Steel plate polishing equipment and method for manufacturing annealed steel plates
The steel plate polishing apparatus with a brush roll and recovery device addresses the issue of oxide buildup on conveyor rolls by efficiently removing these deposits, thereby preventing defects in steel sheets during continuous annealing.
Patent Information
- Application Number
- JP2023214762
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-12-20
- Publication Date
- 2026-11-11
- Estimated Expiration
- 2043-12-20
AI Technical Summary
Existing methods for removing deposits from conveyor rolls in continuous annealing facilities are insufficient in preventing the rapid growth of oxides from easily oxidizable elements like Si and Mn, leading to press flaws on steel sheets.
A steel plate polishing apparatus with a brush roll having metal wires projecting radially from its surface, used to polish steel plates before they enter the conveyor rolls, accompanied by a recovery device to collect detached materials.
Effectively removes oxides from steel plates before they adhere to conveyor rolls, inhibiting deposit growth and preventing indentation defects on the steel sheets.
Smart Images

Figure 0007948156000003 
Figure 0007948156000004 
Figure 0007948156000005
Abstract
Description
Technical Field
[0001] The present invention relates to a steel sheet polishing apparatus for polishing a steel sheet in continuous annealing equipment and a method for manufacturing an annealed steel sheet.
Background Art
[0002] In recent years, demand for high-tensile steel sheets has increased, and the production ratio of high-tensile steel sheets is rising. It has been shown that the addition of Si and Mn to high-tensile steel sheets enables the production of steel sheets that are advantageous in terms of strength and workability. On the other hand, when manufacturing high-tensile steel sheets in a continuous annealing process, a treatment for cooling the heated steel sheet is required from the viewpoint of increasing strength. Further, from the viewpoint of press formability, a tempering treatment for reheating the cooled steel sheet is necessary.
[0003] A steel sheet is subjected to a tempering treatment through an annealing process in which, for example, it is preheated to about 150°C in a preheating zone, heated to about 800°C in an oxidation-reduction zone, and quenched to 500°C in a quenching zone. At that time, in steel sheets containing easily oxidizable elements such as Si and Mn, additive elements such as Si and Mn concentrate on the steel sheet surface in the reduction zone, and these oxides are generated. The roll deposits formed by these oxides adhering to the conveyance rolls cause press flaws (surface defects) on the steel sheet.
[0004] As a technique for preventing press flaws on steel sheets caused by roll deposits, Patent Document 1 discloses a method of preventing press flaws by using an abrasion-resistant coating to cause roll deposit substances to fall off as abrasion proceeds. Patent Document 2 discloses a method of detecting deposits with an image processing device and removing the deposits on the roll surface with a contact member.
Prior Art Documents
Patent Documents
[0005]
Patent Document 1
Patent Document 2
Summary of Invention
[0006] Although the technologies disclosed in Patent Documents 1 and 2 can remove deposits from the rolls, they are insufficient in suppressing the rapid growth of deposits on the conveyor rolls of steel sheets containing easily oxidizable elements such as Mn and Si in a high-temperature environment in a continuous annealing facility. The present invention has been made in view of these problems of the prior art, and its purpose is to provide a steel sheet polishing facility that can remove oxides formed on the steel sheet in a continuous annealing facility before they adhere to the conveyor rolls, and a method for manufacturing annealed steel sheets by polishing the steel sheet with the polishing facility and manufacturing the annealed steel sheet in a continuous annealing facility. [Means for solving the problem]
[0007] The means to solve the above problems are as follows: [1] A steel plate polishing apparatus for polishing steel plates in a continuous annealing apparatus having a plurality of conveying rolls, comprising: a first polishing roll for polishing the steel plates; and a drive device for rotating the first polishing roll. [2] The steel plate polishing apparatus according to [1], wherein the first polishing roll is a brush roll having a plurality of metal wires projecting radially from the circumferential surface. [3] The steel plate polishing apparatus according to [2], wherein the diameter of the wire is 20 μm or more and 500 μm or less. [4] The steel plate polishing equipment according to [2] or [3], wherein the wire is made of tungsten, molybdenum, cobalt, nickel-chromium alloy or stainless steel. [5] A steel plate polishing apparatus according to any one of [1] to [4], having a polishing member that contacts the first polishing roll, wherein the polishing member is a flat plate, a grinding wheel, or a second polishing roll. [6] A steel plate polishing apparatus according to any one of [1] to [5], comprising a recovery device for collecting material that has fallen off the first polishing roll. [7] A method for manufacturing an annealed steel sheet, comprising polishing a steel sheet with a steel sheet polishing facility described in any of [1] to [4], and then annealing it with the continuous annealing facility to produce an annealed steel sheet. [Effects of the Invention]
[0008] By using the steel plate polishing equipment according to the present invention, deposits such as oxides formed on the steel plate in the continuous annealing equipment can be removed before they adhere to the conveyor rolls. This suppresses the adhesion of deposits to the conveyor rolls, thereby inhibiting the growth of deposits that do adhere to the conveyor rolls. [Brief explanation of the drawing]
[0009] [Figure 1] Figure 1 is a schematic diagram showing an example of the configuration of a continuous annealing facility. [Figure 2] Figure 2 is a schematic side view showing an example of the configuration of a steel plate polishing equipment according to this embodiment. [Figure 3] Figure 3 is a schematic side view of the conveyor rolls used in the heating zone of a continuous annealing facility. [Figure 4] Figure 4 is a schematic side view showing another configuration example of the steel plate polishing equipment according to this embodiment. [Figure 5] Figure 5 is a schematic side view showing another configuration example of the steel plate polishing equipment according to this embodiment. [Modes for carrying out the invention]
[0010] The present invention will be described below through embodiments of the present invention. However, the following embodiments are merely preferred examples of the present invention, and the present invention is not limited in any way by these embodiments.
[0011] The steel plate polishing equipment according to this embodiment is suitably used for polishing steel plates 10 in a continuous annealing equipment 100. First, the continuous annealing equipment 100 will be described. Figure 1 is a schematic diagram showing an example of the configuration of the continuous annealing equipment 100. The continuous annealing equipment 100 includes a heating zone 12, a soaking zone 14, a cooling zone 16, and an over-aging zone 18. The continuous annealing equipment 100 may also be equipped with equipment for surface treatment such as zinc plating, as needed.
[0012] The heating zone 12 is equipped with a device for raising the temperature of the steel plate 10. In the heating zone 12, a direct flame or radiant combustion burner is used. In the heating zone 12, the steel plate 10 is heated to a preset temperature of approximately 600 to 900°C, depending on its composition.
[0013] The uniform temperature zone 14 is equipped with a device for maintaining the steel plate 10 at a predetermined temperature. The device for maintaining the steel plate 10 at a predetermined temperature has a heating capacity sufficient to compensate for the heat dissipated from the furnace body, etc.
[0014] The cooling zone 16 is equipped with facilities for cooling the steel plate 10 to a predetermined temperature. Cooling methods used in the cooling zone 16 include liquid cooling, gas jet cooling, roll cooling, and mist cooling (gas-liquid mixed cooling). Liquid cooling is often performed by water cooling (water quenching). Water cooling is a cooling method in which the steel plate 10 is immersed in a water tank installed downstream of the uniform zone 14. Gas jet cooling is a cooling method in which gas is blown onto the surface of the steel plate 10 from a nozzle. Roll cooling is a cooling method in which the steel plate 10 is cooled by contacting it with a water-cooled roll. Mist cooling is a cooling method in which water is sprayed in a fine mist form, and the steel plate 10 is cooled by the absorption of heat of vaporization. In mist cooling, the size of the sprayed water droplets is often about 0.1 to 1 mm.
[0015] The overaging zone 18 is equipment that performs an overaging treatment in which the steel sheet 10 is reheated to a temperature of about 300 to 400°C and held at that temperature for a predetermined time. In such a continuous annealing equipment 100, the steel sheet 10 is heated and subjected to reduction treatment in the heating zone 12 and the soaking zone 14 in a reducing atmosphere composed of a mixed gas such as hydrogen and nitrogen, cooled in the cooling zone 16, and subjected to tempering treatment in the overaging zone 18.
[0016] When the content of Si or Mn in the steel sheet 10 processed by the continuous annealing equipment 100 is 0.3 mass% or more, Si and Mn in the steel sheet 10 are oxidized and tend to concentrate in the surface layer. Si and Mn are elements effective for improving the mechanical properties of the steel sheet 10, and between Si and Mn, Si is more easily oxidized. For this reason, in the case of Si-added steel, Si oxide is generated on the surface layer of the steel sheet 10, while the generation of Mn oxide tends to be suppressed. However, in a steel sheet with a low Si content, Mn is most likely to concentrate in the surface layer, so Mn oxide of the steel sheet 10 is generated and concentrated in the surface layer.
[0017] The concentration of oxides in the surface layer of the steel sheet 10 and the adhesion of the oxides to the conveying rolls have a high correlation with the temperature of the steel sheet 10. The higher the temperature of the steel sheet 10, the more the concentration of Si and Mn oxides on the surface layer of the steel sheet 10 is promoted. The Si and Mn oxides concentrated on the surface layer of the steel sheet 10 adhere to the surface of the conveying rolls. When the Si and Mn oxides adhering to the surface of the conveying roll are heated, a sintered body of the oxides is formed and fixed to the surface of the conveying roll. Since the temperature at which the sintered body is formed is about half the melting point of the oxide, this phenomenon becomes remarkable when the surface temperature of the conveying roll reaches 700°C or higher.
[0018] In a vertical continuous annealing equipment, the steel sheet 10 is conveyed while being wound around the conveying rolls, so strain corresponding to the roll curvature of the conveying rolls is introduced. In order to reduce the introduction of strain during conveyance, a conveying roll with a larger diameter is used in the vertical continuous annealing equipment compared with a horizontal continuous annealing equipment. A conveying roll having a diameter of 400 mm or more is suitably used in the vertical continuous annealing equipment.
[0019] On the other hand, as the diameter of the conveying roll increases, thermal expansion causes the diameter of the central part of the conveying roll in the axial direction to become larger than the diameters of the ends, and the difference in the circumference of the roll between the central part and the ends becomes larger. As a result, a speed difference is created between the steel plate 10 and the conveying roll depending on the axial position of the conveying roll, and the friction between the steel plate 10 and the surface of the conveying roll makes it easier for oxides concentrated on the surface of the steel plate 10 to adhere to the conveying roll.
[0020] The conveying rolls of the continuous annealing equipment 100 are coated with cermet or ceramics to reduce reactivity and adhesion with adhering materials. However, even with such rolls, if the oxide concentrated on the surface of the steel plate 10 adheres firmly to the conveying roll, it does not easily fall off the roll surface, and the adhering material grows from that point, causing indentation defects in the conveyed steel plate 10.
[0021] To suppress the occurrence of such indentation defects, a steel plate polishing facility according to this embodiment is provided upstream of the conveying direction of the steel plate 10 relative to the conveying roll. This allows concentrated oxides and other deposits on the surface of the steel plate 10 to be removed by the polishing facility before they adhere to the conveying roll, thereby suppressing the adhesion and growth of deposits on the surface of the conveying roll and preventing the occurrence of indentation defects on the steel plate 10.
[0022] Furthermore, as described above, when the surface temperature of the conveying rolls exceeds 700°C, oxides tend to adhere to and solidify on the conveying rolls. Therefore, the steel plate polishing equipment according to this embodiment is preferably used for polishing steel plates 10 that are conveyed in the heating zone 12 or homogenization zone 14 of the continuous annealing equipment 100, where the steel plates 10 are heated to 700°C or higher. However, even at temperatures below 700°C, concentrated oxides adhere to the surface layer of the steel plates 10, so the steel plate polishing equipment according to this embodiment may also be applied to steel plates 10 that are conveyed at temperatures below 700°C.
[0023] Figure 2 is a schematic side view showing an example of the configuration of the steel plate polishing equipment 30 according to this embodiment. The steel plate polishing equipment 30 according to this embodiment includes a first polishing roll 32, a flat plate 34, a recovery container 36, and a drive device (not shown) for rotating the first polishing roll 32. The first polishing roll 32 is provided upstream of the conveying direction of the steel plate 10 relative to the conveying roll 20 on the furnace top side, and is in contact with the steel plate 10.
[0024] The first polishing roll 32 is preferably positioned to polish the surface of the steel plate 10 that comes into contact with the conveying roll 20 located downstream of the steel plate polishing equipment 30 in the direction of transport of the steel plate 10, on either the front or back surface of the steel plate 10. However, the continuous annealing equipment 100 is provided with a large number of conveying rolls 20, and the surfaces that come into contact with the conveying rolls 20 and the steel plate 10 alternate. Therefore, the surface of the steel plate 10 polished by the steel plate polishing equipment 30 according to this embodiment may be either the front or back surface of the steel plate 10.
[0025] The first polishing roll 32 is a brush roll having multiple metal wires that protrude radially from the circumferential surface of the roll. By using a brush roll for the first polishing roll 32, even if deposits removed from the steel plate 10 adhere to the first polishing roll 32, the starting point of the deposits becomes the tips of the wires rather than the surface, resulting in a smaller contact area and thus a reduced adhesive force. Therefore, even if deposits adhere to the first polishing roll 32, the adhesive force between the polishing roll and the deposits is small, allowing the deposits to be easily removed from the first polishing roll 32.
[0026] The first polishing roll 32 is preferably a barrel-shaped roll (crown roll) in which the diameter of the central part in the axial direction of the first polishing roll 32 is larger than the diameter of both ends, and the central part and both ends are smoothly connected by a tapered or R-shaped shape. Figure 3 is a schematic side view of a conveying roll 20 used in the heating zone 12 of the continuous annealing equipment 100. As shown in Figure 3, when the conveying roll 20 is used in the heating zone 12 or sonication zone 14 of the continuous annealing equipment 100, the conveying roll 20 expands due to contact with the high-temperature steel plate 10, and a thermal crown is formed on the conveying roll 20. Since the conveyed steel plate 10 is also deformed by the thermal crown of the conveying roll 20, it is preferable that the first polishing roll 32 is also a barrel-shaped roll corresponding to the shape of the thermal crown. The shape of the thermal crown of the conveying roll 20 can be estimated in advance by analysis using continuous annealing conditions.
[0027] The first polishing roll 32 is rotated by a drive device in the same direction as the steel plate 10 at the contact point with the steel plate 10, and at a speed difference between the two. By rotating the first polishing roll 32 in the same direction as the steel plate 10 at the contact point with the steel plate 10, and at a speed difference, over-polishing of the steel plate 10 can be suppressed, and deposits such as concentrated oxides on the surface of the steel plate 10 can be removed. On the other hand, if the first polishing roll 32 is rotated in the opposite direction at the contact point with the steel plate 10, it will result in over-polishing and scratches on the steel plate 10, which is undesirable.
[0028] It is preferable to rotate the first polishing roll 32 so that the speed difference between the steel plate 10 and the first polishing roll 32 is between 0.5 m / min and 15 m / min. This allows for efficient removal of deposits such as concentrated oxides on the surface while suppressing scratches on the steel plate 10. On the other hand, if the speed difference between the steel plate 10 and the first polishing roll is less than 0.5 m / min, it becomes difficult to efficiently remove deposits, which is undesirable. Also, if the speed difference between the steel plate 10 and the first polishing roll is greater than 15 m / min, scratches on the steel plate 10 become more pronounced, which is undesirable.
[0029] The diameter of the brush roll wire is preferably between 20 μm and 500 μm. This allows for improved adhesion removal while suppressing increases in manufacturing costs and shortening of the brush roll's lifespan. On the other hand, a wire diameter of less than 20 μm is undesirable because it makes mass production of brush rolls difficult and increases manufacturing costs. Furthermore, a wire diameter of less than 20 μm is undesirable because it leads to faster wire wear and a shorter brush roll lifespan. Also, a wire diameter greater than 500 μm is undesirable because it increases the contact area between the adhesion and the wire, reducing the adhesion removal efficiency.
[0030] The wire is preferably made of tungsten, molybdenum, cobalt, nickel-chromium alloy, or stainless steel, which have heat resistance and wear resistance. This allows the steel plate 10 to be polished and contaminants removed even in high-temperature environments of 700°C or higher.
[0031] It is preferable to use a heat-resistant metal such as heat-resistant cast steel, chromium alloy, or nickel alloy for the roll portion of the first polishing roll 32. The roll diameter of the first polishing roll 32 is smaller than the roll diameter of the conveying roll 20, and is preferably 100 mm or more. This suppresses a decrease in the roll life of the first polishing roll 32 and deformation due to bending. Furthermore, it is preferable that the wire density in the first polishing roll 32 is 3 / 5 or more of the roll surface area in which the wire is embedded. By using a high-density brush roll with a high wire density, wire damage due to wear is reduced, and the durability of the brush roll is improved.
[0032] The flat plate 34 is a steel or ceramic plate that contacts the first polishing roll 32 and polishes the first polishing roll. By polishing the first polishing roll 32 with the flat plate 34, any deposits removed from the steel plate 10 that adhere to the first polishing roll 32 can be removed. Note that the flat plate 34 is just one example of a polishing member that contacts the circumferential surface of the first polishing roll 32, and a grinding wheel or polishing roll may be used instead of the flat plate.
[0033] The recovery container 36 is a steel box for collecting material that detaches from the first polishing roll 32 (hereinafter referred to as "detached material"). By providing the recovery container 36, the detached material from the first polishing roll 32 can be collected, and it is possible to prevent the detached material from reattaching to the steel plate 10 or to the continuous annealing equipment 100. Note that the recovery container 36 is an example of a recovery device for collecting detached material from the first polishing roll 32.
[0034] Figure 4 is a schematic side view showing another configuration example of the steel plate polishing equipment according to this embodiment. In the steel plate polishing equipment 40 shown in Figure 4, the same reference numerals are used for components that are the same as those in the steel plate polishing equipment 30 shown in Figure 2, and their descriptions are omitted. The steel plate polishing equipment 40 shown in Figure 4 differs from the steel plate polishing equipment 30 shown in Figure 2 in that it has a second polishing roll 38 instead of a flat plate 34.
[0035] As shown in Figure 4, the first polishing roll 32 may be polished using a second polishing roll 38. The second polishing roll 38 is, for example, a roll made of heat-resistant cast steel with a cermet or ceramic spray coating applied to its circumferential surface. The second polishing roll 38 is another example of a polishing member that contacts the circumferential surface of the first polishing roll 32.
[0036] Preferably, the second polishing roll 38 is rotated in a direction opposite to the rotation direction of the first polishing roll 32 at the contact position with the first polishing roll 32. This promotes the removal of any deposits adhering to the first polishing roll 32.
[0037] Furthermore, since a brush roll is used for the first polishing roll 32, if there is a difference in peripheral speed between the first polishing roll 32 and the second polishing roll 38, it is not necessary to rotate them in opposite directions at the contact point. In other words, if there is a difference in peripheral speed between the first polishing roll 32 and the second polishing roll 38, the second polishing roll 38 may be rotated in the same direction as the rotation direction of the first polishing roll 32 at the contact point between the first polishing roll 32 and the second polishing roll 38.
[0038] Figure 5 is a schematic side view showing another configuration example of the steel plate polishing equipment according to this embodiment. In the steel plate polishing equipment 50 shown in Figure 5, the same reference numerals are used for components that are the same as those in the steel plate polishing equipment 30 shown in Figure 2, and their descriptions are omitted. The steel plate polishing equipment 50 shown in Figure 5 differs from the steel plate polishing equipment 30 shown in Figure 2 in that the steel plate polishing equipment 50 is located near the conveying rolls 20 on the hearth side. As shown in Figure 5, the steel plate polishing equipment 50 according to this embodiment can also be provided on the upstream side of the conveying direction of the steel plate 10 of the conveying rolls 20 located on the hearth side.
[0039] As described above, the steel plate polishing equipment according to this embodiment can be installed in the transport path of the steel plate 10 in the continuous annealing equipment 100, so it is preferable to install multiple units in the continuous annealing equipment 100. By installing multiple units of the steel plate polishing equipment according to this embodiment, the ability to remove deposits adhering to the steel plate 10 can be increased.
[0040] As described above, by using the steel plate polishing equipment according to this embodiment, deposits such as oxides formed on the steel plate 10 can be removed before they adhere to the conveyor roll 20, thereby suppressing the adhesion and growth of deposits on the surface of the conveyor roll 20. Furthermore, by suppressing the growth of deposits on the conveyor roll 20 in this way, the occurrence of indentation defects in the steel plate 10 caused by such deposits can also be suppressed. In other words, by polishing the steel plate 10 with the steel plate polishing equipment according to this embodiment in the continuous annealing equipment 100, it becomes possible to manufacture annealed steel plates with suppressed indentation defects.
[0041] In this embodiment, the example described uses a brush roll as the first polishing roll in the steel plate polishing equipment 30, 40, and 50, but it is not limited to this. A polishing roll made of heat-resistant cast steel with cermet spraying or ceramic spraying applied to its circumferential surface may also be used as the first polishing roll. However, as mentioned above, by using a brush roll as the first polishing roll, any deposits that adhere to the brush roll can be easily removed. Therefore, it is preferable that the first polishing roll be a brush roll.
[0042] Furthermore, although this embodiment describes steel plate polishing equipment 30, 40, and 50 having polishing members and recovery devices, it is not limited to this. As a configuration to solve the problem of removing deposits from the steel plate 10, the steel plate polishing equipment 30, 40, and 50 do not necessarily have polishing members and recovery devices. However, as described above, having polishing members makes it possible to remove deposits attached to the first polishing roll, and having a recovery device prevents the deposits removed from the first polishing roll from reattaching to the steel plate 10, etc. Therefore, it is preferable that the steel plate polishing equipment 30, 40, and 50 have polishing members and recovery devices. [Examples]
[0043] [Example 1] Next, we will describe Example 1, in which we continuously annealed 2000 tons or more of steel sheets containing 0.3 mass% or more of Si or Mn in the continuous annealing equipment 100 shown in Figure 1, and then confirmed the number of deposits of 100 μm or more attached to the conveyor rolls. In Example 1, the thickness of the steel sheets continuously annealed was in the range of 0.6 to 1.8 mm, and the width was in the range of 800 to 1500 mm. The continuous annealing conditions were as follows.
[0044] Ambient temperature: 700℃ or higher Atmosphere gas: 5% hydrogen by volume, 95% nitrogen by volume Dew point: -35℃
[0045] After continuous annealing, the conveyor roll installed on the furnace top side of the soaking zone downstream of the continuous annealing equipment 100, where the steel plate temperature is highest, was removed, and the number of deposits larger than 100 μm attached to the conveyor roll was confirmed using a laser microscope.
[0046] In the example invention, the steel plate polishing equipment 30 shown in Figure 2 was installed upstream of the conveying roll and on the side that contacts the conveying roll. As the first polishing roll, a polishing roll or brush roll was used, which had a roll diameter of 300 mm and was made of heat-resistant cast steel with cermet spraying on its circumferential surface. The wire of the brush roll was made of Ni-Cr alloy, with a wire diameter of 300 μm and a length to the wire tip of 15 mm, and the wire density was 3 / 5 as the ratio of the wire embedding area to the roll surface area. The speed difference between the roll rotation speed of the first polishing roll and the steel plate speed was 2 m / min, and the pressing force of the first polishing roll against the steel plate was adjusted to 0.02 kgf / mm. A ceramic plate was used as the polishing member. On the other hand, in the comparative example, continuous annealing was performed without installing the steel plate polishing equipment 30. The results of Example 1 are shown in Table 1 below.
[0047] [Table 1]
[0048] As shown in Table 1, in Invention Example 1-4, where the steel plate was polished with the first polishing roll, the number of deposits larger than 100 μm adhering to the surface of the conveyor roll was reduced compared to the comparative example, which did not use the first polishing roll. From these results, it was confirmed that by using the steel plate polishing equipment according to this embodiment, deposits on the steel plate can be removed before they adhere to the conveyor roll, thereby suppressing the adhesion and growth of deposits on the surface of the conveyor roll.
[0049] Furthermore, in Invention Examples 2 and 4, where a brush roll was used as the first polishing roll, the number of deposits larger than 100 μm adhering to the surface of the conveyor roll was reduced compared to Invention Examples 1 and 3, where a conventional polishing roll was used. From these results, it was confirmed that using a brush roll as the first polishing roll is preferable, and that this can further reduce the number of deposits adhering to the conveyor roll.
[0050] Furthermore, in Invention Examples 1 and 2, which provided a ceramic plate as an abrasive member, the number of deposits larger than 100 μm adhering to the surface of the conveyor roll was reduced compared to the corresponding Invention Examples 3 and 4. From these results, it was confirmed that it is preferable to provide an abrasive member for polishing the first abrasive roll, and that this can further reduce the number of deposits adhering to the conveyor roll.
[0051] [Example 2] Next, we will describe Example 2, which confirmed the effect of wire diameter on the brush roll. In Example 2, a steel plate with a Si content of 1.6 mass% and a Mn content of 0.3 mass% was polished with a small sample of the brush roll in a furnace where the furnace temperature was controlled to 800°C, and the adhesion of deposits to the brush roll as a result of the polishing was confirmed. The test conditions for Example 2 are as follows.
[0052] Wire material: Ni-Cr alloy Wire length: 12mm Sliding time: 30 hours Sliding speed: 300 mm / min Surface pressure between steel plate and brush roll: 0.001 kg / mm 2 Brush roll wire density: 3 / 5 (ratio of wire embedding area to roll surface area)
[0053] After polishing a steel plate with a brush roll for 30 hours under the above test conditions, the number of deposits larger than 30 μm attached to the brush roll and the amount of wire wear after polishing were measured. The number of deposits larger than 30 μm attached to the surface of the brush roll was measured by observing the surface of the brush roll with a laser microscope. The amount of wire wear was measured by measuring the wire length before and after the sliding test, and the difference between these two values was taken as the amount of wear. The results of Example 2 are shown in Table 2 below.
[0054] [Table 2]
[0055] As shown in Table 2, reducing the diameter of the brush roll wire increased the amount of wire wear. In particular, it was confirmed that the amount of wire wear increased significantly when the wire diameter was less than 20 μm. From these results, it was confirmed that a wire diameter of 20 μm or more is preferable, as this can suppress wire wear.
[0056] On the other hand, as the wire diameter increases, the contact area with the deposits increases, and the adhesion force of the deposits to the brush roll surface increases. In particular, when the wire diameter exceeds 500 μm, the adhesion force of the deposits to the brush roll increases, and the number of deposits larger than 30 μm adhering to the brush roll surface increases significantly. From these results, it was confirmed that the wire diameter of the brush roll is preferably 500 μm or less, as this can suppress the adhesion of deposits. [Explanation of Symbols]
[0057] 10 steel plate 12 Heating Zone 14. Average Tropical 16 Cooling Zones 18 Overaged zone 20 Conveyor Rolls 30 Steel plate polishing equipment 32. First polishing roll 34 flat plate 36 Collection containers 38. Second polishing roll 40 Steel plate polishing equipment 50 Steel plate polishing equipment 100 Continuous Annealing Equipment
Claims
1. A steel plate polishing apparatus for polishing steel plates in a continuous annealing apparatus having multiple conveyor rolls, A first polishing roll for polishing the steel plate, A drive device for rotating the first polishing roll, A collection device for collecting material that has fallen off the first polishing roll, A steel plate polishing machine having [a specific feature / feature].
2. The steel plate polishing apparatus according to claim 1, wherein the first polishing roll is a brush roll having a plurality of metal wires protruding radially from its circumferential surface.
3. The steel plate polishing apparatus according to claim 2, wherein the diameter of the wire is 20 μm or more and 500 μm or less.
4. The steel plate polishing apparatus according to claim 2 or 3, wherein the wire is made of tungsten, molybdenum, cobalt, nickel-chromium alloy, or stainless steel.
5. Having an abrasive member that contacts the first abrasive roll, The steel plate polishing apparatus according to any one of claims 1 to 3, wherein the polishing member is a flat plate, a grinding wheel, or a second polishing roll.
6. Having an abrasive member that contacts the first abrasive roll, The steel plate polishing apparatus according to claim 4, wherein the polishing member is a flat plate, a grinding wheel, or a second polishing roll.
7. A method for manufacturing an annealed steel sheet, comprising polishing a steel sheet using a steel sheet polishing equipment described in any one of claims 1 to 3, and then annealing it using the continuous annealing equipment to produce an annealed steel sheet.
8. A method for manufacturing an annealed steel sheet, comprising polishing a steel sheet with the steel sheet polishing equipment described in claim 4 and then annealing it with the continuous annealing equipment to produce an annealed steel sheet.
Citation Information
Patent Citations
Preheating furnace
JP1983180269U
The continuous furnace for the heat treatment of steel
JP1985037061U
Continuous annealing installation for steel strip
JP1987054034A
Production of polyolefin