Clay-containing composition, method for producing same and use thereof

Non-activated Ca bentonites with high smectite content form efficient, moisture-resistant gels when mixed with polymers and additives on-site, addressing the inefficiencies and costs of existing activated smectite systems, enhancing sealing performance and reducing energy consumption.

WO2024213294A1PCT designated stage expired Publication Date: 2024-10-17STEPHAN SCHMIDT
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/053726
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-13
Filing Date
2024-02-14
Publication Date
2024-10-17

AI Technical Summary

Technical Problem

Existing mineral sealing systems using activated smectites are energy-intensive, difficult to compact, and costly, leading to potential leaks and inefficiencies in forming coherent, waterproof gels for applications like landfill sealing and wastewater treatment.

Method used

A clay-containing composition, primarily using non-activated Ca bentonites with high smectite content, forms moisture-resistant gels without the need for activation, allowing for easier and more economical production of mineral sealing systems by mixing with polymers and mineral additives on-site, enhancing compaction and reducing costs.

Benefits of technology

The solution provides a more economically efficient and effective mineral sealing system with improved compaction and reduced risk of leaks, maintaining water resistance without the need for energy-intensive activation processes, while maintaining pollutant and water adsorption capacities.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 000001
    Figure 000001
  • Figure 000002
    Figure 000002
  • Figure 000003
    Figure 000003
Patent Text Reader

Abstract

The invention relates to clay-containing compositions for sealing landfill soil, dump substrate surfaces and the like, comprising non-activated clays or non-activated bentonites and also water, polymers (polyacrylamides) and mineral aggregates (such as, for example, sand).
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Description: Clay-containing composition, process for its preparation and its use

[0002] The present invention relates to a clay-containing, in particular bentonite-containing, composition, a process for its preparation and its use as a mineral sealing system for, for example, surface and base sealing of landfills, dump sites or as a water barrier in civil engineering or pond systems.

[0003] Clay is a naturally occurring, predominantly inorganic material consisting primarily of clay minerals. Bentonite is a natural clay rock (clay) that also consists of various clay minerals. The most important component is smectite, a clay mineral that structurally belongs to the phyllosilicates. The smectite group includes, for example, the minerals montmorillonite, beidellite, hectorite, nontronite, and saponite. Bentonites can also contain minerals such as magnetite, rectorite, calcite, illite, feldspar, and anatase.

[0004] It is known in the art that clays and bentonites containing smectite can form moisture-resistant gels with water-soluble and / or water-swellable polymers in the presence of water. For this purpose, so-called activated or Na-activated smectites are used, which are produced by reacting smectites or smectite-containing clays with an activating agent, such as a sodium carbonate solution or sodium carbonate powder. The starting material used is Ca-bentonites, which, through this activation, are converted into Na-activated bentonites with increased swelling capacity upon exposure to water.

[0005] The moisture-resistant gels described are mixed with water and mineral aggregates, preferably sand, to form a mineral sealing system, which is preferably used for the purposes mentioned above. A well-known commercially available mineral sealing system is the Trisoplast® product group, which consists of a sodium-activated bentonite polymer component, water, and sand. To produce a soil sealant (e.g., for sealing landfill soils), the moisture-resistant gel (components: smectite, activating agent, polymer, and water) can also be mixed with on-site soil before further moistening, e.g., by milling the gel into the soil.

[0006] In the state of the art, numerous documents describe improvements and further developments of such sealing systems, which relate to the product properties, their manufacture and their use.

[0007] EP 0 335 653 A and WO 99 / 1 1732 describe increasing the storage stability of gels by omitting one of their components (activating agent or water).

[0008] EP 0 682 684 A discloses that activated smectites with a sodium and / or lithium ion content of at least 3.0% exhibit improved properties, such as increased swelling capacity. However, the dry mixtures according to this disclosure are difficult to compact, which, especially as the sealing layer dries out, can lead to cracks and fissures, and thus to leaks in the compacted soil layers.

[0009] According to EP 0 335 653 A, a gel suitable for sealing purposes is obtained by vigorously stirring or kneading a smectite-type clay mineral and at least 0.6 wt.% of a water-soluble polymer in the presence of at least 30 wt.% water to effect a reaction between the clay mineral and the polymer. The resulting aqueous suspension is then reacted with at least 0.5 wt.% activating agent (e.g., sodium carbonate) with vigorous stirring or kneading in the presence of water. The final reaction to form the desired gel is carried out at the site of use, where the ultimately formed gel is brought into contact with the mineral additives (e.g., soil, sand), thereby creating the final mineral sealing system. The disadvantage of this procedure is the production of the gel, which is mechanically demanding and therefore energy-intensive.

[0010] Furthermore, the prior art describes processes in which a dry premix for gel formation is first prepared from the gel-forming components with the exception of water, and the dry premix is ​​only brought into contact with water and the mineral aggregates at the site of use (EP 0 244 981 A, GB 1 439 734 and EP 0 682 684 A). The disadvantage of this procedure is the fact that a coherent, water-tight gel without gaps and cracks can only be formed from a well-compacted, dry premix. However, dry powders or granules are difficult to compact. Therefore, for the most important use of these gels as soil compaction agents, it is preferable to mix them with the soil before further moistening with water (e.g. by burying them in the soil), rather than simply spreading them in a dry state or as a slurry with water onto the soil surface to be sealed.This mixing process is complex and reduces the economic efficiency of the described process.

[0011] Finally, DE 601 02 290 T2 describes so-called water-tolerant, dry premixes for gel formation. These premixes contain a special polymer and a limited amount of water, which is sufficient to make the premix readily compactable, while simultaneously eliminating the risk of premature gel formation during storage. The subsequent necessary compaction of the gel (with or without mineral aggregates) can be achieved on-site using various methods, such as compaction rollers, vibrating plates, or even by the weight or compaction of a top layer or structure.

[0012] For all the aforementioned purposes, including the use of the gel for wastewater treatment through ion exchange or the incorporation of harmful substances (such as heavy metal ions) into the clay-containing component of the gel, Na- and / or Li-activated clay minerals of the smectite type, such as montmorillonite, beidellite, hectorite, nontronite, saponite, allevardite, and other representatives, or mixtures thereof, are always used. Also suitable for the aforementioned purposes, as described in the prior art, are rocks containing these clay minerals, such as bentonite, which consists of various clay minerals with montmorillonite as its main component (60 to 80%).

[0013] The disadvantages of this procedure are the associated costs for the activation material (usually soda) and the costs for carrying out the activation process (mixing the clay mineral / clay-containing rock with the activating agent) and the associated loss of time due to an additional required work step.

[0014] The object of the present invention was therefore to further improve the sealing systems known in the prior art with regard to their cost-effectiveness and performance.

[0015] It has now surprisingly been found that the activation of the clay-containing starting minerals described in the prior art and considered absolutely necessary can be completely dispensed with under certain conditions. The present invention therefore relates to clay-containing compositions which, according to the invention, can also be described with regard to their chemical-physical consistency or appearance as a mixture or blend of various components, which, in the presence of a sufficient amount of water, can form moisture-resistant, especially water-resistant, gels and, together with other additives, preferably mineral additives such as sand, constitute mineral sealing systems.

[0016] Ca-bentonites (calcium bentonites) from deposits in the Westerwald region of Germany have proven to be particularly suitable as a clay-containing material for use in the composition, mixture, or blend according to the invention. In principle, all clay-containing minerals with a high content of smectite-type clay minerals (as described above, for example) are suitable. Compared to Na-bentonite, Ca-bentonite is stable in saline waters and does not swell during on-site preparation of the mixture.

[0017] These minerals preferably contain more than 55 wt.%, in particular more than 70 wt.%, and particularly preferably more than 80 wt.% of clay minerals of the smectite type (also referred to herein as "smectite"). Pure smectite is also suitable for the purposes of the present invention without activation. This also applies to mixtures of the aforementioned substance types.

[0018] The preferred Ca-bentonites from the Westerwald deposits are particularly characterized by the following features and parameters:

[0019] Smectite content: 50-80 wt.%, preferably 60-70 wt.%,

[0020] Cation exchange capacity 60-90 meq / 100g,

[0021] MgO content > 2 wt%, preferably > 3 wt%, K2O content < 2 wt%, preferably < 1 wt%, Na2O content < 1 wt%, preferably < 0.5 wt%.

[0022] The low Na2O content of the Ca-bentonites according to the invention or bentonites in general is an important distinguishing feature compared to the activated Na-bentonites or the natural Na-bentonites, which have Na2O contents of > 2 wt.%, usually greater than 3 wt.%.

[0023] In summary, it can be stated that the present invention encompasses all compositions, mixtures, etc. mentioned in the prior art for the purposes described or according to the invention, wherein, according to the invention, the clay-containing component is present in a non-activated form.

[0024] In principle, common clays (with or without smectite content) can also be reacted or modified with suitable polymers to produce a corresponding gel formation. However, such clays are not preferred according to the invention because, due to the lack of or insufficient smectite content, they have no or insufficient pollutant and water adsorption capacities, as required for sealing purposes or in the field of wastewater treatment.

[0025] Gel formation can occur with a wide range of polymers. Examples include polyacrylamides, hydrolyzed polyacrylamides, and acrylic acid / acrylamide copolymers. Straight-chain (co)polymers of the acrylamide type are preferred, either as a single (co)polymer or as mixtures of two or more such (co)polymers.

[0026] In principle, all polymers listed in the above-mentioned prior art documents and suitable for gel formation can also be used according to the invention. This also applies to the proportions of these polymers in the formed gel or in the mineral

[0027] Waterproofing system (e.g. gel + sand)

[0028] In general, anionic polymers and amphoteric polymers are preferred according to the invention, of which the anionic polymers are particularly preferred. In principle, polymer mixtures can also be used.

[0029] With regard to the use of the composition according to the invention (also referred to as mixtures or blends for the purposes of the invention), three procedures are preferred:

[0030] (i) separate delivery of polymer and Ca-bentonite to the construction site, where the components are converted into a mineral waterproofing system by intensive mixing (e.g. stirring or kneading of the starting components) with water to form a gel and, if necessary, with other aggregates, such as sand or local soils, or

[0031] (ii) Production of a bentonite-polymer mixture by intensive mixing with or without aggregates (preferably sand), which is converted into the desired product on site with the addition of water, or

[0032] (iii) Production of a bentonite-polymer mixture by intensive mixing and milling into local soils.

[0033] To ensure the implementation of process variant (ii), the presence of a solid, dry premix, which should also contain a limited amount of water for reasons of simple production and good compactability, is a prerequisite. This can be achieved through the use of suitable water-soluble and / or water-swellable polymers. The production of such storable premixes containing suitable polymers is described in DE 601 02 290 T2. The premixes listed therein and their compositions, including the physical parameters such as particle sizes and the weight proportions of the individual components, are also applicable to the present invention. The difference between these premixes and the present invention lies in the replacement of the activated smectites and bentonites with the non-activated clay minerals and clay-containing minerals or rocks.

[0034] The following examples show preferred compositions of compositions according to the invention (qualitative and quantitative), and further physical parameters of such compositions.

[0035] Example 1

[0036] Ca-Bentonite: 17-23 wt.% Sand / gravel sand: 77-83 wt.% Polymer: 0.1 to 0.7 wt.% Water addition: 12-17 wt.%

[0037] Example 2

[0038] Ca-Bentonite > 10 to 15 wt.% Gravel: 50-56 wt.% Sand / gravel sand: 32-38 wt.% Polymer: 0.1 to 0.7 wt.% Water addition: 12-17 wt.%

[0039] Example 3 (preferred particle sizes) Ca-bentonite 0-10 mm, preferably 0-1 mm, particularly preferably 0-100 pm Sand 0-2 mm Gravel sand 0-8 mm Processed mineral building materials and sieve residues from the processing of the stone industry: analogous to sand and gravel sand Example 4 (further examples of non-activated clays according to the invention) Kaolinitic-illitic clays (e.g., blue clays) with smectite content and / or smectite / illite interlayer minerals < 50%; cation exchange specification 10-35 meq / 100g, preferably 20-30 meq / 100g

[0040] Example 5 (Examples of other aggregates besides sand) processed mineral building materials and screening residues from the processing of the stone industry: analogous to sand and gravel sand

[0041] The clay-containing compositions according to the invention can contain each component in the form of a single substance or as mixtures of different types / representatives of such a component. In this respect, the use of the singular includes the plural, and vice versa. This also applies mutatis mutandis to the patent claims.

[0042] For the purposes of the present invention, the following analytical methods can be used in particular with regard to suitable clays: a) chemical analysis / chemical composition: X-ray fluorescence analysis (XRF or XRF), whereby various elements are given in the form of their oxides (in wt.%), such as SiO2, Fe2O3, CaO, K2O, P2O5, and other elements are given as such in mg / kg of clay, b) mineral composition (in wt.%; e.g. proportion of smectite, illite, kaolinite, quartz): X-ray diffraction with Rietveld analysis (RBA / XRD). c) cation exchange capacity (CEC; e.g. according to the Cu-triene method in the publications of the BGR (Federal Institute for Geosciences and Natural Resources)).

Claims

Patent claims 1 . Use of non-activated smectite-containing clays or bentonites or of non-activated smectites as a substitute for activated clay minerals or activated smectites in compositions which, in combination with polymers and water, form moisture-resistant gels and, by the addition of mineral aggregates, form mineral waterproofing systems.

2. Use according to claim 1, characterized in that the bentonite or bentonite mixture is Ca-bentonite or Ca-bentonite.

3. Use according to claim 1 or 2, characterized in that a Ca-bentonite with the following parameters is used: smectite content: 50-80 wt.%, preferably 60-70 wt.%, cation exchange capacity 60-90 meq / 100g, MgO content > 2 wt%, preferably > 3 wt%, K2O content < 2 wt%, preferably < 1 wt%, Na2O content < 1 wt%, preferably < 0.5 wt%.

4. Use according to one of claims 1 to 3, characterized in that the polymer or polymers used are polyacrylamides, hydrolyzed polyacrylamides and / or acrylic acid / acrylamide Copolymers are used.

5. Use according to any one of claims 1 to 4 for compositions for surface or base sealing of landfills, dump sites, ponds and dam structures.

6. Clay-containing composition (mixture or mixture) for producing a moisture-resistant gel or a mineral sealing system, which comprises clays or bentonites, polymers, water and optionally mineral aggregates, characterized in that the clays or bentonites are a non-activated smectite-containing clay mineral or a non-activated smectite or a non-activated Ca-bentonite or corresponding mixtures.

7. Clay-containing composition according to claim 6, characterized in that the Ca-bentonite has the following parameters: smectite content: 50-80 wt.%, preferably 60-70 wt.%, cation exchange capacity 60-90 meq / 100g, MgO content > 2 wt%, preferably > 3 wt%, K2O content < 2 wt%, preferably < 1 wt%, Na2O content < 1 wt%, preferably < 0.5 wt%.

8. Clay-containing composition according to claim 6 or 7, characterized in that the polymer is a polyacrylamide, hydrolyzed polyacrylamide and / or an acrylic acid / acrylamide copolymer.

9. A moisture-resistant gel comprising or consisting of a clay-containing composition according to any one of claims 6 to 8, which does not comprise any mineral additives.

10. Mineral sealing system comprising or consisting of a clay-containing composition according to any one of claims 6 to 8, which comprises mineral aggregates.

11. Use of a moisture-resistant gel or a mineral sealing system according to claim 9 or 10 for the watertight isolation of surface and base seals of landfills, dams, hydraulic structures, basins, wet areas or other objects exposed to the harmful effects of water or aqueous solutions or chemicals.

12. A method for producing a moisture-resistant gel or a mineral sealing system according to claim 9 or 10 by homogeneous mixing or kneading of the starting components or by milling the starting components into the material to be sealed. Floor.

Citation Information

Patent Citations

  • clay-containing COMPOSITION AND MIXTURE CAPABLE OF FORMING A MOISTURE RESISTANT GEL AND USE

    DE60102290T2

  • Soil sealing compositions and methods

    EP0244981A2

  • Method for the preparation of gels capable of taking up and releasing water in a reversible manner from clay minerals and polymers

    EP0335653A1

  • Clay-containing mixture and blend capable of forming a moisture rsistant gel, and use of that mixture and blend

    EP0682684A1

  • A clay-containing mixture of dry solids to be used in forming a moisture resistant GEL and method for treating a surface

    WO1999011732A1