Through-via substrate, MEMS apparatus and method for manufacturing same, and laminated device

The through electrode substrate configuration with a specific insulating film structure addresses the high costs and reliability issues in MEMS device manufacturing by eliminating the need for deep drilling and allowing thicker insulating films, resulting in cost-effective and reliable MEMS devices with reduced parasitic capacitance.

WO2024204467A1PCT designated stage expired Publication Date: 2024-10-03TDK CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/012511
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-29
Filing Date
2024-03-27
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Conventional methods for manufacturing MEMS devices with through electrode substrates face high costs due to the need for good step coverage of insulating films, which is time-consuming and results in increased parasitic capacitance and electrode resistance, and require multiple etching gases for different materials, leading to high manufacturing expenses.

Method used

A through electrode substrate configuration with an insulating film having a first and second portion and an interface, allowing for reduced manufacturing costs by eliminating the need for deep drilling of the circuit portion and enabling thicker insulating films without keyhole formation, using a method that does not require atomic layer deposition, and forming the insulating film and impurity diffusion regions simultaneously with the signal processing circuit.

Benefits of technology

This configuration reduces manufacturing costs and enhances the reliability of the through electrode substrate and MEMS device by allowing thicker insulating films without keyhole formation and reducing parasitic capacitance, while increasing the number of chips per wafer, thus lowering overall production expenses.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024012511_03102024_PF_FP_ABST
    Figure JP2024012511_03102024_PF_FP_ABST
Patent Text Reader

Abstract

A through-via substrate (21) comprises: a substrate (22) having a first surface (22a) and a second surface (22b) on the side opposite to the first surface (22a) side; at least one electrode (23) extending from the first surface (22a) to the second surface (22b); and an insulating film (30) which includes a first section (31) that extends along the at least one electrode (23) and that is in contact with the at least one electrode (23), a second section (32) that extends along the first section (31) and that is adjacent to the first section (31), and an interface (30a) between the first section (31) and the second section (32).
Need to check novelty before this filing date? Find Prior Art

Description

Through-hole electrode substrate, MEMS device and manufacturing method thereof, and stacked device

[0001] The present disclosure relates to a through-hole electrode substrate, a MEMS device using the through-hole electrode substrate, a manufacturing method thereof, and a stacked device.

[0002] A known small-sized motion sensor for use in smartphones and tablet devices is a capacitive motion sensor. A known capacitive motion sensor is a MEMS device configured to change the capacitance between an electrode of a movable element and an electrode of a fixed element. The MEMS device has a structure for fixing a movable element as a weight and is configured to detect acceleration applied to the movable element.

[0003] In recent years, the incorporation of motion sensors into not only smartphones and tablet devices but also game consoles and the like has been increasing. As a result, there is a strong demand for lower prices for motion sensors, and there is a need to reduce the manufacturing cost of motion sensors. When the motion sensor is a MEMS device, one possible method for reducing the manufacturing cost is to form more chips for the MEMS device from a single wafer. The number of chips per wafer can be increased by reducing the planar area of ​​the chip. One possible method for reducing the planar area of ​​the chip is to use a through-hole electrode substrate.

[0004] In U.S. Pat. No. 6,841,453 B2, + MEMS devices are disclosed in which a through-connection region, which is a region, penetrates a silicon substrate. U.S. Patent No. 6,846,690 B2 discloses a MEMS device in which a contact pad penetrates a substrate. U.S. Patent No. 6,750,516 B2 discloses a structure in which a conductor made of a substrate material such as silicon doped with impurities penetrates a wafer.

[0005] Here, let us consider the case where a through electrode is formed in a chip including a signal processing circuit in a MEMS device. Conventionally, the through electrode has been formed by, for example, forming a signal processing circuit on the chip surface, forming multiple trenches (groove portions) in the chip surface, sequentially forming an insulating film and electrodes in the multiple trenches, polishing the back surface of the chip to expose the electrodes, forming an insulating film with contact holes on the back surface of the chip that expose the electrodes, and forming electrode pads in the contact holes. However, the conventional method has the following problems.

[0006] The insulating film in the multiple trenches requires good step coverage. Therefore, conventionally, the insulating film has been formed by, for example, atomic layer deposition (ALD). However, atomic layer deposition requires a long time to form an insulating film of a given thickness, resulting in high manufacturing costs. Furthermore, if the insulating film becomes thicker or the trench opening becomes smaller, keyholes may form in the electrode formed in the trench, resulting in high resistance of the through-electrode. On the other hand, if the insulating film is made thinner, the parasitic capacitance of the electrode increases. Furthermore, when trenches are formed after the formation of signal processing circuits, multiple etching gases must be used to simultaneously etch the silicon substrate and multiple insulating films made of different materials and formed by different methods, resulting in high manufacturing costs.

[0007] The present disclosure has been made in consideration of such problems, and its purpose is to provide a through electrode substrate that can reduce manufacturing costs, as well as a MEMS device and a stacked device that use this through electrode substrate.

[0008] The through electrode substrate of the present disclosure comprises a substrate having a first surface and a second surface opposite the first surface, at least one electrode extending from the first surface to the second surface, an insulating film including a first portion extending along and in contact with the at least one electrode, a second portion extending along and adjacent to the first portion, and an interface between the first portion and the second portion.

[0009] A MEMS device according to a first aspect of the present disclosure is a MEMS device including a movable part, a circuit part and a cap arranged to sandwich the movable part, and the circuit part is configured using the through electrode substrate according to the present disclosure.

[0010] A method for manufacturing a MEMS device according to a first aspect of the present disclosure includes a step of forming a movable portion and a cap, and a step of forming a circuit portion. The step of forming the circuit portion includes a through-hole forming step of forming at least one electrode and an insulating film on the substrate, and a circuit forming step of forming a signal processing circuit on the substrate.

[0011] A MEMS device according to a second aspect of the present disclosure includes a movable portion, and a circuit portion and a cap arranged to sandwich the movable portion. The cap is configured using the through electrode substrate according to the present disclosure.

[0012] A manufacturing method for a MEMS device according to a second aspect of the present disclosure includes the steps of forming a movable portion and a cap, and forming a circuit portion. The steps of forming the movable portion and the cap include a through-electrode formation step of forming at least one electrode and an insulating film on a substrate, a step of forming an insulating portion on the substrate, a step of forming the movable portion on the substrate and the insulating portion, and a step of removing the insulating portion by etching after forming the movable portion to form a cavity in the substrate.

[0013] The stacked device of the present disclosure includes a plurality of stacked devices, each of which is constructed using the through hole electrode substrate of the present disclosure, and at least one electrode of one of two adjacent devices among the plurality of devices is electrically connected to at least one electrode of the other adjacent device.

[0014] In the present disclosure, the through hole electrode substrate is configured so that the insulating film includes the first portion, the second portion, and the interface, thereby achieving an effect of reducing manufacturing costs.

[0015] 1 is a cross-sectional view showing a device configured using a through hole electrode substrate according to a first embodiment of the present disclosure. FIG. 1 is a cross-sectional view showing an electrode of a single structure according to the first embodiment of the present disclosure. FIG. 2 is a cross-sectional view showing an electrode of a single structure according to the first embodiment of the present disclosure. FIG. 3 is a cross-sectional view showing a plurality of electrodes of a multiplexed structure according to the first embodiment of the present disclosure. FIG. 4 is a cross-sectional view showing a step in a method for manufacturing a through hole electrode substrate according to the first embodiment of the present disclosure. FIG. 5 is a cross-sectional view showing a step subsequent to the step shown in FIG. 6. FIG. 6 is a cross-sectional view showing a step subsequent to the step shown in FIG. 7. FIG. 7 is a cross-sectional view showing a step subsequent to the step shown in FIG. 8. FIG. 8 is a cross-sectional view showing a step subsequent to the step shown in FIG. 9. FIG. 9 is a cross-sectional view showing a step subsequent to the step shown in FIG. 10. FIG. 11 is a cross-sectional view showing a step subsequent to the step shown in FIG. 12. FIG. 13 is a cross-sectional view showing a device of a comparative example. FIG. 14 is a cross-sectional view showing a step in a method for manufacturing a through hole electrode substrate according to a second embodiment of the present disclosure. FIG. 15 is a cross-sectional view showing a step subsequent to the step shown in FIG. 16. FIG. 16 is a cross-sectional view showing a step subsequent to the step shown in FIG. 17. FIG. 17 is a cross-sectional view showing a step subsequent to the step shown in FIG. 18. FIG. 18 is a cross-sectional view showing a step subsequent to the step shown in FIG. 19. 24. A cross-sectional view showing an electrode of a single structure according to a third embodiment of the present disclosure. FIG. 25. A cross-sectional view showing a step in a method for manufacturing a through hole electrode substrate according to a third embodiment of the present disclosure. FIG. 26. A cross-sectional view showing a step subsequent to the step shown in FIG. 27. FIG. 28. A cross-sectional view showing a step subsequent to the step shown in FIG. 29. A cross-sectional view showing a step subsequent to the step shown in FIG. 31. A cross-sectional view showing a step in a method for manufacturing a through hole electrode substrate according to a fifth embodiment of the present disclosure. A cross-sectional view showing a step subsequent to the step shown in FIG. 33.34 . A cross-sectional view showing a step subsequent to the step shown in FIG. 35 . A cross-sectional view showing a step subsequent to the step shown in FIG. 36 . A cross-sectional view showing a MEMS device according to a sixth embodiment of the present disclosure. A plan view showing a MEMS device according to the sixth embodiment of the present disclosure. A block diagram showing a configuration of a MEMS device according to the sixth embodiment of the present disclosure. A cross-sectional view showing a first example of a state in which a MEMS device according to the sixth embodiment of the present disclosure is mounted on a substrate. A cross-sectional view showing a second example of a state in which a MEMS device according to the sixth embodiment of the present disclosure is mounted on a substrate. A cross-sectional view showing a step in a manufacturing method of a MEMS device according to the sixth embodiment of the present disclosure. A cross-sectional view showing a step subsequent to the step shown in FIG. 43 . A cross-sectional view showing a MEMS device of a comparative example. A plan view showing a MEMS device of a comparative example. A cross-sectional view showing a step in a manufacturing method of a MEMS device according to a seventh embodiment of the present disclosure. A cross-sectional view showing a step subsequent to the step shown in FIG. 47 . A cross-sectional view showing a step subsequent to the step shown in FIG. 48 . A cross-sectional view showing a step subsequent to the step shown in FIG. 49 . A cross-sectional view showing a step subsequent to the step shown in FIG. 50 . A cross-sectional view showing a step subsequent to the step shown in FIG. 51 . FIG. 16 is a cross-sectional view showing a MEMS device according to an eighth embodiment of the present disclosure. FIG. 17 is a cross-sectional view showing a stacked device according to a ninth embodiment of the present disclosure. FIG. 18 is a cross-sectional view showing a step in a manufacturing method of a MEMS device according to a tenth embodiment of the present disclosure. FIG. 19 is a cross-sectional view showing a step subsequent to the step shown in FIG. 55. FIG. 20 is a cross-sectional view showing a step subsequent to the step shown in FIG. 56. FIG. 21 is a cross-sectional view showing a step subsequent to the step shown in FIG. 57. FIG. 22 is a cross-sectional view showing a step subsequent to the step shown in FIG. 58. FIG. 23 is a cross-sectional view showing a step subsequent to the step shown in FIG. 59. FIG. 24 is a cross-sectional view showing a step subsequent to the step shown in FIG. 60. FIG. 25 is a cross-sectional view showing a step subsequent to the step shown in FIG. 61. FIG. 26 is a cross-sectional view showing a step subsequent to the step shown in FIG. 62. FIG. 27 is a cross-sectional view showing a step subsequent to the step shown in FIG. 63. FIG. 28 is a cross-sectional view showing a step subsequent to the step shown in FIG. 64. FIG. 29 is a cross-sectional view showing a step subsequent to the step shown in FIG. 65. FIG. 29 is a cross-sectional view showing a step subsequent to the step shown in FIG. 66. FIG. 29 is a cross-sectional view showing a step subsequent to the step shown in FIG. 67. FIG. 29 is a cross-sectional view showing a step subsequent to the step shown in FIG. 68.70. A cross-sectional view showing a step subsequent to the step shown in FIG. 69. A cross-sectional view showing a step subsequent to the step shown in FIG. 70. A cross-sectional view showing a step in a modified example of the manufacturing method of a MEMS device according to the tenth embodiment of the present disclosure. A cross-sectional view showing a step subsequent to the step shown in FIG. 72. A cross-sectional view showing a step in a manufacturing method of a MEMS device according to an eleventh embodiment of the present disclosure. A cross-sectional view showing a step subsequent to the step shown in FIG. 74. A cross-sectional view showing a step subsequent to the step shown in FIG. 75. A cross-sectional view showing a step subsequent to the step shown in FIG. 76. A cross-sectional view showing a step in a manufacturing method of a MEMS device according to a twelfth embodiment of the present disclosure. A cross-sectional view showing a step subsequent to the step shown in FIG. 78. A cross-sectional view showing a step subsequent to the step shown in FIG. 79. A cross-sectional view showing a step subsequent to the step shown in FIG. 80. A cross-sectional view showing a step subsequent to the step shown in FIG. 81. A cross-sectional view showing a step subsequent to the step shown in FIG. 82. A cross-sectional view showing a step subsequent to the step shown in FIG. 83. A cross-sectional view showing a step in a manufacturing method of a MEMS device according to a thirteenth embodiment of the present disclosure. A cross-sectional view showing a step subsequent to the step shown in FIG. 85. A cross-sectional view showing a step subsequent to the step shown in FIG. 86. A cross-sectional view showing a step subsequent to the step shown in FIG. 87. A cross-sectional view showing a step subsequent to the step shown in FIG. 88. Fig. 95 is a cross-sectional view showing a step subsequent to the step shown in Fig. 89. Fig. 90 is a cross-sectional view showing a step subsequent to the step shown in Fig. 91. Fig. 92 is a cross-sectional view showing a step subsequent to the step shown in Fig. 93. Fig. 94 is a cross-sectional view showing a step subsequent to the step shown in Fig. 95. Fig. 96 is a cross-sectional view showing a MEMS device according to a fourteenth embodiment of the present disclosure.

[0016] [First Embodiment] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the drawings. First, with reference to FIG. 1, an overview of a device configured using a through hole electrode substrate according to a first embodiment of the present disclosure will be described. FIG. 1 is a cross-sectional view showing a device according to the present embodiment. A through hole electrode substrate 21 according to the present embodiment includes a substrate 22 and at least one electrode. The substrate 22 has a first surface 22a and a second surface 22b opposite to the first surface 22a. The at least one electrode extends from the first surface 22a to the second surface 22b, and substantially penetrates the substrate 22. In the present embodiment, the through hole electrode substrate 21 includes a plurality of electrodes 23 as the at least one electrode.

[0017] The through-hole electrode substrate 21 further includes an insulating film 30 that insulates the substrate 22 from the plurality of electrodes 23. The insulating film 30 is made of, for example, SiO 2 It is formed by

[0018] Here, the X direction, Y direction, and Z direction are defined as shown in FIG. 1. The X direction, Y direction, and Z direction are orthogonal to one another. In this embodiment, the Z direction is a direction perpendicular to the first surface 22a of the substrate 22 and extending from the second surface 22b toward the first surface 22a. The direction opposite the X direction is defined as the -X direction, the direction opposite the Y direction is defined as the -Y direction, and the direction opposite the Z direction is defined as the -Z direction.

[0019] Hereinafter, a position at the end of the Z direction relative to a reference position will be referred to as "above," and a position on the opposite side of the reference position from "above" will be referred to as "below." Furthermore, with regard to the components of the through-hole electrode substrate 21, the surface located at the end in the Z direction will be referred to as the "top surface," and the surface located at the end in the -Z direction will be referred to as the "bottom surface." Furthermore, the expression "when viewed from a predetermined direction (e.g., the Z direction)" means that the object is viewed from a position away from the predetermined direction or a direction parallel to the predetermined direction.

[0020] 1 shows an arbitrary device 10 configured using a through-hole electrode substrate 21. The device 10 may be, for example, a processor including a signal processing circuit, or a memory chip including a storage circuit. In the example shown in FIG. 1, the substrate 22 is a silicon substrate. The device 10 includes the substrate 22 and a circuit portion 11 formed on a first surface 22a of the substrate 22.

[0021] The circuit portion 11 includes a plurality of electrode portions 12. The plurality of electrode portions 12 are disposed above the plurality of electrodes 23 and are respectively connected to the plurality of electrodes 23. Each of the plurality of electrode portions 12 includes at least one conductive layer. When the at least one conductive layer is a plurality of conductive layers, the plurality of conductive layers may be stacked in the Z direction. The at least one conductive layer may be formed of a metal material or polysilicon.

[0022] The device 10 further includes an insulating film 13 covering the second surface 22b of the substrate 22. The insulating film 13 may be made of, for example, SiO 2 The insulating film 13 has a plurality of openings that expose the plurality of electrodes 23. The device 10 further includes a plurality of electrode pads 14 that are connected to the plurality of electrodes 23 through the plurality of openings, respectively.

[0023] Next, the configuration of the electrode 23 will be described in detail. One electrode 23 may be connected to one electrode portion 12 and one electrode pad 14. Alternatively, multiple electrodes 23 may be connected to one electrode portion 12 and one electrode pad 14. Hereinafter, a structure in which one electrode 23 is connected to one electrode portion 12 and one electrode pad 14 will be referred to as a single structure, and a structure in which multiple electrodes 23 are connected to one electrode portion 12 and one electrode pad 14 will be referred to as a multiple structure.

[0024] First, the electrode 23 having a single structure will be described with reference to Figures 2 and 3. Figures 2 and 3 are cross-sectional views showing the electrode 23 having a single structure. Figure 2 shows a cross section perpendicular to the Y direction. Figure 3 shows a cross section perpendicular to the Z direction.

[0025] In the single-type structure, an insulating film 30 is provided around one electrode 23. The insulating film 30 includes a first portion 31 extending along the electrode 23 and in contact with the electrode 23, a second portion 32 extending along the first portion 31 and adjacent to the first portion 31, and an interface 30a between the first portion 31 and the second portion 32. The first portion 31 and the second portion 32 may or may not be continuous. FIG. 2 shows an example in which the first portion 31 and the second portion 32 are continuous. As shown in FIG. 3, the electrode 23 is doubly surrounded by the first portion 31 and the second portion 32.

[0026] The insulating film 30 further includes a third portion 33 disposed on the first surface 22a of the substrate 22. The total thickness of the first portion 31 and the second portion 32 is equal to or greater than the thickness of the third portion 33. The second portion 32 and the third portion 33 may be continuous or discontinuous. Alternatively, the insulating film 30 may include a third portion 33 that is continuous with the second portion 32 and a third portion 33 that is discontinuous with the second portion 32. FIG. 2 shows the third portion 33 that is continuous with the second portion 32. In FIG. 2, the boundary between the second portion 32 and the third portion 33 is indicated by a dotted line.

[0027] 1 shows both the third portion 33 that is continuous with the second portion 32 and the third portion 33 that is not continuous with the second portion 32. The third portion 33 that is not continuous with the second portion 32 may be used as an insulating film (LOCOS) that separates the multiple CMOS circuits when multiple CMOS circuits are formed on the substrate 22, for example.

[0028] As will be described later, in this embodiment, the electrode 23 is made of silicon with impurities diffused therein, formed by doping the substrate 22 with impurities. The electrode 23 may be an N-type semiconductor with a high impurity concentration, or a P-type semiconductor with a high impurity concentration. In Figures 2 and 3, reference numeral 24 denotes a region of the impurity-diffused region of the substrate 22 that is not used as the electrode 23.

[0029] The electrode 23 has a first end 23a and a second end 23b located at opposite ends in the extension direction of the electrode 23 (a direction parallel to the Z direction). The first end 23a is located closer to the first surface 22a than the second surface 22b. The second end 23b is located closer to the second surface 22b than the first surface 22a. In the vicinity of the electrode 23, the distance between the first end 23a and the second end 23b in the extension direction of the electrode 23 is greater than the distance between the first surface 22a and the second surface 22b in the extension direction of the electrode 23. In this embodiment, the second end 23b and the second surface 22b are located at the same position in the direction parallel to the Z direction. Therefore, the first end 23a is located further in the Z direction than the first surface 22a.

[0030] In FIG. 2 , reference numerals 121 and 122 respectively denote the first and second layers of the electrode portion 12 shown in FIG. 1 . The first layer 121 contacts the first end 23 a of the electrode 23. The device 10 further includes an insulating layer 15 disposed on the third portion 33 of the insulating film 30. The insulating layer 15 has an opening exposing the top surface of the first layer 121. The second layer 122 contacts the top surface of the first layer 121 through the opening in the insulating layer 15. Note that the first layer 121 may be formed of polysilicon, and the second layer 122 may be formed of a metal material. Furthermore, the first layer 121 made of polysilicon is not an essential component and may not be provided. In this case, the second layer 122 contacts the first end 23 a of the electrode 23.

[0031] Next, the multiple electrodes 23 having a multilayer structure will be described with reference to Figures 4 and 5. Figures 4 and 5 are cross-sectional views showing the multiple electrodes 23 having a multilayer structure. Figure 4 shows a cross section perpendicular to the Y direction. Figure 5 shows a cross section perpendicular to the Z direction.

[0032] In the multilayer structure, an insulating film 30 is provided around each of the multiple electrodes 23. In the example shown in FIGS. 4 and 5 , the multiple electrodes 23 include a first electrode 23A located in the center, a second electrode 23B arranged to surround the first electrode 23A, and a third electrode 23C arranged to surround the second electrode 23B. The first electrode 23A has a columnar shape. The second and third electrodes 23B and 23C each have a cylindrical shape. In the example shown in FIGS. 4 and 5 , the first electrode 23A has a cylindrical shape. The second and third electrodes 23B and 23C each have a cylindrical shape.

[0033] Between the first electrode 23A and the second electrode 23B, there are two portions of the insulating film 30 and an interface 30a. When the first electrode 23A is used as a reference, of the two portions of the insulating film 30, the portion that contacts the first electrode 23A corresponds to the "first portion of the insulating film" in the present disclosure, and the portion that does not contact the first electrode 23A corresponds to the "second portion of the insulating film" in the present disclosure. When the second electrode 23B is used as a reference, of the two portions of the insulating film 30, the portion that contacts the second electrode 23B corresponds to the "first portion of the insulating film" in the present disclosure, and the portion that does not contact the second electrode 23B corresponds to the "second portion of the insulating film" in the present disclosure.

[0034] Similarly, two portions of the insulating film 30 and an interface 30a exist between the second electrode 23B and the third electrode 23C. When the second electrode 23B is used as a reference, of the two portions of the insulating film 30, the portion that contacts the second electrode 23B corresponds to the "first portion of the insulating film" in the present disclosure, and the portion that does not contact the second electrode 23B corresponds to the "second portion of the insulating film" in the present disclosure. When the third electrode 23C is used as a reference, of the two portions of the insulating film 30, the portion that contacts the third electrode 23C corresponds to the "first portion of the insulating film" in the present disclosure, and the portion that does not contact the third electrode 23C corresponds to the "second portion of the insulating film" in the present disclosure.

[0035] A first portion 31 of the insulating film 30 contacts the outer periphery of the third electrode 23C, this first portion 31 contacts a second portion 32 of the insulating film 30, and this second portion 32 is continuous with a third portion 33.

[0036] The first layer 121 of the electrode section 12 is in contact with the upper surfaces of the first to third electrodes 23A to 23C, respectively. The electrode pads 14 are in contact with the lower surfaces of the first to third electrodes 23A to 23C, respectively.

[0037] The multiplexed structure is not limited to the examples shown in Figures 4 and 5. For example, the multiplexed structure may be a structure in which a plurality of electrodes 23 having the single structure shown in Figures 2 and 3 are provided. In this case, the first layer 121 of the electrode section 12 contacts the upper surface of each of the plurality of electrodes 23, and the electrode pad 14 contacts the lower surface of each of the plurality of electrodes 23.

[0038] Next, a method for manufacturing the through electrode substrate 21 according to this embodiment will be described with reference to Figures 6 to 14. Figures 6 to 14 are cross-sectional views showing a stack in the manufacturing process of the through electrode substrate 21. Here, an example will be described in which the device 10 shown in Figure 1 is constructed using the through electrode substrate 21. Also, an example will be described in which a single-structure electrode 23 shown in Figures 2 and 3 and a plurality of multi-structure electrodes 23 shown in Figures 4 and 5 are formed. In the following description, it is assumed that the substrate 22 is a silicon substrate.

[0039] In the manufacturing method of the through-hole electrode substrate 21, first, as shown in FIG. 6, a silicon nitride film, for example, is formed on the first surface 22a of the substrate 22. 3 N 4 The insulating film 62 is formed from SiO. The thickness of the insulating film 62 is, for example, in the range of 100 nm to 200 nm. Before forming the insulating film 62, a buffer film (not shown) may be formed. The buffer film is made of SiO 2 The buffer film may be an oxide film made of the material of the present invention. The thickness of the buffer film is, for example, in the range of 10 nm to 20 nm.

[0040] 7 shows the next step. In this step, a photoresist mask 63 is first formed on the insulating film 62. Next, the insulating film 62 is selectively etched using the photoresist mask 63, for example, by reactive ion etching (hereinafter referred to as RIE). Next, using the insulating film 62 and the photoresist mask 63 as an etching mask, the substrate 22 is deeply etched to form multiple trenches 25. The multiple trenches 25 are formed from the first surface 22a of the substrate 22 toward the interior of the substrate 22. For example, the Bosch process can be used to deeply etch the substrate 22. The multiple trenches 25 have shapes corresponding to the first and second portions 31 and 32 of the insulating film 30 to be formed later.

[0041] 8 shows the next step. In this step, the photoresist mask 63 is first removed. Next, impurities are diffused into the substrate 22 from the wall surfaces and bottom surfaces of the plurality of trenches 25, thereby forming impurity diffusion regions 24 in the substrate 22, which will later become the plurality of electrodes 23. Note that FIG. 8 shows the stacked body in the middle of forming the impurity diffusion regions 24.

[0042] 9 shows the next step. In this step, first, the insulating film 62 is selectively removed except for the portion above the region where the plurality of electrodes 23 will be formed later. Next, the insulating film 30 is formed on the portion of the substrate 22 that is not covered by the insulating film 62. The insulating film 30 is formed so as to completely fill the plurality of trenches 25. The thickness of the insulating film 30 is, for example, in the range of 500 nm to 1500 nm. The insulating film 30 is formed, for example, by a SiO 2 film formed by thermal oxidation. 2 In this case, the substrate 22 is oxidized from the wall surface and bottom surface of each of the plurality of trenches 25, and a SiO 2 The oxidation temperature is, for example, in the range of 1000°C to 1100°C.

[0043] In each of the plurality of trenches 25, an insulating film 30 is formed on one wall surface of the trench 25 and the other wall surface opposite to the one wall surface. An interface 30a is formed between the insulating film formed on one wall surface and the insulating film 30 formed on the other wall surface. The insulating film formed on one wall surface corresponds to the "first portion of the insulating film" in this disclosure, and the insulating film formed on the other wall surface corresponds to the "second portion of the insulating film" in this disclosure.

[0044] Furthermore, a third portion 33 of the insulating film 30 is formed on the first surface 22a of the substrate 22. The insulating film 30 may include a third portion 33 that is continuous with the second portion 32 and a third portion 33 that is not continuous with the second portion 32. As described above, the third portion 33 that is not continuous with the second portion 32 may be used as an insulating film (LOCOS) that separates the multiple CMOS circuits when multiple CMOS circuits are formed on the substrate 22. In this case, in the step shown in FIG. 9 , the insulating film 30 that completely fills the multiple trenches and the insulating film that separates the multiple CMOS circuits may be formed simultaneously.

[0045] 10 shows the next step, in which the insulating film 62 is selectively removed to expose the impurity diffusion region 24. By selectively removing the insulating film 62, contact holes are formed in the stack to connect the electrode portion 12 (see FIG. 1) to the impurity diffusion region 24.

[0046] 11 shows the next step. In this step, first, a first layer 121 of the electrode portion 12 is formed on the impurity diffusion region 24. Next, an insulating layer 15 having an opening that exposes the top surface of the first layer 121 is formed on the insulating film 30. Next, as shown in FIG. 12, a second layer 122 of the electrode portion 12 is formed on the first layer 121.

[0047] Although not shown, after the process shown in FIG. 11, a process for forming the circuit portion 11 (see FIG. 1) of the device 10 is carried out.

[0048] 13 shows the next step. In this step, the substrate 22 is polished so that the impurity diffusion regions 24 become a plurality of electrodes 23. The substrate 22 is polished from the polished surface side opposite the first surface 22a of the substrate 22, and is polished until the insulating film 30 and the impurity diffusion regions 24 formed in the plurality of trenches 25 are exposed. The polished surface after polishing becomes the second surface 22b of the substrate 22. Parts of the impurity diffusion regions 24 that remain after polishing become a plurality of electrodes 23. In this way, the through-hole electrode substrate 21 is completed.

[0049] 14 shows the next step. In this step, an insulating film 13 having a plurality of openings that expose a plurality of electrodes 23 is formed on the second surface 22b of the substrate 22. Thereafter, the electrode pads 14 and the like shown in FIG. 1 are formed, thereby completing the device 10.

[0050] Next, the operation and effect of the through electrode substrate 21 according to this embodiment will be described. According to this embodiment, by configuring the device 10 using the through electrode substrate 21, it is possible to reduce the manufacturing cost of the device 10. Below, this effect will be described in comparison with the device 110 of the comparative example.

[0051] First, the configuration of a device 110 of the comparative example will be described with reference to FIG. 15 . FIG. 15 is a cross-sectional view showing the device 110 of the comparative example. The device 110 of the comparative example includes a circuit portion 111 and a substrate 112. The substrate 112 has a first surface 112a and a second surface 112b opposite to the first surface 112a. The circuit portion 111 is formed on the substrate 112 and the first surface 112a of the substrate 112. Note that in FIG. 15 , the circuit portion 111 is depicted in a simplified form compared to the circuit portion 11 shown in FIG. 1 .

[0052] Device 110 further includes a plurality of through holes 125 that penetrate circuit portion 111 and substrate 112, a plurality of electrodes 123 formed in each of through holes 125, and an insulating film 130 that provides insulation between the plurality of electrodes 123 and circuit portion 111 and substrate 112. In particular, in the comparative example, each of the plurality of electrodes 123 extends from the upper surface of device 110 to the lower surface of device 110.

[0053] The device 110 further includes an insulating film 113 covering the second surface 112b of the substrate 112. The insulating film 113 has a plurality of openings that respectively expose the plurality of electrodes 123. The device 110 further includes a plurality of electrode pads 114 connected to the lower surfaces of the plurality of electrodes 123 through the respective openings, and a plurality of electrode pads 115 connected to the upper surfaces of the plurality of electrodes 123.

[0054] Next, a brief description will be given of a manufacturing method for the device 110 of the comparative example. First, the circuit portion 111 is formed on the substrate 112 and the first surface 112a of the substrate 112. Next, the circuit portion 111 and the substrate 112 are deeply etched to form multiple trenches. The deep etching of the circuit portion 111 and the substrate 112 is performed using, for example, the Bosch process. The multiple trenches have shapes corresponding to the multiple electrodes 123 that will be formed later.

[0055] Next, an insulating film 130 is formed so as to cover the upper surface of the circuit portion 111 and the wall and bottom surfaces of each of the plurality of trenches. Next, an electrode material layer that will later become the plurality of electrodes 123 is formed so as to fill the plurality of trenches. Next, the portions of the electrode material layer other than those formed in the plurality of trenches are removed. Next, a plurality of electrode pads 115 are formed on the upper surface of the electrode material layer.

[0056] Next, the substrate 112 is polished until the electrode material layer formed in the plurality of trenches is exposed. The substrate 112 is polished from the polished surface side opposite the first surface 112a of the substrate 112. The polished surface becomes the second surface 112b of the substrate 112, and the plurality of trenches become the plurality of through holes 125. The portions of the electrode material layer that remain after polishing become the plurality of electrodes 123.

[0057] Next, an insulating film 113 having a plurality of openings that expose the plurality of electrodes 123 is formed on the second surface 112b of the substrate 112. Next, a plurality of electrode pads 114 are formed. In this way, the device 110 is completed.

[0058] Problems with the manufacturing method of the device 110 of the comparative example will be described below. In the comparative example, the insulating film 130 needs to be formed in the multiple trenches so as to leave spaces for the multiple electrodes 123, and therefore the insulating film 130 in the multiple trenches is required to have good step coverage. For this reason, the insulating film 130 is formed by, for example, atomic layer deposition (ALD). However, atomic layer deposition requires a long time to form the insulating film 130 of a predetermined thickness, resulting in high manufacturing costs.

[0059] Furthermore, if the insulating film 130 becomes thicker or the trench opening becomes smaller, a keyhole may occur in the electrode material layer formed in the trench. In Figure 15, reference numeral 126 indicates a keyhole. If such a keyhole 126 occurs, the resistance of the electrode 123 increases. On the other hand, if the insulating film 130 is made thinner, the parasitic capacitance of the electrode 123 increases.

[0060] Furthermore, the circuit portion 111 includes a plurality of insulating films made of different materials and formed by different methods, and therefore, when deep etching the circuit portion 111 and the substrate 112, multiple etching gases must be used to simultaneously etch the multiple insulating films and the silicon substrate, which increases manufacturing costs.

[0061] In contrast, in the present embodiment, there is no need to form the insulating film 30 so as to leave spaces for forming the plurality of electrodes 23, and therefore the insulating film 30 can be formed by a method with lower manufacturing costs than atomic layer deposition. Furthermore, in the present embodiment, the insulating film 30 and the impurity diffusion regions 24 that will later become the plurality of electrodes 23 are formed before the circuit portion 11 is formed. Therefore, in the present embodiment, the through-hole electrode substrate 21 can be formed without deep-drilling the circuit portion 11. Furthermore, in the present embodiment, the impurity diffusion regions 24 and the insulating film 30 can be formed while the process of forming the circuit portion 11 is being performed. For these reasons, the present embodiment allows for a reduction in the manufacturing cost of the device 10.

[0062] Furthermore, in this embodiment, there is no need to form the insulating film 30 so as to leave spaces for forming the plurality of electrodes 23, and therefore the insulating film 30 can be made thicker and there is no risk of keyholes being formed in the plurality of electrodes 23. As a result, according to this embodiment, a highly reliable through electrode substrate 21 and device 10 can be realized.

[0063] Second Embodiment Next, a method for manufacturing a through hole electrode substrate 21 according to a second embodiment of the present disclosure will be described. The method for manufacturing a through hole electrode substrate 21 according to this embodiment differs from the first embodiment in the timing at which the plurality of trenches 25 are formed.

[0064] A method for manufacturing the through electrode substrate 21 according to this embodiment will be described below with reference to Figures 16 to 20. Figures 16 to 20 are cross-sectional views showing a stack in the process of manufacturing the through electrode substrate 21. Note that, among the components of the through electrode substrate 21 according to this embodiment, the same components as those of the through electrode substrate 21 according to the first embodiment will be designated by the same reference numerals as those in the first embodiment.

[0065] 16 , in the manufacturing method of the through electrode substrate 21, first, impurities are diffused into the substrate 22 from the first surface 22 a of the substrate 22 to form an impurity diffusion region 24 in the substrate 22. Note that, when a plurality of CMOS circuits are formed in the substrate 22, the impurity diffusion region 24 may be formed simultaneously with the impurity diffusion regions used for the plurality of CMOS circuits.

[0066] 17 shows the next step. In this step, a buffer film 61 is formed on the first surface 22a of the substrate 22. The buffer film 61 is made of SiO 2 The buffer film 61 may be an oxide film made of the material of the present invention. The thickness of the buffer film 61 is, for example, in the range of 10 nm to 20 nm. Next, an insulating film 62 is formed on the buffer film 61.

[0067] 18 shows the next step, in which the buffer film 61 and the insulating film 62 are selectively etched by, for example, RIE using a photoresist mask (not shown) as an etching mask so that the buffer film 61 and the insulating film 62 remain on the impurity diffusion region 24.

[0068] 19 shows the next step. In this step, first, the substrate 22 is deeply etched using the buffer film 61, the insulating film 62, and a photoresist mask (not shown) as an etching mask to form a plurality of trenches 25. The plurality of trenches 25 are formed around the impurity diffusion region 24. Next, the photoresist mask (not shown) is removed.

[0069] 20 shows the next step. In this step, an insulating film 30 is formed on the portion of the substrate 22 that is not covered by the insulating film 62. The insulating film 30 is formed so as to completely fill the plurality of trenches 25. The subsequent steps are the same as those in the first embodiment.

[0070] Other configurations, actions, and effects of this embodiment are the same as those of the first embodiment.

[0071] [Third Embodiment] Next, a third embodiment of the present disclosure will be described. A through hole electrode substrate 21 according to this embodiment includes a plurality of electrodes 27 instead of the plurality of electrodes 23 in the first embodiment. The plurality of electrodes 27 are formed of a metal material. Furthermore, in this embodiment, the impurity diffusion region 24 in the first embodiment is not provided. Other configurations of the through hole electrode substrate 21 according to this embodiment are the same as those in the first embodiment.

[0072] Next, a detailed description will be given of the electrodes 27. As in the first embodiment, the plurality of electrodes 27 can be classified into electrodes 27 of a single structure and electrodes 27 of a multiple structure.

[0073] First, an electrode 27 having a single structure will be described with reference to FIG. 21 . FIG. 21 is a cross-sectional view showing the electrode 27 having a single structure. The electrode 27 includes a first layer 271 and a second layer 272. In the single structure, the second layer 272 extends from the first surface 22 a of the substrate 22 to the second surface 22 b of the substrate 22. The first layer 271 is interposed between the second layer 272 and the first portion 31 of the insulating film 30, and between the second layer 272 and the first layer 121 of the electrode portion 12. The lower surface of the second layer 272 is in contact with the electrode pad 14. The materials of the first layer 271 and the second layer 272 will be described later.

[0074] The electrode 27 has a first end 27a and a second end 27b located at opposite ends in the extension direction of the electrode 27 (a direction parallel to the Z direction). The first end 27a is located closer to the first surface 22a than the second surface 22b. The second end 27b is located closer to the second surface 22b than the first surface 22a. In the vicinity of the electrode 27, the distance between the first end 27a and the second end 27b in the extension direction of the electrode 27 is greater than the distance between the first surface 22a and the second surface 22b in the extension direction of the electrode 27. In this embodiment, the second end 27b and the second surface 22b are located at the same position in the direction parallel to the Z direction. Therefore, the first end 27a is located further in the Z direction than the first surface 22a.

[0075] Next, an electrode 27 having a multilayer structure will be described with reference to FIG. 22 . FIG. 27 is a cross-sectional view showing the electrode 27 having a multilayer structure. In the multilayer structure, the electrode 27 includes multiple electrode portions. In the example shown in FIG. 22 , the electrode 27 includes a first electrode portion 27A located in the center, a second electrode portion 27B arranged to surround the first electrode portion 27A, and a third electrode portion 27C arranged to surround the second electrode portion 27B. The first electrode portion 27A has a columnar shape. The second and third electrode portions 27B and 27C each have a cylindrical shape.

[0076] Between the first electrode portion 27A and the second electrode portion 27B, there exists an interface 30a with two portions of the insulating film 30. The relationship between the first and second electrode portions 27A, 27B and the two portions of the insulating film 30 is similar to the relationship between the first and second electrodes 23A, 23B and the two portions of the insulating film 30 in the first embodiment.

[0077] Similarly, between the second electrode portion 27B and the third electrode portion 27C, there is an interface 30a with two portions of the insulating film 30. The relationship between the second and third electrode portions 27B, 27C and the two portions of the insulating film 30 is similar to the relationship between the second and third electrodes 23B, 23C and the two portions of the insulating film 30 in the first embodiment.

[0078] The outer periphery of the third electrode portion 27C is in contact with a first portion 31 of the insulating film 30, this first portion 31 is in contact with a second portion 32 of the insulating film 30, and this second portion 32 is continuous with a third portion 33.

[0079] Like the single-structure electrode 27, the multi-layered electrode 27 includes a first layer 271 and a second layer 272, and has a first end 27a and a second end 27b. Each of the first to third electrode portions 27A to 27C is composed of a part of the first layer 271 and a part of the second layer 272. The first to third electrode portions 27A to 27C may be connected to another part of the second layer 272 near the second end 27b.

[0080] Next, a method for manufacturing the through electrode substrate 21 according to this embodiment will be described with reference to Figures 23 to 30. Figures 23 to 30 are cross-sectional views showing a stack in the manufacturing process of the through electrode substrate 21. As with the first embodiment, the following description will be given taking as an example a case where the device 10 shown in Figure 1 is constructed using the through electrode substrate 21. The following description will also be given taking as an example a case where the single-structure electrode 27 shown in Figure 21 and the multi-structure electrode 27 shown in Figure 22 are formed.

[0081] The method for manufacturing the through hole electrode substrate 21 in this embodiment is the same as that in the first embodiment up to the step of forming the plurality of trenches 25. Fig. 23 shows the stacked body after the plurality of trenches 25 have been formed.

[0082] 24 shows the next step. In this step, first, the insulating film 62 is selectively removed except for the portion above the region where the plurality of electrodes 27 will be formed later. Next, the insulating film 30 is formed on the portion of the substrate 22 that is not covered by the insulating film 62. The insulating film 30 is formed so as to completely fill the plurality of trenches 25. The method of forming the insulating film 30 is the same as in the first embodiment.

[0083] 25 shows the next step, in which the insulating film 62 is selectively removed so that the regions where the electrodes 27 will be formed later are exposed from the insulating film 30.

[0084] 26 shows the next step. In this step, first, a first layer 121 of the electrode portion 12 is formed on the substrate 22. Next, an insulating layer 15 having an opening that exposes the top surface of the first layer 121 is formed on the insulating film 30. Next, as shown in FIG. 27, a second layer 122 of the electrode portion 12 is formed on the first layer 121.

[0085] Although not shown, after the step shown in FIG. 27, a step of forming the circuit portion 11 (see FIG. 1) of the device 10 is carried out.

[0086] 28 shows the next step. In this step, the substrate 22 is polished until the insulating film 30 formed in the plurality of trenches 25 is exposed. The substrate 22 is polished from the surface to be polished opposite the first surface 22a of the substrate 22. After polishing, the surface to be polished becomes the second surface 22b of the substrate 22.

[0087] 29 shows the next step. In this step, first, an insulating film 13 is formed on the second surface 22b of the substrate 22. Next, a photoresist mask 64 is formed on the insulating film 13. Next, using the photoresist mask 64 as an etching mask, the insulating film 13 and the substrate 22 are etched by, for example, RIE. This etching is continued until a plurality of through-holes 69 are formed in the substrate 22 and the first layer 121 of the electrode portion 12 is exposed. In this etching, the insulating film 30 functions as an etching stopper. Therefore, in this etching, the substrate 22 can be etched without using deep etching such as the Bosch process.

[0088] FIG. 30 shows the next step. In this step, the photoresist mask 64 is first removed. Next, a step of forming multiple electrodes 27 in the multiple through holes 69 is performed. In this step, a first layer 271 is first formed in the multiple through holes 69. The first layer 271 is also formed on the insulating film 13. The first layer 271 is formed, for example, by electroless plating. Examples of materials for the first layer 271 include Ni, Cu, and Au. Next, a second layer 272 is formed on the first layer 271. The second layer 272 is formed, for example, by electrolytic plating. The first layer 271 is used as an electrode and a seed layer when the second layer 272 is formed by electrolytic plating. Examples of materials for the second layer 272 include Ni, NiFe, Fe, W, Ta, and Cu. Next, the first layer 271 and the second layer 272 are polished until the insulating film 13 is exposed. This completes the formation of the multiple electrodes 27. Thereafter, electrode pads 14 and the like are formed, and the device 10 is completed.

[0089] Other configurations, actions, and effects of this embodiment are the same as those of the first embodiment.

[0090] [Fourth embodiment] Next, a fourth embodiment of the present disclosure will be described. A through hole electrode substrate 21 according to this embodiment includes a plurality of electrodes 27 according to the third embodiment, instead of the plurality of electrodes 23 according to the first embodiment. Furthermore, unlike the third embodiment, this embodiment includes the impurity diffusion region 24 according to the first embodiment. The other configurations of the through hole electrode substrate 21 according to this embodiment are the same as those of the first and third embodiments.

[0091] A method for manufacturing a through hole electrode substrate 21 according to this embodiment will be described below with reference to Figures 31 and 32. Figures 31 and 32 are cross-sectional views showing a stack in the process of manufacturing the through hole electrode substrate 21. Here, as in the first embodiment, an example will be described in which the device 10 shown in Figure 1 is configured using the through hole electrode substrate 21.

[0092] The manufacturing method of the through hole electrode substrate 21 according to this embodiment is the same as that of the first embodiment up to the step of polishing the substrate 22. Figure 31 shows the next step. In this step, first, an insulating film 13 is formed on the second surface 22b of the substrate 22. Next, a photoresist mask 65 is formed on the insulating film 13. Next, using the photoresist mask 65 as an etching mask, the insulating film 13 and the impurity diffusion region 24 are etched by, for example, RIE. This etching is performed until the first layer 121 of the electrode portion 12 is exposed.

[0093] 32 shows the next step. In this step, first, the photoresist mask 65 is removed. Next, a first layer 271 and a second layer 272 are formed in this order. The method of forming the first layer 271 and the second layer 272 is the same as in the third embodiment. Next, the first layer 271 and the second layer 272 are polished until the insulating film 13 is exposed. This completes the formation of multiple electrodes 27. Thereafter, electrode pads 14 and the like are formed, thereby completing the device 10.

[0094] Other configurations, actions, and effects of this embodiment are the same as those of the first or third embodiment.

[0095] Fifth Embodiment Next, a fifth embodiment of the present disclosure will be described. The manufacturing method of the through electrode substrate 21 according to this embodiment differs from the third embodiment in the following respects. In this embodiment, the insulating film 30 is formed so as not to completely fill the plurality of trenches 25. Therefore, in this embodiment, the interface 30a is not formed in the insulating film 30.

[0096] A method for manufacturing a through electrode substrate 21 according to this embodiment will be described below with reference to Figures 33 to 37. Figures 33 to 37 are cross-sectional views showing a stack in the manufacturing process of the through electrode substrate 21. As with the first embodiment, the description will be given here taking as an example a case where the device 10 shown in Figure 1 is configured using a through electrode substrate 21. For convenience, several components are omitted from Figures 33 to 37.

[0097] The manufacturing method of the through electrode substrate 21 according to this embodiment is the same as that of the third embodiment up to the step of forming the plurality of trenches 25. Figure 33 shows the next step. In this step, an insulating film 30 is formed. The insulating film 30 is formed so as not to fill the plurality of trenches 25.

[0098] 34 shows the next step. In this step, a silicon film 66 made of polysilicon or amorphous silicon is formed on the surface of the insulating film 30. The silicon film 66 is formed so as to seal the openings of the plurality of trenches 25. Note that the silicon film 66 may be formed so as not to completely fill the plurality of trenches 25.

[0099] 35 shows the next step. In this step, first, the silicon film 66 is polished until the insulating film 30 is exposed. Next, the first layer 121 of the electrode portion 12 is formed on the silicon film 66.

[0100] 36 shows the next step. In this step, the substrate 22 is polished until the silicon film 66 formed in the plurality of trenches 25 is exposed. The substrate 22 is polished from the surface to be polished opposite the first surface 22a of the substrate 22. After polishing, the surface to be polished becomes the second surface 22b of the substrate 22.

[0101] 37 shows the next step. In this step, first, an insulating film 13 is formed on the second surface 22b of the substrate 22. Next, a photoresist mask 67 is formed on the insulating film 13. Next, using the photoresist mask 67 as an etching mask, the insulating film 13 and the silicon film 66 are etched by, for example, RIE. This etching is performed until the first layer 121 of the electrode portion 12 is exposed. Next, the photoresist mask 67 is removed. The subsequent steps are the same as those in the third embodiment.

[0102] In this embodiment, an interface 30a is not formed in the insulating film 30. That is, in this embodiment, during the manufacturing process of the through electrode substrate 21, a part of the insulating film grown from one wall surface of the trench 25 and another part of the insulating film 30 grown from the other wall surface do not press against each other. As a result, this embodiment can suppress the generation of unnecessary stress in the substrate 22. As a result, this embodiment can suppress the generation of defects in the substrate 22 due to stress.

[0103] Other configurations, actions, and effects of this embodiment are the same as those of the third embodiment.

[0104] Sixth Embodiment Next, a MEMS device according to a sixth embodiment of the present disclosure will be described. The MEMS device 100 according to this embodiment is configured using the through electrode substrate 21 according to the first or second embodiment.

[0105] The MEMS device 100 may be a microphone, a pressure sensor, or a motion sensor. The configuration of the MEMS device 100 will be described below using an example in which the MEMS device 100 is a capacitive motion sensor. FIG. 38 is a cross-sectional view showing the MEMS device 100. FIG. 38 shows an example in which the MEMS device 100 is configured using the through electrode substrate 21 according to the first embodiment. FIG. 39 is a plan view showing the MEMS device 100. FIG. 40 is a block diagram showing the configuration of the MEMS device 100.

[0106] The MEMS device 100 includes a movable part 101, a circuit part 102, and a cap 103 arranged to sandwich the movable part 101. The movable part 101 includes a movable element 101a as a weight, a structure for fixing the movable element 101a, and an electrode provided on the lower surface of the movable element 101a. Hereinafter, the electrode provided on the movable element 101a will be referred to as the movable electrode. Note that the movable electrode is omitted in FIG. 38. The portion of the movable part 101 excluding the movable electrode is formed of, for example, a silicon substrate, polysilicon, epi-polysilicon, etc.

[0107] The circuit section 102 is configured using the through electrode substrate 21, and corresponds to the device 10 in the first embodiment. In the following description, the components of the circuit section 102 that are common to the device 10 will be designated by the same reference numerals as the components of the device 10.

[0108] The movable portion 101 is disposed on a first surface 22a of the substrate 22 of the through electrode substrate 21. The MEMS device 100 further includes a plurality of electrode portions 107 that connect the movable portion 101 and the circuit portion 102.

[0109] The circuit section 102 includes a fixed electrode 104a formed on the first surface 22a of the substrate 22 of the through electrode substrate 21, and a processor 105 which is a signal processing circuit formed on the substrate 22 of the through electrode substrate 21 and the first surface 22a of the substrate 22.

[0110] The movable electrode and the fixed electrode 104a constitute a sensor unit 104. When the position of the movable element 101a changes, the distance between the movable electrode and the fixed electrode 104a changes, and as a result, the capacitance between the movable electrode and the fixed electrode 104a changes. The processor 105 is configured to detect the change in capacitance and generate a detection value corresponding to the capacitance. The detection value may be a capacitance value, or may be an acceleration or angular velocity. The processor 105 is also configured to output the generated detection value to an external processor 106.

[0111] The cap 103 is used to seal the internal structure of the MEMS device 100, such as the movable element 101a and the fixed electrode 104a. The cap 103 has a cavity 103a of a predetermined shape. The movable element 101a is located in a space including the cavity 103a, which is surrounded by the circuit unit 102 and the cap 103. The movable element 101a is configured to be movable within the space including the cavity 103a. The cap 103 is formed of, for example, a silicon substrate.

[0112] Figure 39 shows the MEMS device 100 as viewed from the second surface 22b side of the substrate 22. Note that Figure 39 also shows some of the multiple electrode pads 14. The planar shape of the cap 103 (as viewed from the Z direction) is the same as or approximately the same as the planar shape of the movable part 101. The planar shape of the circuit part 102 may be the same as the planar shapes of the movable part 101 and the cap 103, or may be slightly larger than the planar shapes of the movable part 101 and the cap 103. When viewed from the Z direction, the multiple electrode pads 14 are arranged at positions that overlap the movable part 101 and the cap 103.

[0113] Next, first and second examples of mounting the MEMS device 100 on a mountable body will be described. First, the first example will be described with reference to FIG. 41 . FIG. 41 is a cross-sectional view showing a first example of a state in which the MEMS device 100 is mounted on a mountable body 200. The mountable body 200 is, for example, a mounting substrate. The mountable body 200 has a first surface 200 a and a second surface 200 b opposite to the first surface 200 a, and includes a plurality of wiring layers 201 formed on the first surface 200 a.

[0114] In the first example, the MEMS device 100 is fixed to the object 200 such that the circuit section 102 is fixed to the object 200. That is, the MEMS device 100 is fixed to the object 200 with the second surface 22b of the substrate 22 facing the first surface 200a of the object 200. The plurality of electrode pads 14 are directly connected to the plurality of wiring layers 201.

[0115] Next, a second example will be described with reference to Fig. 42. Fig. 42 is a cross-sectional view showing a second example of a state in which the MEMS device 100 is mounted on the object 200. In the second example, the MEMS device 100 is fixed to the object 200 such that the cap 103 is fixed to the object 200. That is, the MEMS device 100 is fixed to the object 200 with the first surface 22a of the substrate 22 facing the first surface 200a of the object 200. The plurality of electrode pads 14 are connected to the plurality of wiring layers 201 via, for example, a plurality of bonding wires 202.

[0116] Next, a description will be given of a method for manufacturing the MEMS device 100 according to this embodiment. The method for manufacturing the MEMS device 100 includes a step of forming the movable portion 101 and the cap 103, and a step of forming the circuit portion 102.

[0117] The process of forming the movable part 101 and the cap 103 includes the steps of forming an insulating part on a cap substrate that will later become the cap 103, forming the movable part 101 on the cap substrate and the insulating part, and, after forming the movable part 101, removing the insulating part by etching to form the cavity 103a. The insulating part is, for example, an insulating layer made of phosphosilicate glass and a SiO 2 In this case, the insulating portion is removed by, for example, a buffered oxide etchant (BOE).

[0118] The process of forming the circuit portion 102 includes a through-hole electrode forming process for forming at least one electrode and an insulating film 30 in the substrate 22, and a circuit forming process for forming a processor 105, which is a signal processing circuit, in the substrate 22. The through-hole electrode forming process is substantially the same as the manufacturing method of the through-hole electrode substrate 21 described in the first embodiment. That is, the through-hole electrode forming process includes a process of forming multiple trenches 25 from the first surface 22a of the substrate 22 toward the interior of the substrate 22, a process of diffusing impurities into the substrate 22 from the wall surfaces and bottom surfaces of the multiple trenches 25 to form impurity diffusion regions 24, a process of forming an insulating film 30 in the multiple trenches 25, and a polishing process of polishing the surface of the substrate 22 opposite the first surface 22a (the surface to be polished) so that the impurity diffusion regions 24 become multiple electrodes 23. The polishing process is performed until the insulating film 30 and the impurity diffusion regions 24 are exposed. The polishing process is also performed after the circuit forming process.

[0119] Here, the circuit unit 102 before the polishing step is performed is referred to as the initial circuit unit 102P. The steps after the polishing step may be performed in a state where the movable unit 101 and the cap 103 are fixed to the initial circuit unit 102P. Hereinafter, with reference to Figures 43 and 44, the steps after the polishing step that are performed in a state where the movable unit 101 and the cap 103 are fixed to the initial circuit unit 102P will be described. Figures 43 and 44 are cross-sectional views showing the stacked body in the manufacturing process of the MEMS device 100.

[0120] 43 shows a state in which the movable part 101 and the cap 103 are fixed to the initial circuit part 102P. The movable part 101 and the cap 103 are fixed to the initial circuit part 102P immediately before the polishing step. The movable part 101 and the cap 103 may be fixed to the initial circuit part 102P by, for example, eutectic bonding.

[0121] FIG. 44 shows the next step. In this step, the substrate 22 is first polished, similarly to the step shown in FIG. 13 of the first embodiment. The substrate 22 is polished from the polished surface opposite the first surface 22a of the substrate 22 until the insulating film 30 and the impurity diffusion regions 24 formed in the trenches 25 are exposed. The polished surface becomes the second surface 22b of the substrate 22. Portions of the impurity diffusion regions 24 remaining after polishing become the electrodes 23. Next, an insulating film 13 having a plurality of openings that expose the electrodes 23 is formed on the second surface 22b of the substrate 22. Thereafter, the electrode pads 14 and the like shown in FIG. 1 are formed, thereby completing the MEMS device 100.

[0122] Next, the operation and effect of the MEMS device 100 according to this embodiment will be described. In this embodiment, the circuit section 102 is configured using the through electrode substrate 21. As a result, according to this embodiment, it is possible to reduce the manufacturing cost of the MEMS device 100. Below, this effect will be described in comparison with a MEMS device 300 as a comparative example.

[0123] Fig. 45 is a cross-sectional view showing a MEMS device 300 of a comparative example. Fig. 46 is a plan view showing the MEMS device 300 of a comparative example. The MEMS device 300 of the comparative example includes a circuit unit 302 of a comparative example instead of the circuit unit 102 of the present embodiment. In the comparative example, a movable part 101 and a cap 103 are fixed on top of the circuit unit 302. The configurations of the movable part 101 and the cap 103 are the same as the configurations of the movable part 101 and the cap 103 of the present embodiment.

[0124] The circuit unit 302 is configured using a substrate 321 instead of the through electrode substrate 21 of the present embodiment. The substrate 321 has a first surface 321a facing the movable unit 101 and a second surface 321b opposite to the first surface 321a. A signal processing circuit is formed on the substrate 321 and the first surface 321a of the substrate 321.

[0125] The circuit unit 302 further includes a plurality of electrode pads 324 formed on the first surface 321a of the substrate 321. The plurality of electrode pads 324 are electrically connected to a wiring layer of a mounting object (not shown). As shown in Figures 45 and 46, the plurality of electrode pads 324 are arranged so as not to overlap with the movable part 101 and the cap 103 when viewed from the Z direction.

[0126] 45 and 46 , in the comparative example, the planar shape of circuit unit 302 is larger than the planar shapes of movable part 101 and cap 103 so that multiple electrode pads 324 are not covered by movable part 101 and cap 103. Therefore, when comparing wafers with the same size, the number of circuit units 302 that can be fabricated from one wafer is smaller than the number of movable parts 101 and caps 103 that can be fabricated from one wafer.

[0127] In contrast to this, in the present embodiment, by configuring the circuit unit 102 using the through electrode substrate 21, as shown in Fig. 39, the planar shape of the circuit unit 102 can be made the same or approximately the same as the planar shapes of the movable unit 101 and the cap 103. As a result, according to the present embodiment, it is possible to increase the number of circuit units 102 that can be fabricated from one wafer compared to the comparative example. As a result, according to the present embodiment, it is possible to reduce the manufacturing cost of the MEMS device 100.

[0128] Other configurations, actions, and effects of this embodiment are the same as those of the first or second embodiment.

[0129] Seventh Embodiment Next, a seventh embodiment of the present disclosure will be described. The MEMS device 100 according to this embodiment differs from the sixth embodiment in that it is configured using the through electrode substrate 21 of the third or fourth embodiment.

[0130] A manufacturing method of the MEMS device 100 according to this embodiment will be described below. In this embodiment, the through electrode formation process is substantially the same as the manufacturing method of the through electrode substrate 21 described in the third embodiment. That is, the through electrode formation process includes the steps of forming a plurality of trenches 25 from the first surface 22 a of the substrate 22 toward the interior of the substrate 22, forming an insulating film 30 in the plurality of trenches 25, polishing the surface of the substrate 22 opposite the first surface 22 a (the surface to be polished) so as to expose the insulating film 30, removing portions of the substrate 22 surrounded by the insulating film 30 to form a plurality of through holes, and forming a plurality of electrodes 27 in the plurality of through holes. The polishing process is performed after the circuit formation process.

[0131] The polishing step and subsequent steps may be performed in a state in which the movable part 101 and the cap 103 are fixed to the initial circuit part 102P. Hereinafter, with reference to Figures 47 to 52, a description will be given of the polishing step and subsequent steps that are performed in a state in which the movable part 101 and the cap 103 are fixed to the initial circuit part 102P. Figures 47 to 52 are cross-sectional views showing the stacked body in the manufacturing process of the MEMS device 100.

[0132] 47 shows a state in which the movable part 101 and the cap 103 are fixed to the initial circuit part 102P. The movable part 101 and the cap 103 are fixed to the initial circuit part 102P immediately before the polishing step.

[0133] 48 shows the next step. In this step, similar to the step shown in FIG. 28 of the third embodiment, the substrate 22 is polished until the insulating film 30 formed in the plurality of trenches 25 is exposed. The substrate 22 is polished from the surface to be polished opposite the first surface 22a of the substrate 22. After polishing, the surface to be polished becomes the second surface 22b of the substrate 22.

[0134] 49 shows the next step. In this step, first, an insulating film 13 is formed on the second surface 22b of the substrate 22. Next, a photoresist mask 68 is formed on the insulating film 13. Next, the insulating film 13 is etched by, for example, RIE using the photoresist mask 68 as an etching mask.

[0135] 50 shows the next step, in which the substrate 22 is etched by, for example, RIE using the photoresist mask 68 as an etching mask. This etching is continued until a plurality of through-holes 69 are formed in the substrate 22 and the electrode portions 12 are exposed.

[0136] 51 shows the next step, in which the photoresist mask 68 is first removed, followed by forming a first layer 271 and a second layer 272 in the plurality of through holes 69.

[0137] 52 shows the next step. In this step, the first layer 271 and the second layer 272 are polished until the insulating film 13 is exposed. This completes the formation of the plurality of electrodes 27. Thereafter, the electrode pads 14 and the like are formed, thereby completing the MEMS device 100.

[0138] Other configurations, actions, and effects of this embodiment are the same as those of the third, fourth, or sixth embodiment.

[0139] Eighth Embodiment Next, an eighth embodiment of the present disclosure will be described. A MEMS device 400 according to this embodiment is configured using the through electrode substrate 21 according to any one of the first to fourth embodiments.

[0140] The configuration of the MEMS device 400 according to this embodiment will be described below by taking as an example a case where the MEMS device 400 is configured using the through electrode substrate 21 of the third embodiment. Fig. 53 is a cross-sectional view showing the MEMS device 400.

[0141] The MEMS device 400 includes a movable part 401, and a circuit part 402 and a cap 403 arranged to sandwich the movable part 401. In this embodiment, the cap 403 is configured using a through electrode substrate 21, and corresponds to the device 10 in the third embodiment (first embodiment). In the following description, the components of the cap 403 that are common to the device 10 will be designated by the same reference numerals as the components of the device 10.

[0142] The cap 403 has cavities 403a and 403b of a predetermined shape. In particular, in this embodiment, the insulating film 30 of the through electrode substrate 21 may be formed on the surfaces of the cavities 403a and 403b.

[0143] The main body of the cap 403 is formed using the substrate 22 of the through electrode substrate 21. The main body of the cap 403 has a first surface facing the movable part 401 and a second surface opposite to the first surface. The first surface and the second surface of the main body of the cap 403 are respectively formed by the first surface 22a and the second surface 22b of the substrate 22. An insulating film 13 and a plurality of electrode pads 14 are provided on the second surface of the main body of the cap 403.

[0144] In particular, in this embodiment, the MEMS device 400 is configured as a motion sensor including an acceleration sensor and a gyro sensor. The movable part 401 includes movable elements 401a and 401b as weights, a structure for fixing the movable elements 401a and 401b, a first electrode (movable electrode) provided on the lower surface of the movable element 401a, and a second electrode (movable electrode) provided on the lower surface of the movable element 401b. The movable element 401a may be a movable element of an acceleration sensor. The movable element 401b may be a movable element of a gyro sensor.

[0145] The movable element 401a is located in a space including a cavity 403a, which is surrounded by the circuit unit 402 and the cap 403. The movable element 401a is configured to be movable within the space including the cavity 403a. Similarly, the movable element 401b is located in a space including a cavity 403b, which is surrounded by the circuit unit 402 and the cap 403. The movable element 401b is configured to be movable within the space including the cavity 403b.

[0146] The movable portion 401 further includes a plurality of electrode portions 401c connected to the plurality of electrodes 27 of the through-hole electrode substrate 21. Each of the plurality of electrode portions 401c is made of silicon in which impurities have been diffused. Each of the plurality of electrode portions 401c may be, for example, an N-type semiconductor with a high impurity concentration, or a P-type semiconductor with a high impurity concentration.

[0147] The configuration of the circuit unit 402 is the same as that of the circuit unit 102 in the sixth embodiment, except that the circuit unit 402 is not configured using the through-hole electrode substrate 21. For convenience, the circuit unit 402 is depicted in a simplified form in FIG. 53 . The circuit unit 402 includes a substrate 422. The substrate 422 has a first surface facing the movable unit 401 and a second surface opposite the first surface. The circuit unit 402 further includes fixed electrodes 404a and 404b formed on the first surface of the substrate 422, and a processor serving as a signal processing circuit formed on the substrate 422 and the first surface of the substrate 422. The fixed electrode 404a faces a first electrode provided on the lower surface of the movable element 401a. The fixed electrode 404b faces a second electrode provided on the lower surface of the movable element 401b.

[0148] The MEMS device 400 further includes a plurality of electrode portions 412 for connecting the plurality of electrode portions 401c to a processor of the circuit portion 402. The plurality of electrode pads 14 are connected to the processor of the circuit portion 402 via the plurality of electrodes 27, the plurality of electrode portions 401c, and the plurality of electrode portions 412.

[0149] Other configurations, actions, and effects of this embodiment are the same as those of any of the first to sixth embodiments.

[0150] Ninth Embodiment Next, a stacked device according to a ninth embodiment of the present disclosure will be described. A stacked device 500 according to this embodiment includes a plurality of stacked devices 501. Each of the plurality of devices 501 is configured using the through electrode substrate 21 according to any one of the first to fourth embodiments.

[0151] The configuration of the stacked device 500 will be described below by taking as an example a case where each of the plurality of devices 501 is configured using the through electrode substrate 21 of the third embodiment. Figure 54 is a cross-sectional view showing the stacked device 500.

[0152] The configuration of each of the multiple devices 501 is the same as the configuration of the device 10 in the third embodiment (first embodiment). In the following description, the same reference numerals as those of the device 10 are used for the components of each of the multiple devices 501 that are common to the device 10. As shown in FIG. 54 , one electrode 27 and the other electrode 27 of two adjacent devices 501 among the multiple devices 501 are electrically connected via electrode pads 14. The two devices 501 may be bonded by eutectic bonding or by using solder.

[0153] 54, the number of the plurality of devices 501 is four. However, the number of the plurality of devices 501 may be two, three, five or more.

[0154] In particular, in this embodiment, the stacked device 500 may be a stacked memory package, and each of the plurality of devices 501 may be a memory chip including a storage circuit such as a flash memory.

[0155] Other configurations, actions, and effects of this embodiment are the same as those of any of the first to fourth embodiments.

[0156] Tenth Embodiment Next, a method for manufacturing a MEMS device 400 according to a tenth embodiment of the present disclosure will be described. The configuration of the MEMS device 400 according to this embodiment is similar to the configuration of the MEMS device 400 according to the eighth embodiment. Hereinafter, with reference to Figs. 55 to 69, a process for forming the movable portion 401 and the cap 403 of the MEMS device 400 will be described. Figs. 55 to 69 are cross-sectional views showing a stacked body in the manufacturing process of the MEMS device 400.

[0157] As explained in the eighth embodiment, the cap 403 is configured using the through electrode substrate 21. In the process of forming the movable portion 401 and the cap 403, first, as shown in FIG. 55, a silicon nitride film, for example, is formed on the first surface 22a of the substrate 22 of the through electrode substrate 21. 3 N 4 An insulating film 71 made of the above is formed.

[0158] 56 shows the next step. In this step, first, a photoresist mask 72 is formed on an insulating film 71. Next, the insulating film 71 is selectively etched by, for example, RIE using the photoresist mask 72 as an etching mask. Next, a plurality of trenches 73 are formed in the substrate 22 by, for example, RIE using the insulating film 71 and the photoresist mask 72 as etching masks. Next, the photoresist mask 72 is removed.

[0159] 57 shows the next step. In this step, a photoresist mask 74 is first formed on the substrate 22 and the insulating film 71. The photoresist mask 74 covers some of the trenches 73 and has openings that expose other parts of the trenches 73. Next, using the insulating film 71 and the photoresist mask 74 as an etching mask, the other parts of the trenches 73 are etched by, for example, RIE so that the depth of the other parts of the trenches 73 is increased. Next, the photoresist mask 74 is removed.

[0160] 58 shows the next step. In this step, first, a photoresist mask 75 is formed on the substrate 22 and the insulating film 71. The photoresist mask 75 covers the plurality of trenches 73 and has openings. Next, the insulating film 71 is etched by, for example, RIE using the photoresist mask 75 as an etching mask. Next, the substrate 22 is deeply etched using the insulating film 71 and the photoresist mask 75 as etching masks to form trenches 76. The trenches 76 are formed from the first surface 22a of the substrate 22 toward the interior of the substrate 22. Next, the photoresist mask 75 is removed.

[0161] The trench 76 corresponds to the plurality of trenches 25 in the first to fourth embodiments. Note that, for convenience, one trench 76 is depicted in FIG. 58 , but a plurality of trenches 76 are formed in the process shown in FIG. 58 . In subsequent processes, as described in the first to fourth embodiments, a plurality of electrodes 23 or a plurality of electrodes 27 are formed using the plurality of trenches 76. The plurality of electrodes 23 or a plurality of electrodes 27 are formed, for example, on the −X direction side of the trench 76 shown in FIG. 58 . In the following description, for convenience, a description of the process of forming the plurality of electrodes 23 or a plurality of electrodes 27 and illustrations of the plurality of electrodes 23 or a plurality of electrodes 27 will be omitted.

[0162] 59 shows the next step. In this step, an insulating film 30 is formed in the plurality of trenches 73 and the trenches 76. The insulating film 30 is, for example, a SiO 2 film formed by thermal oxidation. 2 In this case, the substrate 22 is oxidized from the wall surface and bottom surface of each of the plurality of trenches 73 and 76, and SiO 2 The insulating film 30 is formed so as not to completely fill the trenches 73 and so as to completely fill the trenches 76.

[0163] 60 shows the next step. In this step, first, the insulating film 71 is removed. Next, an insulating layer 77 is formed on the entire top surface of the stack. The insulating layer 77 is formed so as to completely fill the trenches 73. The insulating layer 77 is, for example, a SiO 2 film formed by chemical vapor deposition (CVD). 2 Alternatively, the insulating layer 12 may be made of phosphosilicate glass (PSG) or spin-on-glass (SOG) material.

[0164] 61 shows the next step. In this step, first, a part of the insulating layer 77 is removed until the insulating film 30 is exposed. 2Alternatively, if the insulating layer 77 is made of phosphosilicate glass, it may be polished, for example, by chemical mechanical polishing (CMP). If the insulating layer 77 is made of a spin-on-glass material, it may be selectively removed, for example, by etch-back.

[0165] Fig. 62 shows the next step. In this step, first, a Si 3 N 4 An insulating film 78 made of the insulating film 78 is formed. The insulating film 78 may be formed so as not to cover the region where the plurality of electrodes 23 or the plurality of electrodes 27 are to be formed later. Next, an initial movable portion 401P, which will later become the movable portion 401, is formed on the entire upper surface of the laminate. The initial movable portion 401P may be formed of epitaxial polysilicon or low-stress polysilicon. When the initial movable portion 401P is made of epitaxial polysilicon, the initial movable portion 401P may be formed of, for example, dichlorosilane (SiH 2 Cl 2 ) or monosilane (SiH 4 The temperature of the pyrolysis is, for example, in the range of 1000°C to 1100°C.

[0166] 63 shows the next step. In this step, first, a photoresist mask 79 is formed on the initial movable portion 401P. Next, using the photoresist mask 79 as an etching mask, the upper surface of the initial movable portion 401P is partially etched by, for example, RIE, to form a plurality of protrusions for eutectic bonding. Next, the photoresist mask 79 is removed.

[0167] 64 shows the next step. In this step, a Si 3 N 4 An insulating film 80 made of the above is formed.

[0168] 65 shows the next step. In this step, first, a photoresist mask 81 is formed on the insulating film 80. Next, using the photoresist mask 81 as an etching mask, the insulating film 80 is selectively etched by, for example, RIE so that the multiple protrusions formed on the upper surface of the initial movable portion 401P are exposed.

[0169] 66 shows the next step. In this step, first, a conductive layer 82 is formed on the plurality of protrusions formed on the upper surface of the initial movable portion 401P. The conductive layer 82 may contain a metal used for eutectic bonding. For example, germanium is used for eutectic bonding. Next, the photoresist mask 81 is removed.

[0170] 67 shows the next step. In this step, a photoresist mask 83 having a shape corresponding to the movable portion 401 is first formed on the initial movable portion 401P and the conductive layer 82. Next, using the photoresist mask 83 as an etching mask, the insulating films 78 and 80 are etched by, for example, RIE, and the initial movable portion 401P is deeply processed. The initial movable portion 401P and the insulating films 78 and 80 are etched until the portions of the insulating film 30 formed in the multiple trenches 73 and the insulating layer 77 are exposed. This etching turns the initial movable portion 401P into the movable portion 401.

[0171] 68 shows the next step. In this step, the insulating layer 77 is selectively removed by etching. For example, a buffered oxide etchant (BOE) is used for this etching. This etching forms a plurality of grooves in the insulating film 30.

[0172] FIG. 69 shows the next step. In this step, the portions of the insulating film 30 formed in the trenches 73 are removed by etching. For example, a buffered oxide etchant (BOE) is used for this etching. In this case, the buffered oxide etchant penetrates into the trenches formed in the insulating film 30, causing etching of the insulating film 30 to proceed in a direction perpendicular to the Z direction. This shortens the etching time compared to when etching of the insulating film 30 proceeds from the top surface of the insulating film 30. This etching forms cavities 403a and 403b of the cap 403 in the substrate 22. A plurality of microprotrusions may be formed on the bottom surfaces of the cavities 403a and 403b by etching the insulating film 30. The microprotrusions function to prevent the movable elements 401a and 401b from adhering to the bottom surfaces of the cavities 403a and 403b.

[0173] 70 shows the next step, in which the movable part 401 is fixed to the circuit part 402.

[0174] 71 shows the next step. In this step, first, the substrate 22 is polished until the insulating film 30 formed in the plurality of trenches 76 is exposed. The substrate 22 is polished from the surface to be polished opposite the first surface 22a of the substrate 22. After polishing, the surface to be polished becomes the second surface 22b of the substrate 22. Next, the insulating film 13 is formed on the second surface 22b of the substrate 22. Thereafter, electrode pads 14 and the like are formed, thereby completing the MEMS device 400.

[0175] Next, the operation and effect of the MEMS device 400 according to this embodiment will be described. In this embodiment, the movable portion 401 is formed using the initial movable portion 401P formed on the substrate 22. As a result, according to this embodiment, the number of silicon substrates used can be reduced compared to when a movable portion formed using silicon substrates is fixed to the circuit portion 402 and the cap 403. As a result, according to this embodiment, the manufacturing cost of the MEMS device 400 can be reduced.

[0176] Incidentally, one possible method for forming the cavity 403a of the cap 403 is to form the cavities 403a and 403b in the substrate 22 before forming the initial movable portion 401P. In this case, the initial movable portion 401P is formed on the substrate 22 and the insulating layer after the cavities 403a and 403b are filled with an insulating layer. In this case, the volume of the insulating layer becomes relatively large, and therefore a relatively large stress is applied to the substrate 22 in the subsequent process. As a result, a problem occurs in which the substrate 22 bends.

[0177] In contrast to this, in the present embodiment, a plurality of trenches 73 are formed, an insulating film 30 and an insulating layer 77 are formed in the plurality of trenches 73, and the insulating film 30 and the insulating layer 77 are removed to form cavities 403 a, 403 b in the cap 403. As a result, according to the present embodiment, it is possible to prevent a large stress from being applied to the substrate 22.

[0178] In this embodiment, the cavities 403 a and 403 b are formed by removing the insulating film 30 by etching. As a result, in this embodiment, a plurality of minute protrusions are formed on the bottom surface of each of the cavities 403 a and 403 b. The plurality of minute protrusions has the function of preventing the movable elements 401 a and 401 b from adhering to the bottom surfaces of the cavities 403 a and 403 b.

[0179] Other configurations, actions, and effects of this embodiment are the same as those of any of the first to fourth and eighth embodiments.

[0180] [Modification] Next, a modification of the manufacturing method of the MEMS device 400 according to the present embodiment will be described. In this modification, the cap 403 is configured using a substrate 1422 instead of the through electrode substrate 21. The substrate 1422 may be a silicon substrate. In this modification, the trenches 76 shown in FIG. 58 are not formed in the substrate 1422. Therefore, the cap 403 is not provided with the plurality of electrodes 23 or the plurality of electrodes 27 formed using the plurality of trenches 76.

[0181] 72 and 73, a process for forming the movable portion 401 and the cap 403 of the MEMS device 400 will be described. Figures 72 and 73 are cross-sectional views showing the stacked body in the manufacturing process of the MEMS device 400.

[0182] The manufacturing method up to the step of fixing the movable part 401 to the circuit part 402 is the same as the manufacturing method of the MEMS device 400 according to this embodiment, except that the plurality of trenches 76 and the plurality of electrodes 23 or the plurality of electrodes 27 are not formed. Fig. 72 shows a state in which the movable part 401 is fixed to the circuit part 402. As shown in Fig. 72, the planar shape of the cap 403 is larger than the planar shape of the movable part 401. In this state, the cap 403 covers some of the plurality of electrodes formed in the circuit part 402 that are not connected to the conductive layer 82.

[0183] 73 shows the next step, in which part of cap 403 is removed by, for example, dicing or RIE so as to expose some of the electrodes formed in circuit portion 402 that are not connected to conductive layer 82. This completes MEMS device 400.

[0184] Eleventh Embodiment Next, a method for manufacturing a MEMS device 400 according to an eleventh embodiment of the present disclosure will be described. Differences between the method for manufacturing the MEMS device 400 according to this embodiment and the method for manufacturing the MEMS device 400 according to the tenth embodiment will be described below with reference to Figures 74 to 77. Figures 74 to 77 are cross-sectional views showing a stacked body in the manufacturing process of the MEMS device 400.

[0185] The manufacturing method of the MEMS device 400 according to this embodiment is the same as that of the tenth embodiment up to the step of removing a part of the insulating layer 77 shown in Fig. 61. Fig. 74 shows the next step. In this step, first, a Si 3 N 4An insulating film 78 made of the insulating layer 77 is selectively formed. The insulating film 78 has openings that expose the portions of the insulating film 30 that are formed in the plurality of trenches 73 and the insulating layer 77. Next, an initial movable portion 401P, which will later become the movable portion 401, is formed on the entire upper surface of the stack. The initial movable portion 401P may be formed of epitaxial polysilicon or low-stress polysilicon.

[0186] 75 shows the next step. In this step, first, the upper surface of the initial movable portion 401P is partially etched, similarly to the step shown in FIG. 63 in the tenth embodiment. Next, a conductive layer 181 is formed on the initial movable portion 401P. In this embodiment in particular, the conductive layer 181 may be formed of polysilicon. Next, a layer of, for example, Si 3 N 4 An insulating film 182 made of the insulating film 30 is formed. Next, a photoresist mask 83 having a shape corresponding to the movable portion 401 is formed on the insulating film 182. Next, using the photoresist mask 83 as an etching mask, the insulating film 182 is etched by, for example, RIE. Next, using the insulating film 182 and the photoresist mask 83 as etching masks, the conductive layer 181 is etched by, for example, RIE, and the initial movable portion 401P is deeply etched. The etching of the initial movable portion 401P is performed until the portions of the insulating film 30 formed in the multiple trenches 73 and the insulating layer 77 are exposed. This etching turns the initial movable portion 401P into the movable portion 401. Next, the photoresist mask 83 is removed.

[0187] 76 shows the next step. In this step, the insulating film 30 is etched to remove the portions thereof formed in the trenches 73 and the insulating layer 77. Buffered oxide etchant (BOE), for example, is used for this etching. As a result, cavities 403a and 403b of the cap 403 are formed in the substrate 22.

[0188] 77 shows the next step. In this step, first, an insulating film 84 is formed on the exposed surface of the substrate 22 and the exposed surface of the movable portion 401. The insulating film 84 is made of, for example, SiO 2 formed by thermal oxidation. 2 Next, the insulating film 82 is removed. The insulating film 82 may be removed by dry etching or by etching using hot phosphoric acid as an etchant.

[0189] Next, the movable portion 401 is fixed to the circuit portion 402. The subsequent steps are the same as those in the tenth embodiment.

[0190] Other configurations, actions, and effects of this embodiment are the same as those of the tenth embodiment.

[0191] Twelfth Embodiment Next, a method for manufacturing a MEMS device 400 according to a twelfth embodiment of the present disclosure will be described. Differences between the method for manufacturing the MEMS device 400 according to this embodiment and the method for manufacturing the MEMS device 400 according to the tenth embodiment will be described below with reference to Figures 78 to 84. Figures 78 to 84 are cross-sectional views showing a stacked body in the manufacturing process of the MEMS device 400.

[0192] The manufacturing method of the MEMS device 400 according to this embodiment is basically the same as that of the tenth embodiment up to the step of forming the trench 76 shown in Fig. 58. However, in this embodiment, the step of forming the insulating film 71 is omitted. Fig. 78 shows the next step. In this step, an insulating film 30 is formed in the plurality of trenches 73 and the trench 76. The insulating film 30 is, for example, a SiO 2 In this case, the substrate 22 is oxidized from the wall surface and bottom surface of each of the plurality of trenches 73 and 76, and SiO 2A film (insulating film 30) is formed. FIG. 78 shows a process of forming the insulating film 30. In this embodiment, the insulating film 30 is formed so as to completely fill the plurality of trenches 73 and 76. FIG. 79 shows the stacked body after the insulating film 30 has been formed. In this embodiment, the insulating film 30 is also formed on the first surface 22 a of the substrate 22.

[0193] 80 shows the next step, in which the insulating film 30 is polished until the first surface 22a of the substrate 22 is exposed.

[0194] Fig. 81 shows the next step. In this step, first, a Si 3 N 4 An insulating film 78 made of the insulating film 78 is formed. The insulating film 78 may be formed so as not to cover the regions where the plurality of electrodes 23 or the plurality of electrodes 27 are to be formed later. Next, an initial movable portion 401P, which will later become the movable portion 401, is formed on the entire upper surface of the stack. The initial movable portion 401P may be formed of epitaxial polysilicon or low-stress polysilicon.

[0195] 82 shows the next step. In this step, first, the top surface of the initial movable part 401P is partially etched, similar to the step shown in FIG. 63 of the tenth embodiment. Next, a conductive layer 82 is formed on the initial movable part 401P. The conductive layer 82 may contain a metal used in eutectic bonding.

[0196] 83 shows the next step. In this step, first, a photoresist mask 83 having a shape corresponding to the movable portion 401 is formed on the initial movable portion 401P and the conductive layer 82. Next, using the photoresist mask 83 as an etching mask, the initial movable portion 401P and the insulating film 78 are deeply etched by, for example, RIE. The initial movable portion 401P and the insulating film 78 are etched until the portions of the insulating film 30 formed in the multiple trenches 73 are exposed. This etching turns the initial movable portion 401P into the movable portion 401.

[0197] 84 shows the next step. In this step, the portions of the insulating film 30 formed in the trenches 73 are removed by etching. This forms cavities 403a and 403b of the cap 403 in the substrate 22. A plurality of micro-protrusions may be formed on the bottom surface of each of the cavities 403a and 403b by etching the insulating film 30. The subsequent steps are the same as those in the tenth embodiment.

[0198] Other configurations, actions, and effects of this embodiment are the same as those of the tenth embodiment.

[0199] [Thirteenth Embodiment] Next, a MEMS device 400 according to a thirteenth embodiment of the present disclosure will be described. The MEMS device 400 according to this embodiment includes a movable part 1401 and a cap 1403 instead of the movable part 401 and the cap 403 in the tenth embodiment. A method for manufacturing the MEMS device 400 according to this embodiment will be described below with reference to FIGS. 85 to 96. FIGS. 85 to 96 are cross-sectional views showing a stacked body in the manufacturing process of the MEMS device 400. The following description includes a description of the process of forming the movable part 1401 and the cap 1403.

[0200] In the process of forming the movable portion 1401 and the cap 1403, first, as shown in FIG. 85, a Si 3 N 4 An insulating film 1071 made of the insulating film 1071 is formed. Next, a photoresist mask 1072 is formed on the insulating film 1071. Next, using the photoresist mask 1072 as an etching mask, the insulating film 1071 is selectively etched by, for example, RIE. Next, using the insulating film 1071 and the photoresist mask 1072 as etching masks, a cavity 1403a and an initial cavity 1403bP are formed in the substrate 1022 by, for example, RIE. Next, the photoresist mask 1072 is removed.

[0201] 86 shows the next step, in which a photoresist mask 1073 is formed on the substrate 1022 and the insulating film 1071. The photoresist mask 1073 covers the cavity 1403a and has an opening that exposes a part of the initial cavity 1403bP.

[0202] 87 shows the next step. In this step, first, using the insulating film 1071 and the photoresist mask 1073 as an etching mask, the substrate 1022 is etched by, for example, RIE so that the depth of a portion of the initial cavity 1403bP is increased. This etching turns the initial cavity 1403bP into the cavity 1403b. Next, the photoresist mask 1073 is removed.

[0203] FIG. 88 shows the next step. In this step, first, insulating film 1071 is removed. Next, a photoresist mask 1074 is formed over the entire top surface of the stack. Photoresist mask 1074 covers cavity 1403a and has an opening that exposes a portion of cavity 1403b. Next, using photoresist mask 1074 as an etching mask, substrate 1022 is deeply etched by, for example, RIE, so that trenches 1075, 1076, and 1077 are formed in substrate 1022. In this embodiment, trench 1077 is particularly formed in cavity 1403b. Next, photoresist mask 1074 is removed.

[0204] 89 shows the next step. In this step, first, an insulating film 1079 is formed on the surface of the substrate 1022. The insulating film 1079 is, for example, a SiO 2 film formed by thermal oxidation. 2 It may be a film. Next, an initial movable part 1401P, which will later become the movable part 1401, is bonded to the substrate 1022. The initial movable part 1401P may be a silicon substrate. Alternatively, the initial movable part 1401P may be bonded to the substrate 1022 by fusion bonding. Next, the surface (polished surface) of the initial movable part 1401P opposite to the surface facing the substrate 1022 is polished until the thickness of the initial movable part 1401P reaches a predetermined size.

[0205] 90 shows the next step. In this step, first, the upper surface of the initial movable part 1401P is partially etched, similarly to the step shown in FIG. 63 of the tenth embodiment. Next, a conductive layer 1081 is formed on the initial movable part 1401P. Particularly in this embodiment, the conductive layer 1081 may be formed of polysilicon.

[0206] 91 shows the next step. In this step, first, a photoresist mask (not shown) having a shape corresponding to the movable portion 1401 is formed on the initial movable portion 1401P and the conductive layer 1081. Next, using the photoresist mask (not shown) as an etching mask, the initial movable portion 1401P is deeply etched by, for example, RIE. This etching also forms through-holes communicating with the trench 1075 and through-holes communicating with the trench 1076. This etching turns the initial movable portion 1401P into the movable portion 1401. The movable portion 1401 includes movable elements 1401a and 1401b as weights, a structure for fixing the movable elements 1401a and 1401b, an electrode (movable electrode) 1401c provided on the movable element 1401a, and an electrode (movable electrode) 1401d provided on the movable element 1401b. The electrodes 1401c and 1401d are formed by etching the conductive layer 1081. Next, the photoresist mask (not shown) is removed.

[0207] FIG. 92 shows the next step. In this step, the movable part 1401 is fixed to the circuit part 402. The movable part 1401 may be fixed to the circuit part 402 by, for example, eutectic bonding. In FIG. 92 , reference numeral 1412 denotes an electrode connecting the movable part 1401 and the circuit part 402. Fixed electrodes 404a and 404b formed on the first surface of the substrate 422 of the circuit part 402 face electrodes 1401c and 1401d, respectively. In this embodiment, the movable part 1401 may be fixed to the circuit part 402 so that a space including the cavity 1403a and surrounded by the circuit part 402 and the substrate 1022 is maintained at a vacuum after the movable part 1401 is fixed to the circuit part 402.

[0208] 93 shows the next step. In this step, the substrate 1022 is polished until the insulating film 1079 formed in the trenches 1075-1077 is exposed. The substrate 1022 is polished from the surface to be polished opposite the first surface 1022a of the substrate 1022. After polishing, the surface to be polished becomes the second surface 1022b of the substrate 1022.

[0209] 94 shows the next step. In this step, first, the insulating film 1013 is formed on the second surface 1022b of the substrate 1022. Next, at least one through-hole communicating with the trenches 1075 and 1076 is formed in the insulating films 1013 and 1079.

[0210] FIG. 95 illustrates the next step. In this step, first, an electrode 1027 is formed in each of the trenches 1075 and 1076. The electrode 1027 includes a first layer 1271 and a second layer 1272. In the step of forming the electrode 1027, the first layer 1271 is first formed in the trenches 1075 and 1076. The first layer 1271 is also formed on the insulating film 1013. The first layer 1271 is formed by, for example, electroless plating. Next, the second layer 1272 is formed on the first layer 1271. The second layer 1272 is formed by, for example, electrolytic plating. The first layer 1271 is used as an electrode and a seed layer when the second layer 1272 is formed by electrolytic plating. Next, the portion of the first layer 1271 that is not covered by the second layer 1272 is removed. The electrode 1027 is electrically connected to the electrode 1412.

[0211] FIG. 96 shows the next step. In this step, first, at least one through-hole communicating with the trench 1077 is formed in the insulating films 1013 and 1079. Particularly in this embodiment, the at least one through-hole may be a plurality of through-holes. The cavity 1403b communicates with the outside via the trench 1077 and the at least one through-hole. Next, the at least one through-hole is sealed with a sealing member 1015 made of, for example, a metal material so that the space including the cavity 1403b and surrounded by the circuit unit 402 and the substrate 1022 is maintained at a vacuum. This completes the cap 1403 and the MEMS device 400. Examples of the metal material for the sealing member 1015 include Ti, Au, and an alloy such as AlCu.

[0212] As described above, in this embodiment, the space including cavity 1403a and surrounded by circuit unit 402 and substrate 1022 (hereinafter referred to as the first space) and the space including cavity 1403b and surrounded by circuit unit 402 and substrate 1022 (hereinafter referred to as the second space) are sealed at different times. This allows the degree of vacuum of the first space and the degree of vacuum of the second space to be controlled separately. In this embodiment, the degree of vacuum of the first space and the degree of vacuum of the second space may be different from each other.

[0213] In this embodiment, instead of forming the plurality of electrodes 1027, a plurality of electrodes similar to the plurality of electrodes 23 in the first and second embodiments may be formed, or a plurality of electrodes 27 in the third and fourth embodiments may be formed. The other configurations, actions, and effects of this embodiment are the same as those of any of the first to fourth and tenth embodiments.

[0214] [Fourteenth Embodiment] Next, a MEMS device 400 according to a fourteenth embodiment of the present disclosure will be described. Differences between the MEMS device 400 according to this embodiment and the MEMS device 400 according to the thirteenth embodiment will be described below with reference to Fig. 97. Fig. 97 is a cross-sectional view showing the MEMS device 400 according to this embodiment.

[0215] In the present embodiment, the cap 1403 includes a trench 1078 and a sealing member 1016 instead of the trench 1077 and the sealing member 1015 in the thirteenth embodiment. The trench 1078 is formed in the cavity 1403a. The insulating films 1013 and 1079 each have at least one through-hole communicating with the trench 1077. The sealing member 1016 is made of, for example, a metal, and seals the space including the cavity 1403a, which is surrounded by the circuit unit 402 and the substrate 1022, so that the space is maintained at a vacuum.

[0216] In this embodiment, the movable part 1401 may be fixed to the circuit part 402 so that the space including the cavity 1403b and surrounded by the circuit part 402 and the substrate 1022 is maintained at a vacuum after the movable part 1401 is fixed to the circuit part 402.

[0217] Other configurations, actions, and effects of this embodiment are the same as those of the thirteenth embodiment.

[0218] The present disclosure is not limited to the above-described embodiments, and various modifications are possible. For example, the process of forming the movable part 401 and the cap 403 of the MEMS device 400 according to the tenth embodiment can be applied to the process of forming the movable part 101 and the cap 103 of the MEMS device 100 according to the sixth and seventh embodiments, except for forming the plurality of electrodes 23 or the plurality of electrodes 27 on the cap 403.

[0219] Furthermore, the circuit section 102 in the sixth and seventh embodiments may be configured using the through electrode substrate 21 in the fifth embodiment. Furthermore, the cap 403 in the eighth and tenth embodiments may be configured using the through electrode substrate 21 in the fifth embodiment.

[0220] In the tenth embodiment, the insulating layer 77 is not an essential component and may not be provided.

[0221] As described above, the through electrode substrate of the present disclosure comprises a substrate having a first surface and a second surface opposite the first surface, at least one electrode extending from the first surface to the second surface, a first portion extending along the at least one electrode and contacting the at least one electrode, a second portion extending along the first portion and adjacent to the first portion, and an insulating film including an interface between the first portion and the second portion.

[0222] In the through hole electrode substrate of the present disclosure, the insulating film may further include a third portion provided on the first surface. The total thickness of the first portion and the second portion may be equal to or greater than the thickness of the third portion. The second portion and the third portion may be continuous. Alternatively, the second portion and the third portion may not be continuous.

[0223] In the through hole electrode substrate of the present disclosure, the first portion and the second portion may surround at least one electrode.

[0224] In the through-hole electrode substrate of the present disclosure, at least one electrode may have a first end and a second end located at both ends in an extension direction of the at least one electrode. The first end may be located closer to the first surface than the second surface. The second end may be located closer to the second surface than the first surface. The distance between the first end and the second end in the extension direction may be greater than the distance between the first surface and the second surface in the extension direction.

[0225] In the through hole electrode substrate of the present disclosure, at least one electrode may be made of silicon or metal in which impurities are diffused.

[0226] The through hole electrode substrate of the present disclosure may further include an electrode pad, and the at least one electrode may be a plurality of electrodes connected to the electrode pad.

[0227] A MEMS device according to a first aspect of the present disclosure is a MEMS device including a movable part, a circuit part and a cap arranged to sandwich the movable part, and the circuit part is configured using the through electrode substrate according to the present disclosure.

[0228] The MEMS device according to the first aspect of the present disclosure may be mounted on a substrate such that the circuit unit is fixed to the substrate. The first surface of the substrate may face the movable portion. The second surface of the substrate may face the substrate. The at least one electrode may have a first end and a second end located at opposite ends in an extension direction of the at least one electrode. The first end may be located closer to the first surface than the second surface. The second end may be located closer to the second surface than the first surface. The MEMS device may further include an electrode pad connected to the second end. When the MEMS device is mounted on the substrate, the electrode pad may be directly connected to a wiring layer of the substrate.

[0229] Furthermore, the MEMS device according to the first aspect of the present disclosure may be mounted on a substrate such that the cap is fixed to the substrate. The first surface of the substrate may face the movable portion. The second surface of the substrate may face the opposite side to the substrate. The at least one electrode may have a first end and a second end located at opposite ends in an extension direction of the at least one electrode. The first end may be located closer to the first surface than the second surface. The second end may be located closer to the second surface than the first surface. The MEMS device may further include an electrode pad connected to the second end. When the MEMS device is mounted on the substrate, the electrode pad may be connected to a wiring layer of the substrate via a bonding wire.

[0230] A method for manufacturing a MEMS device according to a first aspect of the present disclosure includes a step of forming a movable portion and a cap, and a step of forming a circuit portion. The step of forming the circuit portion includes a through-hole forming step of forming at least one electrode and an insulating film on the substrate, and a circuit forming step of forming a signal processing circuit on the substrate.

[0231] In the method for manufacturing a MEMS device according to the first aspect of the present disclosure, the substrate may be a silicon substrate. The through electrode forming step may include the steps of forming at least one trench from a first surface of the substrate toward the interior of the substrate, diffusing impurities into the substrate from wall surfaces and a bottom surface of the at least one trench to form an impurity diffusion region that will later become at least one electrode, forming an insulating film in the at least one trench, and polishing the surface of the substrate opposite the first surface so that the impurity diffusion region becomes at least one electrode. The polishing step may be performed after the circuit forming step and may be performed until the insulating film and the impurity diffusion region are exposed.

[0232] In the method for manufacturing a MEMS device according to the first aspect of the present disclosure, the through electrode forming step may include the steps of forming at least one trench from a first surface of the substrate toward the interior of the substrate, forming an insulating film in the at least one trench, polishing the surface of the substrate opposite the first surface to expose the insulating film, removing a portion of the substrate surrounded by the insulating film after the polishing step to form at least one through hole, and forming at least one electrode in the at least one through hole. The polishing step may be performed after the circuit forming step.

[0233] A MEMS device according to a second aspect of the present disclosure includes a movable portion, and a circuit portion and a cap arranged to sandwich the movable portion. The cap is configured using the through electrode substrate according to the present disclosure.

[0234] A manufacturing method for a MEMS device according to a second aspect of the present disclosure includes the steps of forming a movable portion and a cap, and forming a circuit portion. The steps of forming the movable portion and the cap include a through-electrode formation step of forming at least one electrode and an insulating film on a substrate, a step of forming an insulating portion on the substrate, a step of forming the movable portion on the substrate and the insulating portion, and a step of removing the insulating portion by etching after forming the movable portion to form a cavity in the substrate.

[0235] In the method for manufacturing a MEMS device according to the second aspect of the present disclosure, the insulating section may include an insulating layer made of phosphosilicate glass.

[0236] In the method for manufacturing a MEMS device according to the second aspect of the present disclosure, the movable portion may be made of epitaxial polysilicon.

[0237] In the method for manufacturing a MEMS device according to the second aspect of the present disclosure, the substrate may be a silicon substrate. The step of forming the movable portion and the cap may further include the step of forming a plurality of trenches from the first surface of the substrate toward the interior of the substrate. The step of forming the insulating portion may include the step of oxidizing the substrate from the wall surfaces and bottom surfaces of each of the plurality of trenches to form an oxide insulating film, and the step of forming an insulating layer made of phosphosilicate glass in each of the plurality of trenches.

[0238] The stacked device of the present disclosure includes a plurality of stacked devices, each of which is constructed using the through hole electrode substrate of the present disclosure, and at least one electrode of one of two adjacent devices among the plurality of devices is electrically connected to at least one electrode of the other adjacent device.

Claims

1. A through electrode substrate comprising: a substrate having a first surface and a second surface opposite to the first surface; at least one electrode extending from the first surface to the second surface; and an insulating film including a first portion extending along the at least one electrode and in contact with the at least one electrode, a second portion extending along the first portion and adjacent to the first portion, and an interface between the first portion and the second portion.

2. The through electrode substrate according to claim 1, wherein the insulating film further includes a third portion provided on the first surface, and the total thickness of the first portion and the second portion is equal to or greater than the thickness of the third portion.

3. The through electrode substrate according to claim 2, wherein the second portion and the third portion are continuous.

4. The through electrode substrate according to claim 2, wherein the second portion and the third portion are not continuous.

5. The through hole electrode substrate according to claim 1, wherein the first portion and the second portion surround the at least one electrode.

6. The through electrode substrate according to claim 1, wherein the at least one electrode has a first end and a second end located at opposite ends in an extension direction of the at least one electrode, the first end is located closer to the first surface than the second surface, the second end is located closer to the second surface than the first surface, and a distance between the first end and the second end in the extension direction is greater than a distance between the first surface and the second surface in the extension direction.

7. The through hole electrode substrate according to claim 1, wherein the at least one electrode is made of silicon or metal in which impurities are diffused.

8. The through hole electrode substrate according to claim 1, further comprising an electrode pad, and the at least one electrode is a plurality of electrodes connected to the electrode pad.

9. A MEMS device comprising: a movable section; and a circuit section and a cap arranged to sandwich said movable section, said circuit section being configured using the through electrode substrate according to claim 1.

10. The MEMS device as described in claim 9, wherein the MEMS device is mounted on the object to be mounted such that the circuit portion is fixed to the object to be mounted, the first surface of the substrate faces the movable portion, the second surface of the substrate faces the object to be mounted, the at least one electrode has a first end and a second end located at both ends in an extension direction of the at least one electrode, the first end is located closer to the first surface than the second surface, and the second end is located closer to the second surface than the first surface, the MEMS device further comprises an electrode pad connected to the second end, and when the MEMS device is mounted on the object to be mounted, the electrode pad is directly connected to a wiring layer of the object to be mounted.

11. The MEMS device as described in claim 9, wherein the MEMS device is mounted on the object to be mounted such that the cap is fixed to the object to be mounted, the first surface of the substrate faces the movable part, the second surface of the substrate faces the opposite side to the object to be mounted, the at least one electrode has a first end and a second end located at both ends in an extension direction of the at least one electrode, the first end is located closer to the first surface than the second surface, and the second end is located closer to the second surface than the first surface, the MEMS device further comprises an electrode pad connected to the second end, and when the MEMS device is mounted on the object to be mounted, the electrode pad is connected to a wiring layer of the object to be mounted via a bonding wire.

12. A method for manufacturing a MEMS device as described in claim 9, comprising the steps of: forming the movable part and the cap; and forming the circuit part, the step of forming the circuit part including a through electrode forming step of forming the at least one electrode and the insulating film on the substrate, and a circuit forming step of forming a signal processing circuit on the substrate.

13. The manufacturing method according to claim 12, wherein the substrate is a silicon substrate, and the through electrode forming step includes the steps of: forming at least one trench from the first surface of the substrate toward the inside of the substrate; diffusing impurities into the substrate from wall surfaces and a bottom surface of the at least one trench to form an impurity diffusion region which will later become at least one electrode; forming the insulating film within the at least one trench; and polishing the surface of the substrate opposite the first surface so that the impurity diffusion region becomes the at least one electrode, the polishing step being performed after the circuit forming step and being performed until the insulating film and the impurity diffusion region are exposed.

14. The manufacturing method described in claim 12, wherein the through electrode forming process includes the steps of: forming at least one trench from the first surface of the substrate toward the inside of the substrate; forming the insulating film in the at least one trench; polishing the surface of the substrate opposite the first surface so as to expose the insulating film; after the polishing process, removing a portion of the substrate surrounded by the insulating film to form at least one through hole; and forming the at least one electrode in the at least one through hole, and the polishing process is performed after the circuit forming process.

15. A MEMS device comprising: a movable section; and a circuit section and a cap arranged to sandwich said movable section, said cap being constructed using the through electrode substrate according to claim 1.

16. A method for manufacturing a MEMS device as described in claim 15, comprising the steps of forming the movable part and the cap, and forming the circuit part, wherein the step of forming the movable part and the cap includes a through electrode formation step of forming the at least one electrode and the insulating film on the substrate, a step of forming an insulating part on the substrate, a step of forming the movable part on the substrate and the insulating part, and a step of removing the insulating part by etching after forming the movable part to form a cavity in the substrate.

17. The method of claim 16, wherein the insulating portion includes an insulating layer made of phosphosilicate glass.

18. The manufacturing method according to claim 16, wherein the movable portion is made of epitaxial polysilicon.

19. The manufacturing method according to claim 16, wherein the substrate is a silicon substrate, the step of forming the movable portion and the cap further includes a step of forming a plurality of trenches from the first surface of the substrate toward the inside of the substrate, and the step of forming the insulating portion includes a step of oxidizing the substrate from the wall surface and bottom surface of each of the plurality of trenches to form an oxide insulating film, and a step of forming an insulating layer made of phosphosilicate glass in each of the plurality of trenches.

20. A stacked device comprising a plurality of stacked devices, each of the plurality of devices being constructed using the through electrode substrate described in claim 1, and wherein at least one electrode of one of two adjacent devices among the plurality of devices is electrically connected to at least one electrode of the other device.

Citation Information

Patent Citations

  • Wafer level packaging method

    JP2009515338A

  • MEMS device, and manufacturing method of cap substrate used for the same

    JP2011245587A

  • Semiconductor device, manufacturing method thereof, data processing system

    JP2012089566A

  • MEMS device assembly and method of packaging the same

    JP2013154465A

  • Through electrode substrate and method of manufacturing the same

    JP2016072433A