Polycrystalline silicon rod manufacturing apparatus and manufacturing method
The apparatus addresses the challenge of unpredictable growth shapes by using a movable adjustment member with a cooling unit to optimize electrode positioning and prevent silicon deposition, enhancing polycrystalline silicon quality and reactor efficiency.
Patent Information
- Application Number
- JP2021111400
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-07-05
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2041-07-05
AI Technical Summary
Existing polycrystalline silicon manufacturing methods face challenges in determining optimal electrode arrangements due to unpredictable growth shapes, leading to contamination, reduced quality, and increased costs, as well as difficulties in repositioning core wires without causing silicon deposition on adapters.
A polycrystalline silicon rod manufacturing apparatus with a movable adjustment member and cooling unit to prevent silicon deposition, allowing flexible electrode positioning and stress relief during growth and cooling.
Enables smooth movement and optimization of core wire electrodes, preventing silicon contamination and improving product quality by reducing stress-related issues and enabling reuse of reactor components.
Smart Images

Figure 0007591987000001 
Figure 0007591987000002 
Figure 0007591987000003
Abstract
Description
[Technical field]
[0001] The present invention relates to an apparatus and method for producing polycrystalline silicon for depositing polycrystalline silicon by supplying a source gas onto the surface of a heated silicon core wire. [Background technology]
[0002] Polycrystalline silicon is the raw material for single crystal silicon for semiconductors or silicon for solar cells. The Siemens process is known as a method for manufacturing polycrystalline silicon. The Siemens process is a method in which polycrystalline silicon is precipitated on the surface of a silicon core wire by contacting a silane raw material gas with the silicon core wire, generally using a CVD (Chemical Vapor Deposition) method.
[0003] In the Siemens method, silicon core wires are assembled into an inverted U shape, with two vertical and one horizontal, and both ends of the inverted U-shaped silicon core wires are connected to core wire holders and fixed to a pair of metal electrodes placed on a bottom plate. Generally, multiple sets of inverted U-shaped silicon core wires are arranged inside a reactor.
[0004] An inverted U-shaped silicon core wire is heated to the precipitation temperature by passing an electric current through it, and a raw material gas, for example a mixture of trichlorosilane and hydrogen, is brought into contact with the silicon core wire, causing silicon to grow in the vapor phase, and a polycrystalline silicon rod of the desired diameter is formed in an inverted U-shape.
[0005] In the bottom plate used in the Siemens process, the silicon core electrode is generally inserted into a through hole in the bottom plate of the reactor, and since multiple sets of silicon core wires are arranged as described above, there are multiple silicon core electrodes penetrating the bottom plate.
[0006] In this context, various proposals have been made regarding the arrangement of electrodes.
[0007] Patent Document 1 (JP 2011-231005 A) proposes a positional relationship between a silicon seed rod, a raw material gas supply port, and an exhaust port in order to provide a polycrystalline silicon reduction furnace that can easily deposit polycrystalline silicon without causing defects in the surface shape or warping.
[0008] Patent Document 2 (WO2011 / 123998) proposes an arrangement that can increase thermal efficiency and uniformity of gas flow, thereby increasing production volume, improving surface quality, and reducing energy consumption.
[0009] Patent Document 3 (WO2012 / 171149) and Patent Document 4 (WO2013 / 093051) also propose an arrangement within a reactor for the purpose of improving productivity and uniformity within the reactor.
[0010] In this situation, Patent Document 5 (JP 2014-101256 A) proposes making the arrangement of a heater installed in a furnace variable in order to extend the life of the heater. [Prior art documents] [Patent documents]
[0011] [Patent Document 1] JP 2011-231005 A [Patent Document 2] WO2011 / 123998 [Patent Document 3] WO2012 / 171149 [Patent Document 4] WO2013 / 093051 [Patent Document 5] JP 2014-101256 A DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]
[0012] However, the optimal arrangements proposed in Patent Documents 1 to 4 are different from each other. In addition, the reactors are becoming larger, and the cost of the reactors is very high. Nevertheless, the arrangement of the silicon core wire electrode penetrating the bottom plate needs to be determined before installation.
[0013] However, in reality, the growth shape of the polycrystalline silicon cannot be known unless the polycrystalline silicon is actually grown in the installed reactor.
[0014] In addition, an embodiment such as that in Patent Document 5 has been proposed, but even if the heater arrangement can be optimized by Patent Document 5, polycrystalline silicon is precipitated on the adapter, etc., so that the arrangement of the core wire cannot be readjusted, and the adapter itself is difficult to reuse, and must be discarded. Even if it can be reused, the precipitated polycrystalline silicon may peel off from the adjustment member when the arrangement is readjusted. The polycrystalline silicon precipitated on the adapter, etc. is in contact with the member, and the quality is reduced. The polycrystalline silicon falls into the furnace, resulting in increased contamination inside the furnace. In addition, since the precipitated polycrystalline silicon is not suitable as polycrystalline silicon for semiconductors or solar cells, it must be used for products with low quality requirements.
[0015] The present invention has been made in consideration of such problems, and aims to provide a manufacturing apparatus for polycrystalline silicon rods and a manufacturing method for polycrystalline silicon rods that can suppress the deposition of silicon on an adapter or the like and move the position of the core wire electrode without hindrance. [Means for solving the problem]
[0016] The apparatus for producing polycrystalline silicon rods according to the present invention comprises: A core wire for depositing polycrystalline silicon; A core wire electrode provided to penetrate the bottom plate; an adjustment member provided between the silicon core wire and the core wire electrode and movable with respect to the bottom plate; A cooling unit capable of cooling the adjustment member; The present invention may also include:
[0017] In the apparatus for producing polycrystalline silicon rods according to the present invention, The cooling unit may have a nozzle that blows gas toward the adjustment member.
[0018] In the apparatus for producing polycrystalline silicon rods according to the present invention, The gas may be a silane source gas.
[0019] In the apparatus for producing polycrystalline silicon rods according to the present invention, The cooling section may include a heat dissipating insulating member provided between the bottom plate and the adjustment member for cooling the adjustment member by the bottom plate.
[0020] In the apparatus for producing polycrystalline silicon rods according to the present invention, The cooling portion may be provided in the core electrode and may have a flow path for flowing a cooling liquid.
[0021] In the apparatus for producing polycrystalline silicon rods according to the present invention, The adjustment member may connect the core wire electrode and the silicon core wire such that a central axis of the core wire electrode and a central axis of the silicon core wire differ from each other.
[0022] In the apparatus for producing polycrystalline silicon rods according to the present invention, The adjustment member may be made of a material different from that of the core wire electrode.
[0023] In the apparatus for producing polycrystalline silicon rods according to the present invention, The adjusting member may have a lower resistivity than the core wire electrode.
[0024] The method for producing polycrystalline silicon rods according to the present invention includes the steps of: The method includes a step of depositing polycrystalline silicon on a core wire using the above-mentioned polycrystalline silicon rod manufacturing apparatus, In the step of depositing polycrystalline silicon, the adjustment member may be cooled by the cooling section. Effect of the Invention
[0025] By applying the present invention to an apparatus or method for growing polycrystalline silicon rods, the position of the silicon core electrode can be moved smoothly, and the arrangement can be optimized.
[0026] As one aspect of the present invention, by adopting a mechanism or member for cooling the adjusting member, the adjusting member can be cooled during the production of polycrystalline silicon, which prevents the deposition of polycrystalline silicon on the adjusting member and prevents the movement of the adjusting member from being hindered. As a result, the adjusting member can move smoothly, which relieves the stress applied to the core wire electrode by the polycrystalline silicon during growth and cooling after production, and prevents the polycrystalline silicon from cracking or collapsing during growth and cooling after production. [Brief description of the drawings]
[0027] [Figure 1] 1 is a longitudinal sectional view of a reactor according to an embodiment of the present invention; [Diagram 2] FIG. 2 is a plan view showing a silicon core, an adjustment member, and the like used in the embodiment of the present invention, viewed from above. [Diagram 3] 3 is a plan view showing a state in which the silicon core electrode is rotated around the central axis thereof from the state shown in FIG. 2; FIG. [Figure 4] FIG. 4 is a vertical cross-sectional view showing an example of an adjustment member used in the embodiment of the present invention. [Diagram 5] FIG. 4 is a vertical cross-sectional view showing an example of a mechanism for cooling an adjustment member used in the embodiment of the present invention. [Figure 6] FIG. 11 is a vertical cross-sectional view showing another example of a mechanism for cooling the adjustment member used in the embodiment of the present invention. [Figure 7] 5 is a longitudinal sectional view showing a mechanism for moving an adjustment member used in an embodiment of the present invention, the mechanism being different from the embodiment shown in FIGS. 2 to 4. FIG. [Figure 8] FIG. 2 is a vertical cross-sectional view showing a mechanism for cooling an adjustment member, a control unit, and a thermometer used in the embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0028] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of the present invention will be described.
[0029] <composition> As shown in Fig. 1, a reactor 100 used in the Siemens process has a bottom plate (base plate) 80 and a bell jar 81. The silicon core wire electrode 60 is generally inserted into a through hole in the bottom plate 80 of the reactor 100. Since a plurality of sets of silicon core wires 1 are generally arranged, there are a plurality of silicon core wire electrodes 60 penetrating the bottom plate 80.
[0030] For this reason, the position of the through-hole in the bottom plate 80 must be determined at the time of designing the reactor 100. However, in reality, the growth shape of the polycrystalline silicon cannot be known until polycrystalline silicon is grown in the reactor 100 itself after it is installed.
[0031] When the reactor 100 is added under the same conditions, this is not a big problem. However, in many cases, an improved reactor 100 is designed for the purpose of improving productivity, a popcorn shape, which is a type of surface shape, and the shape of polycrystalline silicon during growth. In this case, not only the silicon core electrode 60 but also the supply gas inlet 91 and the exhaust gas outlet 96 are often changed in the arrangement inside the reactor 100. In addition, the reaction conditions such as temperature, supply gas concentration, supply gas flow rate, and reaction pressure are often changed. In this case, the arrangement is changed and the reaction conditions are changed, so that the growth shape of polycrystalline silicon including the popcorn shape cannot be known unless polycrystalline silicon is actually grown in the installed reactor 100 itself.
[0032] In addition, even if the arrangement of only the heater can be optimized as shown in Patent Document 5, the heater is used for initial heating, and since the heater is turned off during the growth of polycrystalline silicon, there is almost no deposition of polycrystalline silicon on the heater. Therefore, although Patent Document 5 is sufficient for adjusting only the position of the heater before polycrystalline silicon is deposited, it may cause problems when moving the arrangement of the silicon core wire 1 after polycrystalline silicon is deposited.
[0033] For this reason, when the arrangement of the silicon core wire 1 moves on the bottom plate 80 when electricity is applied with reactive gas being supplied and the reaction temperature is reached, or when cooling after the reaction is completed, care must be taken to prevent the precipitation of polycrystalline silicon on the moving parts.
[0034] In the present embodiment, the silicon core wire electrode 60 can be freely disposed on the bottom plate 80 regardless of the position of the through hole. In this case, a configuration that allows adjustment on the bottom plate 80 can be used.
[0035] As an example, the manufacturing apparatus for polycrystalline silicon rods of the present embodiment is an apparatus for manufacturing polycrystalline silicon rods by the Siemens method. As shown in Fig. 1, the manufacturing apparatus for polycrystalline silicon rods includes a silicon core wire (core wire) 1 for precipitating polycrystalline silicon, a silicon core wire electrode (core wire electrode) 60 provided to penetrate a bottom plate 80, an adjustment member 10 provided between the silicon core wire 1 and the silicon core wire electrode 60 and made of an adapter or the like movable relative to the bottom plate 80, and a cooling unit (cooling mechanism) capable of cooling the adjustment member 10.
[0036] When the diameter of the polycrystalline silicon increases during the reaction, or when the polycrystalline silicon rod is cooled at the end of the reaction, the adjustment member 10 naturally moves within the plane to relieve stress, but the larger the diameter of the grown polycrystalline silicon, the greater the amount of movement of the adjustment member 10 during the reaction, or during cooling, or during the reaction and cooling. When the average diameter of the polycrystalline silicon in the reactor was 150 mm, the maximum amount of movement of the adjustment member 10 was 10 mm. Similarly, when the diameter of the polycrystalline silicon was 120 mm, the maximum amount of movement was 7 mm.
[0037] The adjustment member 10, such as an adapter, may be connected on the bottom plate 80 such that the central axis of the silicon core wire electrode 60 and the central axis of the silicon core wire 1 differ from each other. A core wire holding member 2 may be provided between the adjustment member 10 and the silicon core wire 1 (see FIGS. 5 and 6).
[0038] 1, both lower ends of an inverted U-shaped silicon core wire 1 are fixed to a pair of silicon core wire electrodes 60 via an adjustment member 10. The silicon core wire electrodes 60 penetrate a bottom plate 80 with an insulator 61 sandwiched therebetween.
[0039] 4, the adjustment member 10 may have an electrode binding member 11 having a recess in the center, a holding member 12 that holds a lower end of the silicon core wire 1 and is rotatable around the central axis of the electrode binding member 11, and a fastening member 13 such as a screw for being inserted into the recess of the electrode binding member 11 to support the holding member 12. The lower end of the silicon core wire 1 may be fixed in a manner such that it is inserted into a hole 12a provided in the holding member 12.
[0040] FIG. 2 is a view showing a state in which both lower ends of the silicon core wire 1 are held by a pair of adjustment members 10 for the silicon core wire 1, as viewed from above the bottom plate 80, and shows an embodiment in which two silicon core wires 1 are provided. In FIG. 2, a cooling nozzle 20, which will be described later, is provided adjacent to both lower ends of the silicon core wire 1. FIG. 3 shows an embodiment in which the adjustment member 10 in the state of FIG. 2 is rotated around the central axis of the silicon core wire electrode 60. In this manner, both lower ends of the silicon core wire 1 of this embodiment are movable. There are various ways in which both lower ends of the silicon core wire 1 can be moved. For example, both lower ends of the silicon core wire 1 may be moved by sliding them in an in-plane direction (horizontal direction) (see FIG. 7). In this case, for example, a recess 115 may be provided on the bottom surface of the adjustment member 10, and a protrusion 110 to be inserted into the recess 115 may be provided on the upper surface of the core wire electrode 60. The adjustment member 10 may be movable along the protrusion 110 and its position may be fixed relative to a fixture 121 fixed to the bottom plate 80 by a fastening member 120 .
[0041] As shown in FIG. 6, the cooling unit may have a gas supply unit 25 that supplies the stored gas or the generated gas, a nozzle (cooling nozzle) 20 that blows the gas toward the adjustment member 10, and a gas supply pipe 26 that is provided between the gas supply unit 25 and the nozzle 20 and guides the gas supplied from the gas supply unit 25 to the nozzle 20. The gas supplied from the gas supply unit 25 may be a silane source gas. In this case, the silane source gas may be, for example, a mixed gas of trichlorosilane and hydrogen. Since the movement distance of the adjustment member 10 due to stress generation during the precipitation reaction of polycrystalline silicon and / or during cooling of the polycrystalline silicon rod is about 10 mm, the adjustment member 10 can be sufficiently cooled even if the position of the nozzle 20 is fixed. However, the present invention is not limited to such an embodiment, and the position of the nozzle 20 may be movable in the in-plane direction by sliding, etc. In addition, the amount of gas supplied from the gas supply unit 25 and / or the direction of the nozzle 20 can be freely changed, and by adjusting the amount of gas supplied and the direction of the nozzle 20, even if the adjustment member 10 moves due to stress generated during the precipitation reaction of polycrystalline silicon and / or during cooling of the polycrystalline silicon rod, sufficient cooling of the adjustment member 10 may be performed. In this case, each member may be controlled in response to a command from the control unit 50 (see FIG. 8).
[0042] As shown in FIG. 5 and FIG. 6, the cooling section may have a heat dissipation insulating member 30 provided between the bottom plate 80 and the adjustment member 10 to cool the adjustment member 10 by the bottom plate 80. A bottom plate cooling liquid passage 70 through which a cooling liquid such as cooling water passes may be provided inside the bottom plate 80, and the bottom plate 80 may be cooled by the cooling liquid passing through the bottom plate cooling liquid passage 70. By providing the above-mentioned heat dissipation insulating member 30, the adjustment member 10 can be cooled by the cooled bottom plate 80. As the heat dissipation insulating member 30, a compound of a thermally conductive filler in silicone rubber or the like may be used. For example, an insulating composition may be used in which 100 parts by weight of synthetic rubber such as silicone rubber is compounded with 100 to 800 parts by weight of at least one metal oxide selected from beryllium oxide, aluminum oxide, hydrated aluminum oxide, magnesium oxide, and zinc oxide. Furthermore, ceramics may be used. As another example of the heat dissipation insulating member 30, for example, silicon nitride, silicon carbide, aluminum nitride, aluminum oxide, zirconia, etc. may be used. When the core wire electrode 60 is made of copper, the thermal conductivity is very high. When cooling water flows through the core wire electrode 60, the core wire electrode 60 can cool the heat dissipation and insulation member 30, and as a result, the adjustment member 10 can also be cooled.
[0043] The heat dissipating insulation member 30 may be fixed to the adjustment member 10, but not fixed to the bottom plate 80. In this case, the heat dissipating insulation member 30 also moves with the movement of the adjustment member 10. If the heat dissipating insulation member 30 has a sufficient size in the in-plane direction (horizontal direction) relative to the movable distance of the adjustment member 10, the heat dissipating insulation member 30 may be fixed to the bottom plate 80, and the bottom plate 80 may not move even if the adjustment member 10 moves within a range of about 10 mm. As an example, when the adjustment member 10 moves about 10 mm during the precipitation reaction of polycrystalline silicon and / or during the cooling of the polycrystalline silicon rod, even if the size of the heat dissipating insulation member 30 in the in-plane direction is not so large, the adjustment member 10 and the bottom plate 80 can always be in contact with each other via the heat dissipating insulation member 30, regardless of the position of the adjustment member 10.
[0044] 5 and 6, the cooling unit may have a liquid supply unit 40 that supplies a cooling liquid such as cooling water, and an electrode cooling liquid flow path 41 that is provided in the core wire electrode 60 and through which the cooling liquid flows. The core wire electrode 60 usually has a cooling liquid such as cooling water flowing therethrough to cool the current-carrying electrode, which is preferable.
[0045] As described above, by adopting, as the cooling unit, any one or more of the following mechanisms: a mechanism for blowing cooling gas toward the adjustment member 10; a mechanism for cooling by the heat dissipation effect of connecting the adjustment member 10 to the bottom plate 80 via the heat dissipation insulating member 30; and a mechanism for cooling the adjustment member 10 via the core wire electrode 60 with a cooling liquid, it is possible to prevent silicon crystals from precipitating on the adjustment member 10. In other words, if no cooling unit (cooling mechanism) is provided, silicon crystals may precipitate on the adjustment member 10 due to heat generated by current flow or the like. If silicon crystals precipitate on the adjustment member 10 in this way, when the position of the adjustment member 10 is adjusted and moved before the growth of the next polycrystalline silicon (new polycrystalline silicon) is started, the precipitated crystals fall into the furnace during the movement, causing contamination. In addition, if silicon crystals precipitate on the adjustment member 10 in this way, a problem may occur in which adjustment by the adjustment member 10 cannot be performed smoothly. In this regard, the use of the cooling unit as described above is extremely beneficial in that it can remove the heat generated by the current passing through the adjustment member 10 and prevent such problems from occurring. In addition, according to this embodiment, it is also possible to prevent the resistance value of the adjustment member 10 from increasing due to heat generation.
[0046] In addition, by adopting a cooling unit (cooling mechanism) for cooling the adjusting member 10 in this manner, the adjusting member can be cooled during the production of polycrystalline silicon, so that deposition of polycrystalline silicon on the adjusting member 10 can be prevented, and the movement of the adjusting member 10 can be prevented from being hindered. As a result, the adjusting member 10 can be moved without hindrance, and the stress applied to the core wire electrode 60 by the polycrystalline silicon during growth and the polycrystalline silicon in the cooling process after growth is completed can be alleviated. Therefore, cracking and collapse of the polycrystalline silicon during growth and during cooling after production can be prevented. Note that a heating process for stress relief may be performed after growth is completed, and even in that case, the adjusting member 10 can be moved without hindrance, so that the stress applied to the core wire electrode 60 can be alleviated.
[0047] The adjustment member 10 may be made of a material different from that of the silicon core wire electrode 60. As an example, a metal is used as the silicon core wire electrode 60, but the adjustment member 10 may be made of the same metal or a different type of metal, or even carbon or other electrically conductive materials.
[0048] The adjusting member 10 may have a lower resistivity than the silicon core wire electrode 60 provided on the silicon core wire electrode 60. By adopting such an embodiment, it is advantageous in that excess heat generation can be avoided.
[0049] If the adjusting member 10 does not have the cooling unit (cooling mechanism) according to this embodiment, the temperature of the adjusting member 10 exceeds 400°C during the precipitation of polycrystalline silicon, and polycrystalline silicon precipitates on the adjusting member 10. On the other hand, by adopting the cooling unit shown in this embodiment, the temperature of the adjusting member 10 can be set to 400°C or less, preferably 350°C or less, and more preferably 200°C or less, and polycrystalline silicon can be prevented from precipitating on the adjusting member 10. A thermometer 90 for measuring the temperature of the adjusting member 10 may be installed on the adjusting member 10, and the cooling temperature of the adjusting member 10 by the cooling unit may be controlled by the control unit 50 based on the measurement result of the thermometer 90 (see FIG. 8). The control unit 50 may be capable of communicating with other members such as the liquid supply unit 40 and the gas supply unit 25 in addition to the thermometer 90, and may be capable of controlling the liquid supply unit 40, the gas supply unit 25, and the like.
[0050] By using an apparatus that employs the adjustment member 10, if growth occurs in a structure that is positioned directly above the through hole of the silicon core wire electrode 60, and, for example, the occurrence of popcorn or the shape of the grown rod is undesirable, the positioning can be adjusted to resolve these issues, and the desired polycrystalline silicon can be obtained by continuing growth.
[0051] <method> An example of a method for producing polycrystalline silicon rods using a polycrystalline silicon rod production apparatus will be described.
[0052] Polycrystalline silicon is deposited on the silicon core wire 1 by passing an electric current through the silicon core wire electrode 60. At this time, silane raw material gas is supplied from a supply gas inlet 91 of the raw material gas supply unit, and the silane raw material gas that is not used in the growth of polycrystalline silicon is exhausted from an exhaust gas outlet 96.
[0053] In this process of precipitating polycrystalline silicon, the adjustment member 10 is cooled by a cooling unit. In this case, any one or more of the following mechanisms may be adopted: a mechanism for blowing cooling gas from a nozzle toward the adjustment member 10 as shown in Fig. 6; a mechanism for cooling by the heat dissipation effect of connecting the adjustment member 10 to the bottom plate 80 via a heat dissipation insulating member 30 as shown in Figs. 5 and 6; and a mechanism for indirectly cooling the adjustment member 10 by a cooling liquid.
[0054] When the diameter of the polycrystalline silicon increases or when the polycrystalline silicon rod is cooled, the adjustment member 10 naturally moves within the plane in order to relieve stress, but by employing the cooling section (cooling mechanism) described in this embodiment, the silicon core wire 1 moves smoothly relative to the bottom plate 80. In other words, by employing the cooling section described in this embodiment, it is possible to prevent silicon crystals from precipitating on the adjustment member 10, and as a result, adjustment by the adjustment member 10 can be performed smoothly.
[0055] In addition, after removing the grown polycrystalline silicon rods, a process of generating the next polycrystalline silicon rods (new polycrystalline silicon rods) is performed, but it may be necessary to adjust and move the position of the adjustment member 10 before growing the next polycrystalline silicon. According to this embodiment, since it is possible to prevent silicon crystals from precipitating on the adjustment member 10, even when the position of the adjustment member 10 is adjusted and moved in this way, it is possible to prevent the crystals precipitated on the adjustment member 10 from falling into the furnace during adjustment by the adjustment member 10 and causing contamination, and also to prevent the problem of adjustment by the adjustment member 10 not being performed smoothly. [Industrial Applicability]
[0056] According to this embodiment, the silicon core wire 1 can be placed at an optimal position in the reactor 100, and the desired polycrystalline silicon can be grown based on that position. Moreover, in the process of growing the polycrystalline silicon, the position of the silicon core wire 1 can be moved (adjusted) without any trouble in order to relieve stress generated in the polycrystalline silicon.
Claims
1. A silicon core wire for depositing polycrystalline silicon; A core wire electrode provided to penetrate the bottom plate; an adjustment member provided between the silicon core wire and the core wire electrode and movable with respect to the bottom plate; A cooling unit capable of cooling the adjustment member; Equipped with The cooling unit has a nozzle that blows gas toward the adjustment member.
2. The apparatus for producing polycrystalline silicon rods according to claim 1 , wherein the gas is a silane raw material gas.
3. A silicon core wire for precipitating polycrystalline silicon; A core wire electrode provided to penetrate the bottom plate; an adjustment member provided between the silicon core wire and the core wire electrode and movable with respect to the bottom plate; A cooling unit capable of cooling the adjustment member; Equipped with The cooling unit is provided between the bottom plate and the adjustment member, and has a heat dissipation insulating member for cooling the adjustment member by the bottom plate.
4. A silicon core wire for precipitating polycrystalline silicon; A core wire electrode provided to penetrate the bottom plate; an adjustment member provided between the silicon core wire and the core wire electrode and movable with respect to the bottom plate; A cooling unit capable of cooling the adjustment member; Equipped with The apparatus for manufacturing polycrystalline silicon rods, wherein the adjustment member is made of a material different from that of the core wire electrode.
5. A silicon core wire for precipitating polycrystalline silicon; A core wire electrode provided to penetrate the bottom plate; an adjustment member provided between the silicon core wire and the core wire electrode and movable with respect to the bottom plate; A cooling unit capable of cooling the adjustment member; Equipped with The apparatus for manufacturing polycrystalline silicon rods, wherein the adjustment member has a lower resistivity than the core electrode.
6. The apparatus for manufacturing polycrystalline silicon rods according to any one of claims 1 to 5, wherein the cooling unit is provided in the core electrode and has a flow path for flowing a cooling liquid.
7. 7. The polycrystalline silicon rod manufacturing apparatus according to claim 1, wherein the adjustment member connects the core electrode and the silicon core wire so that a central axis of the core electrode and a central axis of the silicon core wire are different.
8. A method for producing polycrystalline silicon rods using the polycrystalline silicon rod producing apparatus according to any one of claims 1 to 7, A step of depositing polycrystalline silicon on the silicon core wire is provided, The method for producing polycrystalline silicon rods, wherein the adjustment member is cooled by the cooling unit in the step of precipitating the polycrystalline silicon.
Citation Information
Patent Citations
Apparatus for manufacturing polycrystal silicon
JP2006240934A
Carbon electrode and apparatus for manufacturing polycrystalline silicon rod
JP2011111360A
Polysilicon reducing furnace
JP2011231005A
Apparatus and method for producing polycrystalline silicon rod
JP2014101256A
Reactor and corresponding system for polysilicon production
WO2011123998A1