Substrate fixing device, electrostatic chuck, and method of manufacturing electrostatic chuck

A multi-layered electrostatic chuck with connected heater electrodes via enlarged vias addresses the issue of thermal non-uniformity, achieving enhanced temperature consistency for wafer processing.

JP7595511B2Active Publication Date: 2024-12-06SHINKO ELECTRIC IND CO LTD
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2021067843
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-11-13
Filing Date
2021-04-13
Publication Date
2024-12-06
Estimated Expiration
2041-04-13

AI Technical Summary

Technical Problem

Existing electrostatic chucks face limitations in achieving uniform thermal distribution due to restrictions in heater electrode arrangement, leading to temperature gradients during wafer processing.

Method used

The substrate fixing device incorporates a multi-layered structure with a ceramic layer and two heat generating layers, connected by vias with enlarged ends, allowing flexible electrode arrangement and improved thermal uniformity.

Benefits of technology

This configuration enhances thermal uniformity across the electrostatic chuck's surface, ensuring consistent temperature control for wafer processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007595511000001
    Figure 0007595511000001
  • Figure 0007595511000002
    Figure 0007595511000002
  • Figure 0007595511000003
    Figure 0007595511000003
Patent Text Reader

Abstract

To provide a substrate fixing device that obtains sufficiently high heat soaking property, an electrostatic chuck, and a manufacturing method of the electrostatic chuck.SOLUTION: A substrate fixing device 100 includes a base plate 110 and an electrostatic chuck 120 that is fixed to the base plate and attracts the substrate by electrostatic force. The electrostatic chuck includes an adsorption layer formed by using a ceramic layer 130 and adsorbing and holding the substrate in contact with the substrate, a first heating layer 150 that is laminated on the adsorption layer and has a heater electrode 151 that generates heat, a second heating layer 160 that is laminated on the first heating layer and has a heater electrode 161 that generates heat, and a via 170 both ends of which are connected to the first and second electrodes, respectively, and at least one end of which penetrates the first or second electrode and that has a top 171 with a diameter larger than the diameter of the penetrating part at the one end.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a substrate fixing device, an electrostatic chuck, and a method for manufacturing an electrostatic chuck. [Background technology]

[0002] In general, a substrate fixing device that attracts and holds a wafer when manufacturing semiconductor parts, for example, is equipped with an electrostatic chuck (ESC) that is configured using a ceramic plate with an electrode built in. The substrate fixing device has a structure in which the electrostatic chuck is fixed to a base plate, and the wafer is attracted to the electrostatic chuck by applying a voltage to the electrode built in the ceramic plate, utilizing electrostatic force. By attracting and holding the wafer on the electrostatic chuck, processes such as micromachining and etching can be efficiently performed on the wafer.

[0003] Such electrostatic chucks may be provided with a temperature control function for controlling the temperature of the wafer. Specifically, a heater electrode may be formed by screen printing a metal paste such as tungsten, and the heater electrode may be fired simultaneously with the formation of the ceramic plate. In addition, in order to obtain high thermal uniformity on the wafer mounting surface, a technology has been devised in which an external heater electrode is formed by etching a rolled metal foil on an insulating resin using photolithography. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2016-136611 A [Patent Document 2] JP 2016-100474 A [Patent Document 3] JP 2014-112672 A [Patent Document 4] JP 2018-26427 A Summary of the Invention [Problem to be solved by the invention]

[0005] Recently, as wafers are processed with increasingly finer features, the electrostatic chuck that holds the wafer is also required to have higher temperature uniformity, i.e., it is required to control the temperature of the entire attracting surface of the electrostatic chuck to be uniform.

[0006] However, even when an external heater electrode capable of achieving high thermal uniformity is used, there is a certain limit to the degree of freedom in arranging the heater electrodes, which causes a problem of temperature gradients between heater zones. Specifically, for example, in a power supply section that supplies power to the heater electrodes, the area of ​​the heater electrodes becomes large, making it difficult to arrange the heater electrodes completely uniformly, and there is a limit to the improvement of thermal uniformity over the entire attracting surface of the electrostatic chuck.

[0007] The disclosed technology has been made in consideration of the above points, and aims to provide a substrate fixing device, an electrostatic chuck, and a method for manufacturing an electrostatic chuck that can achieve sufficiently high thermal uniformity. [Means for solving the problem]

[0008] In one aspect, a substrate fixing device disclosed in the present application includes a base plate and an electrostatic chuck fixed to the base plate and configured to attract a substrate by electrostatic force, the electrostatic chuck including an adhesion layer formed of ceramic and contacting the substrate to attract and hold the substrate, a first heating layer stacked on the adhesion layer and including a first electrode that generates heat, a second heating layer stacked on the first heating layer and including a second electrode that generates heat, and a via having both ends connected to the first electrode and the second electrode, respectively, at least one end penetrating the first electrode or the second electrode, the one end having a diameter larger than the diameter of the penetrating portion. Effect of the Invention

[0009] According to one aspect of the substrate fixing device, the electrostatic chuck, and the method for manufacturing an electrostatic chuck disclosed in the present application, it is possible to obtain an effect of obtaining sufficiently high thermal uniformity. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a perspective view showing a configuration of a substrate fixing device according to an embodiment. [Diagram 2] FIG. 2 is a schematic diagram showing a cross section of the substrate fixing device according to one embodiment. [Diagram 3] FIG. 3 is a flow diagram showing a method for manufacturing a substrate fixing device according to one embodiment. [Figure 4] FIG. 4 is a diagram showing a specific example of the ceramic layer forming step. [Diagram 5] FIG. 5 is a diagram showing a specific example of the metal foil layer laminating step. [Figure 6] FIG. 6 is a diagram showing a specific example of the first heater pattern forming step. [Figure 7] FIG. 7 is a diagram showing a specific example of the insulating resin laminating step. [Figure 8] FIG. 8 is a diagram showing a specific example of the metal foil layer laminating step. [Figure 9] FIG. 9 is a diagram showing a specific example of the second heater pattern forming step. [Figure 10] FIG. 10 is a diagram showing a specific example of a via hole forming step. [Figure 11] FIG. 11 is a diagram showing a specific example of a via hole filling step. [Figure 12] FIG. 12 is a diagram showing a specific example of the first heater pattern. [Figure 13] FIG. 13 is a diagram showing a specific example of the second heater pattern. [Figure 14] FIG. 14 is a diagram showing a specific example of the insulating resin laminating step. [Figure 15] FIG. 15 is a diagram showing a specific example of the opening forming step. [Figure 16] FIG. 16 is a diagram showing a specific example of the first heater pattern. [Figure 17] FIG. 17 is a diagram showing a specific example of the second heater pattern. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, an embodiment of a substrate fixing device, an electrostatic chuck, and a manufacturing method for an electrostatic chuck disclosed in the present application will be described in detail with reference to the drawings. Note that the present invention is not limited to the embodiment.

[0012] 1 is a perspective view showing a configuration of a substrate fixing device 100 according to one embodiment. The substrate fixing device 100 shown in FIG.

[0013] The base plate 110 is a circular member made of metal such as aluminum. The base plate 110 is a base material for fixing the electrostatic chuck 120. The base plate 110 is attached to, for example, a semiconductor manufacturing device, and causes the substrate fixing device 100 to function as a semiconductor holding device for holding a wafer.

[0014] The electrostatic chuck 120 adjusts the temperature of an object, such as a wafer, while adsorbing the object by using electrostatic force. That is, the electrostatic chuck 120 is formed by laminating a ceramic layer that adsorbs the object and a heater layer that heats the object. The diameter of the electrostatic chuck 120 is smaller than the diameter of the base plate 110, and the electrostatic chuck 120 is fixed to the center of the base plate 110. At this time, the heater layer of the electrostatic chuck 120 is bonded to the base plate 110, thereby fixing the electrostatic chuck 120 to the base plate 110. A ceramic layer is laminated on the upper surface of the heater layer, and an adsorption surface that adsorbs the object is exposed.

[0015] Fig. 2 is a schematic diagram showing a cross section taken along line II in Fig. 1. As shown in Fig. 2, the substrate fixing device 100 is configured by bonding an electrostatic chuck 120 to a base plate 110.

[0016] The base plate 110 is a metal member having a thickness of, for example, about 20 to 50 mm and having therein a cooling water passage 111 which serves as a flow path for cooling water. The base plate 110 cools the electrostatic chuck 120 by the cooling water flowing into the cooling water passage 111 from the outside of the substrate fixing device 100. As a result of the electrostatic chuck 120 being cooled, an object such as a wafer attracted to the electrostatic chuck 120 is cooled.

[0017] The base plate 110 may have a cooling gas passage that serves as a flow path for cooling gas, instead of the cooling water passage 111. In short, it is sufficient for the base plate 110 to have a refrigerant passage that allows a refrigerant such as cooling water and cooling gas to pass through.

[0018] The electrostatic chuck 120 has a ceramic layer 130 , an insulating resin layer 140 , a first heating layer 150 , and a second heating layer 160 , and the second heating layer 160 is bonded to the base plate 110 .

[0019] The ceramic layer 130 has a conductive electrode 131 inside and is a layer made of ceramic, for example, about 4.5 mm thick. The ceramic is obtained by firing a green sheet made of aluminum oxide, for example. When a voltage is applied to the electrode 131 of the ceramic layer 130, the ceramic layer 130 attracts an object, for example, a wafer, by electrostatic force. That is, in FIG. 2, the upper surface of the ceramic layer 130 becomes the attracting surface, and when a voltage is applied to the electrode 131, the object is attracted to the attracting surface.

[0020] The insulating resin layer 140 is laminated on the ceramic layer 130 and is made of an insulating resin having high thermal conductivity and high heat resistance, such as an epoxy resin, a bismaleimide triazine resin, etc. The insulating resin layer 140 has a thickness of, for example, about 40 to 100 μm.

[0021] The first heating layer 150 is laminated on the insulating resin layer 140, and is a layer made of a heater electrode 151 and an insulating resin 152 that covers the heater electrode 151. The heater electrode 151 is formed on the surface of the insulating resin layer 140, and generates heat when a voltage is applied. The heater electrode 151 is covered with the insulating resin 152. The insulating resin 152 is an insulating resin having high thermal conductivity and high heat resistance, such as an epoxy resin or a bismaleimide triazine resin, like the insulating resin layer 140. The thickness of the insulating resin 152 is, for example, about 40 to 300 μm.

[0022] The second heating layer 160 is laminated on the first heating layer 150 and is a layer including a heater electrode 161, an insulating resin 162 that covers the heater electrode 161, and a power supply unit 163. The heater electrode 161 is formed on the surface of the insulating resin 152 that constitutes the first heating layer 150, and generates heat when a voltage is applied. The heater electrode 161 is covered with the insulating resin 162. The insulating resin 162 is an insulating resin having high thermal conductivity and high heat resistance, such as an epoxy resin or a bismaleimide triazine resin, similar to the insulating resin layer 140 and the insulating resin 152. The thickness of the insulating resin 162 is, for example, about 40 to 300 μm. The power supply unit 163 is a conductive member that supplies power from the base plate 110 to the heater electrode 161. That is, the power supply unit 163 is electrically connected to the base plate 110 and the heater electrode 161, and applies a voltage to the heater electrode 161.

[0023] When a voltage is applied to the heater electrode 151 of the first heating layer 150 and the heater electrode 161 of the second heating layer 160, the heater electrodes 151 and 161 generate heat, thereby heating the ceramic layer 130 and heating the object adsorbed to the ceramic layer 130. The first heating layer 150 and the second heating layer 160 adjust the temperature of the ceramic layer 130 by heating with the heater electrodes 151 and 161 and cooling with the base plate 110, and adjust the temperature of the object adsorbed to the ceramic layer 130 to a desired temperature. Note that the heater electrode 161 of the second heating layer 160 may function as a bypass electrode that electrically connects the heater electrodes 151 of the first heating layer 150 together or electrically connects the heater electrode 151 and the power supply unit 163, instead of functioning as a heater electrode that generates heat.

[0024] The heater electrodes 151, 161 may be made of alloys such as CN49 (constantan) (an alloy of Cu / Ni / Mn / Fe), geranine (an alloy of Cu / Mn / Sn), manganin (an alloy of Cu / Mn / Ni), etc. When the heater electrode 161 is made to function as a bypass electrode, the heater electrode 161 may be made of, for example, copper or a copper alloy. The thickness of the heater electrodes 151, 161 made of these metals is, for example, about 25 to 50 μm, which is within the range of 15 to 200 μm.

[0025] In addition, the thermal conductivity of the insulating resin layer 140, the first heating layer 150, and the second heating layer 160 may be improved by making the insulating resin layer 140, the insulating resin 152, and the insulating resin 162 contain a filler such as alumina or aluminum nitride.

[0026] The via 170 is formed by filling a conductive material such as metal paste or solder into a via hole penetrating the insulating resin 152 of the first heating layer 150 and the heater electrode 161 of the second heating layer 160, and electrically connects the heater electrode 151 of the first heating layer 150 to the heater electrode 161 of the second heating layer 160. Therefore, when a voltage is applied from the power supply unit 163 to the heater electrode 161, the via 170 also applies a voltage to the heater electrode 151 connected to this heater electrode 161. The portion of the via 170 penetrating the insulating resin 152 and the heater electrode 161 may have a tapered shape whose diameter becomes smaller from the heater electrode 161 toward the heater electrode 151.

[0027] The diameter of the portion of the via 170 penetrating the insulating resin 152 and the heater electrode 161 (i.e., the diameter of the via hole) is, for example, within a range of 100 μm to 3 mm. The top 171 of the via 170 on the surface of the heater electrode 161 is larger than the diameter of the via hole and spreads around the via hole. Specifically, the top 171 spreads around the periphery of the via hole by at least 50 μm or more. Therefore, the top 171 is in reliable contact with the surface of the heater electrode 161, and the connection reliability between the heater electrode 151 and the heater electrode 161 can be improved. The thickness of the top 171 of the via 170 is, for example, within a range of 50 to 300 μm and does not exceed the thickness of the insulating resin 162. In other words, the top 171 is covered by the insulating resin 162.

[0028] Next, a method for manufacturing the substrate fixing device 100 configured as above will be described with reference to a flow chart shown in FIG.

[0029] First, a ceramic layer 130 that adsorbs an object is formed (step S101). Specifically, for example, a plurality of green sheets made mainly of aluminum oxide are produced, and an electrode 131 is appropriately formed on one surface of the green sheets. The electrode 131 can be formed, for example, by screen printing a metal paste on the surface of the green sheets. Then, the plurality of green sheets are stacked and fired to form the ceramic layer 130. The ceramic layer 130 has a layer of the electrode 131 inside, for example, as shown in FIG. 4.

[0030] After the ceramic layer 130 is formed, the insulating resin layer 140 is laminated on the surface of the ceramic layer 130 (step S102), and a metal foil layer to become the heater electrode 151 of the first heating layer 150 is laminated on the surface of the insulating resin layer 140 (step S103). Specifically, as shown in Fig. 5, the insulating resin layer 140 having a thickness of, for example, about 40 to 100 µm is laminated on the surface of the ceramic layer 130, and the metal foil layer 151a having a thickness of, for example, about 25 to 50 µm is laminated on the surface of the insulating resin layer 140. The insulating resin layer 140 and the metal foil layer 151a are bonded closely to the ceramic layer 130 by vacuum lamination and vacuum heating and pressure bonding by pressing.

[0031] The insulating resin layer 140 is formed using an insulating resin having high thermal conductivity and high heat resistance, such as an epoxy resin or a bismaleimide triazine resin. The insulating resin layer 140 may contain a filler, such as alumina or aluminum nitride, to improve the thermal conductivity. On the other hand, the metal foil layer 151a may be made of the rolled alloy exemplified as the material of the heater electrodes 151 and 161. That is, the metal foil layer 151a may be made of an alloy, such as CN49 (constantan) (an alloy of Cu / Ni / Mn / Fe), geranine (an alloy of Cu / Mn / Sn), manganin (an alloy of Cu / Mn / Ni), or the like.

[0032] The metal foil layer 151a is etched using, for example, photolithography to form a first heater pattern having a desired pattern (step S104). That is, a resist is formed on the upper surface of the metal foil layer 151a, and the resist is exposed and developed to form a resist pattern that covers the portion to be left as the heater electrode 151. Then, the metal foil layer 151a that is exposed and not covered by the resist pattern is removed by etching to form the heater electrode 151 having a desired pattern, for example, as shown in FIG. 6. In the example shown in FIG. 6, for example, the heater electrode 151 having a double concentric circle pattern is formed.

[0033] Then, the insulating resin 152 that covers the heater electrode 151 is laminated (step S105). Specifically, the insulating resin 152 in a semi-cured state is laminated so as to cover the insulating resin layer 140 and the heater electrode 151, and is heated and pressurized, whereby the insulating resin 152 that covers the heater electrode 151 is cured. As a result, for example, as shown in FIG. 7, the first heating layer 150 laminated on the insulating resin layer 140 is formed.

[0034] Once the first heating layer 150 is formed, a metal foil layer that will become the heater electrodes 161 of the second heating layer 160 is laminated on the surface of the insulating resin 152 that constitutes the first heating layer 150 (step S106). Specifically, as shown in Fig. 8, for example, a metal foil layer 161a having a thickness of, for example, about 25 to 50 µm is laminated on the surface of the first heating layer 150. The metal foil layer 161a is brought into close contact with the first heating layer 150 by vacuum lamination and vacuum heating and pressure bonding by pressing.

[0035] The material of the metal foil layer 161a may be the same as that of the metal foil layer 151a, and may be the rolled alloy exemplified as the material of the heater electrodes 151 and 161. That is, the metal foil layer 161a may be made of an alloy such as CN49 (constantan) (an alloy of Cu / Ni / Mn / Fe), geranine (an alloy of Cu / Mn / Sn), manganin (an alloy of Cu / Mn / Ni), etc. The heater electrode 161 may function as a bypass electrode that electrically connects the heater electrodes 151 of the first heating layer 150 or electrically connects the heater electrode 151 and the power supply unit 163, instead of functioning as a heater electrode that generates heat. When the heater electrode 161 functions as a bypass electrode, a metal having a low electrical resistance, such as copper or a copper alloy, may be used as the material of the metal foil layer 161a.

[0036] The metal foil layer 161a is etched using, for example, photolithography to form a second heater pattern having a desired pattern (step S107). That is, a resist is formed on the upper surface of the metal foil layer 161a, and the resist is exposed and developed to form a resist pattern that covers the portion to be left as the heater electrode 161. Then, the metal foil layer 161a that is not covered by the resist pattern and is exposed is removed by etching to form the heater electrode 161 having a desired pattern, for example, as shown in FIG. 9. The heater electrode 161 is disposed at a position where at least a part of it does not overlap with the heater electrode 151. That is, the heater electrode 161 is formed at a position where, in a plan view, it overlaps with, for example, an area of ​​the first heating layer 150 where the heater electrode 151 is not formed. In addition, an opening 161b is formed in the heater electrode 161 at a position where the via 170 is formed. The opening 161b is formed at a position where the heater electrode 161 overlaps with the heater electrode 151.

[0037] Then, a via hole is formed at the position of the opening 161b (step S108). Specifically, as shown in FIG. 10, for example, a through hole is formed by laser processing in the insulating resin 152 of the first heating layer 150 exposed at the bottom surface of the opening 161b, and a via hole 170a reaching the heater electrode 151 of the first heating layer 150 is formed. At this time, since the via hole 170a is formed at the position of the opening 161b, the heater electrode 161 functions as a mask for the laser processing, and the positional accuracy of the via hole 170a can be ensured, and the taper angle of the via hole 170a can be made close to 0 degrees. The upper surface of the heater electrode 151 is exposed at the bottom surface of the via hole 170a. The via hole 170a may have a tapered shape in which the diameter becomes smaller from the heater electrode 161 to the heater electrode 151. At this time, the taper angle of the via hole 170a is desirably 20 degrees or less with respect to the vertical direction.

[0038] When the hear hole 170a is formed, the via hole 170a is filled with, for example, a metal paste or solder (step S109), and the via 170 is formed. Specifically, as shown in FIG. 11, the via hole 170a is filled with a conductive material such as a semi-hardened silver paste or molten tin-silver-copper solder, and the conductive material is hardened to form the via 170. At this time, a top 171 having a diameter larger than the diameter of the via hole 170a is formed on the upper surface of the heater electrode 161. That is, on the upper surface of the heater electrode 161, the semi-hardened conductive material is hardened in a state in which it spreads around the via hole 170a, and the top 171 that reliably contacts the upper surface of the heater electrode 161 is formed. This can improve the connection reliability between the heater electrode 151 and the heater electrode 161. The method of filling the conductive material may be, for example, thick electroless plating.

[0039] The via 170 electrically connects the heater electrode 151 of the first heating layer 150 and the heater electrode 161 of the second heating layer 160. Therefore, the via 170 is formed at a position where it overlaps with the heater electrode 151 of the first heating layer 150 in a plan view and also overlaps with the heater electrode 161 of the second heating layer 160 in a plan view. For example, as shown in FIG. 12, when the heater electrode 151 of the first heating layer 150 has a double concentric circle pattern, the via 170 is formed at a position where it contacts each of the heater electrodes 151 forming the concentric circle pattern. Also, for example, as shown in FIG. 13, when the heater electrode 161 of the second heating layer 160 is formed at a position where it partially overlaps with the heater electrode 151 in a plan view and the other part does not overlap, the via 170 is formed in a part that overlaps with the heater electrode 151 in a plan view.

[0040] In this way, since the heater electrodes 151, 161 are connected by the vias 170, the degree of freedom in arranging the heater electrodes 151, 161 in the first heating layer 150 and the second heating layer 160 is relatively high. That is, for example, the heater electrode 161 of the second heating layer 160 far from the ceramic layer 130 can flexibly route wiring without imposing restrictions on the heater pattern of the heater electrode 151 of the first heating layer 150. For this reason, it is possible to realize a heater pattern that fully considers thermal uniformity, such as arranging the negative electrode side wiring together or arranging the electrode pad in contact with the power supply unit 163 on the outer periphery of the electrostatic chuck 120. As a result, the temperature distribution in a plan view can be made uniform, and sufficiently high thermal uniformity can be obtained.

[0041] When the heater electrodes 151, 161 are connected by the vias 170, an insulating resin 162 is laminated to cover the heater electrode 161 (step S110). Specifically, the insulating resin 162 in a semi-cured state is laminated so as to cover the first heating layer 150 and the heater electrode 161, and is heated and pressurized to cure the insulating resin 162 covering the heater electrode 161. As a result, for example, as shown in FIG. 14, the second heating layer 160 laminated on the first heating layer 150 is formed.

[0042] Then, an opening is formed in the insulating resin 162 at a position corresponding to the electrode pad of the heater electrode 161 of the second heating layer 160 (step S111). That is, in order to expose the heater electrode 161 at a position that will become the electrode pad in contact with the power supply part 163, an opening 162a is formed in the insulating resin 162 as shown in Fig. 15, for example. As a result, the electrostatic chuck 120 having two layers of heater electrodes 151, 161 connected by the via 170 is obtained.

[0043] The electrostatic chuck 120 is bonded to the base plate 110 by an adhesive (step S112). Specifically, the surface of the insulating resin 162 of the second heating layer 160 in which the opening 162a is formed is bonded to the base plate 110 by, for example, a silane coupling agent and an adhesive. At this time, by bonding the opening 162a to match the position of the power supply part 163, the power supply part 163 and the heater electrode 161 come into contact with each other, and power can be supplied to the heater electrode 161. Furthermore, since the heater electrode 161 is connected to the heater electrode 151 through the via 170, power can also be supplied to the heater electrode 151. By bonding the electrostatic chuck 120 to the base plate 110, the substrate fixing device 100 is completed.

[0044] As described above, according to the present embodiment, the electrostatic chuck is provided with two heater layers, and the heater electrodes of the heater layers are connected by vias. The vias are formed by filling via holes penetrating the insulating resin and the heater electrodes, and the tops of the vias have a larger diameter than the via holes. This allows for a high degree of freedom in the arrangement of the heater electrodes, and a heater pattern that takes thermal uniformity into consideration can be realized to obtain sufficiently high thermal uniformity, while improving the connection reliability of the heater electrodes of each layer by the vias.

[0045] In the above embodiment, two heater layers, the first heating layer 150 and the second heating layer 160, are provided on the electrostatic chuck 120, but it is also possible to provide three or more heater layers on the electrostatic chuck 120. Even when three or more heater layers are provided, the heater electrodes of each heater layer are electrically connected by vias having a configuration similar to that of the via 170. This increases the degree of freedom in arranging the heater electrodes and improves the connection reliability of the heater electrodes of each heater layer.

[0046] Incidentally, an electrode pad is formed on a portion of the heater electrode 151 of the first heating layer 150 that contacts the via 170, and on a portion of the heater electrode 161 of the second heating layer 160 that contacts the power supply unit 163. The electrode pad is an area having a certain diameter or more to ensure a reliable connection to the via 170 or the power supply unit 163, and the periphery of the electrode pad tends to be a blank area of ​​the heater pattern. For this reason, the temperature around the electrode pad tends to decrease, which may lead to a decrease in thermal uniformity.

[0047] Therefore, in the above embodiment, the electrode pad of one heat generating layer may be overlapped with the heater pattern of the other heat generating layer, thereby preventing a drop in temperature around the electrode pads and improving thermal uniformity.

[0048] 16 and 17 are diagrams showing specific examples of the positional relationship between the heater pattern and the electrode pads. Fig. 16 shows a first heater pattern formed by the heater electrode 151 of the first heat generating layer 150, and Fig. 17 shows a second heater pattern formed by the heater electrode 161 of the second heat generating layer 160.

[0049] 16, the heater electrode 151 is separated into an inner heater pattern and an outer heater pattern, an electrode pad 210 is formed on the inner heater pattern, and an electrode pad 220 is formed on the outer heater pattern. The tip of a via 170 connecting the heater electrode 151 and the heater electrode 161 contacts these electrode pads 210, 220.

[0050] 17, a via 170 is formed at a position corresponding to the electrode pads 210, 220, and the via 170 is surrounded by the heater electrode 161 of the second heating layer 160. The diameter of the via 170 is smaller than the diameter of the electrode pads 210, 220, and the periphery of the via 170 is surrounded by the heater electrode 161, so that the blank space of the heater pattern caused by the electrode pads 210, 220 of the heater electrode 151 is complemented by the heater electrode 161. That is, even around the electrode pads 210, 220 of the first heating layer 150, a drop in temperature can be prevented by the heater electrode 161 of the second heating layer 160.

[0051] The heater electrode 161 of the second heating layer 160 is separated into an inner heater pattern and an outer heater pattern corresponding to the heater electrode 151 of the first heating layer 150. An electrode pad 215 is formed in a position different from the via 170 of the inner heater pattern, and an electrode pad 225 is formed in a position different from the via 170 of the outer heater pattern. A power supply unit 163 that connects the heater electrode 161 and the base plate 110 comes into contact with these electrode pads 215, 225.

[0052] The areas around the electrode pads 215, 225 are left blank in the heater pattern, but because the positions of the electrode pads 215, 225 overlap with the heater electrode 151 of the first heating layer 150, this blank in the heater pattern is complemented by the heater electrode 151. In other words, even around the electrode pads 215, 225 of the second heating layer 160, the heater electrode 151 of the first heating layer 150 can prevent a drop in temperature.

[0053] In this way, the electrode pad of one heat generating layer is overlapped with the heater pattern of the other heat generating layer, so that the gap of the heater pattern by the electrode pad is filled, and the decrease in the uniformity of heat caused by the temperature drop around the electrode pad can be suppressed. Also, in the above-mentioned example, the heater electrode 161 of the second heat generating layer 160 can be made into an arbitrary shape, and the electrode pads 215, 225 can be flexibly arranged. Therefore, the heater electrode 161 and the electrode pads 215, 225 can be prevented from interfering with other wiring, etc. [Explanation of symbols]

[0054] 110 Base Plate 111 Cooling Channel 120 Electrostatic Chuck 130 Ceramic Layer 131 Electrode 140 Insulating resin layer 150 First heating layer 151, 161 Heater electrode 152, 162 Insulating resin 160 Second heating layer 163 Power Supply Unit 170 Beer 170a Beer Hall 171 Top 210, 215, 220, 225 Electrode pads

Claims

1. A base plate; an electrostatic chuck fixed to the base plate and configured to attract the substrate by electrostatic force; The electrostatic chuck comprises: an adsorption layer formed of ceramic and in contact with the substrate to adsorb and hold the substrate; a first heat generating layer that is laminated on the adsorption layer and has a first electrode that generates heat; a second heating layer including a second electrode that is laminated on the first heating layer and generates heat; a via having both ends connected to the first electrode and the second electrode, at least one end penetrating the first electrode or the second electrode, and an end portion having a diameter larger than a diameter of the penetrating portion at the one end; A substrate fixing device comprising:

2. The adsorption layer is An electrode to which a voltage can be applied; A ceramic surrounding the electrode; 2. The substrate fixing device according to claim 1, further comprising:

3. The first heating layer is 2. The substrate fixing device according to claim 1, further comprising an insulating resin covering the first electrode.

4. The second heating layer is 2. The substrate fixing device according to claim 1, further comprising an insulating resin that covers the second electrode.

5. The via is The substrate fixing device according to claim 1 , wherein the substrate fixing device is formed at a position overlapping the first electrode and the second electrode in a plan view.

6. The base plate is 2. The substrate fixing device according to claim 1, further comprising a coolant passage for allowing a coolant to pass therethrough.

7. The first heating layer is 2. The substrate fixing device according to claim 1, further comprising a first electrode pad formed on the first electrode at a position overlapping the second electrode in a plan view.

8. The first electrode pad is 8. The substrate fixing device according to claim 7, wherein the substrate fixing device contacts the other end of the via.

9. The second heating layer is 2. The substrate fixing device according to claim 1, further comprising a second electrode pad formed on the second electrode at a position overlapping the first electrode in a plan view.

10. The second electrode pad is 10. The substrate fixing device according to claim 9, wherein the substrate fixing device contacts a power supply section from the base plate.

11. an adsorption layer formed of ceramic and adapted to adsorb and hold an object by electrostatic force; a first heat generating layer that is laminated on the adsorption layer and has a first electrode that generates heat; a second heating layer including a second electrode that is laminated on the first heating layer and generates heat; a via having both ends connected to the first electrode and the second electrode, at least one end penetrating the first electrode or the second electrode, and an end portion having a diameter larger than a diameter of the penetrating portion at the one end; Electrostatic chuck comprising:

12. forming an electrode and a ceramic layer made of ceramic surrounding the electrode; a heat generating layer including a first electrode that generates heat and an insulating resin that covers the first electrode is laminated on the ceramic layer; a second electrode having an opening and generating heat is formed on a surface of the insulating resin of the heat generating layer; forming a via hole penetrating the insulating resin at the position of the opening and exposing the first electrode; filling the formed via hole with a conductive material to form a via connecting the first electrode and the second electrode; covering the formed via and the second electrode with an insulating resin; The step of forming a via includes: A via is formed at one end penetrating the second electrode, the end having a diameter larger than the diameter of the opening. A method for manufacturing an electrostatic chuck comprising the steps of:

Citation Information

Patent Citations

  • Connecting structure of wiring and formation thereof

    JP1983087845A

  • JP1990063542U

  • Power switching system for esc with array of thermal control elements

    JP2014112672A

  • Electrostatic chuck and manufacturing method for the same

    JP2016100474A

  • Electrostatic chuck

    JP2016136611A