SUBSTRATE PROCESSING METHOD AND SUBSTRATE PROCESSING SYSTEM
By forming a water-repellent inhibition film and applying the coating liquid from outside to inside the edge, the method addresses non-uniform film thickness issues, achieving a 41% reduction in hump thickness and enhancing film uniformity on substrate edges.
Patent Information
- Application Number
- JP2020119224
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-07-10
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2040-07-10
AI Technical Summary
Conventional methods for applying a coating liquid to the peripheral edge of substrates, such as semiconductor wafers, result in non-uniform film thickness due to the formation of humps, which reduces yield and are difficult to mitigate through increased rotational speed or liquid composition changes.
A substrate processing method involving the formation of a water-repellent inhibition film on the substrate surface, followed by removing this film from the peripheral edge and applying the coating liquid while rotating, ensuring the liquid is directed from outside to inside the edge, thereby suppressing hump formation and enhancing film thickness uniformity.
The method significantly reduces hump formation and achieves a uniform coating film thickness, improving yield by suppressing the inward diffusion of the coating liquid, with a 41% reduction in hump thickness compared to conventional methods.
Smart Images

Figure 0007583541000001 
Figure 0007583541000002 
Figure 0007583541000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a substrate processing method and a substrate processing system. [Background technology]
[0002] 2. Description of the Related Art Conventionally, a coating liquid is applied to the edge portion of a substrate such as a semiconductor wafer (hereinafter, sometimes simply referred to as a wafer) to protect the edge portion.
[0003] In this regard, Patent Document 1 describes a peripheral coating device that applies a coating liquid to the peripheral portion of a substrate, the peripheral coating device comprising: a rotating holding unit that holds the substrate horizontally and rotates it; a coating liquid supply unit that is positioned above the substrate and has a coating liquid nozzle that ejects the coating liquid downward and supplies the coating liquid to the surface of the substrate; a horizontal transport unit that moves the coating liquid nozzle horizontally; and a coating control unit that controls the rotating holding unit, the coating liquid supply unit, and the horizontal transport unit. The coating control unit performs scan-in control, which controls the rotating and holding unit to rotate the substrate, and the coating liquid supply unit to eject the coating liquid from the coating liquid nozzle, while controlling the horizontal transport unit to move the coating liquid nozzle from outside the periphery of the substrate to above the periphery of the substrate; and scan-out control, which controls the rotating and holding unit to rotate the substrate, and controls the coating liquid supply unit to eject the coating liquid from the coating liquid nozzle, while controlling the horizontal transport unit to move the coating liquid nozzle from above the periphery of the substrate to outside the periphery of the substrate, and is configured to move the coating liquid nozzle at a speed slower than the speed at which the coating liquid moves toward the periphery of the substrate when performing the scan-out control. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2014-110386 A Summary of the Invention [Problem to be solved by the invention]
[0005] The technology according to the present disclosure improves the uniformity of the film thickness of the coating liquid applied to the peripheral edge of the substrate. [Means for solving the problem]
[0006] One aspect of the present disclosure is a substrate processing method for processing a substrate, the method comprising: providing a water-repellent layer on at least a peripheral portion of a surface of the substrate, the water-repellent layer being configured to inhibit diffusion of a coating liquid thereon. or hydrophobic a step of forming an inhibitor film having the above structure; a step of horizontally holding and rotating the substrate on which the inhibitor film has been formed, and removing a part of the inhibitor film on the peripheral edge by moving the nozzle from the outside of the peripheral edge of the substrate to the peripheral edge while discharging a treatment liquid for removing the inhibitor film from the nozzle; and a step of subsequently holding and rotating the substrate horizontally, and moving the coating liquid nozzle from the outside of the peripheral edge of the substrate to the peripheral edge while discharging a coating liquid from the coating liquid nozzle, to form a coating film in the area from which the inhibitor film has been removed. Effect of the Invention
[0007] According to the present disclosure, it is possible to improve the uniformity of the film thickness of a coating liquid applied to the peripheral edge portion of a substrate. [Brief description of the drawings]
[0008] [Figure 1] 1A to 1C are explanatory diagrams showing a conventional method for applying a coating liquid to a peripheral portion of a substrate. [Diagram 2] 1 is a plan view showing a schematic outline of a configuration of a substrate processing system equipped with various devices for performing a substrate processing method according to an embodiment; [Diagram 3] 3 is a front view showing a schematic outline of the configuration of the substrate processing system of FIG. 2.
[0023] FIG. [Figure 4] 3 is a rear view diagrammatically illustrating an outline of the configuration of the substrate processing system of FIG. 2.
[0023] FIG. [Diagram 5]FIG. 2 is an explanatory diagram showing a schematic outline of the configuration of an adhesion device that forms an inhibitory film. [Figure 6] FIG. 2 is an explanatory diagram illustrating a schematic outline of the configuration of a peripheral edge removing device. [Figure 7] FIG. 2 is an explanatory diagram showing a schematic outline of the configuration of a peripheral edge coating device. [Figure 8] 1A to 1C are explanatory diagrams in plan view showing the process of forming and partially removing an inhibition film. [Figure 9] 5A to 5C are explanatory views showing a method of applying a coating liquid to a peripheral edge of a substrate in the substrate processing method according to the embodiment; [Figure 10] 11 is a graph comparing the film thickness of a coating liquid applied to the peripheral portion of a substrate in the conventional technique and the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] In the manufacturing process of semiconductor devices, a series of photolithography steps including a resist coating process in which a resist liquid is supplied onto a wafer to form a resist film are performed, and a predetermined resist pattern is formed on the wafer. The above series of steps are performed in a coating and developing processing system equipped with various liquid processing devices for processing the wafer, heat processing devices, and a transport device for transporting the wafer. After the photolithography process, the wafer is then subjected to an etching process, and the series of photolithography steps may be performed again.
[0010] In such a process, a coating liquid is applied to the peripheral portion of a substrate such as a wafer to form a coating film and protect the peripheral portion. Such peripheral portion coating processing has conventionally been performed through a process such as that shown in FIG.
[0011] That is, first, a nozzle N for applying the coating liquid is placed on the outside of the target wafer W (FIG. 1(a)), and the coating liquid (e.g., resist liquid) R is discharged from the nozzle N while being moved toward the center (inner side) of the rotating wafer W (FIG. 1(b)). Then, the movement of the nozzle N is stopped at a predetermined position (landing point P) (FIG. 1(c)). After a predetermined time has elapsed, the nozzle N is retreated to the outside of the wafer W (FIG. 1(d)).
[0012] However, this method sometimes resulted in the formation of a ring-shaped hump H inside the landing point P, as shown in Figure 1(c). A hump is a coating film that is extremely thick compared to other areas. When this type of hump H is formed, it remains as a residue in subsequent processes, reducing the yield.
[0013] The inventor considers the cause of the formation of the hump H as follows. That is, in the coating process of the edge part of the wafer, the coating liquid R discharged from the nozzle N penetrates inside the landing point P (the point where the discharged coating liquid reaches the surface of the wafer W) during the formation of the coating film. The coating liquid R is not supplied inside the landing point P, so drying proceeds, but the coating liquid R continues to be supplied outside the landing point P, so it does not dry. Therefore, it is considered that this drying time difference is one of the causes of the occurrence of the hump H. The reason why the coating liquid discharged from the nozzle N penetrates inside the landing point P is because the discharge angle of the nozzle N with respect to the wafer W is not in the radial direction in a plan view, but has an angle of, for example, about 30 to 40 degrees with respect to the tangent direction of the wafer W, so that a vector in the inward direction acts.
[0014] To improve this, attempts have been made to reduce the drying time difference described above by increasing the rotation speed of the wafer W or changing the composition of the coating liquid R. However, this resulted in a lack of robustness in the coating film formed by the coating liquid R, and there was also a limit to how much the hump H could be reduced.
[0015] Therefore, the technique disclosed herein prevents the occurrence of the above-mentioned humps when coating a coating liquid on the peripheral edge of a substrate, thereby improving the uniformity of the film thickness of the coating liquid on the peripheral edge of the substrate.
[0016] Hereinafter, the present embodiment will be described with reference to the drawings. In this specification, elements having substantially the same functional configurations are denoted by the same reference numerals, and redundant description will be omitted.
[0017] <Substrate processing system> Fig. 2 is an explanatory diagram showing an outline of the internal configuration of a substrate processing system 1 equipped with various devices for carrying out a substrate processing method according to an embodiment, and Fig. 3 and Fig. 4 are a front view and a rear view, respectively, showing an outline of the internal configuration of the substrate processing system 1.
[0018] 2, the substrate processing system 1 has a cassette station 10 where a cassette C containing a plurality of wafers W is loaded and unloaded, and a processing station 11 equipped with a plurality of various processing devices that perform predetermined processing on the wafers W. The substrate processing system 1 has a configuration in which the cassette station 10, the processing station 11, and an interface station 13 that transfers the wafer W between the processing station 11 and an exposure device 12 adjacent to the processing station 11 are integrally connected.
[0019] The cassette station 10 is provided with a cassette placement stage 20. The cassette placement stage 20 is provided with a plurality of cassette placement plates 21 on which the cassettes C are placed when the cassettes C are carried in and out of the substrate processing system 1.
[0020] The cassette station 10 is provided with a wafer transfer device 23 that is movable on a transfer path 22 that extends in the X direction in the figure. The wafer transfer device 23 is also movable in the up-down direction and around the vertical axis (the θ direction), and can transfer wafers W between the cassettes C on each cassette mounting plate 21 and a transfer device in the third block G3 of the processing station 11, which will be described later.
[0021] The processing station 11 is provided with a plurality of blocks, for example, four blocks G1, G2, G3, and G4, each equipped with various devices. For example, a first block G1 is provided on the front side (negative side in the X direction in FIG. 2) of the processing station 11, and a second block G2 is provided on the rear side (positive side in the X direction in FIG. 2) of the processing station 11. A third block G3 is provided on the cassette station 10 side of the processing station 11 (negative side in the Y direction in FIG. 2), and a fourth block G4 is provided on the interface station 13 side of the processing station 11 (positive side in the Y direction in FIG. 2).
[0022] 4, the first block G1 is provided with a plurality of liquid processing devices, such as a developing device 30, a lower anti-reflection film forming device 31, a resist film forming device 32, an upper anti-reflection film forming device 33, an edge removing device 34, and an edge coating device 35. The developing device 30 develops the wafer W. The lower anti-reflection film forming device 31 forms an anti-reflection film (hereinafter referred to as "lower anti-reflection film") on the lower layer of the resist film of the wafer W. The resist film forming device 32 supplies a resist liquid to the wafer W to form a resist film. The upper anti-reflection film forming device 33 forms an anti-reflection film (hereinafter referred to as "upper anti-reflection film") on the upper layer of the resist film of the wafer W.
[0023] The number and arrangement of the developing treatment device 30, the lower anti-reflection film forming device 31, the resist film forming device 32, the upper anti-reflection film forming device 33, the edge removing device 34, and the edge coating device 35 can be selected arbitrarily.
[0024] In the developing treatment device 30, the lower anti-reflection film forming device 31, the resist film forming device 32, the upper anti-reflection film forming device 33, the peripheral portion removing device 34, and the peripheral portion coating device 35, for example, spin coating using a predetermined processing liquid or coating liquid is performed on the wafer W. In spin coating, for example, the processing liquid or coating liquid is discharged from a nozzle onto the wafer W, and the wafer W is rotated to spread the processing liquid or coating liquid on the surface of the wafer W.
[0025] In the second block G2, as shown in Fig. 4, a heat treatment device 40, an adhesion device 41, and an edge exposure device 42 are arranged vertically and horizontally. The heat treatment device 40 performs heat treatment such as heating and cooling of the wafer W. The adhesion device 41 supplies HMDS or the like in a vapor state onto the wafer W to uniformly form a hydrophobic film on the wafer W in order to improve the adhesion between the resist liquid and the wafer W. The edge exposure device 42 exposes the outer periphery of the wafer W. The number and arrangement of the heat treatment devices 40, adhesion devices 41, and edge exposure devices 42 can be selected arbitrarily.
[0026] For example, in the third block G3, a plurality of transfer devices 50, 51, 52, 53, 54, 55, 56 are provided in this order from the bottom up, while in the fourth block G4, a plurality of transfer devices 60, 61, 62 are provided in this order from the bottom up.
[0027] 4, a region surrounded by the first block G1 to the fourth block G4 forms a wafer transfer region D. In the wafer transfer region D, a wafer transfer device 70 is disposed.
[0028] Each of the wafer transfer devices 70 has a transfer arm 70a that is movable in, for example, the Y direction, the X direction, the θ direction, and the up and down direction. A plurality of wafer transfer devices 70 are arranged one above the other, and each wafer transfer device 70 moves within the wafer transfer region D and can transfer the wafer W to a predetermined device at approximately the same height in each of the blocks G1 to G4.
[0029] In addition, in the wafer transfer region D, a shuttle transfer device 80 is provided which linearly transfers the wafer W between the third block G3 and the fourth block G4.
[0030] The shuttle transfer device 80 is movable linearly, for example, in the Y direction in Fig. 4. The shuttle transfer device 80 moves in the Y direction while supporting the wafer W, and can transfer the wafer W between the delivery device 52 in the third block G3 and the delivery device 62 in the fourth block G4.
[0031] 2, a wafer transfer device 90 is provided next to the third block G3 on the positive side in the X direction. The wafer transfer device 90 has a transfer arm 90a that is movable in, for example, the X direction, the θ direction, and the up and down directions. The wafer transfer device 90 moves up and down while supporting the wafer W, and can transfer the wafer W to each delivery device in the third block G3.
[0032] The interface station 13 is provided with a wafer transfer device 100 and a delivery device 101. The wafer transfer device 100 has a transfer arm 100a that is movable in, for example, the Y direction, the θ direction, and the up and down directions. The wafer transfer device 100 supports a wafer W on, for example, the transfer arm 100a, and can transfer the wafer W between each delivery device in the fourth block G4, the delivery device 101, and the exposure device 12.
[0033] The above-described substrate processing system 1 is provided with a control unit 200. The control unit 200 is configured by a computer including, for example, a CPU, a memory, and the like, and has a program storage unit (not shown). The program storage unit stores programs for controlling various processes in the substrate processing system 1. The above-described programs may be recorded in a computer-readable storage medium and installed in the control unit 200 from the storage medium.
[0034] Various devices mounted in the substrate processing system 1 having the above configuration for carrying out the substrate processing method according to the embodiment will be individually and specifically described below.
[0035] <Adhesion device> As described above, the adhesion device 41 is originally intended to supply HMDS to the entire surface of the wafer W before applying the resist liquid for pattern formation in order to improve the adhesion between the resist liquid and the wafer W. However, it is known that HMDS has water repellency. Therefore, this adhesion device 41 is used in the process of forming the inhibition film in the embodiment.
[0036] 5, the adhesion device 41 has a processing vessel 110. A mounting table 111 on which a wafer W is placed is provided in the processing vessel 110. A heater 112 for heating is provided in the mounting table 111. The mounting table 111 has a plurality of through holes 113 formed therein. Lift pins 114a that move up and down within these through holes 113 are provided on a lift pin support portion 114. The lift pin support portion 114 is raised and lowered by a lift mechanism 115.
[0037] An air supply port 116 is provided in the center of the ceiling of the processing vessel 110, and a supply path 117 is connected to the air supply port 116. The supply path 117 is connected to a supply source of HMDS vapor (not shown). Meanwhile, an exhaust port 118 is provided outside the mounting table 111 at the bottom of the processing vessel 110, and an exhaust path 119 is connected to the exhaust port 118. The exhaust path 119 is connected to an exhaust device M.
[0038] With the above-described configuration, the HMDS vapor supplied from the air inlet 116 is supplied uniformly to the upper surface of the wafer W heated to a predetermined temperature by the heater 112 on the mounting table 111, and a water-repellent HMDS film is formed as an inhibitor film over the entire surface of the wafer W.
[0039] <Edge Removal Device> The peripheral edge removal device 34 has the configuration shown in Fig. 6. That is, the peripheral edge removal device 34 has a processing vessel 120, and a spin chuck 121 is provided in the center thereof as a rotation holding mechanism that horizontally holds and rotates the wafer W by suction. The spin chuck 121 is supported by a rotation support member 122. The rotation support member 122 is connected to a rotation drive mechanism 123 such as a motor. The rotation support member 122 is configured to be movable up and down.
[0040] A filter device 124 is provided on the ceiling of the processing vessel 120 , and a downflow of purified air is formed in the processing vessel 120 via an air supply part 125 .
[0041] A cup 126 is disposed around the spin chuck 121 so as to surround the wafer W held by the spin chuck 121. A drain pipe 127 and an exhaust pipe 128 are provided at the bottom of the cup 126. The exhaust pipe 128 is connected to an exhaust device 129.
[0042] In the processing vessel 120, nozzles 130 and 131 are disposed for discharging a processing liquid capable of removing the HMDS film, such as an alkaline processing liquid, such as a developing liquid. That is, the peripheral edge removal device 34 has a nozzle 130 for discharging a developing liquid from the upper surface side of the wafer W held by the spin chuck 121 toward the peripheral edge of the wafer W, and a nozzle 131 for discharging a developing liquid from the rear surface side of the wafer W toward the rear surface of the peripheral edge of the wafer W. The nozzle 130 located on the upper side can be moved by a support arm (not shown), and moves between the position during discharging shown in FIG. 6 and a retreated position outside the cup 126 when the wafer W is carried in and out. Furthermore, even when discharging, the nozzle 130 can be moved within an arbitrary range from the outside to the inside of the peripheral edge of the held wafer W. The nozzle 131 is for removing the HMDS melt or processing liquid that has reached the rear surface side, and is usually fixedly disposed at a fixed position.
[0043] <Edge Coating Device> The peripheral coating device 35 has the configuration shown in Fig. 7. This peripheral coating device 35 basically has the same configuration as the peripheral removal device 34 described above. That is, the peripheral coating device 35 has a processing vessel 140, in the center of which is provided a spin chuck 141. The spin chuck 141 is supported by a rotation support member 142 that can move up and down, and the rotation support member 142 is connected to a rotation drive mechanism 143.
[0044] A filter device 144 is provided on the ceiling of the processing vessel 140, and a downflow of purified air is formed in the processing vessel 140 via an air supply unit 145. A cup 146 is disposed around the spin chuck 141. A drain pipe 147 and an exhaust pipe 148 are provided at the bottom of the cup 146, and the exhaust pipe 148 is connected to an exhaust device 149.
[0045] A coating liquid nozzle 150 for discharging a coating liquid for protecting the peripheral portion of the wafer W, such as a resist liquid, toward the peripheral portion, and a solvent nozzle 151 for discharging a solvent for removing the coating liquid can be arranged in the processing vessel 140. That is, the peripheral portion coating device 35 has the coating liquid nozzle 150 for discharging a coating liquid from the upper surface side of the wafer W held by the spin chuck 141 toward the peripheral portion of the wafer W, and the solvent nozzle 151 from the back surface side of the wafer W toward the back surface of the peripheral portion of the wafer W.
[0046] 7 and a retracted position outside the cup 146 when the wafer W is loaded or unloaded. Furthermore, when the coating liquid is discharged, the coating liquid nozzle 150 can move within a desired range from the outside to the inside of the peripheral edge of the held wafer W. The solvent nozzle 151 is for removing the coating liquid that has reached the back side, and is usually fixed at a fixed position.
[0047] <Substrate processing method> The adhesion device 41, edge removing device 34 and edge coating device 35 mounted on the substrate processing system 1 have the above-described configurations, and next, a substrate processing method according to an embodiment using each of these devices will be described.
[0048] First, the wafer W, the peripheral portion of which is to be protected by applying the coating liquid to the peripheral portion, is carried into the adhesion device 41 by the wafer transfer device 70 and placed on the mounting table 111. The wafer W is then heated to a predetermined temperature, for example, 90 to 200° C., by the heater 112. When the processing temperature is reached, HMDS vapor is supplied from the gas supply port 116 to the wafer W, as shown in FIG. 5. As a result, a film S of HMDS is formed as an inhibitor film on the entire surface of the wafer W before the supply of HMDS, as shown in FIG. 8(a), as shown in FIG. 8(b).
[0049] After the HMDS film S is formed as an inhibition film in this manner, the wafer W is transported out of the adhesion device 41 by the wafer transport device 70, and then transported into the heat treatment device 40 where it is cooled to a predetermined temperature, for example 23°C.
[0050] The wafer W thus cooled is carried out by the wafer transport device 70, and then carried into the peripheral edge removal device 34. Then, as shown in Fig. 6, the nozzles 130, 131 are placed at the discharge positions with respect to the wafer W held by the spin chuck 121, and the developer is discharged onto the peripheral edge of the wafer W while rotating the wafer W at, for example, 100 to 2000 rpm. In this case, it is preferable that the nozzle 130 is moved from the outer side of the peripheral edge of the wafer W toward the inner side of the peripheral edge while discharging the developer, thereby removing the peripheral edge of the film S.
[0051] As a result, the peripheral portion of the HMDS film S that was formed as an inhibitor film on the entire surface of the wafer W is removed, and as shown in Fig. 8(c), an annular region WE where the film S has been removed appears on the outer peripheral edge of the wafer W. The radial length of the region WE is, for example, 0.5 to 5.0 mm.
[0052] The wafer W having the region WE from which the film S has been removed at the outer peripheral edge of the front surface of the wafer W in this manner is carried out by the wafer transport device 70, and then carried into the peripheral edge coating device 35. In the peripheral edge coating device 35, the wafer W is attracted and held by the spin chuck 141, as shown in Fig. 7, and then rotated by the spin chuck 141 at, for example, 100 to 1500 rpm. In this state, a coating liquid, for example, a resist liquid, is discharged from the coating liquid nozzle 150 onto the region WE of the wafer W, and a solvent is discharged from the solvent nozzle 151 on the back side onto the back surface of the peripheral portion of the wafer W.
[0053] Hereinafter, the peripheral coating process performed by the peripheral coating device 35 will be described with reference to FIG. 9. First, as shown in FIG. 9(a), the coating liquid nozzle 150 discharges the coating liquid R at the outer peripheral portion of the wafer W held by the spin chuck 141. Next, as shown in FIG. 9(b), the coating liquid nozzle 150 is moved toward the center of the wafer W, that is, toward the inner peripheral portion of the wafer W. As a result, the coating liquid R is discharged toward the region WE. Then, as shown in FIG. 9(c), when the landing point P reaches the interface (boundary) So of the HMDS film S as the inhibition film, the movement of the coating liquid nozzle 150 is stopped. In this state, for example, after 0.3 to 5.0 seconds have elapsed, the coating liquid nozzle 150 is moved to the outer peripheral portion of the wafer W as shown in FIG. 9(d). As a result, a film of the coating liquid R is formed on the peripheral portion of the wafer W.
[0054] In the above-described peripheral coating process, as shown in Fig. 9, the occurrence of humps of the coating liquid R that conventionally occurred on the peripheral portion of the wafer W is suppressed. This is because the HMDS film S formed by the adhesion device 41 is water repellent, and therefore the coating liquid, which conventionally would wrap around to the inside of the landing point P, is suppressed by the film S, thereby reducing the difference in drying time between the inside and outside of the landing point P. Therefore, the coating liquid R applied to the area WE outside the interface So of the film S can be made into a coating film having a uniform thickness.
[0055] The inventors actually conducted an experiment and obtained the results shown in Fig. 10. In Fig. 10, the horizontal axis indicates the distance from the edge of the wafer W, and the vertical axis indicates the film thickness of the coating liquid R. According to this, according to the conventional method shown by the dashed line, a hump with a film thickness exceeding 1.5 mm was formed between 1.9 mm and 2.0 mm from the edge, whereas in the example in which a water-repellent inhibiting film was formed according to the embodiment shown by the solid line, a slightly thicker film thickness occurred between 1.9 mm and 2.0 mm, but the thickness was about 0.75 mm.
[0056] And, comparing the film thickness at 1.85 mm from the edge with the maximum film thickness of the formed coating film, the conventional method reached 2.47 times, whereas the example in which the water-repellent inhibiting film was formed according to the embodiment was able to suppress this to 1.45 times. Therefore, a 41% reduction in humps was achieved compared to the conventional method. In addition, the uniformity of the film thickness of the coating film applied to this type of peripheral portion is required to be suppressed to 1.5 times or less of the film thickness at 1.85 mm, and it was confirmed that the substrate processing method according to the embodiment meets this requirement.
[0057] In the above embodiment, the film S as the inhibitor film is formed of HMDS, but of course, this is not limited to this, and other film forming materials can be used as long as they have water repellency and hydrophobicity in relation to the coating liquid R. Also, in the above embodiment, the inhibitor film is formed on the entire surface of the wafer W by the adhesion device 41, but this is not limited to this, and the inhibitor film may be formed on the entire surface of the wafer W by other formation methods, for example, spin coating.
[0058] Furthermore, in terms of the purpose of the inhibitor film, it is not necessarily necessary to form the inhibitor film over the entire surface of the wafer W; it is sufficient that the inhibitor film is formed inside the area of the coating liquid that protects the peripheral portion during the peripheral portion coating process, so for example, the inhibitor film may be formed in a ring shape around the peripheral portion of the wafer W.
[0059] Incidentally, in the peripheral coating film forming process, the position of the landing point P of the coating liquid discharged from the coating liquid nozzle 150 is set to the same position as the outer interface So of the film S as the inhibition film in the above embodiment, but it may be inside the interface So, that is, on the film S. Since the film S itself is water repellent, even if the coating liquid R is discharged on the film S, it is likely to be expelled to the outside by the centrifugal force generated when the wafer W rotates, so that it is possible to prevent the coating liquid R from being left on the film S and drying as it is to form a hump.
[0060] In the above embodiment, the process of removing the HMDS film S as an inhibitor film and the process of forming the peripheral coating film are performed in separate processing vessels, i.e., in the processing vessels 120, 140 of the peripheral removal device 34 and the peripheral coating device 35. This is because the liquid discharged is an alkaline processing liquid such as a developer in the peripheral removal device 34, whereas the coating liquid R applied in the peripheral coating device 35 is a resist liquid and its solvent, which is an organic chemical liquid, and therefore it is not preferable to discharge them directly from the same drain pipe. This has the advantage that the waste liquid treatment can be performed using existing devices and facilities as they are.
[0061] However, from the viewpoint of improving the uniformity of the film thickness applied to the peripheral portion, it is not necessarily necessary to perform the inhibitor film removal process and the peripheral portion coating film formation process in separate processing vessels, and they may be performed in a single processing vessel as long as the vessel is equipped with an apparatus having separate drainage systems.
[0062] In the above embodiment, a water-repellent film, for example, the HMDS film S, is used as the inhibition film, but the thickness d of the film S formed by the normal adhesion process shown in Fig. 9 is several nm to several tens of nm, whereas the thickness D of the coating film R formed by the coating liquid R is 100 nm to 200 nm. Even if there is a considerable difference in film thickness, if the film S is water-repellent or hydrophobic, the diffusion and wraparound of the coating liquid R can be suppressed, and the occurrence of humps can be suppressed.
[0063] However, even if a film that is not water-repellent or hydrophobic is used as the inhibitory film, it is possible to suppress the diffusion and wraparound of the coating liquid R and suppress the occurrence of humps. That is, by forming the thickness of the film S to be at least half the thickness of the coating liquid R, the interface can be made to function as a wall that suppresses the coating liquid R from wrapping around or diffusing inward. Therefore, the inhibitory film in the present disclosure is not necessarily limited to a film that is hydrophobic or water-repellent.
[0064] The embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The above-described embodiments may be omitted, substituted, or modified in various forms without departing from the scope and spirit of the appended claims. [Explanation of symbols]
[0065] 1. Substrate Processing System 34 Edge removal device 35 Edge coating device 41 Adhesion Device 120, 140 Processing container 121, 141 Spin chuck 130 Nozzle 150 Coating fluid nozzle 200 Control section P landing point R Coating Fluid S membrane So interface W wafer WE area
Claims
1. A substrate processing method for processing a substrate, comprising the steps of: forming a water-repellent or hydrophobic inhibition film on at least the periphery of the surface of the substrate to inhibit diffusion of the coating liquid; a step of horizontally holding and rotating the substrate on which the inhibitor film is formed, and discharging a treatment liquid for removing the inhibitor film from a nozzle while moving the nozzle from the outside of the peripheral portion of the substrate to the peripheral portion to remove a part of the inhibitor film on the peripheral portion; Thereafter, while holding the substrate horizontally and rotating the substrate, a coating liquid nozzle is moved from the outside of the peripheral portion of the substrate to the peripheral portion while discharging a coating liquid from the coating liquid nozzle, thereby forming a coating film in the region from which the inhibitor film has been removed; The substrate processing method comprises:
2. 2. The substrate processing method according to claim 1, wherein in the step of forming the inhibition film, the inhibition film is formed over the entire surface of the substrate.
3. The substrate processing method according to claim 1 , wherein the inhibition film is a hydrophobic film.
4. The substrate processing method according to any one of claims 1 to 3, wherein the processing liquid is an alkaline processing liquid.
5. 5. The substrate processing method according to claim 1, wherein in the process of forming the coating film, the position at which the coating liquid ejected from the coating liquid nozzle lands on the substrate is at the boundary of the inhibitor film from which the portion has been removed or inside the boundary.
6. 6. The substrate processing method according to claim 1, wherein the step of removing the part of the inhibitor film and the step of forming the coating film are each performed in separate processing chambers.
7. 6. The substrate processing method according to claim 1, wherein the step of removing the part of the inhibitor film and the step of forming the coating film are performed in the same processing chamber.
8. A substrate processing system for processing a substrate, comprising: an apparatus for forming a water-repellent or hydrophobic inhibiting film that inhibits diffusion of a coating liquid at least on the peripheral portion of the surface of the substrate; A device for removing an inhibitor film from the peripheral portion of the surface of the substrate; a device for applying a coating liquid to a peripheral portion of a surface of the substrate; A control unit for controlling each of the devices, The control unit is forming an inhibitory film that inhibits diffusion of a coating liquid on at least a peripheral portion of a surface of the substrate; and then removing a portion of the inhibitory film on the peripheral portion; thereafter, applying the coating liquid to the area from which the inhibitor film has been removed to form a coating film.
Citation Information
Patent Citations
Peripheral part coating device, peripheral part coating method and recording medium for peripheral part coating
JP2014110386A
Substrate processing method
JP2017098333A
Application and development method and application and development apparatus
JP2018049987A
Substrate processing method
JP2019024129A