Wafer chuck structure and plasma etching equipment

TWI945954BActive Publication Date: 2026-11-11ADVANCED MICRO FAB EQUIP INC CHINA
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
TW114127696
Authority / Receiving Office
TW · TW
Patent Type
Patents
Current Assignee / Owner
Priority Date
2024-09-10
Filing Date
2025-07-22
Publication Date
2026-11-11
Estimated Expiration
2045-07-21

AI Technical Summary

Technical Problem

In plasma etching processes, particulate matter generated by friction between the porous plug and the electrostatic chuck contaminates the wafer and increases the risk of arc discharge due to inconsistent thermal expansion coefficients of materials, leading to contamination and process inefficiencies.

Method used

A wafer chuck structure with a transition layer between the porous plug and the top wall of the first section to prevent friction-induced particulate contamination, using materials with higher wear resistance and deformability to intercept any generated particles, ensuring they do not enter the process cavity.

Benefits of technology

Prevents particulate contamination of the wafer and reduces the risk of arc discharge by intercepting particles at the transition layer, maintaining process cleanliness and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure TWG2TB001920706_001
    Figure TWG2TB001920706_001
  • Figure TWG2TB001920706_002
    Figure TWG2TB001920706_002
  • Figure TWG2TB001920706_003
    Figure TWG2TB001920706_003
Patent Text Reader

Abstract

This invention provides a wafer chuck structure and a plasma etching apparatus. The upper surface of the wafer chuck structure supports the wafer and contains a gas channel for supplying cooling gas to the area below the wafer. Along the gas supply direction, the gas channel includes a first section and a second section that are connected. The second section is formed on the upper surface of the wafer chuck structure. The aperture of the first section is larger than that of the second section. A first porous plug with a porous structure is provided within the first section, allowing the cooling gas to flow through the first porous plug into the second section. A transition layer is provided on top of the first porous plug, between the first porous plug and the top wall of the first section, to prevent particulate matter formed by friction between the first porous plug and the top wall of the first section from contaminating the gas channel in the second section. This invention prevents particulate matter formed by friction on the surface of the porous plug from entering the process chamber and contaminating the wafer.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] This invention relates to the field of semiconductor equipment technology, and in particular to a wafer chuck structure and plasma etching equipment. [Previous Technology]

[0002] Among the various processes in semiconductor device manufacturing, plasma etching is a key process for processing wafers into designed patterns. In a typical plasma processing process, process gases form plasma under radio frequency (RF) excitation. After passing through the electric field (capacitive coupling or inductive coupling) between the upper and lower electrodes, these plasmas physically bombard and chemically react with the wafer surface, thereby processing the wafer.

[0003] Plasma etching equipment includes wafer chuck structures, such as electrostatic chucks (ESCs), whose main functions are to fix the wafer, control its temperature, and feed in radio frequency power. To increase heat conduction between the wafer and the electrostatic chuck, vent holes are usually opened inside the electrostatic chuck. Cooling gas (such as helium) is injected into the vent holes to fill the space between the wafer and the electrostatic chuck surface with cooling gas to control the temperature.

[0004] Under high RF power conditions, a high voltage difference exists between the wafer and the base of the electrostatic chuck. To prevent arcing in the vents inside the electrostatic chuck, the vents are typically made into two parts with different diameters: the vents closer to the wafer have smaller diameters, such as 0.1~0.5mm, while the vents farther from the wafer have larger diameters, such as 1~5mm. Furthermore, porous plugs are filled in the larger diameter areas to compress the discharge space within the vents and increase the electric field strength threshold for arcing. Smaller diameter vents are not filled with porous plugs to ensure the passage of cooling gas.

[0005] However, since the porous plug is generally located in the base part, the thermal expansion coefficients of the base and the electrostatic chuck are inconsistent. Therefore, during the process, temperature changes will cause relative sliding friction between the porous plug and the electrostatic chuck. Since the surface of the porous plug is relatively rough, the sliding surface is prone to friction to produce particles. The particles will enter the reaction chamber through the small-diameter pores above, contaminating the wafer, and may even block the pores above. [Summary of the Invention]

[0006] The purpose of this invention is to provide a wafer chuck structure and plasma etching equipment to prevent particulate matter formed by friction on the surface of the porous plug from entering the process cavity and contaminating the wafer.

[0007] To achieve the above objectives, the present invention is implemented through the following technical solution:

[0008] A wafer chuck structure, wherein the upper surface of the wafer chuck structure is used to support a wafer, and a gas channel is provided therein for conveying cooling gas to the lower part of the wafer. Along the conveying direction of the cooling gas, the gas channel includes a first section and a second section that are connected to each other. The second section is formed on the upper surface of the wafer chuck structure. The aperture of the first section is larger than the aperture of the second section. A first porous plug with a porous structure is provided in the first section. The cooling gas can flow through the first porous plug into the second section. A transition layer is provided on the top of the first porous plug. The transition layer is located between the first porous plug and the top wall of the first section to avoid friction between the first porous plug and the top wall of the first section to form particulate matter that contaminates the gas channel of the second section.

[0009] Optionally, the transition layer is a smooth coating formed on the first porous plug in the area opposite to the top wall of the first section, and the cooling gas can enter the second section through the uncoated area on the upper surface of the first porous plug.

[0010] Optionally, the transition layer is an annular flexible gasket, and the cooling gas can enter the second section through the central through hole of the annular flexible gasket.

[0011] Optionally, the transition layer is a disc-shaped gasket with a porous structure, through which the cooling gas can flow into the second section.

[0012] Optionally, the wear resistance of the transition layer material is higher than that of the first porous plug material, and the surface of the transition layer is polished.

[0013] Optionally, the transition layer is made of a deformable material.

[0014] Optionally, the edge of the transition layer is provided with a downwardly protruding boss, and the upper surface of the first porous plug is provided with a step portion that matches the boss.

[0015] Optionally, the wafer chuck structure includes a base and a dielectric plate, the lower surface of the dielectric plate being connected to the base via an adhesive layer; the second segment is formed on the dielectric plate, and the first segment is at least partially formed on the base.

[0016] Optionally, the first section includes a first sub-section formed on the base and a second sub-section formed on the dielectric plate.

[0017] Optionally, the first porous plug is at least partially located within the first sub-segment, and the transition layer is located within the second sub-segment.

[0018] Optionally, the first porous plug includes a first sub-porous plug and a second sub-porous plug, the first sub-porous plug being located within the first sub-segment, and the second sub-porous plug and the transition layer being located within the second sub-segment.

[0019] Optionally, the wafer chuck structure includes a base and a dielectric plate, the lower surface of the dielectric plate being connected to the base via an adhesive layer; the first section includes a first sub-section formed on the base and a second sub-section formed on the dielectric plate; the transition layer includes a second porous plug with a porous structure, the second porous plug being disposed in the second sub-section and fixedly connected to the dielectric plate.

[0020] Optionally, there is a gap between the first porous plug and the second porous plug.

[0021] A plasma etching apparatus includes a reaction chamber, a wafer chuck structure as described in any of the above, an upper electrode, a cooling device, and a radio frequency power supply; the wafer chuck structure is placed inside the reaction chamber to support the wafer and serves as the lower electrode of the reaction chamber; the cooling device is connected to the wafer chuck structure and is used to supply cooling gas to the wafer; the upper electrode is disposed opposite to the wafer chuck structure, and the radio frequency power supply is applied to the upper electrode and / or the wafer chuck structure to generate a radio frequency electric field between the upper electrode and the wafer chuck structure, thereby dissociating the reaction gas into plasma and etching the wafer.

[0022] Compared with the prior art, the present invention has the following advantages:

[0023] The present invention provides a wafer chuck structure and plasma etching equipment. Since a transition layer is provided between the top of the first porous plug and the top wall of the first section, the first porous plug will not generate particulate contaminants by friction with the top wall of the first section. Even if some particles are generated by friction between the first porous plug and the transition layer, they will be intercepted by the transition layer and will not enter the second section and the back side of the wafer, thereby solving the problem of particulate matter formed by friction on the surface of the porous plug entering the process cavity and contaminating the wafer.

Implementation Method

[0025] The following describes the proposed solution of the present invention in further detail with reference to the drawings and specific embodiments. The advantages and features of the present invention will become clearer from the following description. It should be noted that the drawings are in a very simplified form and use non-precise proportions, only for the purpose of conveniently and clearly illustrating the embodiments of the present invention. Please refer to the drawings to make the objectives, features, and advantages of the present invention more apparent and understandable. It should be understood that the structures, proportions, sizes, etc., depicted in the accompanying drawings are only for the purpose of assisting those skilled in the art in understanding and reading the content disclosed in the specification, and are not intended to limit the implementation conditions of the present invention. Therefore, they have no substantial technical significance. Any modifications to the structure, changes in the proportional relationships, or adjustments to the size, without affecting the effects and objectives achieved by the present invention, should still fall within the scope of the technical content disclosed in the present invention.

[0026] Figure 1 is a simplified schematic diagram of a plasma etching apparatus, which can be a capacitively coupled plasma etching apparatus or an inductively coupled plasma etching apparatus. The apparatus includes a reaction chamber, within which a wafer chuck structure 100 is provided to support a wafer 200 and serve as the lower electrode of the reaction chamber; an upper electrode 400 of the reaction chamber is disposed opposite to the wafer chuck structure 100. Radio frequency power is applied to the upper electrode 400 and / or the wafer chuck structure 100, generating a radio frequency electric field between the upper electrode 400 and the wafer chuck structure 100, dissociating the reactive gas into plasma 300, thereby etching the wafer 200. The wafer chuck structure 100 can also regulate the temperature of the wafer 200 placed thereon. The cooling device 500 is connected to the wafer chuck structure and is used to deliver cooling gas to the wafer. The cooling gas in the cooling device 500 flows to the back side of the wafer 200 through the gas channel and reduces the temperature of the wafer 200 by absorbing the heat of the wafer 200.

[0027] As shown in Figure 2, the wafer chuck structure 100 includes a base 110 and a dielectric plate 130 disposed on the base 110. The dielectric plate 130 is connected to the base 110 through an adhesive layer 120, and the upper surface of the dielectric plate 130 supports the wafer 200. The dielectric plate 130 and the adhesive layer 120 are insulating materials, and the base 110 is a metal material. When the etching equipment is working, a large potential difference will be formed between the wafer 200 and the base 110.

[0028] To regulate the temperature of the wafer 200, a gas channel is provided in the wafer chuck structure 100 for introducing cooling gas from the cooling device 500 into the gap between the wafer chuck structure 100 and the wafer 200. The vertical arrow in Figure 2 shows the flow direction of the cooling gas. Specifically, a first vent 111 is provided in the base 110, and a second vent 131 is provided on the dielectric plate 130, penetrating the dielectric plate 130 axially. The second vent 131 and the first vent 111 are connected. The first vent 111 is connected to the cooling device 500 through a channel 112. The cooling gas flows out from the cooling device 500, passes through the channel 112, the first vent 111, and the second vent 131 in sequence, and thus contacts the back side of the wafer 200 fixed on the dielectric plate 130, thereby achieving temperature regulation of the wafer.

[0029] The second vent 131 has a smaller diameter, for example, 0.1~0.5 mm, while the first vent 111 has a larger diameter, for example, 1~5 mm. A porous plug 113 is filled into the first vent 111 to prevent arc discharge in that area. The porous plug 113 has a porous structure, allowing cooling gas to enter from the bottom surface of the porous plug 113, pass through the porous plug 113, flow out from the top surface, enter the second vent 131, and then contact the wafer 200. To ensure the uniformity of the cooling gas output, the second vent 131 is not filled with any filler.

[0030] The porous plug 113 is mainly located in the base 110 and has a different coefficient of thermal expansion than the wafer chuck structure 100. Therefore, during the process, temperature changes can cause relative sliding between the porous plug 113 and the wafer chuck structure 100. As shown in Figure 2, at high temperatures during the process, there is slight sliding between the dielectric plate 130 and the base 110 (shift, the horizontal arrow in Figure 2 shows the direction of sliding), which causes friction between the porous plug 113 and the bottom surface of the dielectric plate 130. The surface of the porous plug 113 is relatively rough, which causes the porous plug 113 to generate particulate contaminants P due to friction. These particulate contaminants P can enter the reaction chamber and contaminate the wafer 200, and may even block the second pore 131. In addition, these particulate contaminants P can increase the probability of arc discharge.

[0031] Based on this, this embodiment provides a wafer chuck structure capable of preventing particulate contamination. As shown in Figures 3-10, several embodiments are illustrated. The upper surface of the wafer chuck structure 100 is used to support the wafer 200, and a gas channel 140 is provided therein for conveying cooling gas to the lower part of the wafer 200. Along the conveying direction of the cooling gas (as indicated by the arrows in the figures), the gas channel 140 includes a first section 141 and a second section 142 that are connected. The second section 142 is formed on the upper surface of the wafer chuck structure 100, and the aperture of the first section 141 is larger than that of the second section 142. The first section 141 has a pore size of 42. A first porous plug 150 with a porous structure is provided in the first section 141. The cooling gas can flow through the first porous plug 150 into the second section 142. A transition layer 160 is provided on the top of the first porous plug 150. The transition layer 160 is located between the first porous plug 150 and the top wall of the first section 141 to avoid friction between the first porous plug 150 and the top wall of the first section 141 to form particulate matter that contaminates the gas channel of the second section 142.

[0032] In this embodiment, after the cooling gas flows out of the cooling device 500, it flows into the first section 141 of the gas channel 140 through the channel 112, passes through the first porous plug 150 and the transition layer 160, and then flows into the back side of the wafer 200 through the second section 142. Since the transition layer 160 is provided between the top of the first porous plug 150 and the top wall of the first section 141, the first porous plug 150 will not generate particulate contaminants by friction with the top wall of the first section 141. Even if some particulate contaminants are generated by friction between the first porous plug 150 and the transition layer 160, they will be intercepted by the transition layer 160 and will not enter the second section 142 and the back side of the wafer 200, thereby solving the problem of particulate matter formed by friction on the surface of the porous plug entering the process cavity and contaminating the wafer.

[0033] The technical solution of the present invention will be described below through some preferred embodiments.

[0034] As shown in the embodiment of Figure 3, the transition layer 160 is a disc-shaped gasket with a porous structure. The cooling gas can flow through the disc-shaped gasket into the second section 142 to ensure the flowability of the cooling gas. To ensure that no particulate contaminants are generated between the transition layer 160 and the top wall of the first section 141 due to friction, the transition layer 160 can be made of a more wear-resistant material than the first porous plug 150, such as carbon fiber composite material, silicon carbide, diamond, etc. At the same time, the surface of the disc-shaped gasket is polished to reduce its surface roughness. In addition, the transition layer 160 can also be made of a deformable material, such as polymer materials (polyethylene, polyurethane, polytetrafluoroethylene, etc.), which can ensure that no relative friction occurs between the transition layer and the top wall of the first section 141 during thermal expansion and contraction, thereby reducing the generation of particulate contaminants. In this embodiment, the second segment 142 is formed on the dielectric plate 130, the first segment 141 is formed on the base 110, the first porous plug 150 is located in the first segment 141, and the transition layer 160 is located in the adhesive layer 120.

[0035] As shown in the embodiment of Figure 4, the difference from the embodiment of Figure 3 is that the edge of the transition layer 160 is provided with a downwardly protruding boss 161, and the upper surface of the first porous plug 150 is provided with a stepped portion 151 that matches the boss 161. Therefore, the first porous plug 150 and the transition layer 160 can be better engaged, facilitating their installation and reducing the possibility of slippage between the transition layer 160 and the first porous plug 150.

[0036] As shown in the embodiment of FIG. 5, the difference from the embodiment of FIG. 3 is that the first section 141 includes a first sub-section 1411 formed on the base 110 and a second sub-section 1412 formed on the dielectric plate 130. The first porous plug 150 is located within the first sub-section 1411, and the transition layer 160 is located within the second sub-section 1412. Compared with the embodiment of FIG. 3, the embodiment of FIG. 5 places the transition layer 160 within the dielectric plate 130, and selects the transition layer 160 to be a material with the same coefficient of thermal expansion and contraction as the dielectric plate 130, or even the same material, so that there will be no relative sliding between the transition layer 160 and the dielectric plate 130, further reducing the possibility of generating particulate contaminants.

[0037] As shown in the embodiment of FIG. 6, the difference from the embodiment of FIG. 3 is that the first section 141 includes a first sub-section 1411 formed on the base 110 and a second sub-section 1412 formed on the dielectric plate 130. The first porous plug 150 is partially located within the first sub-section 1411 and partially located within the second sub-section 1412, and the transition layer 160 is located within the second sub-section 1412. Compared with the embodiment of FIG. 3, in the embodiment of FIG. 6, the first porous plug 150 also fills the dielectric plate 130, thereby reducing the space of the gas channel in the second section 142 and reducing the risk of arc discharge.

[0038] As shown in the embodiment of FIG. 7, the difference from the embodiment of FIG. 6 is that the first porous plug 150 includes a first sub-porous plug 152 and a second sub-porous plug 153. The first sub-porous plug 152 is located within the first sub-segment 1411, and the second sub-porous plug 153 and the transition layer 160 are located within the second sub-segment 1412. Compared with the embodiment of FIG. 6, the embodiment of FIG. 7 divides the first porous plug 150 into two separate upper and lower parts, located within the first sub-segment 1411 and the second sub-segment 1412 respectively. This can avoid the upper and lower parts of the first porous plug 150 in FIG. 6 from breaking at high temperatures due to different deformation.

[0039] As shown in the embodiment of Figure 8, the difference from the embodiment of Figure 3 is that the transition layer 160 is an annular flexible gasket, and the cooling gas can enter the second section 142 through the central through hole of the annular flexible gasket. Compared with the embodiment of Figure 3, the embodiment of Figure 8 designs the transition layer 160 as an annular structure with a hollowed-out center, which can further increase the flow of cooling gas. In this case, the annular flexible gasket can be a porous structure or a solid structure. When the annular flexible gasket is a solid structure, the hollowed-out portion in the middle should not be smaller than the aperture of the second section to ensure the flow of cooling gas. The hollowed-out portion in the middle can be larger than the aperture of the second section, as long as the annular flexible gasket can isolate the first porous plug 150 from the top wall of the first section 141. It is understood that the transition layer 160 in the embodiments of Figures 4 to 7 can also be replaced with an annular flexible gasket, which will not be elaborated here.

[0040] As shown in the embodiment of FIG9, the transition layer 160 is a smooth coating formed on the first porous plug 150 in the area opposite to the top wall of the first section 141. The cooling gas can enter the second section 142 through the uncoated area on the upper surface of the first porous plug 150. That is, the outer periphery of the upper surface of the first porous plug 150 opposite to the top wall of the first section 141 is coated, while the middle area is not coated to ensure the flow of cooling gas. During the process, when the first porous plug 150 slides against the top wall of the first section 141, no particulate contaminants are generated because the contact area is smooth. It is understood that the transition layer 160 in the embodiments of FIG5 to FIG7 can also be replaced with a smooth coating, which will not be described in detail here.

[0041] In some other embodiments, as shown in FIG10, the transition layer 160 includes a second porous plug with a porous structure. The second porous plug is disposed in the second sub-section 1412 and fixedly connected to the dielectric plate 130. For example, the second porous plug can be bonded to the dielectric plate 130. In this way, the second porous plug can move together with the dielectric plate 130 without relative sliding between them. Therefore, no particulate contaminants will be generated between them. Even if the second porous plug comes into contact with the first porous plug 150 and slides relative to it, generating particulate contaminants, the particulate contaminants will have difficulty entering the gas channel of the second section 142 and reaching the reaction chamber due to the obstruction of the second porous plug. Furthermore, a gap, such as less than 0.5 mm, can be maintained between the first porous plug 150 and the second porous plug. When cooling gas is introduced, the cooling gas can provide an upward buoyancy to maintain this gap between the second porous plug and the first porous plug 150. At this time, since there is no direct contact between the first porous plug 150 and the second porous plug, no particulate contaminants will be generated between them.

[0042] In summary, the wafer chuck structure and plasma etching equipment provided by the present invention, since a transition layer is provided between the top of the first porous plug and the top wall of the first section, the first porous plug will not generate particulate contaminants by friction with the top wall of the first section. Even if some particles are generated by friction between the first porous plug and the transition layer, they will be intercepted by the transition layer and will not enter the second section and the back side of the wafer, thereby solving the problem of particulate matter formed by friction on the surface of the porous plug entering the process cavity and contaminating the wafer.

[0043] It should be noted that, in this document, relational terms such as "first" and "second" are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Furthermore, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes said element.

[0044] Although the present invention has been described in detail through the above preferred embodiments, it should be understood that the above description should not be considered as a limitation of the present invention. Various modifications and substitutions to the present invention will be apparent to those skilled in the art after reading the above. Therefore, the scope of protection of the present invention should be defined by the appended claims. [Simplified Explanation of the Diagram]

[0024] Figure 1 is a schematic diagram of the structure of the plasma etching equipment; Figure 2 is a schematic diagram of the existing wafer chuck structure; Figures 3 to 10 are schematic diagrams of different embodiments of the wafer chuck structure provided by the present invention.

Claims

1. A wafer chuck structure, wherein the upper surface of the wafer chuck structure is used to support a wafer, and a gas channel is provided therein for supplying cooling gas to the area below the wafer, wherein... Along the direction of the cooling gas transport, the gas channel includes a first section and a second section that are connected to each other. The second section is formed on the upper surface of the wafer chuck structure. The aperture of the first section is larger than that of the second section. The first section is provided with a first porous plug with a porous structure. The cooling gas can flow through the first porous plug into the second section. The top of the first porous plug is provided with a transition layer. The transition layer is located between the first porous plug and the top wall of the first section to avoid friction between the first porous plug and the top wall of the first section to form particulate matter that contaminates the gas channel of the second section. The transition layer covers the entire or part of the top surface of the first porous plug.

2. The wafer chuck structure as described in claim 1, wherein, The transition layer is a smooth coating formed on the first porous plug in the area opposite to the top wall of the first section, and the cooling gas can enter the second section through the uncoated area on the upper surface of the first porous plug.

3. The wafer chuck structure as described in claim 1, wherein, The transition layer is an annular flexible gasket, and the cooling gas can enter the second section through the central through-hole of the annular flexible gasket.

4. The wafer chuck structure as described in claim 1, wherein, The transition layer is a disc-shaped gasket with a porous structure, through which the cooling gas can flow into the second section.

5. The wafer chuck structure as described in claim 3 or 4, wherein, The wear resistance of the transition layer material is higher than that of the first porous plug material, and the surface of the transition layer is polished.

6. The wafer chuck structure as described in claim 3 or 4, wherein, The transition layer is made of a deformable material.

7. The wafer chuck structure as described in claim 3 or 4, wherein, The edge of the transition layer is provided with a downward protruding boss, and the upper surface of the first porous plug is provided with a step portion that matches the boss.

8. The wafer chuck structure as described in claim 2, 3, or 4, wherein, The wafer chuck structure includes a base and a dielectric plate, the lower surface of which is connected to the base via an adhesive layer; the second segment is formed on the dielectric plate, and the first segment is at least partially formed on the base.

9. The wafer chuck structure as described in claim 8, wherein, The first section includes a first sub-section formed on the base and a second sub-section formed on the dielectric plate.

10. The wafer chuck structure as described in claim 9, wherein, The first porous plug is located at least partially within the first sub-segment, and the transition layer is located within the second sub-segment.

11. The wafer chuck structure as described in claim 9, wherein, The first porous plug includes a first sub-porous plug and a second sub-porous plug, the first sub-porous plug being located within the first sub-segment, and the second sub-porous plug and the transition layer being located within the second sub-segment.

12. A plasma etching apparatus, wherein, The device includes a reaction chamber, a wafer chuck structure as described in any one of claims 1 to 11, an upper electrode, a cooling device, and a radio frequency power supply; the wafer chuck structure is placed inside the reaction chamber to support the wafer and serves as the lower electrode of the reaction chamber; the cooling device is connected to the wafer chuck structure and is used to supply cooling gas to the wafer; the upper electrode is disposed opposite to the wafer chuck structure, and the radio frequency power supply is applied to the upper electrode and / or the wafer chuck structure to generate a radio frequency electric field between the upper electrode and the wafer chuck structure, thereby dissociating the reaction gas into plasma and etching the wafer.

Citation Information

Patent Citations

  • High power electrostatic chuck with plug having reduced aperture in gas hole

    CN116544171A

  • Porous plug assembly, electrostatic chuck and plasma etching device

    TW202427549A