Semiconductor device and method for manufacturing same
By adopting a multi-layer sacrificial layer structure in the manufacturing of MEMS devices, using an etching process that is not easily damaged to process the adjacent interface layer, and maintaining the conventional etching process to process other parts, the problems of interface layer damage and high cost are solved, and stability is achieved. and efficient manufacturing.
Patent Information
- Application Number
- PCT/CN2023/138488
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-28
- Filing Date
- 2023-12-13
- Publication Date
- 2024-10-31
AI Technical Summary
In the manufacturing process of MEMS devices, the interface layer is easily damaged by the etching reaction when the sacrificial layer is removed, resulting in device failure. Conventional etching processes are also costly and have limited productivity.
A multi-layer sacrificial layer structure is adopted. The adjacent interface layer uses an etching process that is not easily damaged. The other parts maintain the conventional etching process. The sacrificial layer is gradually removed through different etching processes to form a cavity structure and reduce interface layer damage.
It effectively reduces the damage to the interface layer, reduces costs and improves production capacity, ensuring the stability and efficient manufacturing of the device.
Smart Images

Figure CN2023138488_31102024_PF_FP_ABST
Abstract
Description
Semiconductor device and method for manufacturing the same
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This disclosure claims priority to Chinese patent application No. 202310474878.8, filed on April 28, 2023, which is incorporated herein by reference. Technical Field
[0003] The present disclosure relates to the field of semiconductor technology, and in particular to a semiconductor device and a method for manufacturing the same. Background Art
[0004] A micro-electro-mechanical system (MEMS) is a miniature system that integrates mechanical components, drive elements, optical systems, and electronic control systems. MEMS devices, with their advantages of small size and low power consumption, have found widespread application in smartphones, tablets, game consoles, automobiles, drones, and other fields. Similar to integrated circuits, MEMS devices are also developing towards high performance, miniaturization, low cost, and integration.
[0005] In related art, the cavity structure of a MEMS device is formed by removing a sacrificial layer between the MEMS functional layer and the sidewall layer through a release hole using a wet or dry etching process. However, an interface layer typically exists between the MEMS functional layer and the sidewall layer. When removing the sacrificial layer, the etching reaction gas or liquid can corrode the interface layer, causing a reaction and cracking between the MEMS functional layer and the sidewall layer, leading to serious process problems and device failure.
[0006] Summary of the Invention
[0007] The Summary of the Invention introduces a series of simplified concepts that will be further described in the Detailed Description of the Invention. The Summary of the Invention of this disclosure is not intended to limit the key features and essential technical features of the claimed technical solution, nor is it intended to determine the scope of protection of the claimed technical solution.
[0008] In order to solve the existing problems, the present disclosure provides a method for manufacturing a semiconductor device, the method comprising:
[0009] Providing a sensitive material layer, the sensitive material layer comprising a first surface and a second surface opposite to the first surface, wherein a first electrode is formed on the first surface;
[0010] forming a sacrificial layer and a sidewall layer surrounding the sacrificial layer on the first surface of the sensitive material layer, wherein the sacrificial layer includes a first sacrificial layer and a second sacrificial layer surrounding the first sacrificial layer, and the material of the first sacrificial layer is different from the material of the second sacrificial layer;
[0011] forming a release hole in the sidewall layer connected to the first sacrificial layer;
[0012] Using a first etching process to remove the first sacrificial layer inside the sidewall layer through the release hole;
[0013] Using a second etching process different from the first etching process to remove the second sacrificial layer through the release hole to form a cavity structure in the sidewall layer;
[0014] A first through hole is formed penetrating the sensitive material layer, and a first pad is formed on the second surface of the sensitive material layer and electrically connected to the first electrode via the first through hole.
[0015] In some embodiments, a second electrode is formed on the second surface of the sensitive material layer, and the method further includes: forming a second pad electrically connected to the second electrode on the second surface of the sensitive material layer.
[0016] In some embodiments, providing a sensitive material layer includes:
[0017] Providing a first substrate, and sequentially forming an isolation layer and the sensitive material layer on the first substrate, wherein the second surface of the sensitive material layer is in contact with the isolation layer;
[0018] After performing the second etching process and before forming the first through hole, the method further includes: removing the first substrate and forming a second substrate above the sidewall layer.
[0019] In some embodiments, before forming the second substrate, the method further includes:
[0020] A sealing layer is formed on the sidewall layer to seal the release hole.
[0021] In some embodiments, an interface layer is formed between the sidewall layer and the sensitive material layer, and an etching rate of the interface layer by the first etching process is greater than an etching rate of the interface layer by the second etching process.
[0022] In some embodiments, a material of the first sacrificial layer includes silicon oxide, and a material of the second sacrificial layer includes silicon.
[0023] In some embodiments, the sidewall layer includes a first sidewall layer and a second sidewall layer, and the first sidewall layer is disposed between the second sidewall layer and the second sacrificial layer.
[0024] In some embodiments, forming a sacrificial layer and a sidewall layer surrounding the sacrificial layer on the first surface of the sensitive material layer includes:
[0025] forming a first sacrificial layer on the first surface of the sensitive material layer;
[0026] Etching the first sacrificial layer to form a groove exposing the first surface of the sensitive material layer;
[0027] forming a second sacrificial layer on the first sacrificial layer, wherein the second sacrificial layer covers the bottom and sidewalls of the trench;
[0028] removing the second sacrificial layer at the bottom of the trench;
[0029] forming a first sidewall layer on the second sacrificial layer, wherein the first sidewall layer covers the bottom of the trench and covers the second sacrificial layer on the sidewall of the trench;
[0030] A second sidewall layer is formed on the first sidewall layer, and the second sidewall layer fills the trench.
[0031] In some embodiments, the second sacrificial layer includes a first portion of the second sacrificial layer and a second portion of the second sacrificial layer;
[0032] Before forming the first sacrificial layer on the first surface of the sensitive material layer, the method further includes: forming a first portion of a second sacrificial layer on the first surface of the sensitive material layer, wherein the first portion of the second sacrificial layer is located between the trenches;
[0033] The forming of the second sacrificial layer on the first sacrificial layer includes forming the second portion of the second sacrificial layer on the first sacrificial layer.
[0034] In some embodiments, a material of the first sidewall layer includes silicon oxide, and a material of the second sidewall layer includes silicon.
[0035] In some embodiments, the first etching process includes a wet etching process, and the second etching process includes a dry etching process.
[0036] In some embodiments, the sensitive material layer includes a piezoelectric layer.
[0037] Another aspect of the embodiments of the present disclosure provides a semiconductor device, which is manufactured using the method described above.
[0038] According to the manufacturing method of the semiconductor device and the semiconductor device provided by the embodiment of the present disclosure, multiple sacrificial layers are formed from the inside to the outside, and a sacrificial layer that is not easy to damage the interface layer and an etching process are used at the position adjacent to the interface layer to achieve the effect of reducing damage to the interface layer; while the release of the remaining sacrificial layers still maintains the conventional etching process, which can not only reduce costs and maintain production capacity, but also reduce damage to the interface layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] The following drawings of the present disclosure are hereby incorporated into the present disclosure for understanding the present disclosure. The drawings show embodiments of the present disclosure and their descriptions, and are used to explain the principles of the present disclosure. In the drawings:
[0040] FIG1A is a schematic cross-sectional view of a semiconductor device at the first stage obtained by sequentially performing steps in a method for manufacturing a semiconductor device in the related art.
[0041] FIG. 1B is a schematic cross-sectional view of a semiconductor device at a second stage obtained by sequentially performing steps in a method for manufacturing a semiconductor device in the related art.
[0042] FIG1C is a schematic cross-sectional view of a semiconductor device at a third stage obtained by sequentially performing steps in a method for manufacturing a semiconductor device in the related art.
[0043] FIG2 is a schematic flow chart showing a method for manufacturing a semiconductor device according to a specific embodiment of the present disclosure.
[0044] 3A is a schematic cross-sectional view of a semiconductor device at a first stage obtained by sequentially performing steps of a method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0045] 3B is a schematic cross-sectional view of a semiconductor device at a second stage obtained by sequentially performing steps of a method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0046] 3C is a schematic cross-sectional view of a semiconductor device at a third stage obtained by sequentially performing steps of a method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0047] 3D shows a schematic cross-sectional view of a semiconductor device at a fourth stage obtained during the process of sequentially performing steps of the method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0048] 3E is a schematic cross-sectional view of a semiconductor device at a fifth stage obtained during the process of sequentially performing steps of the method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0049] 3F is a schematic cross-sectional view of a semiconductor device at a sixth stage obtained during the process of sequentially performing steps of the method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0050] 3G shows a schematic cross-sectional view of a semiconductor device at a seventh stage obtained during the process of sequentially performing steps of the method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0051] 3H is a schematic cross-sectional view of a semiconductor device at an eighth stage obtained during the process of sequentially performing steps of the method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0052] 3I is a schematic cross-sectional view of a semiconductor device at a ninth stage obtained by sequentially performing steps of a method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0053] 3J is a schematic cross-sectional view of a semiconductor device at a tenth stage obtained during the process of sequentially performing steps of a method for manufacturing a semiconductor device according to an embodiment of the present disclosure. DETAILED DESCRIPTION
[0054] In the following description, a number of specific details are provided to provide a more thorough understanding of the present disclosure. However, it will be apparent to those skilled in the art that the present disclosure may be practiced without one or more of these details. In other examples, some technical features well known in the art are not described to avoid confusion with the present disclosure.
[0055] It should be understood that the present disclosure can be implemented in various forms and should not be construed as limited to the embodiments set forth herein. Rather, these embodiments are provided to make the disclosure thorough and complete and to fully convey the scope of the present disclosure to those skilled in the art. In the accompanying drawings, the dimensions and relative sizes of layers and regions may be exaggerated for clarity. Identical reference numerals throughout represent identical elements.
[0056] It should be understood that when an element or layer is referred to as being "on," "adjacent to," "connected to," or "coupled to" another element or layer, it may be directly on, adjacent to, connected to, or coupled to the other element or layer, or there may be intervening elements or layers. Conversely, when an element is referred to as being "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" another element or layer, there may be no intervening elements or layers. It should be understood that although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers, and / or parts, these elements, components, regions, layers, and / or parts should not be limited by these terms. These terms are merely used to distinguish one element, component, region, layer, or part from another element, component, region, layer, or part. Therefore, without departing from the teachings of the present disclosure, the first element, component, region, layer, or part discussed below may be represented as a second element, component, region, layer, or part.
[0057] Spatially relative terms such as "under," "beneath," "below," "under," "above," "above," etc., may be used herein for convenience of description to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that in addition to the orientations shown in the figures, the spatially relative terms are intended to include different orientations of the device in use and operation. For example, if the device in the drawings is flipped, then the elements or features described as "under the other elements" or "under it" or "under it" will be oriented as "on" the other elements or features. Thus, the exemplary terms "under" and "under" may include both upper and lower orientations. The device may be oriented otherwise (rotated 90 degrees or in other orientations) and the spatial descriptors used herein are interpreted accordingly.
[0058] The purpose of the terms used herein is only to describe specific embodiments and is not intended to limit the present disclosure. When used herein, the singular forms "a", "an", and "the" are intended to include the plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "comprising" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0059] As shown in Figures 1A to 1C, in the manufacturing method of MEMS devices in the related art, in order to obtain a cavity structure, it is first necessary to form a sacrificial layer 103 surrounded by a sidewall layer 102 on the sensitive material layer 302, wherein there is a high etching selectivity ratio between the sidewall layer 102 and the sacrificial layer 103; then, a wet or dry process is used to remove the sacrificial layer 103 through the release hole 104 formed in the sidewall layer 102, thereby forming a cavity structure 106 surrounded by the sidewall layer 102.
[0060] However, there is usually an interface layer 308 between the sensitive material layer 302 and the sidewall layer 102. This interface layer is generally formed when the surface of the sensitive material layer 302 is oxidized during the formation of the sidewall layer 102 and is relatively difficult to remove. When removing the sacrificial layer 103, the etching reaction gas or liquid will react with the interface layer 308, causing the interface layer 308 to be etched away, thereby causing the sensitive material layer 302 and the sidewall layer 102 connected by the interface layer 308 to crack, resulting in serious process problems and causing device failure.
[0061] The main reason why interface layer 308 is laterally corroded during the release of sacrificial layer 103 is that interface layer 308 and sacrificial layer 103 are made of the same or similar materials, and the etchant used to remove sacrificial layer 103 will also react with interface layer 308. If an etchant that is less likely to damage interface layer 308 is used to remove sacrificial layer 103, the release of sacrificial layer 103 will take longer, resulting in higher costs and limiting mass production capacity.
[0062] To address the above problem, as shown in FIG2 , an embodiment of the present disclosure proposes a method 200 for manufacturing a semiconductor device, comprising the following steps S210 to S260 .
[0063] Step S210 : providing a sensitive material layer, wherein the sensitive material layer includes a first surface and a second surface opposite to the first surface, wherein a first electrode is formed on the first surface.
[0064] Step S220, forming a sacrificial layer and a sidewall layer surrounding the sacrificial layer on the first surface of the sensitive material layer, wherein the sacrificial layer includes a first sacrificial layer and a second sacrificial layer surrounding the first sacrificial layer, and the material of the first sacrificial layer is different from the material of the second sacrificial layer.
[0065] Step S230 , forming a release hole in the sidewall layer connected to the first sacrificial layer.
[0066] Step S240 : Using a first etching process to remove the first sacrificial layer inside the sidewall layer through the release hole.
[0067] Step S250 , using a second etching process different from the first etching process to remove the second sacrificial layer through the release hole to form a cavity structure in the sidewall layer.
[0068] Step S260 , forming a first through hole penetrating the sensitive material layer, and forming a first pad on the second surface of the sensitive material layer electrically connected to the first electrode via the first through hole.
[0069] The manufacturing method 200 of the semiconductor device of the embodiment of the present disclosure forms multiple sacrificial layers from the inside to the outside, and uses sacrificial layers and etching processes that are not easy to damage the interface layer at the position adjacent to the interface layer to achieve the effect of reducing damage to the interface layer; while the release of most of the sacrificial layers still maintains the conventional etching process, which can not only reduce costs and maintain production capacity, but also reduce damage to the interface layer.
[0070] In order to fully understand the present disclosure, detailed structures and steps will be presented in the following description to illustrate the technical solutions proposed by the present disclosure. The preferred embodiments of the present disclosure are described in detail below. However, in addition to these detailed descriptions, the present disclosure may also have other implementation methods.
[0071] 3A to 3J illustrate schematic cross-sectional views of a semiconductor device obtained by sequentially implementing steps of the method for manufacturing a semiconductor device according to an embodiment of the present disclosure.
[0072] First, step S210 is performed to provide a first substrate 300. The first substrate 300 can be any suitable semiconductor substrate, such as a bulk silicon substrate. It can also be made of at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, or other III / V compound semiconductors, including multilayer structures composed of these semiconductors, or silicon-on-insulator (SOI), stacked silicon-on-insulator (SSOI), stacked silicon-germanium-on-insulator (S-SiGeOI), silicon-germanium-on-insulator (SiGeOI), and germanium-on-insulator (GeOI). It can also be double-side polished silicon wafers (DSPs), ceramic substrates such as alumina, quartz, or glass substrates.
[0073] Exemplarily, an isolation layer 301 and a second electrode 303 may also be formed on the first substrate 300, and the second electrode 303 may be embedded in the isolation layer 301, or the second electrode 303 may also be embedded in the sensitive material layer 302. In one example, after forming the isolation layer, a second electrode material layer covering the isolation layer may be deposited, and then a patterned mask layer may be formed on the second electrode material layer, wherein the mask layer defines a pattern of the second electrode, and then the second electrode material layer is etched using the patterned mask layer as a mask to form the second electrode, and finally, the patterned mask layer is removed. In another example, a lift-off process may also be used to form the second electrode, that is, first a patterned mask layer is formed on the surface of the isolation layer 301, and then a second electrode material layer covering the patterned mask layer is formed, and finally the patterned mask layer is lifted off, and the second electrode material layer above it is removed to obtain the second electrode.
[0074] The second electrode may be made of a conductive material or a semiconductor material. The conductive material may be a metal material having conductive properties. The metal material may be aluminum (Al), copper (Cu), gold (Au), platinum (Pt), or alloys of other metals and copper. The semiconductor material may be Si, Ge, SiGe, SiC, SiGeC, or the like.
[0075] Next, as shown in FIG3A , a sensitive material layer 302 is formed on the semiconductor substrate. The sensitive material layer 302 includes a first surface and a second surface, and the second surface is in contact with the first substrate 300. The semiconductor device of the embodiment of the present disclosure is a MEMS device. The sensitive material layer 302 is used to implement the micro-electromechanical function of the MEMS device. Sensitive materials refer to materials that can sense small changes in physical, chemical, or biological quantities and can exhibit obvious characteristic changes according to the changes. Specifically, they include thermosensitive materials, force-sensitive materials, photosensitive materials, voltage-sensitive materials, and the like. In some embodiments, the sensitive material layer can be a piezoelectric layer. The piezoelectric layer generates voltage when subjected to external pressure. Conversely, if voltage exists on both sides of the piezoelectric layer, the piezoelectric layer will slightly deform. Based on the above characteristics of the piezoelectric layer, the mutual conversion between sound waves and electrical signals can be achieved.
[0076] For example, a piezoelectric material can be deposited using a deposition method such as chemical vapor deposition, physical vapor deposition, or atomic layer deposition, and a metal element can be doped into the piezoelectric material to form a piezoelectric layer. The doped metal element includes one or more of scandium, zirconium, calcium, titanium, magnesium, and the like. For example, the material of the piezoelectric layer can specifically include aluminum nitride, lead zirconate titanate, zinc oxide, and the like, but this is not limited in the presently disclosed embodiments.
[0077] Continuing with FIG3A , after forming the sensitive material layer 302, a first electrode 304 may be formed on the first surface of the sensitive material layer 302. When the sensitive material layer 302 is a piezoelectric layer, the first electrode, the piezoelectric layer, and the second electrode constitute a composite thin film. The composite thin film may also include other film layers in addition to the aforementioned film layers. These layers may be appropriately configured based on the actual device and are not specifically limited herein.
[0078] In one example, a method for forming the first electrode 304 includes depositing a first electrode material layer covering the sensitive material layer 302. The first electrode material layer can be a metal material layer or a semiconductor material layer. Then, a patterned mask layer is formed on the first electrode material layer, wherein the mask layer defines a pattern of the first electrode. The first electrode material layer is then etched using the patterned mask layer as a mask to form the first electrode 304. Finally, the patterned mask layer is removed.
[0079] In another example, a lift-off process can also be used to form the first electrode 304, that is, first a patterned mask layer is formed on the surface of the sensitive material layer 302, then a first electrode material layer covering the patterned mask layer is formed, and finally the patterned mask layer is lifted off and the first electrode material layer above it is removed to obtain the first electrode.
[0080] Next, step S220 is performed to form a sacrificial layer and a sidewall layer surrounding the sacrificial layer on the first surface of the sensitive material layer 302. The sacrificial layer includes a first sacrificial layer and a second sacrificial layer surrounding the first sacrificial layer, and the material of the first sacrificial layer is different from the material of the second sacrificial layer. Since the second sacrificial layer contacts the interface layer, while the first sacrificial layer is surrounded by the second sacrificial layer and therefore does not contact the interface layer, the material of the first sacrificial layer can be silicon oxide, and the first sacrificial layer can be removed at a relatively fast speed without having to consider the effect of the silicon oxide etchant on the interface layer. The material of the second sacrificial layer can be a material with a certain etching selectivity ratio with the first sacrificial layer, such as silicon, so that the etchant of the second sacrificial layer does not corrode the interface layer.
[0081] Exemplarily, as shown in FIG3A , a first portion of a second sacrificial layer 305 is first formed on the sensitive material layer 302. Exemplarily, the first portion of the second sacrificial layer 305 covers the first electrode 304 inside the cavity. Next, as shown in FIG3B , a first sacrificial layer 306 is formed on the first surface of the sensitive material layer 302. The first sacrificial layer 306 is etched to form a trench exposing the first surface of the sensitive material layer 302. Next, a second portion of the second sacrificial layer 307 is formed on the first sacrificial layer 306. The second portion of the second sacrificial layer 307 covers the bottom and sidewalls of the trench.
[0082] Specifically, the material for the second sacrificial layer is first deposited on the sensitive material layer 302 and patterned to form a first portion of the second sacrificial layer 305. Next, a first sacrificial layer 306 is deposited to cover the first portion of the second sacrificial layer 305 and the sensitive material layer 302. The deposition process employed may include chemical vapor deposition (CVD) or physical vapor deposition (PVD). Next, a patterned photoresist layer is formed on the first sacrificial layer 306, with windows defining the locations of the trenches. Subsequently, the first sacrificial layer 306 is dry-etched using the photoresist layer as a mask to form trenches extending through the first sacrificial layer 306. The etching of the first sacrificial layer 306 stops at the surface of the sensitive material layer 302. After the etching of the first sacrificial layer 306 is complete, the photoresist layer can be removed using a process such as photoresist ashing.
[0083] Thereafter, the material of the second sacrificial layer is deposited again to form a second portion of the second sacrificial layer 307 covering the bottom and sidewalls of the trench and the top of the first sacrificial layer 306. Thus, the first portion of the second sacrificial layer 305 and the second portion of the second sacrificial layer 307 surround the first sacrificial layer 306 located between the trenches. When the second portion of the second sacrificial layer 307 is formed in the trenches, the first surface of the sensitive material layer 302 exposed at the bottom of the trench in the first sacrificial layer 306 is oxidized, thereby forming an interface layer 308 between the sensitive material layer 302 and the second portion of the second sacrificial layer 307. That is, the interface layer 308 is typically an oxide layer.
[0084] 3C , the second portion of the second sacrificial layer 307 at the bottom of the trench is removed to expose the interface layer 308. Since a sidewall layer will be formed in the trench later, and the interface layer will still be formed during the sidewall layer formation process, the interface layer does not need to be removed after removing the second portion of the second sacrificial layer 307.
[0085] As shown in FIG3D , a first sidewall layer 309 is formed on the second portion of the second sacrificial layer 307. The first sidewall layer 309 covers the interface layer 308 at the bottom of the trench and covers the second portion of the second sacrificial layer 307 on the sidewall of the trench. Next, as shown in FIG3E , a second sidewall layer 310 is formed on the first sidewall layer 309. The second sidewall layer 310 completely fills the trench and covers the top of the first sidewall layer 309. The first sidewall layer 309 and the second sidewall layer 310 can be deposited using deposition methods such as chemical vapor deposition, physical vapor deposition, or atomic layer deposition. Exemplarily, the thickness of the second sidewall layer 310 is greater than that of the first sidewall layer 309, that is, the second sidewall layer 310 is the main body of the sidewall layer, and the main function of the first sidewall layer 309 is to protect the second sidewall layer 310 from being corroded during the removal of the second sacrificial layer.
[0086] For example, because the second sidewall layer 310 is exposed, a certain etching selectivity exists between the material of the second sidewall layer 310 and the material of the first sacrificial layer 306, thereby preventing the etchant for the first sacrificial layer 306 from damaging the second sidewall layer 310. For example, when the material of the first sacrificial layer 306 is silicon oxide, the material of the second sidewall layer 310 can be silicon.
[0087] Because the first sidewall layer 309 is in contact with the second sacrificial layer, there is a certain etching selectivity between the material of the first sidewall layer 309 and the material of the second sacrificial layer, so that the etchant for the second sacrificial layer will not damage the first sidewall layer 309. When the material of the second sacrificial layer is silicon, the material of the first sidewall layer 309 can be silicon oxide. Furthermore, because the second sacrificial layer is formed between the first sidewall layer 309 and the first sacrificial layer 306, and the second sidewall layer 310 is formed outside the first sidewall layer 309, even if the materials of the first sidewall layer 309 and the first sacrificial layer 306 are both silicon oxide, the first sidewall layer 309 will not be significantly corroded during the process of etching and removing the first sacrificial layer 306.
[0088] Next, step S230 is performed to form a release hole in the sidewall layer that connects to the first sacrificial layer. Specifically, as shown in FIG3F , the second sidewall layer 310, the first sidewall layer 309, and the second portion of the second sacrificial layer 307 are sequentially etched to form a release hole that exposes the first sacrificial layer 306. The etchant can remove the first sacrificial layer 306 through the release hole.
[0089] Specifically, a patterned photoresist layer is first formed on the second sidewall layer 310 , and windows in the photoresist layer are used to define the positions of the release holes. Next, anisotropic etching is performed using the photoresist layer as a mask to form the release holes.
[0090] Next, as shown in FIG3G , step S240 is performed to perform a first etching process to remove the first sacrificial layer 306 through the release hole. Exemplarily, the first etching process is a wet etching process using hydrofluoric acid (HF) as the etchant. The first etching process can quickly remove the first sacrificial layer 306, saving etching time. Furthermore, because the first sacrificial layer 306 is surrounded by the second sacrificial layer, the first sacrificial layer 306 does not contact the interface layer 308. Therefore, the first etching process cannot damage the interface layer 308, maintaining structural stability.
[0091] As shown in FIG3H , step S250 is performed to continue with a second etching process to remove the second sacrificial layer to form a cavity in the sidewall layer. The etching rate of the second etching process on the interface layer 308 is lower than the etching rate of the first etching process on the interface layer 308 to reduce damage to the interface layer 308.
[0092] Exemplarily, the second etching process can be a dry etching process to reduce the etching rate of the interface layer 308. For example, it can be an etching process based on sulfur fluoride gas or an etching process based on xenon fluoride gas. This type of etching gas hardly reacts with oxides, and therefore can reduce damage to the interface layer 308. However, the second etching process is not limited to a dry etching process. As long as the etching rate of the interface layer 308 of the second etching process is lower than that of the first etching process, damage to the interface layer can be reduced. In some embodiments, the second etching process can also be a wet etching process that matches the properties of the second sacrificial layer. The difference between the first etching process and the second etching process can be different process types, that is, a dry etching process and a wet etching process, respectively; or, the difference between the first etching process and the second etching process can also be different etchants used.
[0093] Since the second sacrificial layer and the second sidewall layer 310 are both made of silicon, the etchant for the second sacrificial layer will also react with the second sidewall layer 310. Since the first sidewall layer 309 is formed inside the second sidewall layer 310, the inner wall of the second sidewall layer 310 is protected from corrosion.
[0094] In one embodiment, after the first etching process is performed, a thin silicon oxide layer may be deposited to cover the top of the second sidewall layer 310. The silicon oxide layer may protect the top of the second sidewall layer 310 from being corroded by the second etching process. At the same time, since the silicon oxide layer is thin, it will not block the release hole.
[0095] In another embodiment, the silicon oxide layer may not be formed, and the top of the second sidewall layer 310 may be etched by the second etching process. As shown in FIG3H , since the top area of the second sidewall layer 310 is large and the width of the trench is small, the second etching process removes the second sidewall layer 310 outside the trench, while retaining the second sidewall layer 310 inside the trench. Since the first sidewall layer 309 is still formed on the top of the cavity, the sealing of the cavity is not affected.
[0096] In yet another embodiment, the second sidewall layer 310 may be thinned before the second etching process is performed to remove part or all of the second sidewall layer 310 located outside the trench. For example, a chemical mechanical polishing process may be used to remove a certain thickness of the second sidewall layer 310. The aforementioned step of depositing the oxide layer may be performed after the step of removing a certain thickness of the second sidewall layer 310. By thinning the second sidewall layer 310, the depth of the release hole can be reduced, making it easier for the etchant to enter the cavity through the release hole, thereby increasing the release rate.
[0097] To reduce damage to the second sidewall layer 310 caused by the second etching process, in some embodiments, the second sacrificial layer can be made of amorphous silicon, and the second sidewall layer 310 can be made of polycrystalline silicon. Amorphous silicon has a loose texture, thus increasing the etching rate; polycrystalline silicon has a dense texture, which can reduce the etching rate and improve structural strength.
[0098] After removing the first and second sacrificial layers within the sidewall layer to form a cavity, a sealing layer 311 is formed above the sidewall layer, as shown in FIG3I . Sealing layer 311 seals the release holes in the sidewall layer, sealing the cavity. Silicon oxide can be used as the material for sealing layer 311, but is not limited thereto.
[0099] Afterwards, the first substrate 300 can be removed through etching or grinding. The isolation layer 301 between the first substrate 300 and the sensitive material layer 302 can be adjusted according to the performance of the semiconductor device and can be completely removed, partially removed, or retained in its entirety. After removing the first substrate 300, a second substrate 312 is formed above the sidewall layer. The second substrate 312 is formed on the sealing layer 311 and is used to provide support for the semiconductor device after the first substrate 300 is removed.
[0100] Next, step S260 is performed. As shown in FIG3J , a first through hole 313 is formed through the sensitive material layer, and a first pad 314 is formed on the second surface of the sensitive material layer 302, electrically connected to the first electrode 304 via the first through hole 313. While retaining the isolation layer 301, the isolation layer 301 and the sensitive material layer 302 are sequentially etched to form the first through hole. In addition, the isolation layer 301 is etched to form a second through hole 315, and a second pad 316 is formed on the second surface of the sensitive material layer 302, electrically connected to the second electrode 303 via the second through hole 315. Subsequently, the second substrate 312 can be bonded to the PCB board, and the first pad 314 and the second pad 316 can be electrically connected to the PCB board using wires, with the sensitive material layer 302 side facing upward to realize the function of the sensitive material layer 302.
[0101] At this point, the process steps of the manufacturing method of the semiconductor device according to an embodiment of the present disclosure have been completed. It can be understood that the manufacturing method of the semiconductor device of the embodiment of the present disclosure not only includes the above steps, but may also include other necessary steps before, during or after the above steps, which are all included in the scope of the manufacturing method of the embodiment of the present disclosure.
[0102] According to the manufacturing method of the semiconductor device provided by the present invention, multiple sacrificial layers are formed from the inside to the outside, and sacrificial layers that are not easy to damage the interface layer and etching processes are used at positions adjacent to the interface layer to achieve the effect of reducing damage to the interface layer; while the release of most of the sacrificial layers still maintains the conventional etching process, which can not only reduce costs and maintain production capacity, but also reduce damage to the interface layer.
[0103] As shown in FIG3J , an embodiment of the present disclosure further provides a semiconductor device, which can be manufactured using the semiconductor device manufacturing method described above. Specifically, the semiconductor device of the embodiment of the present disclosure includes: a sensitive material layer 302, the sensitive material layer 302 including a first surface and a second surface opposite the first surface; a first electrode 304 formed on the first surface, and a second electrode 303 formed on the second surface; sidewall layers formed on the first surface of the sensitive material layer 302, the sidewall layers including a first sidewall layer 309 and a second sidewall layer 310, with the first sidewall layer 309 surrounding the second sidewall layer 310. A sealing layer 311 is formed above the first sidewall layer 309. A cavity is formed within the sidewall layer, and a sacrificial layer is formed outside the sidewall layer, including a second sacrificial layer in contact with the first sidewall layer 309 and a first sacrificial layer 306 located outside the second sacrificial layer; and a second substrate 312 is formed above the sidewall layer. The first through hole 313 passes through the sensitive material layer 302, and the first pad 314 is located on the second surface side of the sensitive material layer 302 and is electrically connected to the first electrode 304 via the first through hole 313; the second through hole 315 passes through the isolation layer 301 formed on the second surface of the sensitive material layer 302, and the second pad 316 is located on the second surface side of the sensitive material layer 302 and is electrically connected to the second electrode 303 via the second through hole 315.
[0104] In some embodiments, the sensitive material layer 302 can be a piezoelectric layer, and the second electrode 303, the piezoelectric layer and the first electrode 304 constitute a composite film. The composite film can also include other film layers in addition to the above-mentioned film layers, which can be reasonably arranged according to the actual device and is not specifically limited here.
[0105] The semiconductor device of the embodiment of the present disclosure is manufactured using the above-mentioned manufacturing method, so the interface layer will not be damaged during the manufacturing process and the structure is more stable.
[0106] The present disclosure has been described through the above-described embodiments, but it should be understood that the above-described embodiments are for illustrative and illustrative purposes only and are not intended to limit the present disclosure to the described embodiments. In addition, it will be understood by those skilled in the art that the present disclosure is not limited to the above-described embodiments, and that various variations and modifications may be made based on the teachings of the present disclosure, all of which fall within the scope of protection claimed by the present disclosure. The scope of protection of the present disclosure is defined by the appended claims and their equivalents.
Claims
1. A method for manufacturing a semiconductor device, comprising: Providing a sensitive material layer, the sensitive material layer comprising a first surface and a second surface opposite to the first surface, the first surface being formed with a first electrode; forming a sacrificial layer and a sidewall layer surrounding the sacrificial layer on the first surface of the sensitive material layer, wherein the sacrificial layer comprises a first sacrificial layer and a second sacrificial layer surrounding the first sacrificial layer, and the material of the first sacrificial layer is different from the material of the second sacrificial layer; forming a release hole in the sidewall layer connected to the first sacrificial layer; Using a first etching process to remove the first sacrificial layer inside the sidewall layer through the release hole; Using a second etching process different from the first etching process to remove the second sacrificial layer through the release hole to form a cavity structure in the sidewall layer; A first through hole is formed penetrating the sensitive material layer, and a first pad electrically connected to the first electrode via the first through hole is formed on the second surface of the sensitive material layer.
2. The manufacturing method according to claim 1, characterized in that A second electrode is formed on the second surface of the sensitive material layer. The method further includes: forming a second pad electrically connected to the second electrode on the second surface of the sensitive material layer.
3. The manufacturing method according to claim 1, characterized in that: The step of providing a sensitive material layer comprises: Providing a first substrate, and sequentially forming an isolation layer and the sensitive material layer on the first substrate, wherein the second surface of the sensitive material layer is in contact with the isolation layer; After performing the second etching process and before forming the first through hole, the method further includes: removing the first substrate and forming a second substrate above the sidewall layer.
4. The manufacturing method according to claim 3, characterized in that: Before forming the second substrate, the method further includes: A sealing layer is formed on the sidewall layer to seal the release hole.
5. The manufacturing method according to claim 1, characterized in that: An interface layer is formed between the sidewall layer and the sensitive material layer, and an etching rate of the material of the interface layer by the first etching process is greater than an etching rate of the material of the interface layer by the second etching process.
6. The manufacturing method according to claim 1, characterized in that: The material of the first sacrificial layer includes silicon oxide, and the material of the second sacrificial layer includes silicon.
7. The manufacturing method according to claim 1, characterized in that: The sidewall layer includes a first sidewall layer and a second sidewall layer, and the first sidewall layer is disposed between the second sidewall layer and the second sacrificial layer.
8. The manufacturing method according to claim 7, characterized in that: The forming of a sacrificial layer and a sidewall layer surrounding the sacrificial layer on the first surface of the sensitive material layer comprises: forming a first sacrificial layer on the first surface of the sensitive material layer; Etching the first sacrificial layer to form a groove exposing the first surface of the sensitive material layer; forming a second sacrificial layer on the first sacrificial layer, wherein the second sacrificial layer covers the bottom and sidewalls of the trench; removing the second sacrificial layer at the bottom of the trench; forming a first sidewall layer on the second sacrificial layer, wherein the first sidewall layer covers the bottom of the trench and covers the second sacrificial layer on the sidewall of the trench; A second sidewall layer is formed on the first sidewall layer, and the second sidewall layer fills the trench.
9. The manufacturing method according to claim 8, characterized in that: The second sacrificial layer comprises a first portion of the second sacrificial layer and a second portion of the second sacrificial layer; Before forming the first sacrificial layer on the first surface of the sensitive material layer, the method further includes: forming a first portion of a second sacrificial layer on the first surface of the sensitive material layer, wherein the first portion of the second sacrificial layer is located between the grooves; The forming of the second sacrificial layer on the first sacrificial layer includes forming the second portion of the second sacrificial layer on the first sacrificial layer.
10. The manufacturing method according to claim 7, characterized in that: The material of the first sidewall layer includes silicon oxide, and the material of the second sidewall layer includes silicon.
11. The manufacturing method according to claim 1, characterized in that: The first etching process includes a wet etching process, and the second etching process includes a dry etching process.
12. The manufacturing method according to any one of claims 1 to 11, characterized in that: The sensitive material layer includes a piezoelectric layer.
13. A semiconductor device manufactured by the method according to any one of claims 1 to 12, wherein: The semiconductor device comprises: A sensitive material layer, comprising a first surface and a second surface opposite to the first surface, wherein a first electrode is formed on the first surface; a sidewall layer, which is disposed on the first surface of the sensitive material layer, and a release hole is formed in the sidewall layer; A first pad, which is disposed on the second surface of the sensitive material layer and is electrically connected to the first electrode; A cavity structure is arranged inside the side wall layer.
14. The semiconductor device according to claim 13, wherein: The second surface of the sensitive material layer is provided with a second electrode and a second pad electrically connected to the second electrode.
15. The semiconductor device according to claim 13, wherein: The second surface of the sensitive material layer is provided with an isolation layer.
16. The semiconductor device according to claim 13, wherein: A sealing layer is arranged above the side wall layer, and the sealing layer seals the release hole.
17. The semiconductor device according to claim 16, wherein: A second substrate is disposed above the sealing layer.
18. The semiconductor device according to claim 13, wherein: The sidewall layer includes a first sidewall layer and a second sidewall layer, and the first sidewall layer surrounds the second sidewall layer.
19. The semiconductor device according to claim 18, wherein: The material of the first sidewall layer includes silicon oxide, and the material of the second sidewall layer includes silicon.
20. The semiconductor device according to claim 13, wherein The sensitive material layer includes a piezoelectric layer.
Citation Information
Patent Citations
MEMS (Micro-electromechanical System) device, preparation method and electronic device
CN107973266A
MEMS device, preparation method and electronic device
CN109956447A
Fingerprint identification module, manufacturing method thereof and electronic equipment
CN112115755A
Ultrasonic fingerprint sensing chip, electronic equipment and manufacturing method
CN112580534A
MEMS microphone structure and manufacturing method thereof
CN112866886A