Melters for glass forming apparatuses

The use of a high electrical resistivity material in the jack arch of glass melters addresses the issue of fire-through, ensuring efficient glass formation by minimizing electrical current through refractory materials and reducing melter damage.

WO2024226239A1PCT designated stage expired Publication Date: 2024-10-31CORNING INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/US2024/022730
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-24
Filing Date
2024-04-03
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Refractory materials in glass melters are susceptible to excessive fire-through at high temperatures when electrodes are used to heat glass batch materials, leading to damage and inefficiency in the glass manufacturing process.

Method used

Incorporating a jack arch made of high electrical resistivity material with a resistivity greater than or equal to 50% of the molten glass's resistivity at melting temperature, reducing electrical current through the jack arch and minimizing fire-through.

Benefits of technology

The high electrical resistivity material in the jack arch reduces fire-through, preventing damage to the melter and ensuring efficient glass formation by directing electrical current through the molten glass rather than the refractory materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure US2024022730_31102024_PF_FP_ABST
    Figure US2024022730_31102024_PF_FP_ABST
Patent Text Reader

Abstract

A melter for forming molten glass includes an inlet wall, an outlet wall, and a pair of sidewalls. The inlet wall, the outlet wall, and the pair of sidewalls define a glass melting space of the melter enclosed by a floor portion and a top. The inlet wall includes a glass contact wall supported on the floor portion and a jack arch positioned over at least a portion of the glass contact wall. The jack arch includes a jack arch electrical path. At least a portion of the jack arch includes a first high electrical resistivity material having a resistivity greater than or equal to 50% of an electrical resistivity of the molten glass, as measured at a melting temperature.
Need to check novelty before this filing date? Find Prior Art

Description

MELTERS FOR GLASS FORMING APPARATUSESCROSS REFERENCE TO RELATED APPLICATION

[0001] This application claims the benefit of priority under 35 U.S. C. §119 of U.S. Provisional Application Serial No. 63 / 497782 filed on April 24, 2023, the content of which is relied upon and incorporated herein by reference in its entirety.Field

[0002] The present specification generally relates to glass manufacturing apparatuses and, more specifically, to melters for forming molten glass and glass manufacturing apparatuses comprising the same.Technical Background

[0003] Optical quality glass sheets are commonly employed in a variety of optical display devices, including LCD displays, LED displays, and the like. Various manufacturing processes may be used to provide the optical quality glass sheets. These manufacturing processes generally involve melting glass batch material in ceramic refractory furnaces (i.e., melters), and then producing a ribbon of glass from the molten glass by drawing the molten glass from a forming body. Individual glass sheets are then cut from the ribbon of glass.

[0004] Refractory materials that form portions of the melters may be susceptible to excessive fire-through at high temperatures when electrodes are used to electrically heat the glass batch materials to form molten glass in the melter, causing damage to the melter.

[0005] Accordingly, a need exists for alternative glass manufacturing apparatuses, and / or components of glass manufacturing apparatuses such as melters, which limit fire-through.SUMMARY

[0006] According to a first aspect Al, a melter for forming molten glass comprises: an inlet wall, an outlet wall positioned opposite the inlet wall, and a pair of sidewalls extending from theinlet wall to the outlet wall, the inlet wall, the outlet wall, and the pair of sidewalls defining a glass melting space of the melter enclosed by a floor portion and a top, the inlet wall comprising: a glass contact wall supported on the floor portion, the glass contact wall comprising a glass contact surface facing the glass melting space and extending vertically away from the floor portion; and a jack arch positioned over at least a portion of the glass contact wall and at least a portion of the glass melting space, the jack arch comprising a jack arch electrical path, the jack arch further comprising a front face facing the glass melting space and extending vertically away from the top towards the floor portion, a back face positioned opposite the front face, and an underside extending horizontally from the front face to the back face, wherein: at least a portion of the jack arch comprises a high electrical resistivity material having a resistivity greater than or equal to 50% of an electrical resistivity of the molten glass, as measured at a melting temperature.

[0007] A second aspect A2 includes the melter of the first aspect Al, wherein the melter further comprises a plurality of electrodes extending through at least one of the sidewalls and the floor portion, and wherein an amount of electrical power flowing through the jack arch electrical path is greater than or equal to 1% and less than or equal to 25% of the electrical power generated by the plurality of electrodes.

[0008] A third aspect A3 includes the melter of the first aspect Al or the second aspect A2, wherein the high electrical resistivity material comprises aluminum, zirconium, or a combination thereof.

[0009] A fourth aspect A4 includes the melter of any one of the first to third aspects Al to A3, wherein another portion of the jack arch comprises a low electrical resistivity material having a resistivity less than 50% of the electrical resistivity of the glass batch material, as measured at the melting temperature.

[0010] A fifth aspect A5 includes the melter of the fourth aspect A4, wherein the low electrical resistivity material comprises aluminum, chromium, zirconium, or a combination thereof.

[0011] A sixth aspect A6 includes the melter of any one of the first to fifth aspects Al to A5, wherein the jack arch comprises skew blocks and wedge blocks; the skew blocks are at leastpartially supported on the sidewalls; and the wedge blocks are positioned between the skew blocks such that the jack arch extends across at least a portion of a width direction of the inlet wall.

[0012] A seventh aspect A7 includes the melter of the sixth aspect A6, wherein at least one of the skew blocks comprises the high electrical resistivity material.

[0013] An eighth aspect A8 includes the melter of the sixth aspect A6 or the seventh aspect A7, wherein at least one of the wedge blocks comprises the high electrical resistivity material.

[0014] A ninth aspect A9 includes the melter of any one of the sixth to eighth aspects A6 to A8, wherein, the jack arch further comprises support bricks and the skew blocks are supported on the support bricks.

[0015] A tenth aspect A10 includes the melter of the ninth aspect A9, wherein at least one of the support bricks comprises the high electrical resistivity material.

[0016] An eleventh aspect Al 1 includes the melter of any one of the sixth to tenth aspects A6 to A10, wherein the jack arch further comprises flat blocks and the flat blocks are positioned adjacent to the skew blocks and extend across the width direction of the inlet wall.

[0017] A twelfth aspect Al 2 includes the melter of the eleventh aspect Al l, wherein at least one of the wedge blocks and at least one of the flat blocks adjacent to the at least one of the wedge blocks comprise the high electrical resistivity material.

[0018] A thirteenth aspect Al 3 includes the melter of any one of the sixth to twelfth aspects A6 to A12, wherein the jack arch further comprises refractory pins positioned at least one of between adjacent wedge blocks or between one of the wedge blocks and one of the skew blocks adjacent to the one of the wedge blocks.

[0019] A fourteenth aspect Al 4 includes the melter of any one of the first to thirteenth aspects Al to Al 3, wherein the glass contact wall comprises the high electrical resistivity material.

[0020] A fifteenth aspect Al 5 includes the melter of any one of the first to fourteenth aspects Al to Al 4, wherein the inlet wall further comprises an inlet wall refractory supported on the jack arch.

[0021] A sixteenth aspect Al 6 includes the melter of the fifteenth aspect Al 5, wherein the inlet wall refractory comprises the high electrical resistivity material.

[0022] A seventeenth aspect Al 7 includes the melter of the sixteenth aspect Al 6, wherein at least one of the glass contact wall or the inlet wall refractory is formed from the same high electrical resistivity material as the portion of the jack arch formed from the high electrical resistivity material.

[0023] An eighteenth aspect Al 8 includes the melter of any one of the fifteenth to seventeenth aspects Al 5 to Al 9, wherein the jack arch further comprises mortar between the inlet wall refractory and the jack arch.

[0024] A nineteenth aspect Al 9 includes the melter of the eighteenth aspect Al 8, wherein the mortar comprises the high electrical resistivity material.

[0025] A twentieth aspect A20 includes the melter of the eighteenth aspect Al 8 or the nineteenth aspect Al 9, wherein the mortar comprises mullite, alumina, or a combination thereof.

[0026] Additional features and advantages of the embodiments described herein will be set forth in the detailed description which follows, and in part will be readily apparent to those skilled in the art from that description or recognized by practicing the embodiments described herein, including the detailed description which follows, the claims, as well as the appended drawings.

[0027] It is to be understood that both the foregoing general description and the following detailed description describe various embodiments and are intended to provide an overview or framework for understanding the nature and character of the claimed subject matter. The accompanying drawings are included to provide a further understanding of the various embodiments, and are incorporated into and constitute a part of this specification. The drawings illustrate the various embodiments described herein, and together with the description serve to explain the principles and operations of the claimed subject matter.BRIEF DESCRIPTION OF THE DRAWINGS

[0028] FIG. 1 schematically depicts a glass manufacturing apparatus, according to one or more embodiments shown and described herein;

[0029] FIG. 2 schematically depicts an isometric rear view of a melter for a glass manufacturing apparatus, according to one or more embodiments shown and described herein;

[0030] FIG. 3 schematically depicts an isometric front view of a melter for a glass manufacturing apparatus, according to one or more embodiments shown and described herein;

[0031] FIG. 4 schematically depicts a cross-section of the melter in the length direction of the melter;

[0032] Fig. 5 schematically depicts the inlet wall of the melter of FIGS. 2-4 without the exoskeleton; and

[0033] FIG. 6 schematically depicts a cross-section of the inlet wall of FIG. 5.DETAILED DESCRIPTION

[0034] Reference will now be made in detail to various embodiments of melters for glass forming apparatuses that reduce fire-through. According to embodiments, a melter for forming molten glass comprises an inlet wall, an outlet wall positioned opposite the inlet wall, and a pair of sidewalls extending from the inlet wall to the outlet wall. The inlet wall, the outlet wall, and the pair of sidewalls define a glass melting space of the melter enclosed by a floor portion and a top. The inlet wall comprises a glass contact wall and a jack arch. The glass contact wall is supported on the floor portion. The glass contact wall comprises a glass contact surface facing the glass melting space and extending vertically away from the floor portion. The jack arch is positioned over at least a portion of the glass contact wall and at least a portion of the glass melting space. The jack arch comprises a jack arch electrical path. The jack arch further comprises a front face facing the glass melting space and extending vertically away from the top towards the floor portion, a back face positioned opposite the front face, and an underside extending horizontally from the front face to the back face. At least a portion of the jack arch comprises a high electrical resistivity material having a resistivity greater than or equal to 50% of an electrical resistivity ofthe molten glass within the melter as measured at a melting temperature. Various embodiments of melters for glass forming apparatuses will be described herein with specific reference to the appended drawings.

[0035] Ranges may be expressed herein as from “about” one particular value, and / or to “about” another particular value. When such a range is expressed, another embodiment includes from the one particular value and / or to the other particular value. Similarly, when values are expressed as approximations, by use of the antecedent “about,” it will be understood that the particular value forms another embodiment. It will be further understood that the endpoints of each of the ranges are significant both in relation to the other endpoint, and independently of the other endpoint.

[0036] Directional terms as used herein - for example up, down, right, left, front, back, top, bottom - are made only with reference to the figures as drawn and are not intended to imply absolute orientation.

[0037] Unless otherwise expressly stated, it is in no way intended that any method set forth herein be construed as requiring that its steps be performed in a specific order, nor that with any apparatus specific orientations be required. Accordingly, where a method claim does not actually recite an order to be followed by its steps, or that any apparatus claim does not actually recite an order or orientation to individual components, or it is not otherwise specifically stated in the claims or description that the steps are to be limited to a specific order, or that a specific order or orientation to components of an apparatus is not recited, it is in no way intended that an order or orientation be inferred, in any respect. This holds for any possible non-express basis for interpretation, including: matters of logic with respect to arrangement of steps, operational flow, order of components, or orientation of components; plain meaning derived from grammatical organization or punctuation, and; the number or type of embodiments described in the specification.

[0038] As used herein, the singular forms “a,” “an” and “the” include plural referents unless the context clearly dictates otherwise. Thus, for example, reference to “a” component includes aspects having two or more such components, unless the context clearly indicates otherwise.

[0039] The term “fire-through,” as used herein, refers to an electrical current extending through an alternative (e.g., parallel) and undesirable electrical path than the intended electrical path. For example, an intended electrical path exists between ones or multiples of electrodes immersed in the molten glass, the intended electrical path further extending through the molten glass and configured to heat the molten glass by Joule heating. On the other hand, an undesired electrical path may also exist through refractory material comprising the melter itself, for example walls of the melter, such that electrical power otherwise intended to heat the molten glass is instead dissipated in the refractory walls of the melter, thereby directly heating the melter walls. Thus, at a least a portion of the electrical current provided to the electrodes “fires” through the refractory walls.

[0040] The term “electrical power,” as used herein, refers to the rate at which electrical energy is transferred by an electric circuit or an electrical path as measured from a power supply, transformer, or any other power system. Electrical power is measured in Watts.

[0041] The term “electrical path,” as used herein, refers to a path along which electrical energy may be transferred.

[0042] The terms “resistivity” or “electrical resistivity,” as used herein, refer to a material’s ability to resist electric current as measured according to ASTM D257.

[0043] The term “high electrical resitivity material,” as used herein, refers to a material having a resitivity greater than or equal to 50% of an electrical resistivity of the molten glass within the melter, as measured at a melting temperature.

[0044] The term “low electrical resitivity material,” as used herein, refers to a material having a resistivity less than the resistivity of the high resistivity material, e.g., 50% of the electrical resistivity of the molten glass within the melter, as measured at the melting temperature.

[0045] The term “melting temperature,” as used herein, refers to the operating temperature of the melter.

[0046] The term “operating temperature,” as used herein, refers to a steady state temperature the melter is operated at during a melting process, unless otherwise noted.

[0047] The term “jack arch,” as used herein, refers to a flat or low-curvature arch used to support weight at and around openings in an inlet wall of a melter.

[0048] Glass articles may generally be formed by melting glass batch material to form molten glass and forming the molten glass into a final glass article such as a glass ribbon or glass sheets. Exemplary processes for forming glass ribbons include the float glass process, the slot draw process, and the fusion downdraw process.

[0049] Referring to FIG. 1 , an exemplary glass manufacturing apparatus 100 for forming glass ribbons from molten glass using a fusion draw machine is schematically depicted. The glass manufacturing apparatus 100 includes a melter 101, a fining vessel 103, a mixing vessel 104, a delivery vessel 108, and a fusion draw machine (FDM) 120. Glass batch material is introduced into the melter 101 though a batch material inlet port 102. The batch material is melted in the melter to form molten glass 106. The fining vessel 103 comprises a high temperature processing area that receives the molten glass 106 from the melter 101 and in which dissolved gases and / or bubbles are removed from the molten glass 106. The fining vessel 103 is fluidly coupled to the mixing vessel 104 by a connecting tube 105. That is, molten glass flowing from the fining vessel 103 to the mixing vessel 104 flows through the connecting tube 105. The mixing vessel 104 is, in turn, fluidly coupled to the delivery vessel 108 by connecting tube 107 such that molten glass flowing from the mixing vessel to the delivery vessel 108 flows through the connecting tube 107.

[0050] The delivery vessel 108 supplies the molten glass 106 through a downcomer 109 into the FDM 120. The FDM 120 comprises an enclosure 122 in which an inlet 110 and a forming vessel111 are positioned. As shown in FIG. 1, the molten glass 106 from the downcomer 109 flows into the inlet 110 which leads to the forming vessel 111. The forming vessel 111 includes an opening112 that receives the molten glass 106, which flows into a trough 113 and then overflows and runs down two converging sides 114a and 114b before fusing together at a bottom edge (root) of the forming vessel, where the two converging sides join, before being contacted and drawn in a downstream direction 121 to form a glass ribbon 148.

[0051] While FIG. 1 schematically depicts a glass manufacturing apparatus 100 for forming glass ribbon using a FDM, it should be understood that other processes may be used to form the glass ribbon, including, without limitation, the float glass process, the slot draw process, or thelike. Further, while the glass manufacturing apparatus 100 is depicted as being used for forming glass ribbon, it should be understood that similar glass manufacturing apparatuses may be used for forming glass articles other than glass sheets including, without limitation, glass tubes and the like.

[0052] Melter 101 may be designed to include a jack arch, which supports the weight of refractory material positioned over openings, e.g., feed ports, in a refractory wall of the melter, as described in U.S. Patent No. 11,492,281 B2, which is incorporated by reference herein in its entirety. Refractory materials that form the jack arch may be susceptible to excessive fire-through at high temperatures when electrodes (e.g., molybdenum- type electrodes) are used to electrically heat the glass batch materials to form molten glass in the melter 101. As the jack arch refractory material heats up to operational conditions (e.g., greater than or equal to 1200 °C and less than or equal to 1800 °C), the electrical resistivity of the jack arch refractory material may decrease and may approach or become lower than the electrical resistivity of the molten glass in the melter. Accordingly, the electrodes may cause current to “fire-through” the jack arch, instead of or in addition to the molten glass, at a magnitude that may cause damage to the jack arch and the melter 101 as a whole.

[0053] Disclosed herein are melters for glass forming apparatuses which mitigate the aforementioned problems such that fire-through is limited. Specifically, melters described herein include a jack arch comprising a high electrical resistivity material having a resistivity greater than or equal to 50% of an electrical resistivity of the molten glass, as measured at a melting temperature. The high electrical resistivity material reduces the electrical current through the jack arch electrical path, thereby reducing the magnitude of fire-through and preventing damage to the melter.

[0054] Referring back to FIG. 1 and now to FIGS. 2-4, a melter 101 for use in a glass manufacturing apparatus is schematically depicted from the rear (FIG. 2), from the front (FIG. 3), and in X-Y cross-section (FIG. 4). The melter 101 comprises an exoskeleton 130 and a base portion 170. The exoskeleton 130 generally defines an exoskeleton interior volume 132. The melter 101 comprises a tank assembly 200, which is supported on the base portion 170 in the exoskeleton interior volume 132. In embodiments, the tank assembly may be positioned on the base portion 170 and spaced apart from the exoskeleton 130. The tank assembly 200 of the melter101 includes an inlet wall 218 (FIG. 2) comprising a plurality of batch material inlet ports 102 through which glass batch material may be introduced into the interior of the tank assembly 200 for melting. The tank assembly 200 also comprises an outlet wall 220 opposite the inlet wall 218 in the length direction of the melter 101 (i.e., the + / - Y direction of the coordinate axes depicted in the figures). The outlet wall 220 includes an outlet port 223 through which molten glass flows from the tank assembly 200 of the melter 101. The tank assembly 200 of the melter 101 further comprises a pair of sidewalls 241, 242 (sidewall 241 is depicted in each of FIGS. 2 and 3; sidewalls 241, 242 are depicted in the cross-section of the tank assembly schematically depicted in FIG. 4), which are opposed to one another in a width direction (i.e., the + / - X direction of the coordinate axes depicted in FIGS. 2 and 3) of the melter 101. The pair of sidewalls 241, 242 connect the inlet wall 218 and the outlet wall 220. In embodiments, the melter 101 may include a plurality of burners 402 (e.g., combustion burners) arrayed in the length direction of the melter 101. The burners 402 may be located in or on the sidewalls 241, 241 of the tank assembly 200. As noted herein, the burners 402 facilitate melting the batch material in the melter 101 and also assist in maintaining the temperature of the molten glass within the melter 101.

[0055] In addition to the inlet wall 218, outlet wall 220, and sidewalls 241, 242, the tank assembly 200 of the melter 101 further includes a top 206 (also referred to as a “crown”) and a floor portion 207 (FIG. 4), which connect the inlet wall 218, outlet wall 220, and the sidewalls 241, 242. The inlet wall 218, the outlet wall 220, the sidewalls 241, 242, and the floor portion 207 enclose a glass melting space 250 of the tank assembly 200 of the melter 101. In embodiments, each of the inlet wall 218, the outlet wall 220, and the sidewalls 241, 242, and the floor portion 207 may be constructed from refractory materials, such as bricks and blocks formed from ceramic refractories. The term “refractory materials,” as used herein, refers to materials that are able to withstand the high temperatures of a glass manufacturing (i.e., melting) process with minimal degradation. Refractory materials, specifically refractory blocks used to construct the melter 101, are generally ceramic materials such as alumina, zirconia, and the like, but other refractory materials are contemplated and possible, including, without limitation, refractory metals and refractory metal alloys. The materials used to form portions of the inlet wall 218 will be described in further detail herein.

[0056] Still referring to FIGS. 1-4, the exoskeleton 130 (FIG. 1) of the melter 101 is coupled to the tank assembly 200 with, for example, pressure bolts. In embodiments, the pressure bolts may be spring-loaded pressure bolts that allow for the expansion and contraction of the refractory blocks. In embodiments, the pressure bolts may be positioned in support members which, in turn, are rigidly affixed to the exoskeleton 130. Alternatively, the pressure bolts may be affixed to (and extend through) portions of the exoskeleton 130.

[0057] Referring now to FIGS. 5 and 6, the inlet wall 218 of the tank assembly 200 of FIGS. 2- 4 is schematically depicted without the exoskeleton. The inlet wall 218 generally comprises a glass contact portion 204 and a superstructure 202. The glass contact portion 204 is the lower part of the tank assembly 200 where glass batch material is heated and turned into molten glass. That is, the glass contact portion 204 is the portion of the tank assembly 200 that comes into contact with molten glass disposed in the glass melting space 250 of the tank assembly 200 of the melter 101. The superstructure 202 is positioned over the glass contact portion 204 (and the glass contact wall 260 of the glass contact portion 204) and, in embodiments, may be at least partially supported on the glass contact wall 260. The superstructure 202, in turn, supports the top 206 of the tank assembly 200 of the melter 101. In embodiments, the batch material inlet ports 102 for receiving glass batch material to be melted in the tank assembly 200 of the melter 101 are positioned in the superstructure 202 of the inlet wall 218.

[0058] In embodiments, the glass contact portion 204 of the inlet wall 218 comprises a glass contact wall 260 supported on the floor portion 207. The glass contact wall 260 may be constructed from stacked refractory blocks 213. The refractory blocks 213 of the glass contact wall 260 are supported on the floor portion 207. In embodiments, the refractory blocks 213 of the glass contact wall 260 may be urged into contact with one another with pressure bolts attached to the exoskeleton.

[0059] In embodiments, the glass contact wall 260 may include a glass contact surface 261 that faces the glass melting space 250 of the tank assembly 200 and extends vertically away from the floor portion 207. In embodiments, at least a portion of the glass contact surface 261 of the glass contact wall 260 is inclined away from the glass melting space 250. For example, in embodiments, the glass contact wall 260 comprises a base portion 262 supported on the floor portion 207 and anupper portion 263 supported on the base portion 262, as depicted in FIG. 6. In these embodiments, the glass contact surface 261 of the base portion 262 is substantially vertical and the upper portion 263 tapers from the base portion 262 to a top of the glass contact wall 260 such that the glass contact surface 261 is angled (relative to vertical) outward in a direction away from the glass melting space 250. In other embodiments (not shown), the entire glass contact surface 261 may be oriented at an inclined angle with respect to vertical. In some embodiments (not shown), the entire glass contact surface 261 may be substantially vertical. As shown in FIG. 6, the base portion 262 may utilize a different block than the upper portion 263. In other embodiments, the base portion 262 and the upper portion 263 may be formed from a single block.

[0060] Referring again to FIGS. 5 and 6, the superstructure 202 of the inlet wall 218 comprises at least one batch material inlet port 102 that extends through refractory blocks 270, and may, in embodiments, comprise a plurality of batch inlet ports. As described hereinabove, the at least one batch material inlet port 102 provides a path for introducing batch material into the glass melting space 250 of the tank assembly 200 of the melter 101. Optionally, the inlet wall 218 may contain at least two batch inlet ports, for example, at least three or more batch material inlet ports 102, as depicted in FIG. 5. These batch material inlet ports 102 may be equidistantly spaced from each other in the width direction of the inlet wall 218.

[0061] Still referring to FIGS. 5 and 6, the superstructure 202 of the inlet wall 218 further comprises a jack arch 280 positioned over at least a portion of the glass contact wall 260 and at least a portion of the glass melting space 250. The jack arch 280 supports the weight of the inlet wall 218 at and above the batch material inlet ports 102, such as inlet wall refractory 290, and may further support at least a portion of the top 206 of the melter 101.

[0062] The jack arch 280 comprises a front face 284 facing the glass melting space 250 and extending vertically away from the top 206 towards the floor portion 207, a back face 283 positioned opposite the front face 284, and an underside 285 extending horizontally (i.e., extending laterally in a horizontal direction) from the front face 284 to the back face 283.

[0063] As shown in FIG. 5, the jack arch 280 may be a flat arch such that the top edge 280a and the bottom edge 280b of the flat arch are substantially flat and / or horizontal. In other embodiments, the jack arch may be a low-curvature arch such that the top edge is flat and thebottom edge is curved. In such embodiments, a rise of a curve of the bottom edge may be greater than 0 cm and less than or equal 25 cm per meter span (e.g., if the jack arch is 5 m wide, the bottom edge of the jack arch may vary between 0 cm and 62.5 cm, starting at an elevation of 0 cm, rising up to an elevation of between 0 cm and 62.5 cm in the center of the jack arch (i.e., at 2.5 m), and then go back down to an elevation of 0 cm on the other side of the jack arch).

[0064] The jack arch 280 may be comprised of refractory blocks. In embodiments, the jack arch280 may comprise skew blocks 281 and wedge blocks 282. Both the skew blocks 281 and wedge blocks 282 are voussoirs, or wedge-shaped or tapered blocks used to construct the jack arch 280.

[0065] The skew blocks 281 are springers, or the lowest voussoir on each side of the jack arch 280. The skew blocks 281 are the bottom-most element of the jack arch 280. The skew blocks281 are at least partially supported by the sidewalls 241, 242 (FIGS. 2-4) of the tank assembly 200 of the melter 101 and partially supported by the exoskeleton 130 of the melter such that the lateral load of the jack arch is transferred to the exoskeleton 130.

[0066] A plurality of wedge blocks 282 are positioned between the skew blocks 281 such that the jack arch 280 extends across at least a portion of the width direction of the inlet wall 218. The wedge blocks 282 are formed with angled mating faces such that, when the wedge blocks 282 are assembled, the angled mating faces of adjacent blocks prevent vertical displacement of one another. The plurality of wedge blocks 282 includes a keystone 282a, which locks the other wedge blocks 282 in place and prevents the jack arch 280 from collapsing. When the wedge blocks 282 are assembled such that the mating faces are in contact with one another, the weight of the wedge blocks 282 (and hence the weight of the jack arch 280, and any other load supported by the jack arch 280) is transferred laterally (i.e., in the width direction of the inlet wall 218) to the skew blocks 281 and, in turn, to the exoskeleton 130 of the melter 101.

[0067] In embodiments, the jack arch 280 may further comprise support bricks 286. The support bricks 286 are imposts, or blocks serving as the base for the skew blocks 281. The support bricks 286 may help transfer the lateral load of the jack arch 280 to the exoskeleton 130.

[0068] In embodiments, the jack arch 280 may further comprise flat blocks 287. Without flat blocks 287, the jack arch 280 may interfere with the portion of the inlet wall 218 above the jackarch (e.g., inlet wall refractory 290) during expansion. The flat blocks 287 provide a surface on which the remainder of the inlet wall 218 may be built and minimize the amount of disruption of the remainder of the inlet wall 218 by the jack arch 280 during expansion. The flat blocks 287 may be positioned adjacent to the skew blocks 281 and extend across the width direction of the inlet wall 218. The flat blocks 287 may be square or rectangular in shape, having four sides, four corners, and four substantially right angles. A lateral dimension (e.g., in the -x - +x direction) of the flat blocks 287 may be greater than a lateral dimension of any one of the skew or wedge blocks 281, 282.

[0069] In embodiments, the jack arch 280 may further comprise refractory pins 288 positioned at least one of between adjacent wedge blocks 282 and between one of the wedge blocks 282 and one of the skew blocks 281 adjacent to the one of the wedge blocks 282. The refractory pins 288 may have a circular or cylindrical structure and may help to lock the skew blocks 281 and wedge blocks 282 together and prevent sliding during thermal expansion of the blocks. For example, adjacent blocks, when assembled, may define a passage configured to receive a refractory pin 288. The refractory pin is inserted into the passage, which prevents relative motion between the adjacent blocks. The refractory pins 288 may be mortared in place.

[0070] Still referring to FIGS. 5 and 6, the superstructure 202 of the inlet wall 218 may further comprise an inlet wall refractory 290, for example comprising refractory bricks or blocks, supported on the jack arch 280. The inlet wall refractory 290 helps to support the top 206 of the tank assembly of the melter 101.

[0071] As described above, the tank assembly 200 is utilized to heat glass batch material and thereby form molten glass in the glass contact portion 204 of the tank assembly 200. In embodiments, the operating temperature of the melter 101 may be greater than or equal to 1200 °C and less than or equal to 1800 °C, greater than or equal to 1200 °C and less than or equal to 1700 °C, greater than or equal to 1300 °C and less than or equal to 1800 °C, greater than or equal to 1300 °C and less than or equal to 1700 °C, greater than or equal to 1400 °C and less than or equal to 1800 °C, greater than or equal to 1400 °C and less than or equal to 1700 °C, greater than or equal to 1500 °C and less than or equal to 1800 °C, or even greater than or equal to 1500 °C and less than or equal to 1700 °C, or any and all subranges formed from any of these endpoints.Various techniques may be utilized to heat the tank assembly 200. For example, in the embodiment of the tank assembly 200 depicted in FIGS. 2-4, the tank assembly 200 may be electrically heated. Referring again to FIGS. 5 and 6, the melter 101 comprises a plurality of electrodes 292 extending through at least one of the sidewalls 241, 241 (not shown) and the floor portion 207. The electrodes 292 deliver electrical energy to the molten glass and / or glass batch material contained within the melter 101. Various configurations of electrodes 214 may be utilized to heat the glass contact portion 204 of the melter 101. Moreover, as noted above, a plurality of burners 402 may be positioned in the sidewalls 241, 242 of the tank assembly 200 to supplement the heating provided by the electrodes.

[0072] In embodiments, electrodes 292 may be comprise molybdenum, while in other embodiments the electrodes may comprise tin oxide (SnCh) or platinum alloys. In embodiments, the platinum alloys may comprise rhodium, iridium, oxide dispersed strengthened (ODS) alloy, graphite, or a combination thereof. In some embodiments, the electrodes 292 may extend from the floor portion 207. In some embodiments, the electrodes 292 may extend from the sidewalls 241, 242.

[0073] Electrical power generated by the electrodes 292 may transfer along a jack arch electrical path (shown as dashed line 294) that extends through at least a portion of the jack arch 280. As described hereinabove, conventional refractory materials that form the jack arch may be susceptible to higher levels of fire-through at high temperatures when electrodes are used to electrically heat the glass batch materials to form molten glass in the melter. That is, at higher temperatures (e.g., operating temperatures), the electrical resistance of the refractory materials comprising the jack arch 280 may be sufficiently lowered that a significant current may be established in the jack arch 280, e.g., an electrical current sufficient to cause a breakdown of the refractory material. Over time, this breakdown may lead to deterioration of the refractory material. Accordingly, to mitigate this problem, at least a portion of the jack arch 280 described herein may comprise a high electrical resistivity material having a resistivity greater than or equal to 50% of an electrical resistivity of the molten glass contained in the glass melting space 250, as measured at a melting temperature. The high electrical resistivity material reduces the electrical current through the jack arch 280, thereby shunting the electrical current to a lower resistance electricalpath (e.g., through the molten glass contained in the glass melting space 250). Accordingly, the electrical power flowing through the jack arch electrical path 294 is reduced.

[0074] For example, in embodiments, the amount of electrical power flowing through the jack arch electrical path 294 of the jack arch 280 including the high electrical resistivity material may be greater than or equal to 1% and less than or equal to 25% of the electrical power generated by the plurality of electrodes 292. In embodiments, the amount of electrical power flowing through the jack arch electrical path 294 of the jack arch 280 including the high electrical resistivity material may be greater than or equal to 1% or even greater than or equal to 2% of the electrical power generated by the plurality of electrodes 292. In embodiments, the amount of electrical power flowing through the jack arch electrical path 294 of the jack arch 280 including the high electrical resistivity material may be less than or equal to 25%, less than or equal to 20%, less than or equal to 15%, less than or equal to 10%, or even less than or equal to 5% of the electrical power generated by the plurality of electrodes 292. In embodiments, the amount of electrical power flowing through the jack arch electrical path 294 of the jack arch 280 including the high electrical resistivity material, may be greater than or equal to 1% and less than or equal to 25%, greater than or equal to 1% and less than or equal to 20%, greater than or equal to 1% and less than or equal to 15%, greater than or equal to 1% and less than or equal to 10%, greater than or equal to 1% and less than or equal to 5%, greater than or equal to 2% and less than or equal to 25%, greater than or equal to 2% and less than or equal to 20%, greater than or equal to 2% and less than or equal to 15%, greater than or equal to 2% and less than or equal to 10%, or even greater than or equal to 2% and less than or equal to 5%, or any and all subranges formed from any of these endpoints, of the electrical power generated by the plurality of electrodes 292.

[0075] In embodiments, the amount of electrical power generated by the plurality of electrodes 292 may be greater than or equal to 100 kW and less than or equal to 10 MW, greater than or equal to 100 kW and less than or equal to 5 MW, greater than or equal to 100 kW and less than or equal to 1 MW, greater than or equal to 250 kW and less than or equal to 10 MW, greater than or equal to 250 kW and less than or equal to 5 MW, greater than or equal to 250 kW and less than or equal to 1 MW, greater than or equal to 500 kW and less than or equal to 10 MW, greater than or equal to 500 kW and less than or equal to 5 MW, or even greater than or equal to 500 kW and less than or equal to 1 MW, or any and all subranges formed from any of these endpoints.

[0076] In embodiments, the high electrical resitivity material may have a resistivity greater than or equal to 50%, greater than or equal to 60%, greater than or equal to 70%, greater than or equal to 80%, or even greater than or equal to 90% of an electrical resistivity of the molten glass contained in the glass melting space 250, as measured at the melting temperature.

[0077] In embodiments, the high electrical resistivity material may have a resistivity greater than or equal to 20 ohm cm, greater than or equal to 30 ohm cm, greater than or equal to 40 ohm cm, or even greater than or equal to 50 ohm cm, as measured at 1600 °C.

[0078] In embodiments, the high electrical resistivity material may be a refractory material comprising aluminum, zirconium, or a combination thereof. For example, a high electrical resistivity material comprising aluminum may comprise alumina, alumina zirconia silica (AZS), mullite, or a combination thereof. A high electrical resistivity material comprising zirconium may comprise zirconia.

[0079] As described hereinabove, at least a portion of the jack arch 280 comprises the high electrical resistivity material. In embodiments, the entire jack arch 280 may comprise the high electrical resistivity material. In embodiments, it may be desirable to reduce costs, which may be achieved by limiting the amount of high electrical resistivity material used. While low electrical resistivity material may not help minimize the level of fire-through, the use of low electrical resistivity material with high electrical resistivity material may be a cost effective solution of reducing the level of fire-through. Accordingly, in embodiments, another portion of the jack arch 280 may comprise a low electrical resistivity material having a resistivity less than a resistivity of the high resistivity refractory material, e.g., less than 50% of the electrical resistivity of the molten glass in the glass melting space 250, as measured at the melting temperature. In embodiments, the low electrical resistivity material may have a resistivity less than 50%, less than or equal to 40%, less than or equal to 30%, or even less than or equal to 20% of the electrical resistivity of the molten glass, as measured at the melting temperature.

[0080] In embodiments, the low electrical resistivity material may have a resistivity less than 20 ohm- cm, less than or equal to 15 ohm cm, less than or equal to 10 ohm- cm, or even less than or equal to 5 ohm cm, as measured at 1600 °C.

[0081] In embodiments, the low electrical resistivity material may be a refractory material comprising aluminum (e.g., alumina), chromium, zirconium (e.g., zirconia), or a combination thereof.

[0082] Referring back to FIGS. 5 and 6, any portion of the jack arch 280 may be formed from the high electrical resistivity material and any combination of the high electrical resistivity material and the low electrical resitivity material may be used as long as electrical current (e.g., electrical power) through the jack arch electrical path 294 is reduced. For example, in embodiments, at least one of the skew blocks 281 may comprise the high electrical resistivity material. In embodiments, both of the skew blocks 281 may comprise the high electrical resistivity material. In embodiments, at least one of the wedge blocks 282 may comprise the high electrical resistivity material. In embodiments, at least two, at least three, at least four, or even at least five of the wedge blocks 282 may comprise the high electrical resistivity material. In embodiments, the wedge blocks 282 may alternate between being comprised of a high electrical resistivity material and a low electrical resitivity material. In embodiments, at least two adjacent wedge blocks 282 may comprise the high electrical resistivity material. In embodiments, at least one of the support bricks 286 may comprise the high electrical resistivity material. In embodiments, both of the support bricks 286 may comprise the high electrical resistivity material. In embodiments, at least one of the wedge blocks 282 and at least one of the flat blocks 287 adjacent to the at least one of the wedge blocks 282 may comprise the high electrical resistivity material. For example, flat block 287a and the keystone 282a may comprise the high electrical resistivity material.

[0083] Because the glass contact wall 260, the jack arch 280, and the inlet wall refractory 290 are adjacent (e.g., contacting), the resistivity of one of these components may affect the overall electrical resistivity of the inlet wall 218. In embodiments, the glass contact wall 260 may comprise the high electrical resistivity material. In embodiments, the inlet wall refractory 290 may comprise the high electrical resistivity material. In embodiments, at least one of the glass contact wall 260 and the inlet wall refractory 290 may be formed from the same high electrical resistivity material as the portion of the jack arch 280 formed from the high electrical resistivity material.

[0084] In embodiments, the jack arch 280 may further comprise a mortar 298 disposed between the inlet wall refractory 290 and the jack arch 280 to lock the structures together and preventslipping during thermal expansion of the refractory material (e.g., during an initial heat up of the melter). In embodiments, the jack arch 280 may further comprise mortar (not shown) disposed between the skew blocks 281, wedge blocks 282, and / or flat blocks 287 of the jack arch 280. In embodiments, the mortar 298 may comprise the high electrical resistivity material. For example, in embodiments, the mortar may comprise mullite, alumina, or a combination thereof.

[0085] Referring again to FIGS. 2-4, the outlet wall 220 and the sidewalls 241, 242 may have a similar construction as the inlet wall 218 with the exception of the jack arch. That is, each of the outlet wall 220 and the sidewalls 241, 242 may be constructed from blocks of refractory material and each may comprise a glass contact portion and a superstructure over the glass contact portion, as described above with respect to the inlet wall 218. In embodiments, the superstructure of each of the outlet wall 220 and the sidewalls 241, 242 comprises courses of refractory blocks without a jack arch, as depicted in FIG. 4. For example, a sidewall 242 in FIG. 4 may include a glass contact portion comprising a glass contact wall, as described herein above with respect to the inlet wall 218. The superstructure of the sidewall 242 may include several courses of refractory blocks. The refractory blocks may be supported on or over the glass contact wall, as described herein with respect to FIGS. 4 and 5. Each of the outlet wall 220 and the sidewall 241 may be similarly constructed.

[0086] Referring to FIGS. 2-3, the top 206 of the tank assembly 200 may likewise be constructed from refractory blocks. To form the top 206, the refractory blocks may be arranged to form a barrel vault over the glass melting space 250 (FIG. 4) of the tank assembly 200 of the melter 101 using traditional masonry techniques for forming arches and / or vaults.

[0087] It should now be understood that the melters for glass forming apparatuses described herein may limit fire-through. The reduction in fire-through is due to the jack arch comprising a high electrical resistivity material having a resistivity greater than or equal to 50% of an electrical resistivity of the molten glass contained in the glass melting space 250, as measured at a melting temperature.

[0088] It will be apparent to those skilled in the art that various modifications and variations may be made to the embodiments described herein without departing from the spirit and scope of the claimed subject matter. Thus, it is intended that the specification cover the modifications andvariations of the various embodiments described herein provided such modification and variations come within the scope of the appended claims and their equivalents.

Claims

CLAIMSWhat is claimed is:

1. A melter for forming molten glass, the melter comprising: an inlet wall, an outlet wall positioned opposite the inlet wall, and a pair of sidewalls extending from the inlet wall to the outlet wall, the inlet wall, the outlet wall, and the pair of sidewalls defining a glass melting space of the melter enclosed by a floor portion and a top, the inlet wall comprising: a glass contact wall supported on the floor portion, the glass contact wall comprising a glass contact surface facing the glass melting space and extending vertically away from the floor portion; and a jack arch positioned over at least a portion of the glass contact wall and at least a portion of the glass melting space, the jack arch comprising a jack arch electrical path, the jack arch further comprising a front face facing the glass melting space and extending vertically away from the top towards the floor portion, a back face positioned opposite the front face, and an underside extending horizontally from the front face to the back face, wherein: at least a portion of the jack arch comprises a high electrical resistivity material having a resistivity greater than or equal to 50% of an electrical resistivity of the molten glass, as measured at a melting temperature.

2. The melter of claim 1 , wherein the melter further comprises a plurality of electrodes extending through at least one of the sidewalls and the floor portion, and wherein an amount of electrical power flowing through the jack arch electrical path is greater than or equal to 1% and less than or equal to 25% of the electrical power generated by the plurality of electrodes.

3. The melter of claim 1 or claim 2, wherein the high electrical resistivity material comprises aluminum, zirconium, or a combination thereof.

4. The melter of any one of claims 1 to 3, wherein another portion of the jack arch comprises a low electrical resistivity material having a resistivity less than 50% of the electrical resistivity of the glass batch material, as measured at the melting temperature.

5. The melter of claim 4, wherein the low electrical resistivity material comprises aluminum, chromium, zirconium, or a combination thereof.

6. The melter of any one of claim 1 to 5, wherein: the jack arch comprises skew blocks and wedge blocks; the skew blocks are at least partially supported on the sidewalls; and the wedge blocks are positioned between the skew blocks such that the jack arch extends across at least a portion of a width direction of the inlet wall.

7. The melter of claim 6, wherein at least one of the skew blocks comprises the high electrical resistivity material.

8. The melter of claim 6 or claim 7, wherein at least one of the wedge blocks comprises the high electrical resistivity material.

9. The melter of any one of claims 6 to 8, wherein the jack arch further comprises support bricks and the skew blocks are supported on the support bricks.

10. The melter of claim 9, wherein at least one of the support bricks comprises the high electrical resistivity material.

11. The melter of any one of claims 6 to 10, wherein the jack arch further comprises flat blocks and the flat blocks are positioned adjacent to the skew blocks and extend across the width direction of the inlet wall.

12. The melter of claim 11, wherein at least one of the wedge blocks and at least one of the flat blocks adjacent to the at least one of the wedge blocks comprise the high electrical resistivity material.

13. The melter of any one of claims 6 to 12, wherein the jack arch further comprises refractory pins positioned at least one of between adjacent wedge blocks or between one of the wedge blocks and one of the skew blocks adjacent to the one of the wedge blocks.

14. The melter of any one of claims 1 to 13, wherein the glass contact wall comprises the high electrical resistivity material.

15. The melter of any one of claims 1 to 14, wherein the inlet wall further comprises an inlet wall refractory supported on the jack arch.

16. The melter of claim 15, wherein the inlet wall refractory comprises the high electrical resistivity material.

17. The melter of claim 16, wherein at least one of the glass contact wall or the inlet wall refractory is formed from the same high electrical resistivity material as the portion of the jack arch formed from the high electrical resistivity material.

18. The melter of any one of claims 15 to 17, wherein the jack arch further comprises mortar between the inlet wall refractory and the jack arch.

19. The melter of claim 18, wherein the mortar comprises the high electrical resistivity material.

20. The melter of claim 18 or claim 19, wherein the mortar comprises mullite, alumina, or a combination thereof.

Citation Information

Patent Citations

  • Structure for improving melting uniformity of borosilicate glass

    CN102643011A

  • Glass melting tank having a doghouse, and method for heating the charge material in such glass melting tanks

    US20130114638A1

  • Melters for glass forming apparatuses

    US20140116095A1

  • Submerged combustion melter comprising a melt exit structure designed to minimize impact of mechanical energy, and methods of making molten glass

    US20150336834A1

  • Melters for glass forming apparatuses

    WO2019006041A1