Engine block, resin block, and method of manufacturing engine block
The integration of a resin block with controlled thermal resistance regions around a metal cylinder liner improves engine thermal efficiency and reduces weight by optimizing heat management and stress relief in engine blocks.
Patent Information
- Application Number
- JP2021097920
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-06-11
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2041-06-11
AI Technical Summary
Existing engine designs that surround the cylinder liner with resin to reduce cooling loss have limitations in further improving energy use efficiency, necessitating advancements for enhanced thermal efficiency.
A cylinder liner with a metal outer peripheral surface surrounded by a resin block, featuring a first portion that forms the cooling waterway wall with controlled thermal resistance, and a second portion with varying thermal resistance regions to optimize heat management, combined with a manufacturing process that integrates the resin block onto the metal block using adhesives or direct bonding.
This configuration enhances thermal efficiency by reducing cooling losses and weight while minimizing thermal stress, allowing for improved energy use and reduced engine weight through optimized heat dissipation and insulation.
Smart Images

Figure 0007595302000001 
Figure 0007595302000002 
Figure 0007595302000003
Abstract
Description
[Technical field]
[0001] The present invention relates to an engine block, a resin block, and a method for manufacturing an engine block. [Background technology]
[0002] In the automotive sector, reducing the weight of cars and improving the efficiency of internal combustion engines remain essential to reduce global carbon dioxide emissions. Improving thermal efficiency requires new technologies that can significantly reduce the energy lost during the combustion process without being converted into power. From the perspective of weight reduction, the mainstream approach to engine weight reduction has been to use light metals such as aluminum alloys and magnesium alloys for engine parts, but the realization of resins is expected to lead to significant weight reductions.
[0003] Non-Patent Document 1 discloses an engine with a resin surrounding an iron cylinder liner, and describes that the cooling loss of an engine is reduced when the cylinder liner is surrounded by resin compared to when the cylinder liner is surrounded by aluminum.
[0004] Patent Documents 1 and 2 disclose an engine block that includes a block made of resin surrounding a metal cylinder liner, with a water jacket formed on the cylinder liner. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] US Patent Application Publication No. 2015 / 0159581 [Patent Document 2] US Patent Application Publication No. 2015 / 0159582 [Non-patent literature]
[0006] [Non-Patent Document 1] Takahiro Mizuno, Tatsuki Tsuji, Toshio Fujimura, "Prediction of fuel efficiency improvement of SI engines using one-dimensional simulation," Proceedings of the 65th General Meeting and Lecture Conference of the Tokai Branch of the Japan Society of Mechanical Engineers (March 17-18, 2016) No. 163-1 Summary of the Invention [Problem to be solved by the invention]
[0007] As mentioned above, engines have been proposed in which the cylinder liner is surrounded by resin to reduce cooling loss. However, in recent years there has been a demand for even greater energy utilization efficiency, and new technology was needed for such engines.
[0008] An object of the present invention is to realize a technique for improving the thermal efficiency of an engine block having a resin block. [Means for solving the problem]
[0009] According to the present invention, A cylinder liner having a metal outer peripheral surface; a resin block formed of a cured product of a thermosetting resin; a cooling water passage provided in an area on the outer periphery side of the cylinder liner; Equipped with the resin block has a first portion provided on the metal outer circumferential surface side of the cylinder liner and a second portion located outside the first portion, the first portion constitutes at least a wall surface of the cooling water passage on the cylinder liner side, In a region where the first portion forms the wall surface, a thermal resistance change portion is formed in which a thermal resistance in a thickness direction, when a direction from the cylinder liner to the cooling water passage is a thickness direction, is different between a region on a top dead center side and a region on a bottom dead center side in a stroke direction of the piston. Engine blocks can be provided. According to the present invention, it is possible to provide a resin block that constitutes the above-mentioned engine block. According to the present invention, there is provided a method for manufacturing an engine block as described above, comprising the steps of: It is possible to provide a manufacturing method for an engine block in which a resin block is fitted onto the outer peripheral surface of a cylinder liner. Effect of the Invention
[0010] According to the present invention, it is possible to realize a technique for improving the thermal efficiency of an engine block having a resin block. [Brief description of the drawings]
[0011] [Figure 1] FIG. 2 is an exploded view of an engine block and a cylinder head according to the embodiment. [Diagram 2] 2A to 2C are diagrams for explaining an example of a manufacturing method for the engine block shown in FIG. 1. [Diagram 3] 2A to 2C are diagrams for explaining an example of a manufacturing method for the engine block shown in FIG. 1. [Figure 4] 2A to 2C are diagrams for explaining an example of a manufacturing method for the engine block shown in FIG. 1. [Diagram 5] 2A to 2C are diagrams for explaining an example of a manufacturing method for the engine block shown in FIG. 1. [Figure 6] FIG. 2 is a cross-sectional view for explaining an example of details of a cylinder liner and a metal block. [Figure 7] FIG. 2 is a vertical cross-sectional view for explaining an example of details of a cylinder liner and a metal block. [Figure 8] FIG. 2 is a vertical cross-sectional view for explaining an example of a structure having different thermal resistances in a first portion. [Figure 9] FIG. 2 is a vertical cross-sectional view for explaining an example of a structure having different thermal resistances in a first portion. [Figure 10] FIG. 2 is a vertical cross-sectional view for explaining an example of a structure having different thermal resistances in a first portion. [Figure 11] FIG. 2 is a vertical cross-sectional view for explaining an example of a structure having different thermal resistances in a first portion. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In all the drawings, the same components are denoted by the same reference numerals, and the description thereof will be omitted as appropriate.
[0013] 1 is a perspective view of an engine block 10 according to an embodiment. In this figure, the cylinder head attached to the upper side of the engine block 10 is omitted, and only a gasket 28 is shown.
[0014] <Engine Block 10 Overview> An overview of an engine block 10 will be described with reference to Figure 1. The engine block 10 includes a cylinder liner 120 and a resin block 200. For convenience, the resin block 200 is shown painted black in Figure 1. The following describes an example of the engine block 10 for a two-cylinder engine.
[0015] The resin block 200 includes a first portion 210 and a gap 230. The first portion 210 covers the metal outer peripheral surface 122 of the cylinder liner 120. The gap 230 is located outside the first portion 210 and defines a water jacket 232.
[0016] According to the above-mentioned configuration, damage to the resin block 200 caused by the heat generated from the cylinder liner 120 can be reduced.
[0017] Specifically, in the above-described configuration, the first portion 210 of the resin block 200 is surrounded by the water jacket 232. The coolant (e.g., water) flowing in the water jacket 232 can reduce thermal damage to the first portion 210 of the resin block 200.
[0018] <Engine Block 10> The engine block 10 will be described in detail with reference to FIG. The engine block 10 includes a block member 110 , a cylinder liner 120 , a metal block 140 , a projection 130 , and a resin block 200 .
[0019] The block member 110 is made of a metal (for example, cast iron, an aluminum alloy, or a magnesium alloy). In the example shown in FIG.
[0020] The cylinder liner 120 is attached to the block member 110. The cylinder liner 120 may be integral with the block member 110 or may be attachable and detachable to the block member 110.
[0021] The cylinder liner 120 is made of a metal (for example, iron or aluminum) and has an outer circumferential surface made of metal (i.e., a metal outer circumferential surface 122).
[0022] The metal block 140 is a part of the block member 110, and is provided in a cylindrical shape so as to cover the metal outer peripheral surface 122 of the cylinder liner 120. The cylindrical shape may be a single block or a structure in which multiple blocks are connected together. A resin block 200 is provided so as to cover the block outer peripheral surface 142 of the metal block 140. Note that the metal block 140 may be omitted and the resin block 200 may be provided directly on the cylinder liner 120.
[0023] The projection 130 projects from the block member 110 toward the cylinder head (or the gasket 28). The projection 130 has an opening 132. The fastener 22 can be inserted into the opening 132. The fastener 22 fixes the cylinder head to the engine block 10 by sandwiching the gasket 28. The fastener 22 can be, for example, a bolt.
[0024] <Resin block 200> The resin block 200 includes a first portion 210, a second portion 220, and a gap 230. The second portion 220 is located outside the gap 230. The gap 230 is between the first portion 210 and the second portion 220. The first portion 210 and the second portion 220 are integrated with each other in a lower portion of the resin block 200.
[0025] The first portion 210 of the resin block 200 is attached to the block outer peripheral surface 142 of the metal block 140 via, for example, an adhesive 300 (see FIG. 4). The adhesive is located between the first portion 210 of the resin block 200 and the block outer peripheral surface 142 of the metal block 140, and bonds the first portion 210 of the resin block 200 and the block outer peripheral surface 142 of the metal block 140 to each other. The adhesive may function as a stress relaxation layer.
[0026] The first portion 210 of the resin block 200 may be integrally joined to the block outer peripheral surface 142 of the metal block 140 without using an adhesive. In this case, a direct bond between the resin (resin block 200) and the metal (metal block 140) is formed at the interface between the first portion 210 of the resin block 200 and the block outer peripheral surface 142 of the metal block 140.
[0027] The resin block 200 has an upper surface 202. The upper surface 202 has a groove that forms a void 230, and the void 230 is exposed from the block member 110. In such a structure, thermal damage to the resin block 200 at the upper end of the cylinder liner 120 and its vicinity can be particularly reduced. Therefore, the above-mentioned structure is particularly meaningful when the temperatures of the metal block 140 and the cylinder liner 120 particularly rise at their upper ends and their vicinity. Furthermore, in the above-mentioned structure, the void 230 can be formed not only before the resin block 200 is attached to the metal block 140, but also after the resin block 200 is attached to the metal block 140. Therefore, the degree of freedom in the process for forming the void 230 can be increased.
[0028] The void 230 may not be exposed from the upper surface 202 of the resin block 200, and may be present inside the resin block 200. Even in this case, the coolant flowing in the water jacket 232 can reduce thermal damage to the first portion 210 of the resin block 200.
[0029] The second portion 220 has an opening 222. The resin block 200 is positioned such that the protrusion 130 passes through the opening 222 of the second portion 220. The protrusion 130 can function as a guide for attaching the resin block 200 to the block member 110.
[0030] <Materials and Properties of Resin Block 200> The first portion 210 and the second portion 220 of the resin block 200 contain a cured product of a thermosetting resin. In other words, the resin block 200 is made of a thermosetting resin. The resin block 200 may further contain an inorganic filler (e.g., glass fiber). The resin block 200 may contain, for example, 50% by weight or more of the inorganic filler with respect to the total weight of the resin block 200. The thermosetting resin forming the resin block 200 may be, for example, a phenolic resin.
[0031] The thermal conductivity of the thermosetting resin forming the resin block 200 can be made low, for example, 1.00 W / m K or less. The low thermal conductivity can reduce the cooling loss of the engine block 10.
[0032] The density of the thermosetting resin forming the resin block 200 can be low, for example, 2.2 g / cm 3 The low density allows the engine block 10 to be made lighter.
[0033] The glass transition point of the thermosetting resin forming the resin block 200 can be high, for example, 160° C. or higher, and preferably 200° C. or higher. The high glass transition point allows the engine block 10 to be used at high temperatures.
[0034] The linear expansion coefficient of the thermosetting resin forming the resin block 200 can be made equal to or close to the linear expansion coefficient of the metal forming the block outer peripheral surface 142 of the metal block 140. For example, the machine direction (MD) linear expansion coefficient of the thermosetting resin forming the resin block 200 may be 75% or more and 125% or less of the MD linear expansion coefficient of the metal forming the metal block 140, and the transverse direction (TD) linear expansion coefficient of the thermosetting resin forming the resin block 200 may be 75% or more and 125% or less of the TD linear expansion coefficient of the metal forming the metal block 140. By making the linear expansion coefficient of the thermosetting resin forming the resin block 200 and the linear expansion coefficient of the metal forming the metal block 140 equal to or close to each other, it is possible to reduce the stress from the metal block 140 to the resin block 200 when both the metal block 140 and the resin block 200 are heated.
[0035] The MD linear expansion coefficient of the thermosetting resin forming the resin block 200 and the MD linear expansion coefficient of the metal forming the metal block 140 can each be, for example, not less than 10 ppm and not more than 40 ppm.
[0036] The TD linear expansion coefficient of the thermosetting resin forming the resin block 200 and the TD linear expansion coefficient of the metal forming the metal block 140 can each be, for example, not less than 10 ppm and not more than 40 ppm.
[0037] When the metal block 140 is omitted and the resin block 200 is provided on the cylinder liner 120, the linear expansion coefficient of the thermosetting resin can be set to the above value in relation to the cylinder liner 120.
[0038] <Method of manufacturing engine block 10> 2 to 5 are diagrams for explaining an example of a method for manufacturing the engine block 10 shown in FIG.
[0039] An example of a manufacturing method for the engine block 10 will be outlined with reference to Figs. 2, 3 and 5. First, as shown in Fig. 2, a base block 100 is formed. The base block 100 has a cylinder liner 120 and a metal block 140. The cylinder liner 120 has a metal outer peripheral surface 122. The metal block 140 surrounds the cylinder liner 120. Next, as shown in Fig. 3, the base block 100 is processed to remove a portion of the metal block 140 so that the thickness of the metal block 140 is reduced. If the metal block 140 before processing has a desired thickness, the removal process is not necessary. Next, as shown in Fig. 5, the metal block 140 is surrounded by a resin block 200.
[0040] According to the above-mentioned process, the manufacturing process for surrounding the metal block 140 and the cylinder liner 120 with the resin block 200 can be realized at low cost. Specifically, in the above-mentioned process, the base block 100 including the metal block 140 can be formed using existing equipment for forming an existing engine block (for example, a mold used in casting for forming an existing engine block). In other words, even when a part of the metal block 140 is processed by removing, it is not necessary to install new equipment for forming the base block 100 from which the metal block 140 has been removed. Therefore, the manufacturing process for surrounding the metal block 140 and the cylinder liner 120 with the resin block 200 can be realized at low cost.
[0041] An example of a method for manufacturing the engine block 10 will be described in detail with reference to FIGS. First, as shown in Fig. 2, a base block 100 is formed. The base block 100 has a block member 110, a cylinder liner 120, and a metal block 140. Each of the block member 110, the cylinder liner 120, and the metal block 140 is made of metal. In particular, the metal block 140 is made of, for example, cast iron, an aluminum alloy, or a magnesium alloy.
[0042] The base block 100 has a gap 150 between the cylinder liner 120 and the metal block 140. The gap 150 defines a water jacket 152. The base block 100 can be formed using existing equipment for forming existing engine blocks (i.e., engine blocks having water jackets 152). In one example, the base block 100 can be formed by casting, or more specifically, die casting. In this example, the mold used for die casting can be the mold for forming the existing engine block.
[0043] The base block 100 further has an opening 132. As described with reference to Fig. 1, the fastener 22 (Fig. 1) can be inserted into the opening 132. The base block 100 includes a portion for forming the protrusion 130 shown in Fig. 3. This portion forms the protrusion 130 in the step shown in Fig. 3 (the step of removing the metal block 140).
[0044] Next, as shown in Fig. 3, a part of the metal block 140 is removed from the base block 100 to reduce the thickness. In the example shown in Fig. 3, the metal block 140 is processed so as to reduce the thickness around the cylinder liner 120, and is removed so as to form the protrusion 130 and leave the opening 132.
[0045] 4, an adhesive 300 is formed on the block outer peripheral surface 142 of the metal block 140. As shown in FIG.
[0046] 5, the resin block 200 is fitted into the metal block 140 so as to surround it. The resin block 200 is attached so that the protrusion 130 penetrates the opening 222 of the resin block 200. The first portion 210 of the resin block 200 and the block outer peripheral surface 142 of the metal block 140 are bonded to each other via an adhesive 300 (FIG. 4), and the inner surface of the opening 222 of the resin block 200 and the outer peripheral surface of the protrusion 130 are bonded to each other via the adhesive 300 (FIG. 4).
[0047] The adhesive 300 (FIG. 4) may not be formed. In the case where the adhesive 300 is not formed, the first portion 210 of the resin block 200 may be integrally joined to the block outer peripheral surface 142 of the metal block 140 without the intervention of an adhesive (for example, the adhesive 300 (FIG. 4)).
[0048] 5, the resin block 200 includes a first portion 210, a second portion 220, and a void 230. The void 230 defines a water jacket 232. The void 230 may be formed before surrounding the metal block 140 with the resin block 200, or may be formed after surrounding the metal block 140 with the resin block 200.
[0049] The method for manufacturing the engine block 10 is not limited to the examples shown in Figures 2 to 5. The engine block 10 may be manufactured as in the following example.
[0050] First, the block shown in FIG. 3 (the block member 110, the cylinder liner 120, and the protrusion 130) may be formed without forming the base block 100 shown in FIG. 2. The block shown in FIG. 3 can be formed by casting, more specifically, by die casting. In this example, the mold used for die casting has a shape corresponding to the block shown in FIG. 3.
[0051] Secondly, the engine block 10 may be manufactured by insert molding. In this example, the block (block member 110 (metal block 140), cylinder liner 120, and protrusion 130) shown in FIG. 3 is placed in a mold, and resin for forming the resin block 200 is supplied into the mold. According to this example, the resin block 200 can be directly bonded to the metal block 140 without providing the adhesive 300 shown in FIG. 4. As the adhesive 300, for example, a high heat dissipation one-component condensation type RTV silicone adhesive sealant (heat transfer coefficient: 0.83 W / mk) can be used.
[0052] <Cylinder liner 120 and metal block 140> 6 and 7 are cross-sectional views for explaining an example of details of the cylinder liner 120 and the metal block 140. Fig. 6 shows a cross section of the cylinder liner 120 and the metal block 140. Fig. 7 shows a cross section of the cylinder liner 120 and the metal block 140.
[0053] The cylinder liner 120 includes an iron layer 120a and an aluminum layer 120b. The iron layer 120a forms the inner peripheral surface of the cylinder liner 120. The iron layer 120a includes at least one of iron and an iron alloy. The aluminum layer 120b is located outside the iron layer 120a and forms a metal outer peripheral surface 122. The aluminum layer 120b includes at least one of aluminum and an aluminum alloy.
[0054] The metal block 140 is provided so as to surround the periphery of the aluminum layer 120 b of the cylinder liner 120 .
[0055] The surface roughness Ra (arithmetic mean roughness) of the block outer peripheral surface 142 of the metal block 140 can be set to, for example, not less than 0.2 μm and not more than 3.0 μm.
[0056] The block outer peripheral surface 142 of the metal block 140 may not have any protrusions having a tip angle of less than 90°. Such protrusions may become a concentration point of thermal stress in the metal block 140 and the resin block 200, and may cause cracks in the resin block 200. If there are no such protrusions, cracks in the resin block 200 can be reduced.
[0057] <Thermal Resistance of First Portion 210 (1)> With reference to Figs. 8 to 11, the thermal resistance Rt of the first portion 210 will be described, focusing in particular on the thickness of the first portion 210. Figs. 8 to 11 are enlarged views of region A in Fig. 7, and a total of four structural examples will be described. In the region where the first portion 210 constitutes the wall surface 232A of the water jacket 232, the thermal resistance Rt in the thickness direction, when the direction from the cylinder liner 120 to the water jacket 232 is the thickness direction, is different between the region on the top dead center TDC side and the region on the bottom dead center BDC side in the stroke direction of the piston 190. When the composition and density of the first portion 210 are constant, the thermal resistance Rt is proportional to the thickness t of the first portion 210.
[0058] In the structural example shown in FIG. 8, the boundary between the water jacket 232 and the first portion 210, i.e., the wall surface 232A of the water jacket 232, forms a continuous change region 211 in which the boundary changes continuously when viewed in cross section, and in particular has a straight portion 212 that changes linearly.
[0059] In the structure of FIG. 8(a), the wall surface 232A is a straight portion 212 that is obliquely straight (inclined) in cross section, and the thickness t of the second portion 220 is thicker on the top dead center TDC side than on the bottom dead center BDC side. In other words, the thermal resistance change portion 170 can be said to have a first region 171 with a large thermal resistance Rt on the upper side (top dead center TDC side) in the figure, and a second region 172 with a smaller thermal resistance Rt than the first region 171 on the lower side (bottom dead center BDC side). By making the thickness t of the first portion 210 thicker on the top dead center TDC side in this manner to increase the thermal resistance Rt, it is possible to realize high thermal efficiency by suppressing the escape of heat during combustion to the water jacket 232 at the timing when the fuel is burned in the combustion chamber (i.e., when the piston 190 is near the top dead center TDC). In addition, since the thickness t changes continuously in a straight line, it is possible to avoid local concentration of thermal distortion and thermal stress. In particular, when the combustion timing (i.e., heat generation timing) is taken into consideration, it is important to design the thermal resistance Rt of the first region 171 in the range from top dead center TDC to 30% of the stroke length, especially in the range up to 20%. Also, by making the top dead center TDC side thicker, the assembly work of assembling the resin block 200 to the metal block 140 becomes easier.
[0060] In the structure of FIG. 8(b), the wall surface 232A is obliquely linear in cross section, and the thickness t of the second portion 220 is thicker on the bottom dead center BDC side than on the top dead center TDC side. In other words, the thermal resistance change portion 170 has a first region 171 with a large thermal resistance Rt on the lower side (bottom dead center BDC side) in the figure, and a second region 172 with a smaller thermal resistance Rt than the first region 171 on the upper side (top dead center TDC side). Since the thermal resistance Rt is reduced by thinning the thickness t of the first portion 210 on the top dead center TDC side in this manner, heat can be released to the water jacket 232 at the timing when fuel is burned in the combustion chamber (i.e., when the piston 190 is near the top dead center TDC), and cooling can be promoted. This is effective in engines in which the temperature in the combustion chamber rises during combustion and knocking is likely to occur. In particular, when considering the combustion timing (i.e., heat generation timing), it is important to design the thermal resistance Rt of the second region 172 in the range from top dead center TDC to 30% of the stroke length, especially in the range up to 20%. In addition, since the thickness t changes continuously and linearly, it is possible to prevent thermal distortion and thermal stress from concentrating locally.
[0061] 9, the boundary between the water jacket 232 and the first portion 210, i.e., the wall surface 232A of the water jacket 232, is a continuously changing region 211 where the boundary changes continuously in a cross-sectional view, and in particular has a curved portion 213 that changes in a curved shape. Note that the curved portion 213 is not limited to a gradually increasing or decreasing curve, and various curves may be used.
[0062] 9(a) is a configuration in which the wall surface 232A approaches the metal block 140 (i.e., the cylinder liner 120) in a curved shape on the bottom dead center BDC side from the top dead center TDC side in a cross-sectional view. In other words, the thickness t of the first portion 210 is thicker on the top dead center TDC side than on the bottom dead center BDC side, and the change in thickness t is curved. In other words, the thermal resistance change portion 170 can be said to have a first region 171 with a large thermal resistance Rt on the upper side (top dead center TDC side) in the figure, and a second region 172 with a smaller thermal resistance Rt than the first region 171 on the lower side (bottom dead center BDC side). In this manner, by making the thickness t of the first portion 210 thicker on the top dead center (TDC) side to increase the thermal resistance Rt, it is possible to suppress the heat generated during combustion from escaping to the water jacket 232 at the timing when the fuel is burned in the combustion chamber (i.e., when the piston 190 is near the top dead center (TDC)), thereby realizing high thermal efficiency. Furthermore, since the thickness t changes continuously, it is possible to prevent thermal distortion and thermal stress from concentrating locally. Furthermore, since the thickness t changes in a curved manner, it is possible to realize an optimal insulation / cooling structure according to the temperature inside the cylinder during and after combustion.
[0063] The structure of FIG. 9(b) is configured such that the wall surface 232A approaches the metal block 140 in a curved shape on the top dead center TDC side from the bottom dead center BDC side in a cross-sectional view. In other words, the thickness t of the first portion 210 is thinner on the top dead center TDC side than on the bottom dead center BDC side, and the change in thickness t is curved. In other words, the thermal resistance change portion 170 can be said to have a first region 171 with a large thermal resistance Rt on the lower side (bottom dead center BDC side) in the figure, and a second region 172 with a smaller thermal resistance Rt than the first region 171 on the upper side (top dead center TDC side). Since the thickness t of the first portion 210 is made thinner on the top dead center TDC side in this manner to reduce the thermal resistance Rt, heat can be released to the water jacket 232 at the timing when the fuel is burned in the combustion chamber (i.e., when the piston 190 is near the top dead center TDC), promoting cooling and suppressing the occurrence of knocking. In addition, because the thickness t changes continuously, it is possible to prevent thermal distortion and thermal stress from concentrating locally. In addition, because the thickness t changes in a curved line, it is possible to realize an optimal insulation / cooling structure according to the temperature inside the cylinder during and after combustion.
[0064] In the structural example shown in FIG. 10, the boundary between the water jacket 232 and the first portion 210, i.e., the wall surface 232A of the water jacket 232, is a continuous change region 211 in which the boundary changes continuously when viewed in cross section, and one cross section of the wall surface 232A1 on the top dead center TDC side and the wall surface 232A2 on the bottom dead center BDC side is vertical and the other is inclined.
[0065] In the configuration of FIG. 10(a), the wall surface 232A1 on the top dead center TDC side of the change point 175 is provided vertically. The wall surface 232A2 on the bottom dead center BDC side of the change point 175 forms a straight line portion 212 (continuous change region 211) that is inclined so as to approach the metal block 140 side as it approaches the bottom, and the thickness t of the second portion 220 is thicker on the top dead center TDC side than on the bottom dead center BDC side. It can be said that the top dead center TDC side of the change point 175 is the first region 171 in which the thermal resistance Rt is relatively large, and the bottom dead center BDC side is the second region 172 in which the thermal resistance Rt is relatively small. In this way, by making the thickness t of the first portion 210 thicker on the top dead center TDC side to increase the thermal resistance Rt, it is possible to suppress the heat during combustion from escaping to the water jacket 232 at the timing when the fuel is burned in the combustion chamber (i.e., when the piston 190 is near the top dead center TDC), thereby achieving high thermal efficiency.
[0066] In the configuration of FIG. 10(b), the wall surface 232A1 on the top dead center TDC side of the change point 175 forms a linear portion 212 (continuous change region 211) that is inclined so as to approach the metal block 140 side toward the upper side, and the thickness t of the second portion 220 is thicker on the top dead center TDC side than on the bottom dead center BDC side. The wall surface 232A2 on the bottom dead center BDC side of the change point 175 is provided vertically. The bottom dead center BDC side of the change point 175 can be called the first region 171 in which the thermal resistance Rt is relatively large, and the top dead center TDC side can be called the second region 172 in which the thermal resistance Rt is relatively small. Since the thickness t of the first portion 210 is made thinner on the top dead center TDC side in this manner to reduce the thermal resistance Rt, heat can be released to the water jacket 232 at the timing when the fuel is burned in the combustion chamber (i.e., when the piston 190 is near the top dead center TDC), promoting cooling and suppressing the occurrence of knocking.
[0067] 11, the boundary between the water jacket 232 and the first portion 210, i.e., the wall surface 232A of the water jacket 232, changes to be discontinuous (i.e., step-like) in a cross-sectional view. One of the cross sections of the wall surface 232A1 on the top dead center TDC side and the wall surface 232A2 on the bottom dead center BDC side is vertical and the other is inclined, and the boundary therebetween forms a step-like discontinuous portion 214. In other words, in the configuration of FIG. 10, the change point 175 is a step-like discontinuous portion 214.
[0068] In the configuration of Fig. 11(a), wall surface 232A1 on the bottom dead center BDC side from discontinuous portion 214 is provided vertically. Wall surface 232A2 on the top dead center TDC side from discontinuous portion 214 is provided in an inclined straight line so that it becomes farther from metal block 140 as it goes upward, i.e., so that it becomes thicker. The top dead center TDC side from discontinuous portion 214 can be called first region 171 with relatively large thermal resistance Rt, and the bottom dead center BDC side can be called second region 172 with relatively small thermal resistance Rt. It is possible to realize the same effect as in Fig. 10, and since the thickness t can be greatly changed at discontinuous portion 214, it is possible to deal with a case where the required thermal resistance Rt is significantly different between the top dead center TDC side and the bottom dead center BDC side.
[0069] In the configuration of Fig. 11(b), wall surface 232A1 on the top dead center TDC side of discontinuous portion 214 is provided vertically. Wall surface 232A2 on the bottom dead center BDC side of discontinuous portion 214 is provided linearly and inclined so as to approach metal block 140 as it approaches downward. The bottom dead center BDC side of discontinuous portion 214 can be called first region 171 having relatively large thermal resistance Rt, and the top dead center TDC side can be called second region 172 having relatively small thermal resistance Rt. It is possible to achieve the same effect as in Fig. 10, and since the thickness t can be greatly changed at discontinuous portion 214, it is possible to deal with a case where the required thermal resistance Rt is significantly different between the top dead center TDC side and the bottom dead center BDC side.
[0070] <Thermal Resistance of First Portion 210 (2)> In Figs. 8 to 11, the thermal resistance Rt of the first portion 210 is different depending on the region due to the difference in thickness of the first portion 210. In addition, the material of the first portion 210 can be used to provide a difference. Specifically, this can be achieved by using materials with different thermal conductivities in the first region 171 and the second region 172. For example, in the first region 171, the hollow ratio per volume in the cured thermosetting resin is increased to reduce the thermal conductivity. That is, the thermal resistance Rt is increased. Conversely, in the second region 172, the hollow ratio is decreased compared to the first region 171 to increase the thermal conductivity. That is, the thermal resistance Rt is decreased. For example, a desired hollow ratio can be achieved by incorporating air bubbles (microballoons) or hollow filler in the cured thermosetting resin and adjusting the content.
[0071] <Thermal Resistance of First Portion 210 (3)> In order to provide a difference in the thermal resistance Rt of the first portion 210 for each region, the adhesive 300 (see FIG. 4) used when attaching the resin block 200 to the metal block 140 (or the cylinder liner 120) may be different. For example, by using more adhesive on the wall surface corresponding to the first region 171 than on the wall surface corresponding to the second region 172, the thermal resistance Rt in the first region 171 can be made larger than the thermal resistance Rt in the second region 172.
[0072] <Thermal Resistance of First Portion 210 (4)> In order to provide a difference in thermal resistance Rt for each region of the first portion 210, unevenness is formed on the inner wall surface of the first portion 210 on the metal block 140 (or cylinder liner 120) side, with more unevenness provided on the wall surface corresponding to the first region 171 than on the wall surface corresponding to the second region 172. For example, the unevenness is formed so as to form grooves around the inner wall surface of the first portion 210. The width, depth, and number of the grooves can be adjusted for each region to achieve the desired thermal resistance Rt. This makes it possible to make the thermal resistance Rt of the first region 171 greater than that of the second region 172.
[0073] Although the embodiments of the present invention have been described above with reference to the drawings, these are merely examples of the present invention, and various configurations other than those described above may also be adopted. For example, in the above embodiment, the resin block 200 is applied to a two-cylinder engine (engine block 10), but the resin block 200 may be applied to a single-cylinder engine or an engine with three or more cylinders, regardless of the number of cylinders. [Explanation of symbols]
[0074] 10 Engine block 20 Cylinder head 100 Base Block 110 Block member 120 Cylinder liner 120a iron layer 120b Aluminum layer 122 Metal outer surface 140 Metal Block 142 Block outer surface 150 void 152 Water jacket (cooling water channel) 170 Thermal resistance change part 171 First Area 172 Second Area 200 Resin Block 210 Part 1 211 Continuously Changing Region 212 Straight section 213 Curved section 220 Part 2 230 void 232 Water jacket (cooling water channel) 232A Wall 300 Adhesive
Claims
1. A cylinder liner having a metal outer peripheral surface; a resin block formed of a cured product of a thermosetting resin; a cooling water passage provided in an area on the outer periphery side of the cylinder liner; Equipped with the resin block has a first portion provided on the metal outer circumferential surface side of the cylinder liner and a second portion located outside the first portion, the first portion constitutes at least a wall surface of the cooling water passage on the cylinder liner side, a thermal resistance change portion is formed in a region where the first portion forms the wall surface, in which a thermal resistance in a thickness direction, when a direction from the cylinder liner to the cooling water passage is a thickness direction, differs between a region on a top dead center side and a region on a bottom dead center side in a stroke direction of the piston, The thermal resistance change portion has a thermal resistance on a top dead center side that is equal to or greater than a thermal resistance on a bottom dead center side, a first region having a relatively large thermal resistance; a second region having a relatively smaller thermal resistance than the first region; The engine block, wherein the first region is provided in a region closer to a top dead center in a stroke direction of a piston than the second region.
2. 2. The engine block according to claim 1, wherein the first region includes at least a region in a range of 20% of the stroke length from the top dead center side.
3. 3. The engine block of claim 1, wherein the first region has a greater thickness than the second region.
4. The engine block according to claim 1 , wherein the first region has a larger volume ratio of a hollow region contained in the hardened material than the second region.
5. The first region and the second region are formed of cured products of different thermosetting resins, 5. The engine block according to claim 1, wherein the thermal conductivity of the cured material of the first region is lower than the thermal conductivity of the cured material of the second region.
6. 6. An engine block according to claim 1, wherein the first portion has a region where the thickness varies continuously.
7. 7. The engine block according to claim 6, wherein the region where the thickness of the first portion changes continuously includes a region where a boundary of the cooling water passage in a cross section changes linearly.
8. 8. The engine block according to claim 6, wherein the region where the thickness of the first portion changes continuously has a region where a boundary of the cooling water passage in a cross section changes in a curved shape.
9. 9. An engine block as claimed in claim 1, wherein the first portion has an area where the thickness varies discontinuously.
10. an adhesive layer is provided on a wall surface of the first portion of the resin block that faces the cylinder liner, 10. The engine block according to claim 1, wherein the adhesive layer is provided in a larger amount on the wall surface corresponding to the first region than on the wall surface corresponding to the second region.
11. The first portion of the resin block has a wall surface on the cylinder liner side formed with projections and recesses, 11. The engine block according to claim 1, wherein the number of projections and recesses is greater on the wall surface corresponding to the first region than on the wall surface corresponding to the second region.
12. The engine block according to claim 1 , further comprising a cylindrical metal block between the first portion of the resin block and the cylinder liner.
13. 13. An engine block as claimed in any one of claims 1 to 12, wherein the thermosetting resin forming the first portion of the resin block comprises a phenolic resin.
14. 14. The engine block according to claim 1, wherein a thermal conductivity of a cured product of the thermosetting resin forming the first portion of the resin block is 1.00 W / (m·K) or less.
15. an MD linear expansion coefficient of the cured product of the thermosetting resin forming the first portion of the resin block is 75% or more and 125% or less of an MD linear expansion coefficient of the metal forming the metal outer peripheral surface, 15. The engine block according to claim 1, wherein a TD linear expansion coefficient of the cured product of the thermosetting resin forming the first portion of the resin block is 75% or more and 125% or less of a TD linear expansion coefficient of the metal forming the metal outer peripheral surface.
16. The density of the cured thermosetting resin forming the first portion of the resin block is 2.2 g / cm 3 16. An engine block according to any one of claims 1 to 15, wherein:
17. 17. The engine block according to claim 1, wherein a glass transition point of the cured product of the thermosetting resin forming the first portion of the resin block is 160°C or higher.
18. A resin block constituting the engine block according to any one of claims 1 to 17.
19. A method for manufacturing an engine block according to any one of claims 1 to 17, comprising the steps of: A manufacturing method for an engine block in which a resin block is fitted onto the outer peripheral surface of a cylinder liner.
Citation Information
Patent Citations
Engine cylinder barrel structure
CN108386290A
Cylinder liner and its manufacturing method
JP2007016737A
Engine block, resin block and method for manufacturing engine block
JP2020112149A
Engine having composite cylinder block
US20150159581A1
Engine having composite cylinder block
US20150159582A1