Method for improving enzymatic hydrolysis efficiency of lignocellulose
By pretreating lignocellulose by using a type IV eutectic solvent prepared by metal salt and glycerol, the problem of low hydrolysis efficiency of lignocellulase in the prior art was solved, and efficient and environmentally friendly enzymatic hydrolysis effect was achieved. The conversion rate of cellulose and the enzymatic hydrolysis efficiency were significantly improved.
Patent Information
- Application Number
- PCT/CN2024/088996
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-30
- Filing Date
- 2024-04-21
- Publication Date
- 2024-11-07
AI Technical Summary
The prior art is difficult to effectively improve the hydrolysis efficiency of lignocellulase, and there is a lack of a green and environmentally friendly pretreatment solvent system to break the dense structure of biomass and reduce the anti-degradation barrier.
The type IV eutectic solvent system prepared by metal salt and glycerol is pretreated on lignocellulose. Through crushing, extraction, drying, stirring and separation, a stable solvent system is formed, reducing equipment requirements and improving Enzyme hydrolysis efficiency.
It realizes low-cost, green and environmentally friendly lignocellulase hydrolysis, significantly improves the enzyme hydrolysis efficiency, reduces processing time and equipment requirements, enhances cellulose looseness, promotes cellulase contact, and thus improves cellulose conversion rate .
Smart Images

Figure CN2024088996_07112024_PF_FP_ABST
Abstract
Description
A method for improving the efficiency of enzymatic hydrolysis of lignocellulose Technical Field
[0001] The invention belongs to the technical field of preparing lignocellulose, and in particular relates to a method for improving the enzymatic hydrolysis efficiency of lignocellulose. Background Art
[0002] Lignocellulose is primarily composed of cellulose, hemicellulose, and lignin. The efficient saccharification of cellulose is key to producing chemicals and liquid fuels. To achieve efficient lignocellulose conversion, it is necessary to identify efficient and environmentally friendly pretreatment solvent systems that break down the lignocellulose's anti-degradation barrier.
[0003] Pretreatment solvent systems can effectively break down the original compact structure of biomass and reduce the anti-degradation barrier, thereby facilitating the conversion of carbohydrates into fermentable monosaccharides or fuel ethanol. The selection of environmentally friendly, mild, and efficient pretreatment solvents is of great significance for the enzymatic saccharification of lignocellulose.
[0004] Deep eutectic solvents (DES), as a new type of ionic liquid, are formed by a simple physical mixture of hydrogen bond donors and hydrogen bond acceptors. They can effectively remove lignin or hemicellulose, have little effect on cellulose degradation, and can also recycle and reuse the solvent.
[0005] Summary of the Invention
[0006] The technical problem to be solved by the present invention is to provide a method for improving the efficiency of enzymatic hydrolysis of lignocellulose, using a low-cost, green and environmentally friendly low eutectic solvent system to enzymatically hydrolyze lignocellulose. This method has the advantages of low equipment requirements, simple operation, and can effectively improve the efficiency of enzymatic hydrolysis.
[0007] The present invention is achieved by providing a method for improving the efficiency of enzymatic hydrolysis of lignocellulose, comprising the steps of:
[0008] Step 1: crushing the agricultural and forestry biomass raw materials into a particle size of 60-80 mesh, extracting with a toluene-ethanol solution, and drying at a constant temperature to obtain an extract-free raw material;
[0009] Step 2: Weighing a metal salt and glycerol in a molar ratio of 1:10 to 1:124, mixing the mixture at a temperature of 80 to 90° C. and a stirring speed of 180 rpm to obtain a uniform and transparent type IV deep eutectic solvent; wherein the metal salt is any one of aluminum chloride, zinc chloride, and ferric chloride;
[0010] Step 3: Weigh the extract-free raw material prepared in step 1, add it to the type IV deep eutectic solvent prepared in step 2 at a solid-liquid ratio of 1:5 to 1:15, and react at a temperature of 80 to 120° C. and a stirring speed of 300 to 500 rpm for 2 to 4 hours to obtain a pretreated mixture;
[0011] Step 4: performing solid-liquid separation on the pretreated mixture by centrifugation or vacuum filtration to obtain a filter residue and a filtrate, respectively; washing and desalting the filter residue with ethanol or deionized water until no metal salt components are detected in the washing liquid; and then drying the washed filter residue to obtain a lignocellulosic residue after pretreatment of the agricultural and forestry biomass raw materials;
[0012] Step 5: Add the pretreated lignocellulose residue to an acetate buffer solution with a pH of 4.8 at a certain substrate concentration, then add cellulose complex enzyme, and react in an air bath shaker at 45-50° C. and 140-150 r / min for a period of time to obtain fermentable sugar.
[0013] Currently, deep eutectic solvents (DES) are classified into four categories. The solvent system prepared using metal salts and glycerol in the present invention is a Type IV deep eutectic solvent system. Glycerol is a commonly used organic solvent in pretreatment. When used alone, it requires higher temperatures and longer times to effectively remove lignin. This removal effect can be improved in an acidic environment. The Lewis acidity provided by the metal salt can increase the lignin removal rate, effectively degrade hemicellulose, and swell rather than dissolve cellulose. The Type IV deep eutectic solvent system of the present invention is highly stable and easy to prepare, making it a green solvent with greater application prospects.
[0014] Furthermore, in step 1, the agricultural and forestry biomass is bamboo.
[0015] Furthermore, in step 4, the drying condition of the washed filter residue is drying at 80° C. to constant weight.
[0016] Furthermore, in step 5, the substrate concentration of the lignocellulose residue is 2-10 wt%, and the cellulose complex enzyme is Novozymes Cellic @ CTec2, the addition amount of cellulose complex enzyme is 15-50 FPU / g substrate, and the enzymatic hydrolysis reaction time is 3h-48h.
[0017] Compared with existing technologies, the present method for improving the efficiency of enzymatic hydrolysis of lignocellulose uses a Type IV deep eutectic solvent prepared from a metal salt and glycerol to pretreat lignocellulose in agricultural and forestry biomass raw materials, followed by enzymatic hydrolysis of the pretreated lignocellulose residue. This method is characterized by low cost, ease of preparation, mild processing conditions, and short processing time. Furthermore, it requires less equipment, is easy to control, and the entire process is environmentally friendly and clean. Furthermore, the cellulose porosity of the pretreated lignocellulose residue is increased, and a large amount of hemicellulose and lignin are removed, which facilitates contact between cellulase and substrate, thereby improving the efficiency of cellulase hydrolysis. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] FIG1 is a schematic flow diagram of a method for improving the efficiency of enzymatic hydrolysis of lignocellulose according to the present invention;
[0019] Figure 2 shows scanning electron micrographs of bamboo powder before (a1, a2, a3) and after (b1, b2, b3) pretreatment with a type IV deep eutectic solvent synthesized by ferric chloride-glycerol;
[0020] FIG3 is a schematic diagram comparing the enzymatic hydrolysis efficiency (i.e., glucose conversion rate) of various embodiments of the present invention and comparative examples;
[0021] FIG4 is a schematic diagram comparing the hemicellulose removal rate and the lignin removal rate of the pretreated bamboo residue according to various embodiments of the present invention. DETAILED DESCRIPTION
[0022] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present invention more clearly understood, the present invention is further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0023] As shown in FIG1 , a preferred embodiment of the method for improving the enzymatic hydrolysis efficiency of lignocellulose according to the present invention comprises the following steps:
[0024] Step 1: crush the agricultural and forestry biomass raw material into a particle size of 60-80 mesh, extract it with a toluene-ethanol solution with a volume ratio of 2:1, and dry it at a constant temperature of 80° C. to obtain an extract-free raw material. The agricultural and forestry biomass is bamboo.
[0025] Step 2: Weigh a metal salt and glycerol in a molar ratio of 1:10 to 1:124 and mix them. The mixture is stirred at 80-90°C and 180 rpm to obtain a homogeneous and transparent Type IV deep eutectic solvent. The metal salt is any one of aluminum chloride, zinc chloride, and ferric chloride. The molar ratio of the metal salt to glycerol is preferably 1:124. Based on the final pretreatment effect, the metal salt is preferably ferric chloride.
[0026] Step 3: Weigh the extract-free raw material prepared in Step 1 and add it to the Type IV deep eutectic solvent prepared in Step 2 at a solid-to-liquid ratio of 1:5 to 1:15. React at 80-120°C with stirring at 300-500 rpm for 2-4 hours to obtain a pretreated mixture. The solid-to-liquid ratio is preferably 1:10.
[0027] Step 4: Use centrifugal separation or vacuum filtration to separate the pretreated mixture into solid and liquid, respectively obtaining a filter residue and a filtrate, washing and desalting the filter residue with ethanol or deionized water until no metal salt component is detected in the washing liquid, and then drying the washed filter residue to obtain a lignocellulosic residue after pretreatment of the agricultural and forestry biomass raw materials; the drying condition of the washed filter residue is drying at 80°C to constant weight.
[0028] Step 5: Add the pretreated lignocellulose residue to an acetate buffer solution with a pH of 4.8 at a certain substrate concentration, then add cellulose complex enzyme, and react in an air bath shaker at 45-50° C. and 140-150 r / min for a period of time to obtain fermentable sugar.
[0029] The substrate concentration of the lignocellulose residue is 2-10 wt%, and the cellulose complex enzyme is Novozymes Cellic @ CTec2, the addition amount of cellulose complex enzyme is 15-50 FPU / g substrate, and the enzymatic hydrolysis reaction time is 3h-48h. The substrate concentration of the lignocellulose reaction residue is preferably 2wt%. The higher the substrate concentration, the longer it takes for the cellulase hydrolysis to reach the plateau phase. The cellulose complex enzyme is Novozymes Cellic @ CTec2. Different amounts of cellulose complex enzyme added have different effects on the time and effect of enzymatic hydrolysis, which affects experimental and future production costs. To achieve high enzymatic hydrolysis efficiency while reducing production costs, a cellulase addition of 15 FPU / g substrate and an enzymatic hydrolysis reaction time of 3 to 48 hours were optimally considered. The enzymatic hydrolysis reaction time can be further optimized to 48 hours based on factors such as lignocellulose pretreatment residue, substrate concentration, cellulose complex enzyme dosage, and optimal enzymatic hydrolysis of the substrate, as well as saving enzymatic hydrolysis time.
[0030] The present invention uses metal salt-glycerol to synthesize a Type IV deep eutectic solvent, which is inexpensive, readily available, recyclable, and environmentally friendly. Furthermore, the metal salt-glycerol has a good removal effect on hemicellulose and lignin, while having minimal dissolution of cellulose, thereby achieving efficient cellulose conversion.
[0031] The method for improving the enzymatic hydrolysis efficiency of lignocellulose of the present invention is further illustrated below by examples and comparative examples.
[0032] Example 1
[0033] The first embodiment of the method for improving the efficiency of enzymatic hydrolysis of lignocellulose of the present invention comprises the following steps:
[0034] The raw bamboo material was crushed and sieved to 60-80 mesh, extracted with toluene-ethanol in a volume ratio of 2:1, and then dried at a constant temperature of 80°C to constant weight to obtain the raw material for extract removal. Ferric chloride and glycerol were weighed in a ratio of 1:10 and stirred at a speed of 180rpm until a uniform transparent liquid was obtained. A certain amount of the raw material for extract removal was weighed and added to the ferric chloride-glycerol solvent in a solid-liquid ratio of 1:15, stirred at 80°C at a speed of 300rpm and reacted for 4 hours. After the reaction, vacuum filtration was used for solid-liquid separation, and the separated bamboo residue was washed and desalted with deionized water until no metal salt components were detected, to obtain the bamboo residue pretreated with the type IV low eutectic solvent synthesized by ferric chloride-glycerol. The bamboo residue was added to an acetic acid buffer solution with a pH of 4.8 at a substrate concentration of 5%, and a cellulose complex enzyme (Cellic @ CTec2), and then reacted in an air shaker at 50°C and 140 rpm for 48 hours to obtain fermentable sugar - glucose. Finally, the enzymatic hydrolysis efficiency of the pretreated bamboo residue was measured to be 46.63%.
[0035] Comparative Example
[0036] Using bamboo as a control, the bamboo was directly hydrolyzed without pretreatment with a metal salt-glycerol type IV deep eutectic solvent to analyze the efficiency of direct enzymatic hydrolysis of bamboo. The process includes the following steps:
[0037] The raw bamboo was crushed into 60-80 mesh, extracted with toluene and ethanol, and then dried at 80℃. A certain amount of raw bamboo without extract was added into an acetate buffer solution with a pH of 4.8 at a substrate concentration of 2%, and a cellulose complex enzyme (Cellic @ CTec2), the enzymatic hydrolysis efficiency was 17.78% after 48 h of reaction at 50°C and 140 r / min in an air bath shaker.
[0038] The enzymatic hydrolysis efficiency of Example 1 is 2.6 times that of the comparative example, indicating that the deep eutectic solvent pretreatment method of the present invention can significantly improve the enzymatic hydrolysis efficiency of bamboo.
[0039] Example 2
[0040] The second embodiment of the method for improving the efficiency of enzymatic hydrolysis of lignocellulose of the present invention comprises the following steps:
[0041] The raw material of moso bamboo was crushed and sieved to 60-80 mesh, extracted with toluene-ethanol in a volume ratio of 2:1, and then dried at a constant temperature of 80°C to constant weight to obtain the raw material without extract. Ferric chloride and glycerol were weighed in a ratio of 1:124 and stirred at a speed of 180rpm until a uniform transparent liquid was obtained. A certain amount of raw material without extract was weighed and added to the ferric chloride-glycerol solvent in a solid-liquid ratio of 1:10, stirred at 300rpm at 100°C and reacted for 3h. After the reaction, vacuum filtration was used for solid-liquid separation, and the separated bamboo residue was washed and desalted with deionized water until no metal salt component was detected, to obtain the bamboo residue pretreated with the type IV low eutectic solvent synthesized by ferric chloride-glycerol. The bamboo residue was added to an acetic acid buffer solution with a pH of 4.8 at a substrate concentration of 2%, and a cellulose complex enzyme (Cellic @ The mixture was stirred at 50°C and 140 rpm for 48 hours to produce fermentable sugar, glucose. The enzymatic hydrolysis efficiency of the pretreated bamboo residue was 67.87%, 3.8 times that of the untreated bamboo in the control sample.
[0042] Example 3
[0043] A third embodiment of the method for improving the efficiency of enzymatic hydrolysis of lignocellulose according to the present invention comprises the following steps:
[0044] The bamboo raw material was crushed and sieved to take 60-80 mesh, extracted with toluene-ethanol in a volume ratio of 2:1, and then dried at a constant temperature of 80°C to constant weight to obtain the extract-free raw material. Ferric chloride and glycerol were weighed in a ratio of 1:124 and stirred at a speed of 180rpm until a uniform transparent liquid was obtained. A certain amount of extract-free raw material was weighed and added to the ferric chloride-glycerol solvent in a solid-liquid ratio of 1:10, stirred at 300rpm at 120°C and reacted for 2h. After the reaction, vacuum filtration was used for solid-liquid separation, and the separated bamboo residue was washed and desalted with deionized water until no metal salt component was detected, to obtain the bamboo residue pretreated with the type IV low eutectic solvent synthesized by ferric chloride-glycerol. The bamboo residue was added to an acetic acid buffer solution with a pH of 4.8 at a substrate concentration of 2%, and a cellulose complex enzyme (Cellic @ The mixture was stirred at 50°C and 140 rpm for 48 hours to produce fermentable sugar, glucose. The enzymatic hydrolysis efficiency of the pretreated bamboo residue was 91.13%, 5.1 times that of the untreated bamboo residue in the control example.
[0045] Example 4
[0046] A fourth embodiment of the method for improving the efficiency of enzymatic hydrolysis of lignocellulose according to the present invention comprises the following steps:
[0047] The raw bamboo material was crushed and sieved to 60-80 mesh, extracted with toluene-ethanol in a volume ratio of 2:1, and then dried at a constant temperature of 80°C to constant weight to obtain the raw material for extract removal. Ferric chloride and glycerol were weighed in a ratio of 1:15 and stirred at a speed of 180rpm until a uniform transparent liquid was obtained. A certain amount of the raw material for extract removal was weighed and added to the ferric chloride-glycerol solvent in a solid-liquid ratio of 1:5, stirred at 300rpm at 100°C and reacted for 3 hours. After the reaction, vacuum filtration was used for solid-liquid separation, and the separated bamboo residue was washed and desalted with deionized water until no metal salt components were detected, to obtain the bamboo residue pretreated with the type IV low eutectic solvent synthesized by ferric chloride-glycerol. The bamboo residue was added to an acetic acid buffer solution with a pH of 4.8 at a substrate concentration of 10%, and a cellulose complex enzyme (Cellic @ The reaction was then continued for 48 hours at 50°C and 140 rpm in an air shaker to produce fermentable sugar, glucose. The enzymatic hydrolysis efficiency of the pretreated bamboo residue was 69.41%, 3.9 times that of the untreated bamboo residue in the control sample.
[0048] Example 5
[0049] A fifth embodiment of the method for improving the efficiency of enzymatic hydrolysis of lignocellulose according to the present invention comprises the following steps:
[0050] The raw material of moso bamboo was crushed and sieved to 60-80 mesh, extracted with toluene-ethanol in a volume ratio of 2:1, and then dried at a constant temperature of 80°C to constant weight to obtain the raw material without extract. Zinc chloride and glycerol were weighed in a ratio of 1:124 and stirred at a speed of 180rpm until a uniform transparent liquid was obtained. A certain amount of raw material without extract was weighed and added to the zinc chloride-glycerol solvent in a solid-liquid ratio of 1:10, stirred at 300rpm at 100°C and reacted for 3h. After the reaction, vacuum filtration was used for solid-liquid separation, and the separated bamboo residue was washed and desalted with deionized water until no metal salt component was detected, to obtain the bamboo residue pretreated with the type IV low eutectic solvent synthesized by zinc chloride-glycerol. The bamboo residue was added to an acetic acid buffer solution with a pH of 4.8 at a substrate concentration of 2%, and a cellulose complex enzyme (Cellic @ The mixture was stirred at 50°C and 140 rpm for 48 hours to produce fermentable sugar, glucose. The enzymatic hydrolysis efficiency of the pretreated bamboo residue was 24.75%, 1.4 times that of the untreated bamboo residue in the control example.
[0051] Example 6
[0052] A sixth embodiment of the method for improving the efficiency of enzymatic hydrolysis of lignocellulose according to the present invention comprises the following steps:
[0053] The raw material of moso bamboo was crushed and sieved to 60-80 mesh, extracted with toluene-ethanol in a volume ratio of 2:1, and then dried at a constant temperature of 80°C to constant weight to obtain the raw material without extract. Aluminum chloride and glycerol were weighed in a ratio of 1:124 and stirred at a speed of 180rpm until a uniform transparent liquid was obtained. A certain amount of raw material without extract was weighed and added to the aluminum chloride-glycerol solvent in a solid-liquid ratio of 1:10, stirred at 300rpm at 100°C and reacted for 3 hours. After the reaction, vacuum filtration was used for solid-liquid separation, and the separated bamboo residue was washed and desalted with deionized water until no metal salt component was detected, to obtain the bamboo residue pretreated with the type IV low eutectic solvent synthesized by aluminum chloride-glycerol. The bamboo residue was added to an acetic acid buffer solution with a pH of 4.8 at a substrate concentration of 2%, and a cellulose complex enzyme (Cellic @ The mixture was stirred at 50°C and 140 rpm for 48 hours to produce glucose, a fermentable sugar. The enzymatic hydrolysis efficiency of the pretreated bamboo residue was 59.78%, 3.4 times that of the untreated bamboo residue in the control example.
[0054] As shown in Figure 2, the surface of the bamboo fiber of the untreated bamboo powder is relatively smooth and intact, as shown in Figures 2-a1, 2-a1, and 2-a1, and is tightly arranged; while the surface of the bamboo fiber of the bamboo powder pretreated with the type IV low eutectic solvent synthesized by ferric chloride-propylene glycol of the present invention is rough, with deeper grooves, as shown in Figures 2-b1, 2-b2, and 2-b3. The fibers are broken in many places, and the degree of damage on the fracture surface is high, which greatly increases the contact area between cellulase and cellulose and the adsorption capacity of cellulose for cellulase, thereby improving the enzymatic hydrolysis efficiency of cellulose.
[0055] As shown in FIG3 , compared with the comparative example, after pretreatment with the type IV deep eutectic solvent synthesized by ferric chloride-glycerol of the present invention, the enzymatic hydrolysis effect of the lignocellulosic biomass is improved, especially for ferric chloride-based DES and aluminum chloride-based DES. This is closely related to the properties of the metal salt, and the pretreatment process conditions have different degrees of influence on the final enzymatic hydrolysis efficiency.
[0056] As shown in Figure 4, pretreatment process conditions and pretreatment solvent systems have varying degrees of influence on the removal of lignin and hemicellulose components. The removal rate can, to a certain extent, reflect the loss of structural density in lignocellulosic biomass. Therefore, the removal of lignin and hemicellulose can promote enzymatic hydrolysis of lignocellulosic biomass and improve its efficiency.
[0057] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.
Claims
1. A method for improving the efficiency of enzymatic hydrolysis of lignocellulose, characterized in that: The steps include: Step 1: crush the agricultural and forestry biomass raw materials into a particle size of 60-80 mesh, extract them with a toluene-ethanol solution, and dry them at a constant temperature to obtain an extract-free raw material; Step 2: weighing metal salt and propylene glycol respectively at a molar ratio of 1:10 to 1:124 and mixing them, and stirring the mixture at a temperature of 80 to 90° C. and a stirring speed of 180 rpm to obtain a uniform and transparent type IV low eutectic solvent; wherein the metal salt is any one of aluminum chloride, zinc chloride, and ferric chloride; Step 3, weighing the extract-free raw material prepared in step 1, adding it to the type IV low eutectic solvent prepared in step 2 at a solid-liquid ratio of 1:5 to 1:15, reacting at a temperature of 80 to 120° C. and a stirring speed of 300 to 500 rpm for 2 to 4 hours to obtain a pretreated mixture; Step 4: Separate the pretreated mixture into solid and liquid by centrifugation or vacuum filtration to obtain filter residue and filtrate, respectively; wash and desalt the filter residue with ethanol or deionized water until no metal salt component is detected in the washing liquid; and then dry the washed filter residue to obtain the lignocellulosic residue after pretreatment of the agricultural and forestry biomass raw materials; Step 5: Add the pretreated lignocellulose residue to an acetate buffer solution with a pH of 4.8 at a certain substrate concentration, then add cellulose complex enzyme, and react for a period of time in an air bath shaker at 45-50° C. and a rotation speed of 140-150 r / min to obtain fermentable sugar.
2. The method for improving the enzymatic hydrolysis efficiency of lignocellulose according to claim 1, characterized in that: In step one, the agricultural and forestry biomass is bamboo.
3. The method for improving the enzymatic hydrolysis efficiency of lignocellulose according to claim 1, characterized in that: In step 4, the washed filter residue is dried at 80° C. to a constant weight.
4. The method for improving the enzymatic hydrolysis efficiency of lignocellulose according to claim 1, characterized in that: In step 5, the substrate concentration of the lignocellulose residue is 2-10 wt%, and the cellulose complex enzyme is Novozymes Cellic @ CTec2, the addition amount of cellulose complex enzyme is 15-50 FPU / g substrate, and the enzymatic hydrolysis reaction time is 3h-48h.
Citation Information
Patent Citations
Method for comprehensively utilizing lignocellulose by using polyol-based acidic eutectic solvent
CN114085876A
Method for improving hydrolysis efficiency of lignocellulose
CN116426588A
Use of metal salts and deep eutectic solvents in a process to solubilize a biomass