Thermoelectric conversion element and sensor
The thermoelectric conversion element addresses durability issues by optimizing surface roughness and internal stresses in the magnetic material, ensuring high performance and resistance to environmental stressors.
Patent Information
- Application Number
- PCT/JP2024/008894
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-31
- Filing Date
- 2024-03-07
- Publication Date
- 2024-10-03
AI Technical Summary
Conventional thermoelectric conversion elements face durability issues in high temperature and high humidity environments due to cracks in the alloy layer, which impair their thermoelectric conversion performance, and existing solutions do not adequately address these durability concerns.
A thermoelectric conversion element is designed with a base material where at least one surface has a maximum height roughness of 30 nm or less, and the thermoelectric converter is formed as a thin wire with internal stresses optimized to minimize cracking, using a magnetic material with large anisotropy for enhanced durability and performance.
The solution significantly enhances the durability and thermoelectric conversion performance of the element by reducing the likelihood of cracks, allowing it to maintain high efficiency even in harsh environments.
Smart Images

Figure JP2024008894_03102024_PF_FP_ABST
Abstract
Description
Thermoelectric conversion element and sensor
[0001] The present invention relates to a thermoelectric conversion element and a sensor.
[0002] 2. Description of the Related Art Conventionally, thermoelectric conversion elements have been known that have a structure in which a material exhibiting thermoelectric conversion properties is disposed on a substrate.
[0003] For example, Patent Document 1 describes a thermoelectric conversion element having a laminate including a substrate, a buffer layer, and two mixed layers. The substrate may be a flexible substrate. The buffer layer is provided on the substrate and has AlN with a predetermined crystal structure. The two mixed layers are provided on the buffer layer. The mixed layer has, from the side closest to the buffer layer, an alloy layer and a cap layer. The alloy layer has a predetermined magnetic material. The magnetic material includes a polycrystalline Co-based Heusler alloy. The Co-based Heusler alloy exhibits a large anomalous Nernst effect. The cap layer includes AlN. This laminate exhibits a large anomalous Nernst effect or anomalous Hall effect due to the alloy layer being sandwiched between layers including AlN, and has high thermoelectric conversion efficiency.
[0004] Japanese Patent Application Laid-Open No. 2022-129848
[0005] There is a growing need for heat monitoring in the Internet of Things (IoT) society, such as in health monitoring and thermal management in technical fields such as electric vehicle (EV) batteries and high-speed data processing chips. To meet these needs, a thermoelectric conversion element with a thermoelectric converter on a substrate can be used for heat sensing. It is considered important for such a thermoelectric conversion element to have high durability in the usage environment.
[0006] The durability of the thermoelectric conversion element described in Patent Document 1 in its usage environment is not specifically considered. The thermoelectric conversion element described in Patent Document 1 has a laminated structure of a substrate, a buffer layer, and two mixed layers. In the laminated structure, cracks may occur in specific layers depending on the usage environment. For example, if cracks occur in the alloy layer of the thermoelectric conversion element described in Patent Document 1, the desired thermoelectric conversion performance may be impaired. Patent Document 1 does not consider this point of view, and the thermoelectric conversion element described in Patent Document 1 has room for reexamination in terms of durability in its usage environment.
[0007] In view of the above circumstances, the present invention provides a thermoelectric conversion element that is advantageous in terms of durability in the usage environment.
[0008] The present invention provides a thermoelectric conversion element comprising: a substrate; and a thermoelectric conversion element disposed on a first surface of the substrate and having a second surface that intersects with a line perpendicular to the first surface, wherein at least one surface selected from the group consisting of the first surface and the second surface has a maximum height roughness Rz of 30 nm or less.
[0009] The present invention also provides a sensor including the above thermoelectric conversion element.
[0010] The above thermoelectric conversion element is advantageous in terms of durability in the environment in which it is used.
[0011] FIG. 1 is a perspective view showing an example of an embodiment of a thermoelectric conversion element. FIG. 2 is a cross-sectional view of the thermoelectric conversion element, cut along plane II shown in FIG. 1. FIG. 3 is a graph showing the relationship between magnetization and an external magnetic field of a thermoelectric conversion body according to an embodiment. FIG. 4 is a side view showing an example of a thermoelectric conversion element having a wound structure. FIG. 5 is a diagram showing an example of an embodiment of a sensor. FIG. 6 is a perspective view showing another example of an embodiment of a thermoelectric conversion element. FIG. 7 is a diagram schematically showing a method for measuring the internal stress of a thermoelectric conversion body.
[0012] Hereinafter, embodiments of the present invention will be described with reference to the drawings. Note that the following description is for illustrative purposes only and is not intended to limit the scope of the present invention.
[0013] As shown in FIGS. 1 and 2 , the thermoelectric conversion element 1a includes a substrate 20 and a thermoelectric converter 11. The thermoelectric converter 11 is disposed on a first surface S1 of the substrate 20. The thermoelectric converter 11 has a second surface S2 that intersects with a perpendicular line P to the first surface S1. In the thermoelectric conversion element 1a, at least one surface selected from the group consisting of the first surface S1 and the second surface S2 has a maximum height roughness Rz of 30 nm or less. The maximum height roughness Rz is determined, for example, in accordance with Japanese Industrial Standards (JIS) B 0601:2013. The first surface S1 and the second surface S2 are, for example, surfaces parallel to the XY plane. In the accompanying drawings, the X-axis, Y-axis, and Z-axis are orthogonal to each other, and the Z-axis is perpendicular to the first surface S1.
[0014] According to the research of the present inventors, it is advantageous to adjust the internal stress in the thermoelectric converter to a predetermined state in order to improve the thermoelectric conversion performance of a thermoelectric conversion element having a thermoelectric converter disposed on a substrate. However, it has been newly discovered that adjusting the internal stress in the thermoelectric converter to a predetermined state may cause cracks in the thermoelectric converter due to the internal stress, depending on the usage environment, and may result in a decrease in the thermoelectric conversion performance of the thermoelectric conversion element. In particular, it has been found that cracks may occur in the thermoelectric converter when the thermoelectric conversion element is exposed to a high-temperature, high-humidity environment for a long period of time. It has been found that the occurrence of such cracks is related not only to the state of the internal stress in the thermoelectric converter but also to the state of the surface of the substrate in contact with the thermoelectric converter.
[0015] In the manufacture of a thermoelectric conversion element having a thermoelectric converter disposed on a substrate, a precursor of the thermoelectric converter may be deposited on the surface of the substrate while the substrate is being transported. For example, when transporting the substrate from a state in which the substrates are stacked on top of each other, a substrate having an uneven surface is used to prevent blocking caused by the stacking of the substrates. The inventors' investigations have revealed that the uneven surface of the substrate is involved in the generation of cracks in the thermoelectric converter when the thermoelectric conversion element is exposed to a high-temperature, high-humidity environment for a long period of time.
[0016] Therefore, after extensive trial and error, the inventors have newly discovered that cracks are less likely to occur in the thermoelectric converter by adjusting the maximum height roughness Rz of at least one surface selected from the group consisting of the surface of the substrate in contact with the thermoelectric converter and the surface of the thermoelectric converter within a predetermined range.
[0017] As described above, at least one surface selected from the group consisting of the first surface S1 and the second surface S2 has a maximum height roughness Rz of 30 nm or less. This makes it difficult for cracks to occur in the thermoelectric conversion element, even when the thermoelectric conversion element is exposed to a high-temperature, high-humidity environment for a long period of time. Therefore, the thermoelectric conversion element 1a is likely to have high durability in the usage environment. The maximum height roughness Rz may be 25 nm or less, 20 nm or less, or 15 nm or less, or may be, for example, 1 nm or more.
[0018] As shown in FIG. 2 , the substrate 20 has, for example, a third surface S3. The third surface S3 extends parallel to the first surface S1 and away from the thermoelectric converter 11. The surface state of the third surface S3 is not limited to a specific state. The third surface S3 has, for example, an arithmetic mean roughness Ra of 8 nm or more. With this configuration, when the substrate 20 is transported in the manufacture of the thermoelectric conversion element 1a, blocking due to overlapping of the substrates 20 is unlikely to occur, making it easy to transport the substrate 20. The arithmetic mean roughness Ra is determined, for example, in accordance with JIS B 0601:2013.
[0019] The arithmetic mean roughness Ra of the third surface S3 may be 9 nm or more, or 10 nm or more. The arithmetic mean roughness Ra of the third surface S3 may be, for example, 20 nm or less, 15 nm or less, or 12 nm or less. The arithmetic mean roughness Ra of the third surface S3 may be included in any of the ranges defined by all combinations of a lower limit of 8 nm, 9 nm, or 10 nm and an upper limit of 20 nm, 15 nm, or 12 nm.
[0020] Minimum internal stress σ in the thermoelectric converter 11 min is not limited to a specific value. The minimum internal stress σ min is the minimum value of the internal stress of the thermoelectric converter 11 in a plane parallel to the first surface S1.min is, for example, -300 MPa or less. In this case, the thermoelectric conversion performance of the thermoelectric conversion element 1a is likely to be improved. In this specification, a positive internal stress indicates tensile stress, and a negative internal stress indicates compressive stress. The minimum internal stress σ min is -300 MPa or less indicates that a relatively large compressive stress exists as an internal stress in the thermoelectric converter 11. When the thermoelectric conversion element is exposed to a high-temperature and high-humidity environment for a long period of time, such compressive stress, in combination with the surface irregularities of the substrate, is likely to cause cracks in the thermoelectric converter. However, when the maximum height roughness Rz of at least one surface selected from the group consisting of the first surface S1 and the second surface S2 is 30 nm or less, the minimum internal stress σ min Even if the applied pressure is −300 MPa or less, cracks are unlikely to occur in the thermoelectric conversion body 11. Therefore, the thermoelectric conversion element 1a is likely to have high durability in the usage environment.
[0021] Minimum internal stress σ min is, for example, -900 MPa or more. min may be included in any of the ranges determined by all combinations of an upper limit value of any one of −300 MPa, −350 MPa, −400 MPa, −450 MPa, −500 MPa, −550 MPa, and −600 MPa and a lower limit value of any one of −900 MPa, −850 MPa, −800 MPa, −750 MPa, and −700 MPa.
[0022] The thermoelectric converter 11 is, for example, a thin wire 11a containing a magnetic material. With this configuration, for example, the thermoelectric conversion element 1a is likely to exhibit desired thermoelectric conversion performance due to the thermoelectric conversion characteristics of the magnetic material. The thermoelectric converter 11 includes, for example, a plurality of thin wires 11a.
[0023] As shown in FIG. 1 , the thin wires 11a extend, for example, along the Y-axis direction. The thickness of the thin wires 11a, which is the dimension in the Z-axis direction, is not limited to a specific value. The thickness is, for example, 1000 nm or less. This allows the amount of material used for the thin wires 11a to be reduced, making it easier to reduce the manufacturing cost of the thermoelectric conversion element 1a. In addition, breaks are less likely to occur in the thermoelectric converter 11. The thickness of the thin wires 11a is, for example, 5 nm or more. This makes it easier for the thermoelectric conversion element 1a to exhibit high durability.
[0024] The thickness of the thin wire 11a may be included in any of the ranges determined by all combinations of a lower limit value of any one of 5 nm, 10 nm, 20 nm, 30 nm, and 50 nm and an upper limit value of any one of 1000 nm, 750 nm, 500 nm, 400 nm, 300 nm, and 200 nm.
[0025] The width of the thin wires 11a, which is the dimension in the X-axis direction, is not limited to a specific value. The width of the thin wires 11a is, for example, 500 μm or less. This reduces the amount of material used for the thin wires 11a, making it easier to reduce the manufacturing cost of the thermoelectric conversion element 1a. In addition, it is easy to arrange a large number of thin wires 11a in the X-axis direction, making it easier for the thermoelectric conversion element 1a to exhibit the desired thermoelectric conversion performance. The width of the thin wires 11a is, for example, 1 μm or more. This makes it less likely for breakage to occur in the thin wires 11a, making it easier for the thermoelectric conversion element 1a to have high durability.
[0026] The width of the thin wire 11a may be included in any of the ranges determined by all combinations of a lower limit value of any one of 1 μm, 2 μm, 5 μm, 10 μm, 20 μm, and 30 μm and an upper limit value of any one of 500 μm, 400 μm, 300 μm, 200 μm, 100 μm, and 50 μm.
[0027] First internal stress σ of the thermoelectric converter 11 Y and the second internal stress σ X Difference from σ X -σ Y | is not limited to a specific value. Y is the internal stress of the thermoelectric converter 11 in the length direction (Y-axis direction) of the thin wire 11a. Xis the internal stress of the thermoelectric converter 11 in the width direction (X-axis direction) of the thin wire 11a. X -σ Y is, for example, 50 MPa or more. In this case, the magnetic properties of the magnetic material contained in the thin wire 11a tend to have large anisotropy in the length direction and width direction, and the thermoelectric conversion body 11 tends to have desired thermoelectric conversion properties. Therefore, the thermoelectric conversion element 1a tends to exhibit desired thermoelectric conversion performance.
[0028] As described above, the thin wire 11a extends linearly in the Y-axis direction. Therefore, when considering the shape magnetic anisotropy, it seems that in the thermoelectric converter 11, an axis of easy magnetization occurs in the length direction of the thin wire 11a, and an axis of hard magnetization occurs in the width direction of the thin wire 11a. However, in the thermoelectric converter 11, the difference |σ X -σ Y When | is 50 MPa or more, the magnetic properties of the magnetic material contained in the thin wire 11a tend to have large anisotropy in the length direction and width direction. For example, the magnetic anisotropy energy E u Is E u In this relationship, λ is the magnetostriction constant of the magnetic material, and σ indicates the internal stress of the magnetic material. Therefore, for example, when the magnetostriction constant λ is a positive value, the difference σ X -σ Y The larger the positive value of σ, or when the magnetostriction constant λ is negative, the larger the difference σ X -σ Y It can be seen that the smaller the negative value of σ, the greater the anisotropy of the magnetic properties of the magnetic material in the length direction and width direction of the thin wire 11a.
[0029] 3 is a graph showing the relationship between the magnetization of the thermoelectric converter 11 and an external magnetic field. In FIG. 3, the solid line graph shows the relationship between the magnetization of the thermoelectric converter 11 in the width direction (X-axis direction) of the thin wire 11a and the external magnetic field. The dashed line graph shows the relationship between the magnetization of the thermoelectric converter 11 in the length direction (Y-axis direction) of the thin wire 11a and the external magnetic field. As shown in FIG. 3, in the thermoelectric converter 11, the difference |σ X -σ YWhen | is 50 MPa or more, the magnetic properties of the thermoelectric converter 11 have large anisotropy in the length direction and width direction of the thin wire 11a. Due to such large anisotropy of the magnetic properties, in the thermoelectric converter 11, a hard axis of magnetization is likely to occur in the length direction of the thin wire 11a, and an easy axis of magnetization is likely to occur in the width direction of the thin wire 11a. This makes it easy for the thermoelectric converter 11 to exhibit stable behavior against an external magnetic field, and for the thermoelectric conversion element 1a to exhibit the desired thermoelectric conversion performance. The magnetic material contained in the thin wire 11a preferably has an easy axis of magnetization in the width direction of the thin wire 11a.
[0030] In the thermoelectric converter 11, the difference |σ X -σ Y may be 100 MPa or more, 150 MPa or more, or 200 MPa or more. X -σ Y The upper limit of | is not limited to a specific value. X -σ Y is, for example, 900 MPa or less. In this case, cracks are unlikely to occur in the thermoelectric converter 11 even if a bending load in the width direction is applied to both ends of the thin wire 11a.
[0031] First internal stress σ Y The first internal stress σ may be a tensile stress or a compressive stress. Y may be included in any of the ranges determined by all combinations of a lower limit value that is any one of −900 MPa, −700 MPa, −500 MPa, and −300 MPa and an upper limit value that is any one of 900 MPa, 700 MPa, 500 MPa, and 300 MPa.
[0032] Second internal stress σ X The second internal stress σ may be a tensile stress or a compressive stress. X may be included in any of the ranges determined by all combinations of a lower limit value that is any one of −900 MPa, −700 MPa, −500 MPa, and −300 MPa and an upper limit value that is any one of 900 MPa, 700 MPa, 500 MPa, and 300 MPa.
[0033] The magnetostriction constant of the magnetic material contained in the thin wire 11a may be either a positive value or a negative value. For example, when the magnetostriction constant of this magnetic material is a positive value, σ X -σ Y ≥ 50 MPa is satisfied, and the magnetostriction constant of the magnetic material is a negative value, σ Y -σ X In the former case, the first internal stress σ Y is the minimum internal stress σ min In the latter case, the second internal stress σ X is the minimum internal stress σ min may be.
[0034] The squareness ratio determined by the M-H curve in the width direction of the thin wire 11a of the thermoelectric converter 11 is not limited to a specific value. The squareness ratio is the ratio Mr / Ms of the remanent magnetization Mr to the saturation magnetization Ms in the M-H curve. The squareness ratio is, for example, 80% or more. This makes it easier for the thermoelectric conversion element 1a to exhibit the desired thermoelectric conversion performance. The squareness ratio may be 85% or more, or may be 90% or more.
[0035] The thermoelectric converter 11 generates an electromotive force in the length direction (Y-axis direction) of the thin wires 11a due to, for example, a temperature gradient ∇T in a direction (Z-axis direction) perpendicular to the first surface S1. With this configuration, the electromotive force generated by thermoelectric conversion can be adjusted by adjusting the length of the thin wires 11a, and the thermoelectric conversion element 1a can be used for various purposes.
[0036] The thermoelectric converter 11 generates an electromotive force by, for example, the magneto-thermoelectric effect, which may be, for example, the anomalous Nernst effect.
[0037] The thermoelectric converter 11 contains, for example, a substance that exhibits the anomalous Nernst effect. The substance that exhibits the anomalous Nernst effect is not limited to a specific substance. The substance that exhibits the anomalous Nernst effect may be, for example, 5×10 -3The thermoelectric converter 11 is a magnetic material having a saturation magnetic susceptibility of 0.1 T or more, or a material having a band structure with a Weyl point near the Fermi energy. The magnetic material may be a ferrimagnetic material. The thermoelectric converter 11 contains, as a material exhibiting the anomalous Nernst effect, at least one material selected from the group consisting of the following (i), (ii), (iii), (iv), and (v): (i) a stoichiometric material having a composition represented by Fe3X; (ii) an off-stoichiometric material in which the composition ratio of Fe to X deviates from that of the material (i) above; (iii) a material in which part of the Fe sites of the material (i) above or part of the Fe sites of the material (ii) above is substituted with a main group metal element or transition element other than X; (iv) Fe3M1 1-x M2 x (v) A substance having a composition expressed by (0<x<1), in which M1 and M2 are different typical group elements. (i) A substance in which a part of the Fe site of the substance (i) is substituted with a transition element other than X, and a part of the X site of the substance (i) is substituted with a typical metal element other than X.
[0038] In the above substances (i) to (v), X is a typical element or a transition element. X is, for example, Al, Ga, Ge, Sn, Si, Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W, Sc, Ni, Mn, or Co. In the above substance (iv), the combination of M1 and M2 is not limited to a specific combination as long as M1 and M2 are different typical elements. In the above substance (iv), the combination of M1 and M2 is, for example, Ga and Al, Si and Al, or Ga and B.
[0039] The thermoelectric converter 11 may contain Co2MnGa or Mn3Sn as a substance that exhibits the anomalous Nernst effect.
[0040] The magnetostriction constant λ of the magnetic material contained in the thin wire 11a is not limited to a specific value. The absolute value of the magnetostriction constant λ is, for example, 5×10 -6 As described above, the magnetic anisotropy energy E u Is E u =(3 / 2)λσ. Therefore, the absolute value of the magnetostriction constant λ is 5×10 -6If this is the case, the anisotropy of the magnetic properties in the length direction and width direction of the thin wire 11a tends to become large.
[0041] The absolute value of the magnetostriction constant λ is 10×10 -6 It may be 20×10 or more. -6 It may be more than that.
[0042] As shown in FIG. 1 , the thermoelectric conversion element 1a has a meander pattern including thermoelectric conversion bodies 11. With this configuration, the total length of the fine wires 11a included in the thermoelectric conversion element 1a tends to be large. The electromotive force generated in the length direction of the fine wires 11a due to the temperature gradient ∇T in the direction perpendicular to the first surface S1 tends to be large as the total length of the fine wires 11a increases. Therefore, when the thermoelectric conversion element 1a has a meander pattern including the thermoelectric conversion bodies 11, the electromotive force generated in the thermoelectric conversion element 1a tends to be large.
[0043] 1 and 2, the thermoelectric conversion element 1a further includes, for example, wiring 12. The wiring 12 electrically connects the thin wires 11a to each other. For example, the wiring 12 electrically connects the plurality of thin wires 11a in the thermoelectric conversion body 11 in series. The wiring 12 includes, for example, a plurality of wirings 12a. The plurality of thin wires 11a and the plurality of wirings 12a are electrically connected in series. With this configuration, a large electromotive force is likely to be generated in the thermoelectric conversion element 1a even if the area of the surface on which the plurality of thin wires 11a and the plurality of wirings 12a are arranged is small.
[0044] The wiring 12 may be made of a single metal or an alloy.
[0045] The plurality of fine wires 11a and the plurality of wirings 12a are arranged, for example, to form the meander pattern described above, thereby forming a conductive path 15. For example, by connecting one end 15p and the other end 15q of the conductive path 15 to external wiring, the electromotive force generated in the thermoelectric conversion element 1a can be extracted to the outside. Alternatively, by applying a voltage between the one end 15p and the other end 15q, a heat flow can be generated in the thickness direction of the substrate 20.
[0046] The multiple thin wires 11a are, for example, spaced apart at a predetermined interval in the X-axis direction and arranged parallel to one another. The multiple thin wires 11a are, for example, arranged at equal intervals in the X-axis direction. The multiple wirings 12a electrically connect, for example, the thin wires 11a that are adjacent to one another in the X-axis direction. The wirings 12a electrically connect, for example, one end of a thin wire 11a in the Y-axis direction to the other end in the Y-axis direction of another thin wire 11a adjacent to that thin wire 11a. One end of each of the multiple thin wires 11a in the Y-axis direction is located on the same side of the thin wire 11a in the Y-axis direction, and the other end of each of the multiple thin wires 11a in the Y-axis direction is located on the opposite side of the one end of the thin wire 11a in the Y-axis direction.
[0047] The thickness of the wiring 12 a in the Z-axis direction is not limited to a specific value and may be within any range defined by any combination of a lower limit of 5 nm, 10 nm, 20 nm, 30 nm, and 50 nm and an upper limit of 1000 nm, 750 nm, 500 nm, 400 nm, 300 nm, and 200 nm.
[0048] The width of the wiring 12a is not limited to a specific value and may be included in any of the ranges determined by all combinations of a lower limit of 0.1 μm, 0.5 μm, 1 μm, 2 μm, 5 μm, 10 μm, 20 μm, and 30 μm and an upper limit of 500 μm, 400 μm, 300 μm, 200 μm, 100 μm, and 50 μm.
[0049] The substrate 20 is not limited to a specific substrate as long as at least one selected from the group consisting of the first surface S1 and the second surface S2 has a maximum height roughness Rz of 30 nm or less.
[0050] The base material 20 contains, for example, an organic material. With this configuration, it is easy to adjust the internal stress in the thermoelectric converter 11 to a desired state from the viewpoint of thermoelectric conversion performance. In addition, it is easy to reduce the manufacturing cost of the thermoelectric conversion element 1 a.
[0051] The substrate 20 includes, for example, an organic polymer as the organic material, such as polyethylene terephthalate (PET), polyethylene naphthalate (PEN), acrylic resin (PMMA), polycarbonate (PC), polyimide (PI), or cycloolefin polymer (COP).
[0052] The thickness of the substrate 20 is not limited to a particular value, and is, for example, 10 to 250 μm.
[0053] The substrate 20 has, for example, flexibility. The substrate 20 has elasticity that allows the strip-shaped test specimen made from the substrate 20 to be elastically deformed when the test specimen is wound around a cylindrical mandrel having a diameter of 10 cm so that both ends in the length direction face the same direction.
[0054] Second dimensional change rate C of the substrate 20 X and the first dimensional change rate C Y Difference with |C X -C Y is not limited to a specific value. Y is a value obtained by dividing the dimension at 25°C after a test in which the substrate 20 is heated at 150°C for 30 minutes in the length direction (Y-axis direction) of the thin wire 11a along the first surface S1 by the dimension at 25°C before the test. X is the value obtained by dividing the dimension of the thin wire 11a in the width direction (X-axis direction) at 25°C after the above test by the dimension at 25°C before the test. X -C Y is, for example, 0.10% or more. In this case, for example, by performing a predetermined heat treatment on the precursor of the thermoelectric converter 11 formed on the first surface S1 of the substrate 20, the degree of shrinkage of the substrate 20 after the heat treatment differs in the length direction and width direction of the thin wires 11a. This makes it easy to adjust the internal stress in the thermoelectric converter 11 to a desired state from the viewpoint of thermoelectric conversion performance.
[0055] Difference | C X -C Y may be 0.2% or more, 0.3% or more, 0.4% or more, or 0.5% or more, for example, 10% or less.
[0056] The first surface S1 of the substrate 20 may be formed by a surface layer such as a hard coat layer, for example.
[0057] An example of a method for manufacturing the thermoelectric conversion element 1a is shown below. The thermoelectric conversion element 1a is manufactured, for example, by a method including the following steps (I) and (II): (I) forming a precursor of the thermoelectric conversion element 11 on the first surface S1 of the substrate 20; (II) heat-treating the substrate 20 and the precursor of the thermoelectric conversion element 11 at a predetermined temperature.
[0058] In (I), a film of a precursor of the thermoelectric converter 11 is formed on the first surface S1 of the substrate 20 by, for example, sputtering, chemical vapor deposition (CVD), pulsed laser deposition (PLD), ion plating, plating, or the like. Next, for example, a photoresist is applied to the film, a photomask is placed on the film, exposure is performed, and then wet etching is performed. This results in the formation of a plurality of thin wires of the precursor of the thermoelectric converter 11 arranged at a predetermined interval. Next, a film of a precursor of the wiring 12 is formed on the first surface S1 of the substrate 20 by, for example, sputtering, CVD, PLD, ion plating, plating, or the like. Next, a photoresist is applied to the film of the precursor of the wiring 12, a photomask is placed on the film of the precursor of the wiring 12, exposure is performed, and then wet etching is performed. This results in the formation of the wiring 12, and the thin wires of the precursor of the thermoelectric converter 11 are electrically connected to each other.
[0059] The temperature of the heat treatment in (II) is not limited to a specific temperature. The ambient temperature of the substrate 20 and the precursor of the thermoelectric converter 11 during the heat treatment is, for example, 50°C or higher. This makes it easy to adjust the internal stress of the thermoelectric converter 11 to a desired state from the perspective of thermoelectric conversion performance. The ambient temperature of the substrate 20 and the precursor of the thermoelectric converter 11 during the heat treatment may be 100°C or higher, 150°C or higher, or 200°C or higher. The ambient temperature is, for example, 300°C or lower.
[0060] The time during which the ambient temperature of the substrate 20 is maintained at 50° C. or higher in the heat treatment is not limited to a specific value, and is, for example, 10 minutes or more and 3 hours or less.
[0061] After the heat treatment, the precursor of the thermoelectric converter 11 is magnetized to obtain the thermoelectric converter 11. For example, a thermoelectric conversion element 1a is manufactured in this manner.
[0062] The thermoelectric conversion element 1 a may be provided together with, for example, an adhesive layer. In this case, the base material 20 is disposed between the thermoelectric converter 11 and the adhesive layer in the thickness direction of the base material 20. This allows the thermoelectric conversion element 1 a to be attached to an article by pressing the adhesive layer against the article.
[0063] The adhesive layer contains, for example, a rubber-based adhesive, an acrylic-based adhesive, a silicone-based adhesive, or a urethane-based adhesive. The thermoelectric conversion element 1a may be provided together with an adhesive layer and a release liner. In this case, the release liner covers the adhesive layer. The release liner is typically a film that can maintain the adhesive force of the adhesive layer when covering the adhesive layer and can be easily peeled off from the adhesive layer. The release liner is, for example, a film made of a polyester resin such as PET. By peeling off the release liner, the adhesive layer is exposed, allowing the thermoelectric conversion element 100 to be attached to an article.
[0064] 4, the thermoelectric conversion element 1a may be provided in a state in which it forms, for example, a wound structure 5. For example, the wound structure 5 is obtained by winding the film- or sheet-shaped thermoelectric conversion element 1a around the side surface of a cylindrical or columnar core 4.
[0065] As shown in Figure 5, for example, a sensor 3 including a thermoelectric conversion element 1a can be provided. In this sensor 3, for example, when a temperature gradient ∇T occurs in the thickness direction of the substrate 20, an electromotive force is generated in the length direction of the thin wire 11a. The sensor 3 can sense heat by processing an electrical signal output to the outside of the thermoelectric conversion element 1a based on this electromotive force. The sensor 3 further includes, for example, a signal processing device 2. The electrical signal output to the outside of the thermoelectric conversion element 1a is processed in the signal processing device 2.
[0066] The thermoelectric conversion element 1a can be modified from various viewpoints. The thermoelectric conversion element 1a may be modified, for example, to a thermoelectric conversion element 1b shown in FIG. 6. The thermoelectric conversion element 1b has the same configuration as the thermoelectric conversion element 1a, except for portions that will be particularly described. The components of the thermoelectric conversion element 1b that are the same as or correspond to the components of the thermoelectric conversion element 1a are given the same reference numerals, and detailed description thereof will be omitted. The description of the thermoelectric conversion element 1a also applies to the thermoelectric conversion element 1b, unless technically inconsistent.
[0067] 6 , in the thermoelectric conversion element 1b, the thermoelectric conversion body 11 extends continuously on the first surface S1, for example. The wiring 12 is disposed on a part of the thermoelectric conversion body 11. For example, the wiring 12 includes a plurality of wirings 12a disposed on the thermoelectric conversion body 11 at predetermined intervals.
[0068] In the thermoelectric conversion element 1b, the thermoelectric conversion body 11 has, for example, a meander pattern. The thermoelectric conversion element 1b is configured such that, in a plan view, single layers of the thermoelectric conversion body 11 and stacked bodies including the thermoelectric conversion body 11 and the wiring 12a appear alternately in the X-axis direction.
[0069] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to the following examples.
[0070] Example 1: A 96-nm-thick thin film was formed on a 54-μm-thick polyethylene terephthalate (PET) film A by DC magnetron sputtering using a target material containing Fe and Ga on the hard coat layer of the film A, which had a 4 μm-thick hard coat layer as a surface layer and a total thickness of 54 μm. In the DC magnetron sputtering, argon gas was supplied as the process gas at a pressure of 0.1 Pa. The target material satisfied a 3:1 atomic ratio of Fe content to Ga content. The ambient temperature of the PET film A was adjusted to 100°C. The PET film A on which the thin film was formed was heat-treated in a 150°C environment for 30 minutes. Next, a photoresist was applied to the thin film, and a photomask was placed on the thin film to perform exposure, followed by wet etching. This resulted in the formation of 115 FeGa-containing thin wires arranged at predetermined intervals. Each FeGa-containing thin wire had a width of 40 μm and a length of 1.5 cm. Then, a Cu thin film having a thickness of 100 nm was formed on the hard coat layer of PET film A by DC magnetron sputtering using a Cu-containing target material. A photoresist was applied to the Cu thin film, and a photomask was placed on the Cu thin film to perform exposure, followed by wet etching. This resulted in the formation of Cu-containing thin wires having a width of 40 μm. The Cu-containing thin wires electrically connected a pair of adjacent FeGa-containing linear patterns, forming a conductive path with a meander pattern.
[0071] Using an electromagnet with a central magnetic flux density of 0.5 T, the FeGa-containing thin wire was magnetized in a width direction parallel to the main surface of the PET film A and perpendicular to the length direction of the FeGa-containing thin wire. In this way, a thermoelectric conversion element according to Example 1 was produced. In this thermoelectric conversion element, the perpendicular direction (TD) of the PET film A coincided with the width direction of the FeGa-containing thin wire.
[0072] Comparative Example 1 A thermoelectric conversion element according to Comparative Example 1 was produced in the same manner as in Example 1, except that PET film B having a total thickness of 50 μm and no hard coat layer was used instead of PET film A.
[0073] <Comparative Example 2> A thermoelectric conversion element according to Comparative Example 1 was produced in the same manner as in Example 1, except for the following points: PET film B used in Comparative Example 1 was used instead of PET film A. The pressure of argon gas supplied as a process gas in DC magnetron sputtering was adjusted to 1.6 Pa.
[0074] Comparative Example 3 A thermoelectric conversion element according to Comparative Example 3 was produced in the same manner as in Example 1, except that a PET film C different from the PET film used in Example 1 and Comparative Example 1 was used.
[0075] [Magnetic Properties] The magnetic properties of the FeGa-containing thin wires of the thermoelectric conversion elements according to each Example and Comparative Example were measured using a Qantum Design compact cryogen-free physical property measurement system, PPMS-versalab. Measurement samples were prepared by cutting out 2 mm squares from the conductive path-arranged portions of the modules according to each Example and Comparative Example. Additionally, a Vibration Sample Magnetrometer (VSM) was used to sweep a magnetic field of ±800 kA / m parallel to the magnetization direction of the magnetized FeGa-containing thin wire. M-H curves were obtained at a temperature of 300 K, taking into account the thickness of the FeGa-containing thin wire and the area of the FeGa-containing thin wire in the measurement sample. The squareness ratio, Mr / Ms, was determined as the ratio of the magnetization Ms value at ±800 kA / m to the magnetization Mr value at 0 kA / m during the magnetic field sweep. The results are shown in Table 1.
[0076] [Measurement of Internal Stress] Using an X-ray diffractometer Smartlab manufactured by Rigaku Corporation, Cu-Kα rays were irradiated onto the sample from a light source of 40 kV and 50 mA through a parallel beam optical system. 2 The first internal stress σ of the FeGa-containing thin wire in each example and each comparative example was calculated based on the principle of the tilt measurement method of the Ψ method. Y and second internal stress σ X The first internal stress σ Y is the internal stress in the length direction of the FeGa-containing thin wire, and the second internal stress σ Xwas the internal stress in the width direction, which was parallel to the main surface of the PET film and perpendicular to the length direction of the FeGa-containing thin wire. The wavelength λ of the Cu-Kα ray was 0.1541 nm. 2 The Ψ method is a technique for determining the internal stress of a polycrystalline thin film from the dependence of the crystal lattice distortion of the thin film on the angle (Ψ). Using the X-ray diffraction device described above, the diffraction intensity was measured at 0.01° intervals in the range of 2θ = 75° to 85° by Θ / 2Θ scan measurement. The integration time at each measurement point was set to 100 seconds. The crystal lattice spacing d of the magnetic material at each measurement angle (Ψ) was calculated from the peak angle 2θ of the obtained X-ray diffraction and the wavelength λ of the X-rays emitted from the light source. The crystal lattice distortion ε was calculated from the crystal lattice spacing d using the relationships in the following formulas (1) and (2). λ is the wavelength of the X-rays (Cu-Kα rays) emitted from the light source, and λ = 0.1541 nm. d0 is the lattice spacing of a crystal in a stress-free state, and d0 = 0.0206 nm. 2d sin θ = λ Equation (1) ε = (d - d0) / d0 Equation (2)
[0077] As shown in Fig. 7, the above-mentioned X-ray diffraction measurement was performed in each case where the angle (Ψ) between the normal to the main surface of the sample Sa and the normal to the crystal plane of the crystal Mb was 0°, 17°, 24°, 30°, 35°, 40°, and 45°, and the crystal lattice strain ε at each angle (Ψ) was calculated. Y and second internal stress σ X sin 2 The relationship between Ψ and the crystal lattice strain ε was plotted and the slope of the line was calculated using the following formula (3). The results are shown in Table 1. Note that in Table 1, positive values for the internal stress indicate tensile stress, and negative values indicate compressive stress. In the side tilt method, stress is measured in a direction at 90° to the beam direction, so the first internal stress σ Y and second internal stress σ X When determining ε, the sample was placed so that the direction of measurement was perpendicular to the beam direction, and the measurement was performed. The results are shown in Table 1. ε = {(1 + ν) / E}σ sin 2 Ψ-(2ν / E)σ Equation (3)
[0078] In the above formula (3), E is the Young's modulus of the magnetic material (130 GPa), and v is the Poisson's ratio of the magnetic material (0.3). Detector D in Fig. 7 detects X-ray diffraction.
[0079] [Surface Roughness Measurement] Using a Zygo NewView 7300 three-dimensional non-contact surface roughness measuring instrument, the surface of each PET film on which the FeGa-containing fine wires were formed and the surface of the FeGa fine wires were measured under conditions of a 10x objective lens and a measurement area of 0.70 mm x 0.52 mm, and a roughness curve for each surface was obtained. From the obtained roughness curves, the arithmetic mean roughness R and maximum height roughness Rz were calculated in accordance with JIS B0601:2013. The results are shown in Table 1.
[0080] [Dimensional Change Rate of Substrate] A heating test was conducted in which test pieces made from the substrates used in each Example and Comparative Example were heated at 150°C for 30 minutes. The value obtained by dividing the dimension at 25°C after the heating test in the longitudinal direction of the FeGa-containing thin wire by the dimension at 25°C before the heating test was the first dimensional change rate C Y The value obtained by dividing the dimension at 25°C after the heating test in the width direction of the FeGa-containing thin wire by the dimension at 25°C before the heating test was determined as the second dimensional change rate C X In addition, the second dimensional change rate C X and the first dimensional change rate C Y Difference with |C X -C Y The results are shown in Table 1.
[0081] [High-Temperature, High-Humidity Environmental Test] The thermoelectric conversion elements according to each Example and Comparative Example were subjected to a high-temperature, high-humidity environmental test by maintaining the environment at a temperature of 85°C and a relative humidity of 85% for 120 hours. The electrical resistance R of the conductive path before the high-temperature, high-humidity environmental test and the electrical resistance R of the conductive path after 24 hours had elapsed since the start of the high-temperature, high-humidity environmental test were measured. 24 , the electrical resistance R of the conductive path after the high temperature and high humidity environment test 120 The electrical resistance R 24 or electrical resistance R 120 The results are shown in Table 1.
[0082] As shown in Table 1, in Example 1, no breaks were observed in the conductive path even after 120 hours of high-temperature, high-humidity environmental testing. On the other hand, in each of the comparative examples, breaks were observed in the conductive path after 120 hours of high-temperature, high-humidity environmental testing. A comparison between Example 1 and each of the comparative examples suggests that high durability can be exhibited over a long period of time in high-temperature, high-humidity environmental testing when the maximum height roughness Rz of the surface on which the FeGa-containing thin wires of each PET film are formed or the surface of the FeGa thin wires is 30 nm or less.
[0083] By comparing Example 1 and Comparative Example 2, the difference |σ X -σ Y It is understood that when | is large, the squareness ratio tends to be high, and the FeGa thin wire tends to have desired magnetic properties from the viewpoint of thermoelectric conversion performance.
[0084] In Comparative Example 1, no breaks in the conductive path were observed 24 hours after the start of the high-temperature, high-humidity environmental test. On the other hand, in Comparative Example 2, breaks in the conductive path were observed 24 hours after the start of the high-temperature, high-humidity environmental test. In Comparative Example 2, a relatively large tensile internal stress was generated in the FeGa-containing thin wire, and cracks were generated in the FeGa-containing thin wire due to the combined effect of the tensile stress generated by the expansion of the PET film caused by exposure to the high-temperature, high-humidity environment. On the other hand, in Comparative Example 1, a compressive internal stress was generated in the FeGa-containing thin wire, and the FeGa-containing thin wire withstood the tensile stress generated by the expansion of the PET film caused by exposure to the high-temperature, high-humidity environment, so no cracks were generated in the FeGa-containing thin wire. On the other hand, when the PET film was exposed to the high-temperature, high-humidity environment for 120 hours, the vicinity of the interface between the FeGa-containing thin wire and the PET film deteriorated, reducing their adhesion, and it is thought that buckling occurred due to the compressive stress in the FeGa-containing thin wire, causing cracks in the FeGa-containing thin wire. The propagation direction of the cracks that occurred in the FeGa-containing thin wire in the high-temperature, high-humidity environmental test of Comparative Example 1 was different from the propagation direction of the cracks that occurred in the FeGa-containing thin wire in the high-temperature, high-humidity environmental test of Comparative Example 2. This suggests that the crack generation mechanisms are different between Comparative Examples 1 and 2, as described above.
[0085] In Comparative Example 3, disconnection of the conductive path was confirmed 24 hours after the start of the high-temperature, high-humidity environmental test. A comparison between Example 1 and Comparative Example 3 shows that high durability is exhibited over a long period of time in the high-temperature, high-humidity environmental test, and therefore the difference in the PET film substrate |C X -C Y It is understood that it is desirable that | is 0.1% or more.
[0086]
[0087] A first aspect of the present invention provides a thermoelectric conversion element comprising: a substrate; and a thermoelectric conversion element disposed on a first surface of the substrate and having a second surface that intersects with a line perpendicular to the first surface, wherein at least one surface selected from the group consisting of the first surface and the second surface has a maximum height roughness Rz of 30 nm or less.
[0088] A second aspect of the present disclosure provides the thermoelectric conversion element according to the first aspect, wherein the substrate has a third surface extending parallel to the first surface and away from the thermoelectric conversion body, and the third surface has an arithmetic mean roughness Ra of 8 nm or more.
[0089] A third aspect of the present disclosure provides a thermoelectric conversion element according to the first or second aspect, wherein the thermoelectric conversion body has a minimum internal stress of −300 MPa or less, and the minimum internal stress is a minimum value of the internal stress of the thermoelectric conversion body in a plane parallel to the first surface.
[0090] A fourth aspect of the present disclosure provides the thermoelectric conversion element according to any one of the first to third aspects, in which the thermoelectric conversion body is a thin wire containing a magnetic material.
[0091] A fifth aspect of the present disclosure provides a thermoelectric conversion element according to the fourth aspect, wherein a difference between a first internal stress of the thermoelectric conversion body in a length direction of the thin wire and a second internal stress of the thermoelectric conversion body in a width direction perpendicular to the length direction and parallel to the first surface is 50 MPa or more.
[0092] A sixth aspect of the present disclosure provides a thermoelectric conversion element according to the fourth or fifth aspect, wherein the thermoelectric conversion body generates an electromotive force in a length direction of the thin wire due to a temperature gradient in a direction perpendicular to the first surface.
[0093] A seventh aspect of the present disclosure provides the thermoelectric conversion element according to any one of the first to sixth aspects, in which the substrate includes an organic material.
[0094] An eighth aspect of the present disclosure provides the thermoelectric conversion element according to any one of the first to seventh aspects, wherein the thermoelectric conversion element has a meander pattern including the thermoelectric conversion body.
[0095] A ninth aspect of the present disclosure provides the thermoelectric conversion element according to any one of the first to eighth aspects, wherein the thermoelectric conversion element has a wound structure.
[0096] A tenth aspect of the present disclosure provides a sensor including the thermoelectric conversion element according to any one of the first to ninth aspects.
Claims
1. A thermoelectric conversion element comprising: a substrate; and a thermoelectric conversion body having a second surface disposed on a first surface of the substrate and intersecting a perpendicular line to the first surface, wherein at least one surface selected from the group consisting of the first surface and the second surface has a maximum height roughness Rz of 30 nm or less.
2. The thermoelectric conversion element according to claim 1, wherein the base material has a third surface extending parallel to the first surface and away from the thermoelectric conversion body, and the third surface has an arithmetic mean roughness Ra of 8 nm or more.
3. The thermoelectric conversion element according to claim 1, wherein the thermoelectric conversion body has a minimum internal stress of -300 MPa or less, and the minimum internal stress is the minimum value of the internal stress of the thermoelectric conversion body within a plane parallel to the first surface.
4. The thermoelectric conversion element according to claim 1, wherein the thermoelectric conversion body is a thin wire containing a magnetic material.
5. The thermoelectric conversion element according to claim 4, wherein a difference between a first internal stress of the thermoelectric conversion body in the length direction of the thin wire and a second internal stress of the thermoelectric conversion body in a width direction perpendicular to the length direction and parallel to the first surface is 50 MPa or more.
6. The thermoelectric conversion element according to claim 4, wherein the thermoelectric conversion body generates an electromotive force in the longitudinal direction of the thin wire due to a temperature gradient in a direction perpendicular to the first surface.
7. The thermoelectric conversion element according to claim 1, wherein the substrate comprises an organic material.
8. The thermoelectric conversion element according to claim 1, wherein the thermoelectric conversion element has a meander pattern including the thermoelectric conversion body.
9. The thermoelectric conversion element according to claim 1, wherein the thermoelectric conversion element has a wound structure.
10. A sensor comprising a thermoelectric conversion element according to any one of claims 1 to 9.
Citation Information
Patent Citations
Magnetic material, laminate, and manufacturing method of laminate, thermoelectric conversion element, and magnetic sensor
JP2022129848A
Thermoelectric conversion devices
WO2023276956A1
Thermoelectric body, method for producing thermoelectric body, thermoelectric device, and method for producing thermoelectric device
WO2023277028A1