Detection method, detection support device, detection support program, and detection support method
The detection method employs a multiscale nanostructured substrate to minimize laser-induced damage and enhance Raman scattering, enabling sensitive detection of trace substances with improved accuracy.
Patent Information
- Application Number
- PCT/JP2024/011343
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-29
- Filing Date
- 2024-03-22
- Publication Date
- 2024-10-03
AI Technical Summary
Existing methods for detecting trace amounts of substances using surface-enhanced Raman scattering (SERS) often damage the target substance due to the focus of the excitation laser, limiting sensitivity and accuracy.
A detection method involving a substrate with a multiscale nanostructure, formed through electrolytic reduction of metal ions or heating reflux of a metal colloid solution, is used to minimize damage while enhancing Raman scattering intensity by optimizing nanostructure scale and laser conditions.
This approach allows for the sensitive detection of trace amounts of substances with reduced damage, achieving stronger Raman scattering intensity and improved detection accuracy by using finer nanostructures and adjusting laser parameters.
Smart Images

Figure JP2024011343_03102024_PF_FP_ABST
Abstract
Description
Detection method, detection support device, detection support program, and detection support method
[0001] The present disclosure relates to a detection method, a detection support device, a detection support program, and a detection support method.
[0002] There are various methods for detecting substances, and methods that can detect trace amounts of substances are required in various fields.
[0003] Surface-enhanced Raman scattering (SERS) is a phenomenon in which, when molecules are adsorbed on the surface of a noble metal with a nanoscale structure, the intensity of Raman scattering is greatly amplified compared to that on a bulk substrate. As a highly sensitive analytical method, SERS is used in a wide range of fields, including trace substance analysis, pathological diagnosis, environmental measurement, and food safety management.
[0004] Patent Document 1 discloses a method for detecting a substance by using surface-enhanced Raman scattering.
[0005] JP 2020-204495 A
[0006] However, one problem is that the focused excitation laser can damage the material.
[0007] Therefore, the present disclosure has been made in consideration of the above problems, and its purpose is to provide a detection method that can detect trace amounts of a target substance with high sensitivity while causing minimal damage to the target substance.
[0008] According to the present disclosure, there is provided a detection method for detecting a substance, comprising an irradiation step of irradiating laser light and a measurement step of measuring Raman scattered light generated by the irradiation of the laser light, wherein in the measurement step, a sample containing the substance is placed on a substrate having a multi-scale nanostructure, and the laser light is irradiated to perform measurement.
[0009] Other problems and solutions disclosed in this application will be made clear in the section on preferred embodiments of the invention and the drawings.
[0010] According to the present disclosure, it is possible to detect trace amounts of a target substance with high sensitivity while minimizing damage to the target substance.
[0011] 1 is a SEM image of AgNSsF5mMA. 2 is a SEM image of AgNSsF10mMA. 3 is a SEM image of AgNSsF15mMA. 4 is a diagram showing the Raman scattering spectrum of Cor / AgNSsF5mMA. 5 is a diagram showing the Raman scattering spectrum of Cor / AgNSsF10mMA. 6 is a diagram showing the Raman scattering spectrum of Cor / AgNSsF15mMA. 7 is a diagram showing the Raman scattering spectrum of Cor / AgNPsF. 8 is a diagram showing the Raman scattering spectrum of Cor / Si. 9 is a diagram showing the Raman scattering spectrum of trisodium citrate. 10 is a diagram showing the Raman scattering spectra of AgNPs / Cor / Si, Cor+AgNPs / Si, and Cor / Si. 11 is a microscope image taken during Raman scattering measurement of AgNPs / Cor / Si. 12 is a diagram showing the Raman scattering spectrum (OD0) of CorS1-6 / Si. 1 is a diagram showing Raman scattering spectra (OD3) of AgNPs / CorS1-6 / Si and AgNPs / Si. FIG. 2 is a diagram showing Raman scattering measurement from the back surface of the well. FIG. 3 is a diagram showing Raman scattering spectra (OD1) of AgNPs / CorS5 / Well, CorS5 / AuNPs / Well, CorS5 / AgNPs+AuNPs / Well, and CorS5 / Well. FIG. 4 is a diagram showing the Raman scattering spectrum (OD1) of AgNPs / CorS1-6 / Well. FIG. 5 is a diagram showing a spectrum obtained by baseline-correcting the Raman scattering spectrum of AgNPs / CorS1-6 / Well. FIG. 6 is a diagram showing an example of the configuration of a detection system according to the present disclosure. FIG. 7 is a diagram showing the hardware configuration of an information processing device 16 according to the present disclosure. FIG. 8 is a diagram showing the software configuration of an information processing device 16 according to the present disclosure. FIG. 9 is a diagram showing an example of a typical processing flow according to the present disclosure.
[0012] The details of the embodiments of the present invention will be listed and explained. One embodiment of the present invention has the following configuration. [Item 1] A detection method for detecting a substance, comprising: an irradiation step of irradiating with laser light; and a measurement step of measuring Raman scattered light generated by the irradiation with the laser light, wherein in the measurement step, a sample containing the substance is placed on a substrate having a multi-scale nanostructure, and the measurement is performed by irradiating with the laser light. [Item 2] The detection method according to Item 1, wherein the nanostructure is formed from a compound containing a metal. [Item 3] The detection method according to Item 1 or 2, wherein the nanostructure includes a nanostructure on a scale of at least 10-100 nm. [Item 4] The detection method according to Item 3, wherein the nanostructure is formed by electrolytic reduction of metal ions or by heating and refluxing a metal colloid solution. [Item 5] When the nanostructure is formed by electrolytic reduction of metal ions, the electrolytic reduction is performed at a current of 5 mA / cm. 2 to 15 mA / cm 2 The method of claim 4, wherein the method is carried out by applying a current of
[0013] <Details of the embodiment> Preferred embodiments of the present disclosure will be described in detail below with reference to the accompanying drawings. In this specification and drawings, components having substantially the same functional configurations are designated by the same reference numerals, and redundant description will be omitted.
[0014] [Device Configuration] As shown in FIG. 19 , a Raman scattering spectrometer according to an embodiment of the present disclosure includes a laser light source 10, a beam splitter 11, an objective lens 12, a spectrometer 13, a CCD detector 14, a sample stage 15, and an information processing device 16. A SERS chip 20 is mounted on the sample stage 15. With a solution containing an analyte introduced into the chip 20, excitation laser light is irradiated from the laser light source 10 and collected by the objective lens 12. The generated Raman scattered light is input to the spectrometer 13 via the objective lens 12 and the beam splitter 11 and dispersed there. The CCD detector 14 is positioned so as to measure a predetermined wavenumber range of Raman shifts. The Raman signal detected by the CCD detector 14 is sent to the information processing device 16 for analysis, display, recording, and the like. The information processing device 16 also controls the laser light source 10, the CCD detector 14, and the sample stage 15.
[0015] When performing Raman scattering measurements, the target may be a solid or a solution. In this disclosure, the target is supported on a surface in a solution state, and the target that has become solid after the solvent evaporates is measured.
[0016] It is known that SERS can be observed when certain types of molecules are adsorbed on the surface of metals such as gold (Au) or silver (Ag). In order for SERS to occur, a "surface nanostructure" must be formed on the metal surface, which generates a strong surface electric field through the interaction of excitation light and the metal.
[0017] In the present disclosure, for example, a surface nanostructure is formed using a metal. Then, a liquid to be measured is dropped onto the formed surface nanostructure, dried, and the sample is mounted on the sample stage 15. An excitation laser beam is irradiated, and the Raman signal is measured. The metal may be a noble metal such as gold, silver, or platinum, or may be any metal that exhibits strong plasmon resonance, such as copper or aluminum.
[0018] In the present disclosure, the surface nanostructure includes structures such as those shown in Figures 1, 2, and 3. The surface nanostructure may have at least one nanoscale structure formed on the surface so as to come into contact with the object to be detected and be irradiated with laser light.
[0019] The surface nanostructure in the present disclosure may be, for example, a polyhedron (including a near-polyhedron) or granular structure, as shown in FIG. 1 . The surface nanostructure may have one or more polyhedral faces that are concave or convex to a certain extent, the faces themselves may be curved, or the points where the faces of the polyhedron meet may be curved rather than straight, but is not limited to these structures. Furthermore, the surface nanostructure in the present disclosure may have a structure in which multiple nanostructures, including polyhedrons and granules, of different scales (hereinafter referred to as multi-scale), are assembled, as shown in FIGS. 2 and 3 . The assembled nanostructures may form, for example, a flower-like structure as shown in FIG. 2 or a branch-and-leaf structure as shown in FIG. 3 , but are not limited thereto. Even if the substance to be detected is easily decomposed by laser light, a multi-scale nanostructure, such as that shown in FIGS. 2 and 3 , is likely to be less likely to decompose the target substance by excitation laser light because it facilitates detection of the substance.
[0020] The surface nanostructure in the present disclosure may include structures with particle sizes on the scale of 1 nm-10 nm, 10 nm-50 nm, 50-100 nm, 100 nm-200 nm, 200 nm-500, 500 nm-1000 nm, 1 μm-2 μm, 3 μm-5 μm, and 6 μm-10 μm, when the nanostructure is considered as a grain, and may be an independent structure of multiple scale nanostructures as shown in the example of FIG. 1, or may be a structure formed by an aggregation of multiple scale nanostructures as shown in the examples of FIG. 2 and FIG. 3.
[0021] In the following examples, multi-scale nanostructures are formed using several materials and conditions, but the materials and formation conditions are merely examples, and any materials and conditions that can form multi-scale nanostructures are acceptable.
[0022] In the following examples, cortisol was used as the substance to be detected. Cortisol is a hormone secreted from the adrenal cortex, and its main functions are known to be promoting metabolism, such as gluconeogenesis in the liver, protein metabolism in muscles, and fat breakdown in adipose tissue, as well as anti-inflammatory and immunosuppressive effects. Cortisol is also known as a stress hormone because it stimulates the sympathetic nervous system when the human body senses stress, thereby maintaining a state of tension in the body. However, it goes without saying that the substance to be detected is not limited to cortisol.
[0023] Example 1: Detection of cortisol by surface-enhanced Raman scattering In this example, a nanostructure was formed using silver as an example of a metal. Specifically, a 10 g / L aqueous solution of silver nitrate was prepared, and silver nanostructures (AgNSs) were formed by electroreduction. The electroreduction conditions were 5 mA / cm 2 , 90Sec. , 10mA / cm 2 , 45Sec. , 15mA / cm 2 The electrolytic reduction was carried out at a current density and time of 30 sec.
[0024] FIG. 1 shows the current density of 5 mA / cm 2 , 90 sec. Figure 2 shows AgNSs prepared under the condition of 10 mA / cm 2 , 45 Sec. Figure 3 shows AgNSs prepared under the conditions of 15 mA / cm 2These are AgNSs prepared under the conditions of 30 seconds. Each was observed with a scanning electron microscope (SEM), and it was possible to successfully produce with good reproducibility: granular nanostructures (at least one or more of the following particle sizes: 1 μm-2 μm, 3 μm-5 μm, 6 μm-10 μm; structures on the order of several μm); flower-shaped nanostructures (at least one of the following particle sizes: 10 nm-50 nm, 50-100 nm, 100 nm-200 nm (several tens of nanometers to approximately 100 nm); and branch-and-leaf nanostructures (at least one of the following particle sizes: 1 nm-10 nm, 10 nm-50 nm, 50-100 nm (several tens of nanometers to approximately 100 nm); formed by assembling these nanostructures) in Figure 3.
[0025] Cortisol standard solution (Cor, 1.0 x 10 -9 mol / L) was used as the analyte, and the following samples were obtained: [A] 2 μL of Cor was dropped onto 5 mA of AgNSs / ITO and dried (Cor / AgNSs5 mA) [B] 2 μL of Cor was dropped onto 10 mA of AgNSs / ITO and dried (Cor / AgNSs10 mA) [C] 2 μL of Cor was dropped onto 15 mA of AgNSs / ITO and dried (Cor / AgNSs15 mA).
[0026] These samples were placed on the sample stage 15 and subjected to microscopic Raman scattering spectrum analysis (excitation wavelength: 532 nm, microscope magnification: 100x). Figures 4, 5, and 6 show the results of measurements of [A], [B], and [C], respectively.
[0027] Figure 7 shows the assignment of Raman scattering peaks. The peaks shown in standard form are cortisol peaks, those in italics are unknown peaks, and those in bold are peaks unrelated to the sample. Peaks that match literature values were confirmed. This demonstrates that cortisol can be detected using each silver nanostructure.
[0028] In addition, when measuring Raman scattering, in the case of [A], 10 times the amount of excitation light was used compared to [B] and [C]. From these facts, the order of the degree of enhancement of Raman scattering is [C]>[B]>>[A], so if you want to obtain a stronger Raman scattering intensity, it is desirable to use a finer, multi-scale nanostructure. When you want to obtain a stronger Raman scattering intensity, the conditions for the electroreduction of an aqueous solution containing metal ions, for example, a 10 g / L aqueous silver nitrate solution, are 10 mA / cm. 2 It is desirable that the current is 15 mA / cm or more. 2 It may be more than 5 mA / cm 2 Even if the excitation laser intensity is increased, detection is possible. 2 Above, 10mA / cm 2 It may be less than 5 mA / cm 2 Above, 15mA / cm 2 It may be less than 10 mA / cm 2 Above, 15mA / cm 2 It may be the following:
[0029] On the other hand, for the production of amorphous carbon by decomposition of cortisol, the peak temperature at 1300 cm in Figs. -1 , 1600 cm -1 From the bulge in the baseline in the wavenumber region around 15 mA, it can be said that 15 mA ≒ 10 mA >> 5 mA. Therefore, if you want to suppress the decomposition of a sample containing cortisol, condition [A] is preferable, but detection is also possible under conditions [B] and [C]. If you want to suppress the decomposition of the substance to be detected, 5 mA / cm is the condition for the electroreduction of an aqueous solution containing metal ions, for example, a 10 g / L silver nitrate aqueous solution. 2 It is desirable that the current is 10 mA / cm or more. 2 Above, 15mA / cm 2 Even if the current is higher than this, detection is possible by adjusting the irradiation time of the excitation laser. 2 Above, 10mA / cm 2 It may be less than 5 mA / cm 2 Above, 15mA / cm 2 It may be less than 10 mA / cm2 Above, 15mA / cm 2 It may be the following:
[0030] Example 2: Exploration of a Method for Using Silver Nanoparticles Suitable for Cortisol Detection by Surface-Enhanced Raman Scattering. In this example, nanostructures were formed using silver colloids as an example of metal colloids. A silver nanoparticle colloidal solution was synthesized using citrate ions as a protective agent. 36 mg of silver nitrate was dissolved in 200 mL of ultrapure water and heated to reflux. 4 mL of a 1 wt % aqueous solution of trisodium citrate was added, and the solution was heated to reflux for an additional hour and allowed to cool, yielding a silver nanoparticle colloidal solution. Although not shown, multiscale nanostructures were obtained, including nanostructures with particle sizes of at least 10-50 nm and 50-100 nm (nanostructures on the scale of several tens of nanometers). The silver nanoparticle colloidal solution was centrifuged, redispersed, and centrifuged again to obtain a concentrated silver nanoparticle solution (AgNPs). This solution was then used without redispersion [Non-Patent Document 2].
[0031] A cortisol standard solution (Cor) was used as the analyte, and [D] Cor was dropped onto a thin film of AgNPs accumulated at the hexane / water interface according to previous reports, followed by drying (Cor / AgNPsF) [Non-patent document 3, Non-patent document 4, Non-patent document 2]. [E] A solution of mixed Cor and AgNPs was dropped onto a silicon single crystal substrate (Si) and dried (Cor+AgNPs / Si). [F] Cor was dropped onto Si and dried (Cor / Si), after which AgNPs were dropped onto the surface of the Cor and dried (AgNPs / Cor / Si). Each sample was obtained.
[0032] These samples were placed on the sample stage 15 and subjected to microscopic Raman scattering spectrum analysis (excitation wavelength: 532 nm, microscope magnification: 100x). Except for trisodium citrate, spectra measured at approximately 10 points for each sample were averaged.
[0033] Measurements were performed on Cor / AgNPsF using neutral density filters of 1 / 100 (OD2), 1 / 1000 (OD3), and 1 / 10,000 (OD4) magnification (Figure 8). As a reference system, the Raman scattering spectrum of Cor / Si measured without a neutral density filter is shown in Figure 9, and the Raman scattering spectrum of trisodium citrate crystals, which are used as a reducing agent and protective agent during the synthesis of silver nanoparticles, is shown in Figure 10. The Raman scattering spectra of AgNPs / Cor / Si, Cor+AgNPs / Si, and Cor / Si are also shown in Figure 11.
[0034] In both samples, cortisol was measured in the solid state. Previously reported, the characteristic peaks in the Raman scattering spectrum of solid-state cortisol were 1150, 1220-1240, 1330-1350, 1430-1450, 1610, and 1640 cm -1 These include the three characteristic broad peaks in Figure 9 [Non-Patent Document 5]. Furthermore, previously reported peaks at 1150, 1270, 1340-1380, 1430-1450, and 1500 cm in the surface-enhanced Raman scattering spectrum of cortisol solution have been reported. -1 It has been suggested that a characteristic peak appears around this wavelength, and that the wavenumber at which the characteristic peak appears may vary significantly depending on the state [Non-Patent Document 5]. This indicates that when attempting to detect cortisol loaded in wells by surface-enhanced Raman scattering, as aimed at in this example, it is difficult to ignore the possibility that the Raman scattering wavenumber will differ between when cortisol is loaded in a "multilayer" and when it is loaded as a "monolayer (isolated molecular system)."
[0035] On the other hand, in this example, nanoparticles containing trisodium citrate as a protective agent were used, and as shown in FIG. -1 The Raman scattering signal that appears in the sample should not be used to confirm the presence and quantitation of cortisol.
[0036] From the above, in this example, 1330-1350, 1500 cm -1It is considered appropriate to use the Raman scattering signal of the above to confirm the presence and quantification of cortisol. Based on this, from the results of Figures 8 and 11, it can be seen that among the prepared samples, the Raman scattering signal of AgNPs / Cor / Si is significantly enhanced, and each peak appears more clearly than other systems. In addition, -1 Since the Raman scattering signal of the nanoparticles can be clearly observed, we decided to use the method of dropping a nanoparticle solution onto the Cor surface of Cor / Si as the method of using the nanoparticles in this study.
[0037] Also, a microscope image of AgNPs / Cor / Si during measurement is shown in Figure 12. The central point L is the excitation laser light for Raman scattering measurement. Enhanced Raman scattering occurs only at black spots such as point R, so black spots such as point R are thought to be aggregates of silver nanoparticles. To detect cortisol, it is sufficient to select and excite point R and obtain a Raman scattering spectrum. From Figure 12, it can be seen that a black spot (cortisol) of the same size as point R is 400 μm 2 It is believed that at least 20 such regions exist within this area, and that enhanced Raman scattering signals can be obtained. Assuming that the quantitativeness of the measurement can be fully ensured, it is expected that similar evaluations will be possible in areas that are orders of magnitude smaller than the 96-well plates often used in ELISA.
[0038] Example 3: Detection of Cortisol Standard Solutions of Different Concentrations by Surface-Enhanced Raman Scattering Concentrated silver nanoparticle solutions (AgNPs) obtained in the same manner as in Example 2 were used without redispersion. Cortisol standard solutions of 3, 1, 0.33, 0.11, 0.037, and 0.012 μg / dL (CorS1, CorS2, CorS3, CorS4, CorS5, and CorS6, respectively) were used as analytes. 1 μL of each solution was dropped onto a single-crystal silicon (Si) substrate, dried, and then supported (Cor1-6 / Si). 1 μL of AgNPs was dropped onto the Cor side of Cor1-6 / Si and dried (AgNPs / CorS1-6 / Si). A reference system was also prepared by dropping AgNPs onto Si and drying (AgNPs / Si). The microscopic Raman scattering measurements were performed under the following conditions: excitation wavelength: 532 nm, microscope magnification: 100x, acquisition time: 5 seconds, and number of integrations: none (single-shot measurement). The spectra measured at approximately 10 points were averaged.
[0039] The Raman scattering spectrum of CorS1-6 / Si measured without using a neutral density filter (OD0) is shown in Figure 13, and the Raman scattering spectra of AgNPs / CorS1-6 / Si and AgNPs / Si measured with a 1 / 1000 neutral density filter (OD3) are shown in Figure 14.
[0040] In the section indicated by A in Figure 13, the results are for CorS4 / Si, CorS5 / Si, CorS2 / Si, CorS6 / Si, CorS3 / Si, and CorS1 / Si from top to bottom. In all cases of CorS1-6 / Si, the Raman scattering intensity did not correspond to the change in the concentration of CorS1-6. In addition, the 1450 cm -1 In Figure 13, for AgNPs / CorS1-6 / Si, the scattering peaks at 1330-1350 and 1500 cm -1 In addition, although detailed attribution is difficult, many new Raman scattering peaks due to the presence of cortisol are observed. It is possible that denaturation occurs due to a local temperature rise during the Raman scattering measurement.
[0041] Furthermore, in the section shown by B in Figure 14, from top to bottom, the results are for AgNPs / CorS5 / Si, AgNPs / CorS6 / Si, AgNPs / CorS2 / Si, AgNPs / CorS1 / Si, AgNPs / CorS3 / Si, AgNPs / CorS4 / Si, and AgNPs / Si. Looking at Figure 14, as with CorS1-6 / Si shown in Figure 13, the concentration of CorS1-6 does not correspond to the Raman scattering signal intensity. This can be explained by the fact that when AgNPs are dropped, the underlying CorS1-6 dissolves, and CorS1-6 is re-concentrated in the gaps between the AgNP aggregates and becomes a solid.
[0042] Generally, the areas where the localized surface plasmon resonance electric field is extremely strong are nanogap (groove)-like regions that occur in nanoparticle aggregates, which corresponds well to the phenomenon observed in this section. Therefore, if an extremely low concentration of cortisol is analyzed to prevent localized concentration of cortisol, or if a method is used to analyze cortisol that is firmly bound to some surface, it is expected that a Raman scattering spectrum closer to that of single-molecule cortisol can be obtained. The intensity of the Raman scattering spectrum of AgNPs / Si is significantly lower than that of AgNPs / CorS1-6 / Si, and is thought to have no significant effect on the spectrum of AgNPs / CorS1-6 / Si.
[0043] Example 4: Detection of cortisol by surface-enhanced Raman scattering in cortisol evaluation wells. Similar to Examples 2 and 3, a gold and silver nanoparticle colloidal solution was synthesized using citrate ions as a protective agent according to a previously reported method (synthesis conditions for obtaining gold nanoparticles with a particle size of approximately 15-20 nm) [Non-Patent Documents 4, 6, and 7]. A concentrated gold nanoparticle solution (AuNPs) obtained by centrifugation of the gold nanoparticle solution was used without redispersion [Non-Patent Documents 8 and 2]. A concentrated silver nanoparticle solution (AgNPs) obtained by the same method as in the previous section was used without redispersion [Non-Patent Document 2].
[0044] In wells for cortisol evaluation by EIA, 3, 1, 0.33, 0.11, 0.037, and 0.012 μg / dL cortisol standard solutions (CorS1, CorS2, CorS3, CorS4, CorS5, and CorS6, respectively) were loaded as analytes (CorS1-6 / well). 1 μL of AgNPs, AuNPs, and an equal mixture of AgNPs and AuNPs (AgNPs + AuNPs) were dropped into these wells to prepare Raman scattering samples (AgNPs / CorS1-6 / well, AuNPs / CorS1-6 / well, and AgNPs + AuNPs / CorS1-6 / well). The Raman scattering measurements were performed under the following conditions: excitation wavelength: 532 nm, microscope magnification: 50x, acquisition time: 1 second, and no integration (single-shot measurement). The spectra measured at approximately 10 points were averaged. For the Raman scattering measurements, excitation was applied from the back of the well (e.g., the part indicated by C in Figure 15), and scattered light was acquired.
[0045] The Raman scattering spectra of AgNPs / CorS5 / Well, CorS5 / AuNPs / Well, CorS5 / AgNPs+AuNPs / Well, and CorS5 / Well are shown in Figure 9. A 1 / 10 (OD1) neutral density filter was used.
[0046] In Figure 16, when AgNPs were used, a significantly higher Raman scattering intensity was obtained compared to the other examples. -1 The Raman scattering peaks at 1350 and 1500 cm were clearly observed when AgNPs were used in combination with AuNPs compared to when AuNPs alone were used. -1 Although there was a tendency for the Raman scattering peak of gold nanoparticles to become higher, no positive synergistic effect was observed in this system due to the simultaneous use of gold nanoparticles and silver nanoparticles [Non-Patent Documents 9-11].
[0047] The Raman scattering spectrum of AgNPs / CorS1-6 / Well is shown in FIG. 17, and the spectrum obtained by subtracting the baseline as a straight line is shown in FIG.
[0048] In the CorS2-6 region, the 1330-1350 and 1500 cm regions are used as cortisol markers.-1 The Raman scattering peaks of amorphous carbon, which are expected to be produced by thermal decomposition of the sample, were clearly observed at 1350 and 1600 cm. -1 The proportion of broad scattering peaks with peak wavenumbers of 1 and 2 is high. This can be a major factor in impairing quantitative accuracy. This is a feature also observed in Examples 2 and 3, and it is thought that this can be addressed by reducing the excitation light density or by taking measures to prevent nanoparticles from getting too close to each other when they aggregate.
[0049] In fact, the Raman scattering intensity of these samples does not correspond to the concentration change up to CorS1-6, and they cannot be used for quantification within this range of concentration conditions. On the other hand, when the relatively low concentration standard sample CorS5-6 was used, the Raman scattering intensity corresponded well to the concentration change, and it is desirable to study cortisol solutions in an even lower concentration range.
[0050] The area required for one measurement point (corresponding to one hole in a well) is 20 μm when using a 100x microscope optical system. 2 This indicates the possibility of significantly reducing the absolute amount of antibody required for quantitative analysis using EIA, ELISA, etc.
[0051] The minimum exposure time required to measure one point was 1 second (due to the performance of the equipment used), and it was found that even if multiple points were measured and it took 2 seconds to move the measurement area per point, it was possible to measure one point in 3 seconds.
[0052] When cortisol is directly measured, it has been found that quantitative measurement is possible at concentrations of 0.037 μg / dL or less.
[0053] It was revealed that the excitation laser caused a high rate of amorphous carbonization of the sample. It is expected that this carbonization can be suppressed by reducing the excitation light density and dispersing the local heat.
[0054] [Non-patented document 1] T. Akiyama, T. Yamamoto, T. Oku, M. Yahiro, T. Kurihara, C. Adachi and S. Yamada, Jpn. J. Appl. Phys. , 52, 122301 (2013). [Non-patented document 2] N. Koyama, T. Akiyama and T. Oku, Jpn. J. Appl. Phys. , 60, 027002 (2021). [Non-patent document 3] M. Suzuki, Y. Niidome, N. Terasaki, K. Inoue, Y. Kuwahara and S. Yamada, J. Appl. Phys., 43, L554 (2004). [Non-patent document 4] T. Akiyama, M. Nakadada, N. Terasaki and S. Yamada, Chem. Commuun., 395 (2006). [Non-patent document 5] T. J. Moore and B. Sharma, Anal Chem. , 92, 2052 (2020). [Non-patented document 6] T. Arakhawa, T. Kawawahara, T. Akiyama and S. Yamada, Jpn. J. Appl. Phys. , 46, 2490 (2007). [Non-patented document 7] T. Akiyama, T. Kawawahara, T. Arakhawa and S. Yamada, Jpn. J. Appl. Phys. , 47, 3063 (2008). [Non-patented reference 8] J. Turkevich, P. C. Stevenson and J. Hillier, Discuss. Faraday Soc. , 11, 55 (1951). [Non-patented reference 9] T. Akiyama, e-J. Surf. Sci. Nanotech. , 10, 157 (2012). [Non-patented reference 10] Y. Liu, Z. Lu, X. Lin, H. Zhu, W. Hasi, M. Zhang, X. Zhao and X. Lou, RSC Adv. , 6, 58387 (2016). [Unauthorized Document 11] N. Koyama, S. Banya, T. Akiyama, K. Sugawa and T. Oku,Appl. Phys. Express, 13, 055001 (2020). ,
[0055] As shown in FIG. 19 , a detection device (Raman scattering spectroscopy measurement device) according to an embodiment of the present disclosure includes a laser light source 10, a beam splitter 11, an objective lens 12, a spectrometer 13, a CCD detector 14, a sample stage 15, and an information processing device 16. With a solution containing an analyte introduced into the sample stage 15, excitation laser light is irradiated from the laser light source 10 and collected by the objective lens 12. The generated Raman scattered light is input to the spectrometer 13 via the objective lens 12 and the beam splitter 11 and dispersed there. The CCD detector 14 is positioned so as to be able to measure a predetermined wavenumber range of Raman shifts. The Raman signal detected by the CCD detector 14 is sent to the information processing device 16 for analysis, display, recording, and the like. The information processing device 16 also controls the laser light source 10, the CCD detector 14, and the sample stage 15.
[0056] The detection system of this embodiment includes an information processing device 16. The information processing device 16 is communicably connected to a laser light source 10, a beam splitter 11, an objective lens 12, a spectrometer 13, a CCD detector 14, and a sample stage 15 via a wired or communication network. The communication network is, for example, the Internet, and is constructed using a public telephone network, a mobile phone network, a wireless communication path, Ethernet (registered trademark), or the like.
[0057] The information processing device 16 may be, for example, a general-purpose computer such as a workstation or a personal computer, or may be logically realized by cloud computing. In this embodiment, for convenience of explanation, one device is illustrated as an example, but the present invention is not limited to this and multiple devices may be used.
[0058] FIG. 20 is a diagram illustrating an example of the hardware configuration of the information processing device 16. Note that the illustrated configuration is an example, and other configurations may also be used. The information processing device 16 includes a CPU 101, a memory 102, a storage device 103, a communication interface 104, an input device 105, and an output device 106. The storage device 103 stores various data and programs, such as a hard disk drive, a solid-state drive, or a flash memory. The communication interface 104 is an interface for connecting to a communication network NW, such as an adapter for connecting to Ethernet (registered trademark), a modem for connecting to a public telephone network, a wireless communication device for wireless communication, or a USB (Universal Serial Bus) connector or an RS232C connector for serial communication. The input device 305 is used to input data, such as a keyboard, a mouse, a touch panel, buttons, or a microphone. The output device 306 is used to output data, such as a display, a printer, or a speaker. Each functional unit of the information processing device 16 described below is realized by the CPU 101 reading a program stored in the storage device 103 into the memory 102 and executing it, and each storage unit of the information processing device 16 is realized as part of the storage area provided by the memory 102 and the storage device 103.
[0059] Fig. 21 shows the functional configuration of the information processing device 16. As shown in Fig. 21 , the information processing device 16 includes storage units, namely, an image storage unit 131, a Raman signal storage unit 132, and a model storage unit 133, as well as processing units, namely, a laser control unit 111, an image acquisition unit 112, a Raman signal acquisition unit 113, a model generation unit 114, and a detection position presentation unit 115.
[0060] The image storage unit 131 stores information about the image acquired by the image acquisition unit 112 using the CCD detector 14 .
[0061] The Raman signal storage unit 132 stores the Raman signal acquired by the Raman signal acquisition unit 113 .
[0062] The model storage unit 133 stores the prediction model generated by the model generation unit 114 .
[0063] The above is a description of each storage unit included in the detection support system. Below, a description will be given of each processing unit included in the detection support system.
[0064] The laser control unit 111 controls the laser light source 10 to irradiate the detection target with excitation laser light. The laser control unit 111 may irradiate the laser light at any position on the sample stage 15, at a position designated by the user, or at a position presented by a detection position presentation unit 115 (described later), but is not limited to these.
[0065] The image acquisition unit 112 acquires an image of the sample using the CCD detector 14. The acquired image may include a video.
[0066] The Raman signal acquisition unit 113 acquires a Raman signal using the CCD detector 14 .
[0067] The model generation unit 114 generates a model that predicts positions suitable for detecting the detection target (i.e., positions where multiple nanoscales exist) in the image acquired by the image acquisition unit 112. The model generation unit 114 may use, as training data, an image in which a black dot portion that is considered to be a multiple nanoscale, such as point R in Figure 12, is cut out, and generate a prediction model that predicts positions where multiple nanoscales exist in other images through machine learning. The input data for this prediction model is image information, and the output data is information on black dots that are considered to be multiple nanoscales among the black dots in the image.
[0068] The detection position presenting unit 115 presents to the user, via the output device 106 or the like, a position to be detected based on image information using the prediction model generated by the model generating unit 114. The detection position presenting unit 115 accepts a selection from a plurality of detection positions in the presented image from the user, and irradiates the position selected by the laser control unit 111 with excitation laser light.
[0069] The result presentation unit 116 presents the signal acquired by the Raman signal acquisition unit 113 to the user via the output device 106 or the like. The result presentation unit 116 may convert the signal acquired by the Raman signal acquisition unit 113 into the form of a graph or a table and present it to the user.
[0070] A typical processing flow of the information processing device 16 of this embodiment will be described with reference to FIG. 22 . The laser control unit 111 irradiates the sample with an excitation laser (1001). The image acquisition unit 112 acquires an image (1002). The Raman signal acquisition unit 113 acquires a Raman signal (1003). The model generation unit 114 generates a prediction model that predicts a detection position in the image (1004). The detection position presentation unit 115 presents the detection position to the user using the prediction model (1005). The detection position presentation unit 115 accepts a selection of a detection position from the user, and irradiates the selected position in the image with excitation laser light via the laser control unit 111 (1006). The result presentation unit 116 presents the signal acquired by the Raman signal acquisition unit to the user (1007).
[0071] Although the preferred embodiments of the present disclosure have been described in detail above with reference to the accompanying drawings, the technical scope of the present disclosure is not limited to such examples. It is clear that a person skilled in the art of the present disclosure can conceive of various modified or altered examples within the scope of the technical idea described in the claims, and it is understood that these also naturally fall within the technical scope of the present disclosure.
[0072] The devices described in this specification may be realized as a single device, or may be realized by a plurality of devices (e.g., cloud servers) some or all of which are connected via a network. For example, the CPU and storage device of the information processing device 16 may be realized by different servers connected to each other via a network.
[0073] The series of processes performed by the device described herein may be implemented using software, hardware, or a combination of software and hardware. A computer program for implementing each function of the information processing device 16 according to this embodiment may be created and installed on a PC or the like. A computer-readable recording medium storing such a computer program may also be provided. Examples of the recording medium include a magnetic disk, an optical disk, a magneto-optical disk, and a flash memory. The computer program may also be distributed, for example, via a network, without using a recording medium.
[0074] Additionally, the processes described herein do not necessarily have to be performed in the order described, some process steps may be performed in parallel, additional process steps may be employed, and some process steps may be omitted.
[0075] Furthermore, the effects described herein are merely descriptive or exemplary and are not limiting. In other words, the technology according to the present disclosure may achieve other effects that will be apparent to those skilled in the art from the description of this specification, in addition to or in place of the above-described effects.
[0076] 10 Laser light source 11 Beam splitter 12 Objective lens 13 Spectrometer 14 CCD detector 15 Sample stage 16 Information processing device
Claims
1. A detection method for detecting a substance, comprising: an irradiation step of irradiating laser light; and a measurement step of measuring Raman scattered light generated by the irradiation of the laser light, in which in the measurement step, a sample containing the substance is placed on a substrate having a multi-scale nanostructure, and the laser light is irradiated to perform the measurement.
2. The detection method according to claim 1, wherein the nanostructure is formed from a compound containing a metal.
3. The detection method according to claim 1 or 2, wherein the nanostructure comprises a nanostructure on the scale of at least 10-100 nm.
4. The detection method according to claim 3, wherein the nanostructure is formed by electrolytic reduction of metal ions or by heating a metal colloid solution under reflux.
5. When the nanostructure is formed by electrolytic reduction of metal ions, the electrolytic reduction is 5 mA / cm 2 to 15mA / cm 2 The method of claim 4, wherein the method is carried out by applying a current of