Optical component, transparent sealing member, substrate, and method for manufacturing optical component

The multi-layered structure with a stress relaxation layer and diffusion prevention layers addresses thermal stress issues in optical components by ensuring effective stress relief between the transparent sealing member and substrate, preventing peeling and damage, and ensuring reliable optical component sealing.

WO2024201707A1PCT designated stage expired Publication Date: 2024-10-03NGK INSULATORS LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/012494
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Optical components face thermal stress issues due to differences in thermal expansion coefficients between transparent sealing members and substrates, leading to cracking or peeling, especially during high-temperature processes like reflow mounting, where existing stress relaxation layers fail to provide sufficient relief.

Method used

A multi-layered structure is implemented with a stress relaxation layer made of materials like Cu, Au, or Ag, having a Young's modulus of 150 GPa or less, and diffusion prevention layers to prevent interdiffusion, ensuring a total thickness of 1.2 μm or more, which effectively alleviates thermal stress between the transparent sealing member and the substrate.

Benefits of technology

This configuration significantly reduces the risk of peeling and damage to the transparent sealing member, maintaining its integrity under thermal stress conditions, even with varying thicknesses and thermal expansion coefficients, thereby ensuring reliable sealing of optical elements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023012494_03102024_PF_FP_ABST
    Figure JP2023012494_03102024_PF_FP_ABST
Patent Text Reader

Abstract

The present invention relates to an optical component (10) for bonding and sealing a transparent sealing member (14) to a substrate (44) on which an optical element (12) is mounted, the transparent sealing member (14), the substrate (44), and a method for manufacturing the optical component (10). On metallization layers (24, 46) that bond the transparent sealing member (14) and the substrate (44), there are provided: one or more stress relaxation layers (30) each configured from a metal film having a Young's modulus of 150 GPa or less, the total thickness of the one or more stress relaxation layers (30) being 1.2 µm or greater; and diffusion-preventing layers (28, 32) that are arranged on both thickness-direction sides of the stress relaxation layer (30) and that prevent diffusion of the metal constituting the one or more stress relaxation layers (30).
Need to check novelty before this filing date? Find Prior Art

Description

Optical component, transparent sealing member, substrate, and method for manufacturing optical component

[0001] The present invention relates to an optical component, a transparent sealing member, a substrate, and a method for manufacturing the optical component.

[0002] Optical components such as light-emitting devices and optical sensors have a structure in which a transparent sealing member is bonded to a substrate on which an optical element is mounted, and the optical element is sealed with the transparent sealing member. The optical element is a light-emitting element (e.g., an LED) or a light-receiving element (e.g., a photodiode). The transparent sealing member is made of glass and is bonded to the substrate using a low-melting-point alloy such as solder.

[0003] Japanese Patent Application Laid-Open No. 2021-118199 discloses a technique for providing a metallized layer on the quartz glass and the mounting substrate in order to solder a transparent sealing member made of quartz glass to the substrate.

[0004] Japanese Patent Application Laid-Open No. 2019-046826 discloses a technology for providing a 0.3 μm to 10 μm thick Au (gold) film as a stress relaxation layer at the joint between a transparent sealing member made of quartz glass and a substrate to prevent cracks in the transparent sealing member due to thermal expansion.

[0005] Optical components may be exposed to high temperatures due to heat generated by light-emitting elements in their operating environment. Furthermore, in the reflow process for mounting optical components, they may be exposed to high temperatures, for example, 200°C to 400°C. This can cause thermal stress at the joint between the transparent sealing member and the substrate due to the difference in thermal expansion coefficient between the two, potentially causing cracks or peeling in the fragile transparent sealing member and potentially breaking the seal on the optical element.

[0006] The metallized layer of JP 2021-118199 A may not provide a sufficient stress relaxation effect.

[0007] The stress relaxation layer in JP 2019-046826 A is made of Au, but due to interdiffusion with the adjacent low-melting-point alloy (solder) containing Sn (tin), the stress relaxation layer may deteriorate, and sufficient stress relaxation effect may not be obtained.

[0008] An object of the present invention is to solve the above-mentioned problems.

[0009] The following are exemplary aspects of the present invention. [Item 1] One aspect of the present invention relates to an optical component comprising a substrate carrying an optical element, a transparent sealing member bonded above the substrate to seal the optical element, and a bonding portion formed by stacking multiple metal films and bonding the transparent sealing member to the substrate. The bonding portion includes one or more stress relaxation layers formed of metal films having a Young's modulus of 150 GPa or less and a total thickness of 1.2 μm or more, and diffusion prevention layers disposed on both sides of the stress relaxation layer in the thickness direction to prevent diffusion of the metal constituting the stress relaxation layer. The optical component can prevent deterioration of the stress relaxation layer with the diffusion prevention layers, maintaining a sufficient stress relaxation layer, thereby effectively suppressing peeling or damage to the transparent sealing member due to thermal stress. [Item 2] In the optical component according to Item 1, the stress relaxation layer may be made of Cu (copper), Au (gold), Ag (silver), or Zn (zinc). This optical component can prevent peeling or damage to the transparent sealing member due to thermal shock. [Item 3] In the optical component according to item 1 or 2, the diffusion prevention layer may be made of Ni (nickel), Pd (palladium), or Pt (platinum). This optical component can prevent deterioration of the stress relaxation layer and prevent peeling or damage to the transparent sealing member. [Item 4] In the optical component according to any one of items 1 to 3, the stress relaxation layer may have a thermal expansion coefficient of 40 ppm / K or less. Such a stress relaxation layer can suppress the generation of thermal stress due to thermal deformation of the stress relaxation layer itself. [Item 5] In the optical component according to any one of items 1 to 4, the total thickness of the stress relaxation layer may be 10 μm or less. [Item 6] In the optical component according to any one of items 1 to 5, the total thickness of the stress relaxation layer may be 0.28% or more of the thickness of the transparent sealing member above the stress relaxation layer. This optical component can relieve thermal stress between the transparent sealing member and the substrate because the stress relaxation layer is formed with a sufficient thickness. [Item 7] In the optical component according to any one of Items 1 to 6, the transparent sealing member above the stress relaxation layer may have a thickness of 0.2 mm or more. As the thickness of the transparent sealing member increases, the transparent sealing member tends to be less flexible and thermal stress tends to increase. This optical component can relieve thermal stress and prevent peeling or damage to the transparent sealing member, even when the transparent sealing member is thick.[Item 8] The optical component according to any one of items 1 to 7, wherein the total thickness of the stress relaxation layer may be 0.25% or more of the thickness of the substrate below the stress relaxation layer. Because the stress relaxation layer is formed with a sufficient thickness, this optical component can relieve thermal stress between the transparent sealing member and the substrate. [Item 9] The optical component according to any one of items 1 to 8, wherein the total thickness of the stress relaxation layer may be 0.05% or more of the sum of the thickness of the transparent sealing member above the stress relaxation layer and the thickness of the substrate below the stress relaxation layer. Because the stress relaxation layer is formed with a sufficient thickness, this optical component can relieve thermal stress between the transparent sealing member and the substrate. [Item 10] The optical component according to any one of items 1 to 9, wherein the value of A×B is 5×10, where A (ppm / K) is the difference between the thermal expansion coefficient of the transparent sealing member and the thermal expansion coefficient of the substrate, and B (mm) is the outer dimension of the joint. -6mm / K or more. [Item 11] In the optical component according to item 10, the outer dimension of the joint may be 3 mm or more. This optical component can prevent peeling or damage even to transparent sealing members of a size common to light-emitting diodes. [Item 12] In the optical component according to any one of items 1 to 11, the transparent sealing member may be made of quartz glass or ultraviolet-transmitting glass. This optical component can prevent peeling or damage to the transparent sealing member of a weaker strength, such as an ultraviolet light-emitting diode or an ultraviolet light-receiving element. [Item 13] In the optical component according to item 12, the transparent sealing member may have a thermal expansion coefficient of 1 ppm / K or less. [Item 14] In the optical component according to any one of items 1 to 13, the substrate may be made of aluminum nitride, alumina, silicon, Kovar, or silicon nitride. [Item 15] In the optical component according to item 14, the substrate may have a thermal expansion coefficient of 2.5 ppm / K or more. [Item 16] In the optical component described in any one of Items 1 to 15, the thickness of the substrate below the stress relaxation layer may be 0.2 mm or more. [Item 17] In the optical component described in any one of Items 1 to 16, the bonding portion includes a first metallization layer formed on the bonding surface of the transparent sealing member facing the substrate and composed of multiple metal films, a second metallization layer formed on the substrate and composed of multiple metal films, and a low-melting-point alloy layer bonding the first metallization layer to the second metallization layer. The stress relaxation layer and the diffusion prevention layer may be provided on at least one of the first metallization layer and the second metallization layer. This optical component can achieve both adhesion provided by the low-melting-point alloy layer and thermal stress relaxation performance. [Item 18] In the optical component described in Item 17, the stress relaxation layer and the diffusion prevention layer may be provided on both the first metallization layer and the second metallization layer. This optical component can relieve thermal stress between the transparent sealing member and the substrate.[Item 19] Another aspect of this embodiment is a transparent sealing member bonded to a substrate carrying an optical element and sealing the optical element, comprising: a lens covering the optical element; a bonding surface provided on the periphery of the lens and bonded to the substrate; and a first metallization layer formed on the bonding surface. The first metallization layer has a stress relief layer formed of a metal film having a Young's modulus of 150 GPa or less and a thickness of 1.2 μm or more; and diffusion prevention layers disposed on both sides of the stress relief layer in the thickness direction to prevent diffusion of the metal constituting the stress relief layer. This transparent sealing member can prevent deterioration of the diffusion prevention layer while alleviating thermal stress with the substrate via the diffusion prevention layers. [Item 20] The transparent sealing member described in Item 19 may further include a low-melting-point alloy layer formed on the first metallization layer. Because this transparent sealing member already has a low-melting-point alloy layer, the bonding process to the substrate can be simplified. [Item 21] Yet another aspect of the present invention is a substrate for mounting an optical element, the substrate comprising: an upper surface located on the periphery of a portion for mounting the optical element and to which a transparent sealing member is bonded; and a second metallized layer formed on the upper surface, the second metallized layer comprising: a stress relief layer formed of a metal film having a Young's modulus of 150 GPa or less and a thickness of 1.2 μm or more; and diffusion prevention layers disposed on both sides of the stress relief layer in a thickness direction to prevent diffusion of the metal constituting the stress relief layer. This substrate can prevent deterioration of the diffusion prevention layer while the diffusion prevention layers can relieve thermal stress between the substrate and the substrate, thereby preventing peeling and damage to the bonded transparent sealing member. [Item 22] Yet another aspect of the present invention is a method for manufacturing an optical component in which an optical element mounted on a substrate is sealed with a transparent sealing member, the method comprising: joining a first metallization layer of the transparent sealing member to a second metallization layer of the substrate with a low-melting-point alloy; and providing, in at least one of the first metallization layer and the second metallization layer, one or more stress relaxation layers each made of a metal film having a Young's modulus of 150 GPa or less and a total thickness of 1.2 μm or more; and diffusion prevention layers disposed on both sides of the stress relaxation layer in the thickness direction to prevent diffusion of the metal constituting the stress relaxation layer. This method for manufacturing an optical component can prevent peeling or damage to the transparent sealing member.

[0010] The above-described optical component, transparent sealing member, substrate, and method for manufacturing an optical component can prevent peeling or damage to the transparent sealing member due to thermal stress.

[0011] FIG. 1A is a perspective view of an array member used in manufacturing a transparent sealing member according to the first embodiment, and FIG. 1B is a perspective view of a first metallization layer formed on the bonding surface of the array member. FIG. 2A is a cross-sectional view of the first metallization layer of FIG. 1B, and FIG. 2B is an explanatory diagram of a singulation process. FIG. 3A is an explanatory diagram of a process of attaching a low-melting-point alloy foil to the first metallization layer, and FIG. 3B is an explanatory diagram of a transparent sealing member having a first metallization layer and a low-melting-point alloy layer. FIG. 4A is an explanatory diagram of a process of bonding the transparent sealing member of FIG. 3B to a substrate, and FIG. 4B is an explanatory diagram of an optical component according to the first embodiment. FIG. 5A is a plan view of the optical component according to the first embodiment, and FIG. 5B is a cross-sectional view of the optical component of FIG. 5A. FIG. 6A is an exploded perspective view of an optical component according to a first modification of the first embodiment, and FIG. 6B is a cross-sectional view of the optical component of FIG. 6A. FIG. 7A is an exploded perspective view of an optical component according to Modification 2 of the first embodiment, and FIG. 7B is a cross-sectional view of the optical component of FIG. 7A. FIG. 8A is a cross-sectional view of an optical component according to Modification 3 of the first embodiment, and FIG. 8B is a cross-sectional view of an optical component according to Modification 4 of the first embodiment. FIG. 9A is a cross-sectional view of an optical component according to a second embodiment, and FIG. 9B is a cross-sectional view of an optical component according to a third embodiment. FIG. 10 is a table showing the configurations of the transparent sealing members and low-melting-point alloy layers of the optical components according to Examples 1 to 5 and Comparative Examples 1 and 2. FIG. 11 is a table showing the relationship between the substrate configurations of the optical components according to Examples 1 to 5 and Comparative Examples 1 and 2 and the thickness of the optical components, as well as the evaluation results of a thermal shock test. FIG. 12 is a graph showing the relationship between the thickness of the stress relaxation layer and the peeling incidence rate for Examples 1 to 5 and Comparative Examples 1 and 2, with the thickness of the stress relaxation layer on the horizontal axis and the peeling incidence rate on the vertical axis. FIG. 13 is a table showing the configurations of the transparent sealing members and low-melting-point alloy layers of Examples 6 to 10. Fig. 14 is a table showing the relationship between the substrate configuration and the thickness of the optical component and the evaluation results of the thermal shock test for Examples 6 to 10. Fig. 15 is a table showing the configurations of the transparent sealing member and the low-melting-point alloy layer for Examples 11 to 15. Fig. 16 is a table showing the relationship between the substrate configuration and the thickness of the optical component and the evaluation results of the thermal shock test for Examples 11 to 15.

[0012] First Embodiment An optical component 10 according to a first embodiment will be described below, along with a manufacturing method thereof. The optical component 10 of this embodiment will be described using an example in which an ultraviolet-emitting LED is sealed in a transparent sealing member 14 as the optical element 12. However, the optical component 10 is not limited to this, and can also be suitably applied to cases in which a light-emitting element such as various LEDs or a light-receiving element such as a photodiode is sealed in a transparent sealing member 14. The terms top, upper, bottom, and below used in this specification refer to the positional relationship within the component, and do not limit the installation direction of the optical component 10.

[0013] First, the manufacture of the transparent sealing member 14 of the optical component 10 will be described with reference to Figures 1A to 3B. In the manufacturing process of the transparent sealing member 14, an array member 16 as shown in Figure 1A is first prepared. The array member 16 is a plate-shaped member in which a plurality of lenses 18 are arranged vertically and horizontally. In this specification, the lenses 18 are portions that allow light to pass through. The lenses 18 are not necessarily limited to hemispherical shapes, and include flat window shapes.

[0014] The array member 16 of this embodiment includes a plurality of lenses 18, and is therefore also referred to as a lens array. The array member 16 has a front surface 16a from which the lenses 18 protrude, and a back surface 16b. In this embodiment, the array member 16 has a concave cavity 20 and a flat bonding surface 22 on the back surface 16b. The array member 16 is made of, for example, quartz glass. Details of a manufacturing method for the array member 16 are described, for example, in International Publication No. WO 2019 / 012743.

[0015] Next, the joining surface 22 of the array member 16 is polished. Polishing eliminates any unevenness on the joining surface 22, making it flat. When the joining surface 22 is flattened, less of the low-melting-point alloy layer 36 (solder) is required for bonding, and the amount of low-melting-point alloy layer 36 containing Au used can be reduced. Note that polishing of the joining surface 22 may be performed as needed depending on the unevenness of the joining surface 22, or may be omitted.

[0016] 1B, a metallization process is performed on the bonding surface 22. The metallization process is a process of forming a metal pattern (first metallization layer 24) on the bonding surface 22, which has excellent wettability with the low-melting-point alloy layer 36 and excellent adhesion with the transparent sealing member 14. As shown in the figure, the first metallization layer 24 is formed in a rectangular ring shape surrounding the periphery of the cavity 20 of each lens 18.

[0017] As shown in FIG. 2A , the process of forming the first metallized layer 24 includes stacking a first adhesion layer 26, a first diffusion prevention layer 28, a first stress relaxation layer 30, a second diffusion prevention layer 32, and a second adhesion layer 34 in this order on the joining surface 22. The first adhesion layer 26 is formed by depositing a metal film such as Ti (titanium) on the joining surface 22, for example, by sputtering. The first adhesion layer 26 is formed to a thickness of, for example, 0.01 to 0.5 μm. The material of the first adhesion layer 26 is selected from metal materials that have excellent adhesion to quartz glass or ultraviolet-transmitting glass. In addition to Ti, other materials for the first adhesion layer 26 include Cr (chromium).

[0018] The first diffusion prevention layer 28 is formed by depositing a Pd (palladium) film on the first adhesion layer 26 by sputtering. The first diffusion prevention layer 28 is formed to a thickness of, for example, 0.01 to 0.5 μm. The first diffusion prevention layer 28 prevents the diffusion of the metal that constitutes the first stress relaxation layer 30. The first diffusion prevention layer 28 is preferably made of a material that has excellent adhesion to the first adhesion layer 26 and the first stress relaxation layer 30. The first diffusion prevention layer 28 may be made of a Ni (nickel) film or a Pt (platinum) film.

[0019] The first stress relaxation layer 30 is formed, for example, by a Cu (copper) film. Such a first stress relaxation layer 30 is formed, for example, by forming a seed layer by sputtering and then depositing a Cu (copper) film on the seed layer by plating. Although not particularly limited, the first stress relaxation layer 30 may be formed to a thickness of, for example, 1.2 μm or more and 10 μm or less. Details of the thickness C of the first stress relaxation layer 30 will be described later. The first stress relaxation layer 30 is not limited to Cu, and a metal material with a Young's modulus of 150 GPa or less can be used. Furthermore, the first stress relaxation layer 30 is preferably made of a material with low thermal expansion, and preferably has a thermal expansion coefficient of 40 ppm / K or less. Examples of materials that can be used for the first stress relaxation layer 30 instead of Cu include Au, Ag (silver), and Zn (zinc).

[0020] The second diffusion prevention layer 32 is formed by depositing a Ni film (which may be a Pd film or a Pt film) on the first stress relief layer 30 by, for example, plating. The second diffusion prevention layer 32 has a thickness of 0.1 to 5 μm. The second diffusion prevention layer 32 prevents interdiffusion between the second adhesion layer 34 or the low-melting-point alloy layer 36 (see FIG. 3A ) and the first stress relief layer 30, thereby preventing deterioration of the first stress relief layer 30. Pd or Pt may be used for the second diffusion prevention layer 32 instead of Ni.

[0021] The second adhesion layer 34 is formed by depositing an Au film on the second diffusion prevention layer 32, for example, by plating. The second adhesion layer 34 is formed to a thickness of, for example, 0.1 to 2 μm. The second adhesion layer 34 is formed of a material that has excellent wettability and adhesion with a low-melting-point alloy containing Sn (tin), such as solder. The second adhesion layer 34 is mixed and integrated with the low-melting-point alloy layer 36 without forming a boundary, thereby exhibiting high adhesion to the low-melting-point alloy layer 36.

[0022] Each of the above-described first to second adhesion layers 26 to 34 is formed over the entire back surface 16b (see FIG. 1A) of the array member 16. Then, a mask (not shown) of a predetermined shape is formed on the second adhesion layer 34. The mask may be formed by applying a photoresist material followed by exposure and development, or by applying a mask material using a printing method. Then, each of the first adhesion layer 26 to the second adhesion layer 34 in the portions exposed from the mask is removed by etching, thereby completing the first metallization layer 24 consisting of the annular pattern shown in FIG. 1B.

[0023] Next, as shown in Fig. 2B, a singulation process is performed. In the singulation process, the array member 16 is cut into individual transparent sealing members 14 by a dicing saw 38. As shown in Fig. 3A, rectangular pedestal portions 40 are formed around the lenses 18 in the cut transparent sealing members 14. The pedestal portions 40 are formed in a flat plate shape. The cut transparent sealing members 14 are stored in a tray (not shown) with the bonding surface 22 facing upward.

[0024] 3A, a low-melting-point alloy foil 42 is placed on the first metallization layer 24. The low-melting-point alloy foil 42 is pre-shaped so as to overlap at least a portion of the first metallization layer 24. The low-melting-point alloy foil 42 is made of, for example, an AuSn (gold-tin) alloy. In addition to an AuSn alloy, various alloys containing Sn and having a melting point of 450°C or less can also be used for the low-melting-point alloy foil 42.

[0025] 3B , the low-melting-point alloy foil 42 is partially bonded onto the first metallized layer 24 by, for example, dot welding as described in Japanese Patent No. 7182596. The bonded low-melting-point alloy foil 42 forms the low-melting-point alloy layer 36. Through the above steps, the transparent sealing member 14 is completed.

[0026] Next, as shown in Figures 4A and 4B, a step of bonding the transparent sealing member 14 to the substrate 44 is performed. As shown in Figure 4A, the substrate 44 has the optical element 12 mounted on its upper surface 44a. The optical element 12 is, for example, an ultraviolet light-emitting diode that emits ultraviolet light. The substrate 44 is made of, for example, aluminum nitride, alumina, silicon, Kovar, or silicon nitride. The substrate 44 has a thermal expansion coefficient of, for example, 2.5 ppm / K or more. The substrate 44 usually has a thermal expansion coefficient different from that of the transparent sealing member 14. The substrate 44 has a second metallized layer 46 at a bonding region 44b on its upper surface 44a.

[0027] The second metallized layer 46 of this embodiment is formed by laminating a third adhesion layer 48, a third diffusion prevention layer 50, and a fourth adhesion layer 56 in this order on the upper surface 44a of the substrate 44. The third adhesion layer 48 is made of a metal film that has excellent adhesion to the substrate 44. The third adhesion layer 48 is made of, for example, a Cr film (or a Ti film) with a thickness of 0.01 to 0.5 μm. Such a Cr film is formed, for example, by sputtering.

[0028] The third diffusion prevention layer 50 is a metal film that prevents diffusion of the fourth adhesion layer 56. The third diffusion prevention layer 50 is made of, for example, a Ni film (or a Pd film or a Pt film) having a thickness of 0.01 to 0.5 μm. Such a Ni film is formed by sputtering.

[0029] The fourth adhesive layer 56 is a metal film that has excellent wettability and adhesiveness with the low-melting-point alloy layer 36. The fourth adhesive layer 56 is made of, for example, an Au film having a thickness of 0.1 to 2 μm.

[0030] The second metallization layer 46 is formed by sequentially depositing the third adhesion layer 48, the third diffusion prevention layer 50, and the fourth adhesion layer 56, and then patterning them by etching using a mask of a predetermined shape.

[0031] Next, the transparent sealing member 14 is placed on the substrate 44. The transparent sealing member 14 is positioned so that the first metallization layer 24 is located on the second metallization layer 46 of the substrate 44, and is placed on the substrate 44. Thereafter, the substrate 44 and the transparent sealing member 14 are heated to a temperature of 200 to 400°C.

[0032] 4B, the low-melting-point alloy layer 36 melts, and the second adhesion layer 34 and the fourth adhesion layer 56 are integrated together. This process forms a bonded portion 58 in which the first metallized layer 24 and the second metallized layer 46 are bonded together without any gaps via the low-melting-point alloy layer 36. The optical component 10 is completed through the above process.

[0033] As shown in FIG. 5A , in a plan view of the optical component 10 of this embodiment, the substrate 44 is covered with a transparent sealing member 14. The transparent sealing member 14 includes a transparent portion 15 and a first metallized layer 24. The transparent sealing member 14 may be made of ultraviolet-transmitting glass (borosilicate glass) instead of quartz glass (thermal expansion coefficient of 1 ppm / K or less). The transparent portion 15 includes a hemispherical lens 18 and a rectangular, plate-like base portion 40 (also called a flange) formed around the lens 18. As shown in FIG. 5B , a hemispherical cavity 20 is formed inside the lens 18. The cavity 20 forms a space for accommodating the optical element 12.

[0034] As shown in Fig. 5A, the first metallization layer 24 is formed on the bonding surface 22 (see Fig. 2A). The first metallization layer 24 extends along the periphery of the lens 18 and is formed in a rectangular ring shape, with its corners located below the pedestal 40. In this embodiment, the thickness of the pedestal 40 is defined as the thickness D of the transparent sealing member 14 above the bonding portion 58. A portion of the first metallization layer 24 may overlap the lens 18. The outer dimension of the first metallization layer 24 is defined as the outer dimension B of the bonding portion 58. The bonding portion 58 has an outer dimension B of, for example, 3 mm or more.

[0035] 5B , the transparent sealing member 14 is bonded to the upper surface 44 a of the substrate 44 via a bonding portion 58. In the optical component 10, thermal stress occurs in both the substrate 44 and the transparent sealing member 14 due to temperature changes when the substrate 44 and the transparent sealing member 14 are bonded together. The magnitude of the thermal stress increases according to the difference in the amount of displacement due to thermal expansion between the transparent sealing member 14 and the substrate 44. If the thermal stress is large, cracks or peeling will occur in the relatively fragile transparent sealing member 14, and the seal on the optical element 12 will be broken.

[0036] The displacement amount of the transparent sealing member 14 and the substrate 44 per 1°C temperature change is related to the product (A×B) of the absolute value A [ppm / K] of the difference between the thermal expansion coefficient of the transparent sealing member 14 and the thermal expansion coefficient of the substrate 44 and the outer dimension B [mm] of the bonding portion 58 (first metallized layer 24). When the value of A×B is 5×10 -6 If it exceeds [mm / K], the transparent sealing member 14 is likely to crack or peel off.

[0037] To prevent damage to the transparent sealing member 14, the optical component 10 has a first stress relaxation layer 30 on the first metallized layer 24. The first stress relaxation layer 30 deforms in response to displacement between the transparent sealing member 14 and the substrate 44, thereby relieving thermal stress at the bonding portion 58. The thicker the first stress relaxation layer 30, the greater the displacement caused by thermal expansion that can be mitigated.

[0038] In the optical component 10, if the transparent sealing member 14 is thin, some of the thermal stress can be alleviated by elastic deformation of the transparent sealing member 14, allowing the thickness C of the first stress relaxation layer 30 to be thin. On the other hand, as the thickness D of the transparent sealing member 14 increases, the transparent sealing member 14 becomes more difficult to deform, and unless the thickness C of the first stress relaxation layer 30 is increased, cracks and peeling due to thermal stress become more likely to occur. If the thickness D of the transparent sealing member 14 is 0.2 mm or greater, peeling and cracking of the transparent sealing member 14 become more likely. In this case, if the thickness C of the first stress relaxation layer 30 is 0.28% or greater of the thickness D of the transparent sealing member 14, cracking and peeling of the transparent sealing member 14 are suppressed.

[0039] In optical component 10, similar to transparent sealing member 14, the substrate 44 becomes less susceptible to elastic deformation as its thickness increases, and therefore requires a thicker first stress relaxation layer 30. If the thickness of substrate 44 below bonding portion 58 is defined as thickness F of substrate 44, thickness C of first stress relaxation layer 30 should be 0.25% or more of thickness F of substrate 44, as this is preferable because cracking and peeling of transparent sealing member 14 can be suppressed.

[0040] Furthermore, it is preferable that the thickness C of the first stress relaxation layer 30 be set to 0.05% or more of the thickness E of the optical component 10, which is the sum of the thickness D of the transparent sealing member 14 and the thickness F of the substrate 44 (D+F).

[0041] 6A and 6B differs from the optical component 10 in Fig. 4B in a transparent sealing member 14A and a substrate 44A. In the configuration of the optical component 10A, the same components as those in the optical component 10 in Fig. 4B are designated by the same reference numerals, and detailed descriptions thereof will be omitted.

[0042] The transparent sealing member 14A has a hemispherical lens 18 and a rectangular base 40 provided around the lens 18. As shown in Fig. 6B, the lens 18 does not have a cavity 20 formed therein, but is filled with quartz glass. The entire bottom side of the transparent sealing member 14A is composed of a flat bonding surface 22.

[0043] The substrate 44A has a box-shaped cavity 60 on its upper surface 44a. The cavity 60 is formed in a rectangular shape in a plan view. The cavity 60 accommodates the optical element 12. The optical element 12 is bonded to the substrate 44A within the cavity 60. A second metallization layer 46 is formed on the upper surface 44a of the substrate 44A. The second metallization layer 46 is formed in a rectangular ring shape so as to surround the cavity 60. The second metallization layer 46 has the same configuration as the second metallization layer 46 described with reference to FIG. 4A .

[0044] In this modification, the thickness of the substrate 44A is defined as the thickness F of the substrate 44A below the bonding portion 58, as shown in Fig. 6B. In this modification, the first metallized layer 24 includes a first stress relief layer 30, the thickness of which is preferably 0.25% or more of the thickness of the substrate 44A.

[0045] This modification also makes it possible to prevent cracks and peeling of the transparent sealing member 14A.

[0046] (Variation 2 of First Embodiment) In an optical component 10B of this variation shown in FIGS. 7A and 7B, a transparent sealing member 14B is configured with a hemispherical lens 18. The transparent sealing member 14B does not have a plate-shaped pedestal 40 around the lens 18. The lens 18 does not have an internal cavity 20, and is filled with quartz glass. The bottom of the transparent sealing member 14B is formed by a flat bonding surface 22. The transparent sealing member 14B has an annular first metallization layer 24B on the bonding surface 22. The configuration of each layer of the first metallization layer 24B is similar to that of the first metallization layer 24 described with reference to FIG. 2A. A low-melting-point alloy layer 36 is formed on the first metallization layer 24B.

[0047] The substrate 44B has a cavity 60B, a lens accommodating recess 62, and a second metallization layer 46B. The cavity 60B is cylindrical. The cavity 60B accommodates the optical element 12. The diameter of the cavity 60B is smaller than the inner diameter of the first metallization layer 24B of the transparent sealing member 14B. The lens accommodating recess 62 is a recess formed on the outer periphery of the cavity 60B and is shallower than the cavity 60B. The lens accommodating recess 62 is formed slightly larger than the outer diameter of the transparent sealing member 14B and accommodates the transparent sealing member 14B. The second metallization layer 46B is formed on the bottom surface of the lens accommodating recess 62. The configuration of each layer of the second metallization layer 46B is similar to that of the second metallization layer 46 described with reference to FIG. 4A.

[0048] The transparent sealing member 14B is disposed so that the first metallized layer 24B faces the second metallized layer 46B in the lens accommodating recess 62. The first metallized layer 24B and the second metallized layer 46B are joined by the low-melting-point alloy layer 36 to form a joint 58.

[0049] In this modification, the thickness of the transparent sealing member 14B above the bonding portion 58 is defined as the thickness D of the transparent sealing member 14B above the center in the width direction of the first metallized layer 24B. In this modification, the thickness C of the first stress relaxation layer 30 is preferably set to be 0.28% or more of the thickness D of the transparent sealing member 14B.

[0050] This modification also makes it possible to prevent cracks and peeling of the transparent sealing member 14B.

[0051] (Third Modification of First Embodiment) As shown in Fig. 8A, optical component 10C of this modification differs from optical component 10 shown in Fig. 4B in that it includes a flat transparent sealing member 14C. In the configuration of optical component 10C, components similar to those of optical component 10 in Fig. 4B are designated by the same reference numerals, and detailed descriptions thereof will be omitted.

[0052] The transparent sealing member 14C has a lens 18 formed in a flat plate shape. The lens 18 is integrated with the base portion 40. The transparent sealing member 14C is formed in a rectangular shape with the same dimensions as the substrate 44 in a plan view. The transparent sealing member 14C has a cavity 20C and a first metallization layer 24. The cavity 20C is formed in a rectangular shape in a plan view. The cavity 20C accommodates the optical element 12 mounted on the substrate 44. The first metallization layer 24 is formed in a rectangular ring shape surrounding the outside of the cavity 20C. The first metallization layer 24 is formed on the bonding surface 22 of the transparent sealing member 14C and is bonded to the second metallization layer 46 of the substrate 44 via a low-melting-point alloy layer 36.

[0053] The configuration of each of the first metallized layer 24 and the second metallized layer 46 is similar to that of the first metallized layer 24 and the second metallized layer 46 of the first embodiment. This modification also makes it possible to prevent cracking and peeling of the transparent sealing member 14C.

[0054] (Fourth Modification of the First Embodiment) As shown in Fig. 8B, an optical component 10D of this modification differs from the optical component 10 shown in Fig. 4B in that it includes a flat transparent sealing member 14D. In the configuration of optical component 10D, components similar to those of optical component 10 in Fig. 4B are designated by the same reference numerals, and detailed descriptions thereof will be omitted.

[0055] The transparent sealing member 14D is formed in a flat plate shape and is rectangular in plan view with the same dimensions as the substrate 44D. No cavity 20 is formed in the transparent sealing member 14D, but a cavity 60D is formed in the substrate 44D. The cavity 60D in the substrate 44D is rectangular in plan view, and the substrate 44D is box-shaped. The optical element 12 is mounted in the cavity 60D in the substrate 44D.

[0056] The transparent sealing member 14D is made of a flat ultraviolet-transmitting glass plate, a flat quartz glass plate, or the like. The transparent sealing member 14D has a first metallization layer 24 formed in a rectangular ring shape so as to surround the cavity 60D of the substrate 44D. The first metallization layer 24 is bonded to the second metallization layer 46 of the substrate 44D via a low-melting-point alloy layer 36.

[0057] This modification also makes it possible to prevent cracks and peeling of the transparent sealing member 14D.

[0058] (Second embodiment) As shown in Figure 9A, the optical component 10E of this embodiment has a second stress relaxation layer 52 on the second metallization layer 46E of the substrate 44, and the first stress relaxation layer 30 is not provided on the first metallization layer 24E of the transparent sealing member 14.

[0059] In this embodiment, the transparent sealing member 14 has a first metallized layer 24E formed on the bonding surface 22. The first metallized layer 24E has a structure in which a first adhesion layer 26, a first diffusion prevention layer 28, and a second adhesion layer 34 are laminated in this order on the bonding surface 22. The first adhesion layer 26 is made of a Ti film or Cr film having a thickness of 0.01 to 0.5 μm. The first diffusion prevention layer 28 is made of a Pd film, Pt film, or Ni film having a thickness of 0.01 to 0.5 μm. The second adhesion layer 34 is made of an Au film having a thickness of 0.1 to 2 μm. The low-melting-point alloy layer 36 is made of an AuSn alloy film having a thickness of 20 μm.

[0060] The substrate 44 has an optical element 12 mounted on its upper surface 44a. A ring-shaped second metallization layer 46E is formed on the upper surface 44a of the substrate 44, surrounding the optical element 12. The second metallization layer 46E has a structure in which a third adhesion layer 48, a third diffusion prevention layer 50, a second stress relief layer 52, a fourth diffusion prevention layer 54, and a fourth adhesion layer 56 are formed in this order on the upper surface 44a of the substrate 44. The third adhesion layer 48 is made of a Ti film (or a Cr film) having a thickness of 0.01 to 0.5 μm. The third diffusion prevention layer 50 is made of a Pd film (or a Ni film or a Pt film) having a thickness of 0.01 to 0.5 μm. The third adhesion layer 48 and the third diffusion prevention layer 50 are formed, for example, by sputtering. The second stress relief layer 52 is made of a metal (for example, Cu) film having a Young's modulus of 150 GPa or less. The second stress relief layer 52 is formed to a thickness of 1.2 μm or more. The thickness of the second stress relief layer 52 may be the same as the thickness of the first stress relief layer 30 described in the first embodiment.

[0061] The fourth diffusion prevention layer 54 is made of a Ni film (or a Pd or Pt film) having a thickness of 0.1 to 5 μm. The fourth adhesion layer 56 is made of an Au film having a thickness of 0.1 to 2 μm. The second stress relief layer 52, the fourth diffusion prevention layer 54, and the fourth adhesion layer 56 are formed by plating.

[0062] In optical component 10E, transparent sealing member 14 is bonded to substrate 44 via first metallized layer 24E, second metallized layer 46E, and low-melting-point alloy layer 36. In optical component 10E, second stress relief layer 52 provided on second metallized layer 46E can relieve thermal stress at bonding portion 58, preventing cracking and peeling of transparent sealing member 14.

[0063] Third Embodiment As shown in FIG. 9B , an optical component 10F of this embodiment has a first metallized layer 24 formed on the bonding surface 22 of the transparent sealing member 14. The optical component 10F also has a second metallized layer 46E on the substrate 44. The first stress relief layer 30 is formed on the first metallized layer 24 (see FIG. 2A ). The second stress relief layer 52 is formed on the second metallized layer 46E (see FIG. 9A ). Thus, the optical component 10F has the first stress relief layer 30 and the second stress relief layer 52 at the bonding portion 58. The other configuration of the first metallized layer 24 is similar to that of the first metallized layer 24 of the first embodiment described with reference to FIG. 2A . The other configuration of the second metallized layer 46E is similar to that of the second metallized layer 46E described with reference to FIG. 9A .

[0064] Although not particularly limited, in this embodiment, the low-melting-point alloy layer 36 is formed on the second metallized layer 46E. The configuration of the low-melting-point alloy layer 36 is similar to that of the low-melting-point alloy layer 36 described with reference to Figures 3A and 3B.

[0065] In the optical component 10F of this embodiment, the sum of the thicknesses of the first stress relaxation layer 30 and the second stress relaxation layer 52 may be 1.2 μm or more. In the optical component 10F of this embodiment, the first stress relaxation layer 30 and the second stress relaxation layer 52 can relax the thermal stress at the bonding portion 58, thereby preventing cracking and peeling of the transparent sealing member 14.

[0066] (Embodiments and Comparative Examples) The following describes the results of fabricating and evaluating the optical components 10, 10A to 10F of the above-described embodiments. The fabricated optical components 10, 10A to 10F were subjected to dimensional measurements of each part using a measuring microscope and a scanning electron microscope (SEM). Cross-section processing was performed on the optical component 10 as necessary. The materials and compositions were measured using an EDS attached to the scanning electron microscope (SEM). The thermal expansion coefficient and Young's modulus were values ​​in the bulk state. The peeling rate of the transparent sealing member 14 was evaluated by conducting a thermal shock test. This thermal shock test was performed by mounting the optical component 10 on an aluminum heat dissipation substrate, subjecting it to a thermal cycle of -40°C to +85°C, and observing for the presence or absence of peeling visually or with an optical microscope.

[0067] (Examples 1 to 5 and Comparative Examples 1 and 2) In Examples 1 to 5 and Comparative Examples 1 and 2, optical components 10 and 10E of the same dimensions were fabricated and evaluated. The dimensions and configuration of each part are shown in FIGS. 10 and 11 . Comparative Example 1 is a case where the first stress relaxation layer 30 is not formed, and the thickness of the first stress relaxation layer 30 is 0 μm. In Comparative Example 2 and Examples 1 to 4, the thickness of the first stress relaxation layer 30 varies from 0.5 μm to 9.2 μm. Example 5 is the optical component 10E shown in FIG. 9A , but is similar to Examples 1 to 4 except for the bonding portion 58. In Example 5, a first stress relaxation layer 30 with a thickness of 1.2 μm and a second stress relaxation layer 52 made of Cu with a thickness of 8.3 μm are provided.

[0068] 12 , in Comparative Example 1, in which the first stress relaxation layer 30 and the second stress relaxation layer 52 were not provided, the peeling incidence rate of the transparent sealing member 14 was 32%. The peeling incidence rate of the transparent sealing member 14 tended to decrease as the thickness of the first stress relaxation layer 30 or the second stress relaxation layer 52 (hereinafter collectively referred to as the stress relaxation layer) increased. In particular, it can be seen that the peeling incidence rate of the transparent sealing member 14 increases sharply when the thickness of the stress relaxation layer is less than 1.2 μm. Therefore, it was confirmed that the peeling incidence rate of the transparent sealing member 14 can be suppressed to 6% or less when the thickness of the stress relaxation layer is 1.2 μm or more.

[0069] Examples 6, 8, 11, and 13 are evaluation results for the optical component 10 shown in FIGS. 5A and 5B . Similar to Example 1, Examples 6, 8, 11, and 13 have a first stress relaxation layer 30 with a thickness of 3.0 μm ( FIGS. 13 and 15 ). Example 6 differs from Example 1 in that, as shown in FIG. 13 , the thickness D of the base portion 40 of the transparent sealing member 14 is increased to 0.5 mm. As shown in FIG. 14 , Example 6 exhibited a peeling incidence rate of 2%, which was an improvement over the peeling incidence rates of Comparative Examples 1 and 2.

[0070] As shown in FIG. 13 , Example 8 differs from Example 1 in that the dimensions of the transparent sealing member 14 are increased. In Example 8, the outer dimension B of the first metallized layer 24 (bonding portion 58) is 3.9 mm. As the dimensions of the transparent sealing member 14 increase, the dimensional difference with the thermally expanded substrate 44 increases. However, as shown in FIG. 14 , the peeling incidence rate of the transparent sealing member 14 in Example 8 was only slightly increased to 4%. The peeling incidence rate in Example 8 was improved over the peeling incidence rates in Comparative Examples 1 and 2.

[0071] As shown in FIG. 16 , Example 11 differs from Example 1 in that alumina is used for the substrate 44. The thermal expansion coefficient of alumina is 7 ppm / K, which is greater than the thermal expansion coefficient of aluminum nitride used in Example 1, 4.6 ppm / K. Therefore, the bonded portion 58 is more susceptible to stress due to thermal expansion. In Example 11, the peeling incidence rate was kept to 6%, which was an improvement over the peeling incidence rates of Comparative Examples 1 and 2.

[0072] In Example 13, alumina was used for the substrate 44, as in Example 11. Example 13 differs from Example 11 in that Au, which has a smaller Young's modulus than Cu, was used as the material for the first stress relaxation layer 30, as shown in Fig. 15. As shown in Fig. 16, Example 13 had a peeling occurrence rate of 0%, which was an improvement over Example 11.

[0073] Example 7 Example 7 shown in Figure 13 shows test and evaluation results for the optical component 10A shown in Figures 6A and 6B. In Example 7, as shown in Figure 6B, the transparent sealing member 14A does not have a cavity 20, making the transparent sealing member 14A less likely to deform. Therefore, in Example 7, it is difficult to achieve the effect of alleviating thermal stress due to deformation of the transparent sealing member 14A. As shown in Figure 14, in Example 7, the peeling incidence rate was limited to 4% due to the effect of the first stress relaxation layer 30, which was an improvement over the peeling incidence rates of Comparative Examples 1 and 2.

[0074] Examples 9 and 10 shown in Figure 13 are test and evaluation results for the optical component 10C shown in Figure 8A. As shown in Figure 14, in Example 9, aluminum nitride with a thermal expansion coefficient of 4.6 ppm / K was used for the substrate 44, and in Example 10, silicon with a thermal expansion coefficient of 2.6 ppm / K was used for the substrate 44. In Example 9, the peeling occurrence rate was 6%. On the other hand, in Example 10, where the difference in the thermal expansion coefficient between the substrate 44 and the transparent sealing member 14 was small, the peeling occurrence rate was 0%. In Examples 9 and 10 above, the peeling occurrence rate was also improved compared to Comparative Examples 1 and 2.

[0075] Example 12 shown in Figure 15 is the test and evaluation results for optical component 10B shown in Figures 7A and 7B. Optical component 10B does not have pedestal 40. As shown in Figure 16, Example 12 had a peeling occurrence rate of 0%, which is lower than Comparative Examples 1 and 2.

[0076] Examples 14 and 15 shown in Figure 15 are test and evaluation results for the optical component 10D shown in Figure 8B. In Example 14, quartz glass was used for the transparent sealing member 14, and aluminum nitride was used for the substrate 44. In Example 15, ultraviolet-transmitting glass (borosilicate glass) was used for the transparent sealing member 14, and alumina was used for the substrate 44. In Example 14, the peeling occurrence rate was 4%, and in Example 15, the peeling occurrence rate was 0%. Therefore, Examples 14 and 15 can reduce the peeling occurrence rate more than Comparative Examples 1 and 2.

[0077] 10, 10A to 10F... Optical component 12... Optical element 14, 14A to 14D... Transparent sealing member 15... Transparent portion 16... Array member 18... Lens 20, 20C, 60, 60B, 60D... Cavity 22... Bonding surface 24, 24B, 24E... First metallized layer 28, 32, 50, 54... Diffusion prevention layer 30, 52... Stress relaxation layer

Claims

1. An optical component comprising: a substrate carrying an optical element; a transparent sealing member disposed above said substrate and sealing said optical element; and a joint formed by laminating a plurality of metal films and joining said transparent sealing member to said substrate, said joint having: one or more stress relaxation layers formed of metal films having a Young's modulus of 150 GPa or less and having a total thickness of 1.2 μm or more; and diffusion prevention layers disposed on both sides of said stress relaxation layers in the thickness direction for preventing diffusion of metal constituting said stress relaxation layers.

2. An optical component according to claim 1, wherein the stress relaxation layer is made of any one of Cu (copper), Au (gold), Ag (silver) and Zn (zinc).

3. An optical component according to claim 2, wherein the diffusion prevention layer is made of any one of Ni (nickel), Pd (palladium), and Pt (platinum).

4. An optical component according to claim 1, wherein the stress relaxation layer has a thermal expansion coefficient of 40 ppm / K or less.

5. An optical component according to claim 1, wherein the total thickness of said stress relaxation layers is 10 μm or less.

6. An optical component according to claim 1, wherein the total thickness of said stress relaxation layers is 0.28% or more of the thickness of said transparent sealing member above said stress relaxation layers.

7. An optical component according to claim 1, wherein the thickness of said transparent sealing member above said stress relaxation layer is 0.2 mm or more.

8. An optical component according to claim 1, wherein the total thickness of said stress relieving layers is 0.25% or more of the thickness of said substrate below said stress relieving layers.

9. An optical component as described in claim 1, wherein the total thickness of the stress relaxation layer is 0.05% or more of the sum of the thickness of the transparent sealing member above the stress relaxation layer and the thickness of the substrate below the stress relaxation layer.

10. An optical component according to any one of claims 1 to 9, wherein the difference between the thermal expansion coefficient of the transparent sealing member and the thermal expansion coefficient of the substrate is A (ppm / K) and the outer dimension of the joint is B (mm), and the value of A x B is 5 x 10 -6mm / K or more.

11. An optical component according to claim 10, wherein the outer dimension of the joint is 3 mm or more.

12. An optical component according to any one of claims 1 to 9, wherein the transparent sealing member is made of quartz glass or ultraviolet-transmitting glass.

13. An optical component according to claim 12, wherein the transparent sealing member has a thermal expansion coefficient of 1 ppm / K or less.

14. An optical component according to any one of claims 1 to 9, wherein the substrate is made of any one of aluminum nitride, alumina, silicon, kovar, and silicon nitride.

15. An optical component according to claim 14, wherein the substrate has a thermal expansion coefficient of 2.5 ppm / K or more.

16. An optical component according to claim 14, wherein the thickness of the substrate below the stress relieving layer is 0.2 mm or greater.

17. An optical component as claimed in any one of claims 1 to 9, wherein the bonding portion comprises: a first metallization layer formed on a bonding surface of the transparent sealing member facing the substrate and consisting of a plurality of metal films; a second metallization layer formed on the substrate and consisting of a plurality of metal films; and a low-melting point alloy layer bonding the first metallization layer and the second metallization layer, and the stress relaxation layer and the diffusion prevention layer are provided on at least one of the first metallization layer and the second metallization layer.

18. An optical component according to claim 17, wherein said stress relieving layer and said diffusion preventing layer are provided on both said first metallization layer and said second metallization layer, respectively.

19. A transparent sealing member that is bonded to a substrate carrying an optical element and seals the optical element, comprising: a lens covering the optical element; a bonding surface provided on the periphery of the lens and bonded to the substrate; and a first metallization layer formed on the bonding surface, wherein the first metallization layer has: a stress relaxation layer composed of a metal film having a Young's modulus of 150 GPa or less and a thickness of 1.2 μm or more; and diffusion prevention layers that are disposed on both sides of the stress relaxation layer in the thickness direction and prevent diffusion of the metal that constitutes the stress relaxation layer.

20. The transparent sealing member according to claim 19, further comprising a low melting point alloy layer formed on said first metallization layer.

21. A substrate for mounting an optical element, comprising: an upper surface located on the outer periphery of a portion for mounting the optical element, to which a transparent sealing member is bonded; and a second metallization layer formed on the upper surface, the second metallization layer having: a stress relaxation layer composed of a metal film having a Young's modulus of 150 GPa or less and having a thickness of 1.2 μm or more; and diffusion prevention layers disposed on both sides of the stress relaxation layer in the thickness direction for preventing diffusion of the metal constituting the stress relaxation layer.

22. A method for manufacturing an optical component in which an optical element mounted on a substrate is sealed with a transparent sealing member, comprising a step of joining a first metallization layer of the transparent sealing member and a second metallization layer of the substrate with a low melting point alloy, and comprising, on at least one of the first metallization layer and the second metallization layer, one or more stress relaxation layers each made of a metal film having a Young's modulus of 150 GPa or less and having a total thickness of 1.2 μm or more, and diffusion prevention layers disposed on both sides of the stress relaxation layer in the thickness direction to prevent diffusion of the metal constituting the stress relaxation layer.

Citation Information

Patent Citations

  • Support structures for light emitting diode packages

    US20220190208A1

  • Window material and optical package

    WO2020071452A1

  • Semiconductor light-emitting device, and water disinfection device

    WO2021251102A1