Self-luminous display device and method for manufacturing self-luminous display device

By employing a self-emissive display device design with balanced capacitance values through carefully controlled pixel circuit configurations and plasma etching, the issue of capacitance variations is addressed, enhancing display quality and longevity.

WO2024201684A1PCT designated stage expired Publication Date: 2024-10-03SHARP DISPLAY TECHNOLOGY CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/012358
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Existing self-emissive display devices suffer from deteriorated display quality due to changes in capacitance values between capacitive elements caused by variations in etching amounts, leading to uneven brightness and luminance issues.

Method used

The design incorporates a first and second pixel circuit with capacitors having the same circuit configuration but differing electrode distances and areas, with the second capacitor having larger distances and areas than the first, and a manufacturing method involving plasma etching to form conductive layers and insulating layers, ensuring balanced capacitance values.

Benefits of technology

This configuration reduces capacitance value differences between capacitors, improving display quality by minimizing original brightness unevenness and maintaining quality over time, especially after aging.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023012358_03102024_PF_FP_ABST
    Figure JP2023012358_03102024_PF_FP_ABST
Patent Text Reader

Abstract

A self-luminous display device according to the present disclosure comprises: a first pixel circuit including a first capacitor (C1); and a second pixel circuit having the same circuit configuration as that of the first pixel circuit and including a second capacitor (C2) corresponding to the first capacitor (C1). An inter-electrode distance (d2) of the second capacitor (C2) is longer than an inter-electrode distance (d1) of the first capacitor (C1) and an electrode area of the second capacitor (C2) is wider than an electrode area of the first capacitor (C1).
Need to check novelty before this filing date? Find Prior Art

Description

Self-luminous display device and method for manufacturing the same

[0001] The present disclosure relates to a self-emissive display device and a method for manufacturing a self-emissive display device.

[0002] Japanese Patent Application Laid-Open No. 2003-124222 discloses a configuration in which the ratio of capacitance values ​​between a plurality of capacitance elements in the same pixel circuit does not change even if the amount of etching varies.

[0003] JP 2010-175987 A (published August 12, 2010)

[0004] However, in the technique disclosed in Patent Document 1, the capacitance value of each capacitive element changes with the change in the amount of etching, which is likely to result in a decrease in display quality.

[0005] A self-luminous display device according to one aspect of the present disclosure comprises a first pixel circuit including a first capacitor, and a second pixel circuit having the same circuit configuration as the first pixel circuit and including a second capacitor corresponding to the first capacitor, wherein the inter-electrode distance of the second capacitor is greater than the inter-electrode distance of the first capacitor, and the electrode area of ​​the second capacitor is greater than the electrode area of ​​the first capacitor.

[0006] A method for manufacturing a self-luminous display device according to one embodiment of the present disclosure includes the steps of forming a first conductor layer, etching the first conductor layer using a first plasma to form a first electrode from the first conductor layer, forming an insulating layer above the first electrode, etching the insulating layer using a second plasma to thin at least a portion of the insulating layer, forming a second conductor layer above the insulating layer, and etching the second conductor layer using a third plasma to form a second electrode from the second conductor layer that overlaps the first electrode in a planar view.

[0007] According to one aspect of the present disclosure, the display quality of a display device can be improved.

[0008] FIG. 1 is a plan view showing a configuration example of a self-luminous display device according to an embodiment of the present disclosure. FIG. 2 is a cross-sectional view showing a configuration example of a first capacitor and a second capacitor shown in FIG. 1. FIG. 3 is a cross-sectional view showing a capacitor of a comparative example. FIG. 4 is a cross-sectional view showing an example of a method for manufacturing a self-luminous display device according to an embodiment of the present disclosure. FIG. 5 is a plan view showing an example of the intensity distribution of plasma shown in FIG. 4. FIG. 6 is a plan view showing a configuration example of a self-luminous display device according to an embodiment of the present disclosure. FIG. 7 is a cross-sectional view showing an example of a method for manufacturing a self-luminous display device according to an embodiment of the present disclosure.

[0009] [Embodiment 1] (Configuration) Fig. 1 is a plan view showing an example configuration of a self-emissive display device according to an embodiment of the present disclosure. As shown in Fig. 1, the self-emissive display device 1 according to the present disclosure includes a display unit DA including a plurality of pixels PX, and a drive circuit 10 that drives the display unit DA. Each of the plurality of pixels PX includes a light-emitting element 2 and a pixel circuit 3 that controls the current or voltage applied to the light-emitting element 2. Each of the pixel circuits 3 includes a capacitor CX.

[0010] The self-luminous display device 1 includes a first pixel circuit 31 including a first capacitor C1 and a second pixel circuit 32 having the same circuit configuration as the first pixel circuit 31 and including a second capacitor C2 corresponding to the first capacitor C1. More specifically, the second pixel circuit 32 has the same circuit element layout and connection relationship as the first pixel circuit 31, and the same characteristics as the corresponding circuit elements. The characteristics of the circuit elements include, for example, the threshold value of a transistor and the capacitance value of a capacitive element. As is well known, the capacitance value of a parallel-plate capacitor is inversely proportional to the distance between the electrodes of the capacitor and proportional to the electrode area of ​​the capacitor. Therefore, the first capacitor C1 and the second capacitor C2 are designed to have the same capacitance value, the same distance between the electrodes, and the same electrode area. The first capacitor C1 and the second capacitor C2 may be storage capacitors. Hereinafter, attention will be focused on the first capacitor C1 and the second capacitor C2.

[0011] 2 is a cross-sectional view showing an example of the configuration of the first capacitor and the second capacitor shown in FIG. 2. As shown in FIG. 2, the actual inter-electrode distance d2 of the second capacitor C2 is larger than the actual inter-electrode distance d1 of the first capacitor C1, and the actual electrode area of ​​the second capacitor C2 is larger than the actual electrode area of ​​the first capacitor C1. These actual differences are due to the manufacturing process. Hereinafter, actual values ​​and differences will be described unless otherwise specified as "design" or "ideal."

[0012] According to the above configuration, the difference between the inter-electrode distances d1 and d2 acts to make the capacitance value of the second capacitor C2 smaller than that of the first capacitor C1. On the other hand, the difference between the electrode areas S1 and S2 acts to make the capacitance value of the second capacitor C2 larger than that of the first capacitor C1. As a result of these effects (at least partially) canceling each other out, the difference in capacitance between the first capacitor C1 and the second capacitor C2 can be reduced.

[0013] FIG. 3 is a cross-sectional view of a comparative capacitor. As shown in FIG. 3, the comparative capacitors have the same inter-electrode distance but different electrode areas. Therefore, differences in electrode area directly lead to differences in capacitance, resulting in large differences in capacitance. In multiple pixel circuits of a self-luminous display device, such large differences in capacitance cause brightness unevenness and degrade display quality. Commercially, adjustments (known as "de-uniformity processing") are typically performed before shipping to make brightness unevenness invisible, but brightness unevenness that is difficult to adjust may remain. Furthermore, differences in capacitance lead to differences in aging, which causes brightness unevenness after aging and degrades display quality.

[0014] According to the configuration of the present disclosure, the difference in capacitance value is small, and therefore the original brightness unevenness before the demurration process is small, which improves the display quality of the self-luminous display device 1, and in particular improves the display quality after aging.

[0015] The first capacitor C1 has a first electrode E1 and a second electrode E2 that face each other, and the second capacitor C2 has a third electrode E3 and a fourth electrode E4 that face each other. The first electrode E1 and the third electrode E3 are formed from the same layer, and the second electrode E2 and the fourth electrode E4 are formed from the same layer. The area A3 of the third electrode E3 is larger than the area A1 of the first electrode E1 (A1<A3), and the area A4 of the fourth electrode E4 is larger than the area A2 of the second electrode E2 (A2<A4). The electrode area of ​​the first capacitor C1 is the area where the first electrode E1 and the second electrode E2 overlap each other in a plan view, and the electrode area of ​​the second capacitor C2 is the area where the third electrode E3 and the fourth electrode E4 overlap each other in a plan view.

[0016] The self-luminous display device 1 further includes an insulating layer 4 having a first portion P1 located between the first electrode E1 and the second electrode E2 and a second portion P2 located between the third electrode E3 and the fourth electrode E4. The thickness of the second portion P2 is greater than the thickness of the first portion P1. The insulating layer 4 may be an inorganic insulating layer and may contain, for example, silicon nitride (SiN), silicon oxide (SiO), or silicon oxynitride (SiNO).

[0017] (Manufacturing Method) Figure 4 is a cross-sectional view showing an example of a manufacturing method for a self-luminous display device according to an embodiment of the present disclosure. As shown in Figure 4, the manufacturing method according to the present disclosure first forms a first conductor layer 11 above a substrate BP (step S10), and then forms a patterned first template layer 21 on the first conductor layer 11 (step S12). Then, the first conductor layer 11 is etched using a first plasma 41 according to the first template layer 21 to form a first electrode E1 and a third electrode E3 from the first conductor layer 11 (step S14), and the first template layer 21 is removed (step S16). In step S14, the stronger the first plasma 41, the smaller the electrodes formed.

[0018] Next, an insulating layer 4 is formed above the first electrode E1 and the third electrode E3 (step S20), and the insulating layer 4 is etched using a second plasma 42 so that at least a portion of the insulating layer 4 becomes thinner (step S24). In step S20, the thickness of the insulating layer 4 is approximately uniform. In step S24, the insulating layer 4 is etched using the second plasma 42 while the entire top surface of the insulating layer 4 is exposed. Therefore, the insulating layer 4 is etched so that the entire insulating layer 4 becomes thinner. Furthermore, the stronger the second plasma 42, the thinner the insulating layer 4 becomes.

[0019] Next, a second conductor layer 12 is formed on the insulating layer 4 (step S30), and a patterned second template layer 22 is formed on the second conductor layer 12 (step S32). Then, the second conductor layer 12 is etched by a third plasma 43 according to the second template layer 22 to form a second electrode E2 and a fourth electrode E4 from the second conductor layer 12 (step S34), and the second template layer 22 is removed. In step S34, the stronger the third plasma 43, the smaller the electrodes formed.

[0020] According to this manufacturing method, the stronger the first to third plasmas 41 to 43 are in the region, the smaller the inter-electrode distance and electrode area of ​​the capacitors. Specifically, the inter-electrode distance d1 and electrode area of ​​the first capacitor C1 formed in the region where the plasma intensity is strong are smaller than the inter-electrode distance d2 and electrode area of ​​the second capacitor C2 formed in the region where the plasma intensity is weak. As a result, the effects of the inter-electrode distance and electrode area on the capacitance value of the capacitors are (at least partially) canceled out, thereby reducing the difference between the design capacitance value of the capacitor and the actual capacitance value of the capacitor. Furthermore, the difference in capacitance value between the first capacitor C1 formed in the region where the plasma intensity is strong and the second capacitor C2 formed in the region where the plasma intensity is weak can be reduced.

[0021] FIG. 5 is a plan view showing an example of the intensity distribution of the plasma shown in FIG. 4. As shown in FIG. 5, the first to third plasmas 41 to 43 may each have a spatially non-uniform intensity distribution. Typically, within the chamber 40 where the plasma is generated, the plasma is weak in the central region F1 and the peripheral region F2, and strong in the intermediate region F3 between them. The shape of the intermediate region F3 corresponds to the shape of the plasma generating electrode and is usually annular. It is beneficial that the intensity distributions of the first to third plasmas 41 to 43 are substantially identical to one another. Specifically, it is beneficial that the first to third plasmas 41 to 43 are strong in the region where the first capacitor C1 is formed and weak in the region where the second capacitor C2 is formed. The intensity distribution may be measured or estimated from the configuration of the plasma generator. If the shape and arrangement of the plasma generating electrodes are identical, it can be determined that the intensity distributions of the first to third plasmas 41 to 43 are identical. Moreover, the first to third plasmas 41 to 43 may be generated by the same device.

[0022] [Embodiment 2] Another embodiment of the present disclosure will be described below. For ease of explanation, the same reference numerals will be used to designate components having the same functions as those described in the above embodiment, and the description thereof will not be repeated.

[0023] 6 is a cross-sectional view showing an example of the configuration of a self-luminous display device according to an embodiment of the present disclosure. As shown in FIG. 6, the self-luminous display device 1 according to the present disclosure may further include a connection structure 50 in which the lower electrode E5 is connected to the upper electrode E6 through a contact hole CH. The lower electrode E5 may be formed from the same layer as the first electrode E1 and the third electrode E3, and the upper electrode E6 may be formed from the same layer as the second electrode E2 and the fourth electrode E4. The contact hole CH penetrates the insulating layer 4.

[0024] 7 is a cross-sectional view illustrating an example of a method for manufacturing a self-luminous display device according to an embodiment of the present disclosure. As illustrated in FIG. 7, steps S10 and S12 are performed in order, and in step S14, the first conductor layer 11 is etched by a first plasma 41 in accordance with the first template layer 21 so as to form the first electrode E1, the third electrode E3, and the lower electrode E5 from the first conductor layer 11.

[0025] Subsequently, steps S16 and S20 are performed to form a photoresist layer 23 on the insulating layer 4 (step S22), which has a first opening O1 that overlaps the first electrode E1 in plan view but does not penetrate therethrough, and a second opening O2 that overlaps the lower electrode E5 in plan view but penetrates therethrough. In step S22, a third opening O3 that overlaps the third electrode E3 in plan view but does not penetrate therethrough is also formed. Ideally, the third opening O3 has the same size as the first opening O1.

[0026] Then, the photoresist layer 23 and the insulating layer 4 are etched by the second plasma 42 (step S24), and the photoresist layer 23 is removed (step S26). In step S24, the insulating layer 4 is etched by the second plasma 42 while the photoresist layer 23 remains on the insulating layer 4. Therefore, the insulating layer 4 is etched so that a portion of the insulating layer 4 (specifically, the portion overlapping with the first opening O1) becomes thinner.

[0027] In step S24, the photoresist layer 23 is etched with the second plasma 42 so that the first opening O1 penetrates the photoresist layer 23, and the insulating layer 4 is further etched so that the portion of the insulating layer 4 overlapping with the first opening O1 in a plan view becomes thinner. At the same time, the insulating layer 4 is etched with the second plasma 42 so that a contact hole CH is formed in the portion of the insulating layer 4 overlapping with the second opening O2 in a plan view. In step S24, the third opening O3 may also penetrate the photoresist layer 23. The depth to which the portion of the insulating layer 4 overlapping with the third opening O3 is removed may be smaller than the depth to which the portion of the insulating layer 4 overlapping with the first opening O1 is removed, and may even be zero.

[0028] Subsequently, steps S30 and S32 are performed in order, and in step S34, the second conductor layer 12 is etched using a third plasma 43 to form a second electrode E2 and a fourth electrode E4 from the second conductor layer 12, and an upper electrode E6 connected to the lower electrode E5 through the contact hole CH. Then, the second template layer 22 is removed.

[0029] The present disclosure is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. Embodiments obtained by appropriately combining the technical means disclosed in different embodiments are also included in the technical scope of the present disclosure. Furthermore, new technical features can be formed by combining the technical means disclosed in each embodiment.

[0030] REFERENCE SIGNS LIST 1 Self-luminous display device 4 Insulating layer 11 First conductor layer 12 Second conductor layer 23 Photoresist layer 31 First pixel circuit 32 Second pixel circuit 41 First plasma 42 Second plasma 43 Third plasma A1, A2, A3, A4 Area C1 First capacitor C2 Second capacitor CH Contact hole d1, d2 Distance between electrodes E1 First electrode E2 Second electrode E3 Third electrode E4 Fourth electrode E5 Lower electrode E6 Upper electrode P1 First portion P2 Second portion

Claims

1. A self-luminous display device comprising: a first pixel circuit including a first capacitor; and a second pixel circuit having the same circuit configuration as the first pixel circuit and including a second capacitor corresponding to the first capacitor, wherein the inter-electrode distance of the second capacitor is larger than the inter-electrode distance of the first capacitor, and the electrode area of ​​the second capacitor is larger than the electrode area of ​​the first capacitor.

2. The self-luminous display device of claim 1, wherein the first capacitor has a first electrode and a second electrode facing each other, the second capacitor has a third electrode and a fourth electrode facing each other, the first electrode and the third electrode being formed from the same layer as each other, and the second electrode and the fourth electrode being formed from the same layer as each other.

3. The self-luminous display device according to claim 2, wherein the area of ​​the third electrode is larger than the area of ​​the first electrode, and the area of ​​the fourth electrode is larger than the area of ​​the second electrode.

4. A self-luminous display device as described in claim 2 or 3, wherein the electrode area of ​​the first capacitor is the area where the first electrode and the second electrode overlap each other in a planar view, and the electrode area of ​​the second capacitor is the area where the third electrode and the fourth electrode overlap each other in a planar view.

5. A self-luminous display device as described in claim 2 or 3, further comprising an insulating layer having a first portion located between the first electrode and the second electrode and a second portion located between the third electrode and the fourth electrode, wherein the thickness of the second portion is greater than the thickness of the first portion.

6. A method for manufacturing a self-luminous display device, comprising: a step of forming a first conductor layer; a step of etching the first conductor layer with a first plasma so as to form a first electrode from the first conductor layer; a step of forming an insulating layer above the first electrode; a step of etching the insulating layer with a second plasma so as to thin at least a portion of the insulating layer; a step of forming a second conductor layer above the insulating layer; and a step of etching the second conductor layer with a third plasma so as to form a second electrode from the second conductor layer that overlaps with the first electrode in a planar view.

7. The method for manufacturing a spontaneous light-emitting display device according to claim 6, wherein each of the first to third plasmas has a spatially non-uniform intensity distribution.

8. The method for manufacturing a spontaneous light-emitting display device according to claim 6 or 7, wherein the intensity distributions of the first, second and third plasmas are identical to each other.

9. The method for manufacturing a self-luminous display device according to any one of claims 6 to 8, wherein the first, second and third plasmas are generated by a same device.

10. The method for manufacturing a self-luminous display device according to claim 6, wherein the insulating layer is etched by the second plasma in a state where the entire upper surface of the insulating layer is exposed.

11. A method for manufacturing a self-luminous display device as described in any one of claims 6 to 9, further comprising the steps of: forming a lower electrode from the first conductor layer; and forming a photoresist layer on the insulating layer, the photoresist layer having a first opening that overlaps with the first electrode in a planar view and does not penetrate the first electrode, and a second opening that overlaps with the lower electrode in a planar view and penetrates the insulating layer; and etching the photoresist layer and the insulating layer with the second plasma.

12. A method for manufacturing a self-luminous display device as described in claim 11, wherein the photoresist layer is etched by the second plasma so that the first opening penetrates the photoresist layer, and the insulating layer is etched so that the portion of the insulating layer that overlaps with the first opening in a planar view becomes thinner.

13. A method for manufacturing a self-luminous display device as described in claim 11 or 12, wherein the insulating layer is etched using the second plasma so as to form a contact hole in a portion of the insulating layer that overlaps with the second opening in a planar view, and an upper electrode is formed using the third plasma from the second conductor layer, the upper electrode being connected to the lower electrode through the contact hole.

Citation Information

Patent Citations

  • Display device

    JP2008129550A

  • Display device and electronic equipment

    JP2008249919A

  • Display device

    JP2012068662A

  • Display and manufacturing method of display

    JP2017120376A

  • Thin film transistor substrate and method for fabricating the same