Reagent solution and purification method for the purification of carbon nanomaterials

A non-mineral acid-based reagent solution using persulfate radicals effectively removes metal impurities from carbon nanomaterials at moderate temperatures, achieving high purity and structural integrity, addressing the inefficiencies of existing purification methods.

JP7584559B2Active Publication Date: 2024-11-15INDIAN OIL CORP LTD
View PDF 18 Cites 0 Cited by

Patent Information

Application Number
JP2023069569
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-06-06
Filing Date
2023-04-20
Publication Date
2024-11-15
Estimated Expiration
2043-04-20

AI Technical Summary

Technical Problem

Existing methods for purifying carbon nanomaterials, such as carbon nanotubes, are inefficient in removing embedded metal impurities without damaging the structural integrity or introducing unwanted functional groups, and often require harsh chemicals or high energy inputs.

Method used

A non-mineral acid-based reagent solution using potassium, ammonium, or sodium persulfate is used to generate persulfate radicals that selectively remove metal impurities from carbon nanomaterials at moderate temperatures, preserving the structural integrity and avoiding the introduction of oxygen functional groups.

Benefits of technology

The method achieves high-purity carbon nanomaterials up to 99.5% without structural damage, reduces environmental impact, and eliminates the need for corrosive acids, making it suitable for industrial-scale applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007584559000002
    Figure 0007584559000002
  • Figure 0007584559000003
    Figure 0007584559000003
  • Figure 0007584559000004
    Figure 0007584559000004
Patent Text Reader

Abstract

To provide a reagent solution and a method for removing catalyst metal from a carbon nanomaterial carrying catalyst metal in an amount of 15 weight % at the maximum, using an environmentally friendly nonmineral-acid based reagent solution.SOLUTION: The reagent solution includes a solid reagent selected from sodium persulfate, potassium persulfate, or ammonium persulfate, the solid reagent being dissolved in deionized water. The reagent solution can remove metal present in a carbon nanomaterial without disturbing the structural integrity of the carbon nanomaterial. The refining method of carbon nanomaterial using a nonmineral-acid-based reagent solution, comprises steps of mixing the reagent solution and an initial carbon nanomaterial to prepare carbon nanomaterial slurry, gradually heating the slurry while stirring it, filtering the slurry under vacuum, subsequently washing the slurry with deionized water to obtain refined carbon nanofiber cake, and drying the refined carbon nanofiber cake in a hot air oven to obtain a carbon nanomaterial of the purity of over 99 to 99.5 wt.%.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for removing catalytic metals embedded in carbon nanomaterials with or without heteroatoms by using an environmentally friendly non-mineral acid based reagent solution. More specifically, the present invention provides a solid reagent comprising sodium, ammonium or potassium salts of persulfate. [Background technology]

[0002] Carbon nanomaterials (CNMs) consist of single-walled carbon nanomaterials, double-walled carbon nanomaterials, multi-walled carbon nanomaterials, carbon nanofibers, carbon nanorings, etc. Among these, carbon nanotubes (CNTs) are single- or multi-walled graphene structures rolled up into seamless cylinders of various lengths and diameters. CNTs possess excellent thermal, electrical, and mechanical properties due to their structure and tube chirality. These properties are significantly affected by the presence of residual metallic impurities present in the CNTs. To fully utilize the properties of CNTs in various electrical, thermal, and mechanical applications, purification of CNTs is essential to achieve maximum purity.

[0003] The process of removing metal impurities from CNMs is traditionally carried out using strong mineral acid-based liquid reagents such as HCl, HNO3, H2SO4 and HF. In addition, a vacuum annealing process has also been used to achieve high purity CNMs.

[0004] In the prior art, a combination of ammonium persulfate and ammonia solution has been used for leaching of precious metals such as copper (Cu), silver (Ag) and gold (Au) from electronic printed circuit board (PCB) components. The leaching process selectively removes precious metals that have no chemical bond with carbon and are essentially independent. However, the current approach is exclusive in nature, with CNMs associated with polyvalent metals characterized by multiple combinations of metal oxides of iron (Fe), cobalt (Co), nickel (Ni), magnesium (Mg) and aluminum (Al). These metal impurities are strongly embedded in carbon atoms in the form of metal carbides. Thus, the removal of all these metal oxides with embedded CNMs in a single step using said reagent solution has not yet been disclosed in the prior art, especially by using said process conditions described in the present invention. Furthermore, no acid or base of any kind has been used in conjunction with said solid reagent.

[0005] The CNT production process involves the decomposition of a hydrocarbon feedstock (with or without heteroatoms such as nitrogen, oxygen, and sulfur) on a catalytic substrate at high temperatures ranging from 500 to 1000 °C, at atmospheric or elevated pressure depending on the desired CNT structure. In this CNT production method, the catalytic substrate acts as a nucleating agent for CNT growth, which follows a tip- or base-based growth mechanism, depending on the adjusted process conditions and the type of catalyst. The growth of the resulting CNTs always originates from catalyst particles that are associated with the CNT structure.

[0006] A catalyst substrate is a combination of two or three metals with a suitable support material. The metals present in the catalyst promote the growth of CNTs during the CNT production process. As a result, the metal particles of the catalyst remain intact at the tip or bottom of the CNT tube. For example, if the CNT growth follows a base growth mechanism, the metal particles are at the base of the tube, while the tip growth mechanism produces CNTs with metal attached to the tip. The CNTs thus produced are always associated with catalytic metal impurities. Furthermore, different processes produce CNTs with purities ranging from 70 to 99 wt. % depending on the type of catalyst used and on the structural requirements of the CNTs for the intended application. However, the use of CNTs in applications such as electrical / electronic / polymer / metal composites, conductive inks, etc. often requires high purity CNTs of 99.5% or more. This is an interesting challenge to achieve without compromising the structure of the CNTs.

[0007] Traditionally, the above carbon nanomaterials or CNTs have been purified by wet chemical methods or high-temperature vacuum deposition of metals at very high temperatures close to the boiling points of the metals, which is very cumbersome and energy intensive. The wet chemical method uses highly concentrated corrosive acids to remove metal impurities, but acid treatment inevitably results in many structural defects, and the structural collapse of some CNTs introduces unwanted oxygen functional groups along with excess carbonaceous material. As a result, the structural integrity of the CNTs after purification is compromised.

[0008] There are numerous reports reviewed in the prior art using different purification strategies, including physical, chemical, and thermal treatments. Physical treatments, i.e. ultracentrifugal liquid dispersion of CNTs, have been reported, but these particles are strongly attached to the carbon structure, so catalytic impurities are not effectively removed (Non-Patent Document 1).

[0009] However, the separation of various CNTs is performed according to density gradients. On the other hand, heat treatment involves heat treating CNTs in a residual air atmosphere at temperatures of about 400-450°C to possibly remove catalytic impurities, which promotes the combustion of CNTs due to the catalytic effect of the inherent catalyst particles at the treatment temperature (e.g., Non-Patent Documents 2 and 3).

[0010] Chemical oxidation, using various acids such as nitric acid or hydrogen peroxide, alone or in combination with metals to generate hydroxyl radicals in situ, has also been employed to purify CNTs. In this method, residual catalyst particles react with the acid to form the corresponding nitrates or hydroxides, which are subsequently dissolved in aqueous solution. These aggressive processes typically result in severe damage and loss to the CNTs. Furthermore, the process is often limited to small batch yields, low yields, and / or low purity. Thus, an efficient industrial-scale purification process to remove these impurities is essential. This is because many of the applications of CNTs require highly purified CNTs.

[0011] US Patent No. 5,399,633 discloses a process for separating impure carbon materials from carbon nanomaterials by grinding and heating at temperatures ranging from 600 to 1000 °C in the presence of an oxidizing agent. This method removes the impure carbon materials that are oxidized and released into the gas. Thus, the nanotubes remain unoxidized, but this method compromises the physical properties of the resulting CNTs, such as some length from the tube tips.

[0012] Patent Document 2 discloses a purification technique using a vacuum high-temperature process for crude carbon nanotube products containing metal catalysts and metal oxide supports. This process effectively removes the metal oxides and support carriers. In the purification process, a CNT sample with a carbon content of 86% is treated at a high temperature of 2300°C for 5 hours under high vacuum to reach a purity of up to 99.93%.

[0013] US Patent No. 5,399,633 discloses a method consisting of two wet purification steps and one dry purification step, which are performed sequentially. The first wet purification step involves treating the crude carbon nanotubes with an acid solution, followed by a second wet purification step in which the carbon nanotubes from the first wet purification process are purified using acetone and an acid solution. A drying step is performed after the second step, which involves a gas purge to purify the carbon nanotubes.

[0014] Patent Document 4 describes the use of Fenton's reagent to remove residual metal impurities in carbon nanotubes. The present invention deals with a purification process by preparing an aqueous slurry of impure CNT material that is treated with Fenton's reagent to create a catalyst slurry with hydrogen peroxide, and the Fe 2+ The ions catalyze the production of hydroxyl radicals, and finally, the hydroxyl radicals in the oxidation slurry are utilized to purify the CNT material to provide purified CNTs.

[0015] US Patent No. 5,399,633 discloses a method for purifying a mixture by removing single-walled carbon nanotubes and amorphous carbon by heating under oxidizing conditions sufficient to remove the amorphous carbon, followed by recovery of a product containing at least about 80% by weight of single-walled carbon nanotubes.

[0016] Patent Document 6 discloses a method for purifying carbon nanotubes using a reagent selected from the group consisting of oxidizing agents such as nitrating agents and sulfonating agents in a liquid phase, thereby reacting the carbon nanotubes with the reagent to remove carbon impurities other than the carbon nanotubes.

[0017] Patent Document 7 discloses a method for purifying carbon nanotubes containing transition metal nanoparticles and carbonaceous impurities by adding an oxidant solution to form a carbon nanotube slurry, and heating the slurry at an elevated temperature of 110° C. to evaporate at least a portion of the oxidant. An acid is then added to the heated carbon nanotube slurry to dissolve the transition metal particles.

[0018] US Patent No. 5,399,633 discloses a demetallization process for removing metal-based catalytic residues from carbon nanotubes by contacting them with an active metal agent, i.e., electropositive metals such as lithium, sodium, calcium, or their organic derivatives, followed by further treatment with an electron transport chain and then treatment with carbon monoxide.

[0019] Patent Document 9 discloses a method for removing Co, Ni, and Fe from CNTs by treating in a hydrogen atmosphere up to 650° C., followed by treatment with CO gas at 150-200° C. The sample is further treated under high temperature vacuum evaporation of the metals.

[0020] Non-Patent Document 4 discloses a process that involves treating a single-walled CNT (SWCNT) sample with 35% impurity by reacting it with an aqueous mixture of H2O2 and HCl at 40-70 °C for 4-8 hours.

[0021] Patent Document 10 discloses a method for removing metal impurities from carbon nanotubes, which comprises treating the carbon nanotubes with distilled bromine in a substantially moisture-free inert atmosphere. After treatment, the distilled bromine is removed from the carbon nanotubes, and the method removes 2.5-3.5 wt. % of iron from the CNTs.

[0022] US Patent No. 5,999,336 discloses a purification process for removing excess carbon from SWCNTs and metal-containing residual catalyst particles by oxidation, reduction, and reaction with a halogen-containing gas. This invention provides scalable high-purity SWCNTs.

[0023] Non-Patent Document 5 relates to a room-temperature method for cutting long entangled multi-walled carbon nanotubes (MWCNTs) into short, dispersible fragments by a combination of ultrasonic irradiation and ammonium persulfate (APS), in which a low concentration of oxygen-containing groups was introduced onto the surface of MWCNTs after ultrasonic irradiation in deionized water without damaging the basic MWCNT structure.

[0024] Non-Patent Document 6 relates to various methods for solubilization of carbon nanotubes. In one method, a solution of potassium persulfate (9.6 mmol) in 45 ml of double distilled water is added to an ethylene glycol solution and stirred at 130 °C for 6 h under nitrogen atmosphere. 0.4 g of MWCNTs are then added to the solution and allowed to react for 24 h under vigorous stirring to produce a surface-coated polyelectrolyte of CNTs.

[0025] US Patent No. 5,399,633 relates to the carboxylic acid functionalization of SWCNTs. In this method, raw (unfunctionalized) SWCNTs are added to a bath of an aqueous composition of ammonium persulfate, and the mixture is typically refluxed at a temperature of 20-120° C. with appropriate stirring for a treatment time ranging from one hour to several days to obtain functionalized SWCNTs. After appropriate heating, a dry powder of functionalized SWCNTs is obtained.

[0026] Patent Document 13 relates to a method for producing single-walled CNTs. Here, single-walled carbon nanotubes are treated with HNO3 to remove metal impurities and improve dispersibility. A (NH4)2S2O8 / H2SO4 solution was used as a cleavage reagent, and 25 mg of HNO3 single-walled carbon nanotubes were pre-dispersed in 50 ml of 96% H2SO4 for 1 h, and the mixture was homogenized. Then, 4 g of ammonium persulfate (NH4)2S2O8 was added as an oxidizing agent, and the mixture was further ultrasonicated at 35-40 °C for 4, 8, 20, and 30 h. Finally, the obtained sample was dried at 120 °C for 24 h.

[0027] Patent Document 14 relates to a method for producing single-walled carbon nanopipes. In this, single-walled carbon nanopipes were treated with HNO3 to remove metal impurities. (NH4)2S2O8 / H2SO4 solution was used as a cleavage reagent, and 25 mg of HNO3 single-walled carbon nanotubes were pre-dispersed in 50 ml of 96% H2SO4 for 1 h and the mixture was homogenized. Then, 4 g of ammonium persulfate (NH4)2S2O8 was added as an oxidizing agent, and the mixture was further ultrasonicated at 35-40 °C for 4, 8, 20, and 30 h. Finally, the obtained sample was dried at 120 °C for 24 h.

[0028] Patent Document 15 relates to a method for producing graphene, comprising: (i) reacting graphite in an acid solution in the presence of an oxidizing agent at 40° C. for 1 hour; and (ii) washing the product obtained in step (i) with water until it becomes neutral and drying. The ratio of graphite:acid:oxidizing agent:solvent is 1:0.1-50:0.1-50:0.1-100 by mass.

[0029] Patent Document 16 relates to a method for the synthesis of nanofluids. In this method, an aqueous mixture containing 0.01-0.1 wt% multi-walled carbon nanotubes was first sonicated for 10 minutes, and then about 20 g of KPS (potassium persulfate) and 10 g of KOH (potassium hydroxide) were added to the solution and exposed to ultrasound for 10 minutes at ambient temperature. The functionalized carbon nanotubes were then separated by a filter and washed with distilled water. The amount of persulfate is at least one of about 5 to about 50 wt%, about 5 to about 20 wt%, and about 5 to about 10 wt% of the water present in the aqueous solution.

[0030] The prior art shows that a series of different methodologies are followed for the purification of carbon nanomaterials, including acid treatment, high-temperature vacuum annealing process, treatment of samples with various harsh chemical reagents, etc. The cited methods are associated with various obstacles. For example, acid-based purification leads to the generation of acid waste and therefore concerns over its disposal, while in the case of high-temperature vacuum annealing process, very high energy is required and it is limited to small scale. In view of this, alternative methods of purification process are needed to alleviate the problems associated with the above mentioned methods. [Prior art documents] [Patent documents]

[0031] [Patent Document 1] U.S. Pat. No. 5,641,466 [Patent Document 2] China Patent Publication No. 1436722 [Patent Document 3] European Patent Application Publication No. 1061040 [Patent Document 4] U.S. Pat. No. 7,494,639 [Patent Document 5] U.S. Patent No. 6,683,783 [Patent Document 6] U.S. Patent No. 5,698,175 [Patent Document 7] US Patent Publication No. 20150225243 [Patent Document 8] U.S. Patent No. 7,868,333 [Patent Document 9] China Patent Application Publication No. 1485271 [Patent Document 10] U.S. Patent No. 8,128,901 [Patent Document 11] US Patent Publication No. 20020159944 [Patent Document 12] U.S. Patent No. 7,645,497 [Patent Document 13] Patent No. 5228323 [Patent Document 14] Chinese Patent No. 101164872 [Patent Document 15] U.S. Patent No. 9,162,894 [Patent Document 16] US Patent Publication No. 20200087149 [Non-patent literature]

[0032] [Non-Patent Document 1] Bandow et al., J. Phys. Chem. B, 1997, 101, 8839-8842 [Non-Patent Document 2] Chiang et al., J. Phys. Chem. B 2001, 105, 1157-1161 [Non-Patent Document 3] Chiang et al., J. Phys. Chem. B 2001, 105, 8297-8301 [Non-Patent Document 4] J. Phys. Chem. B, 2007, 111 (6), pp 1249-1252 [Non-Patent Document 5] Peng Liu et al. [Non-Patent Document 6] Sergio Manzetti et al. Summary of the Invention [Means for solving the problem]

[0033] The inventors of the present invention have discovered that the choice of reagent is important to remove metals encapsulated at the tip or base of carbon nanomaterials, or intercalated between carbon nanomaterials by selective oxidation of metals, while preserving the order of the carbon nanomaterial structure. The potassium or ammonium or sodium persulfate reagent solution of the present invention decomposes under reaction conditions to generate persulfate free radical species, which are responsible for the removal of metals from carbon nanomaterials, thus allowing metal particles to leave the carbon nanomaterials and react with sulfate ions to dissolve in solution. The present invention deals with a non-acid based solid reagent approach, including ammonium or sodium or potassium salts of persulfate in an appropriate molar ratio to the metal concentration of the carbon nanomaterial, which allows the purification of carbon nanomaterials in aqueous solution at moderate process conditions. The same method can also be used for the demetallization of other types of carbon materials, including pet coke.

[0034] The present invention discloses a reagent solution for purifying carbon nanomaterials at ambient to moderate process conditions. The disclosed reagent solution comprises a solid reagent selected from potassium persulfate or ammonium persulfate or sodium persulfate, dissolved in deionized water at a desired molar concentration. The reagent solution is used in an appropriate molar ratio to the metal impurities present in the carbon nanomaterials, and is present in an equal or fractional ratio of 0.1 to 1. The molar ratio of the reagent solution is selected based on the concentration of the metal impurities present in the carbon nanomaterials (CNM).

[0035] The reagent solution is mixed with initial carbon nanomaterials with a purity in the range of 85-99 wt% to produce a slurry of carbon nanomaterials, which is then charged into a vessel equipped with a high torque stirrer for uniform mixing of the slurry. The slurry is kept stirring at room temperature or gradually heated to a temperature in the range of 70-100°C for 4-12 hours. The initial carbon nanomaterials, with catalytic metal impurities in the range of 1-15 wt%, preferably 3-15 wt%, are subsequently treated with the reagent solution to remove residual metals embedded in the carbon nanomaterials.

[0036] [Technical advantages of the present invention] The advantages of the catalyst over the cited prior art are: (a) The solid reagents used are environmentally friendly non-mineral acid based reagents. (b) The purification process of carbon nanomaterials operates at low temperatures (40-90 °C), unlike the vacuum annealing process, where the process temperature is set in the range of 1400-2000 °C under vacuum, which is approximately the same as the boiling point temperature of the metals present in the carbon nanomaterials. Moreover, the vacuum annealing process is very energy intensive, since it requires very high temperatures. (c) High purity carbon nanomaterials, up to 99.5 wt%, can be achieved without compromising the structural integrity of the carbon nanomaterials. (d) No oxygen functional groups are introduced into the carbon nanomaterials, so the electrical properties of the carbon nanomaterials are fully retained. (e) Unlike the acid purification process in which some of the carbon nanomaterials are oxidized, no by-products are produced. Therefore, some functional groups are always introduced into the defect sites of the carbon nanomaterials along with the formation of unwanted carbon soot, which impairs the electrical properties of the carbon nanomaterials. (f) The reagent solution is an aqueous solution, so there is no ecological impact on the environment or human health. Furthermore, the reagent does not cause skin burns even if it comes into contact with the skin, so it can be handled safely. And, (g) Non-corrosive reagents, so the metallurgy of the reactor is protected, whereas in the case of concentrated mineral acid based refining processes, the metallurgy of the reactor is corroded. Alternatively, glass based reactors must be used, but they are fragile and these types of reactors are not suitable for industrial scale use for safety reasons.

[0037] [Objective of the Invention] The main objective of the present invention is to provide a reagent solution for the purification of carbon nanomaterials with or without heteroatoms with catalytic metal impurities. The reagent solution comprises solid reagents dissolved in deionized water in a molar ratio of 0.01 to 1.

[0038] Another object of the present invention is to provide a method for purifying carbon nanomaterials using a reagent solution. Another object of the present invention is to remove multivalent catalytic metals embedded in CNMs using a non-functionalizing, non-destructive methodology without the use of strong acids.

[0039] [Abbreviation:] CNT: Carbon nanotubes CNM: Carbon nanomaterial MWCNT: Multiwalled carbon nanotubes APS: ammonium persulfate SWCNT: Single walled carbon nanotubes KPS: Potassium persulfate TGA: thermogravimetric analysis ICP-AES: Inductive coupled plasma-atomic emission spectroscopy HiPCO: High-pressure carbon monoxide CSTR: Continuous Stirring Temperature Reactor ANFD: Agitated Buchner funnel filter / dryer reactor TEM: Transmission Electron Microscopy [Brief description of the drawings]

[0040] (A) TEM image [Figure 1] (a) TEM image of unpurified CNTs of Example 2, (b) TEM image of purified CNTs of Example 3 [Diagram 2] (c) TEM image of unpurified CNTs of Example 4, (d) TEM image of purified CNTs of Example 5. [Diagram 3] (e) TEM image of unpurified CNTs of Example 6, (f) TEM image of purified CNTs of Example 7

[0041] (B) Raman spectrum image [Figure 4a] Raman spectrum of unpurified CNTs of Example 2 [Figure 4b] Raman spectrum of purified CNTs of Example 3 [Figure 5c]Raman spectrum of unpurified CNTs of Example 4 [Figure 5d] Raman spectrum of purified CNTs of Example 5 [Figure 6e] Raman spectrum of unpurified CNTs of Example 6 (vertical axis is intensity (counts) with scale unit: 50 counts, horizontal axis is Raman shift (cm-1) with scale unit: 500 cm-1, peaks are 1351.97 cm-1, 1579.62 cm-1, 2712.02 cm-1) [Figure 6f] Raman spectrum of purified CNTs of Example 7 (vertical axis is intensity (counts) with scale unit: 50 counts, horizontal axis is Raman shift (cm-1) with scale unit: 500 cm-1, peaks are 1354.02 cm-1, 1577.62 cm-1, 2724.14 cm-1)

[0042] (C) Thermogravimetric analysis (TGA) image [Figure 7] (a) TGA curve of unpurified CNTs of Example 2, (b) TGA curve of purified CNTs of Example 3 (for both (a) and (b), the vertical axis is the weight loss rate with a scale unit of 20%, the horizontal axis is the temperature with a scale unit of 200° C., and the weight loss rates are (a) 0.6%, 92.9%, (b) 0.05%, and 99.75%). [Figure 8] (c) TGA curve of unpurified CNTs of sample 2, (d) TGA curve of purified CNTs of sample 3 (for both (c) and (d), the vertical axis is the weight loss rate with a scale unit of 20%, the horizontal axis is the temperature with a scale unit of 200°C, and the weight loss rates are (c) 0.3%, 94.9%, (d) 0.1%, 99.7%). [Figure 9] (e) TGA curve of the unpurified CNT sample of Example 6, (f) TGA curve of the purified CNT sample of Example 7 (for both (e) and (f), the vertical axis is the weight loss rate with a scale unit of 20%, the horizontal axis is the temperature with a scale unit of 200° C., and the weight loss rates are (e) 0.3%, 96.2%, (f) 0.05%, and 99.85%).

[0043] (D) XRD image [Figure 10](a) XRD image of unpurified CNTs of sample 2, (b) XRD image of purified CNTs of sample 3 (both (a) and (b) show the vertical axis as counts with a scale of 1000, and the horizontal axis as 2θ with a scale of 10 degrees). [Figure 11] (c) XRD image of an unpurified CNT sample of Example 4, (d) XRD image of a purified CNT sample of Example 5 (in both (c) and (d), the vertical axis is counts with a scale unit of 1000, and the horizontal axis is 2θ with a scale unit of 10 degrees). [Figure 12] (e) XRD image of the unpurified CNT sample of Example 4, (f) XRD image of the unpurified CNT sample of Example 5 (for both (e) and (f), the vertical axis is count with a scale unit of 1000, and the horizontal axis is 2θ with a scale unit of 10 degrees). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0044] [Detailed Description of the Invention] Those skilled in the art will recognize that the present disclosure is subject to variations and modifications other than those specifically described. The present disclosure is to be understood to include all such variations and modifications. The present disclosure also includes all process steps, system features, and all combinations of any or more of such steps or features, individually or collectively referred to or shown in this specification.

[0045] [Definition] For convenience, before further describing this disclosure, certain terms and examples used herein are summarized here.These definitions should be read in light of the remaining parts of the disclosure and should be understood by those skilled in the art.Terms used herein have meanings that are recognized and known by those skilled in the art, but for convenience and completeness, certain terms and their meanings are described below.

[0046] The articles "a," "an," and "the" are used to refer to one or to more than one (ie, to at least one) of the grammatical object of the article.

[0047] The terms "comprise" and "comprising" are used in an inclusive and open sense, meaning that additional elements may be included, and are not intended to be interpreted as "consisting only of."

[0048] Throughout this specification, unless the context otherwise requires, the word "comprise" and variations such as "comprise" and "comprising" are understood to mean the inclusion of stated elements or steps or groups of elements or steps but not to the exclusion of other elements or steps or groups of elements or steps.

[0049] The term "including" is used to mean "including, but not limited to." "Including" and "including, but not limited to" are used interchangeably.

[0050] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this disclosure belongs.Although any method and material similar or equivalent to those described herein can be used to carry out or test this disclosure, preferred methods and materials are described herein.All publications mentioned herein are incorporated herein by reference.

[0051] The present disclosure is not limited in scope by the specific embodiments described herein, which are for purposes of illustration only, and functionally equivalent products and processes as described herein are clearly within the scope of the present disclosure.

[0052] The present invention discloses a reagent solution for purifying carbon nanomaterials at ambient to moderate process conditions. The disclosed reagent solution comprises solid reagents selected from potassium persulfate or ammonium persulfate or sodium persulfate, dissolved in deionized water at a desired molar concentration. The reagent solution is used in an appropriate molar ratio to the metal impurities present in the carbon nanomaterial (CNM) or in an equal or fractional ratio of 0.1 to 1. The molar ratio of the reagent solution selected is based on the initial metal impurities present in the carbon nanomaterial. The carbon nanomaterial is characterized by a bulk density in the range of 0.01 to 0.2 g / cc. Also, the carbon nanomaterial with or without heteroatoms is combined with transition metals in the form of metal carbides and encapsulated or intercalated with carrier metal oxides.

[0053] In another embodiment, the reagent solution for the purification of carbon nanomaterials comprises: (a) a solid reagent selected from the group consisting of sodium persulfate, potassium persulfate, ammonium persulfate and mixtures thereof; and (b) deionized water, wherein the solid reagent is dissolved in the deionized water in a molar ratio of 0.01 to 1. This molar ratio of the reagents varies from 0.01 moles to 1 moles depending on the initial purity of the carbon nanomaterial. Also, the solid reagent is a non-mineral acid compound.

[0054] In another embodiment, carbon nanomaterials derived from various supported catalysts of iron, cobalt, nickel, manganese, and magnesium are selected for purification using the aforementioned reagent solutions under defined purification process conditions. The reagents are selected to suppress the formation of persulfate radicals (SO4 -), which reacts with the metal impurities embedded within the carbon nanomaterials. After the purification treatment for a specified time, the carbon nanomaterial slurry is vacuum filtered and subsequently washed with deionized water. The resulting purified carbon nanomaterial cake is dried in a hot air oven at 120°C for 12 hours to remove excess water from the carbon nanomaterials. The oven-dried carbon nanomaterials are further characterized using thermogravimetric analysis (TGA) and inductively coupled plasma atomic emission spectrometry (ICP-AES) techniques to monitor the residual metal content and metal concentration of the carbon nanomaterials.

[0055] In yet another embodiment, a method for purifying carbon nanomaterials comprises: (a) mixing the reagent solution with an initial carbon nanomaterial produced by a catalytic chemical vapor deposition process using a hydrocarbon feedstock to produce a carbon nanomaterial slurry; (b) gradually heating the carbon nanomaterial slurry from room temperature to a temperature of 70-100° C. over a period of 4-12 hours while stirring; (c) filtering the carbon nanomaterial slurry under vacuum followed by washing with deionized water to obtain a purified carbon nanomaterial cake; (d) drying the purified carbon nanomaterial cake in a hot air oven at 120°C for 12 hours to obtain a carbon nanomaterial having a purity of more than 99-99.5% by weight; The process includes:

[0056] In yet another embodiment, the disclosed purification method provides carbon nanomaterials having a purity of >99-99.5 wt% without compromising the structural integrity of the carbon nanomaterial. The structural integrity of the carbon nanomaterial is evident by laser Raman spectroscopy, where the intensity of the carbon bands corresponds to Sp3 to Sp2, similar to the initial carbon nanomaterial that was purified. The current purification method of carbon nanomaterials eliminates the need for corrosive concentrated acid solutions, thereby preventing structural damage to the carbon nanomaterial.

[0057] One embodiment states that the reagent solution is one or a combination of reagents such as ammonium persulfate (APS) or potassium persulfate (KPS) or sodium persulfate dissolved in deionized water.

[0058] In another embodiment, reagent solutions of different molar concentrations are prepared in a container and stored in an airtight container. 0.01 mol to 1 mol reagent solutions of 1 to 100 wt%, preferably 1 to 50 wt%, more preferably 1 to 30 wt% 1 mol reagent solutions were used to treat the initial carbon nanomaterials to remove excess encapsulated / embedded metal impurities from the carbon nanomaterials.

[0059] In another embodiment, the carbon nanomaterials are obtained from gaseous or liquid hydrocarbon feedstocks having carbon numbers from C1 to C30 in the presence of a catalytic substrate at elevated temperatures in a suitable reactor configuration. Carbon nanomaterials are obtained by various processes leading to catalytic chemical vapor deposition in various types of reactors such as horizontal, vertical tubular reactors with incipient fluidization, continuous fluidization, fixed bed or floating catalytic reactors, high pressure carbon monoxide (HiPCO) process reactors, etc.

[0060] In another embodiment, the carbon nanomaterial contains metal impurities of either monometallic, bimetallic, trimetallic or polymetallic form of iron, cobalt, nickel, manganese, molybdenum, the metals being dispersed on a support material such as magnesium oxide, alumina, silica, or combinations thereof.

[0061] In another embodiment, carbon nanomaterials are produced from a fluidization process using a liquid or gaseous hydrocarbon feedstock, preferably in the presence of a catalyst, where the catalyst is preferably selected from iron-manganese supported on magnesia, nickel-manganese supported on magnesia, or cobalt-manganese supported on magnesia.

[0062] In another embodiment, the carbon nanomaterial comprises carbon nanotubes selected from the group consisting of single or double or triple walled carbon nanomaterials, multi-walled carbon nanomaterials, carbon nanofibers, carbon nanorings, etc. The produced carbon nanomaterials have the properties of tube structure with diameters ranging from 1-100 nm, tube lengths ranging from 1-50 μm, bulk density ranging from 0.01-0.25 g / cc, and bearing metal content varying from 0.1-15 wt%, preferably 0.1-10 wt%.

[0063] In another embodiment, the carbon nanotubes (CNTs) thus produced are ball milled to homogenize them into fine powder. Further, a CNT slurry is prepared by mixing the thus formed CNT powder having a metal concentration of 1-15 wt.% with a reagent solution in a continuous stirred temperature reactor (CSTR) or an agitated Buchner funnel filter / dryer (ANFD). The CNT slurry is mixed with the reagent solution in the ANFD and stirred for 4-12 hours at a temperature ranging from room temperature to 100°C, more preferably 40-70°C. The treated CNT slurry is subjected to vacuum to remove excess aqueous solution, followed by washing with deionized water. The filtrate cake thus obtained is oven dried at 120°C for 6-12 hours.

[0064] In another embodiment, the purified CNTs are analyzed by inductively coupled plasma optical emission spectroscopy (ICP-OES), thermogravimetric analysis (TGA), Raman spectroscopy, and transmission electron microscopy (TEM) to monitor metal profiling, residual meal content, structural defects, and structural morphology, respectively.

[0065] In another embodiment, after purification treatment of the CNTs with a reagent, purified CNTs are obtained having a carbon purity of 99.5% by weight or greater while retaining structural integrity.

[0066] [Example] Having described basic aspects of the invention, the following non-limiting examples illustrate specific embodiments thereof. Those skilled in the art will appreciate that many modifications can be made to the invention without altering its essence.

[0067] [Example 1: Preparation of reagent solution] Dissolve 228 g of ammonium persulfate in 10 liters of deionized water under stirring condition, which is solution A. The prepared solution is stored in various sealed containers which can be used as a purification agent in the CNT purification process to remove metals with appropriate concentration.

[0068] [Example 2: Carbon nanotube (CNT) manufacturing process using Fe-Mn catalyst] 100 g of 20 wt% iron and 22 wt% manganese supported on MgO catalyst is loaded into a vertical fluidized bed reactor, and then the reactor is heated to a temperature of 650 °C under an inert gas atmosphere. After reaching the desired temperature, hydrogen is passed over the catalyst along with nitrogen gas to reduce the metal oxide catalyst for 2 hours. After the reduction step is completed, the hydrogen gas is turned off and nitrogen gas is left to pass continuously over the catalyst. The petroleum hydrocarbon feed is fed into the reactor at a flow rate of 400 gm per hour using a continuous high pressure distribution pump. The liquid feed is preheated to 400 °C and the feed steam is conveyed to the reactor with the assistance of nitrogen gas. The feed steam and nitrogen gas enter the reactor where the feed steam passes over the catalyst surface, so that the feed starts to decompose and form a solid carbon product. After 8 hours of the process, the feed is stopped and the reactor is cooled under a nitrogen atmosphere. The solid carbon product weighing 1.5 kg is discharged from the reactor. The theoretical purity of the CNTs is about 93 wt%.

[0069] The carbon samples are analyzed by ICAP, XRD, TEM, Raman spectroscopy, and TGA to obtain the physicochemical characteristics of the produced carbon products.

[0070] [Example 3: Purification process of carbon nanotubes (CNTs)] 1.5 kg of CNTs with carbon purity of 93 wt% produced in Example 2 are placed in a 20 liter stainless steel vessel. CNTs with total metal impurities in the concentration range of 0.45 mol. A 100% reagent solution of 0.1 M reagent solution prepared in Example 1 is added to 1.5 kg of CNT powder to make a CNT slurry. The CNT slurry thus formed is kept under continuous stirring while the vessel is heated at a temperature of 70 °C for 12 hours. The heater is then turned off and the vessel is cooled while stirring, the slurry solution is left to stand for some time to allow the solid mass to settle to the bottom, and the excess solution is decanted. The wet solid CNT sample is washed with water under vacuum and dried in an oven at 100 °C for 12 hours. The resulting CNT material is then crushed into powder and analyzed by ICAP, TGA, XRD, Raman, and TEM characterization methods.

[0071] [Example 4: Manufacturing process of carbon nanotubes (CNTs) using Co-Mn catalyst] 100 g of 20 wt% cobalt and 22 wt% manganese supported on MgO catalyst is loaded into a vertical fluidized bed reactor and then the reactor is heated to a temperature of 650°C under an inert atmosphere. After reaching the desired temperature, hydrogen is passed over the catalyst along with nitrogen gas to reduce the metal oxide catalyst for 2 hours. After the reduction step is completed, the hydrogen gas is turned off and nitrogen gas is left passing continuously over the catalyst. The petroleum hydrocarbon feed is fed to the reactor at a flow rate of 400 gm per hour using a continuous high pressure distribution pump. The liquid feed is preheated to 400°C and the feed steam is conveyed to the reactor with the assistance of nitrogen gas. The feed steam and nitrogen gas enter the reactor where the feed steam passes over the catalyst surface, so that the feed starts to decompose and form a solid carbon product. After 8 hours of the process, the feed is stopped and the reactor is cooled under a nitrogen atmosphere. The solid carbon product weighing 2.5 kg is discharged from the reactor. The theoretical purity of the CNTs is about 96 wt%.

[0072] To obtain the physicochemical characteristics of the produced carbon products, the carbon samples are analyzed by ICAP, XRD, TEM, Raman spectroscopy, and TGA.

[0073] [Example 5: Purification process of carbon nanotubes (CNTs)] 2.5 kg of CNTs with carbon purity of 96 wt% produced in Example 4 are placed in a 20 liter stainless steel vessel. CNTs with total metal impurities in the concentration range of 0.45 mol. 100% reagent solution of 0.1 M reagent solution prepared in Example 1 is added to 2.5 kg of CNT powder to make CNT slurry. The CNT slurry thus formed is kept under continuous stirring while the vessel is heated at a temperature of 70 °C for 12 hours. Further, the vessel is cooled by turning off the heater and the slurry solution is left to stand for some time to allow the solid mass to settle to the bottom, and then the excess solution is decanted. The wet solid CNT sample is washed with water under vacuum and dried in an oven at 100 °C for 12 hours. The obtained CNT material is ground into powder and analyzed by ICAP, TGA, XRD, Raman, TEM / SEM characterization methods.

[0074] [Example 6: Manufacturing process of carbon nanotubes (CNTs) for Ni-Mn catalyst] 100 g of 20 wt% nickel and 22 wt% manganese oxide supported on MgO catalyst is loaded into a vertical fluidized bed reactor, and then the reactor is heated to a temperature of 650 °C under an inert atmosphere. After reaching the desired temperature, hydrogen is passed over the catalyst along with nitrogen gas to reduce the metal oxide catalyst for 2 hours. After the reduction step is completed, the hydrogen gas is turned off and nitrogen gas is passed continuously over the catalyst. The petroleum hydrocarbon feed is fed into the reactor at a flow rate of 400 gm per hour using a continuous high pressure distribution pump. The liquid feed is preheated to 400 °C and the feed steam is conveyed to the reactor with the assistance of nitrogen gas. The feed steam and nitrogen gas are admitted into the reactor, where the feed steam is passed over the catalyst surface, so that the feed starts to decompose and form a solid carbon product. After 8 hours of the process, the feed is stopped and the reactor is cooled under a nitrogen atmosphere. The solid carbon product is discharged from the reactor and the weight of the product is 2 kg. The theoretical purity of the CNTs is about 95 wt%. The obtained CNTs are analyzed by ICAP, TGA, XRD, Raman, and TEM / SEM characterization methods.

[0075] [Example 7: Purification process of carbon nanotubes (CNTs)] 2 kg of CNTs with carbon purity of 95 wt% produced in Example 6 are placed in a 20 liter stainless steel vessel. CNTs with total metal impurities in the concentration range of 0.45 mol. 100% reagent solution of 0.1 M reagent solution prepared in Example 1 is added to 2 kg of CNT powder to make a CNT slurry. The CNT slurry thus formed is kept under continuous stirring while the vessel is heated at a temperature of 70°C for 12 hours. Thereafter, the heater is turned off to cool the vessel and the slurry solution is left to stand for some time to allow the solid mass to settle to the bottom, and then the excess solution is decanted. The decanted solution is analyzed by ICAP for metal analysis. The wet solid CNT sample is washed with water under vacuum and dried in an oven at 100°C for 12 hours. The obtained CNT material is ground into powder and analyzed by ICAP, TGA, XRD, Raman, TEM / SEM characterization methods. [Table 1]

[0076] Thus, from Table 1, it can be seen that CNT purification examples 3, 5, and 7 have lower metal contents compared to their counterparts examples 2, 4, and 6, which are pristine CNTs and have higher metal contents.

[0077] (Additional Note) (Appendix 1) A non-mineral acid based reagent solution for the purification of carbon nanomaterials, comprising: (a) a solid reagent selected from the group consisting of sodium persulfate, potassium persulfate, ammonium persulfate, and mixtures thereof; (b) deionized water; Including, The solid reagent is dissolved in the deionized water in a molar ratio ranging from 0.01 to 1; The carbon nanomaterial has a bulk density in the range of 0.01 to 0.2 g / cc; The carbon nanomaterial, with or without heteroatoms, is associated with a transition metal in the form of a metal carbide and is encapsulated or intercalated with a support metal oxide; A solution characterized in that

[0078] (Appendix 2) 2. The solution of claim 1, wherein the solid reagent is a non-mineral and acid-based solid reagent that is a non-mineral acid compound.

[0079] (Appendix 3) The solution of claim 1, wherein the carbon nanomaterial includes single-layered or double-layered or triple-layered or thin-layered carbon nanomaterial, multi-layered carbon nanomaterial, carbon nanofiber, carbon nanoring, etc.

[0080] (Appendix 4) A method for purifying a carbon nanomaterial using the non-mineral acid reagent solution according to claim 1, (a) mixing a reagent solution with an initial carbon nanomaterial to form a carbon nanomaterial slurry; (b) gradually heating the carbon nanomaterial slurry from room temperature to a temperature of 70-100° C. over a period of 4-12 hours while stirring; (c) filtering the carbon nanomaterial slurry under vacuum followed by washing with deionized water to obtain a purified carbon nanomaterial cake; (d) drying the purified carbon nanomaterial cake in a hot air oven at 120°C for 12 hours to obtain a carbon nanomaterial having a purity of more than 99-99.5% by weight; The process includes: Purification method.

[0081] (Appendix 5) 5. The purification method according to claim 4, wherein the concentration of the reagent solution is in the range of 1 to 50% by weight relative to the weight of the initial carbon nanomaterial.

[0082] (Appendix 6) 5. The purification method of claim 4, wherein the initial carbon nanomaterial comprises metal impurities present in the range of 1-15 wt.%.

[0083] (Appendix 7) 7. The method of claim 6, wherein the metal impurities are in monometallic, bimetallic, trimetallic or polymetallic form including iron, cobalt, nickel, manganese or molybdenum, and the metals are dispersed on a support material such as magnesium oxide, alumina, silica, or combinations thereof.

[0084] (Appendix 8) 5. The purification method according to claim 4, wherein the purity of the initial carbon nanomaterial is in the range of 85 to 99% by weight.

[0085] (Appendix 9) 9. The purification method according to any one of claims 4 to 8, wherein the ratio of the reagent solution to the metal impurities in the initial carbon nanomaterial is in the range of 0.1 to 1.

Claims

1. A non-mineral acid based reagent solution for the purification of carbon nanomaterials, comprising: (a) a solid reagent selected from the group consisting of sodium persulfate, potassium persulfate, ammonium persulfate, and mixtures thereof; (b) deionized water; Including, The solid reagent is dissolved in the deionized water at a molar ratio ranging from 0.05 to 1 mol / L; The carbon nanomaterial has a bulk density in the range of 0.01 to 0.2 g / cc; The carbon nanomaterial, with or without heteroatoms, is associated with a transition metal in the form of a metal carbide and is encapsulated or intercalated with a support metal oxide; A solution characterized in that

2. 2. The solution of claim 1, wherein the solid reagent is a non-mineral and acid-based solid reagent that is a non-mineral acid compound.

3. 2. The solution of claim 1, wherein the carbon nanomaterials include single-walled or double-walled or triple-walled or thin-walled carbon nanomaterials, multi-walled carbon nanomaterials, carbon nanofibers, carbon nanorings, and the like.

4. A method for purifying a carbon nanomaterial using the non-mineral acid reagent solution according to claim 1, (a) mixing a reagent solution with an initial carbon nanomaterial to form a carbon nanomaterial slurry; (b) gradually heating the carbon nanomaterial slurry from room temperature to a temperature of 70-100° C. over a period of 4-12 hours while stirring; (c) filtering the carbon nanomaterial slurry under vacuum followed by washing with deionized water to obtain a purified carbon nanomaterial cake; (d) drying the purified carbon nanomaterial cake in a hot air oven at 120°C for 12 hours to obtain a carbon nanomaterial with a purity of 99-99.5% by weight or more; The process includes: Purification method.

5. The purification method according to claim 4, wherein the concentration of the reagent solution is in the range of 1 to 50% by weight relative to the weight of the initial carbon nanomaterial.

6. 5. The purification method of claim 4, wherein the initial carbon nanomaterial contains metal impurities present in the range of 1-15 wt.%.

7. 7. The purification method of claim 6, wherein the metal impurities are in monometallic or bimetallic or trimetallic or polymetallic form including iron, cobalt, nickel, manganese or molybdenum, and the metals are dispersed on a support material such as magnesium oxide, alumina, silica, or combinations thereof.

8. 5. The purification method of claim 4, wherein the purity of the initial carbon nanomaterial is in the range of 85-99 wt.%.

9. The purification method according to any one of claims 4 to 8, wherein the ratio of the reagent solution to the metal impurities in the initial carbon nanomaterial is in the range of 0.1 to 1.

Citation Information

Patent Citations

  • Method for manufacturing mono-layer carbon nano pipe

    CN101164872A

  • Vacuum high-temperature process of purifying carbon nanotube

    CN1436722A

  • Method for removing cobalt,nickel or (and) iron in nm-class carbon tubes

    CN1485271A

  • Mass purification method of carbon nanotubes

    EP1061040A1

  • Electrophotography

    JP1977028323A