Coil component and method for manufacturing the coil component

By arranging the plating layer in scattered locations and using a resin-containing second electrode layer, the coil component addresses the issue of electrode peeling during plating, maintaining a stable connection and preventing stress-induced separation.

JP7590293B2Active Publication Date: 2024-11-26TDK CORP
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2021146985
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-09-09
Publication Date
2024-11-26
Estimated Expiration
2041-09-09

AI Technical Summary

Technical Problem

The formation of a plating layer on the electrode layer in coil components can cause stress, leading to peeling of the external electrode due to the edges of the electrode layer peeling off during the plating process.

Method used

The plating layer is arranged at multiple scattered locations on the edge of the electrode layer, rather than covering the entire edge, and a second electrode layer containing resin is used to disperse stress, preventing peeling.

Benefits of technology

This configuration effectively suppresses the peeling of external electrodes by dispersing stress during the plating process, ensuring a stable connection between the electrode layers and the element body.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007590293000001
    Figure 0007590293000001
  • Figure 0007590293000002
    Figure 0007590293000002
  • Figure 0007590293000003
    Figure 0007590293000003
Patent Text Reader

Abstract

To provide a coil component and a coil component manufacturing method, capable of inhibiting an external electrode from being peeled.SOLUTION: A laminated coil component 1 comprises an element body 2, a coil 8 disposed in the element body 2, and a first external electrode 4 disposed on a surface of the element body 2. The first external electrode 4 includes: a first electrode layer 40 disposed on the surface of the element body 2; and a first plating layer 42 and a second plating layer 43 that are disposed on the first electrode layer 40. The first plating layer 42 and the second plating layer 43 are disposed on an edge of the first electrode layer 40 so as to be studded at a plurality of locations.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a coil component and a method for manufacturing a coil component. [Background technology]

[0002] Patent Document 1 discloses an electronic component including a ceramic laminate, an internal electrode layer disposed within the ceramic laminate, and an external electrode disposed on a surface of the ceramic laminate. In the electronic component described in Patent Document 1, the external electrode includes an external electrode layer disposed on the surface of the ceramic laminate, and a plating layer disposed on the external electrode layer. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2018-190490 A Summary of the Invention [Problem to be solved by the invention]

[0004] When manufacturing a coil component in which the external electrodes have an electrode layer and a plating layer, the electrode layer is formed on the element body, and then the plating layer is formed on the electrode layer. When the plating layer is formed, the edge of the electrode layer formed on the surface of the element body may peel off due to stress generated during the formation of the plating layer.

[0005] An object of one aspect of the present invention is to provide a coil component that can suppress peeling of external electrodes and a method for manufacturing the coil component. [Means for solving the problem]

[0006] A coil component according to one aspect of the present invention comprises a base body, a coil disposed within the base body, and an external electrode disposed on a surface of the base body, the external electrode having a first electrode layer disposed on the surface of the base body and a plating layer disposed on the first electrode layer, the plating layer being disposed so as to be scattered at multiple locations on the edge of the first electrode layer.

[0007] In a coil component according to one aspect of the present invention, the plating layer is arranged so as to be scattered at multiple locations on the edge of the first electrode layer. In this way, in the coil component, the plating layer is arranged so as to be scattered at multiple locations on the edge of the first electrode layer, rather than over the entire edge of the first electrode layer, so that the stress generated when forming the plating layer can be dispersed. Therefore, in the coil component, peeling of the first electrode layer from the body can be suppressed. Therefore, in the coil component, peeling of the external electrode can be suppressed.

[0008] In one embodiment, the external electrode has a second electrode layer disposed on the first electrode layer, the second electrode layer containing a resin and not disposed on the edge of the first electrode layer, and the plating layer may be disposed on the first electrode layer and the second electrode layer. In this configuration, the edge of the first electrode layer is not covered by the second electrode layer, so that the plating layer is disposed so as to be scattered at a plurality of locations on the edge of the first electrode layer. Therefore, it is possible to suppress peeling of the first electrode layer from the element body. In addition, the second electrode layer contains a resin. This allows the second electrode layer to relieve stress during the formation of the plating layer. Therefore, it is possible to suppress peeling of the second electrode layer from the first electrode layer due to stress during the formation of the plating layer.

[0009] In one embodiment, the external electrode has a second electrode layer disposed on the first electrode layer, the second electrode layer has a surface free of glass components compared to the first electrode layer, and is not disposed on the edge of the first electrode layer, and the plating layer may be disposed on the first electrode layer and the second electrode layer. In this configuration, the edge of the first electrode layer is not covered by the second electrode layer, so that the plating layer is disposed so as to be scattered at a plurality of locations on the edge of the first electrode layer. Therefore, peeling of the first electrode layer from the element body can be suppressed. Also, the second electrode layer has a surface free of glass components compared to the first electrode layer. Therefore, the plating layer can be formed continuously and uniformly on the second electrode layer.

[0010] In one embodiment, the element body may be formed by stacking magnetic layers containing a plurality of metallic magnetic particles of a soft magnetic material.

[0011] A method for manufacturing a coil component according to one aspect of the present invention is a method for manufacturing a coil component comprising a base body, a coil disposed within the base body, and an external electrode disposed on a surface of the base body, the method having an electrode layer disposed on the surface of the base body, and a plating layer disposed on the electrode layer, the plating layer being formed on the edge of the electrode layer so that the plating layer is scattered in multiple locations.

[0012] In a manufacturing method for a coil component according to one aspect of the present invention, a plating layer is formed on an edge of an electrode layer such that the plating layer is scattered at multiple locations. In this manner, in the manufacturing method for a coil component, the plating layer is formed on the edge of the first electrode layer such that the plating layer is scattered at multiple locations, rather than on the entire edge of the electrode layer, so that stress generated when forming the plating layer can be dispersed. Therefore, the manufacturing method for a coil component can suppress peeling of the electrode layer from the base body. Therefore, the manufacturing method for a coil component can suppress peeling of the external electrode in the coil component. Effect of the Invention

[0013] According to one aspect of the present invention, peeling of the external electrodes can be suppressed. [Brief description of the drawings]

[0014] [Figure 1] FIG. 1 is a perspective view showing a laminated coil component according to one embodiment. [Diagram 2] FIG. 2 is an exploded perspective view of the laminated coil component shown in FIG. [Diagram 3] FIG. 3 is an enlarged cross-sectional view showing a portion of the first external electrode. [Figure 4] FIG. 4 is a diagram showing a schematic diagram of a plating layer disposed on an edge of a first electrode layer of a first external electrode. [Diagram 5] FIG. 5 is a diagram showing a schematic diagram of a plating layer disposed on an edge of the second electrode layer of the first external electrode. [Figure 6] FIG. 6 is an enlarged cross-sectional view showing a portion of the second external electrode. [Figure 7] FIG. 7 is a diagram showing a schematic diagram of a plating layer disposed on an edge of the first electrode layer of the second external electrode. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings. In the description of the drawings, the same or corresponding elements are designated by the same reference numerals, and duplicated explanations will be omitted.

[0016] As shown in FIG. 1, the laminated coil component 1 includes an element body 2, and a first external electrode 4 and a second external electrode 5 arranged on both ends of the element body 2, respectively.

[0017] The element body 2 has a rectangular parallelepiped shape. The rectangular parallelepiped shape includes a rectangular parallelepiped shape with chamfered corners and ridges, and a rectangular parallelepiped shape with rounded corners and ridges. The element body 2 has, as its outer surfaces, a pair of end faces 2a, 2b facing each other, a pair of main faces 2c, 2d facing each other, and a pair of side faces 2e, 2f facing each other. The facing direction in which the pair of main faces 2c, 2d face each other is the first direction D1. The facing direction in which the pair of end faces 2a, 2b face each other is the second direction D2. The facing direction in which the pair of side faces 2e, 2f face each other is the third direction D3. In this embodiment, the first direction D1 is the height direction of the element body 2. The second direction D2 is the longitudinal direction of the element body 2 and is perpendicular to the first direction D1. The third direction D3 is the width direction of the element body 2 and is perpendicular to the first direction D1 and the second direction D2.

[0018] The pair of end faces 2a, 2b extend in a first direction D1 so as to connect the pair of principal faces 2c, 2d together. The pair of end faces 2a, 2b also extend in a third direction D3 (the short side direction of the pair of principal faces 2c, 2d). The pair of side faces 2e, 2f extend in the first direction D1 so as to connect the pair of principal faces 2c, 2d together. The pair of side faces 2e, 2f also extend in a second direction D2 (the long side direction of the pair of end faces 2a, 2b). The principal face 2d can be defined as a mounting face that faces another electronic device (for example, a circuit board or an electronic component) when the laminated coil component 1 is mounted on the other electronic device.

[0019] As shown in Fig. 3, the element body 2 is formed by stacking multiple magnetic layers 6. Each magnetic layer 6 is stacked in a first direction D1. That is, the first direction D1 is the stacking direction. The element body 2 has multiple stacked magnetic layers 6. In the actual element body 2, the multiple magnetic layers 6 are integrated to the extent that the boundaries between the layers are not visible.

[0020] Each magnetic layer 6 includes a plurality of metal magnetic particles. The metal magnetic particles are made of a soft magnetic alloy (soft magnetic material). The soft magnetic alloy is, for example, an Fe-Si based alloy. When the soft magnetic alloy is an Fe-Si based alloy, the soft magnetic alloy may include P. The soft magnetic alloy may be, for example, an Fe-Ni-Si-M based alloy. "M" includes one or more elements selected from Co, Cr, Mn, P, Ti, Zr, Hf, Nb, Ta, Mo, Mg, Ca, Sr, Ba, Zn, B, Al, and rare earth elements.

[0021] In the magnetic layer 6, the metal magnetic particles are bonded to each other. The bond between the metal magnetic particles is realized, for example, by bonding between oxide films formed on the surfaces of the metal magnetic particles. In the magnetic layer 6, the metal magnetic particles are electrically insulated from each other by the bonding between the oxide films. The thickness of the oxide film is, for example, 5 to 60 nm or less. The oxide film may be composed of one or more layers.

[0022] The element body 2 contains a resin. The resin exists between a plurality of metal magnetic particles. The resin is a resin having electrical insulation properties (insulating resin). The insulating resin includes, for example, a silicone resin, a phenol resin, an acrylic resin, or an epoxy resin.

[0023] 1, the first external electrode 4 is disposed on the end face 2a side of the element body 2, and the second external electrode 5 is disposed on the end face 2b side of the element body 2. In other words, the first external electrode 4 and the second external electrode 5 are positioned apart from each other in the opposing direction of the pair of end faces 2a, 2b.

[0024] The first external electrode 4 is disposed on one end face 2a side. The first external electrode 4 includes five electrode parts: a first electrode part 4a located on the end face 2a, a second electrode part 4b located on the main face 2c, a third electrode part 4c located on the main face 2d, a fourth electrode part 4d located on the side face 2e, and a fifth electrode part 4e located on the side face 2f. The first electrode part 4a, the second electrode part 4b, the third electrode part 4c, the fourth electrode part 4d, and the fifth electrode part 4e are connected at the ridge part of the element body 2 and are electrically connected to each other. The first external electrode 4 is formed on five faces, namely, one end face 2a, a pair of main faces 2c, 2d, and a pair of side faces 2e, 2f. The first electrode part 4a, the second electrode part 4b, the third electrode part 4c, the fourth electrode part 4d, and the fifth electrode part 4e are integrally formed.

[0025] As shown in FIG. 3, the first external electrode 4 has a first electrode layer 40, a second electrode layer 41, a first plating layer 42, and a second plating layer 43.

[0026] The first electrode layer 40 is formed on five surfaces, namely, one end surface 2a, a pair of main surfaces 2c, 2d, and a pair of side surfaces 2e, 2f. The first electrode layer 40 contains a conductive material (e.g., Ag or Pd). The first electrode layer 40 is formed as a sintered body of a conductive paste containing a conductive metal powder (e.g., Ag powder or Pd powder) and a glass frit.

[0027] The second electrode layer 41 is formed on the first electrode layer 40. The second electrode layer 41 is disposed on the first electrode layer 40 which is formed on five surfaces, namely, one end surface 2a, a pair of main surfaces 2c, 2d, and a pair of side surfaces 2e, 2f. The second electrode layer 41 is a conductive resin layer. The conductive resin is a mixture of a thermosetting resin with a conductive material and an organic solvent. The conductive material is, for example, a conductive filler. The conductive filler is a metal powder. The metal powder is, for example, Ag powder. The thermosetting resin is, for example, a phenol resin, an acrylic resin, a silicone resin, an epoxy resin, or a polyimide resin.

[0028] The first plating layer 42 is disposed so as to cover a portion of the first electrode layer 40 and the second electrode layer 41. The first plating layer 42 is formed on five surfaces, namely, one end face 2a, a pair of main faces 2c, 2d, and a pair of side faces 2e, 2f. The first plating layer 42 is a Ni plating layer formed by Ni plating.

[0029] The second plating layer 43 is disposed so as to cover the first plating layer 42. The second plating layer 43 is formed on five surfaces, namely, one end face 2a, a pair of main faces 2c, 2d, and a pair of side faces 2e, 2f. The second plating layer 43 is a Sn plating layer formed by Sn plating.

[0030] In the first external electrode 4, the second electrode layer 41 is not disposed on the edge 40E of the first electrode layer 40. That is, the edge 40E of the first electrode layer 40 is not covered by the second electrode layer 41. The edge 40E of the first electrode layer 40 is located closer to the center (inner side) of the element body 2 in the second direction D2 than the second electrode layer 41. The edge 40E of the first electrode layer 40 protrudes toward the end face 2b of the element body 2 in the second direction D2 than the second electrode layer 41. In other words, the edge 41E of the second electrode layer 41 is recessed toward the end face 2a of the element body 2 in the second direction D2 than the edge 40E of the first electrode layer 40. The edge 40E of the first electrode layer 40 includes a tip on the end face 2b side of the element body 2 and is an exposed portion that is not covered by the second electrode layer 41, and refers to, for example, a portion having a length of about 1 / 4 of the length in the second direction D2 of the first electrode layer 40 disposed on the main surface 2c of the element body 2. Although FIG. 3 shows the first electrode layer 40 and the second electrode layer 41 on the main surface 2c of the element body 2, the main surface 2d and the side surfaces 2e and 2f also have the same configuration.

[0031] The first plating layer 42 and the second plating layer 43 are disposed on a part of the edge 40E of the first electrode layer 40. In other words, the first plating layer 42 and the second plating layer 43 are not disposed on a part of the edge 40E of the first electrode layer 40. As shown in FIG. 4, the second plating layer 43 (first plating layer 42) is disposed so as to be scattered at a plurality of locations. The second plating layers 43 (first plating layers 42) are scattered independently of each other. Being independent of each other does not mean that they are electrically independent, but means that they are formed with a boundary between them in appearance. It can also be said that the second plating layer 43 (first plating layer 42) is disposed discontinuously on the edge 40E of the first electrode layer 40. It can also be said that the second plating layer 43 (first plating layer 42) is scattered in an island shape. In the region of the edge 40E of the first electrode layer 40 where the second plating layer 43 (first plating layer 42) is not disposed, a glass layer 40G is provided on the surface (glass components are present). That is, the second plating layer 43 (first plating layer 42) is not disposed on the glass layer 40G.

[0032] A first plating layer 42 and a second plating layer 43 are disposed on the second electrode layer 41. As shown in FIG. 5, the second plating layer 43 (first plating layer 42) is continuously and uniformly formed on the second electrode layer 41. Although the resin may be precipitated on the surface of the second electrode layer 41, the region (area) of the resin is smaller than that of the glass layer 40G and is substantially uniformly present on the surface of the second electrode layer 41, so that the distance between the resins is short. Therefore, even if the resin is precipitated on the second electrode layer 41, the second electrode layer 41 is formed so as to bridge (bridge) the portion where the resin is not precipitated and cover the resin. As a result, the first plating layer 42 and the second plating layer 43 are continuously and uniformly formed on the second electrode layer 41.

[0033] The first electrode layer 40 and the second electrode layer 41 are joined with a predetermined strength by an anchor effect due to the unevenness of the boundary between them.

[0034] As shown in FIG. 1, the second external electrode 5 is disposed on the other end face 2b side. The second external electrode 5 includes five electrode parts: a first electrode part 5a located on the end face 2b, a second electrode part 5b located on the main face 2c, a third electrode part 5c located on the main face 2d, a fourth electrode part 5d located on the side face 2e, and a fifth electrode part 5e located on the side face 2f. The first electrode part 5a, the second electrode part 5b, the third electrode part 5c, the fourth electrode part 5d, and the fifth electrode part 5e are connected at the ridge part of the element body 2 and are electrically connected to each other. The second external electrode 5 is formed on five faces, namely, one end face 2b, a pair of main faces 2c and 2d, and a pair of side faces 2e and 2f. The first electrode part 5a, the second electrode part 5b, the third electrode part 5c, the fourth electrode part 5d, and the fifth electrode part 5e are integrally formed.

[0035] As shown in FIG. 6, the second external electrode 5 has a first electrode layer 50, a second electrode layer 51, a first plating layer 52, and a second plating layer 53.

[0036] The first electrode layer 50 is formed on five surfaces, namely, one end surface 2b, a pair of main surfaces 2c and 2d, and a pair of side surfaces 2e and 2f. The first electrode layer 50 contains a conductive material (e.g., Ag or Pd). The first electrode layer 50 is formed as a sintered body of a conductive paste containing a conductive metal powder (e.g., Ag powder or Pd powder) and a glass frit.

[0037] The second electrode layer 51 is formed on the first electrode layer 50. The second electrode layer 51 is disposed on the first electrode layer 50 which is formed on five surfaces, namely, one end surface 2b, a pair of main surfaces 2c, 2d, and a pair of side surfaces 2e, 2f. The second electrode layer 51 is a conductive resin layer. The conductive resin is a mixture of a thermosetting resin with a conductive material and an organic solvent. The conductive material is, for example, a conductive filler. The conductive filler is a metal powder. The metal powder is, for example, Ag powder. The thermosetting resin is, for example, a phenol resin, an acrylic resin, a silicone resin, an epoxy resin, or a polyimide resin.

[0038] The first plating layer 52 is disposed so as to cover a portion of the first electrode layer 50 and the second electrode layer 51. The first plating layer 52 is formed on five surfaces, namely, one end face 2b, a pair of main faces 2c, 2d, and a pair of side faces 2e, 2f. The first plating layer 52 is a Ni plating layer formed by Ni plating.

[0039] The second plating layer 53 is disposed so as to cover the first plating layer 52. The second plating layer 53 is formed on five surfaces, namely, one end face 2b, a pair of main faces 2c, 2d, and a pair of side faces 2e, 2f. The second plating layer 53 is a Sn plating layer formed by Sn plating.

[0040] In the second external electrode 5, the second electrode layer 51 is not disposed on the edge 50E of the first electrode layer 50. That is, the edge 50E of the first electrode layer 50 is not covered by the second electrode layer 51. The edge 50E of the first electrode layer 50 is located closer to the center (inner side) of the element body 2 in the second direction D2 than the second electrode layer 51. The edge 50E of the first electrode layer 50 protrudes toward the end face 2a of the element body 2 in the second direction D2 than the second electrode layer 51. In other words, the edge 51E of the second electrode layer 51 is recessed toward the end face 2b of the element body 2 in the second direction D2 than the edge 50E of the first electrode layer 50. The edge 50E of the first electrode layer 50 includes a tip on the end face 2a side of the element body 2 and is an exposed portion that is not covered by the second electrode layer 51, and refers to, for example, a portion having a length of about 1 / 4 of the length in the second direction D2 of the first electrode layer 50 disposed on the main surface 2c of the element body 2. Although FIG. 6 shows the first electrode layer 50 and the second electrode layer 51 on the main surface 2c of the element body 2, the main surface 2d and the side surfaces 2e and 2f also have the same configuration.

[0041] The first plating layer 52 and the second plating layer 53 are disposed on a portion of the edge 50E of the first electrode layer 50. In other words, the first plating layer 52 and the second plating layer 53 are not disposed on a portion of the edge 50E of the first electrode layer 50. As shown in FIG. 7, the second plating layer 53 (first plating layer 52) is disposed so as to be scattered at a plurality of locations on the edge 50E of the first electrode layer 50. The second plating layers 53 (first plating layers 52) are scattered independently of each other. Being independent of each other does not mean that they are electrically independent, but means that they are formed with a boundary between each other in appearance. It can also be said that the second plating layer 53 (first plating layer 52) is disposed discontinuously on the edge 50E of the first electrode layer 50. It can also be said that the second plating layer 53 (first plating layer 52) is scattered in an island shape. In the region of the edge 50E of the first electrode layer 50 where the second plating layer 53 (first plating layer 52) is not disposed, a glass layer 50G is provided on the surface. That is, the second plating layer 53 (first plating layer 52) is not disposed on the glass layer 50G.

[0042] The first plating layer 52 and the second plating layer 53 are disposed on the second electrode layer 51. The first plating layer 52 and the second plating layer 53 are continuously and uniformly formed on the second electrode layer 51. Although the resin may be precipitated on the surface of the second electrode layer 51, the region (area) of the resin is smaller than that of the glass layer 50G and is present substantially uniformly on the surface of the second electrode layer 51, so that the distance between the resins is short. Therefore, even if the resin is precipitated on the second electrode layer 51, the second electrode layer 51 is formed so as to bridge over (bridge) the portion where the resin is not precipitated and cover the resin. As a result, the first plating layer 52 and the second plating layer 53 are continuously and uniformly formed on the second electrode layer 51.

[0043] The first electrode layer 50 and the second electrode layer 51 are joined with a predetermined strength by an anchor effect due to the unevenness of their boundary.

[0044] As shown in FIG. 2, the laminated coil component 1 has a coil 8 disposed within an element body 2. The coil 8 is configured in a spiral shape by electrically connecting a plurality of coil conductors 10, 11, 12, 13, 14, and 15 with a first connecting conductor 16 and a second connecting conductor 17. Adjacent coil conductors 10, 11, 12, 13, 14, and 15 are electrically connected with through-hole conductors (not shown). The coil conductor 15 and the second connecting conductor 17 are electrically connected with a through-hole conductor (not shown). The first connecting conductor 16 constitutes one end of the coil 8. The first connecting conductor 16 is exposed at an end face 2a of the element body 2 and connected to the first external electrode 4 (first electrode portion 4a). The second connecting conductor 17 constitutes the other end of the coil 8. The second connecting conductor 17 is exposed at an end face 2b of the element body 2 and connected to the second external electrode 5 (first electrode portion 5a).

[0045] The coil conductors 10, 11, 12, 13, 14, and 15, the first connecting conductor 16, and the second connecting conductor 17 are made of a conductive material (such as Ni or Cu) that is typically used as a coil conductor. The coil conductors 10, 11, 12, 13, 14, and 15, the first connecting conductor 16, and the second connecting conductor 17 are formed as a sintered body of a conductive paste containing the above-mentioned conductive material.

[0046] Next, a method for manufacturing the laminated coil component 1 will be described.

[0047] A slurry is prepared by mixing metal magnetic particles, an insulating resin, a solvent, etc. The prepared slurry is applied onto a substrate (e.g., a PET film, etc.) by a doctor blade method to form a green sheet that will become the magnetic layer 6. Next, through holes are formed by laser processing at positions in the green sheet where the through-hole conductors are to be formed.

[0048] Next, a first conductive paste is filled into the through holes of the green sheet. The first conductive paste is made by mixing conductive metal powder and binder resin. Next, conductors that will become the coil conductors 10, 11, 12, 13, 14, and 15, the first connecting conductor 16, and the second connecting conductor 17 are provided on the green sheet. At this time, the conductors are connected to the conductive paste in the through holes.

[0049] Next, the green sheets are stacked. Here, multiple green sheets with conductors provided thereon are peeled off from the base material, stacked, and pressed in the stacking direction to form a laminate. At this time, the green sheets are stacked so that the conductors that will become the coil conductors 10, 11, 12, 13, 14, and 15, the first connecting conductor 16, and the second connecting conductor 17 overlap in the stacking direction.

[0050] Next, the laminate of green sheets is cut into chips of a predetermined size by a cutter to obtain green chips. Next, the binder resin contained in each part is removed from the green chip, and the green chip is fired. In this way, an element body 2 is obtained.

[0051] Next, a second conductive paste is provided on each of the pair of end faces 2a, 2b of the element body 2. The second conductive paste is made by mixing conductive metal powder, glass frit, binder resin, etc. Next, the second conductive paste is baked by performing a heat treatment to form the first electrode layers 40, 50. Glass layers 40G, 50G are precipitated on part of the surfaces of the first electrode layers 40, 50 by the heat treatment.

[0052] Next, a third conductive paste is provided on the first electrode layers 40, 50. The third conductive paste is prepared by mixing a thermosetting resin with a conductive material, an organic solvent, and the like. The third conductive paste is provided so as not to cover the edges 40E, 50E of the first electrode layers 40, 50. Next, the third conductive paste is baked by performing a heat treatment to form the second electrode layers 41, 51. Finally, the surfaces of the first electrode layers 40, 50 and the second electrode layers 41, 51 are plated to form the first plating layers 42, 52 and the second plating layers 43, 53. Through the above steps, the laminated coil component 1 is obtained.

[0053] As described above, in the laminated coil component 1 according to the present embodiment, the first plating layers 42, 52 and the second plating layers 43, 53 are arranged so as to be scattered at a plurality of locations on the edges 40E, 50E of the first electrode layers 40, 50. In this manner, in the laminated coil component 1, the first plating layers 42, 52 and the second plating layers 43, 53 are arranged so as to be scattered at a plurality of locations on the edges 40E, 50E of the first electrode layers 40, 50, rather than on the entire edges 40E, 50E of the first electrode layers 40, 50. This allows the stress generated when the first plating layers 42, 52 and the second plating layers 43, 53 are formed to be dispersed. Therefore, in the laminated coil component 1, it is possible to suppress peeling of the first electrode layers 40, 50 from the element body 2. Therefore, in the laminated coil component 1, it is possible to suppress peeling of the first external electrode 4 and the second external electrode 5.

[0054] In the laminated coil component 1 according to the present embodiment, the first external electrode 4 has a second electrode layer 41 disposed on the first electrode layer 40, and the second external electrode 5 has a second electrode layer 41 disposed on the first electrode layer 50. The second electrode layers 41, 51 contain resin and are not disposed on the edges 40E, 50E of the first electrode layers 40, 50. The first plating layers 42, 52 and the second plating layers 43, 53 are disposed on the first electrode layers 40, 50 and the second electrode layers 41, 51. In this configuration, the edges 40E, 50E of the first electrode layers 40, 50 are not covered by the second electrode layers 41, 51, so that the first plating layers 42, 52 and the second plating layers 43, 53 are disposed so as to be scattered at a plurality of locations on the edges 40E, 50E of the first electrode layers 40, 50. Therefore, it is possible to suppress peeling of the first electrode layers 40, 50 from the element body 2. In addition, the second electrode layers 41, 51 contain resin. This allows the second electrode layers 41, 51 to relieve stress during the formation of the first plating layers 42, 52 and the second plating layers 43, 53. Therefore, peeling of the second electrode layers 41, 51 from the first electrode layers 40, 50 due to stress during the formation of the first plating layers 42, 52 and the second plating layers 43, 53 can be suppressed.

[0055] Although the embodiment of the present invention has been described above, the present invention is not necessarily limited to the above-described embodiment, and various modifications are possible without departing from the gist of the present invention.

[0056] The element body 2 does not necessarily have to be composed of metal magnetic particles, and may be composed of ferrite (e.g., Ni-Cu-Zn ferrite, Ni-Cu-Zn-Mg ferrite, Cu-Zn ferrite), a dielectric material, or the like.

[0057] In the above embodiment, the first external electrode 4 has the first electrode portion 4a, the second electrode portion 4b, the third electrode portion 4c, the fourth electrode portion 4d, and the fifth electrode portion 4e. However, the first external electrode 4 may have only the first electrode portion 4a, or may have only the second electrode portion 4b. The second external electrode 5 may also have only the first electrode portion 5a, or may have only the second electrode portion 5b. The first external electrode 4 and the second external electrode 5 may have various shapes.

[0058] In the above embodiment, an example has been described in which the first external electrode 4 has the first electrode layer 40 and the second electrode layer 41. However, the first external electrode does not necessarily have to have the second electrode layer. The same applies to the second external electrode.

[0059] In the above embodiment, the second electrode layers 41, 51 are conductive resin layers. However, the second electrode layers 41, 51 do not have to be conductive resin layers. In this case, it is preferable that the second electrode layer does not have a glass component (glass layer) on the surface, as compared with the first electrode layer. In this configuration, a plating layer can be formed continuously and uniformly on the second electrode layer.

[0060] In the above embodiment, the plating layers include the first plating layers 42, 52 and 43, 53. However, the plating layer may be a single layer or a three-layer structure.

[0061] The number of coil conductors is not limited to the above values. [Explanation of symbols]

[0062] 1...laminated coil component, 2...element body, 4...first external electrode, 5...second external electrode, 6...magnetic layer, 8...coil, 40,50...first electrode layer, 40E,50E...edge, 41,51...second electrode layer, 42,52...first plating layer, 43,53...second plating layer.

Claims

1. The body and A coil disposed within the element body; and an external electrode disposed on a surface of the element body, the external electrode has a first electrode layer disposed on a surface of the element body and a plating layer disposed on the first electrode layer, The plating layer is disposed so as to be scattered at a plurality of locations on an edge of the first electrode layer.

2. the external electrode includes a second electrode layer disposed on the first electrode layer; the second electrode layer contains a resin and is not disposed on the edge of the first electrode layer; The coil component according to claim 1 , wherein the plating layer is disposed on the first electrode layer and the second electrode layer.

3. the external electrode includes a second electrode layer disposed on the first electrode layer; The second electrode layer has a surface that does not include a glass component compared to the first electrode layer, and is not disposed on the edge of the first electrode layer; The coil component according to claim 1 , wherein the plating layer is disposed on the first electrode layer and the second electrode layer.

4. The coil component according to any one of claims 1 to 3, wherein the base body is formed by laminating magnetic layers containing a plurality of metallic magnetic particles of a soft magnetic material.

5. 1. A method for manufacturing a coil component comprising: an element body; a coil disposed within the element body; and external electrodes disposed on a surface of the element body, the method comprising the steps of: an electrode layer disposed on a surface of the element body; and a plating layer disposed on the electrode layer, The method for manufacturing a coil component includes forming the plating layer on an edge of the electrode layer such that the plating layer is scattered in a plurality of locations.

Citation Information

Patent Citations

  • Thin-film chip parts

    JP1996335529A

  • Chip type electronic component and manufacturing method of the same

    JP2013069713A

  • Multilayer ceramic electronic component and manufacturing method for the same

    JP2013098540A

  • Ceramic electronic component and manufacturing method for ceramic electronic component

    JP2015109410A

  • Ceramic electronic component and method of manufacturing the same

    JP2016031992A