Method for manufacturing high-purity silicon powder
The method of drying and reducing waste silicon sludge in a specific atmosphere effectively removes SiO2 from waste silicon sludge, addressing the limitations of existing recycling methods and producing high-purity silicon powder with enhanced electrochemical properties for improved battery performance.
Patent Information
- Application Number
- PCT/KR2024/004711
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-19
- Filing Date
- 2024-04-09
- Publication Date
- 2024-10-24
AI Technical Summary
Existing methods for recycling waste silicon sludge to produce high-purity silicon powder are limited by the high cost of solid-liquid separation and the inability to increase silicon powder purity, particularly due to the presence of silica (SiO2), which affects the electrochemical properties of the silicon powder.
A method involving drying waste silicon sludge to produce waste silicon powder, followed by heating in a reducing atmosphere to remove moisture and SiO2, thereby reducing oxygen content and improving purity, using gases like H2 or CO, and optionally pulverizing the powder to enhance removal efficiency.
The method achieves ultra-high purity silicon powder with a significant reduction in SiO2 content, improving electrochemical properties and enabling its use as a superior anode material for secondary batteries by removing excess SiO2, which enhances electrical conductivity and reversibility.
Smart Images

Figure KR2024004711_24102024_PF_FP_ABST
Abstract
Description
High-purity silicon powder manufacturing method The present invention relates to a method for producing silicon powder. More specifically, the present invention relates to a method for producing high-purity silicon powder from waste silicon sludge. This application claims priority to Korean Patent Application No. 10-2023-0051483, filed April 19, 2023, the entire disclosure of which is incorporated herein by reference. Silicon wafers are produced by growing high-purity silicon into a silicon ingot in an electric furnace and then going through processes such as cutting and polishing, and are used in semiconductors and solar cells. Cutting fluids and abrasives are used in the cutting and polishing processes used to produce these silicon wafers. These processes generate a large volume of waste silicon slurry, a mixture containing used cutting fluids, abrasives, and silicon debris. Previously, this waste silicon slurry was typically discarded rather than recycled. Various attempts are being made to recycle this discarded waste silicon slurry. Korean Patent Publication No. 10-2016-0044178 discloses a method for obtaining highly purified silicon solids by dispersing the solids of waste silicon slurry in a liquid phase and performing solid-liquid separation. However, commercialization was not successful due to the high cost of the solid-liquid separation process. Accordingly, Korean Patent No. 10-2169875 discloses a method for producing high-purity silicon powder by removing water from waste silicon slurry through drying and removing organic compounds through heat treatment. However, Korean Patent No. 10-2169875 has a problem in that it fails to remove silica (SiO2) generated during the silicon wafer processing process, limiting its ability to increase the purity of the silicon powder. Accordingly, in order to solve the above problem, the inventors of the present invention propose a method for producing ultra-high purity silicon powder by efficiently removing silica contained in waste silicon sludge. [Prior Art Literature] [Patent Document] Prior Document 1. Republic of Korea Patent Publication No. 10-2016-0044178 (Published: April 25, 2016) Prior Document 2. Republic of Korea Patent No. 10-2169875 (Publication Date: October 26, 2020) The present invention aims to provide a method for producing ultra-high purity silicon powder by efficiently removing silica contained in waste silicon sludge in order to solve the above-mentioned problems. In order to solve the above problem, the present invention provides a method for producing silicon powder, comprising the steps of (S1) drying waste silicon sludge to produce waste silicon powder; and (S2) heating the waste silicon powder in a reducing atmosphere to remove moisture and oxygen of SiO2. According to a preferred embodiment of the present invention, the present invention may further include, after step S1, a step of pulverizing the waste silicon powder. According to a preferred embodiment of the present invention, the reducing atmosphere may be formed of a gas containing H2 or CO. According to a preferred embodiment of the present invention, the present invention can provide a method for manufacturing silicon powder by injecting an inert gas in the above S1. According to a preferred embodiment of the present invention, the inert gas may be Ar, He or N2, or a mixed gas of two or more selected from these. According to a preferred embodiment of the present invention, the present invention may be a manufacturing method in which the amount of SiO2 removed is 37.2% or more. The method of producing silicon powder from waste silicon sludge of the present invention enables the production of high-purity silicon powder with a low SiO2 content. SiO2 contained in silicon powder deteriorates the electrochemical properties of silicon, but the silicon powder of the present invention from which SiO2 is removed has excellent electrochemical properties. The following drawings attached to this specification illustrate preferred embodiments of the present invention and, together with the contents of the invention described above, serve to further understand the technical idea of the present invention, and therefore, the present invention should not be interpreted as being limited to matters described in such drawings. Figure 1 shows the results of X-ray diffraction analysis for Example 3 and Comparative Example 1 according to one embodiment of the present invention. Figure 2 is a silicon particle distribution diagram of Example 3 according to one embodiment of the present invention. Figure 3 is a silicon particle distribution diagram of Example 3' according to one embodiment of the present invention. Figure 4 is a photograph of a sample specimen of Example 3 according to one embodiment of the present invention. Figure 5 is an SEM photograph of Example 3 according to one embodiment of the present invention. Hereinafter, the present invention will be described in detail with reference to the drawings. Terms and words used in this specification and claims should not be construed as limited to their conventional or dictionary meanings. Based on the principle that the inventor can appropriately define the meaning of terms to best explain his or her invention, they should be interpreted in the sense and concepts consistent with the technical spirit of the present invention. The method of producing silicon powder from waste silicon sludge of the present invention enables the production of high-purity silicon powder with a low SiO2 content. While SiO2 contained in silicon powder deteriorates the electrochemical properties of silicon, the silicon powder of the present invention from which SiO2 has been removed exhibits excellent electrochemical properties. During processing such as cutting and polishing of silicon wafers, high heat is generated, and during this process, a SiO2 oxide film is formed on the surface of silicon crumbs, so waste silicon sludge contains a large amount of SiO2. In particular, when silicon powder containing such a large amount of SiO2 is used as a secondary battery anode material, it may exhibit low reversible capacity and initial irreversibility due to the low electrical conductivity of the silicon powder caused by SiO2. In addition, silicon powder containing excessive SiO2 may cause a problem in which the capacity decreases as the cycle progresses due to the formation of an unstable interphase layer (SEI, Solid Electrolyte Interphase) on the electrode due to the electrolyte decomposition reaction. Accordingly, the present invention provides a high-purity silicon powder having a minimized SiO2 content by removing oxygen from SiO2 and reducing it to Si. The method for manufacturing silicon powder of the present invention comprises the steps of (S1) drying waste silicon sludge to manufacture waste silicon powder; and (S2) heating the waste silicon powder in a reducing atmosphere to remove moisture and oxygen of SiO2. First, waste silicon sludge is dried to produce waste silicon powder (step S1). Waste silicon slurry is a mixture containing cutting oil, abrasives, and silicon chips generated during silicon wafer processing processes such as cutting and polishing. Waste silicon sludge is produced by removing liquids such as water from waste silicon slurry through a dehydration process such as a filter press. The above-mentioned waste silicone sludge does not have a specific range of moisture content, but it is preferable to use one having a moisture content of 70 wt% or less. It is preferable that the moisture content of the above-mentioned waste silicone powder is 5 wt% or less. The above-mentioned waste silicone sludge is dried by heating, and the method is not particularly limited, and an airflow drying method can be used. There is no specific limitation on the drying temperature, but the drying can be carried out at 150 to 200°C. If the drying temperature is lower than 150°C, the drying efficiency is poor, resulting in a long drying time. If the drying temperature exceeds 200°C, there may be a problem of increased oxidation of silicon. However, if an inert gas is injected, the oxidation of silicon can be prevented from increasing even when the drying temperature exceeds 200°C. Additionally, the present invention can inject an inert gas. This inert gas can prevent silicon from reacting with oxygen, etc. The type of inert gas is not particularly limited, but Ar, He, N2, or a mixture of two or more thereof can be used. Also, there is no specific limit to the drying time, but it is recommended to dry for 1 to 3 hours. Finally, the above-mentioned waste silicon powder is heated in a reducing atmosphere to remove moisture and oxygen of SiO2 to produce silicon powder (step S2). The above-mentioned waste silicon powder is heated in a reducing atmosphere to remove moisture and oxygen from SiO2. The type of reducing atmosphere is not particularly limited, but it is preferable to use a gas containing H2 or CO. When H2 is used as a gas for the above reducing atmosphere, H2 reacts with the oxygen of SiO2 to produce H2O and form Si. When CO is used as a gas for the above reducing atmosphere, CO reacts with the oxygen of SiO2 to produce CO2 and form Si. It is recommended that the heating temperature be 600°C or higher. If the heating temperature is lower than 600°C, SiO2 reduction may not be active. However, if the heating temperature exceeds 800°C, agglomeration of the silicon powder may occur. The heating time at this time is not particularly limited, but it is preferable to heat for 1 to 3 hours. It is preferable that the moisture content of the above silicone powder is 1 wt% or less. According to a preferred embodiment of the present invention, the manufacturing method of the present invention may optionally further include, after step S1, a step of pulverizing the waste silicon powder. By crushing the above-mentioned waste silicon powder, lumps are removed and the uniformity of particle size is increased, so that the surface area in contact with the reducing atmosphere gas increases, facilitating the removal of moisture and oxygen from SiO2. Hereinafter, preferred embodiments and comparative examples of the present invention are described. However, the following examples are only preferred embodiments of the present invention, and the present invention is not limited to the following examples. Example 1. Production of high-purity silicon powder from waste silicon sludge. Waste silicon sludge with a moisture content of 48 wt% was prepared from waste silicon sludge from TSMC, Taiwan, and processed through a filter press. 1 kg of the above waste silicon sludge was dried at 180°C for 2 hours using a self-made air dryer to produce waste silicon powder. The weight of the waste silicon powder was 545 g, and the moisture content at this time was confirmed to be 4.59 wt%. By preparing hydrogen gas and injecting it into a heating device to create a reducing atmosphere, the waste silicon powder was heated at 600°C for 2 hours to produce silicon powder. The weight of the silicon powder thus produced was 509 g, and the moisture content at this time was confirmed to be 0.20 wt%. ClassificationHeating temperature (℃)Reducing atmosphere Whether or not Silicon powder weight (g)Moisture content (wt%)Example 1600Hydrogen 5090.20Example 2650Hydrogen 5080.20Example 3750Hydrogen 5060.20Example 4800Hydrogen 5060.20Comparative example 1350-5210.19Comparative example 2550Hydrogen 5210.19Comparative example 3650-5230.19 Examples 2 to 4. Production of high-purity silicon powder from waste silicon sludge. Silicon powders of Examples 2 to 4 were manufactured according to the heating conditions and reducing atmosphere shown in Table 1 above using the same process as Example 1. Comparative Examples 1 to 3. Production of high-purity silicon powder from waste silicon sludge. The silicon powders of Comparative Examples 1 to 3 were manufactured according to the heating conditions and reducing atmosphere shown in Table 1 using the same process as in Example 1. Test Example 1. Measurement of oxygen content of SiO2 according to X-ray diffraction analysis results of manufactured waste silicon powder and silicon powder Using a SmartLab X-ray diffraction analyzer from Rigaku, Example 3 and Comparative Example 1 were measured under conditions of an acceleration voltage of 45 kV and a current of 200 mA, and the results are shown in Fig. 1. The peak for SiO2 was relatively higher in Comparative Example 1 than in Example 3, confirming that Comparative Example 1 had a high content of SiO2. Test Example 2. Measurement of the oxygen content of SiO2 in manufactured waste silicon powder and silicon powder. Using the Leco ONH 836CR model, the oxygen content of SiO2 of the waste silicon powder and silicon powder for Examples 1 to 4 and Comparative Examples 1 to 3 was measured, and the results are shown in Table 2 below. In addition, the oxygen content was converted to the weight part of SiO2 per 100 weight parts of silicon powder excluding moisture and is shown in Table 2 below. Classification Waste Silicon Powder Silicon Powder Oxygen (wt%) SiO2 (wt%) Oxygen (wt%) SiO2 (wt%) SiO2 Removal Amount Example 16.0211.293.787.0937.2 % Example 26.0211.293.466.4942.5 % Example 36.0211.293.175.9447.4 % Example 46.0211.293.216.0246.7 % Comparative Example 16.0211.296.0711.38- 0.8 % Comparative Example 26.0211.295.9811.210.7 % Comparative Example 36.0211.296.4212.04- 6.6 % According to the results in Table 2 above, the waste silicon powder may contain 11.29 parts by weight of SiO2 per 100 parts by weight of silicon powder excluding moisture. In addition, the silicon powder heated in a reducing atmosphere may contain 7.09 parts by weight or less of SiO2 per 100 parts by weight of silicon powder excluding moisture. The amount of SiO2 removed was calculated by comparing the content of SiO2 before and after the heating process using the following mathematical formula 1, and is shown in Table 2 above. According to Table 2 above, in the cases of Examples 1 to 4, it can be confirmed that the amount of SiO2 removed is 37.2% or more. On the other hand, in the cases of Comparative Examples 1 and 2, there was almost no change in the content of SiO2, and in the case of Comparative Example 3, it was confirmed that the content of SiO2 actually increased by 6% or more. Furthermore, the above comparative example 1 is the Korean Patent No. 10-2169875 of the above prior art document 2.
[0060] ~
[0064] It was confirmed that there was almost no change in the SiO2 content when the experiment was conducted under similar conditions to “Example 1”. Test Example 3. Particle Distribution Measurement Example 3': The silicon powder of Example 3' was manufactured by carrying out the same conditions as Example 3, but adding a process of grinding the waste silicon powder using a ball mill for 30 minutes. For the above examples 3 and 3', particle distribution was measured using Anton Paar's PSA 1090L and is shown in Figs. 2 and 3, respectively. Comparing Figures 2 and 3, it can be seen that the particle distribution of Example 3 is more uniform. Test Example 4. SEM Analysis SEM analysis for Example 3 was performed and is shown in Fig. 5. According to Fig. 5, it is confirmed that the silicon powder of Example 3 has a shape similar to sawdust, which is because it is a by-product of the silicon wafer processing process. In particular, the silicon powder having the form of sawdust has a large surface area and thus has excellent electrochemical performance.
Claims
1. (S1) A step of drying waste silicon sludge to produce waste silicon powder; and (S2) A method for manufacturing silicon powder, comprising the step of heating the above-mentioned waste silicon powder in a reducing atmosphere to remove moisture and oxygen of SiO2.
2. In paragraph 1, (S1') A method for manufacturing silicon powder, characterized in that it further comprises a step of crushing the waste silicon powder after the step S1.
3. In paragraph 1, A method for manufacturing silicon powder, characterized in that the reducing atmosphere is composed of a gas containing H2 or CO.
4. In paragraph 1, A method for manufacturing silicon powder, characterized by injecting an inert gas in the above S1.
5. In paragraph 4, A method for manufacturing silicon powder, characterized in that the above inert gas is Ar, He or N2, or a mixed gas of two or more selected from these.
6. In paragraph 1, A method for manufacturing silicon powder, characterized in that the amount of SiO2 removed is 37.2% or more. [Mathematical Formula 1]
Citation Information
Patent Citations
Silicon purification method and silicon purification apparatus
JP5244500B2
Process for the preparation of silicone powder from wastesilicone
KR100177139B1
Method for refining waste solar cells using steam plasma
KR101837308B1
Recovery method of high purity silicon powder from Waste sludge and Silcon powder recovered using the same method
KR102169875B1
Method for recovering silicon for silicon anode materials
KR102491604B1