Method for surface roughening
The surface roughening treatment method using overlapping pulsed laser irradiation on metal members forms deep grooves and protrusions, effectively improving the bonding strength between metal and resin members, addressing the limitations of existing methods and reducing manufacturing costs.
Patent Information
- Application Number
- PCT/JP2024/011729
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-29
- Filing Date
- 2024-03-25
- Publication Date
- 2024-10-03
AI Technical Summary
The existing surface roughening treatment methods for metal-resin composites using laser irradiation do not effectively enhance the bonding strength between the metal and resin members, as they lack a specific method to optimize the laser irradiation conditions for improved adhesion.
A surface roughening treatment method involving the use of a pulsed laser moved across the joint surface of a metal member, where the irradiation area is overlapped to form protrusions and deep grooves, enhancing the bonding surface by deforming the molten metal before it solidifies, thereby improving the shear bonding strength.
This method significantly increases the bonding strength between the metal and resin members by forming deep grooves and protrusions that prevent the resin from detaching, while reducing manufacturing costs and allowing for direct joining without adhesives or screws, enhancing the composite's strength and airtightness.
Smart Images

Figure JP2024011729_03102024_PF_FP_ABST
Abstract
Description
Surface roughening treatment method
[0001] The present invention relates to a surface roughening method.
[0002] JP2018-58231A discloses a metal-resin composite formed by joining a metal member and a resin. The surface of the metal member is roughened by, for example, laser irradiation, to form irregularities. As a result, the resin penetrates into the recesses of the metal member, solidifies, and becomes fixed so that it does not slip out of the recesses, thereby joining the metal member and the resin.
[0003] JP2018-58231A does not describe a specific method for texture formation by laser irradiation. In the texture formation treatment described in JP2018-58231A, there is room for improving the bonding strength between the metal member and the resin by adjusting the laser irradiation method and conditions.
[0004] An object of the present invention is to improve the bonding strength between a metal member and a resin member.
[0005] According to one aspect of the present invention, there is provided a roughening treatment method for roughening the joining surface of a metal member when joining the metal member and a resin member, the method comprising an irradiation step of irradiating the joining surface of the metal member with a pulsed laser while moving the laser, and in the irradiation step, the irradiation area position is overlapped so that the pulsed laser is irradiated again to the molten portion of the metal member, thereby forming a groove portion and protrusions provided on both sides of the groove portion and protruding from the joining surface of the metal member.
[0006] FIG. 1 is a cross-sectional schematic diagram of a composite. FIG. 2 is a schematic diagram showing the irradiation step of a surface roughening method according to an embodiment of the present invention. FIG. 3 is a top view of the joining surface of a metal member, showing the pulse laser irradiation area in the irradiation step of the surface roughening method. FIG. 4 is a cross-sectional schematic diagram showing the first row of pulse laser irradiation. FIG. 5 is a cross-sectional schematic diagram showing the second row of pulse laser irradiation. FIG. 6 is a cross-sectional schematic diagram showing the state in which the groove portion is covered with a synthetic protrusion and a tunnel shape is formed. FIG. 7 is an optical microscope photograph of the surface of a metal member subjected to a surface roughening method with different numbers of irradiations. FIG. 8 is an electron microscope (SEM) photograph of the surface of a metal member subjected to a surface roughening method with different numbers of irradiations.
[0007] Hereinafter, a surface roughening method according to an embodiment of the present invention will be described with reference to the drawings.
[0008] The surface roughening method of this embodiment is carried out when forming a composite 100 in which a metal member 1 and a resin member 11 are joined together, as shown in FIG.
[0009] In this embodiment, the composite 100 is a so-called multi-material composite formed by combining a metal member 1 and a resin member 11 for the purposes of weight reduction, high strength, etc. The metal member 1 is, for example, iron or aluminum, and the resin member 11 is, for example, any thermoplastic resin that can be injection molded. The surface roughening method of this embodiment is performed to combine the metal member 1 and the resin member 11 to form a multi-material composite. Note that the materials of the metal member 1 and the resin member 11 are not limited to those described above. Furthermore, the composite 100 is not limited to a multi-material composite, and the surface roughening method may be performed when forming a composite 100 that is not a multi-material composite.
[0010] The surface roughening treatment method is performed when directly joining a metal member 1 and a resin member 11 without using screws, adhesive, or the like, and roughens the joining surface 2 of the metal member 1. After the surface roughening treatment method is performed on the joining surface 2 of the metal member 1, the metal member 1 and the resin member 11 are joined together to form a composite 100 by pouring a molten resin member 11 onto the joining surface 2 of the metal member 1. Details of the joining of the metal member 1 and the resin member 11 will be described later.
[0011] 2, the surface roughening method is performed using a pulsed laser L that outputs a laser beam at a constant repetition rate. The surface roughening method includes an irradiation step of irradiating a rectangular joining surface 2 of a metal member 1 with the pulsed laser L while moving the laser beam in a linear direction.
[0012] FIG. 2 is a schematic diagram illustrating an irradiation area P of the pulsed laser L. In the irradiation process, first, as shown in FIG. 2( a), the pulsed laser L is irradiated at the end (the far side in FIG. 2) of the joining surface 2 of the metal members 1 while moving linearly. Next, the pulsed laser L is moved in parallel, and as shown in FIG. 2( b), the pulsed laser L is irradiated while moving linearly at intervals adjacent to the row irradiated with the pulsed laser L in FIG. 2( a) so as not to overlap (in other words, so that the irradiation areas P do not overlap). Then, the pulsed laser L is moved in parallel, and as shown in FIG. 2( c), the pulsed laser L is irradiated while moving linearly adjacent to the row irradiated with the pulsed laser L in FIG. 2( b) so as not to overlap. In this way, the operation of irradiating while moving the pulsed laser L in a linear manner is repeated, and the entire joining surface 2 of the metal members 1 is irradiated with the pulsed laser L. As a result, the joining surface 2 of the metal members 1 is irradiated with multiple parallel rows of the pulsed laser L. As described above, in the irradiation step, the pulsed laser L is irradiated in a plurality of rows in order (starting from the end of the joining surface 2 of the metal member 1) while moving linearly.
[0013] In this specification, the "number of times of irradiation with the pulsed laser L" refers to the number of sets of a series of operations in which the pulsed laser L is irradiated while moving in a linear manner, and the entire joining surface 2 of the metal members 1 is irradiated with the pulsed laser L. In other words, the series of operations shown in FIGS. 2( a) to 2(c) constitute one set. When the number of times of irradiation with the pulsed laser L is two, the pulsed laser L is irradiated while moving in a linear manner, and the entire joining surface 2 of the metal members 1 is irradiated with the pulsed laser L, and then the pulsed laser L is irradiated again while moving in a linear manner in the same manner, and the entire joining surface 2 of the metal members 1 is irradiated with the pulsed laser L. In the irradiation step, the number of times of irradiation with the pulsed laser L is one set or multiple sets.
[0014] 3, in the irradiation step, when the pulsed laser L is irradiated while being moved linearly, the irradiation area P of each laser pulse irradiated at a constant repetition frequency is made to overlap. In other words, in the irradiation step, the pulsed laser L is moved linearly so that the irradiation areas P of adjacent laser pulses on the joining surface 2 of the metal member 1 partially overlap.
[0015] In addition, when the pulse laser L is irradiated multiple times in sets, the irradiation area P of the pulse laser L of the second set or later may be in the same position as the irradiation area P of the pulse laser L of the first set, or may be shifted in the movement direction of the pulse laser L relative to the irradiation area P of the pulse laser L of the first set.
[0016] 4 and 5 are cross-sectional schematic diagrams showing irradiation of a pulsed laser L in a cross section perpendicular to the movement direction of the pulsed laser L. Fig. 4 is a cross-sectional diagram showing irradiation of the first row (the top row in Fig. 3) of pulsed laser L, and Fig. 5 is a cross-sectional diagram showing irradiation of the second row (the middle row in Fig. 3) of pulsed laser L adjacent to the first row. Figs. 4(a) to (d) and Figs. 5(a) to (d) sequentially show cross sections along the movement direction of the pulsed laser L, and the direction perpendicular to the paper surface in Figs. 4 and 5 is the movement direction of the pulsed laser L.
[0017] First, the irradiation of the first pulsed laser beam L will be described. When the joining surface 2 of the metal members 1 is first irradiated with the pulsed laser beam L as shown in FIG. 4( a), the irradiated irradiation area P is melted by the energy of the pulsed laser beam L as shown in FIG. 4( b), forming a molten zone 2a. In the irradiation process, the irradiation areas P of each pulse of the pulsed laser beam L are overlapped, so that the molten zone 2a is irradiated with the pulsed laser beam L again before solidifying as shown in FIG. 4( c). When the molten zone 2a is irradiated with the pulsed laser beam L again, the molten zone 2a is deformed by the impact of the irradiation. Then, the molten zone 2a solidifies, and as shown in FIG. 4( d), a groove portion 3 and protrusions 4 are formed on both sides of the groove portion 3 and protrude from the joining surface 2 of the metal members 1. In the irradiation process, multiple overlapping regions of the irradiation areas P of the pulsed laser beam L are formed, resulting in multiple shapes as shown in FIG. 4( d). Furthermore, since the interval between the overlapping irradiation regions P is small in the moving direction of the pulsed laser L, the grooves 3 and the protrusions 4 are formed to extend in the moving direction of the pulsed laser L.
[0018] Next, the irradiation of the second row of pulsed laser beams L will be described. When the second row is first irradiated with the pulsed laser beam L as shown in FIG. 5( a), the irradiated irradiation area P is melted by the energy of the pulsed laser beam L as shown in FIG. 5( b), forming a molten portion 2a. As shown in FIG. 5( c), when the molten portion 2a is again irradiated with the pulsed laser beam L before it solidifies, the molten portion 2a is deformed by the impact of the irradiation. The molten portion 2a deforms so as to climb onto the protrusions 4 in the adjacent row (first row). Then, the molten portion 2a solidifies, and as shown in FIG. 5( d), adjacent protrusions 4 are combined to form combined protrusions 4a. The combined protrusions 4a are formed higher above the joining surface 2 than the non-combined protrusions 4. During the irradiation process, multiple overlapping regions of the irradiated area P of the pulsed laser beam L are formed, resulting in multiple shapes as shown in FIG. 5( d). Furthermore, since the intervals between overlapping irradiation regions P are small in the direction of movement of the pulsed laser L, the grooves 3, protrusions 4, and composite protrusions 4a are formed to extend in the direction of movement of the pulsed laser L.
[0019] Furthermore, increasing the number of pulsed laser L irradiations results in deeper grooves 3 and higher protrusions 4 and composite protrusions 4a. Furthermore, when the composite protrusions 4a tilt from the state shown in FIG. 5(d), they overcome the grooves 3 and are combined with other protrusions 4 and composite protrusions 4a, as shown in FIG. 6. As a result, the grooves 3 are covered with the composite protrusions 4a, forming a tunnel shape. When multiple sets of pulsed laser L irradiations are performed, it is preferable that the second and subsequent sets of pulsed laser L irradiations be performed before the molten portion 2a formed by the first set of irradiation solidifies. This makes it easier to form deeper grooves 3 and higher protrusions 4 and composite protrusions 4a than when the molten portion 2a has solidified. However, the second and subsequent sets of pulsed laser L irradiations may be performed after the molten portion 2a formed by the first set of irradiation has solidified.
[0020] In this embodiment, the interval (irradiation interval) between the rows irradiated with the pulsed laser L is set so that the composite protrusions 4a can be formed by combining the protrusions 4 as described above. As shown in Fig. 3, the interval D between the rows irradiated with the pulsed laser L is the distance between the centers of the irradiation regions P of adjacent pulsed lasers L. For example, the interval D is 1 µm to 100 µm, and 50 µm is preferable.
[0021] The surface roughening method of this embodiment is carried out in this manner. Figures 7 and 8 are optical microscope photographs and scanning electron microscope (SEM) photographs of the joining surface 2 of the metal member 1 subjected to the surface roughening method using a pulsed laser L with the specifications shown below under the treatment conditions shown below. The number of irradiations was three: 1 set, 5 sets, and 15 sets. In Figure 7, the direction of movement of the pulsed laser L is up and down on the page, and in Figure 8, the direction of movement of the pulsed laser L is perpendicular to the page.
[0022] <Pulse laser specifications> ・Seller name and product name: OMRON "MX-Z2000G" ・Type: MOPA type fiber laser ・Average output: 20 W ・Wavelength: 1.062 nm ・Repetition frequency: 10 to 1000 kHz ・Pulse width: 7.5 nsec ・Spot diameter: Approximately 50 μm ・Travel speed: 1 to 12000 mm / sec ・Maximum energy density: Approximately 50 MW / cm2
[0023] <Processing conditions> Repetition frequency: 100 kHz Pulse width: 5 Travel speed: 100 mm / sec Irradiation interval: 50 μm Energy density: 0.11 MW / cm 2 Number of irradiations: 1 set, 5 sets, 15 sets
[0024] As shown in Figures 7 and 8, it was confirmed that grooves 3 and protrusions 4 were formed by irradiating the joining surface 2 of the metal member 1 with a pulsed laser L. It was confirmed that when the number of irradiations of the pulsed laser L was one set, the grooves 3 and protrusions 4 were formed so as to extend in the direction of movement of the pulsed laser L. It was also confirmed that when the number of irradiations of the pulsed laser L was increased to five sets or 15 sets, the joining surface 2 of the metal member 1 became rougher, and the protrusions 4 (composite protrusions 4a) crossed over the grooves 3 and merged with other protrusions 4 to extend perpendicular to the direction of movement of the pulsed laser L. It was also confirmed that as a result, the grooves 3 were covered with the composite protrusions 4a, forming a tunnel shape as shown by A in Figure 8.
[0025] After the roughening treatment method is performed in this manner, the molten resin member 11 is poured onto the joining surface 2 of the metal member 1, thereby joining the metal member 1 and the resin member 11 to form a composite body 100. Specifically, when the molten resin member 11 is poured onto the joining surface 2 of the roughened metal member 1, the resin member 11 penetrates into the grooves 3 of the metal member 1 and solidifies there. As a result, the resin member 11 is fixed so that it does not come out of the grooves 3 of the metal member 1, and the metal member 1 and the resin member 11 are joined together.
[0026] Here, in the roughening treatment method, when the pulsed laser L is simply moved and irradiated without overlapping the irradiation area P of the pulsed laser L, as shown in FIG. 4( b), the metal member 1 is simply melted, and the molten metal member 1 is removed to form grooves 3. Therefore, relatively shallow grooves 3 are formed on the joining surface 2 of the metal member 1, and protrusions 4 are not formed. In this case, the resin member 11 that has entered the grooves 3 of the metal member 1 and solidified is likely to come out of the grooves 3, and the joining strength (specifically, shear joining strength) between the metal member 1 and the resin member 11 may be insufficient.
[0027] In contrast, in the roughening treatment method of this embodiment, the molten portion 2a of the metal member 1 that has been irradiated once with the pulsed laser L is irradiated again with the pulsed laser L, thereby deforming the molten portion 2a. As a result, unlike when the pulsed laser L is simply moved and irradiated without overlapping the irradiation area P of the pulsed laser L, a deep groove portion 3 is formed and a protrusion 4 protruding from the joining surface 2 is formed. Therefore, the resin member 11 that has entered the groove portion 3 and solidified is less likely to come out of the groove portion 3, and the joining strength (shear joining strength) between the metal member 1 and the resin member 11 is improved. Furthermore, the roughening treatment method of this embodiment does not require a step of removing the molten portion 2a, thereby reducing the manufacturing cost of the composite 100.
[0028] Furthermore, in the roughening treatment method of this embodiment, the protrusions 4 formed in each of the multiple rows are combined together, thereby forming a higher composite protrusion 4a. Therefore, the resin member 11 that has entered the groove 3 and solidified is less likely to slip out of the groove 3, improving the bonding strength between the metal member 1 and the resin member 11. Furthermore, when the protrusions 4 (composite protrusions 4a) are combined beyond the groove 3, the composite protrusions 4a form a tunnel shape, covering the groove 3. Therefore, the resin member 11 that has entered the groove 3 and solidified is less likely to slip out of the groove 3 due to the tunnel-shaped composite protrusions 4a. Therefore, the bonding strength between the metal member 1 and the resin member 11 is improved. In other words, in the roughening treatment method of this embodiment, the pulsed laser L is irradiated while moving (specifically, while moving in parallel) across the multiple rows so that the protrusions 4 formed in each of the multiple rows are combined.
[0029] Furthermore, the roughening treatment method of this embodiment makes it possible to directly join the metal member 1 and the resin member 11 to form the composite member 100 without using screws, adhesives, etc., thereby improving the strength, airtightness, and design freedom of the composite member 100 and reducing the manufacturing cost of the composite member 100.
[0030] According to the above embodiment, the following advantageous effects are achieved.
[0031] In the roughening treatment method of this embodiment, the molten portion 2 a of the metal member 1, which has been irradiated once with the pulsed laser L and melted, is deformed by overlapping the irradiation area P so that the molten portion 2 a is again irradiated with the pulsed laser L. As a result, the grooves 3 are formed deep and protrusions 4 protruding from the joining surface 2 are formed, so that the resin member 11 that has entered the grooves 3 and solidified is less likely to come out of the grooves 3, and the joining strength (shear joining strength) between the metal member 1 and the resin member 11 is improved.
[0032] In the roughening treatment method of this embodiment, the protrusions 4 formed in each of the multiple rows are combined together, thereby forming higher combined protrusions 4a. Furthermore, when the protrusions 4 are combined across the grooves 3, the combined protrusions 4a make it more difficult for the resin member 11 that has entered the grooves 3 and solidified to escape from the grooves 3. This improves the bonding strength between the metal member 1 and the resin member 11.
[0033] Next, modifications of the present embodiment will be described. The following modifications are also within the scope of the present invention, and it is possible to combine the following modifications with the configurations of the above embodiment, or to combine the following modifications with each other.
[0034] <Modification 1> In the above embodiment, in the irradiation step, multiple rows of the pulsed laser L are irradiated. However, the invention is not limited to this, and in the irradiation step, only one row of the pulsed laser L may be irradiated while moving linearly. Even with this configuration, the same effects as those of the above embodiment can be achieved.
[0035] <Modification 2> In the above embodiment, in the irradiation step, when the pulsed laser L is irradiated while moving linearly, the irradiation areas P of the laser irradiated for each pulse at a constant repetition frequency are overlapped. Furthermore, in the direction of movement of the pulsed laser L, multiple overlapping areas of the irradiation areas P are formed with gaps between them. This is not a limitation, and the overlapping areas of the irradiation areas P may be formed continuously without gaps between them in the direction of movement of the pulsed laser L. Furthermore, when irradiating while moving the pulsed laser L linearly, the pulsed laser L may be irradiated so that the irradiation areas P are adjacent or separated from each other without overlapping. Even with this configuration, the surface of the metal member 1 can be roughened, and the bonding strength between the metal member 1 and the resin member 11 is improved.
[0036] <Modification 3> In the above embodiment, in the irradiation step, the pulsed laser L is irradiated while moving linearly so as to be adjacent to and spaced apart from the row that was irradiated immediately before with the pulsed laser L. This is not limiting, and in the irradiation step, the pulsed laser L may be irradiated while moving linearly so as to partially overlap with the row that was irradiated immediately before with the pulsed laser L. Furthermore, the pulsed laser L may be irradiated while moving linearly so as to be in contact with the row that was irradiated immediately before with the pulsed laser L without leaving any space.
[0037] <Modification 4> In the above embodiment, in the irradiation step, the pulsed laser L is irradiated onto the rectangular joining surfaces 2 of the metal members 1 while moving it in a linear manner. However, in the irradiation step, the pulsed laser L does not necessarily have to be irradiated onto the joining surfaces 2 of the metal members 1 while moving it in a linear manner. For example, the pulsed laser L may be irradiated onto the circular joining surfaces 2 of the metal members 1 while moving it in an arc. In other words, in the irradiation step, the moving direction of the pulsed laser L may be changed depending on the shape of the joining surfaces 2 of the metal members 1.
[0038] <Modification 5> In the above embodiment, the resin member 11 is, for example, any thermoplastic resin that can be injection molded. Here, in order to improve the bonding strength between the metal member 1 and the resin member 11, the resin member 11 may contain a filler. The filler is provided between the protrusions 4 of the metal member 1.
[0039] The configuration, operation, and effects of the embodiment of the present invention will be described below.
[0040] This roughening treatment method roughens the joining surface 2 of the metal member 1 when joining the metal member 1 and the resin member 11, and includes an irradiation step of irradiating the joining surface 2 of the metal member 1 with a pulsed laser L while moving it. In the irradiation step, the irradiation area P is overlapped so that the pulsed laser L is irradiated again to the molten portion 2a of the metal member 1, thereby forming a groove portion 3 and protrusions 4 provided on both sides of the groove portion 3 and protruding from the joining surface 2 of the metal member 1.
[0041] In this configuration, the irradiated areas P are overlapped so that the molten portion 2a of the metal member 1, which has been irradiated once with the pulsed laser L and melted, is irradiated again with the pulsed laser L, thereby deforming the molten portion 2a. As a result, unlike when the pulsed laser L is simply moved and irradiated without overlapping the irradiated areas P of the pulsed laser L, deep grooves 3 are formed and protrusions 4 protruding from the joining surface 2 are formed. Therefore, the resin member 11 that has entered the grooves 3 and solidified is less likely to come out of the grooves 3, and the joining strength between the metal member 1 and the resin member 11 is improved.
[0042] In the irradiation step of the surface roughening method, the pulse laser L is irradiated while being moved across multiple rows, so that the protrusions 4 formed in each of the multiple rows are combined with each other.
[0043] In this configuration, the combined protrusions 4a are formed higher by combining the protrusions 4 in multiple rows. Furthermore, when the protrusions 4 are combined beyond the grooves 3, the combined protrusions 4a make it difficult for the resin member 11 that has entered the grooves 3 and solidified to escape from the grooves 3. This improves the bonding strength between the metal member 1 and the resin member 11.
[0044] Although the embodiments of the present invention have been described above, the above embodiments merely illustrate some of the application examples of the present invention, and it is not intended that the technical scope of the present invention be limited to the specific configurations of the above embodiments.
[0045] This application claims priority based on Japanese Patent Application No. 2023-52804, filed with the Japan Patent Office on March 29, 2023, the entire contents of which are incorporated herein by reference.
Claims
1. A roughening method for roughening a joining surface of a metal member when joining the metal member to a resin member, comprising an irradiation step of irradiating the joining surface of the metal member with a moving pulsed laser, in which the irradiation step overlaps the irradiation area position so that the pulsed laser is irradiated again to the molten portion of the metal member, thereby forming a groove portion and protrusions on both sides of the groove portion that protrude from the joining surface of the metal member.
2. A roughening method according to claim 1, wherein in the irradiation step, a pulsed laser is irradiated while moving across multiple rows, thereby causing the protrusions formed in each of the multiple rows to be combined.
Citation Information
Patent Citations
Manufacturing method of joint structure and joint structure
JP2016144823A
Insert metallic member, metal-resin composite compact, and manufacturing method of metal-resin composite compact
JP2017056736A
Method for manufacturing metal member, and method for manufacturing metal resin joined body
JP2023059621A
Laser activation
US11325208B2