Method for coating a web material

The method of using a traveling application unit in a closed loop to control relative speeds with the web material addresses the inefficiencies in achieving precise electrochemically active layers, reducing waste and optimizing the use of precious metals in coating processes for lithium-ion batteries and fuel cells.

WO2024217884A1PCT designated stage expired Publication Date: 2024-10-24ROBERT BOSCH GMBH
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/059170
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-17
Filing Date
2024-04-04
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Existing methods for coating web materials with electrochemically active layers, such as for lithium-ion batteries and fuel cells, using slot nozzles face challenges in achieving precise target geometry and suffer from high waste due to run-in and run-out issues, leading to inefficient use of precious metals and increased costs.

Method used

A method involving a traveling application unit moving in a closed loop with variable speeds to control relative speeds with the web material, allowing for optimal coating parameters to be achieved without abrupt stops, thus eliminating waste and enabling direct formation of target geometries without trimming.

Benefits of technology

This method reduces waste and recycling costs by ensuring precise coating directly to the target geometry, maintaining stable process control, and avoiding rejects, thereby optimizing the use of precious metals and improving coating quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024059170_24102024_PF_FP_ABST
    Figure EP2024059170_24102024_PF_FP_ABST
Patent Text Reader

Abstract

The invention relates to a method for coating a web material (30) with an application material (24) by means of at least one application unit (16, 50). The following method steps are carried out: According to step a), the web material (30) is conveyed in a conveying direction (32) at a substantially constant conveying speed v1; at least one accompanying application unit (50) runs at variable speed v in a closed loop (52) in a direction of rotation (54) according to method step b). According to method step c), the at least one accompanying application unit (50) is moved closer to the web material (30) and accompanies same at a speed v = v1. When optimum coating parameters are achieved, according to method step d), the relative speed between the at least one accompanying application unit (50) and the web material (30) is increased; according to method step e), a coating is applied to the application material (24) at a maximum relative speed between the web material (30) and the at least one accompanying application unit (50); and according to method step f), the at least one accompanying application unit (50) is accelerated to a speed v = v1 to complete the coating.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Method for coating a web material

[0002] Technical area

[0003] The invention relates to a method for coating a web material with a coating material using at least one application unit. Furthermore, the invention relates to the use of the method for coating a web material with a coating material, in particular for producing electrochemically active layers for lithium-ion batteries, fuel cells, or electrolysis cells.

[0004] State of the art

[0005] Methods for coating web material with thin, electrochemically active layers are based on the use of nozzles, doctor blades, screen printing, gravure printing, and spraying the coating. This is typically how electrochemically active layers—i.e., electrodes on the anode and cathode sides for lithium-ion batteries, fuel cells, or electrolysis cells—are produced. Particularly when slot nozzles are used for coating, it is very difficult to directly adjust the coating parameters to the desired target geometry. This is because, following an interruption of the coating process, the application unit, which is designed as a slot nozzle, and the flow conditions there, require a certain amount of time until the coating quality in the application area returns to the target state.When using slot-nozzle application units, a continuous coating process occurs, albeit with imperfections, until sufficient pressure is built up in the coating material to be applied, the flow conditions correspond to the target state, and the optimal coating condition is achieved. Only after a state of equilibrium is reached between the slot-nozzle application unit, the substrate, the web speed, and the application material does the coating reach its desired target state. Until this equilibrium is reached, the coated material is essentially unusable.

[0006] With application units designed as slot nozzles, targeted control of a cell geometry or stop-and-go coating are not trivial to implement, requiring cutting in subsequent work steps. The resulting waste, especially for coatings containing precious metals, such as those used in fuel cells, represents a significant avoidable cost factor.

[0007] Description of the invention

[0008] According to the invention, a method for coating a web material with an application material by means of at least one application unit is proposed, wherein the following method steps are carried out: a) conveying the web material in a conveying direction at a substantially constant conveying speed vi, b) circulating at least one traveling application unit in a closed loop in a circulating direction at a variable speed v such that c) the at least one traveling application unit approaches the web material at a speed v = vi, d) increasing the relative speed between the at least one traveling application unit and the web material when optimal coating parameters are reached,e) a layer of the coating material is applied at maximum relative speed between the web material and the at least one traveling application unit, and f) to complete the coating, the at least one traveling application unit is accelerated to a speed v = vi.

[0009] According to the method proposed according to the invention, an abrupt stop-and-go procedure can be avoided; rather, the method proposed according to the invention creates relative speeds between the web material and the at least one traveling application unit circulating in a closed loop in order to form the corresponding geometries of electrode material on the web material.

[0010] In an advantageous development of the method proposed according to the invention, the at least one traveling application unit passes through several working positions during its rotation along the closed loop. Thus, in an advantageous embodiment of the method proposed according to the invention, before the start of method step c), the application unit is brought closer to the web material, wherein the application material is brought to a fluid-dynamic target state within the at least one traveling application unit.

[0011] In a further advantageous embodiment of the method proposed according to the invention, in method step d) in order to increase the relative speed, the speed v of the at least one traveling application unit is braked and the application unit is moved further towards the web material.

[0012] In a further advantageous embodiment of the method proposed according to the invention, in order to generate the maximum relative speed according to method step e), the speed of the at least one traveling application unit is set to a speed v = 0. The coating process runs in a steady state, a coating meniscus is optimally developed.

[0013] In the method proposed in the invention, after process step f), the pressure in the at least one traveling application unit is reduced. The relative speed is reduced, the application unit is accelerated, and lifted off, which leads to the termination of the coating process. This allows excessive material stress and energy required for pressure generation to be saved until the start of the next application cycle.

[0014] In a further advantageous embodiment of the method proposed according to the invention, individual coating material segments with a rectangular geometry are formed on the upper side of the web material. This procedure can prevent waste that would otherwise occur or the formation of uneven contours on the upper side of the web material. By maintaining the same speed of the application unit relative to the web material (zero relative speed), no coating waste is generated per linear meter. The system between the substrate web, application unit, and flow conditions has time to adjust to a target state or to settle. During this time, no web material is wasted.

[0015] In an advantageous embodiment of the method proposed according to the invention, the individual application material segments are separated from one another by gaps on the upper side of the web material. These gaps can be created in a defined manner during the application process, so that waste strips that would otherwise occur and represent avoidable costs can be eliminated from the outset when applying the method proposed according to the invention.

[0016] The invention further relates to the use of the method for coating a web material with a coating material, in particular for producing electrochemically active layers for lithium-ion batteries or for fuel cells or for electrolysis cells.

[0017] Advantages of the invention

[0018] The method proposed according to the invention, on the one hand, avoids the high waste costs associated with contour trimming that occur in conventional coating processes. Precious metal-containing waste, which is both unfavorable in terms of resource utilization and represents high recycling and storage costs, can be eliminated by applying the method proposed according to the invention. Run-in and run-out behavior at the beginning and end of the coating process occurs entirely on the substrate web or web material to be coated, meaning that this too is no longer usable and constitutes waste.

[0019] In the solution proposed according to the invention, the at least one traveling application unit, preferably designed as a traveling slot nozzle, can advantageously avoid waste costs due to trimming, since no cutting is required; instead, the finished geometry of the electrochemically active layer is created directly during the manufacturing process. Furthermore, it should be emphasized that in the method proposed according to the invention, the infeed and outfeed behavior at the start and end of the coating process are not completely reproduced on the web material, so that the occurrence of rejects or web material with inferior coating quality can be significantly reduced and ideally completely avoided.Furthermore, a stable process control can be achieved by means of a suitable control system, whereby in particular an effective reduction or increase of relative speeds between the at least one traveling application unit and the web material continuously moving in the conveying direction can be maintained.

[0020] The solution proposed by the invention allows coating to be applied directly to the target geometry using slot nozzles; furthermore, a reduction in waste can be advantageously achieved by eliminating the need for trimming to the target geometry by coating to the target contour.

[0021] Short description of the drawings

[0022] Embodiments of the invention are explained in more detail with reference to the drawings and the following description.

[0023] They show:

[0024] Figure 1 shows a defective coating applied via an application unit, Figure 2 shows a continuous coating of an application material onto a web material transported in a conveying direction,

[0025] Figure 3 the creation of a target geometry by cutting gaps and resulting waste and

[0026] Figure 4 is a schematic representation of the method proposed according to the invention with at least one application unit circulating along a closed loop above a web material continuously conveyed in the conveying direction.

[0027] The illustration in Figure 1 shows that a substrate web 12, supported by a carrier 10, is coated on its upper side 14 with an application material 24. The application material 24 is applied essentially in a vertical direction via an application head 18 of an application unit 16. When the application material 24 shown here is applied to the upper side 14 of the substrate web 12, bubbles form and gaps form in the applied application material 24. Furthermore, bubble-shaped air inclusions 22 can be seen in the coating forming on the upper side 14 of the substrate web 12 in Figure 1, which significantly impair the quality of the resulting applied layer by the application material 24, which is why the coating made from the application material 24 and shown schematically in Figure 1 is almost unusable.

[0028] The illustrations in Figures 2 and 3 show a continuous application 36 of the application material 24 onto the upper side 14 of a web material 30 moving in the conveying direction 32, starting from an application start 34. In the illustration in Figure 2, the resulting continuous application web 36 is shown without steps, i.e. without interruptions, and passes through a drying unit 38. Starting from the illustration in Figure 2, individual specific geometries can be configured for later use by a blank as shown in Figure 3. In the illustration in Figure 3, the application material 24 is applied to the upper side 14 of the web material 30 via the application head 18 of the application unit 16. Blanks 40 are produced by individual cutting operations, which are separated from one another by gaps 42 resulting from the cutting.The material from the gaps 42 represents waste pieces 46, which generate a relatively high cost factor because they contain precious metal-containing coating residues from the application material 24 supplied via the application unit 16. The individual blanks 40 obtained essentially have a rectangular geometry 44, as shown in Figure 3.

[0029] Embodiments of the invention

[0030] In the following description of the embodiments of the invention, identical or similar elements are designated by the same reference numerals, whereby a repeated description of these elements is omitted in individual cases. The figures only schematically illustrate the subject matter of the invention.

[0031] Figure 4 shows an embodiment variant of the method proposed according to the invention.

[0032] Above the web material 30 moving in the conveying direction 32 at a speed vi, at least one traveling application unit 50 is accommodated such that the at least one traveling application unit 50 moves within a closed loop 52 in a direction of rotation 54. In the embodiment shown in Figure 4, the direction of rotation 54 is, for example, counterclockwise. The direction of rotation 54 is fundamentally dependent on the actual path of the web material 30.

[0033] In the region of the closed loop 52, which extends essentially parallel to the web material 30 conveyed in the conveying direction 32, the at least one traveling application unit 50 occupies a first position 56, a second position 58, a third position 60, a fourth position 62, a fifth position 64 and a sixth position 66. The first position 56 is a position in which the traveling application unit 50 has approached the web material 30. In the second position 58, a flow-dynamic target state of the application material has been established within the traveling application unit 50. In the third position 60, the traveling application unit 50 has moved closer to the web material 30. The fourth position 62 is a position in which the traveling application unit 50 is about to lift off from the web material 30.In the fifth position 64, the end of the coating process is imminent, whereas in the sixth position 66 the coating process is finished and the traveling application unit 50 moves away from the web material 30 and the fluid conveyance is stopped.

[0034] From the illustration according to Figure 4 it can further be seen that above the web material 30 conveyed in the conveying direction 32 there is at least one drying unit 38 by which the application material 24 applied to the web material 30 is dried.

[0035] The traveling application unit 50 moves from its first position 56 within the closed loop 52 via the second position 58, the third position 60 and the fourth position 62 at a speed v = vi, i.e., the conveying speed of the web material 30. During the passage through these positions 56 to 62, the application material 24 stored in the at least one traveling application unit 50 is brought to a target pressure by a conveying unit not shown in detail here, so that this target pressure is present within the at least one traveling application unit 50 at the start of the application. The coating process, i.e., the application of the application material 24 to the upper side 14 of the web material 30, which is moved in the conveying direction 32 at a speed vi, begins in the fourth position 62.Since the relative speed between the at least one traveling application unit 50 and the web material 30 is zero, the coating meniscus can build up. Only when the optimal coating parameters are reached is the relative speed between the at least one traveling application unit 50 and the web material 30 moving in the conveying direction 32 at the speed vi increased, which occurs by braking the at least one traveling application unit 50; this corresponds to the fourth position 62 as shown in Figure 4. At this point in time, the actual layer application begins, during which the relative speed between the at least one traveling application unit 50 and the web material 30 moving in the conveying direction 32 at the speed vi assumes its maximum value. Ideally, the at least one traveling application unit 50 is stationary.As soon as the end of the coating is reached, the at least one traveling application unit 50 is accelerated to a speed v = vi, i.e. to the conveying speed of the web material 30. During this acceleration phase, the relative speed decreases, as does the pressure on the application material 24 held in the at least one traveling application unit 50. This corresponds to the fifth position 64. Due to the identical speeds (relative speeds zero) between the at least one traveling application unit 50 and the web material 30, the run-out behavior is not depicted on the latter. At the end of the coating, the application material segments 70, which are each separated by gaps 42 in Figure 4 and which essentially have a rectangular geometry 44, are formed.These pass, separated from each other by gaps 42, beneath at least one drying unit 38, under which the application material 24 is dried and volatile substances are expelled from it. The end of the application is reached in the sixth position 66.

[0036] By means of the method proposed according to the invention, defective coatings with the application material 24 can be avoided, and furthermore, a target geometry of the application material 24 is created, in particular the rectangular geometry 44 shown in Figure 4, each separated from one another by gaps 42. This eliminates the need for subsequent cutting, thereby avoiding waste, which represents a considerable cost factor in the case of application material 24 containing precious metals, such as electrochemically active layers in fuel cells or electrolysis cells or lithium-ion batteries.

[0037] The invention is not limited to the embodiments described here and the aspects highlighted therein. Rather, numerous modifications are possible within the scope of the claims, which are within the scope of one skilled in the art.

Claims

Claims 1. A method for coating a web material (30) with an application material (24) by means of at least one application unit (16, 50), comprising the following method steps: g) conveying the web material (30) in a conveying direction (32) at a substantially constant conveying speed vi, h) circulating at least one traveling application unit (50) in a closed loop (52) in a direction of rotation (54) at a variable speed v such that i) the at least one traveling application unit (50) approaches the web material (30) at a speed v = vi, j) increasing the relative speed between the at least one traveling application unit (50) and the web material (30) when optimal coating parameters are reached,k) a layer of the coating material (24) is applied at maximum relative speed between the web material (30) and the at least one traveling application unit (50), and l) to complete the coating, the at least one traveling application unit (50) is accelerated to a speed v = vi.

2. Method according to claim 1, characterized in that the at least one traveling application unit (50) passes through several working positions (56-66) during its circulation along the closed loop (52).

3. Method according to claims 1 and 2, characterized in that before the start of method step c) the application material (24) is brought to a flow-dynamic target state (58) within the at least one traveling application unit (50).

4. Method according to claims 1 to 3, characterized in that in method step d) in order to increase the relative speed, the speed v of the at least one traveling application unit (50) is braked in a third position (60) moved toward the web material (30).

5. Method according to claims 1 to 4, characterized in that, in order to generate the maximum relative speed according to method step e), the at least one traveling application unit (50) assumes the speed v = 0 in a fourth, lifted position (62) 6. Method according to claims 1 to 5, characterized in that after method step f) the pressure in the at least one traveling application unit (50) is reduced in a fifth position (64) at the end of the coating.

7. Method according to claims 1 to 6, characterized in that individual application material segments (70) having a rectangular geometry (44) are formed on an upper side (14) of the web material (30).

8. Method according to claims 1 to 7, characterized in that the individual application material segments (70) are separated from one another by gaps (42).

9. Method according to claims 1 to 8, characterized in that due to a relative location of the traveling application unit (50) to the web material (30) to be coated, a coating meniscus is given sufficient time to form in an optimal manner.

10. Use of the method according to one of claims 1 to 9 for coating a web material (30) with a coating material (24), in particular for producing electrochemically active layers for lithium-ion batteries or for fuel cells or for electrolysis cells.

Citation Information

Patent Citations

  • Material application device and associated method

    DE102014224183B3

  • Intermittent coating device and intermittent coating method

    JP2014176826A