High-voltage cable

By adopting a structural design of a double-layer semiconductor water resistance buffer layer and a copper wire shielding layer in high-voltage cable, combined with the waterproof and corrosion resistance of the metal sheath, the insulation and shielding problems of high-voltage cables are solved, and the shielding performance is significantly improved and corrosion resistance, extending service life.

WO2024230253A1PCT designated stage expired Publication Date: 2024-11-14ZHONGCHEN CABLE (JIANGXI) CO LTD

Patent Information

Application Number
PCT/CN2024/073737
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-10
Filing Date
2024-01-24
Publication Date
2024-11-14

AI Technical Summary

Technical Problem

During the production process, high-voltage cables are prone to insulating eccentricity, uneven thickness of insulation shielding, impurities inside the insulation and protruding internal and external shielding, which affects the insulation and shielding of the cable, resulting in faults and safety hazards.

Method used

Adopt cable structure from the inside to the outside: conductor, conductor shielding layer, insulation layer, insulation shielding layer, semiconducting water buffer layer, copper wire shielding layer, semiconducting water buffer layer, metal sheath and anti-corrosion layer, through double The layer semiconductor water buffer layer and copper wire shielding layer share the fault current, enhance mechanical properties and longitudinal waterproofing, and utilize the radial waterproofing and corrosion resistance of metal sheaths.

Benefits of technology

It significantly improves the shielding and corrosion resistance of high-voltage cables, extends service life, and significantly improves shielding performance at test frequencies of 100MHz and 1GHz.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure PCTCN2024073737-FTAPPB-I100001
    Figure PCTCN2024073737-FTAPPB-I100001
Patent Text Reader

Abstract

Disclosed is a high-voltage cable, which belongs to the technical field of cable manufacturing. The high-voltage cable comprises a cable conductor, a conductor shielding layer, an insulating layer, an insulation shielding layer, a semi-conductive water-blocking buffer layer, a copper wire shielding layer, a semi-conductive water-blocking buffer layer, a metal sheath, an anti-corrosion layer, and a non-metal sheath layer that are sequentially arranged from inside to outside. By means of adopting two semi-conductive water-blocking buffer layers, and arranging the copper wire shielding layer between the two semi-conductive water-blocking buffer layers, a fault current of a cable system can be shared, and the mechanical performance of the high-voltage cable can also be enhanced at the same time. The structural design of the two water-blocking buffer layers meets the mechanical impact of copper wires on insulation shielding, and has excellent longitudinal waterproof performance. Meanwhile, the radial waterproof performance and the corrosion resistance of the metal sheath are adopted, such that the cable has strong corrosion resistance and a waterproof capability, and the metal sheath can also carry a certain amount of the system fault current at the same time.
Need to check novelty before this filing date? Find Prior Art

Description

A high-voltage cable

[0001] This application claims priority to the Chinese patent application filed with the China Patent Office on May 10, 2023, with application number 202310518716X and invention name “A High Voltage Cable”, the entire contents of which are incorporated by reference into this application. Technical Field

[0002] The present invention relates to the technical field of cable manufacturing, in particular to a high-voltage cable. Background Art

[0003] High-voltage cables are a type of power cable used to transmit power between 66 and 220 kV. They are primarily used for power transmission and distribution, particularly for long-distance transmission. Armored high-voltage cables are primarily used for underground burial, offering protection against high-intensity ground pressure and damage from other external forces. The structure of medium- and high-voltage cables is primarily: conductor + three-layer co-extrusion (inner shield, insulation, and outer shield) + metal shield + protective layer.

[0004] Generally, problems that are prone to occur during the production of high-voltage cables include: insulation eccentricity, uneven insulation shield thickness, impurities in the insulation, protrusions on the inner and outer shields, etc., which affect the insulation and shielding properties of the cable. In some serious cases, failures may occur during the completion test or shortly after commissioning. Most of them exist in the form of defects in the cable system, posing a serious hidden danger to the long-term safe operation of the cable.

[0005] Therefore, how to improve the shielding performance of high-voltage cables has become a technical problem that needs to be solved urgently in this field.

[0006] Summary of the Invention

[0007] The object of the present invention is to provide a high-voltage cable. The high-voltage cable provided by the present invention has good insulation and shielding properties, and excellent corrosion resistance.

[0008] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions:

[0009] The present invention provides a high-voltage cable, comprising a cable conductor, a conductor shielding layer, an insulating layer, an insulating shielding layer, a semiconducting water-repellent buffer layer, a copper wire shielding layer, a semiconducting water-repellent buffer layer, a metal sheath, an anti-corrosion layer and a non-metallic sheath layer, which are arranged in sequence from the inside to the outside.

[0010] Preferably, the high-voltage cable is suitable for a voltage of 66 to 220 kV.

[0011] Preferably, the cable conductor is composed of copper wire.

[0012] Preferably, the copper wire complies with GB / T3953.

[0013] Preferably, the copper wires are twisted in layers and compressed to form a cable conductor.

[0014] Preferably, the conductor shielding layer is made of cross-linked polyethylene insulation material for high-voltage DC cables; and the thickness of the conductor shielding layer is 0.5-1.0 mm.

[0015] Preferably, the insulating layer is made of radiation cross-linked polyethylene material or soft polyvinyl chloride plastic; and the thickness of the insulating layer is 0.8-2.0 mm.

[0016] Preferably, the raw materials of the insulating shielding layer include, by weight: 47-82 parts of polypropylene, 35-48 parts of ethylene-octene copolymer, 3-8 parts of nano-silicon dioxide, 23-37 parts of conductive carbon black, 1-2 parts of antioxidant and 0.5-1.5 parts of lubricating dispersant.

[0017] Preferably, the polypropylene is a blend of homopolypropylene and copolymer polypropylene, and the mass ratio of the homopolypropylene to the copolymer polypropylene is 1:(1-10).

[0018] Preferably, the melt index of the homopolypropylene is 1.0 to 5.0 g / 10 min, and the melt index of the copolymer polypropylene is 1.0 to 4.0 g / 10 min.

[0019] Preferably, the antioxidant is 4,4'-thiobis(6-tert-butyl-3-methylphenol), and the lubricating dispersant is polyethylene wax.

[0020] Preferably, the preparation method of the insulating shielding layer is: polypropylene, ethylene-octene copolymer, nano-silica, conductive carbon black, antioxidant and lubricating dispersant are mixed and kneaded, and then extruded and granulated to obtain particles, and then the particles are melted and coated on the surface of the insulating layer to obtain the insulating shielding layer.

[0021] Preferably, the semiconducting water-blocking buffer layer is a semiconducting water-blocking tape or a semiconductive buffer water-blocking tape; the performance of the semiconducting water-blocking buffer layer complies with the JB / T10259 standard; and the thickness of the semiconducting water-blocking buffer layer is 0.6 to 0.8 mm.

[0022] Preferably, the copper wire shielding layer is formed by twisting copper wires; the thickness of the copper wire shielding layer is 1 to 1.5 mm.

[0023] Preferably, the metal sheath is an aluminum sheath or a lead sheath.

[0024] Preferably, the raw materials of the anti-corrosion layer include, by weight, 52 to 65 parts of asphalt, 1 to 5 parts of emulsifier, 1 to 2 parts of stabilizer and 35 to 40 parts of water.

[0025] Preferably, the method for preparing the anti-corrosion layer comprises the following steps:

[0026] (1) mixing an emulsifier, a stabilizer, and water to obtain an emulsified aqueous solution;

[0027] (2) heating the asphalt to obtain molten asphalt;

[0028] (3) mixing the emulsified aqueous solution obtained in step (1) and the molten asphalt obtained in step (2) and stirring them at high speed, and then coating them on the surface of the metal sheath to obtain an anti-corrosion layer;

[0029] There is no order in which steps (1) and (2) are performed.

[0030] The present invention provides a high-voltage cable comprising, arranged in order from the inside out, a cable conductor, a conductor shielding layer, an insulation layer, an insulation shielding layer, a semiconducting water-repellent buffer layer, a copper wire shielding layer, a semiconducting water-repellent buffer layer, a metal sheath, an anti-corrosion layer, and a non-metallic sheathing layer. The present invention utilizes a double-layer semiconducting water-repellent buffer layer and arranges a copper wire shielding layer between the two layers of the semiconducting water-repellent buffer layer. The copper wire shielding layer can share the fault current of the cable system while also enhancing the mechanical properties of the high-voltage cable. The structural design of the two layers of the semiconducting water-repellent buffer layer satisfies the mechanical impact of the copper wire on the insulation shielding, while also having excellent longitudinal waterproof performance. By arranging a metal sheath behind the semiconducting water-repellent buffer layer and utilizing the radial waterproof performance and corrosion resistance of the metal sheath, the cable has strong corrosion resistance and waterproof capabilities, while also being able to carry a certain amount of system fault current. The results of the embodiments show that when the test frequency is 100 MHz, the shielding properties of the high-voltage cables prepared in Examples 1 to 3 of the present invention are ≥95 dB, while the shielding properties of the high-voltage cables prepared in Comparative Examples 1 to 2 are <85 dB. When the test frequency is 1 GHz, the shielding properties of the high-voltage cables prepared in Examples 1 to 3 of the present invention are ≥60 dB, while the shielding properties of the high-voltage cables prepared in Comparative Examples 1 to 2 are ≤56 dB. This indicates that the shielding properties of the high-voltage cables prepared in the present invention are significantly improved compared to other high-voltage cables. At the same time, the high-voltage cables have excellent corrosion resistance and a longer service life. DETAILED DESCRIPTION

[0031] The present invention provides a high-voltage cable, comprising a cable conductor, a conductor shielding layer, an insulating layer, an insulating shielding layer, a semiconducting water-repellent buffer layer, a copper wire shielding layer, a semiconducting water-repellent buffer layer, a metal sheath, an anti-corrosion layer and a non-metallic sheath layer, which are arranged in sequence from the inside to the outside.

[0032] Unless otherwise specified, the raw materials used in the high-voltage cable provided by the present invention are all commercially available products well known to those skilled in the art.

[0033] In the present invention, the voltage applicable to the high-voltage cable is preferably 66 to 220 kV, more preferably 110 to 220 kV.

[0034] The high-voltage cable provided by the present invention includes a cable conductor. In the present invention, the cable conductor is preferably composed of copper wire; the copper wire preferably complies with GB / T3953; and the copper wire is preferably formed by layered twisting and compaction. The present invention does not specifically limit the size of the cable conductor; it can be determined based on the required high-voltage cable specifications. Through the above-mentioned method, the present invention can improve the strength of the cable conductor.

[0035] The high-voltage cable provided by the present invention includes a conductor shielding layer arranged outside the cable conductor. In the present invention, the conductor shielding layer is preferably a cross-linked polyethylene insulation material for high-voltage DC cables; the thickness of the conductor shielding layer is preferably 0.5 to 1.0 mm. The present invention has no special restrictions on the specific source of the cross-linked polyethylene insulation material for high-voltage DC cables, and commercially available products familiar to those skilled in the art can be used. By providing a conductor shielding layer, the present invention can make the conductive core and the insulation electric field uniform, eliminate the increase in the electric field strength on the conductor surface caused by the roughness of the conductor surface, and improve the transmission efficiency.

[0036] The high-voltage cable provided by the present invention includes an insulating layer disposed outside the conductor shielding layer. The insulating layer is preferably made of irradiated cross-linked polyethylene or soft polyvinyl chloride, more preferably irradiated cross-linked polyethylene. The thickness of the insulating layer is preferably 0.8 to 2.0 mm, more preferably 1.0 to 1.5 mm. The insulating layer primarily serves to improve the cable's insulation and prevent problems such as leakage.

[0037] The high-voltage cable provided by the present invention includes an insulating shielding layer arranged outside the insulating layer. In the present invention, the raw materials of the insulating shielding layer preferably include, by weight, 47 to 82 parts of polypropylene, 35 to 48 parts of ethylene-octene copolymer, 3 to 8 parts of nano-silicon dioxide, 23 to 37 parts of conductive carbon black, 1 to 2 parts of antioxidant, and 0.5 to 1.5 parts of lubricating dispersant. More preferably, it is 55 to 68 parts of polypropylene, 38 to 43 parts of ethylene-octene copolymer, 4 to 6 parts of nano-silicon dioxide, 25 to 30 parts of conductive carbon black, 1 to 2 parts of antioxidant, and 0.5 to 1.5 parts of lubricating dispersant. The present invention optimizes the composition of the insulating shielding layer and utilizes polypropylene and ethylene-octene copolymer as the base materials to solve the shortcomings of polypropylene's poor toughness and brittleness at low temperatures. By adding a certain amount of nano-silicon dioxide to improve the dielectric strength, and combining with conductive carbon black to improve its shielding effect, the addition of antioxidants improves its corrosion resistance, so that the insulating shielding layer can lastingly play an insulating shielding role.

[0038] In the present invention, the polypropylene is preferably a blend of homopolypropylene and copolymer polypropylene; the melt index of the homopolypropylene is preferably 1.0 to 5.0 g / 10 min; the melt index of the copolymer polypropylene is preferably 1.0 to 4.0 g / 10 min; the mass ratio of the homopolypropylene to the copolymer polypropylene is preferably 1:(1 to 10), more preferably 1:(2 to 8). By using two different types of polypropylene as raw materials, the insulation effect of the present invention can be further improved.

[0039] The present invention has no particular limitation on the specific particle sizes of the nano-silicon dioxide and conductive carbon black, and commercially available products well known to those skilled in the art may be used.

[0040] In the present invention, the antioxidant is preferably 4,4'-thiobis(6-tert-butyl-3-methylphenol). By adding the antioxidant, the present invention can improve the antioxidant effect of the insulating shielding layer, and by selecting a specific type of antioxidant, precipitation of the antioxidant from the insulating shielding layer at high temperatures can be avoided.

[0041] In the present invention, the lubricating dispersant is preferably polyethylene wax. The addition of the lubricating dispersant in the present invention facilitates better mixing of the components during preparation and facilitates coating.

[0042] In the present invention, the preparation method of the insulating shielding layer is preferably: polypropylene, ethylene-octene copolymer, nano-silica, conductive carbon black, antioxidant and lubricating dispersant are mixed and kneaded, and then extruded and granulated to obtain particles, and then the particles are melted and coated on the surface of the insulating layer to obtain the insulating shielding layer.

[0043] In the present invention, the mixing is preferably carried out in a continuous mixing unit; the continuous mixing unit is preferably one of a mixing reciprocating machine, a co-rotating twin-screw extruder and a continuous internal mixing unit of four or more combinations.

[0044] The present invention has no particular limitation on the mixing and melting temperatures, which can be determined according to the common technical knowledge of those skilled in the art. The present invention has no particular limitation on the specific operation of the coating, which can be carried out using coating methods well known to those skilled in the art.

[0045] The high-voltage cable provided by the present invention includes a semiconducting water-blocking buffer layer disposed outside the insulating shielding layer. In the present invention, the semiconducting water-blocking buffer layer is preferably a semiconducting water-blocking tape or a semiconductive buffer water-blocking tape; the performance of the semiconducting water-blocking buffer layer preferably complies with the JB / T10259 standard. In the present invention, the thickness of the semiconducting water-blocking buffer layer is preferably 0.6 to 0.8 mm.

[0046] The high-voltage cable provided by the present invention includes a copper wire shielding layer disposed outside the semiconducting water-repellent buffer layer. In the present invention, the copper wire shielding layer is preferably formed by twisting copper wires. In the present invention, the copper wire shielding layer preferably has a thickness of 1 to 1.5 mm. By controlling the thickness of the copper wire shielding layer, the present invention can further enhance the mechanical properties of the high-voltage cable.

[0047] The high-voltage cable provided herein includes a semiconducting water-blocking buffer layer disposed outside the copper wire shielding layer. In the present invention, the semiconducting water-blocking buffer layer is preferably a semiconducting water-blocking tape or a semiconductive buffer water-blocking tape; the performance of the semiconducting water-blocking buffer layer preferably complies with the JB / T10259 standard. In the present invention, the thickness of the semiconducting water-blocking buffer layer is preferably 0.6 to 0.8 mm.

[0048] The present invention adopts a double-layer semiconducting water buffer layer and arranges a copper wire shielding layer between the two layers of semiconducting water buffer layers. The copper wire shielding layer can share the fault current of the cable system and also enhance the mechanical properties of the high-voltage cable.

[0049] The high-voltage cable provided by the present invention includes a metal sheath disposed over a semiconducting water-repellent buffer layer. In the present invention, the metal sheath is preferably an aluminum sheath or a lead sheath, more preferably an alloy-lead sheath. The present invention does not specifically limit the specific composition of the alloy-lead sheath; commercially available products familiar to those skilled in the art may be used. By disposing a metal sheath behind the semiconducting water-repellent buffer layer, the present invention utilizes the radial waterproof and corrosion-resistant properties of the metal sheath to provide the cable with strong corrosion resistance and waterproof capabilities. Furthermore, the metal sheath can also carry a certain amount of system fault current.

[0050] The high-voltage cable provided by the present invention includes an anti-corrosion layer provided on the outside of the metal sheath. In the present invention, the raw materials of the anti-corrosion layer preferably include, by weight, 52 to 65 parts of asphalt, 1 to 5 parts of emulsifier, 1 to 2 parts of stabilizer, and 35 to 40 parts of water, and more preferably 55 to 60 parts of asphalt, 2 to 3 parts of emulsifier, 1 to 2 parts of stabilizer, and 35 to 40 parts of water. In the present invention, the asphalt is preferably 10# petroleum asphalt; the emulsifier is preferably any one of asphalt emulsifiers BH-Z1 and BH-Z2; the stabilizer is preferably any one of bentonite, attapulgite, and aluminum silicate. By optimizing the composition of the anti-corrosion layer, the present invention improves the thermal stability of the anti-corrosion layer on the one hand, so that it can still have a good anti-corrosion effect at higher temperatures, and on the other hand, it can reduce the pollution caused by it; the addition of the stabilizer can improve the stability of the anti-corrosion layer and avoid problems such as cracking.

[0051] In the present invention, the method for preparing the anti-corrosion layer preferably comprises the following steps:

[0052] (1) mixing an emulsifier, a stabilizer, and water to obtain an emulsified aqueous solution;

[0053] (2) heating the asphalt to obtain molten asphalt;

[0054] (3) mixing the emulsified aqueous solution obtained in step (1) and the molten asphalt obtained in step (2) and stirring them at high speed, and then coating them on the surface of the metal sheath to obtain an anti-corrosion layer;

[0055] There is no order in which steps (1) and (2) are performed.

[0056] In the present invention, the emulsifier, stabilizer and water are preferably mixed and stirred to obtain an emulsified aqueous solution. The present invention has no particular limitation on the stirring rate and time, as long as the components are mixed evenly.

[0057] In the present invention, the water temperature is preferably 60-70°C. If the water temperature does not meet the above conditions, the present invention preferably heats the water. By controlling the water temperature, the present invention prevents the asphalt from rapidly cooling and solidifying when it is subsequently mixed with molten asphalt.

[0058] The present invention preferably heats the asphalt to produce molten asphalt. The present invention does not specify the temperature of the heat treatment, as long as it can melt the asphalt into a liquid state. The present invention heats the asphalt to remove moisture from the asphalt and facilitates emulsification by mixing with other solutions.

[0059] After obtaining the emulsified aqueous solution and the molten asphalt, the present invention preferably mixes the emulsified aqueous solution and the molten asphalt, stirs them at high speed, and then coats them on the surface of the metal sheath to obtain an anti-corrosion layer.

[0060] In the present invention, the high-speed stirring is preferably performed in an emulsifier. The stirring rate is not particularly limited and can be determined based on common technical knowledge in the art, as long as it is sufficient to emulsify the asphalt. High-speed stirring allows the aqueous emulsifier solution and asphalt to form an oil-in-water asphalt emulsion, thereby improving its anti-corrosion performance.

[0061] The high-voltage cable provided by the present invention includes a non-metallic sheath layer disposed outside the anti-corrosion layer. In the present invention, the non-metallic sheath layer preferably comprises an outer sheath layer and a semi-conductive layer; the outer sheath layer is preferably extruded from a polyvinyl chloride sheath material or a polyethylene sheath material; and the semi-conductive layer is preferably a graphite semi-conductive layer.

[0062] The present invention adopts a double-layer semiconducting water-repellent buffer layer and arranges a copper wire shielding layer between the two layers. The copper wire shielding layer can share the fault current of the cable system and also enhance the mechanical properties of the high-voltage cable. The structural design of the two layers of semiconducting water-repellent buffer layer satisfies the mechanical impact of the copper wire on the insulation shield and has excellent longitudinal waterproof performance. By arranging a metal sheath behind the semiconducting water-repellent buffer layer and utilizing the radial waterproof performance and corrosion resistance of the metal sheath, the cable has strong corrosion resistance and waterproof capabilities. At the same time, the metal sheath can also carry a certain amount of system fault current.

[0063] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions of the present invention. Obviously, the embodiments described are only some of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.

[0064] Example 1

[0065] The high-voltage cable provided in this embodiment is composed of a cable conductor, a conductor shielding layer, an insulating layer, an insulating shielding layer, a semi-conductive water-repellent buffer layer, a copper wire shielding layer, a semi-conductive water-repellent buffer layer, a metal sheath, an anti-corrosion layer, and a non-metallic sheathing layer, which are arranged in sequence from the inside to the outside.

[0066] The cable conductor is composed of copper wires; the copper wires are twisted and compressed in layers to form the cable conductor; the conductor shielding layer is made of cross-linked polyethylene insulation material for high-voltage DC cables; the thickness of the conductor shielding layer is 0.7 mm; the insulation layer is made of irradiated cross-linked polyethylene material, and the thickness of the insulation layer is 0.8 mm; the semi-conductive water-repellent buffer layer is a semi-conductive water-repellent tape, the performance of which shall comply with the JB / T10259 standard, and the thickness of each layer of the semi-conductive water-repellent buffer layer is 0.6 mm; the thickness of the copper wire shielding layer is 1.5 mm; the metal sheath is an alloy lead sheath; the non-metallic sheathing layer is composed of an outer sheath layer and a semi-conductive layer; the outer sheath layer is extruded from polyvinyl chloride sheathing material; the semi-conductive layer is a graphite semi-conductive layer;

[0067] The raw materials of the insulating shielding layer are, by weight, 55 parts of polypropylene, 42 parts of ethylene-octene copolymer, 5 parts of nano-silica, 28 parts of conductive carbon black, 1 part of antioxidant and 1 part of lubricating dispersant; the polypropylene is a blend of homopolypropylene and copolymer polypropylene; the melt index of the homopolypropylene is 3.0-4.0 g / 10 min, the melt index of the copolymer polypropylene is 2.0-3.0 g / 10 min, and the mass ratio of the homopolypropylene to the copolymer polypropylene is 1:10; the antioxidant is 4,4'-thiobis(6-tert-butyl-3-methylphenol); and the lubricating dispersant is polyethylene wax;

[0068] The insulating shielding layer is prepared by adding polypropylene, ethylene-octene copolymer, nano-silica, conductive carbon black, antioxidant and lubricating dispersant into a co-rotating twin-screw extruder, mixing and kneading, then extruding and granulating to obtain granules, and then melting the granules and coating them on the surface of the insulating layer to obtain the insulating shielding layer;

[0069] The raw materials of the anti-corrosion layer are as follows: 55 parts of asphalt, 3 parts of emulsifier, 2 parts of stabilizer and 40 parts of water, calculated by weight; the asphalt is 10# petroleum asphalt; the emulsifier is asphalt emulsifier BH-Z2; the stabilizer is bentonite;

[0070] The preparation method of the anti-corrosion layer is:

[0071] (1) mixing an emulsifier, a stabilizer, and 70° C. water to obtain an emulsified aqueous solution;

[0072] (2) heating the asphalt to obtain molten asphalt;

[0073] (3) The emulsified aqueous solution obtained in step (1) and the molten asphalt obtained in step (2) are mixed in an emulsifier and stirred at high speed, and then coated on the surface of the metal sheath to obtain an anti-corrosion layer.

[0074] Example 2

[0075] The raw materials of the insulating shielding layer are as follows: 65 parts of polypropylene, 40 parts of ethylene-octene copolymer, 8 parts of nano-silicon dioxide, 25 parts of conductive carbon black, 1 part of antioxidant and 1 part of lubricating dispersant, calculated by weight.

[0076] The raw materials of the anti-corrosion layer are as follows: 53 parts of asphalt, 2 parts of emulsifier, 2 parts of stabilizer and 40 parts of water.

[0077] Other conditions are the same as in Example 1.

[0078] Example 3

[0079] The raw materials of the insulating shielding layer are as follows: 68 parts of polypropylene, 40 parts of ethylene-octene copolymer, 6 parts of nano-silicon dioxide, 32 parts of conductive carbon black, 1 part of antioxidant and 1 part of lubricating dispersant, calculated by weight.

[0080] The raw materials of the anti-corrosion layer are as follows: 65 parts of asphalt, 4 parts of emulsifier, 2 parts of stabilizer and 40 parts of water.

[0081] Other conditions are the same as in Example 1.

[0082] Comparative Example 1

[0083] The insulating shielding layer is cross-linked polyethylene that has been cross-linked and cured;

[0084] Other conditions are the same as in Example 1.

[0085] Comparative Example 2

[0086] The anti-corrosion layer is obtained by coating 10# asphalt after melting;

[0087] Other conditions are the same as in Example 1.

[0088] Performance Testing

[0089] The shielding properties of the high-voltage cables prepared in Examples 1 to 3 and Comparative Examples 1 to 2 were tested using a triaxial method and a line injection method, respectively. The test frequency of the triaxial method was 100 MHz, and the reference standard was GB9023-88. The test frequency of the line injection method was 1 GHz, and the reference standard was GB / T17737.1-2000. The results are shown in Table 1.

[0090] Table 1 Shielding properties of high voltage cables prepared in Examples 1 to 3 and Comparative Examples 1 to 2

[0091] It can be seen from Table 1 that the shielding property of the high-voltage cable prepared by the present invention is significantly improved compared with other high-voltage cables, indicating that the present invention can obtain a high-voltage cable with better shielding property.

[0092] The description of the above embodiments is only intended to help understand the method of the present invention and its core concept. It should be noted that for those skilled in the art, without departing from the principles of the present invention, several improvements and modifications may be made to the present invention, and these improvements and modifications also fall within the scope of protection of the claims of the present invention. Various modifications to these embodiments are obvious to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A high voltage cable, comprising a cable conductor, a conductor shielding layer, an insulating layer, an insulating shielding layer, a semiconducting water-repellent buffer layer, a copper wire shielding layer, a semiconducting water-repellent buffer layer, a metal sheath, an anti-corrosion layer and a non-metallic sheath layer, which are arranged in sequence from the inside to the outside.

2. The high voltage cable according to claim 1, characterized in that The high voltage cable is suitable for a voltage of 66 to 220 kV.

3. The high voltage cable according to claim 1, characterized in that: The cable conductor is composed of copper wire.

4. The high voltage cable according to claim 3, characterized in that: The copper conductor complies with the provisions of GB / T3953.

5. The high voltage cable according to claim 3, characterized in that: The copper wires are twisted in layers and compressed to form a cable conductor.

6. The high voltage cable according to claim 1, characterized in that The conductor shielding layer is made of cross-linked polyethylene insulation material for high-voltage DC cables; the thickness of the conductor shielding layer is 0.5-1.0 mm.

7. The high voltage cable according to claim 1, characterized in that The material of the insulating layer is irradiated cross-linked polyethylene material or soft polyvinyl chloride plastic; the thickness of the insulating layer is 0.8-2.0 mm.

8. The high voltage cable according to claim 1, characterized in that Calculated by weight, the raw materials of the insulating shielding layer include: 47-82 parts of polypropylene, 35-48 parts of ethylene-octene copolymer, 3-8 parts of nano-silicon dioxide, 23-37 parts of conductive carbon black, 1-2 parts of antioxidant and 0.5-1.5 parts of lubricating dispersant.

9. The high voltage cable according to claim 8, characterized in that The polypropylene is a blend of homopolypropylene and copolymer polypropylene, and the mass ratio of the homopolypropylene to the copolymer polypropylene is 1:(1-10).

10. The high voltage cable according to claim 9, characterized in that The melt index of the homopolypropylene is 1.0 to 5.0 g / 10 min, and the melt index of the copolymer polypropylene is 1.0 to 4.0 g / 10 min.

11. The high voltage cable according to claim 8, characterized in that The antioxidant is 4,4'-thiobis(6-tert-butyl-3-methylphenol), and the lubricating dispersant is polyethylene wax.

12. The high voltage cable according to claim 8, characterized in that The preparation method of the insulating shielding layer is: polypropylene, ethylene-octene copolymer, nano silicon dioxide, conductive carbon black, antioxidant and lubricating dispersant are mixed and kneaded, then extruded and granulated to obtain particles, and then the particles are melted and coated on the surface of the insulating layer to obtain the insulating shielding layer.

13. The high voltage cable according to claim 1, characterized in that The semiconductive water-blocking buffer layer is a semiconductive water-blocking tape or a semiconductive buffer water-blocking tape; the performance of the semiconductive water-blocking buffer layer meets the JB / T10259 standard; the thickness of the semiconductive water-blocking buffer layer is 0.6-0.8 mm.

14. The high voltage cable according to claim 1, characterized in that The copper wire shielding layer is formed by twisting copper wires; the thickness of the copper wire shielding layer is 1 to 1.5 mm.

15. The high voltage cable according to claim 1, characterized in that The metal sheath is an aluminum sheath or a lead sheath.

16. The high voltage cable according to claim 1, characterized in that Calculated by weight, the raw materials of the anti-corrosion layer include: 52 to 65 parts of asphalt, 1 to 5 parts of emulsifier, 1 to 2 parts of stabilizer and 35 to 40 parts of water.

17. The high voltage cable according to claim 1, characterized in that The method for preparing the anti-corrosion layer comprises the following steps: (1) mixing an emulsifier, a stabilizer and water to obtain an emulsified aqueous solution; (2) heating the asphalt to obtain molten asphalt; (3) mixing the emulsified aqueous solution obtained in step (1) and the molten asphalt obtained in step (2), stirring the mixture at high speed, and then coating the mixture on the surface of the metal sheath to obtain an anti-corrosion layer; There is no order of precedence for step (1) and step (2).

Citation Information

Patent Citations

  • High-transmission efficiency high-voltage crosslinked polyethylene insulated power cable

    CN107068284A

  • High-voltage cable coated with novel anticorrosive material

    CN108389649A

  • Semiconductive shielded layer material for high-voltage cable polypropylene insulation and preparation method

    CN108864527A

  • High-voltage cable

    CN116386940A

  • High voltage direct current power cable

    US20200185123A1

Cited By

  • Special photoelectric composite cable used in extremely cold weather

    CN119230180A

  • Waterproof corrosion-resistant floating cable

    CN120118467A