Machinable glass-ceramics
The development of glass-ceramic compositions for CAD/CAM applications addresses the lack of machinability and aesthetics in current dental ceramics by using specific chemical compositions and a two-step heat treatment process, resulting in cost-effective, efficient, and aesthetically pleasing dental restorations with reduced wear on opposing teeth.
Patent Information
- Application Number
- PCT/EP2024/061213
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-24
- Filing Date
- 2024-04-24
- Publication Date
- 2024-10-31
AI Technical Summary
Current CAD/CAM dental ceramics lack machinability, aesthetics, and are costly, leading to increased wear on opposing teeth and higher restoration costs due to the need for high-cost diamond/silicon carbide burs and requiring sintering processes that not all dental practices can afford or perform.
Development of glass-ceramic compositions comprising SiO2, Al2O3, BaO, MgO, and optionally MgF2 or F2, with specific weight percentages, which can be processed without sintering and exhibit improved machinability, aesthetics, and reduced wear on opposing teeth, using a two-step heat treatment process to achieve desired properties.
The glass-ceramic compositions demonstrate exceptional machinability, reducing production costs and time, while maintaining strength and aesthetics comparable to commercial materials, with lower wear on opposing teeth and the ability to be formed into desired shapes directly without sintering.
Smart Images

Figure IMGF000028_0001 
Figure IMGF000029_0001 
Figure IMGF000030_0001
Abstract
Description
[0001]MACHINABLE GLASS-CERAMICS The present application relates to glass-ceramics, in particular to glass-ceramic compositions, methods of producing said glass-ceramics and uses of said glass-ceramics. BACKGROUND Digital dentistry comprises materials and computer controlled technologies that are used to fabricate dental prostheses. It is anticipated that with technologies evolving and affordability improving, the global digital dentistry market, which includes technologies such as 3D printing and computer-aided design / computer-aided manufacturing (CAD / CAM). These technologies allow for minimal human intervention, which reduces infection risk. Despite advances in technologies, the current CAD / CAM market does not offer any dental ceramic materials specifically designed as machinable. The currently offered materials for use with CAD / CAM technologies are the same formulations used in traditional artisanal fabrication of prostheses, which are not considered machinable. They typically have high strength and exceedingly high hardness (>6 GPa) (Homaei et al., 2016). As a result, the produced restoration can wear the opposing tooth structure, of which the enamel hardness is approximately 3.3-4 GPa (Guess et al., 2011). The widely used hard dental ceramics also lack aesthetics with unrealistic colouring. As a result, these dental ceramics are not favoured by patients. A further disadvantage to the widely available commercial CAD / CAM ceramics is the requirement for high cost diamond / silicon carbide burs. Additionally, in order to enable digital milling or grinding, the restoration can only be milled in an un-sintered or partially sintered form, therefore further sintering step(s) using high temperature furnaces are required for completion of the restoration. Many dental practices or labs may not have such equipment, therefore , the costs for restoration are increased. These problems arise as the currently commercially available materials were developed before introduction of CAD / CAM dentistry and have not been optimised for digital processing technology. There therefore remains in the art a need for machinable, aesthetic dental ceramics with hardness near to that of enamel. Examples of available glass-ceramics are Vita Mark II® HT, Empress CAD® HT, Emax CAD® HT, VITRONIT®, MACOR®, and DICOR®. Vita Mark II® HT, Empress CAD® HT, Emax CAD® HT, VITRONIT®, and MACOR® were used for comparative studies in the present application. Vita Mark II® HT is a feldspar ceramic suitable for dental restorations. Empress CAD® is a leucite-reinforced glass-ceramic block. Emax CAD® HT is a lithium disilicate glass-ceramic. VITRONIT® is a mica glass ceramic. MACOR® is a glass-ceramic composed of fluorphlogopite mica and borosilicate glass. DICOR® is a potassium-based fluoromica glass-ceramic. Dicor® MGC was the first potassium-based fluoromica glass-ceramics to be used with CAD / CAM technology in dentistry. However, with poor mechanical properties (flexural strength of approximately [152 MPa] and fracture toughness values of approximately [1.0-1.40 MPa.m0.5]) (Seghi et al., 1995). MACOR® is a commercially available potassium fluoromica glass-ceramic exhibiting a house of cards microstructure. MACOR® generally consists of K-fluorphlogopite (KMg3BSI3O10F2) crystals. VITRONIT® is a commercially available cabbage-head mica. Thus far VITRONIT® applications include, for example, vacuum technology, laser industries and semiconductor technology. The cabbage-head mica glass-ceramic has not been used in dental applications. To date, there is no evidence of a cabbage-head microstructure forming with a barium fluorphlogopite mica with optimised properties for use in CAD / CAM applications. The present invention provides new highly machinable glass-ceramics, compositions, methods and uses of the same. SUMMARY OF THE INVENTION The invention related to glass-ceramics, methods of producing glass-ceramics and uses of said glass- ceramics. In a first aspect of the invention, there is provided a glass-ceramic composition comprising, consisting essentially of, or consisting of SiO2, Al2O3, BaO, and MgO, either MgF2or F2, and optionally B2O3. In some embodiments: a. the amount of SiO2 in the composition by weight % is from about 41% to about 49%; b. the amount of Al2O3 in the composition by weight % is from about 8% to about 23%; c. the amount of BaO in the composition by weight % is from about 14% to about 17%; d. the amount of MgO in the composition by weight % is from about 4% to about 15%; e. the amount of MgF2in the composition, if present, is from about 5% to about 11% by weight; f. the amount of F2 in the composition, if present, is from about 2% to about 4% by weight; and g. the amount of B2O3 in the composition by weight % is from about 0% to about 15%, or B2O3 is absent. In some embodiments, for example in some embodiments in which the composition is yet to be exposed to the two-step heat treatment process referred to herein: a. the amount of SiO2in the composition by weight % is from about 41% to about 49%; b. the amount of Al2O3in the composition by weight % is from about 8% to about 23%; c. the amount of BaO in the composition by weight % is from about 14% to about 16%; d. the amount of MgO in the composition by weight % is from about 4% to about 8%; e. the amount of MgF2 in the composition by weight % is from about 5% to about 11%; and f. the amount of B2O3 in the composition by weight % is from about 0% to about 15%, or B2O3 is absent. Such compositions may be referred to herein as “pre-treated glass-ceramic compositions”. In some embodiments, for example in some embodiments in which the composition is yet to be exposed to the two-step heat treatment process referred to herein: a. the amount of Al2O3 in the composition by weight % is from about 16% to about 23%; b. the amount of BaO in the composition by weight % is from about 14% to about 16%; c. the amount of MgO in the composition by weight % is from about 4% to about 8%; d. the amount of MgF2in the composition by weight % is from about 9% to about 11%; and e. the amount of B2O3 in the composition by weight % is from about 0% to about 8%, or B2O3 is absent. Such compositions may be referred to herein as “pre-treated glass-ceramic compositions”. In some embodiments, for example in some embodiments in which the composition has been exposed to the two-step heat treatment process referred to herein: a. the amount of SiO2 in the composition by weight % is from about 42% to about 47%; b. the amount of Al2O3 in the composition by weight % is from about 16% to about 18%; c. the amount of BaO in the composition by weight % is from about 15% to about 17%; d. the amount of MgO in the composition by weight % is from about 13% to about 15%; e. the amount of F2in the composition by weight % is from about 2% to about 4%; and f. the amount of B2O3in the composition by weight % is from about 0% to about 12%, or B2O3is absent. Such compositions may be referred to herein as “post-treated glass-ceramic compositions” or “final glass- ceramic compositions”. In any embodiments in which the composition is described as having a certain amount of components by % weight, the total weight of each component will be 100% of the weight of the total composition. The skilled person will appreciate that, due to rounding, adding the individual percentage numbers may arrive at a number that is different to 100, but the skilled person understands how to reconcile this and will appreciate the total weight of the composition cannot be more than 100%. In the present disclosure, any number provided includes values that would approximate to the given value at its given degree of accuracy or number of significant figures. For example, a value of 10 will include 9.5 and 10.5. In a second aspect of the invention, there is provided a method of producing a glass-ceramic composition, comprising providing a pre-treated glass-ceramic composition of the invention, and exposing the pre- treated composition to a two-step heat treatment process. In some embodiments, the method comprises a method of producing a glass-ceramic composition, comprising: providing a pre-treated glass-ceramic composition, wherein the pre-treated glass-ceramic composition has been obtained or is obtainable according to a method comprising the steps of: (i) combining SiO2, Al2O3, BaO, MgO, MgF2and optionally B2O3in the weight % amounts of: from about 41% to about 49% of SiO2; from about 8% to about 23% of Al2O3; from about 14% to about 16% of BaO; from about 4% to about 8% of MgO; from about 5% to about 11% of MgF2; and from about 0% to about 15% B2O3 or B2O3 is absent; (ii) melting the combined compounds to provide a melted composition; (iii) quenching the melted composition, optionally in water, to provide a quenched composition, (iv) drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; (v) milling the dry composition to provide a milled composition; (vi) melting the milled composition to provide a melted composition; and (vii) casting the melted composition in a die or mold to provide a cast glass-ceramic composition; and exposing the cast glass monolith to a two-step heat treatment process. In some embodiments, the two-step heat treatment process of the invention comprises: a. a first heat treatment step comprising heating the composition to the, or around the, nucleation temperature of the composition; and b. a second, subsequent, heat treatment step comprising heating the composition to the, or around the, crystallization temperature of the composition. As used in the present disclosure, references to “around” a specified temperature include a temperature that is 50oC above or below the stated temperature. In a third aspect of the invention, there is provided a glass-ceramic composition obtainable or obtained by a method of the invention. In a fourth aspect of the invention, there is provided the use of a glass-ceramic composition of the invention in dentistry. In some embodiments, the composition is the post-fired or final composition. In a further aspect of the invention, there is provided the use of a glass-ceramic composition of the invention as or in a dental implant product. In some embodiments, the composition is the post-fired or final composition. In a further aspect of the invention, there is provided a dental implant product comprising or consisting of a glass-ceramic composition of the invention. In some embodiments, the composition is the post-fired or final composition. As used herein, “consisting essentially of” means that specific further component can be present, but only those not materially affecting the essential characteristics of the composition. DETAILED DESCRIPTION The invention provides glass-ceramics, as well as methods for their preparation and their use in dentistry and wider applications. More details of the various aspects of the inventions are now provided. The invention provides novel glass-ceramics with surprising exceptional machinability and universal properties for the rapid and most efficient digital processing / fabrication of dental restorations. Machinability may be referred to as the ease with which a material (in this case a ceramic material) can be cut to shape while providing a satisfactory surface finish. Materials with good machinability (free machining materials) require little power to cut, can be cut quickly, easily obtain a good finish, and do not cause significant wear on the tooling. Unlike existing CAD / CAM ceramics, the developed materials help in reducing both cost and time required to produce dental restorations. The final restorations have superior aesthetics and strength of ceramics, comparable to other commercial materials but incur much lower wear to the opposing teeth compared to existing CAD / CAM ceramics. Machinability is inherently difficult to predict, and thus compositions having improved machinability are difficult to produce. Surprisingly, the glass-ceramic compositions of the invention have good machinability, even when the material has not undergone sintering. Instead, the glass-ceramic compositions of the invention may be formed into desired shapes directly, for example by casting. Components of the compositions The compositions of the invention may comprise, consist essentially of, or consist of SiO2, Al2O3, BaO, and MgO, either MgF2 or F2, and optionally B2O3. Compositions of the invention may preferably consists of (or consist essentially of) the stated components. In the invention, the amount of SiO2 in the composition by weight % is from about 41% to about 49%; the amount of Al2O3 in the composition by weight % is from about 8% to about 23%; the amount of BaO in the composition by weight % is from about 14% to about 17%; the amount of MgO in the composition by weight % is from about 4% to about 15%; the amount of MgF2in the composition, if present, is from about 5% to about 11% by weight; the amount of F2in the composition, if present, is from about 2% to about 4% by weight; and the amount of B2O3in the composition by weight % is from about 0% to about 15%, or B2O3 is absent. The compositions of the invention may be classed as “pre-treated” compositions, which are compositions that have not yet been subjected to the two-step heat treatment process of the invention. Alternatively, the compositions of the invention may be classed as “post-treated” or “final” compositions, which are compositions that have been subjected to the two-step heat treatment process of the invention For the pre-treated compositions: a. the amount of SiO2 in the composition by weight % may be from about 41% to about 49%; b. the amount of Al2O3 in the composition by weight % may be from about 8% to about 23%; c. the amount of BaO in the composition by weight % may be from about 14% to about 16%; d. the amount of MgO in the composition by weight % may be from about 4% to about 8%; e. the amount of MgF2in the composition by weight % may be from about 5% to about 11%; and f. the amount of B2O3 in the composition by weight % may be from about 0% to about 15%, or B2O3 is absent. In some embodiments of the pre-treated compositions: a. the amount of SiO2 in the composition by weight % may be from about 42% to about 48%; b. the amount of Al2O3in the composition by weight % may be from about 16% to about 23%; c. the amount of BaO in the composition by weight % may be from about 14% to about 16%; d. the amount of MgO in the composition by weight % may be from about 4% to about 8%; e. the amount of MgF2 in the composition by weight % may be from about 9% to about 11%; and f. the amount of B2O3 in the composition by weight % may be from about 0% to about 8%, or B2O3 is absent. In such embodiments, the compositions may exhibit improved characteristics, for example demonstrating a cabbage-head like microstructure. In some embodiments, the glass-ceramic composition (for example the pre-treatment composition) comprises, consists essentially of, or consists of from about 41% to about 49% by weight SiO2. In some embodiments, the glass-ceramic composition (for example the pre-treatment composition) comprises, consists essentially of, or consists of from about 8% to about 23% by weight of Al2O3; In some embodiments, the glass-ceramic composition (for example the pre-treatment composition) comprises, consists essentially of, or consists of from about 14% to about 16% by weight of BaO; In some embodiments, the glass-ceramic composition (for example the pre-treatment composition) comprises, consists essentially of, or consists of from about 4% to about 8% by weight of MgO; In some embodiments, the glass-ceramic composition (for example the pre-treatment composition) comprises, consists essentially of, or consists of from about 0% to about 15% by weight of B2O3, or wherein B2O3 is absent. In some embodiments, the glass-ceramic composition (for example the pre-treatment composition) comprises, consists essentially of, or consists of from about 5% to about 11% by weight of MgF2. Some specific pre-treated compositions include those provided in Table 1 below: Table 1 – pre-fired compositions SiO2 Al2O3 BaO MgO B2O3 MgF2 Examples (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) A 41 15 14 7 15 9 "High Boric oxide" B 44 16 15 7 8 10 "Original" C 46 16 15 8 4 10 "Low Boric Oxide" D 48 17 16 8 0 11 "Zero Boric oxide" E 46 16 15 4 8 10 "Low Magnesia" F 49 8 15 8 9 11 "Low Alumina" G 42 21 14 7 8 9 "High Alumina" H 47 17 15 8 8 5 "Low Fluorine" I "Low Boric oxide High 43 23 14 7 4 9 Alumina" For the post-treatment compositions: a. the amount of SiO2in the composition by weight % may be from about 42% to about 47%; b. the amount of Al2O3in the composition by weight % may be from about 16% to about 18%; c. the amount of BaO in the composition by weight % may be from about 15% to about 17%; d. the amount of MgO in the composition by weight % may be from about 13% to about 15%; e. the amount of F2 in the composition by weight % may be from about 2% to about 4%; and f. the amount of B2O3 in the composition by weight % may be from about 0% to about 12%, or B2O3is absent. In some embodiments, the glass-ceramic composition (for example the post-treatment composition) comprises, consists essentially of, or consists of from about 42% to about 47% by weight SiO2. In some embodiments, the glass-ceramic composition (for example the post-treatment composition) comprises, consists essentially of, or consists of from about 16% to about 18% by weight of Al2O3; In some embodiments, the glass-ceramic composition (for example the post-treatment composition) comprises, consists essentially of, or consists of from about 15% to about 17% by weight of BaO; In some embodiments, the glass-ceramic composition (for example the post-treatment composition) comprises, consists essentially of, or consists of from about 13% to about 15% by weight of MgO; In some embodiments, the glass-ceramic composition (for example the post-treatment composition) comprises, consists essentially of, or consists of from about 0% to about 12% by weight of B2O3, or wherein B2O3 is absent. In some embodiments, the glass-ceramic composition (for example the post-treatment composition) comprises, consists essentially of, or consists of from about 2% to about 4% by weight of F2. Some specific post-treated compositions include those provided in Table 2 below: Table 2 – post-fired compositions SiO2 Al2O3 BaO MgO B2O3 Examples F2 (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) A 42 16 15 13 12 4 "High Boric oxide" B 45 17 15 13 7 2 "Original" C 47 17 16 13 4 3 "Low Boric oxide" D 46 18 17 15 0 4 "Zero Boric oxide" The amount of each component may be the nominal amount. For example, the amount of each component may be the amount (by weight) of each component that is used to make the composition. This may be particularly the case for the pre-treated compositions. Alternatively, the amount of each component may be the analysed (i.e. measured) amount. For example, the amount of each component may be the amount (by weight) of each component that is determined to be present in the composition by measuring the amount of the component. This may be the case for pre- or post-treated compositions, but may particularly be the case for the post-treated compositions The chemical composition of the glass-ceramic compositions may be determined according to any suitable method, for example using X-ray fluorescence (XRF). XRF is a technique commonly used to determine the elemental composition of a material, including ceramics. XRF can detect and quantify the abundance of elements in a sample, and can be used to evaluate the amount or likely amount of different compounds with a sample. Determining the amount of compounds within a composition can be achieved using a variety of techniques known in the art, such as using empirical relationships or theoretical calculations based on known factors, such as starting materials. For example, if a ceramic is known to contain different types of oxides, the relative amounts of these compounds can be determined or estimated from XRF data by assuming each oxide contributes a known fraction of its overall constituent elements to the overall elemental composition. Such methods are known to the person skilled in the art. The glass-ceramic compositions may exhibit curved crystals or curved crystal agglomerates which may be identified in scanning electron micrographs. The apparent radius of the curved crystals or curved crystal agglomerates may be less than 300 microns, less than 250 microns, less than 200 microns, less than 150 microns, less than 100 microns, less than 90, 80, 70, 60, 50, 40, 30, microns, or less than 20 microns. The apparent radius is an angular distance describing how large a sphere or circle appears from a given point of view. Apparent radius may be measured by any suitable method, for example by scanning electron microscopy (SEM). The glass-ceramic compositions, for example those exhibiting curved crystals, may comprise of barium fluorphlogopite. The glass-ceramic compositions, for example those exhibiting curved crystals, may comprise of barium kinoshitalite. The glass-ceramic compositions, for example those exhibiting curved crystals, may comprise of a mixture of a solid solution phase of barium fluorphlogopite and barium kinoshitalite. The glass-ceramic compositions may be a barium fluoromica. The glass-ceramic composition may exhibit a cabbage-head microstructure. The glass-ceramic composition may be a barium fluoromica exhibiting a cabbage-head microstructure. The glass-ceramic composition may exhibit a cabbage-head microstructure forming with a barium fluorphlogopite mica. A cabbage-head microstructure is so named as the mica crystals become curved and group together into cabbage-head leaf appearance. The mica flakes occur in the form of spherically arranged lamellae. The curved crystals are arranged in a radial fashion around a centre (Höland et al, 1983) and interwoven giving the appearance of a cabbage-head “the cabbage-head microstructure”. Despite crystallo-chemical analysis in the literature (Holand and Beall, 2012), the main reason behind the formation of such curved crystals is unclear. Cabbage-head microstructures are advantageous because they can result in higher strengths, fracture toughness, lower hardness and improved machinability and more importantly improved light transmission. In some embodiments, the amount B2O3 may be kept low, or be eliminated, to promote the formation of cabbage-head microstructures. Thus in some embodiments, the amount of B2O3may be from 0% to 8%, or B2O3may be absent. The glass-ceramic compositions may exhibit hardness (e.g. Vickers hardness) of from about 2.5 to about 5.5 GPa,. In some embodiments, the glass-ceramic compositions may exhibit hardness (e.g. Vickers hardness) of from about 3 to about 5 GPa. In some embodiments, the glass-ceramic compositions may exhibit hardness (e.g. Vickers hardness) of from about 3 to about 4.5 GPa. The hardness may preferably be Vickers Hardness. In some embodiments, the hardness (for example the Vickers hardness) may be measured according to BSI ENV 843-4:1995 (British Standards Institution, Advanced technical ceramics. Monolithic ceramics. Mechanical properties at room temperatures. Vickers, Knoop and Rockwell superficial hardness tests, published 15 February 1995). The glass-ceramic compositions may exhibit a biaxial flexural strength of from about 100 to about 400 MPa. In some embodiments, the glass-ceramic compositions may exhibit a biaxial flexural strength of from about 200 to about 350 MPa. In some embodiments, the glass-ceramic compositions may exhibit a biaxial flexural strength of from about 200 to 300 MPa. Biaxial flexural strength may be measured according to any suitable means. In some embodiments, biaxial flexural strength may be measured according to ISO 6872:2015 (edition 5, published June 2015). Flexural strength is the ability of a composition or material to resist bending deflection when energy is applied to the structure. Biaxial flexural strength is the ability of a composition or material to resist bending deflection when force is applied to the structure across two axes. The glass-ceramic compositions may exhibit translucency with a light transmission of from about 30 to about 80%. In some embodiments, the glass-ceramic compositions may exhibit translucency with a light transmission of from about 35 to about 75%. In some embodiments, the glass-ceramic compositions may exhibit translucency with a light transmission of from about 60 to about 75%. Translucency as used herein refers to the percentage of light transmitted through the tested material. Translucency may therefore be referred to as a light transmission percentage. The translucency may refer to the translucency of a sample of material having a thickness of 1mm. The translucency may refer to the translucency of a sample of material when measuring the transmission of 600 nm wavelength light. In some embodiments, the translucency refers to the percentage of 600 nm wavelength light that is transmitted through a 1mm thick sample of the composition. Translucency may be measured according to any suitable method known in the art. For example, translucency may be measured according to the following method: a) providing a planar sample of the composition having a thickness of 1mm, optionally wherein the planar sample of the composition has been polished; b) transmitting 600 nm wavelength light through the sample at an angle perpendicular to the planar surface of the sample; and c) measuring the amount of light that passes through the sample as a percentage of the light transmitted to provide a % translucency. In some embodiments, translucency may be measured according to the following method: a) providing a planar sample of the composition having a thickness of 1mm; b) polishing the sample of the composition; c) cleaning the polished sample; d) drying the cleaned sample, or allowing the cleaned sample to dry; e) transmitting 600 nm wavelength light through the dried sample at an angle perpendicular to the planar surface of the sample; and f) measuring the amount of light that passes through the sample as a percentage of the light transmitted to provide a % translucency. In some embodiments, translucency may be measured according to the following method: a) providing a planar sample of the composition having a thickness of 1mm; b) polishing the sample of the composition using 1 μm alumina oxide polishing media on a lapping machine; c) cleaning the polished sample in an ultrasonic bath for 10 minutes; d) drying the cleaned sample, or allowing the cleaned sample to dry; e) transmitting 600 nm wavelength light through the dried sample at an angle perpendicular to the planar surface of the sample; and f) measuring the amount of light that passes through the sample as a percentage of the light transmitted to provide a % translucency. The step of measuring the amount of light that passes through the sample in any of the above embodiments may be undertaken using a spectrometer, for sample a Lambda 950 UV-vis spectrometer (Perkin Elmer, CT, USA). The specified weight of each component provided may be the nominal weight amount. In some embodiments the specified weight of each component provided may be the analysed weight amount. In some embodiments the specified weight of each component may be determined by X-Ray Fluorescence (XRF). Methods of making the compositions The present invention provides methods for making the glass-ceramics of the invention. In particular, the present invention provides starting (or pre-treated) compositions for making glass-ceramics, the methods of making such starting (or pre-treated) compositions, and the method provided post-treated or final glass-ceramic compositions. The methods of the invention may clearly be combined with the more detailed embodiments of the glass-ceramics of the invention, since the methods are used to produce said compositions. There are also additional methods available for production of glass-ceramics. Generally, a method of the invention may comprise providing a pre-treated glass-ceramic composition according to the invention and exposing the pre-treated composition to a two-step heat treatment process. In some embodiments, the methods comprise steps of making the pre-treated glass-ceramic composition, or such steps may take place earlier, such that the method begins with the pre-treated glass- ceramic composition. In some embodiments, the methods comprises: a. providing a pre-treated glass-ceramic composition, wherein the pre-treated glass-ceramic composition has been obtained or is obtainable according to a method comprising the steps of: i. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of: 1. from about 41% to about 49% of SiO2; 2. from about 8% to about 23% of Al2O3; 3. from about 14% to about 16% of BaO; 4. from about 4% to about 8% of MgO; 5. from about 5% to about 11% of MgF2; and 6. from about 0% to about 15% B2O3 or B2O3 is absent; ii. melting the combined compounds to provide a melted composition; iii. quenching the melted composition, optionally in water, to provide a quenched composition, iv. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; v. milling the dry composition to provide a milled composition; vi. melting the milled composition to provide a melted composition; vii. casting the melted composition in a die or mold to provide a pre-treated glass- ceramic composition; b. exposing the pre-treated glass-ceramic composition to a two-step heat treatment process. The pre-treated glass-ceramic composition may be in the form of a cast glass monolith In some embodiments the step of melting the combined compounds in the method of producing the glass- ceramics of the present invention comprises heating the combined components to a temperature of from about 1300°C to about 1600°C. In some embodiments, the combined components are heated to a temperature of from about 1400°C to about 1500°C. In some embodiments the step of heating comprises heating the combined components for up to about 5 hours. In some embodiments the step of heating comprises heating the combined components for up to about 3 hours. In some embodiments, the method comprises heating the combined components to a temperature of from about 1300°C to about 1600°C for up to about 3 hours. The quenching step can be performed according to any suitable method. For example, quenching may comprise immersing the melted composition in a liquid, such as water. The drying step can be performed according to any suitable method. In some embodiments, the drying step may simply be leaving the quenched composition for a period sufficiency for the liquid used to quench the composition to evaporate. This may be instead of, or may be combined with, an active step of drying. In some embodiments, the step of drying the quenched composition in the method of producing the glass-ceramics of the present invention comprises a step of heating. In some embodiments the step of drying comprises heating from a temperature of about 50°C to about 150°C. In some embodiments the step of drying comprises heating from a temperature of about 60°C to about 100°C. In some embodiments the step of drying comprises heating from a temperature of about 60°C to about 100°C. In some embodiments the step of drying comprises heating for up to 24 hours. In some embodiments, the step of drying comprises heating from a temperature of about 50°C to about 150°C for up to 24 hours. The step of casting can be performed according to any suitable method. Generally, the milled and melted composition will be poured into a mold or die that will cause the composition to harden in a desired shape. After casting the composition, the composition may be left to cool. Alternatively, the composition may be actively cooled (for example by exposure to cold temperatures). In some embodiments, the composition is left to cool to room or ambient temperature (for example from about 15 to about 30oC). In some embodiments, this step of cooling does not comprise quenching. The cast composition may be in the form of a glass monolith. The above method steps refer to methods for making the pre-treated compositions. Methods of the invention for making the post-treated compositions may include the steps of making the pre-treated compositions. Alternatively, the methods of making the post-treated compositions may begin with a pre- treated compositions that was made at an earlier point in time. Methods of the invention extend to methods of making the pre-treated compositions, as well as to compositions obtained or obtainable by such methods. The method of producing the glass-ceramics of the present invention may comprise subjecting a pre- treatment composition (for example in the form of a cast glass monolith) to a two-step heat treatment process. The first heat treatment step comprising heating the composition to the, or around the, nucleation temperature of the composition. The second, subsequent, heat treatment step comprising heating the composition to the, or around the, crystallization temperature of the composition. The nucleation and / or crystallisation temperatures may be determined according to any suitable method known to the skilled person. For example, the nucleation and / or crystallisation temperature may be determined by differential thermal analysis (DTA), X-ray diffraction (XRD), differential scanning calorimetry (DSC), thermogravimetric analysis (TGA) or hot-stage microscopy. Nucleation is the process by which small crystal nuclei form in a material, and is the first step in the process of crystallisation. When a material is heated to or around its nucleation temperature, the energy of the system is sufficient to overcome the activation energy barrier and allow for the formation of crystal nuclei. Once crystal nuclei form, they can grow and develop into larger crystals, leading to the overall crystallisation of the material. The crystallization temperature refers to the temperature at which a material undergoes transformation from a non-crystalline, or amorphous, state to a crystalline state. This temperature is typically higher than the nucleation temperature, as the material needs to be heated to a higher temperature to complete the transformation from an amorphous to a crystalline structure. The nucleation temperature may be below the crystallization temperature. The nucleation temperature may be at or above the glass transition temperature (Tg) of the composition. In some embodiments, the nucleation temperature may be within (i.e. above or below) about 50°C of the glass transition temperature. The nucleation temperature is a temperature that causes crystal nucleation to take place. The crystal nucleation may comprise bulk crystal nucleation by amorphous phase separation. A glass transition temperature of a composition may be determined according to any suitable method known to the skilled person. For example, the glass transition temperature may be determined using differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA) or thermo-mechanical analysis (TMA). In some embodiments, the methods may comprise a step of determining the nucleation temperature, crystallisation temperature and / or glass transition temperature of the composition. Such a determination will allow the skilled person to determine the temperatures to use for the different steps of the method. Usually the crystallisation temperature will be above the nucleation and / or the glass transition temperature. The first step of the heat treatment process may comprise heating the composition to the, or around the, nucleation temperature of the composition for a period of time sufficient for crystal nucleation of the composition to take place. In some embodiments the first heat treatment step comprises heating the composition to the, or around the, nucleation temperature of the composition for at least about 30 minutes. In some embodiments, the method comprises heating the composition to the, or around the, nucleation temperature of the composition for at least about 1 hour. In some embodiments the first heat treatment step comprises heating the composition to the, or around the, nucleation temperature of the composition for up to 5 hours. In some embodiments the first heat treatment step comprises heating the composition to the, or around the, nucleation temperature of the composition for from about 30 minutes to about 5 hours. In some embodiments, the nucleation temperature may be from about 500°C to about 700°C. The second heat treatment step of the heat treatment process may comprise heating the composition to the, or around the, crystallization temperature for a period of time sufficient for crystallization of the composition to take place. In some embodiments, the second heat treatment step comprises heating the composition to the, or around the, crystallization temperature for at least about 30 minutes. In some embodiments, the second heat treatment step comprises heating the composition to the, or around the, crystallization temperature for up to 12 hours. In some embodiments, the second heat treatment step comprises heating the composition to the, or around the, crystallization temperature for from about 30 minutes to about 12 hours. In some embodiments, the crystallization temperature may be from about 700°C to about 1200°C. Although example ranges of nucleation and crystallisation temperatures are provided, the nucleation and crystallisation temperatures of any given composition will depend on its specific components and the relative amount of each component. Generally, the invention may require the nucleation and crystallisation temperatures of the compositions to be determined to allow appropriate temperatures for each stage of the method to be carried out. The determination of nucleation and crystallisation temperatures is within the remit of the skilled person and be achieved using known techniques, as discussed above. Generally, the nucleation and crystallisation temperatures may differ by at least about 50oC. In some embodiments, the method comprises providing a pre-treated glass-ceramic composition of the invention, and exposing the pre-treated composition to a two-step heat treatment process comprising: a. a first heat treatment step comprising heating the composition to the, or around the, nucleation temperature of the composition for from about 30 minutes to about 5 hours; and b. a second, subsequent, heat treatment step comprising heating the composition to the, or around the, crystallization temperature of the composition for from about 30 minutes to about 12 hours. In some embodiments, the method comprises providing a pre-treated glass-ceramic composition of the invention, and exposing the pre-treated composition to a two-step heat treatment process comprising: a. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC; and b. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC. The temperature of the second heat treatment step may be at least about 50oC higher than the first heat treatment step. In some embodiments, the method comprises providing a pre-treated glass-ceramic composition of the invention, and exposing the pre-treated composition to a two-step heat treatment process comprising: a. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC for at least about 30 minutes; and b. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC for at least about 30 minutes; wherein the temperature of the second heat treatment step is at least about 50oC higher than the first heat treatment step. In some embodiments, the method comprises providing a pre-treated glass-ceramic composition of the invention, and exposing the pre-treated composition to a two-step heat treatment process comprising: a. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC for at least about 30 minutes and up to about 5 hours; and b. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC for at least about 30 minutes and up to about 12 hours; wherein the temperature of the second heat treatment step is at least about 50oC higher than the first heat treatment step. In the two-step heat treatment process, the method may lead directly from the first heat treatment step to the second heat treatment step, without any intermediate steps. After the second heat treatment step, the composition may be left to cool. Alternatively, the composition may be actively cooled (for example by exposure to cold temperatures. In some embodiments, the composition is left to cool to room or ambient temperature (for example from about 15 to about 30oC). In some embodiments, this step of cooling does not comprise quenching. In preferred embodiments, the method of producing the glass-ceramics or products of the present invention does not comprise sintering. Advantageously, the method of the invention allows the compositions to be cast directly into a desired shape, for example into the shape of a dental implant product or part thereof. The ability to provide compositions of desired shapes without the need for sintering is advantageous as it does not require the effort or expense of sintering and does not expose the ceramic to methods that could adversely affect its structure or appearance. Post-crystallisation the glass-ceramic of the present invention may have a volume fraction of the mica crystal phase from about 5 to about 95% by volume mica, or from about 10 to about 90% by volume mica, or from about 20 to about 80% by volume mica. The glass-ceramic of the present invention may be full crystallised. The volume fraction may be determined according to any suitable methods, for example by SEM. In some embodiments, the SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 are provided in powdered form. In some embodiments, the components are provided in the amounts of: a. from about 41% to about 48% of SiO2; b. from about 15% to about 17% of Al2O3; c. from about 14% to about 16% of BaO; d. from about 7% to about 8% of MgO; e. from about 9% to about 11% of MgF2; and f. from about 0% to about 15% B2O3 or B2O3 is absent. BaO may alternatively or additionally be provided as BaCO3, which decomposes to BaO with lost of CO2. The methods of the invention may cause the amounts of different specific compound in the ceramic to change. For example, the methods of the invention may cause the amount of MgO to increase, the amount of MgF2 to decrease, and the amount of F2 to increase, compared to the starting (nominal) amounts. In some embodiments the method may comprise A. providing a pre-treated glass-ceramic composition, wherein the pre-treated glass-ceramic composition has been obtained or is obtainable according to a method comprising the steps of: a. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of: i. from about 41% to about 49% of SiO2; ii. from about 8% to about 23% of Al2O3; iii. from about 14% to about 16% of BaO; iv. from about 4% to about 8% of MgO; v. from about 5% to about 11% of MgF2; and vi. from about 0% to about 15% B2O3 or B2O3 is absent; b. melting the combined compounds to provide a melted composition; c. quenching the melted composition, optionally in water, to provide a quenched composition, d. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; e. milling the dry composition to provide a milled composition; f. melting the milled composition to provide a melted composition; g. casting the melted composition in a die or mold to provide a pre-treated glass- ceramic composition; B. exposing the pre-treated composition to a two-step heat treatment process comprising: a. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC for at least about 30 minutes and up to about 5 hours; and b. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC for at least about 30 minutes and up to about 12 hours; wherein the temperature of the second heat treatment step is at least about 50oC higher than the first heat treatment step. In some embodiments the method may comprise: a. combining SiO2, Al2O3, BaO, MgO, MgF2and optionally B2O3in the weight % amounts of: i. from about 41% to about 49% of SiO2; ii. from about 8% to about 23% of Al2O3; iii. from about 14% to about 16% of BaO; iv. from about 4% to about 8% of MgO; v. from about 5% to about 11% of MgF2; and vi. from about 0% to about 15% B2O3or B2O3is absent; b. melting the combined compounds to provide a melted composition; c. quenching the melted composition, optionally in water, to provide a quenched composition, d. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; e. milling the dry composition to provide a milled composition; f. melting the milled composition to provide a melted composition; g. casting the melted composition in a die or mold to provide a pre-treated glass- ceramic composition; h. exposing the pre-treated composition to a two-step heat treatment process comprising: i. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC for at least about 30 minutes and up to about 5 hours; and ii. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC for at least about 30 minutes and up to about 12 hours; wherein the temperature of the second heat treatment step is at least about 50oC higher than the first heat treatment step. The present invention also provide class-ceramic compositions obtained and obtainable by the methods of the invention. Other embodiments of the invention The present invention provides a number of methods and uses. For example, there is provided pre- and post-treatment glass-ceramic compositions obtained or obtainable using the methods of the invention. The invention also provides use of the glass-ceramics of the invention in the manufacture of dental restorations and / or dental implant products. These dental restorations or dental implant products may be used in dentistry, included but not limited to, general dentistry, cosmetic dentistry, periodontal dentistry, paediatric dentistry, endodontic dentistry, or to restore teeth following a disease or disorder. The disease or disease may be any disease or disorder that affects oral health. The present invention provides dental implant products such as a dental restoration products. Dental implant products (or dental restoration products) composed of the glass-ceramic compositions of the present invention may include, but are not limited to, veneers, inlays, onlays, bridges, crowns, custom- made post and core, constructs. In some embodiments, the dental implant product is a dental post or dental core. A dental post is generally a small rod or pin-shaped structure that is used to support a dental restoration, such as a crown or bridge, in a tooth that has been treated with a root canal. The dental post is typically made of materials such as metal, ceramic, or fiber-reinforced composite, and is inserted into the root canal after the damaged or diseased portion of the tooth has been removed. The post provides a stable foundation for the restoration to be attached to, helping to restore function and aesthetics to the tooth. The present invention allows the production of ceramic dental posts for the first time. The present invention therefore provides a dental post implant, wherein the dental post implant consists or consists essentially of the glass-ceramic composition of the invention. The dental post may be capable of being inserted into the root canal of a patient's tooth and having a structural and compositional compatibility with the natural tooth being restored. A dental core is a filling material that is used to rebuild the part of the tooth that has been lost due to decay, fracture or other damage. A core is used to create a stable foundation for the dental restoration. In some cases, a dental post is used in conjunction with a dental core. The post may be inserted into the root canal to provide support, and the core material used to rebuild the portion of the tooth that has been lost. A dental restoration, such as a crown or bridge, is then placed on top of the post and core to complete the reconstruction of the tooth. The glass-ceramic compositions may be present as a coating in dental implant products. The dental implant product may consist of or consist essentially of the glass-ceramic composition. The present invention also provides methods for dental surgery, comprising applying or implanting a dental implant product of the invention to the mouth of a patient. More specifically, the method may comprise implantation of the product into the alveolar bone or tooth socket of a patient. The glass-ceramic compositions of the present invention may also include wider applications in, for example, welding technology, vacuum technology, electrical engineering, electronics and semiconductor technology, laser industries, mechanical engineering, apparatus engineering, aerospace industry and nuclear technology. Glass-ceramics are defined as polycrystalline materials produced by controlled nucleation and crystallisation of parent glass, which results in the formation of crystalline phases embedded in a residual glass phase. The present invention will now be further described by way of illustration only with reference to the following Figures and Examples, which are not to be construed as being limiting on the invention. BRIEF DESCRIPTION OF THE FIGURES The figures of the present invention are a result of investigations of boric oxide content using compositions Series A, B, C and D. Reference is made to a number of Figures as follows: Figure 1 – Schematic of machinability tester. Figure 2 – Scanning Electron Micrograph (SEM) of mica-glass ceramics series D and C (see Tables 1 and 2). SEMs of compositions D and C show cabbage-head microstructure. Figure 3 - Hardness values of series B, C and D (see Tables 1 and 2). The hardness of B, C and D compared with commercial glass-ceramics (Vita Mark II® HT, Empress CAD® HT, Emax CAD® HT). Figure 4 - Machinability test force of series B, C and D (see Tables 1 and 2). The machinability of B, C and D compared with commercial glass-ceramics (Vita Mark II® HT, Empress CAD® HT, Emax CAD® HT). Figure 5 – Average biaxial flexural strength of series B, C and D (see Tables 1 and 2). The average biaxial flexural strength of B, C and D compared with commercial glass-ceramics (Vita Mark II® HT, Empress CAD® HT, Emax CAD® HT, VITRONIT®, MACOR®). Figure 6 – Indentation fracture toughness of series B, C and D (see Tables 1 and 2). Indentation fracture toughness of B, C and D compared with commercial glass-ceramics (Vita Mark II® HT, Empress CAD® HT, Emax CAD® HT). Figure 7 – Average transmittance percentage of series B, C and D (see Tables 1 and 2). Average transmittance percentage of B, C and D as a function of wavelength compared with commercial glass- ceramics (Vita Mark II® HT, Empress CAD® HT, Emax CAD® HT, and VITRONIT®) at wavelength 600 nm. EXAMPLES Glass compositional design as calculated examples A-J: Cabbage SiO2 Al2O3 BaO MgO B2O3 MgF2 K2O microstructure Examples (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) or curved crystals 1 A ‘’High Boric 41.18 14.57 13.52 6.86 14.83 9.01 0 No oxide’’ 2 B ‘’ Original’’ 44.48 15.74 14.60 7.4165 8.01 9.73 0 Yes 3 C ‘’Low Boric 46.42 16.42 15.24 7.73 4.01 10.15 0 Yes oxide’’ Cabbage SiO2 Al2O3 BaO MgO B2O3 MgF2 K2O microstructure Examples (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) or curved crystals D ‘’Zero Boric 48.36 17.11 15.87 8.06 0 10.58 0 Yes oxide’’ E ‘’Low 46.30 16.38 15.20 3.62 8.33 10.13 0 Yes Magnesia’’ F ‘’Low 49.31 8.28 14.50 8.22 8.88 10.79 0 No Alumina’’ G ‘’High 41.70 21.01 13.69 6.95 7.51 9.12 0 Yes Alumina’’ H ‘’Low 46.88 16.58 15.39 7.81 8.44 4.86 0 No Fluorine’’ I ‘’Low Boric oxide High 42.67 22.96 14.01 7.11 3.89 9.33 0 Yes Alumina’’ J ‘’Potassium 0 47.15 16.68 7.86 8.49 10.32 9.49 No substitute’’ Table 3 - Starting glass composition as calculated (weight %) Si2O Al2O3BaO MgO B2O3F2Examples (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) (Wt%) 1 A ‘’High Boric 42.03 16.00 14.60 12.59 12.10 3.70 oxide’’ 2 B 44.86 16.84 15.45 13.11 7.4 2.07 ‘’ Original’’ 3 C ‘’Low Boric 46.90 17.27 16.08 13.42 3.77 3.48 oxide’’ 4 D ‘’Zero Boric 46.49 18.07 17.16 14.75 0.0 3.56 oxide’’ Table 4 – Examples of post firing glass compositions. Series A-D compositions were used to investigate the effect of boric oxide content on synthesis and crystallisation of barium fluoromica glass-ceramics with cabbage-head microstructures. The inventors identified that the development of cabbage-head microstructure is strongly affected by the boric oxide content in the glass compositions. As boric oxide content decreases the cabbage-head microstructure develops more readily and at a lower temperature. Moreover, the size of each cabbage-head structure decreases with decreasing boric oxide content. Example 1 – Synthesis Glass synthesis The glasses were synthesised using thoroughly mixed batches of reagent-grade silica (SiO2), alumina (Al2O3), barium oxide (BaO) (and / or barium carbonate (BaCO3), boric oxide (B2O3), magnesium oxide (MgO), and magnesium fluoride (MgF2) powders. After weighing and mixing the powders, each batch was placed in a platinum crucible and fired in an electric furnace (EHF 17 / 3 Lenton, Hope Valley, UK) at temperatures between 1400 - 1500oC for 2 hrs. Glass melt was then quenched in deionized water and collected in 500 µm sieve [Endecotts Ltd., London, UK). The glass frit was left to dry overnight in an electric oven at 80 °C. Glass frit (100 g) was then milled using a Gy-Ro mill (Glen Creston, London, UK) for 3-5 minutes. The milled glass was then re-melted in a platinum crucible for 30 mins at 1500-1550 °C and then cast into pre-heated graphite moulds (Morgan Matroc, Stourport, England) to produce the desirable glass cast. The cast glass monoliths were then left to rest in an annealing furnace. Once the cast glass rods were inside, the furnace was turned off and the rods were left to cool down overnight inside the annealing furnace. Glass ceramic synthesis Cast glass monoliths produced were placed into a high temperature furnace [UAF 16 / 10, Hope Valley, Lenton, U.K] at room temperature and heated at a rate of 5-40 °C / min. Glasses were heat treated using a two-step heat treatment protocol by holding for 1 hour at nucleation temperature 660oC followed by crystal growth hold at crystallisation temperature for 5 hours at 1000oC. After heat treatment, the glass- ceramics were left inside the furnace to cool overnight. Example 2 – Glass-ceramics characterisation Scanning electron microscopy (SEM) Glass-ceramic samples from each heat treatment series were cut and embedded in resin (Epofix, Struers A / S, Ballerup, Denmark) and then left to set overnight. Samples were ground using silicon carbide papers (320, 600, 800, 1200, 2500and 4000 grit-size) and polished to an optical finish with 1μm alumina oxide polishing media (Buehler, USA) on a lapping machine (Struers, Knuth Rotor, Glasgow, UK), then cleaned in an ultrasonic bath [Kerry Ultrasonics, North Yorkshire, UK] for 10 minutes. Samples were gold coated using a sputter Coater (Emitech SC 7620, Quorum Technologies, and UK.) for 60 seconds. Specimens were viewed in scanning electron microscopy (FEI Inspect F, Hillsboro, Oregon, USA) in the back scattered imaging modes. Figure 2 shows the SEM micrographs of Mica glass-ceramics series D (Fig. 2A) and C (Fig. 2D) showing cabbage-head microstructures. D and C correspond to zero boric oxide and low boric oxide compositions, respectively. These compositions give rise to a cabbage-head microstructure. These cabbage-head microstructures provide better mechanical and machinable properties. Vickers Microhardness test Microhardness analysis was obtained on both experimental glass-ceramic samples (series B, C and D) and commercial glass-ceramics (Vita Mark II®HT, Empress CAD®HT, Emax CAD®HT), see Figure 3. Samples were embedded in epoxy resin. Samples were lapped using silicon carbide grinding paper (220, 320, 500, 800 and 1200 grit-size) and polished using 1μm alumina oxide polishing media (Buehler, USA) on a lapping machine (Struers, Knuth Rotor, Glasgow, UK). A Vickers hardness tester [ZHV30-S, Zwick / Roell AG, Germany] was used with an attached high sensitivity camera [902B WATEC, Japan]. Samples were indented using a pyramid diamond indenter with an angle of 136°, under an applied load of 1Kgf. The test force was maintained for 10 seconds, and then diagonal lengths of the indentation were measured and used to calculate the Vickers hardness. 2^^ sin Where: Hv is Vickers hardness; P is applied load (N); ^^ is the angle of the pyramid and d is the mean diagonal of indentation (mm). For each sample. For each sample, Vickers microhardness values of 12 points were recorded and converted to GPa by multiplying by 9.806 [standard gravity] and divided by 1000. Figure 3 demonstrates that hardness is reduced in series B, C and D, corresponding to original, low boric oxide and zero boric oxide compositions, respectively, when compared with commercially available glass- ceramics. For series B glass-ceramics were heat-treated at both 900°C and 1000°C. The high hardness of commercial glass-ceramics gives rise to reduced machinability and increased wearing of the opposing tooth structure due to the lower enamel hardness. Machinability Utilising the method outlined in Cresswell-Boyes et al. (A.J. Cresswell-Boyes et al., 2022), samples were cut into rods (ø 14.0 mm, lgth 20.0 mm) using a diamond cutter and were subsequently mounted to a 3- axis load cell (Model 3A60A, Interface Force Measurements Ltd., UK). A high-speed dental handpiece (TE- 95 BC Alegra Dental Air Rotor Handpiece, The W&H Group, Austria) with a straight fissure diamond bur (111-012M, Dentsply Sirona, USA) was mounted to a vertical stage (LMS-180 Precision Linear Stage, Physik Instrumente GmBH, Germany), which in turn was attached to a horizontal stage. Both stages were controlled using an A-81x PIglide Motion Controller (Physik Instrumente Ltd., Germany) running PIMikroMove (Version 2.10, 2015; Physik Instrumente GmBH, Germany). The handpiece was connected and powered by a portable turbine unit (GXJ Lab, China) and kept at a constant speed of 40000 rpm. The rate in which the dental handpiece cut into the sample was held at a set rate of 0.1 mm / s and was consistently 1.0 mm deep (from the highest point of the surface), with the forces being measured in real- time. Load data was recorded via a 4-channel signal amplifier (ME-Meβsysteme GmbH, Germany) connected to a computer running GSVmulti (Version 1.40, 2018; ME-Meβsysteme GmbH, Germany) which records real-time load data into a dynamic graph. A schematic of the machinability tester is shown in Figure 1. For analysis of the data, the 5–95th percentile range is taken, excluding the initial touch cut and the exit cut. This data is dependent on the geometry of the sample, so to ensure the comparison between different materials, this data is omitted from the analysis. The remaining 5–95th percentile range is averaged to give the average force required to cut. The first cut of a sample was also omitted due to the forces being dependent on the geometry of the material; therefore, measurements were only taken after the first 1 mm deep cut. Figure 4 demonstrates surprisingly reduced force required for cutting of series B, C and D, corresponding to original, low boric oxide and zero boric oxide compositions, respectively, when compared with commercially available glass-ceramics. For series B glass-ceramics were heat-treated at both 900°C and 1000°C. The reduced force required corresponds to increased machinability of these structures. Increased machinability (i.e. reduced force required) is desirable to reduce the need for high cost diamond / silicon carbide burs. Biaxial flexural strength (BFS) Glass-ceramic samples (series B, C and D) for the biaxial flexural strength test were cut from 14 mm diameter rods using a diamond saw into 2 mm discs (n = 20). Discs were then polished on one side using silicon carbide grinding paper (1200 and 2400 grit-size). Using Ball on Ring test configuration specimens were supported by a 10 mm diameter knife-edge and loaded in a universal testing machine (Instron 5567, Illinois Tool Works Inc., USA) at a crosshead speed of 1 mm / min until failure. Discs were placed with their polished surface under tension and the biaxial flexural strength was calculated using the Timoshenko and Woinowsky-Krieger and Timoshenko, : σ 0.48) where; σ max is the maximum tensile stress, P is the measured load at fracture, a is the radius of the knife- edge support, v is the Poisson’s ratio for the material [a value of 0.25 was substituted for porcelain], h is the specimen thickness measured with the digital micrometre, ln is the natural logarithm. Figure 5 shows the average biaxial flexural strength (BFS) of series B, C and D, corresponding to original, low boric oxide and zero boric oxide compositions, respectively, when compared with commercially available glass-ceramics. For series B glass-ceramics were heat-treated at both 900°C and 1000°C. Despite the increased machinability and reduced hardness of series B, C and D they surprisingly maintained biaxial flexural strengths comparable to commercially available glass-ceramics. Fracture toughness using indentation method (IF) Experimental glass-ceramic samples (series B, C and D) and commercial glass-ceramics ( Vita Mark II®HT, Empress CAD®HT, Emax CAD®HT) were cut into circular discs (4mm thickness X 14mm diameter) using a diamond saw and embedded in resin (Epofix, Struers A / S, Ballerup, Denmark) then left to set overnight. Samples were polished using silicon carbide grinding paper (220, 320, 500, 800 and 1200 grit-size) and polished using 1μm alumina oxide polishing media (Buehler, USA) on a lapping machine (Struers, Knuth Rotor, Glasgow, UK). Vickers hardness indenter was used to calculate fracture toughness with a 1Kgf load maintained for 10 seconds. Each glass-ceramic sample was tested 10-15 times to calculate the mean IF using the following (Lawn and Wilshaw, 1975): WhereK1cis the indentation fracture toughness; ψbis the half angle of the Vickers pyramidal indenter (68°) giving ψb= 0.072558; P is the indentation load in Newton; c0is the radial crack length in meters. Figure 6 shows the fracture toughness of series B, C and D, corresponding to original, low boric oxide and zero boric oxide compositions, respectively, using the indentation method, when compared with commercially available glass-ceramics. For series B glass-ceramics were heat-treated at both 900°C and 1000°C. Despite the increased machinability and reduced hardness of series B, C and D they surprisingly maintained fracture toughness comparable to commercially available glass-ceramics. Light transmission percentage (T%) Experimental glass-ceramic samples (series B, C and D) and commercial glass-ceramics (Vita Mark II®HT, Empress CAD®HT, Emax CAD®HT and VITRONIT®) of 1mm thickness were cut using a diamond cutting machine (Struers, Germany). The samples were then polished using silicon carbide grinding papers (320, 600, 800 and 1200, 2400 and 4000 grit-size) and polished using 1 μm alumina oxide polishing media (Buehler, USA) on a lapping machine (Knuth Rotor, Struers, UK). Samples were then cleaned in an ultrasonic bath for 10 minutes and then left to dry. The light transmission percentage (T%) of the prepared samples was measured using Lambda 950 UV-vis spectrometer (Perkin Elmer, CT, USA). The following parameters have been used to measure T%: slit of 0.5 nm, scan speed of 260 nm / min, 10 nm smooth. Measurements were made on the wavelength range of 350– 800 nm with a data interval of 1 nm. The mean T% values at 600 nm wavelength were used for comparison between samples. Figure 7 shows the light transmission percentage (T%) of series B, C and D, corresponding to original, low boric oxide and zero boric oxide compositions, respectively, when compared with commercially available glass-ceramics. For series B glass-ceramics were heat-treated at both 900°C and 1000°C. Series B, C and D have comparable light transmission percentage (T%) with commercially available glass-ceramics. REFERENCES Cresswell-Boyes, A.J., Davis, G.R., Krishnamoorthy, M., Mills, D. and Barber, A.H., 2022. Composite 3D printing of biomimetic human teeth. Scientific Reports, 12(1), pp.1 -11. Guess, P.C., Schultheis, S., Bonfante, E.A., Coelho, P.G., Ferencz, J.L., Silva, N.R.F.A., 2011. All-ceramic systems: Laboratory and clinical performance. Dental Clinics of North America 55, 333-352 Holand, W., Beall, G.H., 2012. Glass-Ceramic Technology: Second Edition, Glass-Ceramic Technology: Second Edition. John Wiley & Sons, Inc., Hoboken, NJ, USA. Homaei E, Farhangdoost K, Tsoi JKH, Matinlinna JP, Pow EHN. Static and fatigue mechanical behavior of three dental CAD / CAM ceramics. J Mech Behav Biomed Mater.2016 Jun;59:304-313 Lawn, B., Wilshaw, R., 1975. Indentation fracture: principles and applications. Journal of Materials Science 10, 1049-1081 Seghi, R., Denry, I., Dentistry, S.R.-J. of P., 1995, U., 1995. Relative fracture toughness and hardness of new dental ceramics. The Journal of Prosthetic Dentistry 74, 145-150 Ho land W, Vogel W, Mortier W, Duvigneaud PH, Naessens G, Plumat E (1983). A new type of phlogopite crystal in machineable glass ceramics. Glass Technology 24, 318-322. EMBODIMENTS The present invention relates at least to the following numbered embodiments: 1. A glass-ceramic composition comprising, consisting essentially of, or consisting of SiO2, Al2O3,BaO, and MgO, either MgF2 or F2, and optionally B2O3, wherein: a. the amount of SiO2 in the composition by weight % is from about 41% to about 49%; b. the amount of Al2O3 in the composition by weight % is from about 8% to about 23%; c. the amount of BaO in the composition by weight % is from about 9% to about 17%; d. the amount of MgO in the composition by weight % is from about 4% to about 15%; e. the amount of MgF2in the composition, if present, is from about 3% to about 11% by weight; f. the amount of F2 in the composition, if present, is from about 2% to about 4% by weight; and g. the amount of B2O3in the composition by weight % is from about 0% to about 15%, or B2O3is absent. 2. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 41% to about 49% by weight SiO2. 3. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 8% to about 23% by weight of Al2O3; 4. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 14% to about 17% by weight of BaO; 5. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 4% to about 15% by weight of MgO; 6. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 0% to about 15% by weight of B2O3, or wherein B2O3is absent. 7. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 5% to about 11% by weight of MgF2. 8. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 2% to about 4% by weight of F2. 9. The glass-ceramic composition of embodiment 1, wherein the glass-ceramic composition comprises, consists essentially of, or consist of SiO2, Al2O3, BaO, MgO, MgF2, and optionally B2O3, wherein: a. the amount of SiO2 in the composition by weight % is from about 41% to about 49%; b. the amount of Al2O3 in the composition by weight % is from about 8% to about 23%; c. the amount of BaO in the composition by weight % is from about 14% to about 16%; d. the amount of MgO in the composition by weight % is from about 4% to about 8%; e. the amount of MgF2in the composition by weight % is from about 5% to about 11%; and f. the amount of B2O3in the composition by weight % is from about 0% to about 15%, or B2O3 is absent. 10. The glass-ceramic composition of embodiment 1 or embodiment 2 comprising, consisting essentially of, or consisting of SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3, wherein: a. the amount of SiO2in the composition by weight % is from about 42% to about 48%; b. the amount of Al2O3in the composition by weight % is from about 16% to about 23%; c. the amount of BaO in the composition by weight % is from about 14% to about 16%; d. the amount of MgO in the composition by weight % is from about 4% to about 8%; e. the amount of MgF2 in the composition by weight % is from about 9% to about 11%; and f. the amount of B2O3 in the composition by weight % is from about 0% to about 8%, or B2O3 is absent. 11. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 41% to about 49% by weight SiO2. 12. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 8% to about 23% by weight of Al2O3; 13. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 14% to about 16% by weight of BaO; 14. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 4% to about 8% by weight of MgO; 15. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 0% to about 15% by weight of B2O3, or wherein B2O3 is absent. 16. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 5% to about 11% by weight of MgF2. 17. The glass-ceramic composition of embodiment 1, wherein: a. the composition comprises, consists essentially of, or consists of: i. about 41% by weight of SiO2; ii. about 15% by weight Al2O3; iii. about 14% by weight BaO; iv. about 7% by weight MgO; v. about 15% by weight B2O3; and vi. about 9% by weight MgF2; b. the composition comprises, consists essentially of, or consists of: i. about 44% by weight of SiO2; ii. about 16% by weight Al2O3; iii. about 15% by weight BaO; iv. about 7% by weight MgO; v. about 8% by weight B2O3; and vi. about 10% by weight MgF2; c. the composition comprises, consists essentially of, or consists of: i. about 47% by weight of SiO2; ii. about 16% by weight Al2O3; iii. about 15% by weight BaO; iv. about 8% by weight MgO; v. about 4% by weight B2O3; and vi. about 10% by weight MgF2; d. the composition comprises, consists essentially of, or consists of: i. about 48% by weight of SiO2; ii. about 17% by weight Al2O3; iii. about 16% by weight BaO; iv. about 8% by weight MgO; and v. about 11% by weight MgF2; e. the composition comprises, consists essentially of, or consists of: i. about 46% by weight of SiO2; ii. about 16% by weight Al2O3; iii. about 15% by weight BaO; iv. about 4% by weight MgO; v. about 8% by weight B2O3; and vi. about 10% by weight MgF2; f. the composition comprises, consists essentially of, or consists of: i. about 49% by weight of SiO2; ii. about 8% by weight Al2O3; iii. about 15% by weight BaO; iv. about 8% by weight MgO; v. about 9% by weight B2O3; and vi. about 11% by weight MgF2; g. the composition comprises, consists essentially of, or consists of: i. about 42% by weight of SiO2; ii. about 21% by weight Al2O3; iii. about 14% by weight BaO; iv. about 7% by weight MgO; v. about 8% by weight B2O3; and vi. about 9% by weight MgF2; h. the composition comprises, consists essentially of, or consists of: i. about 47% by weight of SiO2; ii. about 17% by weight Al2O3; iii. about 15% by weight BaO; iv. about 8% by weight MgO; v. about 8% by weight B2O3; and vi. about 5% by weight MgF2; i. the composition comprises, consists essentially of, or consists of: i. about 43% by weight of SiO2; ii. about 23% by weight Al2O3; iii. about 14% by weight BaO; iv. about 7% by weight MgO; v. about 4% by weight B2O3; and vi. about 9% by weight MgF2; or j. the composition comprises, consists essentially of, or consists of: i. about 49% by weight of SiO2; ii. about 8% by weight Al2O3; iii. about 15% by weight BaO; iv. about 8% by weight MgO; v. about 9% by weight B2O3; and vi. about 11% by weight MgF2; 18. The glass-ceramic composition of embodiment 1 comprising, consisting essentially of, or consisting of SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3, wherein: a. the amount of SiO2 in the composition by weight % is from about 42% to about 47%; b. the amount of Al2O3 in the composition by weight % is from about 16% to about 18%; c. the amount of BaO in the composition by weight % is from about 15% to about 17%; d. the amount of MgO in the composition by weight % is from about 13% to about 15%; e. the amount of F2in the composition by weight % is from about 2% to about 4%; and f. the amount of B2O3in the composition by weight % is from about 0% to about 12%, or B2O3 is absent. 19. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 42% to about 47% by weight SiO2. 20. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 16% to about 18% by weight of Al2O3; 21. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 15% to about 17% by weight of BaO; 22. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 13% to about 15% by weight of MgO; 23. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 0% to about 12% by weight of B2O3, or wherein B2O3is absent. 24. The glass-ceramic composition of any preceding embodiment, wherein the composition comprises, consists essentially of, or consists of from about 2% to about 4% by weight of F2. 25. The glass-ceramic composition of embodiment 1, wherein: a. the composition comprises, consists essentially of, or consists of: i. about 42% by weight of SiO2; ii. about 16% by weight Al2O3; iii. about 15% by weight BaO; iv. about 13% by weight MgO; v. about 12% by weight B2O3; and vi. about 4% by weight F2; b. the composition comprises, consists essentially of, or consists of: i. about 45% by weight of SiO2; ii. about 17% by weight Al2O3; iii. about 15% by weight BaO; iv. about 13% by weight MgO; v. about 7% by weight B2O3; and vi. about 3% by weight F2; c. the composition comprises, consists essentially of, or consists of: i. about 47% by weight of SiO2; ii. about 17% by weight Al2O3; iii. about 16% by weight BaO; iv. about 13% by weight MgO; v. about 4% by weight B2O3; and vi. about 3% by weight F2; or d. the composition comprises, consists essentially of, or consists of: i. about 46% by weight of SiO2; ii. about 18% by weight Al2O3; iii. about 17% by weight BaO; iv. about 15% by weight MgO; and v. about 4% by weight F2; 26. The glass-ceramic composition of any preceding embodiment wherein the compositions exhibit curved crystals or curved crystal agglomerates in scanning electron micrographs. 27. The glass-ceramic composition of embodiment 26 wherein the apparent radius of the curved crystals or curved crystal agglomerates is less than 200 microns 28. The glass-ceramic composition of embodiment 26 wherein the apparent radius of the curved crystals or curved crystal agglomerates is less than 20 microns. 29. The glass-ceramic composition of any one of embodiments 26 to 28 wherein the curved crystals comprise of barium fluorphlogopite. 30. The glass-ceramic composition of any one of embodiments 26 to 29 wherein the curved crystals comprise of barium kinoshitalite. 31. The glass-ceramic composition of any one of embodiments 26 to 30 wherein the curved crystals comprise of a mixture of a solid solution phase of barium fluorphlogopite and barium kinoshitalite. 32. The glass-ceramic composition of any preceding embodiment wherein the glass-ceramic is a barium fluoromica. 33. The glass-ceramic composition of embodiment 32 wherein the barium fluoromica exhibits a cabbage-head microstructure. 34. The glass-ceramic composition of any preceding embodiment wherein the glass-ceramic composition exhibit a hardness of from about 3 to about 4.5 GPa. 35. The glass-ceramic composition of embodiment 34, wherein the hardness is the Vickers hardness. 36. The glass-ceramic composition of any one of embodiments 34 to 35, wherein the hardness is measured according to BSI ENV 843-4:1995. 37. The glass-ceramic composition of any preceding embodiment wherein the biaxial flexural strength is about 200 MPa to about 300 MPa. 38. The glass-ceramic composition of embodiment 37, wherein the biaxial flexural strength is measured according to ISO 6872:2015 (edition 5). 39. The glass-ceramic composition of any preceding embodiment wherein the glass-ceramics exhibits translucency, with a light transmission of from about 35% to about 75%. 40. The glass-ceramic composition of any preceding embodiment wherein the glass-ceramics exhibits translucency, with a light transmission of from about 60% to about 75%. 41. The glass-ceramic composition of embodiment 39 or embodiment 40, wherein the translucency is measured through a sample of composition having a thickness of about 1mm. 42. The glass-ceramic composition of any one of embodiments 39 to 41, wherein the translucency is the translucency of the material to 600 nm wavelength light. 43. The glass-ceramic composition of any one of embodiments 39 to 42, wherein the translucency is measured according to the following method: a. providing a planar sample of the composition having a thickness of 1mm, optionally wherein the planar sample of the composition has been polished; b. transmitting 600 nm wavelength light through the sample at an angle perpendicular to the planar surface of the sample; and c. measuring the amount of light that passes through the sample as a percentage of the light transmitted to provide a % translucency. 44. The glass-ceramic composition of any one of embodiments 39 to 43, wherein the method comprises: a. providing a planar sample of the composition having a thickness of 1mm; b. polishing the sample of the composition; c. cleaning the polished sample; d. drying the cleaned sample, or allowing the cleaned sample to dry; e. transmitting 600 nm wavelength light through the dried sample at an angle perpendicular to the planar surface of the sample; and f. measuring the amount of light that passes through the sample as a percentage of the light transmitted to provide a % translucency. 45. The glass-ceramic composition of any one of embodiments 39 to 44, wherein the method comprises: a. providing a planar sample of the composition having a thickness of 1mm; b. polishing the sample of the composition using 1 μm alumina oxide polishing media on a lapping machine; c. cleaning the polished sample in an ultrasonic bath for 10 minutes; d. drying the cleaned sample, or allowing the cleaned sample to dry; e. transmitting 600 nm wavelength light through the dried sample at an angle perpendicular to the planar surface of the sample; and f. measuring the amount of light that passes through the sample as a percentage of the light transmitted to provide a % translucency. 46. The glass-ceramic composition of any preceding embodiment (preferably the pre-fired compositions, e.g. those of embodiments 1 to 18 and embodiments 26 to 45 when dependent on any of embodiments 1 to 18), wherein the specified weight amount of each component is the nominal weight amount. 47. The glass-ceramic composition of any preceding embodiment (preferably the post-fired compositions, e.g. those of embodiments 19 to 25 and embodiments 26 to 45 when dependent on any of embodiments 19 to 25), wherein the specified weight amount of each component is the analysed weight amount. 48. The glass-ceramic composition of any preceding embodiment (preferably the post-fired compositions, e.g. those of embodiments 19 to 25 and embodiments 26 to 45 when dependent on any of embodiments 19 to 25), wherein the specified weight amount of each component is determined by X-ray fluorescence. 49. A method of producing a glass-ceramic composition, comprising providing a glass-ceramic composition according to any one of embodiments 1 to 48, and exposing the pre-treated composition to a two-step heat treatment process. 50. The method of embodiment 49, wherein the method comprises: a. providing a pre-treated glass-ceramic composition, wherein the pre-treated glass- ceramic composition has been obtained or is obtainable according to a method comprising the steps of: i. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of: 1. from about 41% to about 49% of SiO2; 2. from about 8% to about 23% of Al2O3; 3. from about 14% to about 16% of BaO; 4. from about 4% to about 8% of MgO; 5. from about 5% to about 11% of MgF2; and 6. from about 0% to about 15% B2O3 or B2O3 is absent; ii. melting the combined compounds to provide a melted composition; iii. quenching the melted composition, optionally in water, to provide a quenched composition, iv. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; v. milling the dry composition to provide a milled composition; vi. melting the milled composition to provide a melted composition; vii. casting the melted composition in a die or mold to provide a pre-treated glass- ceramic composition; b. exposing the pre-treated glass-ceramic composition to a two-step heat treatment process. 51. The method of any one of embodiments 49 to 50, wherein the pre-treated glass-ceramic composition is in the form of a cast glass monolith. 52. The method of any one of embodiments 49 to 51, wherein the step of melting the combined compounds comprises a step of heating the combined compounds to a temperature of from about 1300oC to about 1600oC. 53. The method of embodiment 52, wherein the step of melting the combined compounds comprises a step of heating the combined compounds to a temperature of from about 1400 oC to about 1500oC 54. The method of any one of embodiments 49 to 53, wherein the step of heating comprising heating the combined compounds for up to about 3 hours. 55. The method of any one of embodiments 49 to 54, wherein the step of drying the quenched composition comprises a step of heating. 56. The method of embodiment 55, wherein the step of heating comprises heating to a temperature of between 60oC and 100oC, for up to 24 hours. 57. The method of any one of embodiments 49 to 56, wherein the two-step heat treatment process comprises: a. a first heat treatment step comprising heating the composition to the, or around the, nucleation temperature of the composition; and b. a second, subsequent, heat treatment step comprising heating the composition to the, or around the, crystallization temperature of the composition. 58. The method of embodiment 57, wherein the nucleation temperature is below the crystallization temperature. 59. The method of embodiment 57 or 58, wherein the nucleation temperature is within about 50oC of the glass transition temperature. 60. The method of any one of embodiments 57 to 59, wherein the nucleation temperature is a temperature that causes crystal nucleation to take place. 61. The method of embodiment 60, wherein crystal nucleation comprises bulk crystal nucleation by amorphous phase separation. 62. The method of any one of embodiments 57 to 61, wherein the first heat treatment step comprises heating the composition to the, or around the, nucleation temperature of the composition for a period of time sufficient for crystal nucleation of the composition to take place. 63. The method of any one of embodiments 57 to 62, wherein the first heat treatment step comprises heating the composition to the, or around the, nucleation temperature of the composition for at least about 30 minutes. 64. The method of any one of embodiments 57 to 63, wherein the first heat treatment step comprises heating the composition to the, or around the, nucleation temperature of the composition for up to 5 hours. 65. The method of any one of embodiments 57 to 64, wherein the first heat treatment step comprises heating the composition to the, or around the, nucleation temperature of the composition for from about 30 minutes to about 5 hours. 66. The method of any one of embodiments 57 to 65, wherein the crystallization temperature is from about 700°C to about 1200°C. 67. The method of any one of embodiments 57 to 66, wherein the second heat treatment step comprises heating the composition to the, or around the, crystallization temperature for a period of time sufficient for crystallization of the composition to take place. 68. The method of any one of embodiments 57 to 67, wherein the second heat treatment step comprises heating the composition to the, or around the, crystallization temperature for at least about 30 minutes. 69. The method of any one of embodiments 57 to 68, wherein the second heat treatment step comprises heating the composition to the, or around the, crystallization temperature for up to 12 hours. 70. The method of any one of embodiments 57 to 69, wherein the second heat treatment step comprises heating the composition to the, or around the, crystallization temperature for from about 30 minutes to about 12 hours. 71. The method of any one of embodiments 57 to 70, wherein post crystallization, the volume fraction of the mica crystal phase in the composition is between 5 and 95% by volume mica. 72. The method of any one of embodiments 57 to 5971, wherein post crystallization, the volume fraction of the mica crystal phase in the composition is between 20 and 80% by volume mica. 73. The method of any one of embodiments 57 to 72, wherein post crystallization, the composition is fully crystallized. 74. The method of any one of embodiments 49 to 73, wherein the method comprising the steps of a. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of: i. from about 41% to about 49% of SiO2; ii. from about 8% to about 23% of Al2O3; iii. from about 14% to about 16% of BaO; iv. from about 4% to about 8% of MgO; v. from about 5% to about 11% of MgF2; and vi. from about 0% to about 15% B2O3 or B2O3 is absent; b. melting the combined compounds to provide a melted composition; c. quenching the melted composition, optionally in water, to provide a quenched composition, d. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; e. milling the dry composition to provide a milled composition; f. melting the milled composition to provide a melted composition; g. casting the melted composition in a die or mold to provide a glass-ceramic composition. 75. A method of producing a glass-ceramic composition, comprising, wherein the method comprising the steps of a. combining SiO2, Al2O3, BaO, MgO, MgF2and optionally B2O3in the weight % amounts of: i. from about 41% to about 49% of SiO2; ii. from about 8% to about 23% of Al2O3; iii. from about 14% to about 16% of BaO; iv. from about 4% to about 8% of MgO; v. from about 5% to about 11% of MgF2; and vi. from about 0% to about 15% B2O3or B2O3is absent; b. melting the combined compounds to provide a melted composition; c. quenching the melted composition, optionally in water, to provide a quenched composition, d. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; e. milling the dry composition to provide a milled composition; f. melting the milled composition to provide a melted composition; g. casting the melted composition in a die or mold to provide a glass-ceramic composition. 76. The method of any one of embodiments 49 to 75, wherein the SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 are provided in powdered form. 77. The method of any one of embodiments 49 to 76, wherein the SiO2, Al2O3, BaO, MgO, MgF2and optionally B2O3are combined in the weight % amounts of: a. from about 41% to about 48% of SiO2; b. from about 15% to about 17% of Al2O3; c. from about 14% to about 16% of BaO; d. from about 7% to about 8% of MgO; e. from about 9% to about 11% of MgF2; and f. from about 0% to about 15% B2O3 or B2O3 is absent. The method of any one of embodiments 49 to 77 wherein the method does not comprise sintering. The method of any one of embodiments 49 to 77, wherein the method is a method of producing the glass-ceramic composition of any one of embodiments 1 to 48. The method of any one of embodiments 49 to 79, wherein the method comprises: a. providing a pre-treated glass-ceramic composition, wherein the pre-treated glass- ceramic composition has been obtained or is obtainable according to a method comprising the steps of: i. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of: 1. from about 41% to about 49% of SiO2; 2. from about 8% to about 23% of Al2O3; 3. from about 14% to about 16% of BaO; 4. from about 4% to about 8% of MgO; 5. from about 5% to about 11% of MgF2; and 6. from about 0% to about 15% B2O3 or B2O3 is absent; ii. melting the combined compounds to provide a melted composition; iii. quenching the melted composition, optionally in water, to provide a quenched composition, iv. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; v. milling the dry composition to provide a milled composition; vi. melting the milled composition to provide a melted composition; vii. casting the melted composition in a die or mold to provide a pre-treated glass- ceramic composition; b. exposing the pre-treated composition to a two-step heat treatment process comprising: i. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC for at least about 30 minutes and up to about 5 hours; and ii. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC for at least about 30 minutes and up to about 12 hours; wherein the temperature of the second heat treatment step is at least about 50oC higher than the first heat treatment step. The method of any one of embodiments 49 to 80, wherein the method comprises: a. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of: i. from about 41% to about 49% of SiO2; ii. from about 8% to about 23% of Al2O3; iii. from about 14% to about 16% of BaO; iv. from about 4% to about 8% of MgO; v. from about 5% to about 11% of MgF2; and vi. from about 0% to about 15% B2O3or B2O3is absent; b. melting the combined compounds to provide a melted composition; c. quenching the melted composition, optionally in water, to provide a quenched composition, d. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; e. milling the dry composition to provide a milled composition; f. melting the milled composition to provide a melted composition; g. casting the melted composition in a die or mold to provide a pre-treated glass-ceramic composition; h. exposing the pre-treated composition to a two-step heat treatment process comprising: i. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC for at least about 30 minutes and up to about 5 hours; and ii. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC for at least about 30 minutes and up to about 12 hours; wherein the temperature of the second heat treatment step is at least about 50oC higher than the first heat treatment step. A glass-ceramic composition obtainable by a method according to any one of embodiments 49 to 71. A glass-ceramic composition obtained by a method according to any one of embodiments 49 to 71. 84. Use of the glass-ceramic composition of any one of embodiments 1 to 48, 82 or 83 in dentistry. 85. Use of the glass-ceramic composition of any one of embodiments 1 to 48, 82 or 83 as or in a dental implant product. 86. A dental implant product comprising or consisting of the glass-ceramic composition of any one of embodiments 1 to 48, 82 or 83. 87. The dental implant product of embodiment 86 wherein the dental implant product is a veneer, an inlay, onlay, a bridge, a crown, a post and core, or a construct. 88. The dental implant product of embodiment 86 or 87, wherein the glass-ceramic composition is present as a coating. 89. The dental implant product of any one of embodiments 86 to 88, wherein the dental implant product consists of or consists essentially of the glass-ceramic composition.
Claims
CLAIMS 1. A glass-ceramic composition comprising, consisting essentially of, or consisting of SiO2, Al2O3,BaO, and MgO, either MgF2or F2, and optionally B2O3,wherein: a. the amount of SiO2 in the composition by weight % is from about 41% to about 49%; b. the amount of Al2O3 in the composition by weight % is from about 8% to about 23%; c. the amount of BaO in the composition by weight % is from about 9% to about 17%; d. the amount of MgO in the composition by weight % is from about 4% to about 15%; e. the amount of MgF2in the composition, if present, is from about 3% to about 11% by weight; f. the amount of F2in the composition, if present, is from about 2% to about 4% by weight; and g. the amount of B2O3 in the composition by weight % is from about 0% to about 15%, or B2O3 is absent.
2. The glass-ceramic composition of claim 1, wherein the glass-ceramic composition comprises, consists essentially of, or consist of SiO2, Al2O3,BaO, MgO, MgF2, and optionally B2O3,wherein: a. the amount of SiO2in the composition by weight % is from about 41% to about 49%; b. the amount of Al2O3 in the composition by weight % is from about 8% to about 23%; c. the amount of BaO in the composition by weight % is from about 14% to about 16%; d. the amount of MgO in the composition by weight % is from about 4% to about 8%; e. the amount of MgF2 in the composition by weight % is from about 5% to about 11%; and f. the amount of B2O3in the composition by weight % is from about 0% to about 15%, or B2O3is absent.
3. The glass-ceramic composition of claim 1 or claim 2 comprising, consisting essentially of, or consisting of SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3, wherein: a. the amount of SiO2 in the composition by weight % is from about 42% to about 48%; b. the amount of Al2O3 in the composition by weight % is from about 16% to about 23%; c. the amount of BaO in the composition by weight % is from about 14% to about 16%; d. the amount of MgO in the composition by weight % is from about 4% to about 8%; e. the amount of MgF2in the composition by weight % is from about 9% to about 11%; and f. the amount of B2O3 in the composition by weight % is from about 0% to about 8%, or B2O3 is absent.
4. The glass-ceramic composition of claim 1, wherein:a. the composition comprises, consists essentially of, or consists of: i. about 41% by weight of SiO2; ii. about 15% by weight Al2O3; iii. about 14% by weight BaO; iv. about 7% by weight MgO; v. about 15% by weight B2O3; and vi. about 9% by weight MgF2; b. the composition comprises, consists essentially of, or consists of: i. about 44% by weight of SiO2; ii. about 16% by weight Al2O3; iii. about 15% by weight BaO; iv. about 7% by weight MgO; v. about 8% by weight B2O3; and vi. about 10% by weight MgF2; c. the composition comprises, consists essentially of, or consists of: i. about 47% by weight of SiO2; ii. about 16% by weight Al2O3; iii. about 15% by weight BaO; iv. about 8% by weight MgO; v. about 4% by weight B2O3; and vi. about 10% by weight MgF2; d. the composition comprises, consists essentially of, or consists of: i. about 48% by weight of SiO2; ii. about 17% by weight Al2O3; iii. about 16% by weight BaO; iv. about 8% by weight MgO; and v. about 11% by weight MgF2; e. the composition comprises, consists essentially of, or consists of: i. about 46% by weight of SiO2; ii. about 16% by weight Al2O3; iii. about 15% by weight BaO; iv. about 4% by weight MgO; v. about 8% by weight B2O3; and vi. about 10% by weight MgF2; f. the composition comprises, consists essentially of, or consists of: i. about 49% by weight of SiO2;ii. about 8% by weight Al2O3; iii. about 15% by weight BaO; iv. about 8% by weight MgO; v. about 9% by weight B2O3; and vi. about 11% by weight MgF2; g. the composition comprises, consists essentially of, or consists of: i. about 42% by weight of SiO2; ii. about 21% by weight Al2O3; iii. about 14% by weight BaO; iv. about 7% by weight MgO; v. about 8% by weight B2O3; and vi. about 9% by weight MgF2; h. the composition comprises, consists essentially of, or consists of: i. about 47% by weight of SiO2; ii. about 17% by weight Al2O3; iii. about 15% by weight BaO; iv. about 8% by weight MgO; v. about 8% by weight B2O3; and vi. about 5% by weight MgF2; i. the composition comprises, consists essentially of, or consists of: i. about 43% by weight of SiO2; ii. about 23% by weight Al2O3; iii. about 14% by weight BaO; iv. about 7% by weight MgO; v. about 4% by weight B2O3; and vi. about 9% by weight MgF2; or j. the composition comprises, consists essentially of, or consists of: i. about 49% by weight of SiO2; ii. about 8% by weight Al2O3; iii. about 15% by weight BaO; iv. about 8% by weight MgO; v. about 9% by weight B2O3; and vi. about 11% by weight MgF2; 5. The glass-ceramic composition of claim 1 comprising, consisting essentially of, or consisting of SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3, wherein:a. the amount of SiO2 in the composition by weight % is from about 42% to about 47%; b. the amount of Al2O3in the composition by weight % is from about 16% to about 18%; c. the amount of BaO in the composition by weight % is from about 15% to about 17%; d. the amount of MgO in the composition by weight % is from about 13% to about 15%; e. the amount of F2 in the composition by weight % is from about 2% to about 4%; and f. the amount of B2O3 in the composition by weight % is from about 0% to about 12%, or B2O3 is absent.
6. The glass-ceramic composition of claim 11, wherein: a. the composition comprises, consists essentially of, or consists of: i. about 42% by weight of SiO2; ii. about 16% by weight Al2O3; iii. about 15% by weight BaO; iv. about 13% by weight MgO; v. about 12% by weight B2O3; and vi. about 4% by weight F2; b. the composition comprises, consists essentially of, or consists of: i. about 45% by weight of SiO2; ii. about 17% by weight Al2O3; iii. about 15% by weight BaO; iv. about 13% by weight MgO; v. about 7% by weight B2O3; and vi. about 3% by weight F2; c. the composition comprises, consists essentially of, or consists of: i. about 47% by weight of SiO2; ii. about 17% by weight Al2O3; iii. about 16% by weight BaO; iv. about 13% by weight MgO; v. about 4% by weight B2O3; and vi. about 3% by weight F2; or d. the composition comprises, consists essentially of, or consists of: i. about 46% by weight of SiO2; ii. about 18% by weight Al2O3; iii. about 17% by weight BaO; iv. about 15% by weight MgO; and v. about 4% by weight F2;7. The glass-ceramic composition of any preceding claim wherein the glass-ceramic is a barium fluoromica.
8. The glass-ceramic composition of any preceding claim wherein the glass-ceramic is a barium fluoromica that exhibits a cabbage-head microstructure.
9. The glass-ceramic composition of any preceding claim wherein the glass-ceramic composition exhibit a hardness of from about 3 to about 4.5 GPa.
10. The glass-ceramic composition of any preceding claim wherein the biaxial flexural strength is about 200 MPa to about 300 MPa.
11. The glass-ceramic composition of any preceding claim wherein the glass-ceramics exhibits translucency, with a light transmission of from about 35% to about 75%, wherein the translucency is measured according to the following method: a. providing a planar sample of the composition having a thickness of 1mm, optionally wherein the planar sample of the composition has been polished; b. transmitting 600 nm wavelength light through the sample at an angle perpendicular to the planar surface of the sample; and c. measuring the amount of light that passes through the sample as a percentage of the light transmitted to provide a % translucency.
12. A method of producing a glass-ceramic composition, comprising providing a glass-ceramic composition according to any one of claims 1 to 11, and exposing the pre-treated composition to a two-step heat treatment process.
13. The method of claim 12, wherein the method comprises: a. providing a pre-treated glass-ceramic composition, wherein the pre-treated glass- ceramic composition has been obtained or is obtainable according to a method comprising the steps of: i. combining SiO2, Al2O3, BaO, MgO, MgF2and optionally B2O3in the weight % amounts of:
1. from about 41% to about 49% of SiO2; 2. from about 8% to about 23% of Al2O3; 3. from about 14% to about 16% of BaO;4. from about 4% to about 8% of MgO; 5. from about 5% to about 11% of MgF2; and 6. from about 0% to about 15% B2O3or B2O3is absent; ii. melting the combined compounds to provide a melted composition; iii. quenching the melted composition, optionally in water, to provide a quenched composition, iv. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; v. milling the dry composition to provide a milled composition; vi. melting the milled composition to provide a melted composition; vii. casting the melted composition in a die or mold to provide a pre-treated glass- ceramic composition; b. exposing the pre-treated glass-ceramic composition to a two-step heat treatment process.
14. The method of claim 12 or claim 13, wherein the pre-treated glass-ceramic composition is in the form of a cast glass monolith.
15. The method of any one of claims 12 to 14, wherein the two-step heat treatment process comprises: a. a first heat treatment step comprising heating the composition to the, or around the, nucleation temperature of the composition; and b. a second, subsequent, heat treatment step comprising heating the composition to the, or around the, crystallization temperature of the composition.
16. The method of any one of claims 12 to 15, wherein the two-step heat treatment process comprises: a. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC for at least about 30 minutes and up to about 5 hours; and b. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC for at least about 30 minutes and up to about 12 hours; wherein the temperature of the second heat treatment step is at least about 50oC higher than the first heat treatment step.
17. The method of any one of claims 12 to 16, wherein post crystallization, the volume fraction of the mica crystal phase in the composition is between 5 and 95% by volume mica.
18. The method of any one of claims 12 to 17, wherein post crystallization, the composition is fully crystallized.
19. The method of any one of claims 12 to 18, wherein the method comprising the steps of a. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of: i. from about 41% to about 49% of SiO2; ii. from about 8% to about 23% of Al2O3; iii. from about 14% to about 16% of BaO; iv. from about 4% to about 8% of MgO; v. from about 5% to about 11% of MgF2; and vi. from about 0% to about 15% B2O3 or B2O3 is absent; b. melting the combined compounds to provide a melted composition; c. quenching the melted composition, optionally in water, to provide a quenched composition, d. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; e. milling the dry composition to provide a milled composition; f. melting the milled composition to provide a melted composition; g. casting the melted composition in a die or mold to provide a glass-ceramic composition.
20. The method of any one of claims 12 to 19, wherein the method comprises: a. providing a pre-treated glass-ceramic composition, wherein the pre-treated glass- ceramic composition has been obtained or is obtainable according to a method comprising the steps of: i. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of:
1. from about 41% to about 49% of SiO2; 2. from about 8% to about 23% of Al2O3; 3. from about 14% to about 16% of BaO; 4. from about 4% to about 8% of MgO; 5. from about 5% to about 11% of MgF2; and 6. from about 0% to about 15% B2O3 or B2O3 is absent; ii. melting the combined compounds to provide a melted composition;iii. quenching the melted composition, optionally in water, to provide a quenched composition, iv. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; v. milling the dry composition to provide a milled composition; vi. melting the milled composition to provide a melted composition; vii. casting the melted composition in a die or mold to provide a pre-treated glass- ceramic composition; b. exposing the pre-treated composition to a two-step heat treatment process comprising: i. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC for at least about 30 minutes and up to about 5 hours; and ii. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC for at least about 30 minutes and up to about 12 hours; wherein the temperature of the second heat treatment step is at least about 50oC higher than the first heat treatment step.
21. The method of any one of claims 12 to 20, wherein the method comprises: a. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of: i. from about 41% to about 49% of SiO2; ii. from about 8% to about 23% of Al2O3; iii. from about 14% to about 16% of BaO; iv. from about 4% to about 8% of MgO; v. from about 5% to about 11% of MgF2; and vi. from about 0% to about 15% B2O3 or B2O3 is absent; b. melting the combined compounds to provide a melted composition; c. quenching the melted composition, optionally in water, to provide a quenched composition, d. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; e. milling the dry composition to provide a milled composition; f. melting the milled composition to provide a melted composition; g. casting the melted composition in a die or mold to provide a pre-treated glass-ceramic composition; h. exposing the pre-treated composition to a two-step heat treatment process comprising:i. a first heat treatment step comprising heating the composition to a temperature of from about 500oC to about 700oC for at least about 30 minutes and up to about 5 hours; and ii. a second, subsequent, heat treatment step comprising heating the composition to a temperature of from about 700oC to about 1200oC for at least about 30 minutes and up to about 12 hours; wherein the temperature of the second heat treatment step is at least about 50oC higher than the first heat treatment step.
22. A method of producing a glass-ceramic composition, comprising, wherein the method comprising the steps of a. combining SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 in the weight % amounts of: i. from about 41% to about 49% of SiO2; ii. from about 8% to about 23% of Al2O3; iii. from about 14% to about 16% of BaO; iv. from about 4% to about 8% of MgO; v. from about 5% to about 11% of MgF2; and vi. from about 0% to about 15% B2O3or B2O3is absent; b. melting the combined compounds to provide a melted composition; c. quenching the melted composition, optionally in water, to provide a quenched composition, d. drying the quenched composition or allowing the quenched composition to dry to provide a dry composition; e. milling the dry composition to provide a milled composition; f. melting the milled composition to provide a melted composition; g. casting the melted composition in a die or mold to provide a glass-ceramic composition.
23. The method of any one of claims 12 to 22, wherein the SiO2, Al2O3, BaO, MgO, MgF2 and optionally B2O3 are provided in powdered form.
24. The method of any one of claims 12 to 23, wherein the SiO2, Al2O3, BaO, MgO, MgF2and optionally B2O3are combined in the weight % amounts of: a. from about 41% to about 48% of SiO2; b. from about 15% to about 17% of Al2O3; c. from about 14% to about 16% of BaO; d. from about 7% to about 8% of MgO;e. from about 9% to about 11% of MgF2; and f. from about 0% to about 15% B2O3or B2O3is absent.
25. The method of any one of claims 12 to 24 wherein the method does not comprise sintering.
26. A glass-ceramic composition obtained or obtainable by a method according to any one of claims 12 to 25.
27. Use of the glass-ceramic composition of any one of claims 1 to 11 and 26 in dentistry or in a dental implant product.
28. A dental implant product comprising or consisting of the glass-ceramic composition of any one of claims 1 to 11 and 26.
29. The dental implant product of claim 28 wherein the dental implant product is a veneer, an inlay, onlay, a bridge, a crown, a post and core, or a construct.
30. The dental implant product of claim 28 or claim 29, wherein the glass-ceramic composition is present as a coating.
31. The dental implant product of any one of claims 28 to 30, wherein the dental implant product consists of or consists essentially of the glass-ceramic composition.
Citation Information
Patent Citations
Glass ceramic material and method for producing the same, and product for dentistry
JP2016113314A
Durable glass-ceramic housings / enclosures for electronic device
US20110092353A1
Mica-spodumene glass-ceramic articles
US3997352A