumps 81 and 82. The integrated circuit 6 is formed slightly smaller than the base 2 except for the outer periphery of the second surface 5b in order to secure a joining space with the lid 3 on the second surface 5b of the semiconductor substrate 5. With this configuration, the integrated circuit 6 can be accommodated and protected in the accommodation section S together with the vibration element 4.

[0051] In the terminal layer 68 of the integrated circuit 6, wirings 682 and 683 that electrically connect the vibration element 4 and the wiring layer 65 are arranged instead of the mounting terminal 681 of the first embodiment described above. Moreover, on the first surface 5a side of the semiconductor substrate 5, a plurality of mounting terminals 26 are arranged instead of the wirings 28 and 29 described above. Each mounting terminal 26 is electrically connected to the integrated circuit 6 via a through electrode 230 that passes through the semiconductor substrate 5, the etching stop layer 61, and the insulating layer 62 through an annular metal layer 693 formed by penetrating the insulating layer 62. The through electrode 230 has the same configuration as the through electrodes 210 and 220 of the first embodiment described above, and the metal layer 693 has the same configuration as the metal layers 691 and 692 of the first embodiment described above. Moreover, these are formed by the same method as the first embodiment described above.

[0052] As described above, in the resonator device 1 of this embodiment, the resonator element 4 is disposed on the second surface 5b side of the semiconductor substrate 5. The resonator device 1 also has the lid 3 that houses the resonator element 4 and the integrated circuit 6 between the base 2. This makes it possible to protect the resonator element 4 and the integrated circuit 6.

[0053] The second embodiment as described above can also achieve the same effects as the first embodiment described above.

[0054] <Third embodiment> FIG. 16 is a cross-sectional view showing a metal layer of the resonation device according to the third embodiment.

[0055] The resonator device 1 of this embodiment is similar to the resonator device 1 of the first embodiment described above, except that the configurations of the metal layers 691 and 692 are different. In the following description, the present embodiment will be described with a focus on the differences from the previous embodiment, and the description of the similarities will be omitted. In addition, in FIG. 16, the same reference numerals are used for the same configurations as the previous embodiment.

[0056] As shown in FIG. 16, the resonator device 1 of the present embodiment has a plurality of metal layers 691 arranged concentrically. Specifically, the plurality of metal layers 691 include a first metal layer 691a located at the innermost position and surrounding the through electrode 210, a second metal layer 691b located outside the first metal layer 691a and surrounding the first metal layer 691a, and a third metal layer 691c located outside the second metal layer 691b and surrounding the second metal layer 691b. According to this configuration, the leakage of the etching solution can be prevented by the triple metal layer 691, so that the pattern defects of the wiring caused by the side etching can be more reliably suppressed. However, the number of the metal layers 691 is not particularly limited, and may be two or four or more.

[0057] Similarly, the resonator device 1 of the present embodiment has a plurality of metal layers 692 arranged concentrically. Specifically, the plurality of metal layers 692 include a first metal layer 692a located at the innermost position and surrounding the through electrode 220, a second metal layer 692b located outside the first metal layer 692a and surrounding the first metal layer 692a, and a third metal layer 692c located outside the second metal layer 692b and surrounding the second metal layer 692b. According to this configuration, the leakage of the etching solution can be prevented by the triple metal layer 692, so that the pattern defects of the wiring caused by the side etching can be more reliably suppressed. However, the number of the metal layers 692 is not particularly limited, and may be two or four or more.

[0058] As described above, in the resonator device 1 of the present embodiment, the metal layers 691, 692 include the first metal layers 691a, 692a surrounding the through electrodes 210, 220, and the second metal layers 691b, 692b surrounding the first metal layers 691a, 692a. This makes it possible to more reliably suppress wiring pattern defects caused by side etching.

[0059] The third embodiment as described above can also achieve the same effects as the first embodiment described above.

[0060] The vibration device and the manufacturing method of the vibration device of the present invention have been described above based on the illustrated embodiment, but the present invention is not limited thereto, and the configuration of each part can be replaced with any configuration having a similar function. In addition, any other configuration may be added to the present invention. In addition, each embodiment may be appropriately combined. [Explanation of symbols]

[0061] 1...Vibration device, 10...Package, 2...Base, 21...Through hole, 210...Through electrode, 211...Through hole, 212...Through hole, 213...Through hole, 22...Through hole, 220...Through electrode, 221...Through hole, 222...Through hole, 223...Through hole, 230...Through electrode, 26...Mounting terminal, 28...Wiring, 29...Wiring, 3...Lid, 31...Recess, 4...Vibration element, 41...Vibration substrate, 42...Electrode, 421...Excitation electrode, 422...Excitation electrode, 423...Terminal, 424...Terminal, 425...Wiring, 426...Wiring, 5...Semiconductor substrate, 5a...First surface, 5b...Second surface, 50...Insulating film, 6...Integrated circuit, 6A...Oscillation circuit, 60...Laminate, 61...Etching stop layer, 62...Insulating layer, 63... Wiring layer, 631...connection pad, 632...connection pad, 64...insulating layer, 65...wiring layer, 66...insulating layer, 67...passivation film, 68...terminal layer, 681...mounting terminal, 682...wiring, 683...wiring, 7...joint member, 81...metal bump, 82...metal bump, 691...metal layer, 691a...first metal layer, 691b...second metal layer, 691c...third metal layer, 692...metal layer, 692a...first metal layer, 692b...second metal layer, 692c...third metal layer, 693...metal layer, E...conductive material, S...accommodation portion, S1...base preparation step, S2...through electrode formation step, S21...through hole formation step, S22...conductive material arrangement step, S3...vibration element arrangement step, S4...lid arrangement step

Claims

1. With the base, a vibration element disposed on the base, The base includes a semiconductor substrate having a first surface and a second surface that are opposite to each other; a wiring layer disposed on the second surface side and including a connection pad; an insulating layer disposed therebetween; and A through electrode that passes through the semiconductor substrate and the insulating layer and is connected to the connection pad. and, an etching stop layer disposed between the second surface and the insulating layer and made of SiN; and, a first insulating layer that is disposed between the second surface and the wiring layer and that extends through the insulating layer; a ring-shaped metal layer surrounding the through electrode in plan view, device.

2. With the base, a vibration element disposed on the base, The base includes a semiconductor substrate having a first surface and a second surface that are opposite to each other; a wiring layer disposed on the second surface side and including a connection pad; an insulating layer disposed therebetween; and A through electrode that passes through the semiconductor substrate and the insulating layer and is connected to the connection pad. and, a first insulating layer that is disposed between the second surface and the wiring layer and that extends through the insulating layer; a ring-shaped metal layer surrounding the through electrode in a plan view; The metal layer includes a first metal layer surrounding the through electrode and a second metal layer surrounding the first metal layer. A vibration device comprising:

3. In a plan view of the semiconductor substrate, the metal layer is preferably included in the connection pad. The vibration device according to claim 1 or 2.

4. The integrated circuit has a plurality of the wiring layers stacked in a thickness direction of the semiconductor substrate. 、 The through electrode is the wiring layer located closest to the semiconductor substrate among the plurality of wiring layers.

4. The transducer according to claim 1, further comprising a connecting pad included in said connecting pad. Operating device.

5. 5. The method according to claim 1, wherein the wiring layer and the through electrode are made of the same material.

2. The vibration device according to claim 1.

6. The vibration element is disposed on the first surface side of the semiconductor substrate, 6. The method according to claim 1, further comprising: a lid for accommodating the vibration element between the base and the lid.

2. The vibration device according to claim 1.

7. The vibration element is disposed on the second surface side of the semiconductor substrate, a lid for housing the vibration element and the integrated circuit between the base and the lid; 6. A vibration device according to any one of claims 1 to 5.

8. A semiconductor substrate having a first surface and a second surface, the first surface and the second surface being in a reverse relationship, and a a wiring layer having a connection pad; and an insulating layer disposed between the second surface and the wiring layer. an edge layer; and an integrated circuit including the edge layer and disposed between the second surface and the wiring layer through the insulating layer. a base preparation step of preparing a base having an annular metal layer; The semiconductor substrate and the insulating layer are penetrated, and the metal layer is passed through the inside of the metal layer to the connection pad. a through electrode forming step of forming a through electrode connected to the a vibration element arrangement step of mounting a vibration element on the base after the through electrode formation step; Including, The through electrode forming step includes: After penetrating the semiconductor substrate by dry etching, The insulating layer is penetrated to form the connection pad from the first surface through the inside of the metal layer. a through hole forming step of forming a through hole facing the bed; a conductive material disposing step of disposing a conductive material in the through hole to form the through electrode; A method for manufacturing a vibration device, comprising:

9. The base is disposed between the second surface and the insulating layer and is an etched silicon nitride (SiN) substrate. The method for manufacturing a vibration device according to claim 8 , further comprising a stop layer.

Citation Information

Patent Citations

  • Electronic component and manufacturing method thereof

    JP2007281289A

  • Semiconductor device and manufacturing method of same

    JP2009259876A

  • Method for forming vertical electrical connections in a multilayer semiconductor structure

    JP2014519201A

  • Piezoelectric oscillator and manufacturing method therefor

    JP2017139717A

  • Vibration device, method for manufacturing vibration device, electronic device, and mobile body

    JP2020028095A