Precursor compound for thin film formation and method for manufacturing semiconductor device using same

The use of a precursor compound with specific functional groups for forming an ultra-thin lower layer in semiconductor devices addresses the issue of photoresist layer damage during etching, improving pattern formation and device performance by reducing etching times and costs.

WO2024219908A1PCT designated stage expired Publication Date: 2024-10-24SK HYNIX INC +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2024/095197
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-18
Filing Date
2024-02-15
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

In semiconductor device manufacturing, the photoresist layer is often damaged during etching due to its poor pattern shape and the etching of the lower layer, leading to reduced device performance.

Method used

A precursor compound for forming a thin film is used, specifically containing materials like Si, Sn, or Ge, with functional groups that enhance bonding with the photoresist and substrate, allowing for an ultra-thin lower layer formation through atomic layer deposition, minimizing etching damage and exposure time.

Benefits of technology

This approach prevents pattern collapse of the photoresist layer by reducing the thickness of the lower layer to 10 Å or less, shortening exposure and etching times, and improving bonding strength, thereby enhancing semiconductor device performance and reducing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2024095197_24102024_PF_FP_ABST
    Figure KR2024095197_24102024_PF_FP_ABST
Patent Text Reader

Abstract

The present techniques provide a precursor compound of [chemical formula 1] for thin film formation and a preparation method therefor, wherein a photoresist layer can be prevented from undergoing pattern collapse by reducing the exposure time for pattern formation and minimizing the thickness of a lower layer with an etching selectivity similar to that of a photoresist or omitting the lower layer during post-exposure etching. (In [chemical formula 1], R0 is Si, Sn, Ge, Sb, In, Hf, Zr, Ti, or Te; R1 is CH3, CF3, CH=CH2, halogen, or phenyl; R2 and R2' each are independently alkyl or alkoxy; R3 is amine or halogen; R is hydrogen or halogen; n is an integer of 1-7)
Need to check novelty before this filing date? Find Prior Art

Description

Precursor compound for forming a thin film and method for manufacturing a semiconductor device using the same

[0001] The present invention relates to a precursor compound for forming a thin film and a method for manufacturing a semiconductor device, and more particularly, to a precursor compound for a lower layer formed under a photoresist layer and a method for manufacturing a semiconductor device using the same.

[0002] Photolithography is a technology that forms high-resolution circuitry within a semiconductor device by exposing a photoresist (hereinafter referred to as “resist”) on a substrate to a light source.

[0003] Lithography technology using the above resist can be typically performed in the following manner.

[0004] First, a resist composition including a polymer matrix, a photoacid generator, a solvent, and other performance-enhancing additives is spin-coated on a silicon wafer, and then cured to form a resist film. Next, the formed resist film is pattern-wise exposed to a light source and selectively heated to induce a post-exposure bake (PEB) chemical transformation. This chemical transformation causes a difference in solubility between exposed and unexposed areas of the resist film, and a solvent-based development process is performed to create a resist pattern image on the wafer. In the exposure process, radiation having wavelengths ranging from near ultraviolet (UV) to deep ultraviolet (DUV) and extreme ultraviolet (EUV) is typically used as a light source.

[0005] These lithography processes typically utilize a laminate comprising a substrate, a sublayer, and a photoresist layer. Post-exposure etching is performed to form a pattern on the laminate, selectively etching the sublayer to form the pattern. However, in actual application, the photoresist layer on the surface is etched together with the substrate during post-exposure etching, resulting in poor pattern quality and degraded performance of the semiconductor device.

[0006] An embodiment of the present invention provides a precursor compound for forming a thin film and a method for producing the same, which can prevent pattern collapse of a photoresist layer by shortening the exposure time for pattern formation and minimizing or omitting the thickness of a lower layer having an etching selectivity similar to that of a photoresist during etching after exposure.

[0007] A precursor compound for forming a thin film according to an embodiment of the present invention may be a precursor compound for forming a thin film including a material of [chemical formula 1].

[0008] [Chemical Formula 1]

[0009] (In the above [chemical formula 1], R 0 is Si, Sn, Ge, Sb, In, Hf, Zr, Ti or Te, and R 1 is CH3, CF3, CH=CH2, halogen or phenyl, and R 2 and R 2 ' are each independently an alkyl group or an alkoxy group, and R 3 is an amine or halogen, R is hydrogen or halogen, and n is an integer from 1 to 7.

[0010] Preferably, R of the above [chemical formula 1] 0 is Si or Sn, and R 1 is CF3 or I, and R 2 and R 2 ' are each independently CH3, C2H5, C3H7, OCH3, OC2H5, and R 3is N(CH3)2, N[(CH2)CH3]2, and R can be H, and in the above [chemical formula 1], n can be an integer from 1 to 4.

[0011] A method for manufacturing a semiconductor device according to an embodiment of the present invention may include: a step of preparing a substrate; a step of preparing a precursor including a material of [chemical formula 1], which is a material for forming a lower layer; a step of depositing a precursor including a material of [chemical formula 1] on the substrate using an atomic layer deposition (ALD) method to form a lower layer; and a step of forming a photoresist layer on the lower layer.

[0012] The step of forming the above lower layer includes a step of supplying a precursor including the material of the above [chemical formula 1] and a step of supplying a purge gas, and a cycle in which the step of supplying the precursor and the step of supplying the purge gas are defined as one cycle may be repeated at least once.

[0013] This technology can prevent pattern collapse of the photoresist layer by shortening the exposure time for pattern formation and minimizing or omitting the thickness of the lower layer that has an etching selectivity similar to that of the photoresist during post-exposure etching.

[0014] In addition, the lower layer can be formed into an ultra-thin film of less than 10 Å while sufficiently securing adhesion between the photoresist layer and the substrate.

[0015] FIG. 1 is a drawing schematically illustrating a stacked structure of a semiconductor device (100) according to the present embodiment.

[0016] Figure 2 is a process flow chart for explaining a method for manufacturing a semiconductor device of the present embodiment.

[0017] FIG. 3 is a schematic diagram illustrating a precursor deposition process according to one embodiment.

[0018] Terms or words used in this specification and claims should not be interpreted as limited to their usual or dictionary meanings, but should be interpreted as meanings and concepts that conform to the technical ideas of the present embodiment, based on the principle that the inventor can appropriately define the concept of the term to best explain his or her own invention.

[0019] The terms used herein are for the purpose of describing exemplary embodiments only and are not intended to be limiting. Singular expressions include plural expressions unless the context clearly dictates otherwise.

[0020] The identifiers used in each step are for convenience of explanation and do not indicate the order of the steps. The steps may be performed in a different order than stated, unless the context clearly dictates otherwise. In other words, the steps may be performed in the same order as stated, substantially simultaneously, or in the opposite order.

[0021] In this specification, it should be understood that the terms “include,” “comprising,” or “having” are intended to specify the presence of a feature, number, step, component, or combination thereof, but do not preclude the possibility of the presence or addition of one or more other features, numbers, steps, components, or combinations thereof.

[0022] The atomic layer deposition (ALD) process may be performed as one cycle of a. source gas injection, b. purge, c. reaction gas injection, and d. purge, or may include a half atomic layer deposition process performed as one cycle of two steps of a'. gas injection and b'. purge. In the present specification, the “atomic layer deposition process using a precursor compound of [chemical formula 1]” may be performed as such a half atomic layer deposition process.

[0023] Referring to FIG. 1, the present embodiment relates to a precursor compound for forming a thin film and a method for producing the same. More specifically, the precursor compound for forming a thin film is formed on a substrate (110) and can form a lower layer (120) formed under a photoresist layer (130).

[0024] The precursor compound for forming a thin film according to the present embodiment can be expressed by [chemical formula 1].

[0025] [Chemical Formula 1]

[0026] (In the above [chemical formula 1], R 0 is Si, Sn, Ge, Sb, In, Hf, Zr, Ti or Te, and R 1 is CH3, CF3, CH=CH2, halogen or phenyl, and R 2 and R 2 ' are each independently an alkyl group or an alkoxy group, and R 3 is an amine or halogen, R is hydrogen or halogen, and n is an integer from 1 to 7.

[0027] Preferably, a precursor comprising the above [chemical formula 1] is R 0 is Si or Sn, and R 1 is CF3 or I, and R 2 and R 2' are each independently CH3, C2H5, C3H7, OCH3 or OC2H5, and R 3 Compounds can be used in which N(CH3)2 or N[(CH2)CH3]2, R is H, and n is an integer from 1 to 4.

[0028] Among the precursors containing the above [chemical formula 1], precursors represented by the following chemical formulas 2 to 9 can be applied.

[0029] [Chemical Formula 2]

[0030] [Chemical Formula 3]

[0031] [Chemical Formula 4]

[0032] [Chemical Formula 5]

[0033] [Chemical Formula 6]

[0034] [Chemical Formula 7]

[0035] [Chemical Formula 8]

[0036] [Chemical Formula 9]

[0037] The precursor material represented by the above [chemical formula 1] is a precursor compound capable of forming a thin film or a metal thin film on a semiconductor substrate, and a hydrophobic group such as an alkyl or olefin is formed at one end, and an amine group or a halogen group is formed at the other end, so that a bonding force can be formed between one end and the photoresist layer (130) and the other end with the substrate (110).

[0038] Specifically, a straight carbon chain such as alkyl or olefin is formed at one end of the precursor material represented by [Chemical Formula 1], so that the bonding strength can be improved by enhancing the van der Waals force and the bonding strength can be improved by physical entanglement of the straight carbon chain and the photoresist layer (130), and the bonding strength with the photoresist layer (130) can be improved by improving the surface deposition coverage through the formation of a self-assembling monolayer. In addition, R 1 As the functional group is introduced, the dipole moment is improved, and the bonding strength with the hydrophobic photoresist layer (130) can be further improved.

[0039] In particular, R 1 In this case of CF3, the hydrophobicity increases further, further improving the bonding strength with the photoresist layer (130), and when exposed for pattern formation, the absorbance for the EUV light source becomes excellent, so the EUV irradiation amount for pattern formation can be reduced.

[0040] Additionally, when a halogen substance is included as a functional group, the EUV irradiance can be reduced due to the excellent absorption efficiency of the halogen substance itself.

[0041] Fig. 2 is a process flow chart for explaining a method for manufacturing a semiconductor device according to the present embodiment. The method for manufacturing a semiconductor device according to the present embodiment will be explained with reference to Fig. 2. In addition, for convenience of explanation, a semiconductor device manufactured according to the present embodiment is illustrated in Fig. 1.

[0042] First, FIG. 1 is a drawing schematically illustrating a laminated structure of a semiconductor device (100) manufactured according to a method for manufacturing a semiconductor device of the present embodiment.

[0043] A semiconductor device (100) manufactured according to the method for manufacturing a semiconductor device of the present embodiment includes a substrate (110); a lower layer (120) formed by depositing a precursor of [chemical formula 1] on the substrate (110); and a photoresist layer (130) formed on the lower layer (120).

[0044] [Chemical Formula 1]

[0045] (In the above [chemical formula 1], R 0 is Si, Sn, Ge, Sb, In, Hf, Zr, Ti or Te, and R 1 is CH3, CF3, CH=CH2, halogen or phenyl, and R 2 and R 2 ' are each independently an alkyl group or an alkoxy group, and R 3 is an amine or halogen, R is hydrogen or halogen, and n is an integer from 1 to 7.

[0046] The precursor containing the above [chemical formula 1] is the same as described above, so redundant description is omitted.

[0047] The above substrate (110) is capable of forming elements, circuits, films, etc., and includes a base substrate (111) and a surface film (112). The base substrate (111) may be formed of a group IV material such as silicon or germanium, or may be formed of a compound such as a group III-V material such as GsAs, GaN, InP, InGaN, etc., a group II-VI material such as ZnSe, and a group IV-IV material such as SiC or SiGe.

[0048] The surface of the substrate (110) may include silicon oxynitride (SiON) or amorphous carbon. Specifically, the substrate may have a surface film (112) formed thereon containing silicon oxynitride or amorphous carbon. For example, the substrate (110) may include a silicon oxynitride film or an amorphous carbon film as the surface film (112) on the surface.

[0049] In this way, the substrate (110) containing silicon oxynitride or amorphous carbon on the surface has a hydrophilic surface, so when the precursor represented by [chemical formula 1] contains an amine group, it can form a high bonding force with the substrate (110), and a film can be easily formed by depositing the precursor represented by [chemical formula 1] on the substrate (110).

[0050] The above lower layer (120) can be formed through an atomic layer deposition process or a half atomic layer deposition process.

[0051] A precursor represented by [chemical formula 1] can be deposited on a substrate (110) through an atomic layer deposition process to form a lower layer (120), and the thickness of the lower layer (120) can be 10 Å or less, and can be 1 to 10 Å.

[0052] The conventional lower layer (120) is formed by spin coating and is formed thicker than 50 Å. In this case, since the minimum amount of light irradiation required for pattern formation of a semiconductor is large and the etching time is long, only the lower layer (120) must be selectively etched during the pattern formation process, but the photoresist layer (130) is also etched, causing a problem of pattern collapse.

[0053] Since the semiconductor device (100) of the present embodiment forms the lower layer (120) using the atomic layer deposition method, it is possible to form the lower layer (120) having a thickness of 10 Å or less. At this time, if the lower layer (120) is implemented in the form of an ultra-thin film, the amount of light irradiation for pattern formation can be reduced and the etching time can be shortened, so that the pattern can be formed without damaging the photoresist layer (130). In addition, since the amount of etching solution used during etching can be reduced, the cost consumed in the process can be reduced.

[0054] The atomic layer deposition method may include a step of first vaporizing a liquid precursor represented by [chemical formula 1], depositing it on a substrate (110), and purging it, and the deposition and purging may be performed repeatedly multiple times as one cycle.

[0055] At this time, when transporting the vaporized precursor of [chemical formula 1], an inert gas such as argon (Ar), nitrogen (N2), and helium (He) may be used together as a carrier gas, but the type thereof is not limited thereto. In addition, the purge gas used in the purge step may also be an inert gas as described above, but is not limited thereto.

[0056] The photoresist layer (130) formed on the lower layer (120) may include at least one of the CAR (Chemical amplified Resist) Type and the MOR (Metal Oxide Resist) Type.

[0057] FIG. 2 is a process flow chart for explaining a method for manufacturing a semiconductor device (100) of the present embodiment. The method for manufacturing a semiconductor device (100) of the present embodiment is explained with reference to FIG. 2.

[0058] The present embodiment includes a method for manufacturing a semiconductor device (100), including a step (S10) of preparing a substrate (110); a step (S20) of preparing a precursor of [chemical formula 1], which is a material for forming a lower layer (120); a step (S30) of depositing a precursor of [chemical formula 1] on the substrate (110) using an atomic layer deposition (ALD) method to form a lower layer (120); and a step (S40) of forming a photoresist layer (130) on the lower layer (120).

[0059] The precursor represented by the above [chemical formula 1] is the same as that described above, so redundant description is omitted.

[0060] Step S10 is a step for preparing a substrate (110), and may be a step for introducing the substrate (110) into a reaction chamber.

[0061] The above substrate (110) is formed with a device, circuit, film, etc., and includes a base substrate (111) and a surface film (112). The base substrate (111) may be formed of a group IV material such as silicon or germanium, or may be formed of a compound such as a group III-V material such as GsAs, GaN, InP, InGaN, etc., a group II-VI material such as ZnSe, and a group IV-IV material such as SiC or SiGe.

[0062] The surface of the substrate (110) may include silicon oxynitride or amorphous carbon. Specifically, the substrate may have a surface film (112) formed thereon containing silicon oxynitride or amorphous carbon. For example, the substrate (110) may include a silicon oxynitride film or an amorphous carbon film as the surface film (112) on the surface.

[0063] The above step S20 is a step for preparing a precursor including [chemical formula 1], which is a material for forming a lower layer (120). Since the precursor including [chemical formula 1] exists in a liquid state at room temperature, the precursor can be vaporized through a vaporizer in this step to apply the precursor to an atomic layer deposition (ALD) method.

[0064] The above step S30 is a step of supplying a precursor containing [chemical formula 1] to a chamber and reacting it to form a lower layer (120), and the step of supplying a precursor containing [chemical formula 1] (S31) and the step of supplying a purge gas (S32) can be performed at least once by repeating the cycle. This step can be performed in a temperature range of 100 to 250°C, and R 0 Inland R 3 Since each type of precursor defined according to the precursor has a different decomposition temperature, it is preferable to perform the process at a temperature lower than the decomposition temperature of the precursor.

[0065] In step S31, a precursor containing vaporized [chemical formula 1] is supplied in a gaseous state to a chamber containing a substrate (110), and at this time, an inert gas such as argon (Ar), nitrogen (N2), and helium (He) may be supplied to the chamber together with the precursor containing vaporized [chemical formula 1] as a carrier gas.

[0066] The amine group formed at one end of the precursor supplied to the chamber containing the substrate (110) has a hydrophilic characteristic, and thus can be deposited as a thin film on the surface of the substrate (110) by combining with silicon oxynitride or amorphous carbon having a hydrophilic characteristic on the surface of the substrate (110). Specifically, the amine group of the precursor including [Chemical Formula 1] can form a monolayer arranged in a row by combining with a reaction portion formed by degassing at a high temperature and a nucleophile such as a hydroxyl group, an amino group, or an sp2 carbon bond on the surface of the substrate (110). This series of processes can be more clearly understood through FIG. 3.

[0067] FIG. 3 is a drawing exemplarily illustrating a deposition process of a precursor comprising [Chemical Formula 1] according to one embodiment. In the embodiment shown in FIG. 3, a precursor represented by [Chemical Formula 1] in which R is H is exemplarily described.

[0068] First, when the precursor of [chemical formula 1] is exposed to heat, the hydroxyl group or amino group or unsaturated bond, which is a nucleophile of the surface film (112) of the substrate (110), and the R of the precursor 0 are combined and R 3 is dropped, and accordingly, a precursor containing [chemical formula 1] is combined in a row on the surface of the surface film (112) to form a single film.

[0069] Meanwhile, step S32 is performed to purge byproducts including unreacted reactants and gaseous products generated through the reaction in the previous step, and can be performed by supplying an inert gas into the chamber. At this time, the inert gas may include, but is not limited to, argon (Ar), nitrogen (N2), and helium (He).

[0070] The above step S40 is a step of forming a photoresist layer (130) on the lower layer (120), and may be a step of forming the photoresist layer (130) on the lower layer (120) using an atomic layer deposition method. At this time, the photoresist layer (130) may be formed of or include at least one material of the CAR (Chemical amplified Resist) Type and the MOR (Metal Oxide Resist) Type.

[0071] As described above, the lower layer (120) is formed in the form of a single film in which the precursor including [chemical formula 1] is arranged in a row, and at this time, the hydrophilic part is arranged toward the substrate (110), and the hydrophobic part of the alkyl or olefin carbon chain structure is arranged on the opposite side, so that when the lower layer (120) is deposited on the substrate (110) through the step of forming the lower layer (120), the surface of the lower layer (120) exposed to the outside exhibits hydrophobic characteristics. Therefore, when the photoresist layer (130) is formed on the surface of the hydrophobic lower layer (120) using a photoresist material, a van der Waals force acts between the hydrophobic surface of the lower layer (120) and the hydrophobic photoresist layer (130), forming a strong bonding force, and the carbon chain structure of the precursor including [chemical formula 1] can be entangled with the photoresist layer (130) to form an additional bonding force. In particular, R of the precursor [chemical formula 1] 1 When this is CF3 or phenyl group, the bonding strength with the photoresist layer is further improved, and the bonding strength in the case of CF3 is the best.

[0072] The semiconductor device (100) according to the present embodiment can reduce the EUV irradiance for pattern formation by improving the EUV absorption rate of the lower layer (120), and since the lower layer (120) is formed as a thin film of 10 Å or less through an atomic layer deposition process, the EUV exposure time of the photoresist layer (130) and the time it is exposed to an etchant can be shortened, thereby preventing damage (pattern collapse) of the photoresist layer (130), and reducing process costs and shortening the process time through reducing the irradiance, reducing the amount of etchant used, and reducing the pattern formation time can be achieved.

[0073] In addition, when compared with the semiconductor device (100) of the comparative example in which the lower layer (120) is formed by a conventional spin coating process, the semiconductor device (100) according to the present embodiment has a similar line width reduction (LWR) and a minimum critical dimension (CD) value at which the pattern is damaged, but the dose to size (DtS) can be significantly reduced, and a DtS reduction of about 3 to 30% can be confirmed compared to the conventional spin coating method.

[0074] Above, one embodiment of the present invention has been described, but a person having ordinary skill in the art will be able to modify and change the present invention in various ways by adding, changing, deleting or adding components, etc., within the scope that does not depart from the spirit of the present invention described in the claims, and this will also be considered to be included within the scope of the rights of the present invention.

[0075] The method for manufacturing a semiconductor device using a precursor compound for forming a thin film according to the present invention has the effect of preventing pattern collapse of a photoresist layer by shortening the exposure time for pattern formation and minimizing or omitting the thickness of a lower layer having an etching selectivity similar to that of a photoresist during etching after exposure, and therefore has industrial applicability.

Claims

1. A precursor compound for forming a thin film comprising a substance of [chemical formula 1]. [Chemical Formula 1] (In the above [chemical formula 1], R 0 is Si, Sn, Ge, Sb, In, Hf, Zr, Ti or Te, and R 1 is CH3, CF3, CH=CH2, halogen or phenyl, and R 2 and R 2 ' are each independently an alkyl group or an alkoxy group, and R 3 is an amine or halogen, R is hydrogen or halogen, and n is an integer from 1 to 7.

2. In paragraph 1, In the above [chemical formula 1], R 0 is Si or Sn, and R 1 is CF3 or I, and R 2 and R 2 ' are each independently CH3, C2H5, C3H7, OCH3, OC2H5, and R 3 A precursor compound for forming a thin film, wherein N(CH3)2, N[(CH2)CH3]2, and R is H.

3. In paragraph 2, A precursor compound for forming a thin film, wherein n in the above [chemical formula 1] is an integer from 1 to 4.

4. In paragraph 1, A precursor compound for forming a thin film, characterized in that the precursor compound for forming a thin film is any one of the substances represented by the following [chemical formula 2] to [chemical formula 9]. [Chemical Formula 2] [Chemical Formula 3] [Chemical Formula 4] [Chemical Formula 5] [Chemical Formula 6] [Chemical Formula 7] [Chemical Formula 8] [Chemical Formula 9] 5. In paragraph 1, The above precursor compound for forming a thin film is a precursor compound for forming a thin film on the surface of a semiconductor substrate.

6. In paragraph 5, A precursor compound for forming a thin film, wherein the thickness of the thin film is 10 Å or less.

7. In paragraph 5, A precursor compound for forming a thin film, which contains silicon oxynitride or amorphous carbon on the surface of the semiconductor substrate.

8. Step for preparing the substrate; A step of forming a lower layer by depositing a precursor of [chemical formula 1] on the substrate using an atomic layer deposition (ALD) method; and A method for manufacturing a semiconductor device, comprising: forming a photoresist layer on the lower layer. [Chemical Formula 1] (In the above [chemical formula 1], R 0 is Si, Sn, Ge, Sb, In, Hf, Zr, Ti or Te, and R 1 is CH3, CF3, CH=CH2, halogen or phenyl, and R 2 and R 2 ' are each independently an alkyl group or an alkoxy group, and R 3 is an amine or halogen, R is hydrogen or halogen, and n is an integer from 1 to 7.

9. In paragraph 8, The step of forming the above lower layer is: A step of supplying a precursor comprising the above [chemical formula 1] and a step of supplying a purge gas, A method for manufacturing a semiconductor device, wherein a cycle in which a step of supplying a precursor and a step of supplying a purge gas are defined as one cycle are repeated at least once.

10. In paragraph 8, A method for manufacturing a semiconductor device, wherein the step of forming the lower layer is performed at a temperature of 100 to 250°C.

11. In paragraph 8, A method for manufacturing a semiconductor device, wherein the surface of the substrate contains silicon oxynitride or amorphous carbon.

12. In paragraph 8, A method for manufacturing a semiconductor device, wherein the thickness of the lower layer is 10 Å or less.

13. In paragraph 8, A method for manufacturing a semiconductor device, characterized in that the precursor is any one of the materials represented by the following [chemical formula 2] to [chemical formula 9]. [Chemical Formula 2] [Chemical Formula 3] [Chemical Formula 4] [Chemical Formula 5] [Chemical Formula 6] [Chemical Formula 7] [Chemical Formula 8] [Chemical Formula 9]

Citation Information

Patent Citations

  • Surface processing method for wafer and composition to be used for the same

    JP2018182112A

  • Film formation composition, film-equipped substrate, manufacturing method thereof, and manufacturing method of thin film

    JP2019220494A

  • Vapor phase treatment of dielectric materials

    KR1020080002856A

  • Wireless positioning system and method based on multiple reference sensors

    KR1020220138494A

  • Method for supporting establishment and sharing of information on global company and information on collective intelligence regarding technology, server and user terminal using the same

    KR1020220149882A