Process parameter determination method and semiconductor process device

By establishing a model of the relationship between process parameters and film thickness and Kalman filter gain correction technology, the problem of relying on personal experience for film thickness control in LPCVD process equipment is solved, and automatic and efficient debugging of film thickness uniformity is achieved, which is suitable for large-volume, high-capacity production. .

WO2024199318A1PCT designated stage expired Publication Date: 2024-10-03BEIJING NAURA MICROELECTRONICS EQUIP CO LTD

Patent Information

Application Number
PCT/CN2024/084268
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-28
Filing Date
2024-03-28
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

In the semiconductor manufacturing process, the film thickness control, film thickness uniformity control and product yield control of low-pressure chemical vapor deposition (LPCVD) process equipment rely on the personal experience of engineers, resulting in a high risk of evaluation errors and low debugging efficiency, which cannot meet the needs of large-volume, Requirements for high-capacity automated production.

Method used

By establishing a relationship model between process parameters and film thickness, the experimental process parameters are determined according to the target film thickness. If the film thickness is uneven, the model is updated until the uniformity requirements are met. The Kalman filter gain correction relationship matrix is ​​used to reduce reliance on personal experience and improve Debugging efficiency.

Benefits of technology

It realizes the automation of film thickness uniformity control, reduces the number of experiments, improves process debugging efficiency, and meets the needs of large-volume and high-capacity production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024084268_03102024_PF_FP_ABST
    Figure CN2024084268_03102024_PF_FP_ABST
Patent Text Reader

Abstract

Provided in the present disclosure are a process parameter determination method and a semiconductor process device. The method comprises: establishing a relationship model between a process parameter and the film thickness of each partition; calculating an experimental process parameter of a deposition process according to the relationship model; and if the film thickness which is obtained by means of performing film deposition on a wafer on the basis of the experimental process parameter does not meet the requirement for film thickness uniformity, updating the relationship model and then executing the calculation process until the film thickness, which is obtained by means of performing film deposition on the wafer on the basis of the experimental process parameter, meets the requirement for film thickness uniformity. The process parameter determination method no longer relies on the personal experience of engineers, such that experimental blindness is reduced, the efficiency of process debugging is improved, and the requirement of a production line for large-batch, high-yield and automated production is met.
Need to check novelty before this filing date? Find Prior Art

Description

Method for determining process parameters and semiconductor process equipment Technical Field

[0001] The present disclosure relates to, but is not limited to, the field of semiconductor technology, and in particular to a method for determining process parameters and semiconductor process equipment. Background Art

[0002] In semiconductor manufacturing, various thin films are deposited on wafer substrates to create discrete devices and integrated circuits. Low-pressure chemical vapor deposition (LPCVD) is a widely used thin film deposition method. Because super integrated circuits (SIs) have stringent quality requirements for their manufacturing processes, this poses new challenges to LPCVD process equipment in terms of film thickness control, film thickness uniformity control, film quality, and product yield control.

[0003] Film thickness performance indicators (such as wafer temperature, process gas flow, pressure, and process time) are typically adjusted by engineers based on offline data and empirical data. This adjustment method is largely limited by the engineer's accumulated experience, carries the risk of miscalculation, and does not meet the basic requirements of high-volume, high-capacity, and automated production lines.

[0004] Summary of the Invention

[0005] The problem solved by the present disclosure is that the existing adjustment of process parameters affecting film thickness is limited by the individual experience of engineers, resulting in the risk of evaluation errors and low process debugging efficiency.

[0006] To solve the above problems, an embodiment of the present disclosure provides a method for determining process parameters, which is applied to semiconductor process equipment. The method for determining process parameters includes: obtaining a relationship model between process parameters of a deposition process and the thickness of a deposited film on wafers in each partition within the semiconductor process equipment; the process parameters include at least one of the following: a temperature setting value, a process gas flow rate, a pressure, and a process time of each partition; determining experimental process parameters based on the current relationship model and the target film thickness of the wafers in each partition, and performing wafer thin film deposition based on the experimental process parameters; if the film thickness currently deposited on the wafer meets the film thickness uniformity requirement, determining the experimental process parameters as the set process parameters; if the film thickness currently deposited on the wafer does not meet the film thickness uniformity requirement, updating the current relationship model based on the experimental process parameters and the corresponding film thickness currently deposited on the wafer, and then turning to the steps of determining the experimental process parameters based on the current relationship model and the target film thickness of the wafers in each partition, and performing wafer thin film deposition based on the experimental process parameters, until the film thickness currently deposited on the wafer meets the film thickness uniformity requirement.

[0007] As a feasible implementation method, the experimental process parameters are determined based on the current relationship model and the target film thickness of the wafers in each partition, including: calculating the intermediate results of the process parameters based on the target film thickness of the wafers in each partition and the current relationship model; and calculating the experimental process parameters based on the intermediate results of the process parameters and the target process parameters.

[0008] As a feasible implementation method, the current relationship model is updated according to the experimental process parameters and the corresponding film thickness currently deposited on the wafer, including: obtaining the film thickness of each partition obtained by wafer thin film deposition according to the experimental process parameters; and updating the current relationship model using the experimental process parameters and the film thickness.

[0009] As a feasible implementation method, the relationship model is a relationship matrix, and the current relationship model is updated according to the experimental process parameters and the corresponding film thickness currently deposited on the wafer, including: obtaining the film thickness matrix of each partition obtained by wafer thin film deposition according to the experimental process parameters; calculating the difference matrix between the film thickness matrix of each partition and the target film thickness matrix of each partition, multiplying the difference matrix with the Kalman filter gain and then summing it with the current relationship matrix to obtain an updated relationship matrix; and determining the updated relationship matrix as the current relationship matrix.

[0010] As a feasible implementation manner, the method further includes: updating the Kalman filter gain according to a difference matrix between the film thickness matrix and the target film thickness matrix.

[0011] As a feasible implementation method, the relationship model between the process parameters of the deposition process and the thickness of the deposited film on the wafer of each partition in the semiconductor process equipment includes: obtaining multiple sets of the process parameters and the thickness of the deposited film on the wafer of each partition corresponding to each process parameter; converting the multiple sets of the process parameters and the thickness of the deposited film on the wafer of each partition corresponding to each process parameter into a matrix expression to obtain the relationship model between the process parameters and the thickness of the deposited film on the wafer of each partition; or, obtaining the relationship model between the process parameters known in advance and the thickness of the deposited film on the wafer of each partition.

[0012] As a feasible implementation manner, the method further includes: performing wafer thin film deposition according to the set process parameters.

[0013] As a feasible implementation method, the experimental process parameters are calculated based on the intermediate results of the process parameters and the target process parameters, including: normalizing the intermediate results of the process parameters to obtain the normalized intermediate results of the process parameters; multiplying the normalized intermediate results of the process parameters by the target process parameters to calculate the experimental process parameters.

[0014] As a feasible implementation, the relationship model is a relationship matrix, and the relationship matrix is ​​as follows:

[0015] Wherein, n represents multiple sets of data of the process parameters, and m represents multiple different partitions in the semiconductor process equipment.

[0016] An embodiment of the present disclosure provides a semiconductor process equipment, comprising: a furnace body, wherein a heating element and a process tube are provided in the furnace body, wherein a wafer boat is placed in the process tube; and a controller connected to the heating element, for executing the above-mentioned process parameter determination method.

[0017] As a feasible implementation manner, it further includes: a gas input component for inputting process gas into the process pipe; and / or a pressure control component for controlling the pressure in the process pipe.

[0018] The method for determining process parameters and the semiconductor process equipment provided by the embodiments of the present disclosure can establish a relationship model between process parameters and the film thickness of each partition, and infer the experimental process parameters of the deposition process based on the relationship model. If the film thickness of the wafer thin film deposited based on the experimental process parameters does not meet the film thickness uniformity requirements, the above-mentioned relationship model can be updated and then the above-mentioned inference process can be performed again until the film thickness of the wafer thin film deposited based on the obtained experimental process parameters meets the film thickness uniformity requirements. The method for determining process parameters no longer relies on the personal experience of engineers, reduces the blindness of experiments, improves the efficiency of process debugging, and meets the large-scale, high-capacity, and automated production requirements of the production line. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In order to more clearly illustrate the embodiments of the present disclosure or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are only embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying any creative work.

[0020] FIG1 is a schematic diagram showing the principle of the existing MBTC technology;

[0021] FIG2 is a schematic diagram showing the principle of establishing a thermal model of the existing MBTC technology;

[0022] Figure 3 is a schematic diagram of the furnace temperature, gas concentration, and film thickness corresponding to different zones in an existing vertical furnace LPCVD device;

[0023] Figure 4 is a schematic diagram of the furnace temperature, gas concentration, and film thickness corresponding to different zones in the improved vertical furnace LPCVD equipment;

[0024] FIG5 is a schematic flow chart of a method for determining process parameters in an embodiment of the present disclosure. DETAILED DESCRIPTION

[0025] To make the above-mentioned objectives, features and advantages of the present disclosure more clearly understood, the following detailed description of the specific embodiments of the present disclosure is given in conjunction with the accompanying drawings. It should be understood that the specific embodiments described herein are only used to explain the present disclosure and are not intended to limit the present disclosure.

[0026] Conventional technologies for adjusting film thickness uniformity across wafers primarily rely on furnace temperature control, such as using MBTC (Model Based Temperature Control) technology. Unlike traditional PID (Proportional Integration Differentiation) temperature control techniques, MBTC directly estimates the temperature of the silicon wafer and uses it as the control target, ensuring that the wafer temperature is equal to the target temperature. Figure 1 shows a schematic diagram of the existing MBTC technology.

[0027] Figure 1 shows a vertical furnace on the left and a thermal model on the right. During furnace operation, the internal temperature (InnerTC) and furnace power values ​​are input into the thermal model's estimator to generate an estimated silicon wafer temperature. This is then input into the controller, which then controls the furnace's heater output power based on this estimated wafer temperature.

[0028] The thermal model used in MBTC technology is obtained by measuring thermal characteristics using a temperature-controlled wafer (TC Wafer). Figure 2 shows a schematic diagram of the principle of establishing a thermal model for MBTC technology in related art. Figure 2 shows that establishing a thermal model on the client side includes: collecting the internal temperature value of the vertical furnace, the power value of the furnace body, and the actual silicon wafer temperature value to jointly establish the thermal model.

[0029] The MBTC technology can directly predict the temperature of the silicon wafer. Based on the customer's target film thickness, deposition time, and specified process temperature, combined with the Arrhenius equation, it can reversely calculate the silicon wafer temperature corresponding to the target film thickness in each partition of the furnace and adjust the film thickness.

[0030] Among them, the accuracy of the above thermal model determines the accuracy and efficiency of the client's process film thickness adjustment. When the equipment has large mechanical differences (equipment differences) or some configurations of the equipment have slight changes (for example, the structure of the boat has changed), the standard model obtained by the above thermal model in the factory will not be applicable. When the equipment has large mechanical differences, some key hardware needs to be replaced to solve the equipment mechanical differences before the standard model obtained in the factory can be used normally. When the customer has special needs, some configurations of the equipment will change slightly according to their special requirements. The client's engineers need to re-consult and select which standard model in the factory is more appropriate, or even need to re-experiment in the factory to obtain a matching thermal model. Re-obtaining the thermal model in the factory will take a lot of time, manpower and machine resources, affecting the client's installation plan.

[0031] The embodiment of the present disclosure proposes a method for determining process parameters based on a small amount of process data. By collecting a small amount of process parameters of the equipment (such as temperature setting data and other process data and film thickness data), a relationship model between process parameters and film thickness is established, and the experimental process parameters are calculated based on the relationship model to improve the surface uniformity.

[0032] By using this method, we no longer rely on the engineer's personal experience, reduce the blindness of the experiment, and the number of adjustments required will be significantly less than the number of manual adjustments to achieve the required inter-surface uniformity target value, thereby improving process debugging efficiency.

[0033] In the actual batch CVD (Chemical Vapor Deposition) film deposition process, the film thickness of each silicon wafer depends on parameters such as the main process settings, temperature, process gas flow, pressure, and process time. Variations in film thickness are highly sensitive to changes in these process conditions. On the customer side, vertical furnace equipment must match the standard process recipe of a baseline machine. Typically, in this scenario, process gas flow and pressure cannot be changed, allowing the manufacturer to adjust only the set temperature and process time.

[0034] For example, low-pressure chemical vapor deposition (LPCVD) is not a saturated-reaction-atmosphere process due to its film-forming principle. LPCVD introduces one or more reactive gases into a low-pressure reaction chamber heated by a heater. The thermal energy causes thermal decomposition or chemical reactions, ultimately depositing a thin film on the silicon wafer surface.

[0035] LPCVD film growth is limited by process gas consumption; once the process gas is depleted, film growth ceases. Conversely, the oxidation process involves a chemical reaction between the silicon wafer surface and oxygen to form SiO2. During this oxidation reaction, the oxygen introduced exceeds the oxygen required to form the SiO2 film, resulting in a saturated reaction atmosphere. Because LPCVD film thickness is limited by the process gas flow rate, film growth ceases once it is depleted. Therefore, it is an unsaturated reaction atmosphere process, making debugging much more difficult than oxidation processes. Due to the structural design of the equipment's gas inlet, excessive process gas consumption during film growth at the bottom of the device leaves insufficient process gas available to support film deposition at the top.

[0036] To address this issue, the set temperature at the bottom of the equipment needs to be lowered to reduce process gas consumption. Therefore, the set temperature of each zone from the bottom to the top of the vertical furnace needs to be optimized (i.e., each zone has a different set temperature). This requires extensive process experimentation, adjusting the set temperature of each zone to achieve consistent target film thickness. Therefore, adjusting film thickness based on experience is quite unreliable. If the machine is debugged, the debugging time is extended; if new process research and development is carried out, the R&D time is also extended, both of which consume a lot of manpower and material resources, resulting in immeasurable economic losses.

[0037] FIG3 shows a schematic diagram of the furnace temperature, gas concentration, and film thickness corresponding to different partitions in the vertical furnace LPCVD equipment in the related art. If the vertical furnace LPCVD equipment adopts the method of supplying process gas from the bottom (BTM for short), when the thermal field of the equipment is uniform in temperature from the top TOP to the bottom BTM, the growth of the silicon wafer film in the bottom BTM first consumes a part of the process gas during the process gas flowing from bottom to top. This makes the growth of the silicon wafer film at the top TOP smaller due to the reduced concentration of the process gas, so that the top TOP and the bottom BTM cannot form the same film thickness. FIG3 shows that the temperature corresponding to different partitions in the vertical furnace LPCVD equipment is set to 760°C, and the resulting film thickness shows a trend of becoming thinner from bottom to top.

[0038] In order to compensate for the reduced film growth rate and film thickness caused by the reduced gas concentration on the top silicon wafer, it is necessary to increase the reaction temperature of the corresponding partition to increase the reaction rate. By increasing the growth rate of the film, the film thickness from the TOP end to the BTM end is made consistent. Figure 4 shows a schematic diagram of the furnace temperature, gas concentration, and film thickness corresponding to different wafer positions (i.e., different partitions) in the improved vertical furnace LPCVD equipment. Figure 4 shows that the temperatures of each partition are set to 730°C, 740°C, 760°C, 780°C, and 790°C, respectively, and the resulting film thickness is consistent.

[0039] Therefore, to address the issue of inconsistent wafer film thickness across different zones, a specific target main process temperature must be set for each zone. If engineers were to set the temperature based on experience, extensive verification experiments would be required to ultimately meet the customer's target process film thickness requirements, resulting in low efficiency.

[0040] The disclosed embodiment proposes a method for determining process parameters, which mainly adjusts the film thickness uniformity between wafers in different partitions to meet the target requirements by adjusting the optimal temperature setting of the process.

[0041] FIG5 shows a schematic flow chart of a method for determining process parameters in an embodiment of the present disclosure. The method is applied to semiconductor process equipment and includes the following steps:

[0042] S502 , obtaining a relationship model between process parameters of a deposition process and the thickness of a deposited film on a wafer in each partition within a semiconductor process equipment.

[0043] The process parameters may include any one or more of the following: temperature settings for each zone, process gas flow rate, pressure, or process duration. In this embodiment, each process parameter can be adjusted individually to obtain experimental process parameters that meet the film thickness uniformity requirements; or multiple process parameters can be adjusted simultaneously to obtain experimental process parameters that meet the film thickness uniformity requirements.

[0044] In some embodiments, a relationship model between the process parameters and the film thickness deposited on the wafer of each partition is constructed by collecting a small number of sets of process parameters of the semiconductor device and the corresponding data of the film thickness deposited on the wafer of each partition; alternatively, a more accurate relationship model is obtained by using the same type of experimental equipment (i.e., the same model of semiconductor equipment) and similar process experiments. Based on this, the following steps can be performed: obtain multiple sets of process parameters and the film thickness deposited on the wafer of each partition corresponding to each process parameter; convert the multiple sets of process parameters and the film thickness deposited on the wafer of each partition corresponding to each process parameter into a matrix expression to obtain a relationship model between the process parameters and the film thickness deposited on the wafer of each partition; alternatively, obtain a relationship model between the process parameters and the film thickness deposited on the wafer of each partition known in advance.

[0045] S504 , determining experimental process parameters according to the current relationship model and the target film thickness of the wafer in each partition, and performing wafer thin film deposition according to the experimental process parameters.

[0046] In some embodiments, an intermediate process parameter result is calculated based on the target deposition film thickness of the wafer in each partition and the current relationship model; then, the experimental process parameter is calculated based on the intermediate process parameter result and the target process parameter. For example, if the relationship model is a relationship matrix, the target film thickness of each partition can be multiplied by the pseudo-inverse matrix of the relationship matrix to calculate the intermediate process parameter result; then, the experimental process parameter is calculated based on the intermediate process parameter result and the target process parameter.

[0047] The target film thickness for each partition can be expressed in matrix form. By multiplying this matrix with the pseudo-inverse matrix of the aforementioned relationship matrix, an intermediate process parameter result can be calculated. Typically, the target film thickness for each partition is equal. The aforementioned experimental process parameters include an experimentally set value for at least one of the aforementioned process parameters. The target process parameters are the initial process parameters set for the aforementioned deposition process and can also be expressed in matrix form.

[0048] Since the intermediate process parameter results are affected by the target film thickness, the collected process parameters, and the corresponding film thickness data, they need to be normalized. Therefore, the following steps are included: first, the intermediate process parameter results are normalized to obtain normalized intermediate process parameter results; then, the normalized intermediate process parameter results are multiplied by the target process parameters to calculate the experimental process parameters.

[0049] S506: Determine whether the thickness of the film currently deposited on the wafer meets the film thickness uniformity requirement. If so, execute S508; if not, execute S510. In actual production, semiconductor process equipment can use the set process parameters to perform wafer thin film deposition.

[0050] S508: Determine the above experimental process parameters as set process parameters.

[0051] S510 , updating the current relationship model according to the experimental process parameters and the corresponding film thickness currently deposited on the wafer, and then turning to execute step S504 until the film thickness currently deposited on the wafer meets the film thickness uniformity requirement.

[0052] When the thickness of the film currently deposited on the wafer does not meet the film thickness uniformity requirements, the current relationship model needs to be updated, and then the aforementioned steps of determining the experimental process parameters and performing wafer thin film deposition according to the experimental process parameters are continued with the updated relationship model to obtain the uniformity of the film thickness currently deposited on the wafer, and then S508 or S510 is executed respectively according to the uniformity judgment result.

[0053] The method for determining process parameters provided by the embodiment of the present disclosure can establish a relationship model between process parameters and the film thickness of each partition, and infer the experimental process parameters of the deposition process based on the relationship model. If the film thickness of the wafer thin film deposited based on the experimental process parameters does not meet the film thickness uniformity requirements, the above-mentioned relationship model can be updated and then the above-mentioned inference process can be performed again until the film thickness of the wafer thin film deposited based on the obtained experimental process parameters meets the film thickness uniformity requirements. The method for determining process parameters no longer relies on the personal experience of engineers, reduces the blindness of experiments, improves the efficiency of process debugging, and meets the large-scale, high-capacity, and automated production requirements of the production line.

[0054] After obtaining the above experimental process parameters, further iterative experiments can be performed to obtain more optimal experimental process parameters. The embodiment of the present disclosure provides a method for updating a relational model, and based on the updated relational model, more optimal experimental process parameters can be obtained.

[0055] As a feasible approach, the relationship matrix is ​​updated by adding the experimental film thickness corresponding to the experimental process parameters to the relationship model. It should be noted that the number of process parameters and film thickness data of each partition in the relationship model can be adaptively adjusted. Based on this, the above relationship model update step may include:

[0056] First, the film thickness of each partition is obtained by performing wafer thin film deposition according to the experimental process parameters. The semiconductor process equipment actually performs wafer thin film deposition according to the above experimental process parameters, and then directly measures the film thickness of each partition.

[0057] Then, the current relationship model is updated using the experimental process parameters and the film thickness. Specifically, the experimental process parameters and the film thickness of each partition can be added to the relationship model to obtain an updated relationship matrix.

[0058] As another feasible approach, if the relationship model is a relationship matrix, Kalman filtering can be used to update the relationship matrix. If the above relationship matrix is ​​constructed by pre-collecting a small number of sets of process parameters and corresponding film thickness data (for example, at least 2 sets of temperature and film thickness data), it is necessary to manually adjust the temperature of the first two sets of experiments based on personal experience before the temperature estimation of the next set of experiments can be performed. The optimized calculation results that can be obtained can only be used in the third set of experiments. In order to reduce the number of optimization times, the following Kalman filter correction method can be used:

[0059] First, a film thickness matrix of each partition is obtained by performing wafer thin film deposition according to experimental process parameters. Semiconductor process equipment performs wafer thin film deposition according to experimental process parameters to obtain an experimental film thickness matrix of each partition.

[0060] Secondly, the difference matrix between the film thickness matrix of each partition and the target film thickness matrix of each partition is calculated, the difference matrix is ​​multiplied by the Kalman filter gain and then summed with the current relationship matrix to obtain the updated relationship matrix.

[0061] The Kalman filter gain can be updated by fusion based on the updated experimental process parameters obtained in the subsequent steps. If the uncertainty is reduced after the new experimental process parameters are integrated, then this gain is positive, which helps to improve the accuracy of the prediction. If the uncertainty increases, then this gain is negative, which has a negative effect on the accuracy of the system prediction. The above uncertainty can be quantified by the covariance of the variables calculated each time. The covariance will change with each iterative fusion, and the Kalman filter gain will also change accordingly. For example, the above Kalman filter gain can be updated based on the difference matrix between the above film thickness matrix and the target film thickness matrix.

[0062] Then, the updated relationship matrix is ​​determined as the current relationship matrix. After obtaining the updated current relationship matrix, the above S504-S508 can be executed again.

[0063] In the embodiment of the present disclosure, the relationship matrix is ​​corrected by using Kalman filtering, and then the relationship matrix is ​​iteratively corrected continuously according to the experimental results, which can reduce the number of adjustments for inter-chip uniformity.

[0064] Furthermore, the steps of calculating and obtaining an updated relationship matrix and the steps of calculating and obtaining updated experimental process parameters are repeatedly performed until the experimental film thickness of each partition obtained by the experiment meets the film thickness uniformity requirement.

[0065] For example, the process parameter matrix is ​​as follows:

[0066] Here, n represents multiple sets of data of a process parameter, and m represents multiple different partitions in the semiconductor process equipment.

[0067] In the following embodiments, the optimization of LPCVD film thickness uniformity between surfaces is used as an example for explanation. In this embodiment, the film thickness uniformity between wafers in different partitions is adjusted to meet the target requirements mainly by adjusting the optimal temperature setting of the next set of processes. For example, the calculation process may include: first, collecting a small amount of temperature setting and corresponding film thickness data of the equipment (at least 2 groups are required); then, calculating the coefficient matrix of the temperature setting and film thickness data based on the generalized inverse matrix; then, calculating the intermediate results based on the requirements of the target film thickness uniformity between wafers, and normalizing them; finally, calculating the temperature setting values ​​of each partition based on the process-specific temperature (for example, 760°C or 725°C) (where the temperature of the intermediate partition is the process-specific temperature).

[0068] In this embodiment, a small amount of process data (mainly including temperature setting and film thickness data, for example, two sets of process data) is collected from the equipment to establish a relationship model between temperature and film thickness. Based on this relationship model, the optimal temperature setting for the next set of processes is calculated to improve the surface uniformity. The process is as follows:

[0069] (1) Collect a small amount of equipment temperature setting values ​​and corresponding film thickness data. At least two sets of data are required, as shown in Table 1. The first five columns represent the process temperature (unit: °C) of each zone (Zone 1-Zone 5), the next five columns represent the film thickness (unit: A) of each zone (Zone 1-Zone 5 corresponds to TOP, CTOP, CTR, CBTM, and BTM, respectively), and the last column is the main process (Deposition) time.

[0070] Table 1

[0071] (2) Convert the data into a matrix mathematical expression:

[0072] Z11x11+Z12x12+…+Z15x15=t11+t12+…+t15

[0073] Zn1xn1+Zn2xn2+…+Zn5xn5=tn1+tn2+…+tn5

[0074] Here Z11 is the set temperature of the first zone Zone1, and t11 is the film thickness of Zone1. The conversion matrix is ​​as follows:

[0075] in, is the temperature matrix, is the film thickness matrix, It is the coefficient matrix between temperature setting and film thickness data, X1-Xn are row vectors, and Xn includes Xn1-Xn5.

[0076] (3) Use the generalized inverse matrix to obtain the relationship matrix:

[0077] (4) Uniformity adjustment to obtain the set temperature for the next set of experiments

[0078] Where Tk is the set temperature [Z1′…Z5′] for the next set of experiments based on the target film thickness specified by the customer.

[0079] Among them, the obtained [Z1′...Z5′] is an intermediate result, which needs to be normalized and the temperature setting value [Z1...Z5] of each partition is calculated according to the target process temperature (for example, 760°C or 725°C).

[0080] Among them, TargetTemp is the target process temperature.

[0081] The entire calculation process described above requires obtaining at least two sets of temperature and film thickness data before estimating the temperature for the next set of experiments. This means that the temperature of the first two sets of experiments must be manually adjusted based on personal experience. The optimized calculation results can only be used in the third set of experiments.

[0082] In order to reduce the number of optimization times, in this embodiment, the relationship matrix can also be corrected using Kalman filtering. The optimal temperature setting is deduced based on the corrected relationship matrix, and iterative experiments are performed to improve the uniformity between surfaces. The process is as follows:

[0083] (1) Assume that a relatively accurate relationship matrix can be obtained from the same type of experimental machine and similar processes

[0084] (2) Based on the target film thickness [TK TK TK TK TK ], the temperature setting value is reversed. The temperature setting value of the first group of experiments is [Tk11...TK15].

[0085] (3) Collect the film thickness results of the first set of experiments [Tk11...Tk15], use Kalman filtering to modify the relationship matrix, and obtain a new relationship matrix

[0086] Among them, Gain_1 is the Kalman filter gain.

[0087] (4) According to the results of the n-1th group of process experiments, the Kalman filter is used to correct and obtain the new relationship matrix Xn-1, and the target film thickness [Tk Tk Tk Tk Tk] is reversed to infer the next group of experimental temperatures [Zn1...Zn5].

[0088] (5) Collect the film thickness results of the latest experiment [Tkn1...Tkn5], and then use Kalman filtering to correct the relationship matrix again to obtain a new relationship matrix Xn.

[0089] Where Xn-1 is Gain_n is the Kalman filter gain calculated based on the latest experimental corrections.

[0090] (6) Repeat the above steps (4) and (5) until the uniformity between slices meets the requirements.

[0091] To further reduce the number of optimization experiments, the aforementioned Kalman filter was used to modify the relationship matrix. The optimal temperature setting was then calculated based on the modified relationship matrix. Iterative experiments were then conducted to improve inter-surface uniformity. This method eliminated reliance on individual engineers' experience and reduced experimental blindness. The number of adjustments required was significantly less than manual adjustments, achieving the customer's target inter-surface uniformity value, improving process debugging efficiency.

[0092] The embodiment of the present disclosure establishes a relationship model between temperature and film thickness, and calculates the optimal temperature setting for the next set of processes based on the relationship model to improve the uniformity between surfaces; by collecting a small amount of temperature setting and corresponding film thickness data of the equipment (at least 2 groups are required), the relationship matrix between the temperature setting and film thickness data is calculated based on the generalized inverse matrix; according to the requirements of the target film thickness uniformity between slices, the intermediate results are calculated and normalized; the relationship matrix is ​​corrected using Kalman filtering, and then the relationship matrix is ​​continuously iteratively corrected based on the experimental results, which can reduce the number of uniformity adjustments between slices.

[0093] This method breaks the traditional requirement for process experience and reduces process adjustment time. Even junior process engineers can use this method to optimize process recipe parameters in the shortest possible time, improving process debugging efficiency.

[0094] The embodiment of the present disclosure also provides a semiconductor process equipment, including: a furnace body, in which a heating element and a process tube are provided, and a wafer boat is placed in the process tube; a controller connected to the heating element, and used to execute the above-mentioned process parameter determination method.

[0095] As an embodiment, the semiconductor process equipment further includes: a gas input component for inputting process gas into the process tube; and / or a pressure control component for controlling the pressure in the process tube.

[0096] The semiconductor process equipment provided in this embodiment can implement each process in the embodiment of the above-mentioned process parameter determination method and can achieve the same technical effect. To avoid repetition, it will not be described here.

[0097] This embodiment further provides a computer-readable storage medium having a computer program stored thereon. When executed by a processor, the computer program implements each process of the above-described method for determining process parameters and achieves the same technical effect. To avoid repetition, the details are not described here. The computer-readable storage medium may be, for example, a read-only memory (ROM), a random access memory (RAM), a magnetic disk, or an optical disk.

[0098] Of course, those skilled in the art will understand that all or part of the processes in the above-mentioned embodiment methods can be implemented by a computer program instruction control device, and the computer program can be stored in a computer-readable storage medium. When the computer program is executed, it may include processes such as the above-mentioned method embodiments, wherein the storage medium may be a memory, a disk, an optical disk, etc.

[0099] Although the present disclosure is disclosed above, the present disclosure is not limited thereto. Any person skilled in the art may make various changes and modifications without departing from the spirit and scope of the present disclosure. Therefore, the scope of protection of the present disclosure shall be based on the scope defined by the claims.

[0100] Finally, it should be noted that, in this document, relational terms such as first and second, etc., are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any actual relationship or order between these entities or operations. Moreover, the terms "comprises," "comprising," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or device comprising a series of elements includes not only those elements, but also other elements not explicitly listed, or elements inherent to such process, method, article, or device. In the absence of further limitations, an element defined by the phrase "comprising a ..." does not exclude the presence of additional identical elements in the process, method, article, or device comprising the element.

[0101] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0102] The above description of the disclosed embodiments is intended to enable one skilled in the art to implement or use the present disclosure. Various modifications to these embodiments will be readily apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present disclosure. Therefore, the present disclosure is not limited to the embodiments shown herein, but is intended to be construed in the widest manner consistent with the principles and novel features disclosed herein.

Claims

1. A method for determining process parameters, wherein: Applied to semiconductor process equipment, the method for determining the process parameters includes: Obtaining a relationship model between process parameters of a deposition process and the thickness of a deposited film on a wafer in each partition of the semiconductor process equipment; the process parameters include at least one of the following: a temperature setting value, a process gas flow rate, a pressure, and a process duration of each partition; Determining experimental process parameters according to the current relationship model and the deposition target film thickness of the wafers in each partition, and performing wafer thin film deposition according to the experimental process parameters; If the film thickness currently deposited on the wafer meets the film thickness uniformity requirements, the experimental process parameters are determined as the set process parameters; if the film thickness currently deposited on the wafer does not meet the film thickness uniformity requirements, the current relationship model is updated according to the experimental process parameters and the corresponding film thickness currently deposited on the wafer, and then the steps of determining the experimental process parameters based on the current relationship model and the deposition target film thickness of the wafers in each partition and performing wafer thin film deposition according to the experimental process parameters are executed until the film thickness currently deposited on the wafer meets the film thickness uniformity requirements.

2. The method according to claim 1, wherein: The step of determining the experimental process parameters according to the current relationship model and the deposition target film thickness of the wafers in each partition includes: According to the deposition target film thickness of the wafer in each partition and the current relationship model, an intermediate result of the process parameter is calculated; The experimental process parameters are calculated based on the intermediate results of the process parameters and the target process parameters.

3. The method according to claim 1, wherein: The updating of the current relationship model according to the experimental process parameters and the corresponding film thickness currently deposited on the wafer includes: Obtaining the film thickness of each partition obtained by performing wafer thin film deposition according to the experimental process parameters; The current relationship model is updated using the experimental process parameters and the film thickness.

4. The method according to claim 1, wherein: The relationship model is a relationship matrix, and the updating of the current relationship model according to the experimental process parameters and the corresponding film thickness currently deposited on the wafer includes: Acquire a film thickness matrix of each partition obtained by performing wafer thin film deposition according to the experimental process parameters; Calculating a difference matrix between the film thickness matrix of each partition and the target film thickness matrix of each partition, multiplying the difference matrix by a Kalman filter gain and then summing the difference matrix with the current relationship matrix to obtain an updated relationship matrix; The updated relationship matrix is ​​determined as the current relationship matrix.

5. The method according to claim 4, wherein: The method further comprises: The Kalman filter gain is updated according to a difference matrix between the film thickness matrix and the target film thickness matrix.

6. The method according to any one of claims 1 to 5, wherein: The relationship model between the process parameters of the deposition process and the thickness of the deposited film on the wafer in each partition of the semiconductor process equipment includes: Acquire multiple sets of the process parameters and the thickness of the film deposited on the wafer of each partition corresponding to each process parameter; convert the multiple sets of the process parameters and the thickness of the film deposited on the wafer of each partition corresponding to each process parameter into a matrix expression to obtain a relationship model between the process parameters and the thickness of the film deposited on the wafer of each partition; or, A relationship model between the previously known process parameters and the thickness of the deposited film on the wafer in each partition is obtained.

7. The method according to any one of claims 1 to 5, wherein: The method further comprises: Wafer thin film deposition is performed according to the set process parameters.

8. The method according to claim 2, wherein: The step of calculating the experimental process parameters according to the process parameter intermediate results and the target process parameters includes: Normalizing the process parameter intermediate result to obtain a normalized process parameter intermediate result; The normalized process parameter intermediate result is multiplied by the target process parameter to calculate the experimental process parameter.

9. The method according to claim 1, wherein: The relationship model is a relationship matrix, and the relationship matrix is ​​as follows: Wherein, n represents multiple sets of data of one process parameter, and m represents multiple different partitions in the semiconductor process equipment.

10. A semiconductor process equipment, wherein: include: A furnace body, wherein a heating element and a process tube are arranged in the furnace body, and a wafer boat is placed in the process tube; A controller is connected to the heating element and is used to execute the method for determining the process parameters according to any one of claims 1 to 8.

11. The semiconductor process equipment according to claim 10, wherein: Also includes: A gas input assembly, used for inputting process gas into the process pipe; and / or, The pressure control assembly is used to control the pressure in the process pipe.

Citation Information

Patent Citations

  • Thermal processing apparatus, method for regulating temperature of thermal processing apparatus, and program

    CN101540275A

  • Parameter adjustment method of semiconductor processing device

    CN104332435A

  • Film thickness adjusting optimization method used in CVD (chemical vapor deposition) film forming process

    CN104404479A

  • Process optimization method capable of improving uniformity of boron phosphorous silicate glass (BPSG) film obtained from low pressure chemical vapor deposition (LPCVD)

    CN104451607A

  • Method for monitoring silicon film thickness and uniformity in low pressure chemical vapor deposition (LPCVD) process

    CN111996514A

Cited By

  • Film homogenization deposition method and device for wafer surface treatment

    CN118996380A

  • Method and system for improving utilization rate of target material for magnetron sputtering coating

    CN121023456A