Calcium remover, method for removing calcium ions from treated water, method for producing calcium remover, and method for removing heavy metal ions and calcium ions from heavy metal-containing treated water

A calcium removing agent using phosphate and carbonate ions addresses the challenge of calcium sulfate scale by forming easily removable calcium carbonate and hydroxyapatite, offering cost-effective and efficient scale prevention in water systems.

JP7593826B2Active Publication Date: 2024-12-03DOWA TECH
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2021023202
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-02-17
Publication Date
2024-12-03
Estimated Expiration
2041-02-17

AI Technical Summary

Technical Problem

Calcium sulfate scale is difficult to remove and its formation in industrial and household water systems poses significant challenges, leading to clogging and reduced efficiency, and existing methods are costly and complex.

Method used

A calcium removing agent containing phosphate and carbonate ions is used to react with calcium ions in water, forming insoluble calcium carbonate and hydroxyapatite, which can be easily removed, thereby preventing the formation of calcium sulfate scale.

Benefits of technology

The agent effectively reduces calcium ion levels in water, preventing scale formation at low cost and with reduced equipment complexity, facilitating easy handling and treatment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007593826000001
    Figure 0007593826000001
  • Figure 0007593826000002
    Figure 0007593826000002
  • Figure 0007593826000003
    Figure 0007593826000003
Patent Text Reader

Abstract

To provide an inexpensive method and a calcium removing agent suitable for carrying out the method, possible to reduce an amount of calcium ions in water to be treated containing at least one selected from a group consisting of copper ions, nickel ions and zinc ions, and sulfate ions, calcium ions and water, to a level that can sufficiently suppress a formation of a calcium sulfate scale in the water to be treated.SOLUTION: There is provided a calcium removing agent comprising a phosphate ion source and a carbonate ion source.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a calcium remover, a method for removing calcium ions from water to be treated, a method for producing a calcium remover, and a method for removing heavy metal ions and calcium ions from heavy metal-containing water to be treated. [Background technology]

[0002] Industrial wastewater contains carbonate ions, sulfate ions, calcium ions, etc., and when the amount of these ions exceeds the solubility limit, they precipitate as calcium carbonate or calcium sulfate, forming what is known as scale. Scale can clog pipes or reduce the heat transfer efficiency of pipes. In order to discharge or reuse industrial wastewater, it is necessary to remove harmful substances from the wastewater, and the wastewater becomes concentrated during the removal process, making it more susceptible to the formation of the above-mentioned scale.

[0003] Furthermore, the formation of calcium carbonate scale is also a problem in household water heaters and bathtubs. Thus, the formation of scale is a major problem in a wide range of fields.

[0004] Patent Document 1 (JP Patent Publication No. 2010-275212) discloses that bath additives, which contain carbonate as an essential ingredient and become alkaline when dissolved in bath water, contain calcium ions in tap water (bath water obtained by heating the water), which can form precipitates with the carbonate and cause the formation of scale. The disclosure discloses that trisodium phosphate is added to the bath additive to prevent this.

[0005] Furthermore, Patent Document 2 (JP Patent Publication No. 2003-172593 A) discloses a method for treating cooling water in an open circulating cooling water system capable of preventing scale adhesion, in which hardness components such as calcium in the cooling water are removed by crystallization using seed crystals mainly composed of calcium carbonate or the like.

[0006] Furthermore, calcium carbonate can be dissolved and removed with an acid such as hydrochloric acid, and even if it forms scale, it is a substance that is relatively easy to deal with.

[0007] On the other hand, it is difficult to completely remove calcium sulfate scale using chemicals such as acids, and it is necessary to remove it physically, for example by scraping it off (for example, Patent Document 3 (JP Patent Publication 6-269602 A) discloses a method for removing calcium sulfate scale from an evaporator with a built-in heating element, which comprises one or more steps of (1) heating and drying the scale, (2) cooling the scale and the heating element, (3) washing the scale with a liquid, and then (4) spraying the scale remaining on the end of the heating element with a high-pressure fluid from a nozzle provided on the side of the end of the heating element of the evaporator). Therefore, removing calcium sulfate scale requires a great deal of effort.

[0008] Therefore, it is essential to prevent calcium sulfate scale from forming. For example, Patent Document 4 (JP Patent Publication 7-155558 A) discloses a scale inhibitor that contains a water-soluble organic phosphonate and an N-substituted acrylamide polymer as a scale inhibitor that prevents calcium sulfate scale from forming in the liquid to be treated. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] JP 2010-275212 A [Patent Document 2] JP 2003-172593 A [Patent Document 3] Japanese Patent Application Publication No. 6-269602 [Patent Document 4] Japanese Patent Application Publication No. 7-155558 Summary of the Invention [Problem to be solved by the invention]

[0010] As explained above, calcium sulfate scale is a substance that is very difficult to remove, and it is very important to prevent its generation. For this purpose, it is considered to capture free calcium ions in wastewater and remove them from the wastewater (liquid phase). For example, in the technology described in Patent Document 4, it is considered that a water-soluble organic phosphonate or an N-substituted acrylamide polymer captures calcium ions.

[0011] Although this technique is said to sufficiently suppress the generation of calcium sulfate scale, the chemicals used are expensive, which poses a cost problem.

[0012] The present inventors have now investigated the removal of calcium ions from wastewater that may generate calcium sulfate scale and further contains metal ions such as copper ions that form basic carbonates in the alkaline region. As a result, it was found that calcium ions could not be sufficiently removed even when a large amount of an (inexpensive) carbonate ion source (which reacts with calcium ions to generate calcium carbonate) was supplied to the wastewater. It is desirable to sufficiently prevent the generation of calcium sulfate scale in such wastewater as well.

[0013] Furthermore, if the scale inhibitor is in liquid form, it is easy to add it to various wastewaters and handle it. In particular, when the scale inhibitor is composed of two or more components, it is difficult to uniformly supply them to wastewater from separate supply lines, and the equipment becomes complicated (increasing the equipment costs), so it is desirable to use a liquid form in which the components are dissolved and in a uniform state. Furthermore, if the liquid scale inhibitor can sufficiently prevent the generation of calcium sulfate scale in wastewater by adding a small amount, the amount of liquid required is small, which is advantageous in terms of the load on the equipment for storage, transportation, and the treatment process of wastewater.

[0014] In view of the above, an object of the present invention is to provide an inexpensive method for reducing the amount of calcium ions in treated water containing at least one member selected from the group consisting of copper ions, nickel ions, and zinc ions (metal ions that form basic carbonates), sulfate ions, calcium ions, and water, to a level that sufficiently inhibits the formation of calcium sulfate scale in the treated water, and a calcium remover suitable for carrying out said method.Another object of the present invention is to provide the calcium remover, preferably the calcium remover, which, when in liquid form, allows the amount of liquid to be reduced. [Means for solving the problem]

[0015] In order to solve the above problems, the inventors have conducted extensive research and have found that by supplying phosphate ions and carbonate ions to the water to be treated, the amount of calcium ions in the water to be treated can be reduced inexpensively to a level at which the generation of calcium sulfate scale in the water to be treated can be sufficiently suppressed. The inventors have found that a calcium remover containing a phosphate ion source and a carbonate ion source is suitable for carrying out such a method. Furthermore, the inventors have also found that when potassium carbonate is used as the carbonate ion source, the amount of liquid of the calcium remover can be reduced when it is in liquid form. Based on the above, the inventors have completed the present invention.

[0016] That is, the present invention is as follows. [1] A calcium remover containing a source of phosphate ions and a source of carbonate ions.

[0017] [2] The calcium remover according to [1], wherein the carbonate ion source is an alkali metal salt of carbonate.

[0018] [3] The calcium remover described in [2], wherein the alkali metal is potassium.

[0019] [4] A calcium remover comprising phosphate ions, carbonate ions, metal ions, and water.

[0020] [5] The calcium remover according to [4], having a pH of 8 to 15.

[0021] [6] The calcium removing agent according to [4] or [5], wherein the calcium removing agent contains potassium ions and has a carbonate ion content of 130 g / L to 430 g / L.

[0022] [7] The calcium removing agent according to any one of [4] to [6], wherein the calcium removing agent has a phosphate ion content of 10 g / L to 200 g / L.

[0023] [8] The calcium remover according to any one of [1] to [7], which is used for removing calcium ions from treatment water containing at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water.

[0024] [9] A method for removing calcium ions from water to be treated, comprising supplying phosphate ions and carbonate ions to the water to be treated, the water containing at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water.

[0025]

[10] The method for removing calcium according to [9], wherein the supply of phosphate ions and carbonate ions is carried out by adding a calcium remover according to any one of [1] to [8] to the water to be treated.

[0026]

[11] The method according to [9] or

[10] , wherein the calcium removing agent contains water, and 2 mL to 100 mL of the calcium removing agent is added per 1 L of the water to be treated.

[0027]

[12] The method according to any one of [9] to

[11] , wherein the content of sulfate ions in the water to be treated is 300 mg / L to 60 g / L.

[0028]

[13] The method according to any one of [9] to

[12] , wherein the calcium ion content in the water to be treated is 50 mg / L to 1000 mg / L.

[0029]

[14] The method according to any one of [9] to

[13] , wherein the total content of copper ions, nickel ions and zinc ions in the water to be treated is 10 mg / L to 200 mg / L.

[0030]

[15] The method according to any one of [9] to

[14] , wherein the supply of phosphate ions and carbonate ions is carried out while maintaining the pH of the water to be treated in the range of 8 to 14.

[0031]

[16] The amount of phosphate ions supplied is 0.2 mol to 3 mol per mol of calcium ions in the water to be treated; The method according to any one of [9] to

[15] , wherein the amount of carbonate ions supplied is 0.3 mol to 10 mol per mol of calcium ions in the water to be treated.

[0032]

[17] A method for producing a calcium remover, comprising mixing a phosphate ion source and a carbonate ion source.

[0033]

[18] A method for producing a calcium remover by mixing trisodium phosphate hydrate, potassium carbonate, and water.

[0034]

[19] The method for producing a calcium remover according to

[18] , wherein the amounts of trisodium phosphate hydrate, potassium carbonate and water used are 5 to 30 parts by mass, 5 to 50 parts by mass and 35 to 90 parts by mass, respectively (the total amounts of trisodium phosphate hydrate, potassium carbonate and water used are 100 parts by mass).

[0035]

[20] A method for producing a precipitate containing a hydroxide of a heavy metal by adding a hydroxide ion source to heavy metal-containing water to be treated, the heavy metal-containing water containing at least one selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and heavy metal ions other than copper ions, nickel ions, and zinc ions, and water; The obtained precipitate-containing liquid is subjected to solid-liquid separation to obtain calcium-containing water containing at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water; The calcium-containing water is treated as the water to be treated, and the method for removing calcium ions from the water to be treated according to any one of [9] to

[16] is carried out. A method for removing heavy metal ions and calcium ions from heavy metal-containing treated water.

[0036]

[21] In the heavy metal-containing treated water, The total content of copper ions, nickel ions and zinc ions is 500mg / L to 30g / L; The sulfate ion content is 300mg / L to 60g / L. The calcium ion content is 50mg / L to 1000mg / L. The method for removing iron ions according to

[20] , wherein the iron ion content is 0.2 mg / L to 200 mg / L. Effect of the Invention

[0037] According to the present invention, there are provided an inexpensive method for reducing the amount of calcium ions in treated water containing at least one selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water to a level at which the generation of calcium sulfate scale can be sufficiently suppressed, a calcium remover suitable for carrying out said method, and related techniques.Furthermore, according to a preferred embodiment of the present invention, there are provided the calcium remover, which, when in the form of a liquid, allows the amount of liquid to be reduced, and related techniques. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0038] BEST MODE FOR CARRYING OUT THE DISCLOSURE Hereinafter, embodiments of the calcium remover and its production method, as well as the method for removing calcium ions from water to be treated, of the present invention will be described in detail.

[0039] [Calcium remover] The calcium removing agent of the present invention includes a phosphate ion source and a carbonate ion source. Since the phosphate ion source and the carbonate ion source are inexpensive substances, the calcium removing agent can be provided at low cost. This calcium removing agent is suitably used for removing calcium ions from water to be treated that contains at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water.

[0040] Examples of the phosphate ion source include phosphoric acid and trisodium phosphate hydrate, with trisodium phosphate hydrate being preferred. An example of trisodium phosphate hydrate is dodecahydrate. An example of the carbonate ion source is a metal salt of carbonate. As the metal, an alkali metal is preferred from the viewpoint of the cost of the metal salt of carbonate, and among these, sodium and potassium are more preferred. Potassium carbonate is particularly preferred because it has high solubility in water and has the advantage described below when the calcium remover of the present invention is in the form of a liquid.

[0041] When the calcium remover of the present invention is added to the water to be treated, the phosphate ions, calcium ions, and hydroxide ions (supplied from water or hydroxide) generated from the phosphate ion source react to form hydroxyapatite (hereinafter also referred to as HAP), and the carbonate ions generated from the carbonate ion source react with calcium ions to form calcium carbonate. Since HAP and calcium carbonate are poorly soluble in water, they may form scale in piping, but this can be easily removed with a chemical solution such as hydrochloric acid. As described above, the calcium remover of the present invention fixes calcium ions in the water to be treated as HAP or calcium carbonate, which can be easily removed even if they form scale, thereby removing them from the water to be treated (the liquid phase of the water), thereby preventing the formation of calcium sulfate scale, which is difficult to remove, in the subsequent treatment step (where the water to be treated is further concentrated).

[0042] In addition, since a carbonate ion source is generally cheaper than a phosphate ion source, if calcium ions can be sufficiently removed using a carbonate ion source alone, the carbonate ion source should be used alone without using a phosphate ion source. However, for the water to be treated that contains at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions (which can generate basic carbonates in the alkaline region) that is the subject of the present invention, calcium ions cannot be sufficiently removed by using the above alone, and a phosphate ion source must be used in combination. From the viewpoint of suitably removing calcium ions from the water to be treated, the molar ratio of the phosphate ion source to the carbonate ion source in the calcium remover (phosphate ion source:carbonate ion source) is preferably 1:1 to 1:15, more preferably 1:2 to 1:8.

[0043] When the calcium removing agent of the present invention is in the form of a liquid (liquid agent), the calcium removing agent contains water. A liquid agent is preferable because it is easy to add to the water to be treated and easy to handle.

[0044] In such a calcium removing agent, which is a liquid preparation, phosphate ions are generated from the phosphate ion source, and carbonate ions are generated from the carbonate ion source. Furthermore, the carbonate ion source is typically a metal salt of carbonic acid as described above, and metal ions that serve as counter cations of the carbonate ions are also generated in the calcium removing agent, which is a liquid preparation. When the phosphate ion source is a metal salt, metal ions that serve as counter cations of the phosphate ions are also generated.

[0045] The content of phosphate ions in the calcium remover is preferably 10 g / L to 200 g / L, more preferably 15 g / L to 180 g / L, and particularly preferably 25 g / L to 150 g / L. Increasing the content of phosphate ions in the calcium remover in this manner reduces the amount of calcium remover required to treat the water to be treated (to sufficiently remove calcium ions), which is advantageous in terms of storage and transportation of the liquid agent and the load on the equipment in the treatment process of the water to be treated. On the other hand, from the viewpoint of chemical costs, the content of phosphate ions is preferably 200 g / L or less as described above.

[0046] In addition, when the carbonate ion source is potassium carbonate, carbonate ions and potassium ions are generated in the calcium remover which is a liquid agent, and the content of carbonate ions in the calcium remover is preferably 130 g / L to 430 g / L, more preferably 140 g / L to 430 g / L, and particularly preferably 150 g / L to 430 g / L (the content as potassium carbonate is preferably about 300 g / L to 1000 g / L, more preferably about 320 g / L to 1000 g / L, and particularly preferably about 350 g / L to 1000 g / L). Increasing the content of carbonate ions in the calcium remover in this way reduces the amount of calcium remover required to treat the water to be treated (to sufficiently remove calcium ions), which is advantageous in terms of storage and transportation of the liquid agent and the load on the equipment of the treatment process of the water to be treated. Potassium carbonate as a carbonate ion source has high solubility in water, so such a high content of carbonate ions can be realized. On the other hand, if the carbonate ion concentration exceeds 430 g / L, it approaches the solubility of potassium carbonate and there is a risk of precipitation.

[0047] As described later, in the method of removing calcium ions from water to be treated of the present invention, the pH (reaction pH) of the mixed liquid when the calcium remover is added to the water to be treated and mixed (when HAP and calcium carbonate are produced) is preferably 8 to 14, but it is also preferable for the pH of the calcium remover (which is a liquid agent) itself to be in a similar range of 8 to 15, since this will not cause a large change in the pH of the water to be treated and will allow carbonate ions to exist stably. From the viewpoint of calcium ion removal efficiency, the pH of the calcium remover is more preferably 8.8 to 15, even more preferably 9.5 to 15, and particularly preferably 10.5 to 15.

[0048] The calcium remover of the present invention may contain, in addition to the components described above, for example, sodium hydroxide, in order to adjust the pH of the calcium remover, which is a liquid preparation.

[0049] [Method of producing calcium remover] Next, a method for producing the calcium remover of the present invention will be described. The calcium remover of the present invention can be produced by mixing the active ingredients, a phosphate ion source and a carbonate ion source, by any method. In this case, the ratio of the amounts of the phosphate ion source and the carbonate ion source used (phosphate ion source:carbonate ion source) is preferably 3 parts by mass to 20 parts by mass: 80 parts by mass to 97 parts by mass (the total of both is 100 parts by mass), and more preferably 5 parts by mass to 15 parts by mass: 85 parts by mass to 95 parts by mass (the total of both is 100 parts by mass), from the viewpoint of the efficiency of removing calcium ions from the water to be treated.

[0050] Furthermore, it is preferable that the calcium remover is a liquid. In this case, water is further mixed into the calcium remover. As described above, potassium carbonate can increase the (carbonate ion) content in the calcium remover, which is a liquid, and therefore, in the method for producing a calcium remover, which is a liquid, of the present invention, it is preferable to employ potassium carbonate as the carbonate ion source.

[0051] As mentioned above, the suitable pH of the calcium remover, which is a liquid agent, is in the alkaline range, but when phosphoric acid is used as the phosphate ion source, for example, an alkaline substance such as sodium hydroxide is added to adjust the pH because phosphoric acid is an acidic substance. In that case, a strong exothermic reaction occurs, which raises safety concerns when considering the industrial-scale production of the calcium remover.

[0052] Therefore, in the present invention, it is preferable to use trisodium phosphate hydrate instead of phosphoric acid. When trisodium phosphate hydrate is dissolved in water, no exothermic reaction occurs (a slight endothermic reaction occurs), and the resulting mixed solution is alkaline. As a result, the pH falls within the suitable pH range for the calcium remover without the need for pH adjustment. An example of trisodium phosphate hydrate is the dodecahydrate.

[0053] In addition, the solubility of trisodium phosphate hydrate in water (25°C) is not very high, but it increases significantly when heated (whereas an exothermic reaction may occur spontaneously and be uncontrollable, in the case of heating, the degree of temperature increase can be controlled). And, although the mechanism is unclear, once trisodium phosphate hydrate has dissolved, it is extremely unlikely to precipitate, even if the liquid temperature is lowered.

[0054] The amounts of trisodium phosphate hydrate, potassium carbonate, and water used in producing the liquid calcium remover are as follows: Preferably, the amount is 5 parts by mass to 30 parts by mass, 5 parts by mass to 50 parts by mass, and 35 parts by mass to 90 parts by mass (the total amount of the three is 100 parts by mass), More preferably, the amount is from 10 to 25 parts by mass, from 10 to 40 parts by mass, and from 45 to 80 parts by mass (the total amount of the three used is 100 parts by mass).

[0055] When the amounts of the three components used fall within these ranges, a calcium remover (liquid) having a high content of phosphate ions and carbonate ions can be obtained, which is preferable in terms of the efficiency of removing calcium ions from the treated water and the storage and transportation of the liquid, and is also preferable in terms of placing a small load on the equipment in the treatment process for the treated water.

[0056] In addition, NaOH may be added to the calcium remover to adjust the pH of the calcium remover.

[0057] [Method for removing calcium ions from treated water] Next, a method for removing calcium ions from water to be treated according to the present invention (hereinafter also referred to as removal method 1 of the present invention) will be described. The water to be treated contains at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water, and is at risk of forming calcium sulfate scale.

[0058] In removal method 1 of the present invention, calcium ions are removed by supplying phosphate ions and carbonate ions to the water to be treated. As described above, phosphate ions and carbonate ions can be supplied inexpensively, and react with components in the water to be treated to form calcium carbonate and HAP, preventing the production of calcium sulfate. Carbonate ions can be supplied more inexpensively than phosphate ions, but as described above, in order to sufficiently remove calcium ions from the water to be treated that is the subject of the present invention, it is necessary to use phosphate ions and carbonate ions in combination.

[0059] In typical treated water to be treated by removal method 1 of the present invention, the total content of copper ions, nickel ions and zinc ions is, for example, 10 mg / L to 200 mg / L, and preferably 25 mg / L to 100 mg / L.

[0060] In typical water to be treated that is the target of removal method 1 of the present invention, the sulfate ion content is, for example, 300 mg / L to 60 g / L, and preferably 2000 mg / L to 30 g / L.

[0061] In typical treated water to be treated by removal method 1 of the present invention, the calcium ion content is, for example, 50 mg / L to 1000 mg / L, and preferably 80 mg / L to 500 mg / L.

[0062] The water to be treated by the removal method 1 of the present invention may contain heavy metal ions other than copper ions, nickel ions, and zinc ions. The heavy metals are metals with a specific gravity of 4 or more, and specific examples thereof include tin and iron. The content of iron ions in the water to be treated is, for example, 0.01 mg / L to 50 mg / L (preferably 0.02 mg / L to 35 mg / L).

[0063] An example of the water to be treated as described above is the treated liquid from a factory after heavy metal treatment (in which heavy metal ions including copper, nickel, and zinc are precipitated as hydroxides and removed by filtration, etc.).

[0064] In the removal method 1 of the present invention, phosphate ions and carbonate ions can be suitably supplied by adding the calcium remover of the present invention (preferably in the form of a liquid agent) to the water to be treated.

[0065] From the viewpoint of calcium ion removal efficiency, it is preferable to form HAP and calcium carbonate by supplying phosphate ions and carbonate ions while maintaining the pH (reaction pH) of the water to be treated in the alkaline region. Note that a large amount of chemicals is required to bring the pH into a strongly alkaline region, and even in such a strongly alkaline region, the calcium ion removal efficiency is saturated. For the above reasons, the pH (reaction pH) of the water to be treated is preferably maintained in a range of 8 to 14, more preferably 8.8 to 13.5, even more preferably 9.5 to 13, and particularly preferably 10.5 to 12.5.

[0066] From the viewpoint of calcium ion removal efficiency and chemical costs, the amount of phosphate ions supplied to the water to be treated is preferably 0.2 mol to 3 mol, and more preferably 0.3 mol to 2 mol, per mol of calcium ions in the water to be treated.

[0067] From a similar viewpoint, the amount of carbonate ions supplied to the water to be treated is preferably 0.3 mol to 10 mol, and more preferably 1 mol to 6 mol, per mol of calcium ions in the water to be treated.

[0068] The amount of calcium removing agent (in the form of a liquid agent) added to the water to be treated is preferably 2 mL to 100 mL, more preferably 2 mL to 50 mL, and particularly preferably 2 mL to 20 mL, per 1 L of water to be treated. The calcium removing agent of the present invention, which is a liquid agent, can also impose a burden on the treatment equipment for the water to be treated if the amount of liquid is large. However, as described above, if potassium carbonate is used as the carbonate ion source, the carbonate ion content in the calcium removing agent can be increased, so that the amount of calcium removing agent required to remove calcium from the water to be treated is reduced, and the amount added to the water to be treated can be reduced.

[0069] In the removal method 1 of the present invention, the calcium remover may be added after adding seed crystals such as calcium carbonate to the water to be treated. The amount of seed crystals added is preferably 1 g to 20 g per 1 g of calcium in the water to be treated.

[0070] <Subsequent processing process> In the removal method 1 of the present invention, HAP and calcium carbonate are generated as solids in the water to be treated to which phosphate ions and carbonate ions have been supplied. These are separated by solid-liquid separation, and the liquid component is concentrated, for example, in an evaporative concentration device, and the solid component is dehydrated in a dehydrator. This concentration process is likely to cause calcium sulfate scale to form, but in the present invention, the calcium ions in the water to be treated are sufficiently removed in a previous stage, so that the formation of calcium sulfate scale is prevented. The solids remaining after the above process can be disposed of, for example, as industrial waste, and the water separated from the solids can be reused or discharged.

[0071] [Method for removing heavy metal ions and calcium ions from heavy metal-containing treated water] The removal method 1 of the present invention can be suitably used as a part of the process of the removal method described below. At least one selected from the group consisting of copper ions, nickel ions, and zinc ions; Sulfate ions, Calcium ions, Heavy metal ions other than copper ions, nickel ions and zinc ions; The present invention relates to a method for removing heavy metal ions and calcium ions from heavy metal-containing treatment water that contains calcium ions and calcium ions (hereinafter also referred to as removal method 2 of the present invention).

[0072] As described above, the heavy metals are metals with a specific gravity of 4 or more, and specific examples thereof include tin and iron. The content of iron ions in the heavy metal-containing water to be treated is, for example, 0.2 mg / L to 200 mg / L, and preferably 0.4 mg / L to 150 mg / L.

[0073] In a typical heavy metal-containing water to be treated by the removal method 2 of the present invention, the total content of copper ions, nickel ions, and zinc ions is, for example, 500 mg / L to 30 g / L, and preferably 1000 mg / L to 25 g / L. In a typical heavy metal-containing water to be treated by the removal method 2 of the present invention, the content of sulfate ions is, for example, 300 mg / L to 60 g / L, and preferably 2000 mg / L to 45 g / L. In a typical heavy metal-containing water to be treated by the removal method 2 of the present invention, the content of calcium ions is, for example, 50 mg / L to 1000 mg / L, and preferably 80 mg / L to 500 mg / L.

[0074] In the removal method 2 of the present invention, a hydroxide ion source is added to the heavy metal-containing water to be treated as described above, and the heavy metals are converted into hydroxides and precipitated (if ions of non-heavy metals that easily form hydroxides, such as magnesium, are contained in the heavy metal-containing water to be treated, these also form hydroxides and precipitate). At this time, copper ions, nickel ions, and zinc ions (which are also heavy metals) also form hydroxides and precipitate. From the viewpoint of chemical costs, alkali metal hydroxides such as sodium hydroxide and potassium hydroxide are suitable as the hydroxide ion source. The amount of metal hydroxide to be added is, for example, 0.8 g to 20 g per 1 g of the total of heavy metals, including copper, nickel, and zinc, in the heavy metal-containing water to be treated.

[0075] If necessary, a flocculant such as an anionic flocculant or a nonionic flocculant may be further added to ensure the precipitation of heavy metals, etc. The amount of the flocculant to be added is, for example, an amount such that the content of the flocculant in the heavy metal-containing water to be treated is 1 to 5 mg / L.

[0076] For the precipitate-containing liquid obtained by adding the hydroxide ion source (and, if necessary, a flocculant), solid-liquid separation is performed. For the solid content, a further separation operation may be performed to recover valuable metals. On the other hand, the liquid component is calcium-containing water containing at least one selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water. For the removal of calcium ions therefrom, the method for removing calcium ions from the water to be treated of the present invention described above (Removal Method 1 of the present invention) can be preferably applied.

Examples

[0077] Hereinafter, the present invention will be described in more detail with reference to Examples and Comparative Examples. In the following, various evaluations were carried out by the following methods.

[0078] <Temperature measurement> The liquid temperature was measured using the temperature measurement function of a pH meter (pH meter D-73 manufactured by HORIBA).

[0079] <pH measurement> For the measurement of the pH value, a pH meter D-73 manufactured by HORIBA was used. When the temperature at the time of measurement was 25°C, the actually measured value was adopted. When it was not 25°C, the pH value at 25°C was determined by the calibration function built into the pH measuring device.

[0080] <Measurement of metal element content> The content of metal elements was measured by an inductively coupled plasma optical emission spectrometer (ICP-OES, SPS5100 manufactured by Hitachi).

[0081] <Measurement of sulfate ion content> The content of sulfate ions was measured by an ion chromatography system (ICS-1600 manufactured by Thermo Fisher Scientific). A mixed solution of 2.7M Na2CO3 and 0.3M NaHCO3 was used as the eluent, DIONEX ionPac AS12A was used as the separation column, and ADRS600 was used as the suppressor.

[0082] [Comparative Examples and Reference Examples] Various amounts of sodium carbonate were added to wastewater having the composition shown in Test No. 1 in Table 1 below, and the extent to which calcium ions in the wastewater could be removed was evaluated. In Tests No. 2 to 6, sodium hydroxide was added to the wastewater to adjust its pH to 10. In Tests No. 3 to 6, various amounts of sodium carbonate were added to the wastewater (whose pH had been adjusted to 10), and the wastewater was stirred and mixed for 15 minutes. In Test No. 7, phosphoric acid was further added to the wastewater in Test No. 4. In Tests No. 3 to 7, the pH of the wastewater during stirring and mixing was maintained at 10 by adding sodium hydroxide. In Table 1, the concentration notations such as "1 mmol / L" refer to the amount of sodium carbonate (as carbonate ions) added to 1 L of wastewater.

[0083] [Table 1]

[0084] In Test Nos. 2 to 7, a precipitate was formed by the addition of the agent, so the liquid in which the precipitate was formed was filtered and the amount of calcium ion and copper ion in the filtrate was measured. The results are shown in Table 1.

[0085] From Table 1, it can be seen that in order to remove calcium ions, it is necessary to add a certain amount of carbonate ion source (sodium carbonate), and the calcium removal effect is saturated at 10 mmol / L, and the amount of calcium ions cannot be reduced below 60 mg / L. Furthermore, from Test No. 7, it can be seen that by using a carbonate ion source in combination with phosphoric acid, calcium ions can be sufficiently reduced even in wastewater containing copper. The solubility of sodium carbonate in water is 22 g / 100 g water (25°C), and when trying to make sodium carbonate into a liquid, the maximum concentration is 220 g / L (the content of carbonate ions is about 125 g / L). In general, increasing the temperature of the solvent increases the solubility of the solute, but in the case of sodium carbonate, carbon dioxide gas is generated.

[0086] [Preparation Example 1] 8.6 g of an 85% by mass aqueous solution of phosphoric acid was added to 70 g of pure water (pH 7) and mixed. The pH of the resulting mixture was 1.83 and the temperature was 26.2°C.

[0087] Next, 9 mL of a 48% by mass aqueous solution of sodium hydroxide was added to this mixture and mixed, causing heat generation and raising the temperature of the mixture to 51.5° C. The pH of the mixture at this time was 10.21.

[0088] The mixed liquid was allowed to naturally dissipate heat and cooled to 25.1°C, and 50g of potassium carbonate was added to the mixed liquid and mixed to prepare a calcium remover. The temperature of the resulting calcium remover was 40°C and the pH was 12.3. 25g of water was added to this to adjust the liquid volume to 125mL. The final calcium remover 1 (pH was 12.3) had a phosphoric acid content of 58.5g / L (phosphate ion content of 56.7g / L) and a potassium carbonate content of 400g / L (carbonate ion content of 174g / L).

[0089] [Preparation Example 2] 114 g of trisodium phosphate dodecahydrate (Fujifilm Wako Pure Chemical Industries, Ltd.) was added to 300 g of pure water (pH 7, temperature 23°C) and mixed. An endothermic reaction occurred, and the temperature of the resulting mixture was 19.9°C. The pH of the mixture was 14. Note that the amount of trisodium phosphate dodecahydrate added here exceeded its solubility in water at a water temperature of about 20°C, so some of the powder did not dissolve.

[0090] 200 g of potassium carbonate was added to this mixture and mixed to prepare a calcium remover. The pH of the resulting calcium remover was 15 and the temperature was 40.5°C. The heat generated at this time caused the remaining trisodium phosphate dodecahydrate to completely dissolve.

[0091] To the liquid to which the potassium carbonate had been added, 100 g of water was added to adjust the volume to 500 mL. The final pH of Calcium Remover 2 was 14.6, the temperature was 38.7°C, the phosphate ion content (derived from trisodium phosphate dodecahydrate) was 57 g / L, and the potassium carbonate content was 400 g / L (the carbonate ion content was 174 g / L).

[0092] In the following Examples and Comparative Examples, this calcium removing agent 2 was used as the calcium removing agent.

[0093] [Example 1] The raw water (heavy metal-containing water to be treated) was a factory wastewater with the composition shown in Table 2. The pH of this raw water was 5.19.

[0094] [Table 2]

[0095] When 10.6 mL of 48% by mass sodium hydroxide aqueous solution was added to 2.2 L of this raw water, the pH of the raw water became 11, and a precipitate (presumably containing hydroxides of copper, nickel, zinc, and other heavy metals) was formed.

[0096] This raw water was filtered, and calcium chloride was added to the filtrate. Filtrate A (treated water) had a calcium ion content of 325 mg / L and was used to evaluate the calcium ion removal ability of calcium remover 2 (the composition of filtrate A is shown in Table 3 below).

[0097] Calcium removing agent 2 was added to the filtrate A at a ratio of 6 mL / L and 8 mL / L (calcium removing agent 2 / filtrate A) of the volume of calcium removing agent 2 to the volume of filtrate A, and mixed to fix calcium as calcium carbonate or hydroxyapatite. During this fixation reaction, the pH of the mixture was maintained at 12 by adding a 48 mass% aqueous sodium hydroxide solution as necessary.

[0098] The mixed liquid containing precipitates of calcium carbonate and the like was filtered, and the metal component content of the obtained filtrate B was measured. The results are shown in Table 3 below, along with the measurement results of the metal component content of filtrate A. The sulfate ion content of filtrate A and filtrate B obtained by adding calcium remover 2 at a rate of 8 mL / L were also measured, and the results are also shown in Table 3.

[0099] [Table 3]

[0100] It can be seen that calcium ions in filtrate A were sufficiently removed by adding the calcium removing agent of the present invention.

[0101] [Example 2] The industrial wastewater used in Example 1 was used as raw water (heavy metal-containing water to be treated). A 48% by mass aqueous solution of sodium hydroxide was added to 1 L of this raw water to adjust the pH of the raw water to 8. As a result, a precipitate (presumably containing hydroxides of heavy metals) was formed.

[0102] An anionic flocculant (Acofloc A-150 MT Aquapolymer Co., Ltd.) and a nonionic flocculant (Acofloc N-100 MT Aquapolymer Co., Ltd.) were added to the raw water in which the precipitate had formed, and the contents of each in the raw water were adjusted to 2 mg / L, and the mixture was mixed to cause further precipitation.

[0103] The raw water containing this precipitate was filtered. The calcium ion content in the obtained filtrate C (treated water) was 129 mg / L. Calcium carbonate was added as seed crystals to this filtrate C at a ratio of 2 g per 1 L of filtrate C.

[0104] 10 mL of calcium remover 2 was added to 1 L of filtrate C to which calcium carbonate had been added, and then the mixture was divided into 4 portions of approximately 250 mL each. The pH was adjusted to 9, 10, 11, and 12, respectively, and the mixture was allowed to react for 15 minutes.

[0105] The mixed liquid in which precipitates such as calcium carbonate had formed was filtered, and the calcium ion content of the obtained filtrate D was measured. The results are shown in Table 4 below, along with the measurement result of the calcium ion content of filtrate C.

[0106] [Table 4]

[0107] It can be seen that calcium ions in filtrate C were sufficiently removed by adding the calcium removing agent of the present invention.

Claims

1. 1. A calcium removing agent comprising a source of phosphate ions and a source of carbonate ions, the carbonate ion source is an alkali metal salt of carbonate; The present invention is used for removing calcium ions from water to be treated, the water containing at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water; The content of sulfate ions in the water to be treated is 300 mg / L to 60 g / L, The total content of copper ions, nickel ions and zinc ions in the treated water is 10 mg / L to 200 mg / L. Calcium remover.

2. 2. The calcium removing agent according to claim 1, wherein the alkali metal is potassium.

3. A calcium remover comprising: phosphate ions; carbonate ions obtained by using an alkali metal salt of carbonate as an ion source; metal ions; and water, The present invention is used for removing calcium ions from water to be treated, the water containing at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water; The content of sulfate ions in the water to be treated is 300 mg / L to 60 g / L, The total content of copper ions, nickel ions and zinc ions in the treated water is 10 mg / L to 200 mg / L. Calcium remover.

4. The calcium removing agent according to claim 3, which has a pH of 8 to 15.

5. 5. The calcium removing agent according to claim 3, wherein the calcium removing agent contains potassium ions and the content of carbonate ions in the calcium removing agent is 130 g / L to 430 g / L.

6. 6. The calcium removing agent according to claim 3, wherein the calcium removing agent has a phosphate ion content of 10 g / L to 200 g / L.

7. A method for removing calcium ions from water to be treated, comprising the steps of: supplying phosphate ions and carbonate ions obtained by using an alkali metal salt of carbonate as an ion source to water to be treated, the water containing at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water; The content of sulfate ions in the water to be treated is 300 mg / L to 60 g / L, The total content of copper ions, nickel ions and zinc ions in the treated water is 10 mg / L to 200 mg / L. A method for removing calcium ions from treated water.

8. The method for removing calcium according to claim 7, wherein the supply of phosphate ions and carbonate ions is carried out by adding the calcium remover according to any one of claims 1 to 6 to the water to be treated.

9. 9. The method according to claim 8, wherein the calcium removing agent contains water, and 2 mL to 100 mL of the calcium removing agent is added per 1 L of the water to be treated.

10. The method according to any one of claims 7 to 9, wherein the calcium ion content in the water to be treated is 50 mg / L to 1000 mg / L.

11. The method according to any one of claims 7 to 10, wherein the supply of the phosphate ions and carbonate ions is carried out while maintaining the pH of the water to be treated in the range of 8 to 14.

12. the amount of phosphate ions supplied is 0.2 mol to 3 mol per mol of calcium ions in the water to be treated; The method according to any one of claims 7 to 11, wherein the amount of carbonate ions supplied is 0.3 mol to 10 mol per mol of calcium ions in the water to be treated.

13. A method for producing a calcium remover, comprising mixing a phosphate ion source with an alkali metal salt of carbonate, which is a carbonate ion source, The calcium remover is used for removing calcium ions from water to be treated, which contains at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water; The content of sulfate ions in the water to be treated is 300 mg / L to 60 g / L, The total content of copper ions, nickel ions and zinc ions in the treated water is 10 mg / L to 200 mg / L. A method for producing a calcium remover.

14. A method for producing a calcium remover, comprising mixing trisodium phosphate hydrate, potassium carbonate, and water, The calcium remover is used for removing calcium ions from water to be treated, which contains at least one ion selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, and water; The content of sulfate ions in the water to be treated is 300 mg / L to 60 g / L, The total content of copper ions, nickel ions and zinc ions in the treated water is 10 mg / L to 200 mg / L. A method for producing a calcium remover.

15. The method for producing a calcium remover according to claim 14, wherein the amounts of trisodium phosphate hydrate, potassium carbonate and water used are 5 to 30 parts by mass, 5 to 50 parts by mass and 35 to 90 parts by mass, respectively (the total amounts of trisodium phosphate hydrate, potassium carbonate and water used is 100 parts by mass).

16. A hydroxide ion source is added to heavy metal-containing water to be treated, the heavy metal-containing water containing at least one selected from the group consisting of copper ions, nickel ions, and zinc ions, sulfate ions, calcium ions, heavy metal ions other than copper ions, nickel ions, and zinc ions, and water, to form a precipitate containing a hydroxide of the heavy metal; the obtained precipitate-containing liquid is subjected to solid-liquid separation to obtain calcium-containing water containing at least one ion selected from the group consisting of copper ions, nickel ions and zinc ions, sulfate ions, calcium ions and water, the calcium-containing water having a sulfate ion content of 300 mg / L to 60 g / L and a total content of copper ions, nickel ions and zinc ions of 10 mg / L to 200 mg / L; The calcium-containing water is treated as the water to be treated, and the method for removing calcium ions from the water to be treated according to any one of claims 7 to 12 is carried out. A method for removing heavy metal ions and calcium ions from heavy metal-containing treated water.

17. In the heavy metal-containing water to be treated, The total content of copper ions, nickel ions and zinc ions is 500 mg / L to 30 g / L, The content of sulfate ions is 300 mg / L to 60 g / L, The calcium ion content is 50 mg / L to 1000 mg / L, The method according to claim 16, wherein the iron ion content is 0.2 mg / L to 200 mg / L.

Citation Information

Patent Citations

  • JP1974121359A

  • Method for preventing orainage removing device from scale

    JP1977030060A

  • Device and method for removing calcium sulfate scale from evaporation device

    JP1994269602A

  • Method of preventing formation of scale and / or dispersing iron in reverse osmosis device

    JP1995155558A

  • Cooling water processing method and device for open-type circulating cooling water system

    JP2003172593A