Coating device, coating method, and metal strip manufacturing equipment
The coating device uses an air pad to form a static pressure region, addressing warping and vibration issues in roll coaters, ensuring uniform coating application and defect-free metal strip surfaces.
Patent Information
- Application Number
- JP2021087805
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-05-25
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2041-05-25
AI Technical Summary
Existing roll coater methods for applying coating liquids to metal strips suffer from appearance defects like ribbing and uneven coating distribution due to warping and vibration, which are not adequately addressed by previous techniques that involve gas wiping or electromagnetic damping.
A coating device with an air pad on the exit side of the roll coater that forms a static pressure region using gas injection parts to stabilize the metal strip, suppressing warping and ensuring uniform coating application.
The static pressure region effectively suppresses warping and vibration, resulting in uniform coating distribution and eliminating appearance defects on the metal strip.
Smart Images

Figure 0007589644000002 
Figure 0007589644000003 
Figure 0007589644000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a technique for applying a liquid or slurry coating solution to a continuously passing metal strip by using a roll coater. [Background technology]
[0002] Conventionally, coating liquids having various physical properties have been applied to the surface of a continuously transported metal strip, such as a steel plate, to form a coating film, thereby imparting properties such as corrosion resistance, workability, aesthetics, and insulation properties to the metal strip.
[0003] A roll coater is generally used as a coating device (applicator) for applying a coating treatment to a metal strip. In a roll coater type applicator, for example, a coating liquid is supplied to the metal strip surface or to a roll, and the excess of the supplied coating liquid is squeezed out of the metal strip by the pressing load of the roll against the metal strip surface. This adjusts the amount of coating liquid attached to the metal strip. In such a roll coater method, a rubber roll having grooves engraved on the outer circumferential surface of the roll may be used in order to ensure that the necessary amount of coating solution is applied to the metal strip. In addition, a spray nozzle or a slit nozzle is generally used to supply the coating solution to the metal strip surface.
[0004] Here, a typical coating defect caused by the roll coater method is an appearance defect called ribbing. Ribbing occurs when a streak-like pattern that occurs in the outer circumferential direction of the roll is transferred to the metal strip. Specifically, ribbing is known as a defect that occurs when the fluid pressure fluctuation of the liquid meniscus between the roll and the metal strip exceeds the stabilizing effect of surface tension. Various methods have been proposed so far as technologies for preventing such ribbing.
[0005] For example, Patent Document 1 proposes a method in which the amount of MgO slurry applied to a steel sheet is first temporarily adjusted by a roll coater, and then adjusted to a desired amount by an air wiper, while eliminating localized coating distribution in the width direction that occurs at the roll coater. However, the method described in Patent Document 1 has problems such as the steel sheet coming into contact with the air wiper when the steel sheet is warped, the amount of coating being uneven, and ribbing not being completely prevented. Various techniques have been proposed so far as techniques for preventing such warping and vibration of steel sheets.
[0006] For example, Patent Document 2 proposes a method in which a guide member is provided above (on the exit side of) the wiping nozzle to guide the wiping gas sprayed from the wiping nozzle between the opposing surface of the band plate, generating static pressure and suppressing the plate shape and vibration of the band plate. In addition, in Patent Document 3, multiple electromagnets are arranged on at least one of both sides of a metal strip, at positions other than the positions facing each other across the metal strip. Also, a vibration measuring sensor is provided corresponding to each of the multiple electromagnets and measures the vibration displacement at the position where the corresponding electromagnet exerts an attractive force, and a control device is provided that applies a bias current to the electromagnet to apply a static attractive force to the metal strip, and then controls the electromagnet to suppress at least the vibration of the metal strip based on information from the vibration measuring sensor. Patent Document 3 proposes that vibration of the metal strip is suppressed by this configuration.
[0007] Patent Document 4 describes a technology related to gas wiping, which controls the amount of plating applied when applying molten metal plating to a metal body. In Patent Document 4, a gas flow discharged from one gas outlet of the wiping die generates a pressure loss near the gas outlet across the entire width of the plated metal body. This causes the gas to form a static pressure distribution on the surface of the metal body. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] Japanese Patent Application Publication No. 7-62445 [Patent Document 2] JP 2009-114534 A [Patent Document 3] JP 2004-124191 A [Patent Document 4] Japanese Patent Application Publication No. 7-188888 Summary of the Invention [Problem to be solved by the invention]
[0009] However, the method described in Patent Document 2 has a problem in that the wiping gas injected from the wiping nozzle leaks above (downstream) the guide member, and the effect of suppressing the plate shape and vibration of the band plate is insufficient. Furthermore, the method described in Patent Document 3 has the problem that the distance between the gas wiper and the electromagnet is large and the electromagnet is only on the outlet side of the gas wiper, so that warping and vibration at the gas wiper position are not sufficiently suppressed. Furthermore, the method described in Patent Document 4 has the problem that the wiping gas sprayed from the wiping nozzle leaks above (downstream) and below (upstream) the wiping nozzle, resulting in insufficient effect in suppressing the plate shape and vibration of the band plate.
[0010] The present invention has been made to solve such problems, and has an object to provide a coating method that, when applying a coating liquid to a continuously passing metal strip using a roll coater, can ensure a uniform amount of coating liquid adhered while suppressing the occurrence of appearance defects, even if the passing metal strip is warped. [Means for solving the problem]
[0011] As a result of extensive research into solving such problems, the inventors have discovered that by forming a static pressure region having a stable positive pressure of a predetermined magnitude or more along the sheet passing direction between the metal strip surface and the roll exit side, it is possible to eliminate or suppress ribbing while making the amount of coating liquid adhered uniform, even if the metal strip is warped. The present invention has been made based on the above findings and ideas.
[0012] That is, in order to solve the problem, one aspect of the present invention is a coating device that uses a roll coater to apply a coating liquid to a continuously passing metal strip, and the roll exit side of the roll coater has an air pad that has an opposing surface that faces the surface of the metal strip without contacting it, and two or more gas injection parts that inject gas onto the metal strip surface, and the two or more gas injection parts include at least a pair of gas injection parts that are spaced apart in the passing direction, and the opposing surface is disposed between the pair of gas injection parts. Another aspect of the present invention is a coating method for coating a metal strip with a coating liquid using the coating apparatus of the above aspect. Another aspect of the present invention is a metal strip manufacturing facility including the coating device of the above aspect. Effect of the Invention
[0013] According to the aspect of the present invention, when a coating liquid is applied to a continuously passing metal strip using a roll coater, even if the metal strip is warped, the static pressure area formed suppresses the warping of the metal strip, and at the same time, the static pressure area makes it possible to eliminate appearance defects of the paint applied to the metal strip while making the amount of coating liquid applied uniform. [Brief description of the drawings]
[0014] [Figure 1] FIG. 1 is a schematic side view illustrating a coating device according to an embodiment of the present invention. [Diagram 2] 1 is a schematic diagram showing an example of warping of a metal strip in the sheet width direction and a relationship between the metal strip and an opposing surface of an air pad. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of the present invention will be described with reference to the drawings. (composition) As shown in FIG. 1, the coating device according to this embodiment includes a coating liquid jet nozzle 2 for supplying a coating liquid, an adhesion amount adjustment roll 3 for adjusting the adhesion amount, an air pad 5, and a gas jet nozzle 4, which are provided in this order along the passing direction of a metal strip 1. This coating device is provided, for example, in a manufacturing facility for the metal strip 1. The manufacturing facility has, for example, a rolling process and the like upstream of the process in which the coating device is provided. 1, a coating process is performed on a metal strip 1 while it is continuously transported (passed) in a lateral direction (hereinafter also referred to as a longitudinal direction) along a pass line P. The metal strip 1 is made of, for example, a steel strip.
[0016] <Coating liquid spray nozzle 2> The coating liquid jet nozzle 2 includes an upper coating liquid jet nozzle 2A and a lower coating liquid jet nozzle 2B, which are disposed with the pass line P of the metal strip 1 interposed therebetween. The upper coating liquid ejection nozzle 2A ejects coating liquid 21A onto the upper surface of the metal strip 1. The lower coating liquid ejection nozzle 2B ejects coating liquid 21B onto the lower surface of the metal strip 1. The upper coating liquid ejecting nozzle 2A and the lower coating liquid ejecting nozzle 2B are not limited to nozzles such as a spray nozzle or a slit nozzle, and may have any structure as long as they are capable of supplying the coating liquid to the surface of the metal strip 1. In this embodiment, from the viewpoint of ease of supplying the coating liquid, a case in which a spray nozzle is used as the upper coating liquid ejecting nozzle 2A and the lower coating liquid ejecting nozzle 2B is exemplified.
[0017] <Adhesion amount adjustment roll 3> The adhesion amount adjusting roll 3 includes a pair of grooved rolls (upper grooved roll 3A and lower grooved roll 3B) arranged with the pass line P of the metal strip 1 in between. The adhesion amount adjustment roll 3 adjusts the adhesion amount of the coating liquid on the metal strip 1 by sandwiching the metal strip 1 between the upper grooved roll 3A and the lower grooved roll 3B. That is, the upper grooved roll 3A adjusts the adhesion amount on the upper surface of the metal strip 1 onto which the coating liquid is sprayed. The lower grooved roll 3B adjusts the adhesion amount on the lower surface of the metal strip 1 onto which the coating liquid is sprayed.
[0018] The grooved rolls 3A and 3B are made of, for example, rubber, and are preferably made of, for example, urethane rubber, nitrile rubber, or hypalon rubber, which has particularly excellent abrasion resistance. The roll diameter of the upper grooved roll 3A and the lower grooved roll 3B is preferably in the range of, for example, 50 mm or more and 400 mm or less. The nip pressure is preferably 1 kg / cm or more and 10 kg / cm or less. The rotation direction of the grooved rolls 3A, 3B is preferably the same as the running direction (passing direction) of the metal strip 1 at the contact position as shown in Fig. 1. There is no problem if the grooved rolls 3A, 3B rotate in the opposite direction, but in that case, the rubber of the rolls 3A, 3B will wear out quickly, and the rolls will need to be replaced frequently.
[0019] <Air Pad 5> The air pad 5 is disposed on the exit side of the adhesion amount adjusting roll 3 . The air pad 5 in this embodiment includes an upper air pad 5A and a lower air pad 5B disposed on either side of the pass line P of the metal strip 1. The upper air pad 5A and the lower air pad 5B may be disposed at different positions along the passing direction of the metal strip 1. However, it is preferable that the upper air pad 5A and the lower air pad 5B are disposed opposite each other as shown in FIG.
[0020] [Upper Air Pad 5A] The upper air pad 5A has an opposing surface 51Aa that faces the upper surface of the metal strip 1 without contacting it, and two or more gas jetting units that jet gas onto the upper surface of the metal strip 1. The two or more gas jetting units include at least a pair of gas jetting units 53A that are spaced apart in the sheet passing direction (the direction of the pass line P). The opposing surface 51Aa is disposed between the pair of gas jetting units 53A. The opposing surface 51Aa extends along the upper surface of the metal strip 1. As shown in Fig. 2, the width of the opposing surface 51Aa is preferably wider than the width of the metal strip 1 so as to cover the entire upper surface of the metal strip 1 in the sheet width direction. Note that the opposing surface 51Aa does not need to be a surface or a plane parallel to the opposing upper surface of the metal strip 1.
[0021] In FIG. 1, reference numeral 51A denotes a plate-like member that forms the opposing surface 51Aa. The pair of gas jetting parts 53A are formed on the upstream and downstream sides of the plate-like member 51A and are capable of jetting gas toward the upper surface of the metal strip 1, respectively. The pair of gas injection units 53A communicate with a header chamber 52A formed on the surface side opposite to the opposing surface 51Aa of the plate-shaped member 51A, and inject gas in a direction along the inclined surfaces of the front surface (upstream side) and rear surface (downstream side) of the plate-shaped member 51A in the plate passing direction. The injection ports of the pair of gas injection units 53A are composed of slits extending in the width direction of the metal strip 1. The injection ports may be composed of a plurality of holes lined up in the width direction of the metal strip 1, but a slit is preferable.
[0022] The gas injection direction 7A of at least one of the pair of gas injection parts 53A is inclined toward the opposing surface 51Aa with respect to the direction perpendicular to the sheet passing direction. That is, the gas injection direction 7A of at least one of the pair of gas injection parts 53A is directed toward a space (called a static pressure region 6) formed between the opposing surface 51Aa and the upper surface of the metal strip 1 facing the opposing surface 51Aa. In the example of FIG. 1, both of the pair of gas injection parts 53A are configured to inject gas toward the static pressure region 6. Reference numeral 8A denotes a pipe for supplying gas to the header chamber 52A.
[0023] With the above-mentioned configuration, a high pressure region (static pressure region 6) is formed between the upper air pad 5A and the upper surface of the metal strip 1, where the positive pressure is generated by the gas injected from the pair of gas injection units 53A. The static pressure region 6 is an area that extends in the sheet passing direction by the opposing surfaces. The high pressure region (static pressure region 6) makes it possible to suppress warping of the metal strip 1 in the sheet width direction.
[0024] [Lower air pad 5B] The lower air pad 5B includes an opposing surface 51Ba that faces the lower surface of the metal strip 1 without contacting the lower surface of the metal strip 1, and two or more gas injection parts that inject gas onto the lower surface of the metal strip 1. The two or more gas injection parts include at least a pair of gas injection parts 53B that are spaced apart in the sheet passing direction. The opposing surface 51Ba is disposed between the pair of gas injection parts 53B. The opposing surface 51Ba extends along the lower surface of the metal strip 1. The width of the opposing surface 51Ba is preferably wider than the width of the metal strip 1 so as to cover the entire lower surface of the metal strip 1 in the sheet width direction. Note that the opposing surface 51Ba does not need to be a surface or a plane parallel to the opposing lower surface of the metal strip 1.
[0025] In FIG. 1, reference numeral 51B denotes a plate-like member that forms the opposing surface 51Ba. The pair of gas jetting parts 53B are formed on the upstream and downstream sides of the plate-like member 51B and are capable of jetting gas toward the lower surface of the metal strip 1, respectively. The pair of gas injection parts 53B communicate with a header chamber 52B formed on the surface side opposite to the opposing surface 51Ba of the plate-shaped member 51B, and inject gas in a direction along the inclined surfaces of the front surface (upstream side) and rear surface (downstream side) of the plate-shaped member 51B in the sheet passing direction. The injection ports of the pair of gas injection parts 53B are formed of slits extending in the sheet width direction of the metal strip 1. The injection ports may be formed of a plurality of holes aligned in the width direction of the metal strip 1, but a slit is preferable.
[0026] The gas injection direction 7B of at least one of the pair of gas injection parts 53B is inclined toward the opposing surface 51Ba with respect to the direction perpendicular to the sheet passing direction. That is, the gas injection direction 7B of at least one of the pair of gas injection parts 53B is directed toward a space (called a static pressure region 6) formed between the opposing surface 51Ba and the lower surface of the metal strip 1 facing the opposing surface 51Ba. In the example of FIG. 1, both of the pair of gas injection parts 53B are configured to inject gas toward the static pressure region 6. Reference numeral 8B denotes a pipe for supplying gas to the header chamber 52B.
[0027] With the above-mentioned configuration, a high pressure region (static pressure region 6) is formed between the lower air pad 5B and the lower surface of the metal strip 1 by the positive pressure of the gas injected from the pair of gas injection units 53B. The static pressure region 6 extends in the sheet passing direction by the opposing surfaces. The high pressure region (static pressure region 6) makes it possible to suppress warping of the metal strip 1 along the sheet width direction.
[0028] <Function of Air Pad 5> Here, in this embodiment, each air pad 5 injects gas onto the surface of the metal strip 1 from both the upstream and downstream sides of the opposing surfaces 51Aa and 51Ba. The gas is injected from a slit-shaped injection port along the strip width direction. As a result, the injected gas forms an air curtain-like gas partition along the strip width direction on the upstream and downstream sides of the static pressure region 6, respectively, and air is constantly supplied to the static pressure region 6. This makes it possible to keep the static pressure region 6 in a high pressure state while preventing the gas supplied to the static pressure region 6 from leaking out in the strip passing direction. In addition, the static pressure region 6 is formed as an area of a predetermined length along the strip passing direction by the opposing surface 51Ba. As a result, the strip shape of the metal strip 1 can be corrected and vibration can be suppressed.
[0029] By setting the gas injection direction 7B of at least one of the pair of gas injection parts 53B to face the static pressure region 6, gas is reliably supplied to the static pressure region 6 and the static pressure region 6 is adjusted to a predetermined positive pressure. Here, the air pads 5 suppress gas leakage to both sides in the sheet passing direction, so that the gas in the static pressure region 6 flows in the sheet width direction. For this reason, the ribs formed along the vertical direction (sheet passing direction) are eliminated or suppressed by the positive pressure of the static pressure region 6 and the flow of gas in the sheet width direction, further uniforming the amount of adhesion. In particular, in this embodiment, upper and lower static pressure regions 6 are formed by sandwiching the metal strip 1 between the upper and lower air pads 5A, 5B, making it possible to more effectively suppress vibration of the metal strip 1 while effectively suppressing warping in the plate width direction. From the viewpoint of vibration suppression and warpage suppression, only one of the upper and lower air pads 5A, 5B may be used.
[0030] <Airpad 5 specifications and other information> The gas ejected from the air pad 5 is, for example, air or an inert gas such as nitrogen. The gap between the slits forming the nozzles of the pair of gas ejection parts 53A, 53B of the air pad 5 is set to, for example, 3 mm or more and 10 mm or less. The injection pressure of the gas injected from the pair of gas injection parts 53A, 53B is, for example, 3 kPa or more and 9 kPa or less. If the injection pressure is less than 3 kPa, it may be difficult to suppress warping of the metal strip 1. There is also a problem that ribbing is difficult to eliminate. If the injection pressure is greater than 9 kPa, scattering of the coating liquid adhering to the metal strip 1 is likely to occur. It is more preferable to set the injection pressure to 5 kPa or more and 7 kPa or less.
[0031] The pressure generated in the static pressure region 6 is preferably 1 kPa or more and 3 kPa or less. Moreover, the opposing distance between the opposing surfaces 51Aa, 51Ba of the air pad 5 and the metal strip 1 is preferably 5 mm or more and 20 mm or less. If the distance is less than 5 mm, there is a risk of contact between the air pad 5 and the metal strip 1. If the distance is greater than 20 mm, it becomes difficult to suppress warping of the metal strip 1. In addition, it is preferable that the gas injection direction 7B of at least one of the pair of gas injection sections 53A, 53B is inclined toward the static pressure region 6 side (the opposing surfaces 51Aa, 51Ba side) by 30 degrees or more and 60 degrees or less with respect to the direction perpendicular to the pass line P (the surface of the metal strip 1).
[0032] Moreover, the length of the opposing surfaces 51Aa, 51Ba in the sheet passing direction is preferably 300 mm or more and 1000 mm or less. As described above, the width of the opposing surfaces 51Aa, 51Ba of the air pad 5 is preferably larger than the plate width of the metal strip 1. If it is smaller than the plate width of the metal strip 1, it becomes difficult to suppress warping of the metal strip 1. Here, the material of the upper air pad 5A and the lower air pad 5B is not particularly limited, but it is preferable to use a strong material such as iron so that the header chamber 52B is not damaged by the gas pressure.
[0033] <Gas ejection nozzle 4> The gas ejection nozzles 4 are disposed on the outlet side of the air pad 5. In this embodiment, the gas ejection nozzles 4 are disposed in pairs, an upper gas ejection nozzle 4A and a lower gas ejection nozzle 4B, with the metal strip 1 in between, as shown in FIG. Each gas ejection nozzle 4 ejects a gas such as air or nitrogen toward the surface of the metal strip 1 that it faces.
[0034] Here, in this embodiment, the gas ejection nozzle 4 provided on the exit side of the grooved roll 3 is not essential. However, when the upper gas ejection nozzle 4A and the lower gas ejection nozzle 4B are installed, the upper gas ejection nozzle 4A and the lower gas ejection nozzle 4B serve as auxiliary roles for the air pad 5, and can more reliably eliminate ribbing. The gas ejection nozzle 4 is preferably in the form of a slit nozzle in order to ensure a uniform deposition amount.
[0035] The gap at the tip of the slit nozzle is preferably 0.5 to 3 mm. The injection pressure of the gas such as air or nitrogen is preferably 1 kPa or more and 5 kPa or less. If the injection pressure is less than 1 kPa, there is a problem that the ribs are difficult to eliminate. If the injection pressure is more than 5 kPa, the coating liquid is likely to scatter. It is more preferable that the injection pressure is 2 kPa or more and 3 kPa or less.
[0036] (Operation etc.) According to this aspect of the present invention, when a coating liquid is applied to a continuously passing metal strip 1 using a roll coater, the static pressure area 6 formed by the air pad 5 suppresses warping of the metal strip 1 even if the metal strip 1 is warped. Furthermore, the amount of coating liquid attached to the metal strip 1 is made uniform, eliminating appearance defects of the paint applied to the metal strip 1.
[0037] (others) The present disclosure may also have the following configuration. (1) A coating device that uses a roll coater to apply a coating liquid to a continuously passing metal strip, and has an air pad on the roll exit side of the roll coater, the air pad having an opposing surface that faces the surface of the metal strip without contacting it, and two or more gas injection parts that inject gas onto the metal strip surface, and the two or more gas injection parts include at least a pair of gas injection parts 53B that are spaced apart in the passing direction, and the opposing surface is disposed between the pair of gas injection parts. (2) The gas injection direction of at least one of the pair of gas injection parts is inclined toward the opposing surface with respect to a direction perpendicular to the sheet passing direction. (3) The nozzles of the pair of gas injection parts are formed of slits extending in a direction parallel to the width direction of the opposing metal strips. (4) A coating method for applying a coating liquid to a metal strip using the coating device of the present disclosure. (5) A metal strip manufacturing facility equipped with the coating device of the present disclosure. EXAMPLES
[0038] Next, an example of this embodiment will be described. (Example 1 of the present invention) In Example 1, a coating apparatus having the configuration shown in FIG. 1 was used. A steel strip was used as the metal strip 1 to be coated. The steel strip had a thickness of 0.3 mm, a width of 1000 mm, and a warp amount of 20 mm before coating. The metal strip 1 is passed through the 2 The coating process was carried out while the plate was being fed at a conveying speed of 2500 mm / s, and the target post-dry coating weight was 6.0 g / mm 2 A coating film was formed.
[0039] The amount of warping of the steel sheet before coating was measured using a laser shape measuring device. As shown in Fig. 2, when warping occurs in the steel sheet width direction, high and low parts are formed in the width direction of the metal strip 1. In this example, the difference in height between the highest part and the lowest part of the metal strip 1 before coating was taken as the amount of warping.
[0040] A slurry of magnesium oxide (MgO) powder mixed with water was used as the coating liquid to be applied to the metal strip 1, and the solid content of the slurry was adjusted to 10 wt %. The roll diameter of the roll coater was 150 mm, and the nip pressure was 3 kg / cm. The air pad 5 used for injecting gas onto the metal strip 1 had the following specifications: That is, for the pair of gas ejection parts 53B, the slit width was set to 3 mm and the ejection pressure was set to 5 kPa. The opposing surfaces 51Aa, 51Ba were spaced 10 mm from the metal strip 1. The opposing surfaces 51Aa, 51Ba were rectangular, with a length of 500 mm in the sheet passing direction and a length of 1500 mm in the sheet direction. The jetting direction of the pair of gas jetting parts 53B was set to be inclined at 45 degrees toward the static pressure region 6 side.
[0041] (Example 2 of the present invention) As an example 2 of the present invention, a coating apparatus having the configuration shown in Fig. 1 was used. An experiment was carried out under the same conditions as in this example 1, except that the injection pressure of the upper gas ejection nozzle 4A and the lower gas ejection nozzle 4B was set to 0 kPa.
[0042] Comparative Example 1 An experiment was carried out in the same manner as in Example 1 of this embodiment using the coating device shown in Patent Document 1. However, the metal strip 1 came into contact with the air wiper, and the production was unsuccessful. For this reason, it is not shown in Table 1 below. Comparative Example 2 Except for using the coating device shown in Patent Document 2, the experiment was carried out under the same conditions as in Example 1. The opposing distance between the guide member and the metal strip was set to 10 mm, the same as the opposing distance between the air pad. Comparative Example 3 An experiment was carried out under the same conditions as in Example 1 using the coating device shown in Patent Document 3. Comparative Example 4 An experiment was carried out under the same conditions as in Example 1 using the coating device shown in Patent Document 4.
[0043] <Evaluation of coating amount uniformity and appearance> For each metal strip 1 after coating and drying, the adhesion amount was measured multiple times in the width direction using a fluorescent X-ray film thickness meter. The uniformity of the adhesion amount was evaluated from the average, maximum, and minimum values of the measurement results. In addition, the appearance of the metal strip 1 after coating was evaluated according to the following criteria. [Appearance evaluation criteria] ⊚: No appearance defects were observed. ◯: Slight appearance defects are observed, but the product standard is met (irregularities cannot be detected by touching with the hand). ×: Appearance defects were observed and the product standards were not met (irregularities were noticeable when touched with the hand). The evaluation results of Example 1 and Comparative Examples 2 to 4 are shown in Table 1.
[0044] [Table 1]
[0045] As can be seen from Table 1, Example 1 based on the present invention was found to be superior to the comparative examples in terms of the uniformity of the deposition amount and the evaluation criteria for appearance. In addition, the evaluation criteria for the uniformity of the adhesion amount and the appearance of the invention example 2 are similar to those of the invention example 1. This shows that the upper gas ejection nozzle 4A and the lower gas ejection nozzle 4B provided downstream of the air pad 5 are not necessarily required. This confirmed the effectiveness of the present invention. [Explanation of symbols]
[0046] 1 Metal Strip 2. Coating liquid spray nozzle 2A Upper coating liquid ejection nozzle 2B Lower coating liquid ejection nozzle 3. Adhesion amount adjustment roll (grooved roll) 3A Top Grooved Roll 3B Roll with bottom groove 4 Gas ejection nozzle 4A Upper gas ejection nozzle 4B Lower gas ejection nozzle 5 Air Pad 5A Upper Air Pad 5B Lower Air Pad 6 Static Pressure Area 7A, 7B Gas injection direction 51A, 51B Plate-shaped member 51Aa, 51Ba Opposite side 53A, 53B gas injection section P Pass Line
Claims
1. A coating device that applies a coating liquid to a continuously passing metal strip using a roll coater, an air pad provided on the roll exit side of the roll coater, the air pad having a surface facing the metal strip without contacting the metal strip surface and two or more gas injection units for injecting gas onto the metal strip surface to which the coating liquid is attached; The two or more gas injection parts include at least a pair of gas injection parts spaced apart from each other in the sheet passing direction, and the opposing surface is disposed between the pair of gas injection parts, Each of the pair of gas injection parts is formed with a slit having a gap of 3 mm or more and 10 mm or less, and the injection pressure of the gas injected from the gas injection part is set to 3 kPa or more and 9 kPa or less. A coating device comprising:
2. A gas injection direction of at least one of the pair of gas injection parts is inclined toward the opposing surface side with respect to a direction perpendicular to the sheet passing direction.
2. The coating device according to claim 1.
3. The pair of gas injection parts each have an injection port formed of a slit extending in a direction along the sheet width direction of the opposing metal strips.
3. The coating device according to claim 1 or 2.
4. A coating method for coating a metal strip with a coating liquid by using the coating device according to any one of claims 1 to 3.
5. A metal strip manufacturing facility comprising the coating device according to any one of claims 1 to 3.
Citation Information
Patent Citations
Insoluble electrode pad
JP1981127799A
Apparatus and method for suppressing vibration of strip of continuous coating line
JP1990172562A
Method for coating steel sheet with liquid and slurry
JP1995062445A
Method for controlling coating weight of hot dip metal coating, the control device, and controlling nozzle
JP1995188888A
Device for damping vibration of metal strip, and method for manufacturing metal strip
JP2004124191A