Press die manufacturing method

The method addresses human error and individual differences in press mold manufacturing by using CAD-defined cutting planes and automated welding, achieving consistent quality and reduced costs.

JP7594074B1Active Publication Date: 2024-12-03G TEKT CORPORATION
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023189144
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-11-06
Publication Date
2024-12-03
Estimated Expiration
2043-11-06

AI Technical Summary

Technical Problem

Existing press mold manufacturing methods are prone to human errors and individual differences, leading to increased costs and reduced wear resistance due to inaccurate machining of hardened portions.

Method used

A method involving four processing steps to manufacture a press mold with a hardened portion, using CAD-defined cutting planes and ruled surfaces to ensure precise machining, and automation of overlay welding to minimize human error and waste.

Benefits of technology

The method stabilizes the quality of press molds by reducing human error and optimizing material usage, ensuring consistent wear resistance and cost-effectiveness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007594074000001_ABST
    Figure 0007594074000001_ABST
Patent Text Reader

Abstract

To provide a manufacturing technique for a press die having a hardened portion, which is less susceptible to personal differences or human error. [Solution] In Fig. 3(a), a first intermediate product 31 is obtained. This first intermediate product 31 includes a soft bow cross section portion 11a. In Fig. 3(b), a second intermediate product 32 including a cut surface 14 is obtained by cutting away the soft bow cross section portion 11a. In Fig. 3(c), a padding portion 15 is formed on the cut surface 14. In Fig. 3(e), a press die 10 is obtained by cutting away the excess pad (Fig. 3(c), reference numeral 16).
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a manufacturing technique for a press die having a partially hardened portion. [Background technology]

[0002] Press dies are used to draw, cut, and bend blank materials. The blank material is a flat metal plate and is sufficiently hard. Therefore, when the pressing process is repeated, the corners and protrusions of the press die wear out before the other surfaces (general surfaces).

[0003] As one of the countermeasures, a hardened portion having a harderness higher than that of the general surface has been formed partially at the corners (for example, see Patent Document 1 (FIG. 2) in the case of cutting).

[0004] Patent Document 1 will be explained with reference to the following figure. 11(a) to (d) are diagrams illustrating a conventional method for manufacturing a press die. A block of spheroidal graphite cast iron is machined to prepare a base material 101 for a die. This base material 101 is machined to have a notch 102 with a triangular cross section at one corner.

[0005] In FIG. 11( a ), a base material 104 is attached to a cut surface 103 of a cutout portion 102 . In FIG. 11(b), high speed steel 105 is build-up welded onto base material 104.

[0006] In FIG. 11(c), the build-up welded high speed steel 105 is shaped by machining. In Fig. 11(d), the shaped high speed steel 105 is heated by a halogen lamp 106. The high speed steel 105 is subjected to heat treatment by heating and cooling.

[0007] As a result of the above, a press die 100 is provided in which high speed steel 105 is attached to the corners of a base material 101 made of spheroidal graphite cast iron. High speed steel 105 has the advantage of being much harder and less prone to wear than spheroidal graphite cast iron.

[0008] However, the press die 100 according to the conventional technology has the following problems. In FIG. 11(a), a cutout portion 102 having a triangular cross section is formed by hand or by an NC machine tool (machining center), a milling machine, or the like. When done by humans, over-cutting or under-cutting inevitably occurs due to personal differences. When using NC machine tools (machining centers) or milling machines, human error can occur when inputting data. This error inevitably results in over-cutting or under-cutting.

[0009] In FIG. 11(a), when h is too large, that is, when the die is cut too much, the required amount of high speed steel 105 increases. High speed steel 105 is more expensive than die base material 101. As a result, the manufacturing cost of press die 100 increases. The cut base material becomes waste material, which is not environmentally friendly. In FIG. 11(a), when h is too small, that is, when cutting is insufficient, the amount of high speed steel 105 decreases, and the wear resistance performance decreases.

[0010] However, not only the trimming portion (the notch portion 102 to be cut) but also the press portion that forms the design line, the outline, the uneven shape, and the outer shape, are required to have manufacturing techniques that are less prone to personal differences or human errors while reducing manufacturing costs and improving wear resistance. 。 However, while there is a need to reduce manufacturing costs and maintain wear resistance, there is a demand for manufacturing techniques that are less prone to personal differences or human error. [Prior art documents] [Patent documents]

[0011] [Patent Document 1] Patent No. 6118625 Summary of the Invention [Problem to be solved by the invention]

[0012] An object of the present invention is to provide a manufacturing technique for a press die having a partially hardened portion that is less susceptible to personal differences or human error. [Means for solving the problem]

[0013] The invention according to claim 1 is a method for manufacturing a press die comprising a base material and a hardened portion locally provided on the base material, the base material has a flat first surface and a flat second surface different from the first surface; The hardened portion is provided between the first surface and the second surface, and Outer curved ridge It is composed of the press die is shown by a wire frame, and the wire frame is defined by vertices which are points on a screen, ridge lines each connecting two of the vertices by a straight line or a curved line, wires connecting a plurality of the ridge lines in series, and a skeleton structure constituted by a plurality of the wires; A vertex at a joint between a straight edge line passing through the first surface and the curved edge line connected to the straight edge line is defined as a first inflection point, and a vertex at a joint between a straight edge line passing through the second surface and the curved edge line connected to the straight edge line is defined as a second inflection point, and when a cut surface is defined by a straight line connecting the first inflection point and the second inflection point, Processed into a shape that matches the press die was done a first processing step for obtaining a first intermediate product; The first intermediate product Same shape as the hardened part Soft bow cross section Along the cut surface By removing it, The above A second processing step of obtaining a second intermediate product including a cut surface; A third processing step of providing a padding portion having a cross-sectional shape in which excess material is added to the soft bow cross-section by providing a padding portion to the cut surface of the second intermediate product using a material having a higher hardness than the base material, and obtaining a third intermediate product having a padding portion having a cross-sectional shape in which excess material is added to the soft bow cross-section; The third intermediate Goods? and others The above A fourth processing step of obtaining the press die by removing the excess material. The present invention provides a method for manufacturing a press die comprising the steps of:

[0016] Claim 2 The present invention relates to a method for manufacturing a press die as described in claim 1, The base material is made of carbon steel for machine construction, and the hardened portion is made of high-speed tool steel.

[0020] Claim 3 The present invention relates to a method for manufacturing a press die as described in claim 1, The excess pad includes a protruding portion that protrudes from the bottom of the soft bow cross-section portion onto the first surface and the second surface.

[0021] Claim 4 The invention according to claim 1 The press die manufacturing method according to the present invention comprises the steps of: The cutting surface is a ruled surface formed on the wire frame, and in the second processing step, processing is performed based on ruled surface processing data created based on the ruled surface.

[0022] Claim 5 The invention according to claim 4 The press die manufacturing method according to the present invention comprises the steps of: The padding is formed based on padding data that is created by adding excess padding to the soft bow cross section formed on the wire frame.

[0023] Claim 6 The invention according to claim 5 The press die manufacturing method according to the present invention comprises the steps of: The deposition data is stored in a control unit, and deposition welding is performed based on the deposition data stored in the control unit. Effect of the Invention

[0024] In the invention according to claim 1, the press die is shown as a wireframe by CAD, and the cutting surface is determined by a straight line connecting the first inflection point and the second inflection point. As a result, the cutting surface is uniquely determined, leaving no room for personal differences or human error. In addition, In the invention according to claim 1, the first intermediate product obtained in the first processing step has the same shape as the press die which is the final product. That is, the first intermediate product has a soft bow cross section between the flat first surface and the flat second surface. The boundary between the first and second surfaces and the soft bow cross section is visible. In cutting by a person, cutting can be stopped when the boundary is reached, so there is no risk of over-cutting or under-cutting. In other words, because the boundary is clear, there is no risk of problems due to individual differences.

[0025] In addition, NC data can be easily created using data on the first and second surfaces and the surface (machined surface) of the cross section of the soft bow. When cutting with an NC machine (machining center) or milling machine using this NC data, human error is less likely to occur, and by managing the data on the surface (machined surface) with a computer, the amount of cutting and the amount of build-up can be stabilized, stabilizing quality. In addition, the quality of the mold can be ensured when multiple identical molds are manufactured. Therefore, the present invention provides a manufacturing technique for a press die having a partially hardened portion, which is less prone to personal differences or human error and can stabilize quality.

[0026] Furthermore, since the first intermediate product has the same shape as the press die which is the final product, the shape of the first intermediate product is uniquely determined, and the first intermediate product can be easily manufactured.

[0029] Claim 2 In the invention according to the present invention, the base material is made of carbon steel for machine construction, and the hardened portion is made of high-speed tool steel. Carbon steel for machine construction is more flexible and ductile than high-speed tool steel, so it can obtain a hardness (e.g., HRC60 or higher) that is sufficient to withstand the wear associated with press working without heat treatment.

[0033] Claim 3 In the invention according to claim 1, the excess metal includes an overhanging portion that overhangs the first and second surfaces. The presence of the overhanging portion enables the boundary between the hardened portion and the base material to be finished into a smooth, continuous surface without steps in the fourth processing step.

[0034] Claim 4 In the invention according to the present invention, in the second processing step, processing is performed based on ruled surface processing data created based on the ruled surface. When the ruled surface processing data is created, high hardness materials can be overlaid by laser welding, gas welding, or arc welding. Welding can be performed by humans, robots, or multi-tasking machines such as 3D printers.

[0035] Claim 5 In the invention according to the present invention, the build-up is formed based on build-up data that is created by adding excess metal to the soft bow cross section formed on the wire frame. This makes it possible to automate build-up welding even for press dies with complex shapes.

[0036] Claim 6 In the invention according to the present invention, the deposition data is stored in the control unit, and deposition welding is performed based on the deposition data stored in the control unit. Since deposition welding is performed based on the deposition data, precise deposition welding is performed. Since the deposition welding is precise, wasteful use of expensive high-hardness materials is prevented, and manufacturing costs are optimized. [Brief description of the drawings]

[0037] [Figure 1] FIG. 2 is a perspective view of a main part of the press die according to the present invention. [Diagram 2] FIG. 2 is an enlarged view of part 2 of FIG. [Diagram 3] 1(a) to 1(e) are diagrams illustrating a method for manufacturing a press die according to the present invention. [Figure 4] 13(a) to 13(e) are diagrams for explaining a wire frame, and 13(f) and 13(g) are diagrams for explaining a ruled surface. [Diagram 5] FIG. 1 is a diagram illustrating the implementation of the present invention in a general diagram. [Figure 6] 13(a) and 13(b) are diagrams illustrating an example in which a groove is provided on the cut surface. [Figure 7] 1, and (b) is a cross-sectional view taken along line b-b in (a). [Figure 8] 13(a) and 13(b) are diagrams illustrating an example in which two rigid bow cross-sections are arranged close to each other. [Figure 9] FIG. 1 is a diagram illustrating the principle of a build-up welding device. [Figure 10] FIG. 1 is a flow diagram illustrating ruled surface processing and overlay welding. [Figure 11] 1(a) to 1(d) are diagrams illustrating a conventional method for manufacturing a press die. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0038] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of the present invention will now be described with reference to the accompanying drawings. EXAMPLES

[0039] [Press mold] As shown in FIG. 1, a press die 10 is made up of a base material 11 which occupies the majority of the die, and a hardened portion 20 which is locally provided on the base material 11. The hardened portions 20 are provided in principle at the corners or protruding portions of the press die 10.

[0040] Generally, one press die 10 is provided with a plurality of stripes or a plurality of hardened portions 20 . When it is necessary to distinguish between locations, they are distinguished by adding letters, such as one hardened portion 20A and the adjacent hardened portion 20B. The basic shape of the hardened portion 20 is illustrated in FIG.

[0041] [Base material] 2, the base material 11 has a flat first surface 12 and a flat second surface 13 different from the first surface 12. The material of the base material 11 will be described later.

[0042] [Hardened part] The hardened portion 20 is provided between the first surface 12 and the second surface 13, and is composed of a hard bow cross section 21 whose cross section has the shape of a bow including a string. T is the maximum thickness of the hard bow cross section 21. The material of the hardened portion 20 will be described later. A method for manufacturing the press die 10 having the above configuration will be described in detail with reference to FIG.

[0043] [Press die manufacturing method] FIG. 3(a) shows the first processing step. ,figure Processed into a shape following the press die 10 shown in 2 was done A first intermediate product 31 is obtained.

[0044] The first intermediate product 31 has a soft bow cross section 11a at a corner. The soft bow cross section 11a has the same shape as the hard bow cross section (FIG. 2, reference numeral 21). Since the shape is modeled after the press die, the data of the press die (FIG. 2, reference numeral 10) which is the final product can be used as is, which makes it easy to manufacture the first intermediate product 31.

[0045] 3(b) shows the second processing step, in which the soft bow cross section portion 11a is cut out from the first intermediate product 31. As a result, a second intermediate product 32 including a cut surface 14 can be obtained.

[0046] 3(c) shows the third processing step, in which a padding portion 15 is formed on the cut surface 14. The padding portion 15 has a shape in which an excess pad 16 is added to the soft bow cross section portion 11a. In addition, the padding portion 15 is made of a material harder than the base material.

[0047] [Base material material] The base material is preferably carbon steel for machine construction as specified in JIS G 4051 or an equivalent carbon steel. Carbon steel for machine construction is less expensive than high-speed tool steel, has flexible ductility, and has a hardness (e.g., HRC60) that can withstand wear during press processing even without heat treatment. HRC stands for Rockwell C scale hardness. Although S10C to S58C are standardized for carbon steel for machine construction, S50C, which has a C (carbon) content of 0.50%, is superior in terms of strength and hardness and is more suitable for the base material.

[0048] [Materials with higher hardness than the base material] The material that is harder than the base material is preferably high-speed tool steel as specified in JIS G 4403 or an equivalent steel. High-speed tool steel has a hardness after heat treatment that is higher than S50C, and can be expected to be about HRC65. This is because the higher the hardness, the better the wear resistance.

[0049] [Welding] For build-up welding, arc welding using a welding rod, laser welding using welding powder (powder of high-speed tool steel or equivalent steel, the same applies below), etc. can be used. The latter (laser welding using welding powder) is more preferable. The welding powder is arranged in an orderly manner on the cut surface (ruled surface) and melted by the heat of the laser (plasma arc heat). The amount of welding powder used can be optimized. Compared to excessive use, the amount of welding powder used can be reduced, and the amount of carbon dioxide generated can be reduced. Therefore, laser welding using welding powder enables environmentally friendly production (manufacturing), which is more preferable. Laser welding using welding powder will be described later with reference to FIG. 9.

[0050] [Protruding part] Although it is optional, as shown in FIG. 3(d), the excess pad 16 includes a protruding portion 17 that protrudes onto the second surface 13 (and the first surface 12). The extension length L of the extension portion 17 may be about 0.1 to 0.5 mm. The thickness of the extension portion 17 may be the thickness of the first layer when the welding powder is laminated.

[0051] Due to the presence of the overhanging portion 17, the boundary between the hardened portion 20 and the base material 11 can be finished into a smooth continuous surface without steps in the fourth processing step shown in FIG. 3(e).

[0052] In addition, due to an insufficient amount of padding, a V-shaped depression (notch) may occur at the boundary between the hard bow cross section 21 and the second surface 13 (or the first surface 12). If left unattended, this V-shaped notch becomes the starting point of fatigue fracture, which is undesirable. In this regard, the provision of the overhanging portion 17 has the advantage of more reliably preventing the occurrence of notches.

[0053] 3(e) shows a fourth processing step, in which the excess metal 16 shown in FIG. 3(c) is cut away to obtain the press die 10. This press die 10 has the same shape as that shown in FIG.

[0054] The first intermediate product 31 shown in Fig. 3(a) has the same shape as the press die (Fig. 2, reference numeral 10) which is the final product. That is, the first intermediate product 31 has a soft bow cross section 11a between the flat first surface 12 and the flat second surface 13, and the boundary between the first and second surfaces 12, 13 and the soft bow cross section 11a is an inflection point where a straight line changes to a curve, so it is visible. In cutting by a person, cutting can be stopped when the boundary is reached, so there is no risk of over-cutting or under-cutting. In other words, because the boundary is clear, there is no risk of problems due to individual differences.

[0055] In addition, NC data can be easily created using data on the first and second faces 12, 13 and the surface (machined surface) of the soft bow cross section portion 11a. When cutting with an NC machine tool (machining center) or milling machine using this NC data, human error is unlikely to occur, and by managing the data on the surface (machined surface) by computer, the amount of cutting and the amount of padding can be stabilized, stabilizing quality. In addition, the quality of the mold can be ensured when multiple identical molds are manufactured. Therefore, the present invention provides a manufacturing technique for a press die 10 having a partially hardened portion 20 that is less prone to personal differences or human error and can stabilize quality.

[0056] Incidentally, the specification or setting of the cutting plane 14 described in Fig. 3(b) is important. This specification or setting can be done in both a wireframe created by CAD (computer-aided design) and a general drawing. Below, we will explain each of these in turn.

[0057] Wireframe The wire frame will be explained based on Figs. 4(a) to (e), and the ruled surface corresponding to the cut surface will be explained based on Figs. 4(f) and (g). A ruled surface is a CAD term, written as "ruled surface" in English, and refers to a surface surrounded by a specific group of edges (the definition of edges will be described later). Since edges appear on the surface, a ruled surface is the same as a ruled surface.

[0058] 4(a) shows a vertex 35. This vertex 35 is a point set on a CAD screen. 4(b) shows a straight edge 36. This edge 36 is a line in which two vertices 35 are connected by a straight line. 4(c) shows a curved edge 37. This edge 37 is a line in which two vertices 35 are connected by a curve. The curve is defined by a radius of curvature R.

[0059] 4(d) shows a wire 38. The wire 38 is a bent line or a meandering line in which straight edge lines 36 are connected in series, or curved edge lines 37 are connected in series, or a straight edge line 36 and a curved edge line 37 are connected in series. 4(e) shows a wire frame 39. The wire frame 39 is a skeletal structure in which a plurality of wires 38 are arranged in a lattice pattern.

[0060] [Rule surface] In FIG. 4(d), the vertical edge 36 is interpreted as a linear edge 36v passing through the first surface, and the horizontal edge 36 is interpreted as a linear edge 36h passing through the second surface. Then, a vertex 35 existing at the joint between a straight edge line 36v passing through the first face and a curved edge line 37 connected to this straight edge line 36v is determined as a first inflection point 41. Similarly, a vertex 35 existing at the joint between a straight edge line 36h passing through the second face and a curved edge line 37 connected to this straight edge line 36h is defined as a second inflection point 42.

[0061] Next, as shown in Fig. 4(f), the first inflection point 41 and the second inflection point 42 are connected by a line 43. This line 43 corresponds to the bowstring of the soft bow cross section portion 11a shown in Fig. 3(a), and also corresponds to the cut surface 14 shown in Fig. 3(b). When the two-dimensional display of FIG. 4(f) is converted into a three-dimensional display, it becomes FIG. 4(g).

[0062] 4(g), a surface surrounded by a line 43 connecting the first inflection point 41 and the second inflection point 42, the wires 38, 38 perpendicular to this line 43 (including substantially perpendicular thereto), and a line 44 at the back forms a ruled surface 45. This ruled surface 45 corresponds to the cut surface 14.

[0063] As described above, the press die is shown by the wire frame 39 created by CAD, and the bowstring for the soft bow cross section is determined by the line 43 connecting the first inflection point 41 and the second inflection point 42. As a result, the cut surface 14 is uniquely determined, leaving no room for personal differences or human error.

[0064] [General Drawing] Fig. 5 is a re-illustration of Fig. 2 (however, the reference numerals are different), and is a general drawing showing a cross section of a main part of a press die. The cutting plane 14 can be specified or set based on such Fig. 5. 5, a point at one end of the first surface 12 where the straight line changes to a curve is defined as a first inflection point 41. Similarly, a point at one end of the second surface 13 where the straight line changes to a curve is defined as a second inflection point . Next, the first inflection point 41 and the second inflection point 42 are connected by a line 43. This line 43 corresponds to the string of the bow and also corresponds to the cut surface 14.

[0065] Therefore, the method of the present invention can be easily implemented using either CAD or general drawings.

[0066] In Fig. 2, if the maximum thickness T of the hard bow cross section 21 is less than a predetermined value (for example, 1.0 mm), the hardened portion 20 may peel off from the base material 11. A countermeasure to this will be described with reference to Figs. 6(a) and (b).

[0067] [Grooves on cutting surface] As shown in FIG. 6(a) or FIG. 6(b), when the maximum thickness T of the hard bow cross section 21 (or more precisely, the soft bow cross section 11a) is less than a predetermined value, a gutter-like groove 47 is formed on the cut surface 14, and a part of the hardened portion 20 is accommodated in this groove 47. Since the part of the hardened portion 20 that is accommodated exerts an anchoring effect, the bonding strength of the hardened portion 20 to the base material 11 is increased.

[0068] The cross-sectional shape of the groove 47 is arbitrary, but may be an arched cross section as shown in FIG. 6(a), and if the cross section is an arched cross section, the groove 47 can be easily formed by machining. Alternatively, as shown in Figure 6(b), the groove 47 may be of rectangular cross-section, which, although slightly more difficult to machine, provides stronger anchoring action than an arcuate cross-section. Therefore, the cross-sectional shape of the groove 47 may be determined taking into consideration cost-effectiveness.

[0069] 1 is provided with an island-shaped protrusion 48. The present invention can also be applied to this island-shaped protrusion 48.

[0070] [Island hardened area] FIG. 7(a) is an enlarged view of portion 7a in FIG. As shown in FIG. 7(a), the island-shaped protrusions 48 are formed into island-shaped hardened portions 20C according to the present invention. FIG. 7(b) is a cross-sectional view taken along line b-b in FIG. 7(a), and the island-shaped hardened portion 20C is a hard bow cross-sectional portion 21 formed between the first surface 12 and the second surface 13. Therefore, the hardened portion (FIG. 1, reference numeral 20) according to the present invention may be an island-shaped protrusion in addition to a ridge.

[0071] In FIG. 1, a hardened portion 20A may be located very close to an adjacent hardened portion 20B. That is, as shown in Fig. 8(a), a certain hardened portion 20A is placed in close proximity to an adjacent hardened portion 20B. In this case, the configuration shown in Fig. 8(b) can be adopted.

[0072] [Two-humped camel] As shown in FIG. 8(b), the hardened portion 20 is formed with two hard arch cross-section portions 21 merging together like the humps of a Bactrian camel.

[0073] 8(a), of the two inflection points 41, 42 of a certain hardened portion 20A, the one farther from the adjacent hardened portion 20B is determined as the first inflection point 41. Next, of the two inflection points 41, 42 of the adjacent hardened portion 20B, the one farther from the certain hardened portion 20A is determined as the second inflection point 42. As shown in FIG. 8(b), the cut surface 14 is specified by connecting the determined first inflection point 41 and second inflection point 42 with a straight line.

[0074] Compared to FIG. 8(a), FIG. 8(b) requires only one overlay welding step instead of two. On the other hand, compared to Figure 8(a), Figure 8(b) produces more expensive welding powder. Therefore, it is recommended to use the configuration shown in FIG. 8(a) when the two hardened portions 20 are separated from each other, and to use the configuration shown in FIG. 8(b) when the two hardened portions 20 are very close to each other.

[0075] [Welding equipment] The build-up welding apparatus 50 comprises, for example, a welding robot 52 equipped with a welding gun 51, a powder supplying machine 54 that supplies a predetermined amount of welding powder 53 to the welding gun 51, a high-voltage power supply 56 that supplies electrical energy to the welding gun 51 for the plasma jet 55 emitted by the welding gun 51, a gas container 58 that supplies argon gas for the shielding gas 57 emitted by the welding gun 51, and a control unit 59 that controls the welding robot 52, the welding gun 51, the powder supplying machine 54, the high-voltage power supply 56, and the gas container 58.

[0076] Appropriate amounts of welding powder 53, argon gas, and electrical energy are supplied to the welding gun 51 by the control unit 59. Plasma jet 55, welding powder 53, and shielding gas 57 are sprayed from the welding gun 51. The spray causes the welding powder 53 to be layered on the cut surface 14.

[0077] The accumulated welding powder 53 is melted in sequence by the plasma heat. During this time, the welding powder 53 is shielded by the shielding gas 57, so that the welding powder 53 does not oxidize and a sound hardened portion 20 is formed.

[0078] It is more preferable that the press die manufacturing method described based on Fig. 3(a) to (e) is performed based on ruled surface machining data and build-up data. Therefore, the ruled surface machining data and build-up data will be described based on Fig. 10.

[0079] [Rule surface machining data] In step number (hereinafter, ST) 01 in FIG. 10, a wireframe as shown in FIG. 4(e) is created. In ST02, a ruled surface is set as shown in FIG. 4(g). Based on this ruled surface, ruled surface machining data is created (ST03). A ruled surface (i.e., a cut surface) is formed based on this ruled surface processing data (ST04).

[0080] By creating ruled surface processing data, high hardness materials can be built up by laser welding, gas welding, or arc welding. Welding has the advantage that it can be performed by humans, robots, or multi-tasking machines such as 3D printers.

[0081] [Meat data] Based on the ruled surface processing data created in ST03, build-up data is created (ST05). Based on this build-up data, build-up welding is performed in the form shown in FIG. 3(c) (ST06). This meat filling is then finished by machining (ST07).

[0082] That is, the build-up is formed based on build-up data that is created by adding excess metal to the soft bow cross section formed on the wire frame. This makes it possible to automate build-up welding even for press dies with complex shapes.

[0083] This build-up welding data is stored in a control unit 59 shown in Fig. 9, and build-up welding is performed based on the build-up data stored in this control unit 59. Since build-up welding is based on the build-up data, precise build-up welding is performed. Because it is precise, wasteful use of expensive high-hardness materials is corrected, and manufacturing costs can be optimized. [Industrial Applicability]

[0084] The present invention is suitable for a technique for manufacturing a press die comprising a base material and a hardened portion locally provided on the base material. [Explanation of symbols]

[0085] 10...press die, 11...base material, 11a...soft bow cross section, 12...first surface, 13...second surface, 14...cut surface, 15...padded portion, 16...excess pad, 17...projection portion, 20...hardened portion, 20A...certain hardened portion, 20B...adjacent hardened portion, 20C...island-shaped hardened portion, 21...hard bow cross section, 31...first intermediate product, 32...second intermediate product, 33...third intermediate product, 35...vertex, 36...straight ridge, 37...curved ridge, 38...wire, 39...wire frame, 41...first inflection point, 42...second inflection point, 43...connecting line (line connecting the first and second inflection points), 45...ruled surface, 47...groove, 59...control portion, T...maximum thickness (maximum thickness of the soft bow cross section, also maximum thickness of the hard bow cross section).

Claims

1. A method for manufacturing a press die comprising: a base material and a hardened portion locally provided on the base material, the method comprising the steps of: the base material has a flat first surface and a flat second surface different from the first surface; the hardened portion is provided between the first surface and the second surface, and is configured with a ridge line having a curved outer surface; the press die is shown by a wire frame, and the wire frame is defined by vertices which are points on a screen, ridge lines each connecting two of the vertices by a straight line or a curved line, wires connecting a plurality of the ridge lines in series, and a skeleton structure constituted by a plurality of the wires; A vertex at a joint between a straight edge line passing through the first surface and the curved edge line connected to the straight edge line is defined as a first inflection point, and a vertex at a joint between a straight edge line passing through the second surface and the curved edge line connected to the straight edge line is defined as a second inflection point, and when a cut surface is defined by a straight line connecting the first inflection point and the second inflection point, A first processing step of obtaining a first intermediate product processed into a shape conforming to the press die; A second processing step of obtaining a second intermediate product including the cut surface by cutting a soft bow cross-section portion having the same shape as the hardened portion from the first intermediate product along the cut surface; A third processing step of providing a padding portion on the cut surface of the second intermediate product with a material having a higher hardness than the base material to obtain a third intermediate product including a padding portion having a cross-sectional shape in which excess padding is added to the soft bow cross-sectional portion; and a fourth processing step of obtaining the press die by cutting off the excess material from the third intermediate product.

2. The press die manufacturing method according to claim 1, A method for manufacturing a press die, wherein the base material is made of carbon steel for mechanical construction, and the hardened portion is made of high-speed tool steel.

3. The press die manufacturing method according to claim 1, A press die manufacturing method, characterized in that the excess material includes an overhanging portion overhanging from the bottom of the soft bow cross-section portion to the first surface and the second surface.

4. The press die manufacturing method according to claim 1, A press die manufacturing method characterized in that the cutting surface is a ruled surface formed on the wire frame, and in the second processing step, processing is performed based on ruled surface processing data created based on the ruled surface.

5. The press die manufacturing method according to claim 4, The press die manufacturing method according to the present invention, characterized in that the padding is formed based on padding data created by adding excess padding to the soft bow cross-section portion formed on the wire frame.

6. The press die manufacturing method according to claim 5, The press die manufacturing method is characterized in that the deposition data is stored in a control unit, and deposition welding is performed based on the deposition data stored in the control unit.

Citation Information

Patent Citations

  • Conveyer apparatus

    JP1986018625A

  • Forming method for die

    JP1988230236A

  • Welding material for cladding and overlay welding method

    JP2004066261A