Laminating method of display screen
By cleaning, preheating, baking, and UV curing the TFT screen and cover plate, the problem of uneven display caused by uneven force during the full lamination process of the TFT screen and cover plate was solved, achieving a high-quality full lamination effect.
Patent Information
- Application Number
- CN202411011020.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-26
AI Technical Summary
In existing technologies, uneven bonding force during the full lamination process of the TFT screen and cover glass leads to uneven display.
After cleaning and drying the cover plate and TFT screen, the OCA optical adhesive, preheated to a transparent state, is used for initial bonding. The OCA optical adhesive is then baked at 50℃~70℃ for 3~5 hours and then irradiated with UV light to cure it, thus achieving full bonding.
It effectively reduces uneven display and improves the bonding quality and consistency of the display screen.
Smart Images

Figure CN119024586A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of optical bonding technology, and in particular to a bonding method for a display screen. Background Art
[0002] Monitors are widely used in mobile phones, notebooks, televisions, etc., and may become the mainstream choice of future users. They have broad market prospects. Efficient and easy-to-operate touch screen and display bonding technology is becoming increasingly important.
[0003] Currently, the bonding methods of cover plates and TFT screens in the industry can be divided into non-full bonding and full bonding. Non-full bonding screens are also called frame bonding, which uses double-sided tape to bond the cover plate and TFT screen together. The disadvantages are that there is an air layer between the cover plate and the TFT screen, which makes it easy for dust to enter, is not drop-resistant, and causes the display effect to be greatly reduced after light refraction. Full bonding screens refer to the use of OCA optical glue or UV glue to seamlessly bond the TFT screen and the cover plate.
[0004] In the prior art, when the TFT screen and the cover plate are fully bonded, the bonding force is prone to be uneven, resulting in light leakage when the display screen is not powered but the backlight is powered, thereby causing uneven display. Summary of the invention
[0005] In order to solve the deficiencies in the prior art, the purpose of the present application is to provide a method for bonding a display screen to avoid the problem of uneven display caused by uneven bonding force.
[0006] To achieve the above-mentioned purpose, the present application provides a method for bonding a display screen, comprising:
[0007] Providing a cover plate and a TFT screen to be bonded, and cleaning the surfaces of the cover plate and the TFT screen until they are clean;
[0008] Preheating the OCA optical adhesive, melting it to a transparent state and pasting it on the surface of the cover plate;
[0009] The TFT screen and the cover plate are bonded to the surface with OCA optical adhesive to form a preliminary bonded product;
[0010] Bake the preliminary bonded product at 50℃~70℃ for 3~5 hours;
[0011] Use UV light to irradiate the preliminary bonded products to solidify the transparent OCA optical adhesive and achieve full bonding of the TFT screen and the cover plate.
[0012] Furthermore, the method further comprises:
[0013] After cleaning the surfaces of the cover plate and the TFT screen until they are clean, the cover plate and the TFT screen are dried.
[0014] Furthermore, the method also includes, before baking, performing pressing and bubbling treatment on the preliminary bonded product.
[0015] Furthermore, an air bag machine is used to perform pressure and bubble baking treatment on the preliminary bonded product.
[0016] Furthermore, the temperature during the bubbling process is 25-35° C., the air pressure is 0.35-0.45 MPa, and the bubbling time is 5-15 minutes.
[0017] Furthermore, the intensity of the UV light is between 400-4000 MW, the wavelength of the light is between 200-400 NM, and the irradiation time is 30 s-3 min.
[0018] Furthermore, the intensity of the UV light is 800 MW, the wavelength of the light is 365 NM, and the irradiation time is 130 s.
[0019] Furthermore, the preliminary bonded product was baked at 60° C. for 4 hours.
[0020] Furthermore, the OCA optical adhesive includes at least one of polyurethane acrylic resin, polyester acrylic resin, monofunctional acrylate, bifunctional acrylate, and multifunctional acrylate.
[0021] Furthermore, the thickness of the OCA optical adhesive is 50-250 μm.
[0022] The present application discloses a method for bonding a display screen, which releases the stress of the OCA optical adhesive through a heat baking process. Since the OCA optical adhesive has not yet solidified, the heat baking process can soften the OCA optical adhesive and reduce the adhesion, thereby reducing the stress on the TFT screen and reducing the uneven display.
[0023] Other features and advantages of the present application will be set forth in the following description, and in part will become apparent from the description, or may be understood by practicing the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] The accompanying drawings are used to provide a further understanding of the present application and constitute a part of the specification. Together with the embodiments of the present application, they are used to explain the present application and do not constitute a limitation of the present application. In the accompanying drawings:
[0025] Figure 1 This is a schematic diagram of the process of the display screen bonding method of Example 1 of the present application;
[0026] Figure 2 This is a schematic flow chart of the method for bonding a display screen according to Example 2 of the present application. DETAILED DESCRIPTION
[0027] The embodiments of the present application will be described in more detail below with reference to the accompanying drawings. Although certain embodiments of the present application are shown in the accompanying drawings, it should be understood that the present application can be implemented in various forms and should not be construed as being limited to the embodiments described herein. Instead, these embodiments are provided to provide a more thorough and complete understanding of the present application. It should be understood that the drawings and embodiments of the present application are only for exemplary purposes and are not intended to limit the scope of protection of the present application.
[0028] It should be understood that the various steps described in the method implementation of the present application can be performed in different orders and / or performed in parallel. In addition, the method implementation may include additional steps and / or omit the steps shown. The scope of the present application is not limited in this respect.
[0029] The term "including" and its variations used herein are open inclusions, i.e., "including but not limited to". The term "based on" means "based at least in part on". The term "one embodiment" means "at least one embodiment"; the term "another embodiment" means "at least one additional embodiment"; the term "some embodiments" means "at least some embodiments". The relevant definitions of other terms will be given in the following description.
[0030] It should be noted that the modifications of "one" and "plurality" mentioned in this application are illustrative rather than restrictive, and those skilled in the art should understand that unless otherwise clearly indicated in the context, it should be understood as "one or more". "Plurality" should be understood as two or more.
[0031] TFT (Thin Film Transistor) LCD is a thin film transistor LCD, which is a type of active matrix liquid crystal display (AM-LCD).
[0032] CA optical adhesive is one of the important raw materials for touch screens. It is a double-sided adhesive tape without a base material, made by making optical acrylic adhesive without a base material, and then laminating a layer of release film on the upper and lower base layers. It is the best adhesive for touch screens. Its advantages are clarity, high light transmittance (total light transmittance> 99%), high adhesion, high weather resistance, water resistance, high temperature resistance, UV resistance, controlled thickness, uniform spacing, and no yellowing (yellowing), peeling and deterioration after long-term use.
[0033] OCA optical glue is divided into two categories, one is resistive and the other is capacitive. Resistive optical glue can be divided into 50um and 25um according to different thicknesses, and capacitive optical glue can be divided into 100um, 175um, 200um, and 250um.
[0034] OCA optical adhesive can be applied to different fields according to its thickness. Its main uses are: electronic paper, transparent device bonding, projection screen assembly, aerospace or military optical device assembly, display assembly, lens assembly, resistive touch screen G+F+F, F+F, capacitive touch screen, panel, ICON and glass and polycarbonate and other plastic materials bonding. It is a special adhesive used for bonding transparent optical components (such as lenses, etc.). It is required to be colorless and transparent, with a light transmittance of more than 90%, good bonding strength, can be cured at room temperature or medium temperature, and has small curing shrinkage.
[0035] Silicone rubber, acrylic resin, unsaturated polyester, polyurethane, epoxy resin and other adhesives can be used to bond optical components. Some treatment agents are usually added during preparation to improve their optical properties or reduce the curing shrinkage. Suitable for fixing various films and screens (acrylic, glass screens, touch screens, etc.) around the display of mobile machines.
[0036] UV light radiation, namely ultraviolet radiation curing, UV is the abbreviation of ultraviolet light, curing refers to the process of converting a substance from a low molecular weight to a high molecular weight. UV curing generally refers to the curing conditions or requirements of coatings (paints), inks, adhesives (glue) or other potting sealants that need to be cured by ultraviolet light, which is different from heat curing, crosslinking agent (curing agent) curing, natural curing, etc.
[0037] Hereinafter, embodiments of the present application will be described in detail with reference to the accompanying drawings.
[0038] Example 1
[0039] An embodiment of the present application provides a method for laminating a display screen to avoid the problem of uneven display caused by uneven lamination force.
[0040] Figure 1 This is a flow chart of the bonding method of the display screen of Example 1 of the present application, and the following will refer to Figure 1 The bonding method of the display screen of the present application is described in detail, including:
[0041] S101: providing a cover plate and a TFT screen to be bonded, and cleaning the surfaces of the cover plate and the TFT screen until they are clean;
[0042] In this embodiment, after the surfaces of the cover plate and the TFT screen are cleaned, the cover plate and the TFT screen are dried.
[0043] S102: preheating the OCA optical adhesive, melting it to a transparent state and pasting it on the surface of the cover plate;
[0044] In this embodiment, the OCA optical adhesive is evenly coated on the cover plate, and the thickness of the OCA optical adhesive is 75 μm.
[0045] In some other embodiments, the thickness of the OCA optical adhesive is 50-250 μm.
[0046] S103: performing a bonding operation on the TFT screen and the cover plate on the surface where the OCA optical adhesive is attached to form a preliminary bonded product;
[0047] S104: performing pressing and bubble baking treatment on the preliminary bonded finished product;
[0048] In this embodiment, an air bag machine is used to perform pressure and bubble baking on the preliminary bonded product. The bubble baking temperature is set to 30° C., the bubble baking pressure is set to 0.4 MPa, and the bubble baking time is 8 minutes.
[0049] In some other embodiments, the temperature of the bubble baking can also be 25-35° C., the corresponding air pressure of the bubble baking can be 0.35-0.45 MPa, and the bubble baking time can be 5-15 min.
[0050] S105: baking the preliminary bonded product at 50°C to 70°C for 3 to 5 hours;
[0051] In this embodiment, the preliminary bonded product is baked at 60° C. for 4 hours.
[0052] It should be noted that the stress relief effect is best when the process parameter of baking the preliminary bonded product at 60°C for 4 hours.
[0053] S106: Use UV light to irradiate the preliminary bonded product to solidify the transparent OCA optical adhesive, thereby achieving full bonding of the TFT screen and the cover plate;
[0054] In this embodiment, the intensity of the UV light is 800 MW, the wavelength of the light is 365 NM, and the irradiation time is 130 s.
[0055] In other embodiments, the intensity, wavelength and time of the UV light can be adaptively selected within the ranges of 400-4000 MW, 200-400 NM and 30s-3min, respectively.
[0056] It is understandable that UV light irradiation causes the OCA optical adhesive exposed to UV light to react with light and change its structural properties, thereby curing.
[0057] In this embodiment, the OCA optical adhesive includes at least one of polyurethane acrylic resin, polyester acrylic resin, monofunctional acrylate, bifunctional acrylate, and multifunctional acrylate.
[0058] Example 2
[0059] An embodiment of the present application provides a method for laminating a display screen to avoid the problem of uneven display caused by uneven lamination force.
[0060] Figure 2 This is a flow chart of the bonding method of the display screen of Example 2 of the present application, which will be referred to below Figure 2 The bonding method of the display screen of the present application is described in detail, including:
[0061] S201: providing a cover plate and a TFT screen to be bonded, and washing the cover plate and the TFT screen with pure water until they are clean;
[0062] Specifically, the cover plate and the TFT screen are cleaned with pure water under the action of a water pump to remove dirt on the surface of the cover plate and the TFT screen until the substrate is clean.
[0063] In this embodiment, after the surfaces of the cover plate and the TFT screen are cleaned, the cover plate and the TFT screen are dried.
[0064] S202: preheating the OCA optical adhesive, melting it to a transparent state, and pasting it to the surface of the cover plate, wherein the thickness of the OCA optical adhesive is 80 μm;
[0065] In some other embodiments, the thickness of the OCA optical adhesive is 50-250 μm.
[0066] S203: performing a bonding operation on the TFT screen and the cover plate on the surface where the OCA optical adhesive is attached to form a preliminary bonded product;
[0067] S204: using an air bag machine to perform pressure and bubble baking treatment on the preliminary bonded finished product;
[0068] In this embodiment, the bubble baking temperature is set to 35° C., the bubble baking pressure is set to 0.35 MPa, and the bubble baking time is 10 minutes.
[0069] In some other embodiments, the temperature of the bubble baking can also be 25-35° C., the corresponding air pressure of the bubble baking can be 0.35-0.45 MPa, and the bubble baking time can be 5-15 min.
[0070] S205: baking the preliminary bonded product at 65° C. for 3 hours and 20 minutes;
[0071] S206: using UV light to irradiate the preliminary bonded product to solidify the transparent OCA optical adhesive, thereby achieving full bonding of the TFT screen and the cover plate;
[0072] In this embodiment, the intensity of the UV light is 1000 MW, the wavelength of the light is 365 NM, and the irradiation time is 100 s.
[0073] In other embodiments, the intensity, wavelength and time of the UV light can be adaptively selected within the ranges of 400-4000 MW, 200-400 NM and 30s-3min, respectively.
[0074] It is understandable that UV light irradiation causes the OCA optical adhesive exposed to UV light to react with light and change its structural properties, thereby curing.
[0075] In this embodiment, the OCA optical adhesive includes at least one of polyurethane acrylic resin, polyester acrylic resin, monofunctional acrylate, bifunctional acrylate, and multifunctional acrylate.
[0076] The above description is only a partial embodiment of the present application and an explanation of the technical principles used. Those skilled in the art should understand that the scope of disclosure involved in the present application is not limited to the technical solution formed by a specific combination of the above technical features, but should also cover other technical solutions formed by any combination of the above technical features or their equivalent features without departing from the above disclosed concept. For example, the above features are replaced with the technical features with similar functions disclosed in this application (but not limited to) by each other to form a technical solution.
[0077] In addition, although each operation is described in a specific order, this should not be construed as requiring these operations to be performed in the specific order shown or in a sequential order. Under certain circumstances, multitasking and parallel processing may be advantageous. Similarly, although some specific implementation details are included in the above discussion, these should not be construed as limiting the scope of the application. Some features described in the context of a separate embodiment can also be implemented in a single embodiment in combination. On the contrary, the various features described in the context of a single embodiment can also be implemented in multiple embodiments individually or in any suitable sub-combination mode.
[0078] Although the subject matter has been described in language specific to structural features and / or methodological logical actions, it should be understood that the subject matter defined in the appended claims is not necessarily limited to the specific features or actions described above. On the contrary, the specific features and actions described above are merely example forms of implementing the claims.
Claims
1. A method for bonding a display screen, comprising: Providing a cover plate and a TFT screen to be bonded, and cleaning the surfaces of the cover plate and the TFT screen until they are clean; Preheating the OCA optical adhesive, melting it to a transparent state and pasting it on the surface of the cover plate; The TFT screen and the cover plate are bonded to the surface with OCA optical adhesive to form a preliminary bonded product; Bake the preliminary bonded product at 50℃~70℃ for 3~5 hours; Use UV light to irradiate the preliminary bonded products to solidify the transparent OCA optical adhesive and achieve full bonding of the TFT screen and the cover plate.
2. The method for bonding a display screen according to claim 1, characterized in that: The method further comprises: After cleaning the surfaces of the cover plate and the TFT screen until they are clean, the cover plate and the TFT screen are dried.
3. The method for bonding a display screen according to claim 1, characterized in that: The method further comprises, before baking, performing pressing and bubbling treatment on the preliminary bonded product.
4. The method for bonding a display screen according to claim 3, characterized in that: Use an air bag machine to press and remove bubbles from the preliminary bonded products.
5. The display screen bonding method according to claim 4, characterized in that: The temperature during the bubbling process is 25-35°C, the air pressure is 0.35-0.45MPa, and the bubbling time is 5-15min.
6. The method for bonding a display screen according to claim 1, characterized in that: The intensity of UV light is between 400-4000MW, the wavelength of light is between 200-400NM, and the irradiation time is 30s-3min.
7. The method for bonding a display screen according to claim 6, characterized in that: The intensity of UV light is 800MW, the wavelength of light is 365NM, and the irradiation time is 130s.
8. The display screen bonding method according to claim 1, characterized in that: The preliminary laminated product was baked at 60°C for 4 hours.
9. The display screen bonding method according to claim 1, characterized in that: The OCA optical adhesive includes at least one of polyurethane acrylic resin, polyester acrylic resin, monofunctional acrylate, bifunctional acrylate, and multifunctional acrylate.
10. The display screen bonding method according to claim 1, characterized in that: The thickness of the OCA optical adhesive is 50-250 μm.
Citation Information
Cited By
Ultra-thin and ultra-large display screen fitting method, display screen and display equipment
CN119937193A
Optical adhesive coating parameter design optimization method, system and equipment
CN120103806A
Method, system and equipment for designing and optimizing coating parameters of optical adhesive
CN120103806B
Method for separating a glass cover of an optical display device from the optical display device and separating device
DE102026131380A1