BAW resonator and electronic apparatus

The BAW resonator design addresses the issue of diagonal resonance and noise in conventional BAW resonators by using a resonator region defining layer to cover the piezoelectric layer's end, ensuring perpendicular orientation and reducing noise, thus enhancing piezoelectric performance for high-frequency applications.

WO2024203308A1PCT designated stage expired Publication Date: 2024-10-03NITTO DENKO CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/009661
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2024-03-12
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Conventional BAW resonators suffer from resonance occurring diagonally in the piezoelectric layer, leading to transverse waves and noise due to misalignment and edge exposure during manufacturing, which deteriorates film quality and prevents proper electrical conductivity between electrodes.

Method used

A BAW resonator design featuring a support substrate, an acoustic mirror layer, a first electrode, a piezoelectric layer, a second electrode, and a resonator region defining metal layer, where the first electrode extends outward and the resonator region defining layer covers the end of the piezoelectric layer, suppressing transverse wave generation by ensuring perpendicular orientation of the piezoelectric layer's end surface.

Benefits of technology

This design effectively reduces noise generation and maintains excellent piezoelectric properties by preventing transverse waves and ensuring stable electrical conductivity, suitable for high-frequency applications like filters and other electronic components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024009661_03102024_PF_FP_ABST
    Figure JP2024009661_03102024_PF_FP_ABST
Patent Text Reader

Abstract

A BAW resonator according to the present invention is provided by laminating a support substrate, an acoustic mirror layer disposed on the support substrate, a first electrode, a piezoelectric layer, and a second electrode. A resonator region defining layer separated from the second electrode and comprising a metal layer is provided on the surface, of the piezoelectric layer, on the side thereof that contacts the second electrode. The first electrode extends farther to the outside than the piezoelectric layer. The resonator region defining layer is provided on a portion of the first-electrode-side surface of the piezoelectric layer, on an end surface of the piezoelectric layer, and on an exposed portion of the first electrode.
Need to check novelty before this filing date? Find Prior Art

Description

BAW resonator and electronic device

[0001] The present invention relates to a BAW resonator and an electronic device.

[0002] A bulk acoustic wave (BAW) resonator has a piezoelectric layer made of a piezoelectric material between two electrode layers. Utilizing the piezoelectric effect of the piezoelectric layer, BAW resonators are used in electronic devices as electronic components such as pressure sensors, acceleration sensors, and acoustic emission (AE) sensors that detect elastic waves, as well as high-frequency filters, piezoelectric actuators, and radio frequency (RF) filters.

[0003] As a BAW resonator, for example, a BAW resonator has been disclosed that includes a lower electrode layer including a lower electrode, a piezoelectric layer, and an upper electrode layer, with the piezoelectric layer and the upper electrode layer stacked on top of the lower electrode layer (see, for example, Patent Document 1).

[0004] U.S. Patent No. 9,602,076

[0005] However, in the BAW resonator of Patent Document 1, the piezoelectric layer is laminated between the lower electrode layer and the upper electrode layer with the end faces of the piezoelectric layer exposed, so that resonance occurring in the piezoelectric layer tends to occur in an oblique direction rather than in a direction perpendicular to the thickness. The oblique resonance becomes a transverse wave, which causes a problem of becoming a noise component in the BAW resonator.

[0006] In conventional BAW resonators such as the BAW resonator of Patent Document 1, processing errors such as misalignment during exposure during manufacturing, and deterioration of the film quality near the end of the piezoelectric layer due to the end of the piezoelectric layer being immersed in a chemical solution during etching, are likely to occur. Therefore, in conventional BAW resonators, the piezoelectric layer is generally formed so that its end is exposed from the upper electrode so that no current flows between the lower electrode and the upper electrode.

[0007] An object of one aspect of the present invention is to provide a BAW resonator capable of suppressing the generation of transverse waves from a piezoelectric layer.

[0008] One aspect of the BAW resonator according to the present invention is a BAW resonator comprising a support substrate, an acoustic mirror layer arranged on the support substrate, a first electrode, a piezoelectric layer, and a second electrode stacked together, wherein the piezoelectric layer has a resonator region defining layer made of a metal layer spaced apart from the second electrode on the surface of the piezoelectric layer that contacts the second electrode, the first electrode extending outward beyond the piezoelectric layer, and the resonator region defining layer is provided on a portion of the surface of the piezoelectric layer facing the first electrode, on an end face of the piezoelectric layer, and on an exposed portion of the first electrode.

[0009] One aspect of the BAW resonator according to the present invention can suppress the generation of transverse waves from the piezoelectric layer.

[0010] Fig. 1 is a schematic cross-sectional view showing a configuration of a BAW resonator according to an embodiment of the present invention;Fig. 2 is a schematic cross-sectional view showing an example of another configuration of a BAW resonator;Fig. 3 is a schematic cross-sectional view showing an example of another configuration of a BAW resonator;Fig. 4 is a schematic cross-sectional view showing an example of another configuration of a BAW resonator;Fig.

[0011] Hereinafter, embodiments of the present invention will be described in detail. To facilitate understanding of the description, the same components in each drawing are denoted by the same reference numerals, and duplicate descriptions will be omitted. The scale of each component in the drawings may differ from the actual scale. In this specification, unless otherwise specified, the symbol "to" indicating a range of values ​​means that the values ​​before and after it are included as the lower and upper limits.

[0012] <BAW Resonator> Fig. 1 is a schematic cross-sectional view showing the configuration of a BAW resonator according to this embodiment. As shown in Fig. 1, the BAW resonator 1A includes a support substrate 10, an acoustic mirror layer 20, a first electrode 30, a piezoelectric layer 40, a second electrode 50, and a resonator area defining layer 60. The BAW resonator 1A includes the support substrate 10, the acoustic mirror layer 20, the first electrode 30, the piezoelectric layer 40, and the second electrode 50, stacked in this order from the support substrate 10 side. The BAW resonator 1A includes a portion of the top surface of the acoustic mirror layer 20, the first electrode 30, and a portion of the end of the piezoelectric layer 40, covered with the resonator area defining layer 60. The BAW resonator 1A may be formed in any shape, such as a sheet (film).

[0013] In this specification, a three-dimensional Cartesian coordinate system with three axes (X-axis, Y-axis, and Z-axis) is used, with the width direction of the BAW resonator 1A defined as the X-axis, the length direction defined as the Y-axis, and the height (thickness) direction (vertical direction) defined as the Z-axis. The second electrode 50 side in the Z-axis direction is defined as the +Z-axis, and the supporting substrate 10 side is defined as the −Z-axis. In the following description, for convenience of explanation, the +Z-axis direction will be referred to as up or upward, and the −Z-axis direction will be referred to as down or downward, but this does not represent a universal up-down relationship.

[0014] The BAW resonator 1A has a resonator region defining layer 60 that covers a portion of the end of the piezoelectric layer 40 provided on the acoustic mirror layer 20, thereby preventing resonances occurring in the piezoelectric layer 40 from occurring in an oblique direction relative to the piezoelectric layer 40, thereby preventing transverse waves from being generated from the piezoelectric layer 40 and reducing noise generation.

[0015] [Supporting Base] As shown in FIG. 1, the supporting base 10 is a substrate on which a laminate of an acoustic mirror layer 20, a first electrode 30, a piezoelectric layer 40, a second electrode 50, and a resonator region defining layer 60 is placed, and may be flexible so as to impart flexibility to the BAW resonator 1A.

[0016] As the material for forming the support substrate 10, any material can be used, regardless of type, as long as it can stably support the laminate. For example, a plastic substrate, a metal foil, a metal plate, a silicon (Si) substrate, an inorganic dielectric substrate, a glass substrate, etc. may be used.

[0017] When a plastic substrate is used, it is preferable to use a flexible material that can impart flexibility to the BAW resonator 1A including the piezoelectric layer 40.

[0018] Examples of materials that can be used to form the plastic substrate include polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polycarbonate (PC), acrylic resins, cycloolefin polymers, polyamide (PA) resins, polyimide (PI) resins, polyphenylene sulfide (PPS), polytetrafluoroethylene (PTFE), and diallyl phthalate resin (PDAP).

[0019] The metal foil may be made of a metal such as Au, Pt, Ag, Ti, Al, Mo, Ru, or Cu.

[0020] The metal plate may be made of a material such as aluminum, copper, stainless steel, or tantalum.

[0021] Examples of materials that may be used to form the inorganic dielectric substrate include MgO and sapphire.

[0022] The thickness of the support substrate 10 is not particularly limited and may be appropriately determined depending on the application of the BAW resonator 1A, the material of the support substrate 10, etc., and may be, for example, 20 μm to 725 μm. If the thickness of the support substrate 10 is 20 μm to 725 μm, it can stably support the laminate including the laminate of the acoustic mirror layer 20, the first electrode 30, the piezoelectric layer 40, and the second electrode 50. Furthermore, warping of the support substrate 10 is suppressed, and the influence of warping of the support substrate 10 on the piezoelectric characteristics can be reduced, allowing the BAW resonator 1A to have the desired flexibility.

[0023] In this specification, the thickness of the support substrate 10 refers to the length in the direction perpendicular to the main surface of the support substrate 10. The method for measuring the thickness of the support substrate 10 is not particularly limited, and any measurement method can be used. The thickness of the support substrate 10 may be, for example, the thickness measured at an arbitrary location on the cross section of the support substrate 10, or may be the average value of the measured values ​​measured at several arbitrary locations. Hereinafter, the definition of thickness is similarly defined for other members.

[0024] [Acoustic Mirror Layer] As shown in Fig. 1 , the acoustic mirror layer 20 is provided on the upper main surface (top surface) 101 of the support substrate 10. The acoustic mirror layer 20 may be composed of acoustic multilayer films with different specific acoustic impedances. The acoustic mirror layer 20 is a multilayer film in which two or more pairs of high acoustic impedance layers having a predetermined specific acoustic impedance and low acoustic impedance layers having a lower specific acoustic impedance than the high acoustic impedance layers are alternately stacked.

[0025] When resonant vibrations are transmitted to the acoustic mirror layer 20, the vibration energy of the resonance is reflected by the acoustic mirror layer 20. The speed at which vibration waves (elastic waves) propagate through high acoustic impedance layers is different from the speed at which they propagate through low acoustic impedance layers. By designing the thickness of the acoustic mirror layer 20 so that the reflected waves reinforce each other due to interference at the interfaces of the layers that make up the acoustic mirror layer 20, the vibration energy of the resonance is returned in the direction of incidence of the elastic waves without being affected by the support substrate 10, while the thermal energy is released in the direction of the support substrate 10.

[0026] The high acoustic impedance layer is made of W, Mo, or Ta. 2 O 5 The low acoustic impedance layer is formed of a material having a high density or bulk modulus, such as ZnO, etc. The low acoustic impedance layer is formed of a material having a lower density or bulk modulus than the high acoustic impedance layer.

[0027] The low acoustic impedance layer is made of SiO 2 The low acoustic impedance layer may be formed of a material with a low density or a low deposition modulus of elasticity, such as a silicon dioxide film. The low acoustic impedance layer may be an amorphous layer or a layer in which the amorphous phase is predominant. By forming the low acoustic impedance layer as a layer in which the amorphous phase is predominant, stress in the high acoustic impedance layer can be alleviated.

[0028] The high acoustic impedance layer and the low acoustic impedance layer may be formed on the support substrate 10 by sputtering or the like.

[0029] [First Electrode] As shown in Fig. 1 , the first electrode 30 is provided on the upper principal surface (top surface) 201 of the acoustic mirror layer 20. The first electrode 30 may be formed as a thin film on a part of or the entire top surface 201 of the acoustic mirror layer 20. The first electrode 30 is provided so as to extend outward beyond the piezoelectric layer 40. Note that "extending the first electrode 30 outward beyond the piezoelectric layer 40" refers to a state in which the first electrode 30 is also disposed outside the piezoelectric layer 40 in a plan view seen from the stacking direction of the first electrode 30.

[0030] Any conductive material can be used for the first electrode 30. Examples of such a material include metals such as Pt, Au, Ag, Cu, Mg, Al, Si, Ti, Cr, Fe, Ni, Zn, Rb, Zr, Nb, Mo, Rh, Pd, Ru, Sn, Ir, Ta, and W.

[0031] The first electrode 30 may be an amorphous film from the viewpoint of suppressing unevenness and grain boundaries at the interface between the first electrode 30 and the piezoelectric layer 40. By using an amorphous film, it is possible to suppress unevenness on the surface of the first electrode 30 and the generation of grain boundaries that cause leak paths.

[0032] The thickness of the first electrode 30 can be appropriately designed and may be, for example, 40 nm to 300 nm. If the thickness of the first electrode 30 is 40 nm to 300 nm, the first electrode 30 can exhibit its function as an electrode and the BAW resonator 1A can be made thinner.

[0033] 1, the piezoelectric layer 40 is provided on the main surface (top surface) 301 above the first electrode 30. The end surface of the piezoelectric layer 40 may be provided substantially perpendicular to the top surface 301 of the first electrode 30. In other words, the angle formed between the end surface 402 of the piezoelectric layer 40 and a plane parallel to the top surface 301 of the first electrode 30 may be approximately 90°.

[0034] The piezoelectric layer 40 preferably contains an inorganic material as a main component, where the content of the inorganic material is 95 atm % or more, preferably 98 atm % or more, and more preferably 99 atm % or more.

[0035] As the inorganic material, a piezoelectric material having a perovskite crystal structure (perovskite crystal material), a piezoelectric material having a wurtzite crystal structure (wurtzite crystal material), or the like can be used.

[0036] The wurtzite crystal structure is represented by the general formula AB, where A is an electropositive element and B is an electronegative element. Wurtzite crystal materials have a hexagonal unit cell with a polarization vector parallel to the c-axis.

[0037] As the wurtzite crystal material, it is preferable to use a material that exhibits piezoelectric properties above a certain value and can be crystallized in a low-temperature process at 200°C or less. The wurtzite crystal material contains Zn, Al, Ga, Cd, Si, etc. as the electropositive element A represented by the general formula AB. Examples of wurtzite crystal materials that can be used include zinc oxide (ZnO), zinc sulfide (ZnS), zinc selenide (ZnSe), zinc telluride (ZnTe), aluminum nitride (AlN), gallium nitride (GaN), cadmium selenide (CdSe), cadmium telluride (CdTe), and silicon carbide (SiC). Among these, ZnO is preferred as the wurtzite crystal material because it is relatively easy to achieve good c-axis orientation even in a low-temperature process. These materials may be used alone or in combination of two or more. When two or more wurtzite crystal materials are used in combination, one or more of these may be contained as the main component and other components may be contained as optional components. In addition, each material may be laminated, or multiple targets may be used to form a single layer.

[0038] The wurtzite crystal material preferably contains ZnO, more preferably consists essentially of ZnO, and even more preferably consists only of ZnO. "Substantially" means that the wurtzite crystal material may contain, in addition to ZnO, inevitable impurities that may be inevitably contained during the manufacturing process.

[0039] Inorganic materials such as wurtzite crystal materials may contain, in addition to the above-mentioned ZnO, AlN, ZnS, ZnSe, and ZnTe, alkaline earth metals such as Mg, Ca, and Sr, or metals such as V, Ti, Zr, Si, Sr, and Li, in a predetermined range of proportions. These components may be contained in the elemental state or in the oxide state. Among these, Mg-doped ZnO (MgZnO), in which ZnO is doped with Mg, is preferred as the inorganic material because it achieves both a K value, which is an index of the piezoelectric properties of the piezoelectric layer 40, and a Q value, which is an index of the steepness of the piezoelectric properties, and thereby exhibits excellent piezoelectric properties.

[0040] The K value is the value of the electromechanical coupling constant k. The square value (k 2The k value) indicates the energy conversion efficiency of the electrical energy determined for the piezoelectric material. The higher the energy conversion efficiency of the electrical energy, the better the operating efficiency of the BAW resonator 1A including the piezoelectric layer 40, and the BAW resonator 1A has excellent piezoelectric characteristics. For the same material and composition, the smaller the disorder in the crystal orientation of the piezoelectric material contained in the piezoelectric layer 40, the higher the k value of the piezoelectric material. 2 The value increases and then gradually becomes constant. That is, as the disorder of the crystal orientation of the piezoelectric material decreases, the energy conversion efficiency of the piezoelectric material increases and then gradually becomes constant, and the piezoelectricity becomes constant. Therefore, the larger the electromechanical coupling constant k, the 2 The larger the value, the higher the energy conversion efficiency of the piezoelectric material, which means that the piezoelectric properties are improved. Also, the larger the electromechanical coupling constant k, the smaller the disturbance in the crystal orientation, which means that the crystal orientation is improved.

[0041] The Q value is a value that represents the sharpness (sharpness) of frequency characteristics. The larger the Q value, the sharper the frequency characteristics.

[0042] The content of the additive element in the piezoelectric layer 40 is not particularly limited as long as it is within a range that allows the piezoelectric layer 40 to have a wurtzite crystal structure. The method for measuring the content of the additive element contained in the piezoelectric layer 40 is not particularly limited as long as it is a measurable method. The content of the additive element contained in the piezoelectric layer 40 may be measured by, for example, Rutherford backscattering spectroscopy (RBS) using a Pelletron 3SDH (manufactured by NEC Corporation) as a measuring device, or may be measured by secondary ion mass spectrometry using dynamic SIMS (D-SIMS) or the like.

[0043] The thickness of the piezoelectric layer 40 is not particularly limited, and may be any thickness that provides sufficient piezoelectric characteristics, i.e., polarization characteristics proportional to pressure, and that can stably exhibit piezoelectric characteristics by reducing the occurrence of cracks or the like in the piezoelectric layer 40. The thickness of the piezoelectric layer 40 may be, for example, 50 nm to 5 μm. If the thickness of the piezoelectric layer 40 is 50 nm to 5 μm, the occurrence of cracks is suppressed and sufficient piezoelectric characteristics can be exhibited.

[0044] The crystal orientation of the piezoelectric layer 40 is preferably 5° or less. If the crystal orientation is 5° or less, the crystal orientation in the c-axis direction (c-axis orientation) of the piezoelectric material contained in the piezoelectric layer 40 is good, and the energy conversion efficiency is improved, thereby improving the piezoelectric characteristics in the thickness direction of the piezoelectric layer 23. If the piezoelectric layer 40 contains ZnO as the piezoelectric material, ZnO has a wurtzite crystal structure, and there is a higher correlation between the crystal orientation and the piezoelectric characteristics than with piezoelectric materials having other crystal structures. If the crystal orientation of ZnO is 5° or less, it is easier to increase the energy conversion efficiency, thereby improving the piezoelectric characteristics of the BAW resonator 1A.

[0045] The crystalline orientation of the piezoelectric layer 40 can be evaluated by the full width at half maximum (FWHM) obtained when the surface of the piezoelectric layer 40 is measured by the X-ray rocking curve (XRC) method. That is, the crystalline orientation of the piezoelectric layer 40 is represented by the FWHM of the peak waveform of the rocking curve obtained when the diffraction from the (0002) plane of the crystal of the piezoelectric material contained as a main component in the piezoelectric layer 40 is measured by the XRC method. When the piezoelectric material contained in the piezoelectric layer 40 has a wurtzite crystal structure such as ZnO, the FWHM indicates the degree of parallelism of the crystals constituting the piezoelectric material in the c-axis direction. Therefore, the FWHM of the peak waveform of the rocking curve obtained by the XRC method can be used as an indicator of the c-axis orientation of the piezoelectric layer 40. Therefore, the smaller the FWHM of the rocking curve, the better the crystalline orientation of the piezoelectric layer 40 in the c-axis direction can be evaluated.

[0046] The crystal orientation of the piezoelectric layer 40 may be evaluated using the XRC method to measure diffraction from a specific crystal plane of the piezoelectric material (e.g., the (0002) plane of a ZnO crystal) in the piezoelectric layer 40, and may also be evaluated using the peak intensity as well as the FWHM of the rocking curve. That is, the crystal orientation of the piezoelectric layer 40 may be evaluated using the value obtained by dividing the integrated value of the peak intensity by the FWHM as an evaluation value. For example, the larger the evaluation value obtained by dividing the integrated value of the peak intensity by the FWHM, the better the crystal orientation of the piezoelectric layer 40 can be evaluated to be.

[0047] When two or more inorganic materials are used in combination, the piezoelectric layer 40 may be formed by laminating piezoelectric layers made of the respective inorganic materials.

[0048] 1 , the second electrode 50 is provided on the upper principal surface (top surface) 401 of the piezoelectric layer 40, and is disposed so as to face the first electrode 30. The second electrode 50 can be formed of any conductive material, and the same material as the first electrode 30 can be used.

[0049] Similar to the first electrode 30, the second electrode 50 may be formed as a thin film on a part of or the entire upper surface 401 of the piezoelectric layer 40, or may be formed in any appropriate shape.

[0050] The thickness of the second electrode 50 can be appropriately designed, and is preferably, for example, 40 nm to 300 nm. If the thickness of the second electrode 50 is within the above-mentioned preferred range, the function of the electrode can be exhibited and the BAW resonator 1A can be made thinner.

[0051] 1 , the resonator region defining layer 60 is provided so as to cover a portion of the upper surface 201 of the acoustic mirror layer 20, the first electrode 30, and a portion of the end portion 41 of the piezoelectric layer 40. The resonator region defining layer 60 is provided over the entire periphery of the acoustic mirror layer 20, the first electrode 30, and the piezoelectric layer 40. That is, the resonator region defining layer 60 is provided on the exposed portion 201 a of the upper surface 201 of the acoustic mirror layer 20, the exposed portion 301 a and the end face 302 of the upper surface 301 of the first electrode 30, and the exposed portion 401 a and the end face 402 of the upper surface 401 of the piezoelectric layer 40.

[0052] The upper surfaces of the acoustic mirror layer 20, the first electrode 30, and the piezoelectric layer 40 are the surfaces of these layers facing the second electrode 50, and are the main surfaces of these layers that come into contact with the layers stacked on top of them. For example, the upper surface 401 of the piezoelectric layer 40 is the main surface that comes into contact with the second electrode 50.

[0053] The lower surfaces of the acoustic mirror layer 20, the first electrode 30, and the piezoelectric layer 40 are the surfaces on which each of these layers is positioned facing the support substrate 10, and are the main surfaces on which each of these layers comes into contact with the layer on which it is placed.

[0054] The lower surfaces of the acoustic mirror layer 20, the first electrode 30, and the piezoelectric layer 40 are different from the upper and lower surfaces of these layers.

[0055] The upper and lower surfaces of the acoustic mirror layer 20, the first electrode 30, and the piezoelectric layer 40 may or may not have the same area. For example, when the upper surface has a smaller area than the lower surface, the end surface may have a forward tapered shape with an obtuse angle formed with the upper surface.

[0056] The resonator region defining layer 60 has the function of suppressing resonance occurring in the piezoelectric layer 40 from occurring in the thickness direction and oblique directions.

[0057] The material for forming the resonator region defining layer 60 may be any material that can have the same potential as the first electrode 30, and examples of materials that can be used for forming the resonator region defining layer 60 include Au, Ag, Al, and Cu. These may be used alone or in combination with two or more of these. Because the resonator region defining layer 60 also shares wiring, it is preferable that the material for forming the resonator region defining layer 60 be a metal with high conductivity, such as Au, Ag, Al, or Cu.

[0058] The resonator region defining layer 60 may be formed by a commonly used method such as vapor deposition or coating.

[0059] The thickness of the resonator region defining layer 60 should be sufficient to cover the end portions of the piezoelectric layer 40, and is preferably 50 nm or more, more preferably 100 nm or more, and even more preferably 200 nm or more. If the thickness of the resonator region defining layer 60 is 50 nm or more, resonance occurring in the piezoelectric layer 40 can be suppressed from occurring in a direction oblique to the thickness.

[0060] The thickness of the resonator region defining layer 60 may be the same or different from the upper surface 401 of the piezoelectric layer 40 to the acoustic mirror layer 20, but it is preferable that the thickness of the resonator region defining layer 60 located on the end surface 402 of the piezoelectric layer 40 is thicker than the thickness of the resonator region defining layer 60 provided on the upper surface 401 of the piezoelectric layer 40.

[0061] The method for manufacturing the BAW resonator 1A is not particularly limited, and any suitable manufacturing method can be used. An example of the method for manufacturing the BAW resonator 1A will be described.

[0062] First, high acoustic impedance layers and low acoustic impedance layers are stacked alternately on the upper surface of a support substrate 10 formed to a predetermined size, forming a pair of high acoustic impedance layers and low acoustic impedance layers, to form an acoustic mirror layer 20.

[0063] The method for forming the high acoustic impedance layer and the low acoustic impedance layer is not particularly limited, and may be either a dry process or a wet process. If a dry process is used as the method for forming the high acoustic impedance layer and the low acoustic impedance layer, thin high acoustic impedance layer and low acoustic impedance layer can be easily formed.

[0064] Examples of dry processes include sputtering and vapor deposition, and examples of wet processes include plating.

[0065] As the sputtering, for example, DC (direct current) or RF (radio frequency) magnetron sputtering or the like can be used.

[0066] By using sputtering as a method for forming the high acoustic impedance layer and the low acoustic impedance layer, it is possible to easily form thin high acoustic impedance layer and low acoustic impedance layer with high density, and therefore sputtering is preferred as a method for forming the high acoustic impedance layer and the low acoustic impedance layer.

[0067] The high acoustic impedance layer may be, for example, a W, Mo, or Ta film formed by DC or RF magnetron sputtering. 2 O 5A thin film formed of a material with a high density or bulk modulus, such as ZnO, can be used.

[0068] The low acoustic impedance layer may be, for example, a SiO film formed by DC or RF magnetron sputtering. 2 An oxide such as a film can be used.

[0069] When using DC or RF magnetron sputtering, the high acoustic impedance layer or the low acoustic impedance layer is Ta. 2 O 5 , ZnO, SiO 2 For example, when the high acoustic impedance layer is a ZnO film formed by DC or RF magnetron sputtering, either a Zn sputtering target or a ZnO sputtering target may be used for sputtering, depending on the gas atmosphere.

[0070] Next, the first electrode 30 is deposited (formed) on the upper surface of the acoustic mirror layer 20. The method for forming the first electrode 30 is not particularly limited, and either a dry process or a wet process may be used, similar to the method for forming the high acoustic impedance layer and the low acoustic impedance layer. Details of the dry process and the wet process are similar to the method for forming the high acoustic impedance layer and the low acoustic impedance layer, and therefore will not be described here.

[0071] The first electrode 30 may be formed on the entire upper surface 201 of the acoustic mirror layer 20. Alternatively, the first electrode 30 may be formed into any appropriate shape by processing it into a pattern having a predetermined shape by etching or the like.

[0072] Next, the piezoelectric layer 40 is formed on the upper surface 301 of the first electrode 30. For example, the piezoelectric layer 40 may be formed by DC or RF magnetron sputtering in a mixed gas atmosphere containing an inert gas such as Ar and a trace amount of oxygen, using a target containing elements constituting the piezoelectric material. The piezoelectric layer 40 is formed by sputtering the piezoelectric material onto the first electrode 30.

[0073] The laminate including the support substrate 10, the acoustic mirror layer 20, and the first electrode 30 may be placed on a deposition plate, which serves as an anode, in a deposition chamber of a sputtering apparatus. The deposition plate may be rotatable, for example. By placing the laminate including the support substrate 10, the acoustic mirror layer 20, and the first electrode 30 on the deposition plate, the piezoelectric layer 40 can be deposited on the first electrode 30 in a batch process.

[0074] Furthermore, the laminate including the support substrate 10, the acoustic mirror layer 20, and the first electrode 30 may be wound around a drum roll, which is a film-forming roll, instead of a film-forming plate, as an anode. By placing the drum roll in a film-forming chamber, the piezoelectric layer 40 can be continuously formed on the first electrode 30 while the laminate including the support substrate 10, the acoustic mirror layer 20, and the first electrode 30 is transported in a roll-to-roll manner.

[0075] A target containing elements that constitute the piezoelectric material is used as a cathode.

[0076] When the piezoelectric material includes, for example, a wurtzite crystalline material, a target containing the wurtzite crystalline material may be used. The target containing the wurtzite crystalline material may be a single or multiple targets containing the wurtzite crystalline material contained as a main component in the piezoelectric layer 40. The single or multiple targets may be arranged to face the deposition plate at an interval. The piezoelectric layer 40 containing the wurtzite crystalline material can be formed by using a multi-target sputtering method when multiple targets are used as cathodes, or by using a one-dimensional sputtering method when a single target is used as the cathode.

[0077] When multiple targets are used as cathodes, each target contains a different type of material that constitutes the wurtzite crystal material contained as a main component in the piezoelectric layer 40. When multiple targets are used, for example, a target containing Zn, a target containing Si or Sn, and a target containing Al or Mg may be used. Note that each target may be a metal oxide target containing oxygen. The multiple targets may be arranged in the film formation chamber at intervals. During sputtering, the power applied to each target is adjusted depending on the type of wurtzite crystal material contained in the piezoelectric layer 40, thereby adjusting the atomic ratio between the materials that constitute the piezoelectric layer 40.

[0078] When a single target is used as the cathode, the single target contains the wurtzite crystalline material contained in the piezoelectric layer 40. When a single target is used, an alloy target in which the atomic ratio of the wurtzite crystalline material contained in the piezoelectric layer 40 is adjusted may be used. For example, an alloy target containing Zn, Si or Sn, and Al or Mg may be used. The alloy target may be a metal oxide target containing a wurtzite crystalline material and oxygen.

[0079] For example, when the piezoelectric material is a wurtzite crystal material made of ZnO, a ZnO sintered compact target may be used. The ZnO sintered compact target is placed in a sputtering apparatus, and a mixed gas containing an inert gas such as Ar and oxygen is supplied into the sputtering apparatus. By sputtering using the ZnO sintered compact target in an atmosphere of the mixed gas containing the inert gas and oxygen, the piezoelectric layer 40 can be obtained on the first electrode 30 while suppressing the amount of inert gas that enters during ZnO film formation.

[0080] For example, when the piezoelectric material is a wurtzite crystal material made of MgZnO containing ZnO and MgO in a predetermined mass ratio, a multi-sputtering method using a target made of ZnO sintered body and a target made of MgO sintered body may be used. Alternatively, a one-dimensional sputtering method using an alloy target containing ZnO and MgO, such as a ZnO sintered body target to which MgO has been added in advance at a predetermined ratio, may be used.

[0081] When the multi-target sputtering method is used, a multi-target sputtering apparatus is used as the sputtering apparatus, and a mixed gas containing an inert gas such as Ar and oxygen is supplied into the multi-target sputtering apparatus. In an atmosphere of the mixed gas containing the inert gas and oxygen, a ZnO sintered compact target and an MgO sintered compact target are simultaneously and independently sputtered onto the first electrode 30, thereby forming the piezoelectric layer 40 composed of an MgZnO thin film on the first electrode 30.

[0082] When the one-dimensional sputtering method is used, a sputtering apparatus is used to perform sputtering in a mixed gas atmosphere containing an inert gas such as Ar and oxygen, using, for example, a target of ZnO sintered body to which MgO has been added in advance at a predetermined ratio, thereby forming the piezoelectric layer 40 composed of an MgZnO thin film on the first electrode 30.

[0083] The gas atmosphere during sputtering may be an inert gas atmosphere or a mixed gas atmosphere containing an inert gas and oxygen.

[0084] The pressure in the gas atmosphere during sputtering may be appropriately determined depending on the type of piezoelectric material, the sputtering method, etc., and may be set to, for example, 0.1 Pa to 2.0 Pa.

[0085] The deposition temperature of the piezoelectric layer 40 is not particularly limited and may be appropriately selected depending on the layer structure of the BAW resonator 1A, for example, the piezoelectric layer 40 may be deposited at 150° C. or lower.

[0086] By using a sputtering method to form the first electrode 30 and the piezoelectric layer 40, it is possible to form a uniform film with strong adhesion while maintaining the composition ratio of the compound target. Furthermore, by simply controlling the time, it is possible to form the first electrode 30 and the piezoelectric layer 40 with a desired thickness with high precision.

[0087] The piezoelectric layer 40 may be configured by laminating a plurality of layers.

[0088] Next, the end surface 402 of the piezoelectric layer 40 may be processed so that the angle between the end surface 402 of the piezoelectric layer 40 and a plane parallel to the upper surface 301 of the first electrode 30 is approximately 90°.

[0089] The processing method is Cl 2 , C.F. 4 , CHF 3 Dry etching using reactive gases such as HCl and HNO 3 A common method such as wet etching using an acid solution such as HCl or HClCl can be used.

[0090] Next, the resonator region defining layer 60 is formed on the upper surface 401 and the end surface 402 of the piezoelectric layer 40. The resonator region defining layer 60 may be formed using the same method as that used to form the first electrode 30 on the upper surface 201 of the acoustic mirror layer 20.

[0091] Next, a second electrode 50 having a predetermined shape is formed on the upper surface of the piezoelectric layer 40. The second electrode 50 can be formed using the same method as that used for the first electrode 30.

[0092] The thickness of the second electrode 50 can be designed appropriately and may be, for example, 40 nm to 300 nm.

[0093] The second electrode 50 may be formed on a part of the upper surface 401 of the piezoelectric layer 40, or may be formed in any suitable shape.

[0094] Next, a resonator region defining layer 60 is formed on the upper surfaces of the acoustic mirror layer 20 and the first electrode 30, and on the end portions of the piezoelectric layer 40 (the upper surface 401 and the end surface 403 of the piezoelectric layer 40). The method for forming the resonator region defining layer 60 is not particularly limited, and either a dry process or a wet process may be used, similar to the method for forming the high acoustic impedance layer and the low acoustic impedance layer. Details of the dry process and the wet process are similar to those of the method for forming the high acoustic impedance layer and the low acoustic impedance layer, and therefore will not be repeated here.

[0095] The second electrode 50 is formed on the upper surfaces of the acoustic mirror layer 20 and the first electrode 30 and on the end of the piezoelectric layer 40, thereby forming the BAW resonator 1A.

[0096] After the second electrode 50 is formed, the entire BAW resonator 1A may be heat-treated. This heat treatment can crystallize the first electrode 30 and the second electrode 50 and reduce their resistance. The heat treatment is not essential, and may not be performed after the formation of the BAW resonator 1A in cases such as when the support substrate 10 is made of a material that is not heat-resistant.

[0097] As described above, the BAW resonator 1A according to this embodiment includes a support substrate 10, a first electrode 30, a piezoelectric layer 40, a second electrode 50, and a resonator area defining layer 60. In the BAW resonator 1A, the first electrode 30 extends outward beyond the piezoelectric layer 40, and the resonator area defining layer 60 is made of a metal layer and is spaced apart from the second electrode 50 on the top surface 401 of the piezoelectric layer 40, and is provided on a part of the top surface 401 and an end surface 402 of the piezoelectric layer 40. "The first electrode 30 extends outward beyond the piezoelectric layer 40" means that the first electrode 30 is also disposed outside the piezoelectric layer 40 in a plan view seen from the stacking direction of the first electrode 30. In the BAW resonator 1A, by covering the end 41 of the piezoelectric layer 40 with the resonator region defining layer 60, when vibration occurs in the piezoelectric layer 40, the vibration of the end 41 can be suppressed by the resonator region defining layer 60. Therefore, in the BAW resonator 1A, it is possible to suppress the generation of transverse waves at the end of the piezoelectric layer 40.

[0098] The BAW resonator 1A can suppress the generation of transverse waves at the end 41 of the piezoelectric layer 40, thereby suppressing the generation of noise due to transverse waves.

[0099] In the BAW resonator 1A, the resonator region defining layer 60 can be provided continuously from the end face 402 of the piezoelectric layer 40 to the exposed portion of the first electrode. By providing the resonator region defining layer 60 continuously from the end 41 of the piezoelectric layer 40 to the exposed portion of the first electrode 30, the BAW resonator 1A can more reliably cover the end 41 of the piezoelectric layer 40 and more reliably suppress vibration of the end 41 of the piezoelectric layer 40, thereby more reliably suppressing the generation of transverse waves at the end 41 of the piezoelectric layer 40.

[0100] In the BAW resonator 1A, the resonator region defining layer 60 can be provided on the top surface 301 and the end surface 302 as exposed portions of the first electrode 30. In the BAW resonator 1A, the resonator region defining layer 60 is provided continuously from the end 41 of the piezoelectric layer 40 to the top surface 301 and the end surface 302 of the first electrode 30, thereby more reliably covering the end 41 of the piezoelectric layer 40 and more reliably suppressing vibration of the end 41 of the piezoelectric layer 40, thereby more reliably suppressing the generation of transverse waves at the end 41 of the piezoelectric layer 40.

[0101] The BAW resonator 1A may contain at least one of Al, Cu, and Au in the resonator region defining layer 60. Al, Cu, and Au are easily made to have the same potential as the first electrode 30 and have high conductivity, so the BAW resonator 1A can use the resonator region defining layer 60 as wiring while suppressing vibrations generated at the end 41 of the piezoelectric layer 40 with the resonator region defining layer 60.

[0102] In the BAW resonator 1A, the angle between the end face 402 of the piezoelectric layer 40 and a plane parallel to the upper surface 301 of the first electrode 30 can be set to approximately 90°. In the BAW resonator 1A, even if the end face 41 of the piezoelectric layer 40 is approximately perpendicular to the upper surface 301 of the first electrode 30, the end face 41 can be covered with the resonator region defining layer 60. Therefore, when vibration occurs in the piezoelectric layer 40, the vibration of the end face 41 can be suppressed by the resonator region defining layer 60.

[0103] In the BAW resonator 1A, the resonator region defining layer 60 can be made 50 nm or thicker. This allows the resonator region defining layer 60 to suppress vibrations at the end portion 41 of the piezoelectric layer 40 and suppress the generation of transverse waves. Therefore, even when used for a long period of time, the BAW resonator 1A can suppress deterioration in the piezoelectric properties of the piezoelectric layer 40 and reliably maintain the piezoelectric properties.

[0104] The BAW resonator 1A can be configured such that the first electrode 30 and the second electrode 50 contain at least one of Pt, W, Mo, Ru, and Ir.

[0105] The BAW resonator 1A can include MgZnO as a piezoelectric material in the piezoelectric layer 40. Generally, there is a trade-off between the K value and Q value of a piezoelectric layer formed by doping a piezoelectric material with other elements. For example, when a piezoelectric element is used in a high-frequency filter that extracts only signals in a high-frequency range, such as the 5 GHz band, and removes signals in other frequency bands, the Q value tends to decrease once the required K value is achieved in the high-frequency range. By including MgZnO as a piezoelectric material in the piezoelectric layer 40, there is no trade-off between the K value and Q value of MgZnO depending on the Mg concentration, and both the K value and Q value can be achieved even in the high-frequency range. Therefore, by including MgZnO as a piezoelectric material in the piezoelectric layer 40, the BAW resonator 1A can stably exhibit piezoelectric characteristics even in the high-frequency range of a high-frequency filter, etc.

[0106] The BAW resonator 1A can reduce noise generation even in high frequency bands and has excellent piezoelectric characteristics, and therefore can be effectively used as a BAW filter.

[0107] Furthermore, since the BAW resonator 1A can reduce noise generation and have excellent piezoelectric characteristics, it can also be used in electronic devices for various purposes as an electronic component that utilizes the positive piezoelectric effect or the inverse piezoelectric effect in electronic devices, in addition to BAW filters.

[0108] (Modification) In this embodiment, the BAW resonator 1A is not limited to the above configuration, and other configurations may be used as long as the end portion 41 of the piezoelectric layer 40 is covered with the resonator region defining layer 60 to prevent transverse waves from being generated from the piezoelectric layer 40. An example of another configuration of the BAW resonator 1A is shown below.

[0109] 2 , the BAW resonator 1B may be configured such that the end face 402 of the piezoelectric layer 40 is inclined. The angle between the end face 402 of the piezoelectric layer 40 and a plane parallel to the top surface 301 of the first electrode 30 may be less than 90°. This prevents deterioration of the film quality at the surface of the end face 402 of the piezoelectric layer 40 and in the depth direction near the end face 402. Therefore, the BAW resonator 1B can cover the end face 402 of the piezoelectric layer 40 with the resonator region-defining layer 60 while preventing deterioration from the end of the piezoelectric layer 40. This prevents transverse waves from being generated at the end 41 of the piezoelectric layer 40 and prevents deterioration of the piezoelectric characteristics.

[0110] In this case, it is preferable that the BAW resonator 1B has the resonator region defining layer 60 located at a widthwise distance of λ / 4 or more from the second electrode 50, where λ is the wavelength of the resonant frequency defined by the thickness of the piezoelectric layer 40. When the distance between the first electrode 30 and the second electrode 50 is less than λ / 4 in a plan view, surface acoustic waves generated at the end 41 of the piezoelectric layer 40 tend to be easily excited, and transverse waves tend to be easily generated. By locating the resonator region defining layer 60 at a widthwise distance of λ / 4 or more from the second electrode 50, where λ is the wavelength of the resonant frequency defined by the thickness of the piezoelectric layer 40, the BAW resonator 1B can further suppress the generation of transverse waves while suppressing degradation of the piezoelectric characteristics.

[0111] In the present embodiment, the BAW resonator 1A has the acoustic mirror layer 20 formed of an acoustic multilayer film, but the acoustic mirror layer 20 may also be formed of a space. For example, as shown in Fig. 3, the BAW resonator 1C may have a recess 11 formed on the upper surface 101 of the support substrate 10, and the space S formed between the recess 11 of the support substrate 10 and the first electrode 30 may function as the acoustic mirror layer 20.

[0112] In this case, the resonator region defining layer 60 may be provided on the exposed portion 101a of the upper surface 101 of the support substrate 10, the exposed portion 101a and end surface 302 of the upper surface 301 of the first electrode 30, and the exposed portion 401a and end surface 402 of the upper surface 401 of the piezoelectric layer 40.

[0113] In the BAW resonator 1C, the space S can function as the acoustic mirror layer 20, and therefore the first electrode 30 can be provided directly on the upper surface 101 of the support substrate 10. This allows the overall thickness of the BAW resonator 1E to be reduced, thereby enabling miniaturization.

[0114] In this embodiment, the BAW resonator 1A does not need to include the acoustic mirror layer 20. As shown in Fig. 4, the BAW resonator 1D may include a support substrate 10, a first electrode 30, a piezoelectric layer 40, and a second electrode 50, which are stacked in this order from the support substrate 10 side.

[0115] In this case, the support substrate 10 may be a conductive substrate. If the support substrate 10 is a conductive substrate, the support substrate 10 can also function as the first electrode, and therefore the BAW resonator 1A does not need to include the first electrode 30. For example, as shown in FIG. 5 , the BAW resonator 1E may include the support substrate 10, the piezoelectric layer 40, and the second electrode 50, stacked in this order from the support substrate 10 side. The support substrate 10 may be a metal plate or a conductive transparent substrate such as ITO, IZO, IZTO, or IGZO. When the support substrate 10 is a metal plate, a metal film such as Al foil, Cu foil, Al-Ti alloy foil, Cu-Ti alloy foil, or stainless steel foil may be used. Since a thin metal film increases the flexibility of the support substrate 10, a metal adhesive film such as Ti or Ni may be inserted between the support substrate 10 and the piezoelectric layer 40. 5, the thickness of the BAW resonator 1E can be reduced by the amount of the first electrode 30. This allows the overall thickness of the BAW resonator 1F to be reduced, thereby enabling miniaturization.

[0116] Although the embodiments have been described above, they are presented as examples and the present invention is not limited to the above embodiments. The above embodiments can be implemented in various other forms, and various combinations, omissions, substitutions, modifications, etc. can be made without departing from the spirit of the invention. These embodiments and their modifications are included within the scope and spirit of the invention, and are also included in the inventions and their equivalents as set forth in the claims.

[0117] Examples of embodiments of the present invention are as follows: <1> A BAW resonator comprising a support substrate and a first electrode, a piezoelectric layer, and a second electrode laminated in this order, the BAW resonator comprising a resonator region defining layer made of a metal layer and spaced apart from the second electrode on a surface of the piezoelectric layer that contacts the second electrode, the first electrode extending outward beyond the piezoelectric layer, and the resonator region defining layer being provided on a portion of the surface of the piezoelectric layer facing the second electrode and on an end surface of the piezoelectric layer. <2> The BAW resonator according to <1>, wherein the resonator region defining layer is provided continuously from the end surface of the piezoelectric layer to an exposed portion of the first electrode. <3> The BAW resonator according to <2>, wherein the exposed portion of the first electrode is the end surface of the first electrode and at least a portion of the surface of the first electrode facing the piezoelectric layer. <4> The BAW resonator according to any one of <1> to <3>, wherein an angle formed between an end face of the piezoelectric layer and a plane parallel to the surface of the first electrode is 90° or less. <5> The BAW resonator according to any one of <1> to <4>, wherein the resonator region defining layer contains at least one of Al, Cu, and Au. <6> The BAW resonator according to any one of <1> to <5>, wherein the resonator region defining layer is spaced apart from the second electrode in the width direction by λ / 4 or more, where λ is the wavelength of a resonant frequency defined by the thickness of the piezoelectric layer. <7> The BAW resonator according to any one of <1> to <6>, wherein the resonator region defining layer has a thickness of 50 nm or more. <8> The BAW resonator according to any one of <1> to <7>, wherein the first electrode and the second electrode contain at least one of Pt, W, Mo, Ru, and Ir. <9> The BAW resonator according to any one of <1> to <8>, wherein the piezoelectric layer contains ZnO doped with Mg. <10> The BAW resonator according to any one of <1> to <9>, further comprising an acoustic mirror layer between the support substrate and the first electrode, the acoustic mirror layer being a laminate in which one or more pairs of high acoustic impedance layers and low acoustic impedance layers are alternately stacked, or a gap formed between the support substrate and the first electrode. <11> An electronic device comprising the BAW resonator according to any one of <1> to <10>.

[0118] This application claims priority based on Japanese Patent Application No. 2023-55030, filed with the Japan Patent Office on March 30, 2023, and incorporates the entire contents of said application by reference.

[0119] 1A to 1E BAW resonator 10 Support substrate 20 Acoustic mirror layer 30 First electrode 40 Piezoelectric layer 50 Second electrode 60 Resonator area defining layer 101, 201, 301, 401 Main surface (upper surface) 101a, 201a, 301a, 401a Exposed portion 302, 402 End surface S Space

Claims

1. A BAW resonator comprising a first electrode, a piezoelectric layer and a second electrode laminated in this order on a supporting substrate, a resonator region defining layer made of a metal layer and spaced apart from the second electrode on the surface of the piezoelectric layer that contacts the second electrode, the first electrode extending outward beyond the piezoelectric layer, and the resonator region defining layer being provided on a portion of the surface of the piezoelectric layer facing the second electrode and on an end face of the piezoelectric layer.

2. A BAW resonator according to claim 1, wherein the resonator region defining layer is provided continuously from an end face of the piezoelectric layer to an exposed portion of the first electrode.

3. A BAW resonator according to claim 2, wherein the exposed portions of the first electrode are the surface of the first electrode facing the piezoelectric layer and an end face of the first electrode.

4. The BAW resonator according to claim 1, wherein the resonator region defining layer includes at least one of Al, Cu, and Au.

5. A BAW resonator according to claim 1, wherein an angle between an end face of said piezoelectric layer and a plane parallel to the surface of said first electrode is 90° or less.

6. A BAW resonator as described in claim 5, wherein an angle between an end face of the piezoelectric layer and a plane parallel to a surface of the first electrode is less than 90°, and the resonator region defining layer is spaced from the second electrode in the width direction by λ / 4 or more, where λ is the wavelength of a resonant frequency defined by the thickness of the piezoelectric layer.

7. The BAW resonator according to claim 1, wherein said resonator region defining layer has a thickness of 50 nm or more.

8. The BAW resonator of claim 1, wherein the first electrode and the second electrode include at least one of Pt, W, Mo, Ru, and Ir.

9. The BAW resonator of claim 1, wherein the piezoelectric layer comprises Mg-doped ZnO.

10. A BAW resonator as described in claim 1, further comprising an acoustic mirror layer between the support substrate and the first electrode, the acoustic mirror layer being a laminate in which one or more pairs of high acoustic impedance layers and low acoustic impedance layers are alternately stacked, or a gap formed between the support substrate and the first electrode.

11. An electronic device comprising the BAW resonator according to claim 1.

Citation Information

Patent Citations

  • Piezoelectric thin film resonator, filter, and duplexer

    JP2017158161A

  • Piezoelectric thin film resonator, filter and multiplexer

    JP2019016835A

  • Piezoelectric thin film resonator, filter and duplexer

    JP2019134221A