Film forming apparatus and film forming method

The susceptor design with a recessed portion and purge gas supply system addresses film deposition on substrate edges, improving productivity and reducing maintenance by preventing gas contact, thus enhancing substrate processing efficiency.

JP7586599B2Active Publication Date: 2024-11-19TOKYO ELECTRON LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021003756
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-01-13
Publication Date
2024-11-19
Estimated Expiration
2041-01-13

AI Technical Summary

Technical Problem

Existing substrate processing apparatuses face challenges in suppressing film formation on the back end of substrates due to the design of the susceptor, which leads to film deposition on the edges and warping, resulting in particle generation and reduced productivity.

Method used

The apparatus incorporates a susceptor with a recessed portion supporting the center of the substrate and a groove around it, along with a porous ring and purge gas supply to the groove, preventing film deposition on the back end of the substrate by suppressing gas contact with the edge and inner surfaces.

Benefits of technology

This design effectively suppresses film formation on the substrate edges, reduces particle generation, enhances productivity by minimizing etching and maintenance cycles, and extends the lifespan of the susceptor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007586599000001
    Figure 0007586599000001
  • Figure 0007586599000002
    Figure 0007586599000002
  • Figure 0007586599000003
    Figure 0007586599000003
Patent Text Reader

Abstract

To provide a technique capable of suppressing film formation on the back surface edge of a substrate.SOLUTION: A film forming device according to an embodiment of the present disclosure includes a processing container, a susceptor provided in the processing container and having a recessed portion on the surface, in which the recessed portion includes a support portion that supports a region that includes the center of the substrate and does not include the edge portion, and a groove portion that is located around the support portion and is recessed from the support portion, a processing gas supply portion that supplies processing gas to the surface of the susceptor, and a purge gas supply portion that supplies purge gas to the groove portion.SELECTED DRAWING: Figure 8
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a film forming apparatus and a film forming method. [Background technology]

[0002] In a substrate processing apparatus that processes a wafer placed on a susceptor while revolving the wafer in a processing chamber and supplying a processing gas to the wafer, a configuration is known in which a recess for placing the wafer is provided on the surface of the susceptor (see, for example, Patent Document 1). In this substrate processing apparatus, a mounting table for supporting the center of the wafer from below is provided in the recess, and the peripheral edge of the wafer is raised above the bottom surface of the recess. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2013-222948 A Summary of the Invention [Problem to be solved by the invention]

[0004] The present disclosure provides a technique capable of suppressing film formation on the edge portion of the back surface of a substrate. [Means for solving the problem]

[0005] A film forming apparatus according to one aspect of the present disclosure includes a processing vessel, a susceptor provided within the processing vessel and having a recess on a surface thereof, the recess including a support portion supporting an area including a center of a substrate but not including an edge of the substrate, and a groove portion located around the support portion and recessed further than the support portion, a processing gas supply portion supplying a processing gas to a surface of the susceptor, and a purge gas supply portion supplying a purge gas to the groove portion; a porous ring provided around the support and between the rear surface of the substrate supported by the support and the bottom surface of the groove; Equipped with The inner surface of the porous ring is in contact with the outer wall surface of the support portion. . Effect of the Invention

[0006] According to the present disclosure, film formation on the edge portion of the back surface of the substrate can be suppressed. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a cross-sectional view showing an example of a film forming apparatus according to an embodiment. [Diagram 2] A cross-sectional plan view of the film forming apparatus of FIG. [Diagram 3] A cross-sectional plan view of the film forming apparatus of FIG. [Figure 4] FIG. 2 is a perspective view showing a part of the inside of the film forming apparatus of FIG. [Diagram 5] FIG. 2 is a plan view showing an example of a susceptor of the film forming apparatus of FIG. [Figure 6] FIG. 6 is an enlarged view of a recess in the susceptor of FIG. 5. [Figure 7] FIG. 7 is a cross-sectional view taken along dashed line IIV-IIV in FIG. 6. [Figure 8] Enlarged view of area A1 in Figure 7. [Figure 9] Enlarged view of area A2 in Figure 7. [Figure 10] Cross-sectional view showing the operation of a conventional susceptor [Figure 11] Cross-sectional view showing the operation of a conventional susceptor [Figure 12] Cross-sectional view showing the operation of a conventional susceptor [Figure 13] Cross-sectional view showing the operation of a conventional susceptor [Figure 14] FIG. 1 is a diagram for explaining deposition of a film on a wafer when a conventional susceptor is used. [Figure 15] FIG. 2 is a cross-sectional view showing another example of a susceptor of the film forming apparatus of FIG. [Figure 16] 1 is a flowchart showing an example of a film forming method according to an embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, non-limiting exemplary embodiments of the present disclosure will be described with reference to the accompanying drawings. In all of the accompanying drawings, the same or corresponding members or parts are designated by the same or corresponding reference numerals, and duplicated descriptions will be omitted.

[0009] [Film forming equipment] An example of a film forming apparatus according to an embodiment will be described with reference to Figures 1 to 4. The film forming apparatus according to the embodiment includes a processing vessel 1 having a generally circular planar shape, and a susceptor 2 that is provided in the processing vessel 1 and has a rotation center at the center of the processing vessel 1, and is configured as an apparatus for performing a film forming process on a substrate (e.g., a wafer W). Each part of the film forming apparatus will be described below.

[0010] The processing vessel 1 is a vacuum vessel whose interior can be depressurized. The processing vessel 1 has a top plate 11 and a vessel body 12. The top plate 11 is detachably attached to the vessel body 12 via a seal member 13. A separation gas supply pipe 51 is provided in the center of the upper surface of the top plate 11. The separation gas supply pipe 51 supplies nitrogen (N2) gas as a separation gas to prevent different processing gases from mixing with each other in a central region C of the processing vessel 1.

[0011] A heater unit 7 is provided above the bottom 14 of the processing vessel 1 (FIG. 1). The heater unit 7 heats the wafer W on the susceptor 2 to a film formation temperature (e.g., 300° C.) via the susceptor 2. A cover member 71a is provided on the side of the heater unit 7, and a cover member 7a that covers the heater unit 7 is provided above the heater unit 7. Purge gas supply pipes 73 for purging the arrangement space of the heater unit 7 are provided at multiple locations around the circumferential direction of the bottom 14 below the heater unit 7.

[0012] The susceptor 2 is fixed at its center to a core portion 21 having a generally cylindrical shape. The susceptor 2 is configured to be rotatable about a vertical axis, in this example, clockwise, by a rotating shaft 22 connected to the lower surface of the core portion 21 and extending in the vertical direction. The rotating shaft 22 is rotated about the vertical axis by a driving portion 23. The rotating shaft 22 and the driving portion 23 are housed in a case body 20. The upper flange portion of the case body 20 is airtightly attached to the lower surface of the bottom portion 14 of the processing vessel 1. In addition, a purge gas supply pipe 72 is connected to the case body 20 for supplying N2 gas as a purge gas to a region below the susceptor 2. The outer periphery of the core portion 21 at the bottom portion 14 of the processing vessel 1 is formed in an annular shape so as to approach the susceptor 2 from below, forming a protruding portion 12a.

[0013] A recess 24 is provided on the surface of the susceptor 2. The recess 24 has a circular shape in a plan view, and the wafer W is dropped and held therein. The wafer W may be, for example, a disk-shaped (circular) silicon wafer. The recess 24 is formed at a plurality of locations along the rotation direction (circumferential direction) of the susceptor 2. In the example of Figs. 1 to 4, the recess 24 is formed at five locations along the rotation direction (circumferential direction) of the susceptor 2. Each recess 24 is formed to have a larger diameter than the wafer W in a plan view in order to provide a gap area (clearance) between the recess 24 and the outer edge of the wafer W. The diameter of the susceptor 2 is, for example, about 1000 mm. The recess 24 is formed with a through hole 24a through which, for example, three lift pins (not shown) for pushing up the wafer W from below and lifting it up and down are protruding and recessed. Note that in Figs. 2 and 3, the diameter of the recess 24 is shown in a simplified manner. Also, in Figs. 1 to 3, the through hole 24a is not shown.

[0014] At positions facing the passage area of ​​the recess 24, six nozzles 31, 32, 34, 35, 41, 42, each made of, for example, quartz, are radially arranged at intervals in the circumferential direction of the processing vessel 1. Each of the nozzles 31, 32, 34, 35, 41, 42 is attached so as to extend horizontally from the outer wall surface of the processing vessel 1 toward the central area C facing the wafer W. In this example, the plasma generation gas nozzle 34, the separation gas nozzle 41, the cleaning gas nozzle 35, the first processing gas nozzle 31, the separation gas nozzle 42, and the second processing gas nozzle 32 are arranged in this order in the rotation direction of the susceptor 2 as viewed from the transfer port 15 described later. A plasma generation unit 80 is provided above the plasma generation gas nozzle 34 to generate plasma from the gas discharged from the plasma generation gas nozzle 34. The plasma generation unit 80 will be described later.

[0015] The first process gas nozzle 31 and the second process gas nozzle 32 form a first process gas supply unit and a second process gas supply unit, respectively, the separation gas nozzles 41 and 42 form a separation gas supply unit, and the cleaning gas nozzle 35 forms a cleaning gas supply unit. 2 and 4 show a state in which a plasma generating unit 80 and a housing 90, which will be described later, have been removed so that the plasma generating gas nozzle 34 can be seen, and Fig. 3 shows a state in which the plasma generating unit 80 and the housing 90 are attached.

[0016] Each of the nozzles 31, 32, 34, 35, 41, 42 is connected to the following gas supply sources (not shown) via a flow rate control valve. That is, the first process gas nozzle 31 is connected to a supply source of a first process gas containing Si (silicon). The first process gas may be, for example, BTBAS (bisterial butyl amino silane, SiH2(NH-C(CH3)3)2) gas. The second process gas nozzle 32 is connected to a supply source of a second process gas (for example, a mixed gas of ozone (O3) gas and oxygen (O2) gas) (more specifically, an oxygen gas supply source provided with an ozonizer). The plasma generation gas nozzle 34 is connected to a supply source of a plasma generation gas consisting of, for example, a mixed gas of argon (Ar) gas and O2 gas. The separation gas nozzles 41, 42 are each connected to a gas supply source of N2 gas, which is a separation gas. For example, on the lower surface of each of the nozzles 31, 32, 34, 41, 42, a plurality of gas ejection holes (not shown) are formed at equal intervals along the radial direction of the susceptor 2.

[0017] The area below the first process gas nozzle 31 is a first process area P1 for adsorbing the first process gas onto the wafer W. The area below the second process gas nozzle 32 is a second process area P2 for reacting the components of the first process gas adsorbed onto the wafer W with the second process gas. The separation gas nozzles 41 and 42 are each for forming a separation area D for separating the first process area P1 from the second process area P2. As shown in FIG. 2 and FIG. 3, a roughly fan-shaped convex portion 4 is provided on the top plate 11 of the process vessel 1 in the separation area D, and the separation gas nozzles 41 and 42 are accommodated in the convex portion 4. Therefore, on both sides of the separation gas nozzles 41 and 42 in the circumferential direction of the susceptor 2, low ceiling surfaces that are the lower surfaces of the convex portions 4 are arranged to prevent the process gases from mixing with each other, and on both sides of the ceiling surfaces in the circumferential direction, ceiling surfaces higher than the ceiling surfaces are arranged. The peripheral portion of the convex portion 4 (the portion on the outer edge side of the processing vessel 1) is bent in an L shape so as to face the outer end surface of the susceptor 2 and be slightly spaced from the vessel body 12 in order to prevent mixing of the processing gases.

[0018] Next, the plasma generating unit 80 will be described. The plasma generating unit 80 is configured by winding an antenna 83 made of a metal wire in a coil shape, and is arranged so as to straddle the passage area of ​​the wafer W from the center to the periphery of the susceptor 2. The antenna 83 is connected to a high-frequency power source 85 having a frequency of, for example, 13.56 MHz and an output power of, for example, 5000 W via a matching device 84, and is arranged so as to be airtightly separated from the internal area of ​​the processing vessel 1. The plasma generating unit 80, the matching device 84, and the high-frequency power source 85 are electrically connected by a connection electrode 86. That is, the top plate 11 above the plasma generating gas nozzle 34 has an opening that is approximately fan-shaped in a plan view, and is airtightly sealed by a housing 90 made of, for example, quartz. The housing 90 is formed so that the peripheral portion extends horizontally in a flange shape in the circumferential direction and the center portion is recessed toward the internal area of ​​the processing vessel 1, and the antenna 83 is stored inside the housing 90. A seal member 11a is provided between the housing 90 and the top plate 11. The peripheral edge of the housing 90 is pressed downward by a pressing member 91.

[0019] 1, the outer edge of the lower surface of the housing 90 extends vertically downward (toward the susceptor 2) in the circumferential direction to form a gas regulating protrusion 92 in order to prevent the intrusion of N2 gas, O3 gas, and the like into the area below the housing 90. The area surrounded by the inner circumferential surface of the protrusion 92, the lower surface of the housing 90, and the upper surface of the susceptor 2 houses the plasma generating gas nozzle 34.

[0020] Between the housing 90 and the antenna 83, as shown in Figs. 1 and 3, a generally box-shaped Faraday shield 95 with an opening at the top is disposed. The Faraday shield 95 is made of a metal plate, which is a conductive plate-like body, and is grounded. A slit 97 is provided in the bottom surface of the Faraday shield 95, which is formed to extend in a direction perpendicular to the winding direction of the antenna 83, in the circumferential direction below the antenna 83. The slit 97 prevents the electric field component of the electric field and magnetic field (electromagnetic field) generated in the antenna 83 from heading toward the wafer W below, and allows the magnetic field to reach the wafer W. An insulating plate 94 is interposed between the Faraday shield 95 and the antenna 83. The insulating plate 94 is made of, for example, quartz, and insulates the Faraday shield 95 from the antenna 83.

[0021] An annular side ring 100 is disposed at a position slightly lower than the susceptor 2 on the outer periphery side of the susceptor 2. Exhaust ports 61, 62 are formed at two locations on the upper surface of the side ring 100 so as to be spaced apart from each other in the circumferential direction. In other words, two exhaust ports are formed in the bottom 14 of the processing vessel 1, and the exhaust ports 61, 62 are formed in the side ring 100 at positions corresponding to these exhaust ports. The exhaust port 61 is formed at a position closer to the separation region D between the first processing gas nozzle 31 and the separation region D downstream of the first processing gas nozzle 31 in the rotation direction of the susceptor. The exhaust port 62 is formed at a position closer to the separation region D between the plasma generation gas nozzle 34 and the separation region D downstream of the plasma generation gas nozzle 34 in the rotation direction of the susceptor.

[0022] The exhaust port 61 is for exhausting the first processing gas and separation gas, and the exhaust port 62 is for exhausting the plasma generating gas in addition to the second processing gas and separation gas. During cleaning, a cleaning gas is exhausted. A groove-shaped gas flow path 101 is formed on the upper surface of the side ring 100 on the outer edge side of the housing 90 to allow gas to flow to the exhaust port 62 while avoiding the housing 90. As shown in FIG. 1, the exhaust ports 61 and 62 are connected to a vacuum pump 64, which is a vacuum exhaust mechanism, by an exhaust pipe 63 in which a pressure adjustment unit 65 such as a butterfly valve is interposed.

[0023] 2, a protrusion 5 is provided in the center of the lower surface of the top plate 11, which is formed in a generally annular shape in the circumferential direction, continuous with a portion of the convex portion 4 on the central region C side, and whose lower surface is formed at the same height as the lower surface of the convex portion 4. A labyrinth structure 110 is disposed above the core portion 21 on the side of the rotation center of the susceptor 2 closer to the protrusion 5 than the protrusion 5, for suppressing the first process gas and the second process gas from mixing with each other in the central region C. The labyrinth structure 110 has a configuration in which a first wall portion 111 extending vertically in the circumferential direction from the susceptor 2 side toward the top plate 11 side and a second wall portion 112 extending vertically in the circumferential direction from the top plate 11 side toward the susceptor 2 are alternately disposed in the radial direction of the susceptor 2.

[0024] 2 and 3, a transfer port 15 is formed in the side wall of the processing vessel 1 for transferring the wafer W between an external transfer arm (not shown) and the susceptor 2. The transfer port 15 is airtightly opened and closed by a gate valve G. Lifting pins (not shown) are provided below the susceptor 2 at a position facing the transfer port 15. The lifting pins lift the wafer W from the backside through through holes 24a of the susceptor 2.

[0025] The film forming apparatus is provided with a control unit 120 consisting of a computer for controlling the operation of the entire apparatus. A program for performing a film forming method described below is stored in the memory of the control unit 120. The program is composed of steps for executing the operation of the apparatus described below, and is installed in the control unit 120 from a storage unit 121 which is a storage medium such as a hard disk, a compact disk, a magneto-optical disk, a memory card, or a flexible disk.

[0026] [Susceptor Structure] An example of the susceptor 2 of the film forming apparatus of the embodiment will be described with reference to FIGS.

[0027] The susceptor 2 is made of, for example, quartz. As described above, the center of the susceptor 2 is fixed to the roughly cylindrical core portion 21. The susceptor 2 is configured to be rotatable about a vertical axis, in this example, clockwise, by a rotation shaft 22 that is connected to the lower surface of the core portion 21 and extends in the vertical direction (FIGS. 1 to 4).

[0028] The susceptor 2 includes a recess 24 , a support portion 25 , a groove portion 26 , a porous ring 27 , a purge gas supply portion 28 and a circular protrusion 29 .

[0029] The recesses 24 are formed at multiple locations (six locations in FIG. 5) along the rotation direction (circumferential direction) of the susceptor 2. Each recess 24 has a circular shape. Each recess 24 is formed to have a larger diameter than the wafer W in a plan view in order to provide a gap region (clearance) between the outer edge of the wafer W. In one embodiment, the diameter r of the wafer is 300 mm, and the diameter R of the recess is 302 mm.

[0030] The support portion 25 is provided on the bottom surface of each recess 24. The support portion 25 supports the center portion of the wafer W from below. The support portion 25 is configured to have a cylindrical shape, and the upper surface is formed as a horizontal surface. The support portion 25 is formed to have a circular shape smaller than the wafer W in a plan view so that the peripheral portion of the wafer W is raised from the bottom surface of the recess 24 in the circumferential direction, i.e., so that the peripheral portion does not touch the support portion 25 (protrudes from the support portion 25). Therefore, the support portion 25 is formed so that when the wafer W is placed on the support portion 25, the peripheral portion of the wafer W faces the bottom surface of the recess 24 in the circumferential direction.

[0031] The height dimension h of the support portion 25 is set so that, for example, when the wafer W is placed on the support portion 25, the surface of the wafer W is aligned with the surface of the susceptor 2. In one embodiment, the height dimension h of the support portion 25 is about 0.03 mm to 0.2 mm, and the diameter dimension d of the support portion 25 is 297 mm.

[0032] The groove portion 26 is formed around the support portion 25, more specifically, between the inner wall surface of the recess 24 and the outer wall surface of the support portion 25. The groove portion 26 has an annular shape. The support portion 25 is disposed at the center of the recess 24 in a plan view. That is, the center position of the support portion 25 coincides with the center position of the recess 24 in a plan view. As a result, the width dimension L of the groove portion 26 is constant in the circumferential direction in a plan view. In one embodiment, the width dimension L of the groove portion 26 is 2.5 mm.

[0033] The porous ring 27 is disposed at the peripheral portion of the support portion 25, between the rear surface of the wafer W supported by the support portion 25 and the bottom surface of the groove portion 26. The porous ring 27 has an annular shape. In one embodiment, the porous ring 27 is disposed such that its inner edge portion is on a step portion 25a formed on the outer wall surface of the support portion 25, with a gap V between the porous ring 27 and the inner wall surface of the recess 24. The porous ring 27 is formed of a porous material such as SiC or SiN.

[0034] The purge gas supply unit 28 supplies the purge gas to the grooves 26. In one embodiment, the purge gas supply unit 28 includes gas flow paths extending radially from the central region C in the processing vessel 1 to the grooves 26 formed in each recess 24 (FIG. 5). The purge gas supply unit 28 may be a flow path that guides the separation gas supplied to the central region C in the processing vessel 1 from the separation gas supply pipe 51 to the grooves 26 formed in each recess 24. The purge gas supplied to the grooves 26 is supplied to the rear surface of the wafer W through the porous ring 27. This allows the flow rate of the purge gas to be reduced and the purge gas to be supplied widely and evenly, thereby preventing the wafer W from floating due to the purge gas. The purge gas supply unit 28 supplies the purge gas to the grooves 26 when the processing gas is supplied to the front surface of the susceptor 2 with the wafer W placed on the support 25, for example. The purge gas supplied to the groove 26 suppresses the contact of the processing gas with the back edge of the wafer W, the inner wall surface of the groove 26, the bottom surface of the groove 26, and the like. Therefore, deposition of a film on the back edge of the wafer W, the inner wall surface of the groove 26, the bottom surface of the groove 26, and the like is suppressed. As a result, particles generated in the groove 26 due to accumulation of deposited films can be reduced, and the yield is improved. In addition, since deposition of a film on the back edge of the wafer W can be suppressed, the time of the process of etching and removing the film deposited on the back edge of the wafer W can be shortened or omitted, and the productivity is improved. In addition, since deposition of a film on the groove 26 can be suppressed, the time of dry cleaning for removing the film deposited on the susceptor 2 can be shortened, and the time of exposure of the susceptor 2 to the etching gas can be shortened, and the life of the susceptor 2 can be extended. As a result, the cost associated with replacing the susceptor 2 can be reduced. In addition, the maintenance cycle can be extended, and the productivity is improved.

[0035] In one embodiment, the purge gas supply unit 28 starts supplying the purge gas to the groove 26 before starting the supply of the processing gas to the surface of the susceptor 2, and stops supplying the purge gas to the groove 26 after stopping the supply of the processing gas to the surface of the susceptor 2. The purge gas supply unit 28 may be formed, for example, by drilling a hole inside the susceptor 2, or by providing a groove on the surface of the susceptor 2.

[0036] The annular protrusion 29 is provided along the groove 26. The annular protrusion 29 has an annular shape in a plan view and protrudes from the bottom surface of the groove 26. In one embodiment, the annular protrusion 29 has a height 29h that is lower than a height 27h of the lower surface of the porous ring 27 relative to the bottom surface of the groove 26. The annular protrusion 29 distributes the purge gas supplied from the purge gas supply unit 28 from the inner wall surface side of the recess 24 toward the outer wall surface side of the support part 25 in the circumferential direction of the groove 26. As a result, the purge gas supplied from the purge gas supply unit 28 to the groove 26 is uniformly supplied around the entire circumference of the rear surface of the wafer W.

[0037] 10 to 14, the reasons for forming groove 26 between the inner wall surface of recess 24 and the outer wall surface of support portion 25 and providing purge gas supply portion 28 for supplying purge gas to groove 26 will be described.

[0038] First, a case where the wafer W is directly placed on the bottom surface of the recess 24 without providing the support 25 will be described. When the unprocessed wafer W is at room temperature before being placed on the susceptor 2, when the wafer W is placed on the susceptor 2, temperature variations occur within the surface, and then the temperature rises toward the film formation temperature, and the temperature variations become smaller. On the other hand, when the wafer W has already been subjected to another heat treatment in a heat treatment device other than the film formation device, the wafer W naturally dissipates heat during the transfer to the film formation device, and the temperature drop rate at this time becomes non-uniform within the surface of the wafer W. Therefore, when the wafer W has been subjected to a heat treatment in advance, the wafer W already has temperature variations when placed on the susceptor 2, and then the temperature variations gradually become smaller due to the heat input from the susceptor 2.

[0039] Therefore, when an unprocessed wafer W is placed on the susceptor 2, even if it is at room temperature or has already been heat-treated, temperature variations occur within the surface. At this time, the wafer W may be warped in a mountain shape (upwardly convex) based on the temperature variations of the wafer W. When the wafer W is warped in a mountain shape, the center of the wafer W is separated from the surface of the susceptor 2 and the peripheral portion of the wafer W comes into contact with the susceptor 2. As shown in FIG. 10, if the wafer W warped in a mountain shape is placed directly on the bottom surface of the recess 24, the peripheral portion of the wafer W and the surface of the susceptor 2 (more specifically, the bottom surface of the recess 24) rub against each other when the wafer W is flattened as the temperature of the wafer W is uniformed. As a result, particles P are generated. As shown in FIG. 11, the particles P go around the peripheral portion of the wafer W and adhere to the surface of the wafer W when the wafer W is fully horizontally stretched. Therefore, in order to reduce the number of particles P adhering to the surface of the wafer W as much as possible, it is not preferable to place the wafer W directly on the bottom surface of the recess 24.

[0040] Therefore, as shown in FIG. 12 and FIG. 13, by providing a support 25 on the bottom surface of the recess 24, the peripheral portion of the wafer W does not contact the bottom surface of the recess 24, and the number of particles adhering to the front surface of the wafer W can be reduced. In this case, when a processing gas is supplied to the wafer W to perform a film forming process, a part of the processing gas supplied to the peripheral portion of the wafer W passes between the peripheral portion of the wafer W and the inner wall surface of the recess 24 and flows around to the back side of the wafer W, and a film may be deposited on the back end of the wafer W. The film thickness of the film deposited on the back end of the wafer W can be equal to or greater than the film thickness of the film deposited on the front surface of the wafer W, as shown in FIG. 14, for example. When the film thickness of the film deposited on the back end of the wafer W becomes thick, the film peels off and particles are generated. In FIG. 14, the horizontal axis indicates the radial position of the wafer W with a diameter dimension r of 300 mm, and the vertical axis indicates the film thickness of the film deposited on the back surface of the wafer W when the film thickness of the film deposited on the front surface of the wafer W is set to 1.

[0041] Therefore, in the embodiment, an annular groove 26 is formed between the inner wall surface of the recess 24 and the outer wall surface of the support 25, and a purge gas supply unit 28 is provided to supply a purge gas to the groove 26. This allows the purge gas to be supplied to the groove 26 when the processing gas is supplied to the surface of the susceptor 2 with the wafer W placed on the support 25. The purge gas supplied to the groove 26 prevents the processing gas from contacting the back end of the wafer W, the inner wall surface of the groove 26, the bottom surface of the groove 26, and the like. Therefore, deposition of a film on the back end of the wafer W, the inner wall surface of the groove 26, the bottom surface of the groove 26, and the like is suppressed. In this way, in the embodiment, generation of particles P due to rubbing between the peripheral portion of the wafer W and the surface of the susceptor 2 can be suppressed, and deposition of a film on the back end of the wafer W, the inner wall surface of the groove 26, the bottom surface of the groove 26, and the like can be suppressed.

[0042] [Modifications of susceptor structure] Another example of the susceptor of the film forming apparatus of the embodiment will be described with reference to Fig. 15. The susceptor 2A shown in Fig. 15 is different from the susceptor 2 described above in that it includes a porous portion 25b that communicates from the front surface to the back surface in a region including the support portion 25. Other configurations may be the same as those of the susceptor 2 described above.

[0043] The porous portion 25b communicates from the front surface to the back surface in a region including the support portion 25. The porous portion 25b is formed, for example, to have a smaller diameter than the wafer W in a plan view. The porous portion 25b may be fixed to the susceptor 2, or may be detachable from the susceptor 2. When the porous portion 25b is detachable from the susceptor 2, the porous portion 25b may be configured to be rotatable with respect to the susceptor 2. The porous portion 25b is formed, for example, from the same material as the porous ring 27, such as SiC or SiN.

[0044] In this manner, by providing the porous portion 25b in the region including the supporting portion 25, when the wafer W is placed on the supporting portion 25, the purge gas that enters between the upper surface of the supporting portion 25 and the rear surface of the wafer W can be discharged below the susceptor 2A through the porous portion 25b. This makes it possible to suppress misalignment of the wafer W when it is placed on the supporting portion 25.

[0045] [Film formation method] An example of a film forming method according to an embodiment will be described with reference to Fig. 16. In the following, a case where a silicon oxide film (SiO2 film) is formed on a wafer W in the above-mentioned film forming apparatus will be described as an example. Note that the susceptor 2 is assumed to have already been heated by the heater unit 7 so that the wafer W placed on the susceptor 2 is at a film forming temperature (e.g., about 300°C).

[0046] First, wafers W are loaded into the processing chamber 1 (step S1). In one embodiment, the gate valve G is opened, and while the susceptor 2 is being rotated intermittently, for example, five wafers W are placed on the susceptor 2 via the transfer port 15 by a transfer arm (not shown). These wafers W are placed at the center positions of the recesses 24, and are therefore arranged so as to be spaced apart (not in contact) from the inner wall surface of the recesses 24 in the circumferential direction. At this time, each wafer W is at room temperature or has already been subjected to another heat treatment, and when placed on the susceptor 2, the wafers W may be warped in a mountain shape due to temperature variations within the surface of the wafer W, as shown in FIG.

[0047] Next, the gate valve G is closed, the inside of the processing chamber 1 is evacuated by the vacuum pump 64, and the susceptor 2 is rotated clockwise at, for example, 2 rpm to 240 rpm. At this time, since the groove 26 is formed in the recess 24, even if the wafer W is warped in a mountain shape, the peripheral portion of the wafer W is separated from the surface of the susceptor 2 and the surface of the support portion 25, so that generation of particles due to sliding between the peripheral portion and the support portion 25 is suppressed.

[0048] Next, the supply of purge gas to the groove 26 is started (step S2). In one embodiment, N2 gas is discharged from the separation gas supply pipe 51 at a predetermined flow rate, and the N2 gas is supplied to the groove 26 via the purge gas supply unit 28 as a purge gas.

[0049] Next, supply of the processing gas to the surface of the susceptor 2 is started (step S3). In one embodiment, the first processing gas and the second processing gas are discharged from the first processing gas nozzle 31 and the second processing gas nozzle 32, respectively, and the plasma generation gas is discharged from the plasma generation gas nozzle 34. Furthermore, the separation gas is discharged from the separation gas nozzles 41 and 42 at a predetermined flow rate, and N2 gas is also discharged from the separation gas supply pipe 51 and the purge gas supply pipes 72 and 72 at a predetermined flow rate. Then, the pressure adjustment unit 65 adjusts the inside of the processing vessel 1 to a preset processing pressure, and high frequency power is supplied to the plasma generation unit 80.

[0050] At this time, each process gas supplied to the wafer W tries to flow into the back side region of the wafer W through the gap between the peripheral edge of the wafer W and the inner peripheral surface of the recess 24, but since the purge gas is supplied to the groove 26, the process gas is prevented from flowing into the groove 26. This prevents deposition of a film on the end of the back side of the wafer W, the inner wall surface of the groove 26, the bottom surface of the groove 26, etc.

[0051] The first process gas is adsorbed on the surface of the wafer W in the first process region P1 due to the rotation of the susceptor 2, and then the first process gas adsorbed on the wafer W reacts with the second process gas in the second process region P2. As a result, one or more molecular layers of a silicon oxide film, which is a thin film component, are formed on the surface of the wafer W, forming a reaction product. At this time, the reaction product may contain impurities such as moisture (OH groups) and organic matter due to residual groups contained in the first process gas.

[0052] Meanwhile, below the plasma generating unit 80, the electric field of the electric field and the magnetic field generated by the high frequency power supplied from the high frequency power supply 85 is reflected or absorbed (attenuated) by the Faraday shield 95, and is prevented (blocked) from reaching the inside of the processing vessel 1. The magnetic field passes through the slits 97 of the Faraday shield 95 and reaches the inside of the processing vessel 1 through the bottom surface of the housing 90. Therefore, the plasma generating gas discharged from the plasma generating gas nozzle 34 is activated by the magnetic field passing through the slits 97, and plasma such as ions and radicals is generated.

[0053] Then, when the plasma (active species) generated by the magnetic field comes into contact with the surface of the wafer W, a modification process of the reaction products is performed. Specifically, for example, the plasma collides with the surface of the wafer W, which causes, for example, the impurities to be released from the reaction products, or the elements in the reaction products to be rearranged and densified (high density). By continuing to rotate the susceptor 2 in this manner, the adsorption of the first process gas onto the surface of the wafer W, the reaction of the components of the first process gas adsorbed onto the surface of the wafer W, and the plasma modification of the reaction products are performed many times in this order, and the reaction products are layered to form a thin film.

[0054] In addition, since N2 gas is supplied between the first processing region P1 and the second processing region P2, the first processing gas, the second processing gas, and the plasma generating gas are exhausted so as not to be mixed with each other. Furthermore, since a purge gas is supplied to the lower side of the susceptor 2, the gas that tends to diffuse to the lower side of the susceptor 2 is pushed back toward the exhaust ports 61 and 62 by the purge gas.

[0055] After the film formation process is completed, the supply of the process gas to the surface of the susceptor 2 is stopped (step S4). In one embodiment, the supply of gas from each of the nozzles 31, 32, 34, 41, and 42 is stopped.

[0056] After the supply of the process gas to the surface of the susceptor 2 is stopped, the supply of the purge gas to the groove 26 is stopped (step S5). In one embodiment, the supply of N2 gas from the purge gas supply unit 28 to the groove 26 is stopped.

[0057] Next, the wafers W are unloaded (step S6). In one embodiment, the rotation of the susceptor 2 is stopped. Then, the susceptor 2 is rotated intermittently to unload the wafers W one by one from the transfer port 15. When all the wafers W have been unloaded, one run (one rotation of film formation process) is completed.

[0058] The embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The above-described embodiments may be omitted, substituted, or modified in various forms without departing from the scope and spirit of the appended claims. [Explanation of symbols]

[0059] 1 Processing vessel 2 Susceptor 24 Recess 25 Support part 26 Groove 31 First processing gas nozzle 32 Second processing gas nozzle 28 Purge gas supply section W wafer

Claims

1. A processing vessel; a susceptor provided in the processing chamber and having a recess on a surface thereof, the recess including a support portion supporting an area including a center of a substrate and not including an edge of the substrate, and a groove portion located around the support portion and recessed from the support portion; a processing gas supply unit that supplies a processing gas to a surface of the susceptor; a purge gas supply unit that supplies a purge gas to the groove; a porous ring provided around the support and between the rear surface of the substrate supported by the support and the bottom surface of the groove; Equipped with The inner surface of the porous ring contacts the outer wall surface of the support portion. Film deposition equipment.

2. The porous ring is provided so as to form a gap between the porous ring and an inner wall surface of the recess. The film forming apparatus according to claim 1 .

3. The purge gas supply unit supplies the purge gas between a bottom surface of the groove and a back surface of the porous ring. The film forming apparatus according to claim 1 or 2.

4. The porous ring is made of SiC. The film forming apparatus according to claim 1 .

5. The recess is provided along the groove and further includes a protrusion protruding from a bottom surface of the groove. The film forming apparatus according to claim 1 .

6. The susceptor includes a porous portion that communicates from the front surface to the back surface in a region including the support portion. The film forming apparatus according to claim 1 .

7. The substrate has a disk shape, The recess has a circular shape having a diameter larger than that of the substrate. The film forming apparatus according to claim 1 .

8. A film formation method for processing a substrate in a film formation apparatus including a susceptor, the susceptor being provided in a processing chamber and having a recess on a surface thereof, the recess including a support portion supporting an area including a center of the substrate but not including an edge of the substrate, and a groove portion located around the support portion and recessed below the support portion, the method comprising the steps of: the film forming apparatus includes a porous ring provided around the support portion and between a rear surface of the substrate supported by the support portion and a bottom surface of the groove portion; The inner surface of the porous ring is in contact with the outer wall surface of the support portion, The film forming method includes: starting a supply of a purge gas to the groove portion while the substrate is supported by the support portion; supplying a process gas to a surface of the susceptor while supplying the purge gas to the groove; stopping the supply of the process gas; stopping the supply of the purge gas after stopping the supply of the process gas; The film forming method includes the steps of:

Citation Information

Patent Citations

  • Cvd deposition apparatus and cvd deposition method

    JP1999036076A

  • Fabrication apparatus and fabrication method of semiconductor device

    JP2009071122A

  • Substrate processing device

    JP2013222948A

  • Deposition device

    JP2015228404A

  • Atomic layer growth device

    JP2016225325A