Resin, resin composition, and display device using same
The novel photosensitive resin composition addresses the stability and durability issues in organic light emitting display devices by enabling low-temperature thermosetting and fine pigment dispersion, resulting in high-resolution and stable patterns with reduced power consumption and extended device lifespan.
Patent Information
- Application Number
- PCT/KR2024/006059
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-08
- Filing Date
- 2024-05-06
- Publication Date
- 2024-11-14
AI Technical Summary
Conventional photosensitive compositions used in organic light emitting display devices face challenges in achieving stable patterns at low temperatures, as they often result in low pattern stability during post-heat treatment and are affected by external sunlight and solvents, while also contributing to high power consumption and reduced lifespan due to the use of polarizers and color filters.
A novel photosensitive resin composition incorporating an alkali-soluble resin, reactive unsaturated compounds, photoinitiators, and reactive silica particles with a chromophore-based dye, which allows for photocuring and low-temperature thermosetting, providing excellent light resistance and chemical resistance, and enabling fine pigment dispersion for high-resolution and stable pattern formation.
The solution enables the formation of highly reliable, high-resolution patterns with improved stability and reduced residue, even at low temperatures, while minimizing power consumption and extending the lifespan of organic light emitting display devices by eliminating the need for polarizers and enhancing the durability of color filters.
Smart Images

Figure KR2024006059_14112024_PF_FP_ABST
Abstract
Description
Resin, resin composition and display device using the same
[0001] The present invention relates to a photosensitive resin composition, a pattern or film formed from the photosensitive composition, and an organic light-emitting display device using the pattern or film.
[0002] Liquid crystal display devices (LCDs) and organic light-emitting display devices (OLEDs) are widely used in flat panel displays. Among these, OLEDs, in particular, offer advantages such as low power consumption, fast response speed, high color reproducibility, high brightness, and wide viewing angles.
[0003] After depositing an organic layer including a light-emitting layer in the above organic light-emitting display device, a photopatterning process may be performed to form a sealing layer, a color filter, an insulating layer of a touch screen panel, etc. on the organic layer.
[0004] The post-heat treatment process in the above-mentioned photopatterning process is a process of applying heat to the pattern formed in the development process to finally harden it, and a low process temperature is required to prevent the organic layer from being damaged by heat.
[0005] Therefore, for photosensitive compositions that form sealing layers, color filters, and insulating layers of touch screen panels, the post-heat treatment process must be performed at a temperature of 100°C or lower. However, in the case of conventional photosensitive compositions, when the post-heat treatment process is performed at a temperature of 100°C or lower, there was a problem in that the stability of the patterns obtained after curing was low.
[0006] To overcome this, a photosensitive composition is required that not only enables sufficient photocuring during the exposure process during the photopatterning process, but also enables heat curing at low temperatures during the subsequent post-heat treatment process, thereby ensuring pattern stability.
[0007] Meanwhile, various structures are being proposed for flexible OLED displays to reduce their curvature, one of which is the non-polarized OLED display. While polarizing plates are essential for LCDs, they are used in OLEDs to improve visibility by preventing external light from reflecting off the panel.
[0008] Polarizers are composite films composed of multiple layers, and their thick thickness poses a challenge in reducing the curvature of flexible OLED displays. Furthermore, polarizers absorb 50-60% of the light emitted from the OLED, resulting in high power consumption. Furthermore, the high current required to generate higher-brightness light in the light-emitting layer also impacts the display's lifespan.
[0009] To address these shortcomings, non-polarized OLED displays, which eliminate polarizers, are attracting attention. Various technologies have been proposed to eliminate polarizers, but the most promising is the introduction of a color filter above the OLED's light-emitting layer to filter the color of light reflected internally.
[0010] However, when the polarizing plate is removed, there is a problem that the colorant used in the color filter is affected by external sunlight and exhibits different optical characteristics than the initial one, and there is a problem that the pattern must be formed at a low temperature so as not to affect the OLED light-emitting layer deposited underneath during the color filter formation process.
[0011] Meanwhile, in the case of planar layers (via layers), pixel definition layers, and color filters formed with photoresist compositions in organic light-emitting displays, as the pixel size of the organic light-emitting display device decreases, improvement in pattern resolution and reduction of residue have become important factors influencing performance.
[0012] Key factors for increasing resolution and reducing residue include the type and composition ratio of the photopolymerization initiator, photopolymerizable monomer, and binder resin, as well as the pigment dispersion composition. Among these factors, the pigment dispersion composition must have a small particle size to form fine patterns and must be composed of a composition that leaves no residue upon development. To reduce the particle size of the pigment dispersion composition, the primary particle size of the pigment used must be small, and the type and amount of the dispersant are also crucial.
[0013] Recently, the primary particle size of pigments mainly manufactured for electronic materials is manufactured to be around 50 nm, and the dispersed particle size can be further reduced after dispersion. In the case of dispersants, functional groups capable of adhering to the pigment surface are introduced, and the steric hindrance effect is used to control the gap between pigment particles at a certain level, thereby maintaining dispersion. Looking at the types of dispersants mentioned above, most are resins that can sufficiently impart steric hindrance, such as polyesters, acrylic resins, modified urethane resins, and polyethers.
[0014] Pigments with such small primary particle sizes can be finely dispersed using a dispersant that can adhere well to the pigment surface and disperse well between particles through steric hindrance. A pigment dispersion composition is prepared by using a dispersant that can reduce residue during development, and a photosensitive resin composition for color filters containing such a pigment dispersion composition can implement fine patterns during the production of color filters.
[0015] On the other hand, in the case of ionic dispersants containing ionic groups among the dispersants of pigment dispersions, there is a problem that the ionic groups may cause defects in the electrodes of organic light-emitting displays, and therefore, there is a recent demand for the development of pigment dispersions using dispersants that do not contain ionic groups.
[0016] In order to solve the problems of the above-mentioned prior art, one embodiment of the present invention comprises a novel photosensitive resin capable of photocuring and low-temperature heat curing; a dye having excellent light resistance that is not deformed by external sunlight and excellent chemical resistance that is not color-deformed by other solvents during a process even when molded at a low temperature; and / or silica particles having a reactive functional group introduced on the surface; and a photosensitive composition capable of finely dispersing a pigment, thereby providing a pattern or film having high resolution and stability by implementing a highly reliable curing pattern even in a low-temperature post-heat treatment process, and providing an organic light-emitting display device using the same.
[0017] The present invention provides a photosensitive composition comprising: an alkali-soluble resin; a reactive unsaturated compound; a photoinitiator; a reactive dye comprising a chromophore of the following chemical formula (3) and a protecting group of the following chemical formula (4); a solvent; and reactive silica particles comprising a structure represented by the following chemical formula (1).
[0018] Chemical formula (1)
[0019]
[0020] Chemical formula (3)
[0021]
[0022] Chemical formula (4)
[0023]
[0024] It is preferable that the above alkali-soluble resin includes a resin including a repeating unit represented by the following chemical formula (2).
[0025] Chemical formula (2)
[0026]
[0027] It is preferable that the above alkaline soluble resin includes a repeating unit represented by the following chemical formula (10) and a repeating unit represented by the following chemical formula (12).
[0028] Chemical formula (10) Chemical formula (12)
[0029]
[0030] It is preferable that the above alkaline soluble resin further includes a dispersant having a structure represented by the following chemical formula (21).
[0031] Chemical formula (21)
[0032]
[0033] As another specific example, the present invention provides a pattern or film formed from the photosensitive resin composition.
[0034] As another specific example, the present invention provides an organic light-emitting display device including the pattern or film.
[0035] As another specific example, the present invention provides an electronic device including the display device and a control unit for driving the display device.
[0036] The present invention manufactures a photosensitive composition using a dye having excellent light resistance that is not deformed by external sunlight and excellent chemical resistance that is not deformed by other solvents during the process even when molded at a low temperature, and silica particles having a reactive functional group introduced on the surface, thereby achieving high photosensitivity and enabling a highly reliable curing pattern to be implemented even in a low-temperature post-heat treatment process.
[0037] In addition, the present invention uses a photosensitive composition including a resin including repeating units represented by chemical formula (1) and chemical formula (2) to apply the photosensitive composition to at least one of a pixel separation section of an organic light-emitting device, a color filter, a flat layer, and an insulating film of a touch panel, thereby enabling low-temperature curing (100°C or less), thereby preventing damage to the organic device layer due to heat during the process.
[0038] In addition, the present invention can provide a pattern or film having high resolution, low outgassing, and stability in which the generation of residue is suppressed by using a photosensitive composition including a dispersant capable of finely dispersing a pigment.
[0039] Figure 1 conceptually illustrates a display device for implementing the present invention.
[0040] The present invention provides a photosensitive composition comprising: an alkali-soluble resin; a reactive unsaturated compound; a photoinitiator; a reactive dye comprising a chromophore of the following chemical formula (3) and a protecting group of the following chemical formula (4); a solvent; and reactive silica particles comprising a structure represented by the following chemical formula (1).
[0041] Chemical formula (1)
[0042]
[0043] Chemical formula (3)
[0044]
[0045] Chemical formula (4)
[0046]
[0047] Hereinafter, some embodiments of the present invention will be described in detail with reference to exemplary drawings. When assigning reference numerals to components in each drawing, identical components may be assigned the same numerals, as much as possible, even if they are depicted in different drawings.
[0048] When describing the present invention, detailed descriptions of related known components or functions may be omitted if they are deemed to obscure the gist of the present invention. When "includes," "has," and "consists of" are used in this specification, other parts may be added, unless "only" is used. When a component is expressed in the singular, it may also include plurals, unless otherwise explicitly stated.
[0049] Additionally, terms such as first, second, A, B, (a), (b), etc. may be used to describe components of the present invention. These terms are only intended to distinguish the components from other components, and the nature, order, sequence, or number of the components are not limited by these terms.
[0050] In a description of the positional relationship of components, when it is described that two or more components are "connected," "combined," or "connected," it should be understood that the two or more components may be directly "connected," "combined," or "connected," but that the two or more components may also be further "interposed" with another component to be "connected," "combined," or "connected." Here, the other component may be included in one or more of the two or more components that are "connected," "combined," or "connected" to each other.
[0051] Furthermore, when a component such as a layer, membrane, region, or plate is said to be "on" or "over" another component, it should be understood that this includes not only the case where it is "directly on" the other component, but also the case where there are other components in between. Conversely, when a component is said to be "directly on" another part, it should be understood that there are no other components in between.
[0052] In the description of the temporal flow relationship related to components, operation methods, or manufacturing methods, for example, when the temporal or flow relationship is described as “after”, “following”, “next to”, “before”, etc., it may also include cases where it is not continuous, unless “immediately” or “directly” is used.
[0053] Meanwhile, when numerical values or corresponding information for components are mentioned, even without separate explicit description, the numerical values or corresponding information may be interpreted as including an error range that may occur due to various factors (e.g., process factors, internal or external impact, noise, etc.).
[0054] The terms used in this specification and the appended claims have the following meanings, unless otherwise stated, without departing from the spirit of the present invention.
[0055] The term “halo” or “halogen” as used in this application includes fluorine (F), chlorine (Cl), bromine (Br), and iodine (I) unless otherwise stated.
[0056] The term "alkyl" or "alkyl group" as used in this application, unless otherwise stated, means a radical of a saturated aliphatic functional group having 1 to 60 carbon atoms connected by a single bond, including a straight-chain alkyl group, a branched-chain alkyl group, a cycloalkyl (alicyclic) group, an alkyl-substituted cycloalkyl group, and a cycloalkyl-substituted alkyl group.
[0057] The term “haloalkyl group” or “halogenalkyl group” as used in this application means an alkyl group substituted with a halogen, unless otherwise stated.
[0058] The term "alkenyl" or "alkynyl" as used in this application, unless otherwise stated, refers to a group having a double bond or a triple bond, including a straight or branched chain group, and having 2 to 60 carbon atoms, but is not limited thereto.
[0059] The term "cycloalkyl" as used in this application, unless otherwise stated, means, but is not limited to, an alkyl group forming a ring having 3 to 60 carbon atoms.
[0060] The term “alkoxy group” or “alkyloxy group” used in this application means an alkyl group to which an oxygen radical is bonded, and unless otherwise stated, has 1 to 60 carbon atoms, but is not limited thereto.
[0061] The term “alkenoxyl group,” “alkenoxy group,” “alkenyloxy group,” or “alkenyloxy group” as used in this application means an alkenyl group having an oxygen radical attached thereto, and unless otherwise stated, has from 2 to 60 carbon atoms, but is not limited thereto.
[0062] The terms "aryl group" and "arylene group" used in this application, unless otherwise stated, each have 6 to 60 carbon atoms, but are not limited thereto. The aryl group or arylene group in this application includes a single ring, a ring aggregate, a fused multiple ring compound, etc. For example, the aryl group may include a phenyl group, a monovalent functional group of biphenyl, a monovalent functional group of naphthalene, a fluorenyl group, a substituted fluorenyl group, and the arylene group may include a fluorenylene group, a substituted fluorenylene group.
[0063] The term "ring assemblies" as used herein means two or more ring systems (single ring or fused ring systems) directly connected to each other via single or double bonds, wherein the number of such direct links between rings is one less than the total number of ring systems in the compound. Ring assemblies may be formed by the same or different ring systems being directly connected to each other via single or double bonds.
[0064] In the present application, since the aryl group includes a ring aggregate, the aryl group includes biphenyl and terphenyl in which a single aromatic ring, a benzene ring, is connected by a single bond. In addition, the aryl group also includes a compound in which an aromatic single ring and an aromatic ring system fused together are connected by a single bond, and thus, for example, the aryl group also includes a compound in which an aromatic single ring, a benzene ring, and an aromatic ring system fused together, a fluorene ring, are connected by a single bond.
[0065] The term "fused multiple ring system" as used in this application means a fused ring structure sharing at least two atoms, and includes a structure in which two or more hydrocarbon ring systems are fused, and a structure in which at least one heterocyclic system containing at least one heteroatom is fused, etc. Such fused multiple ring systems may be aromatic rings, heteroaromatic rings, aliphatic rings, or a combination of these rings. For example, in the case of an aryl group, it may be a naphthalenyl group, a phenanthrenyl group, a fluorenyl group, etc., but is not limited thereto.
[0066] The term "spiro compound" used in this application has a "spiro union," which means a connection formed by two rings sharing only one atom. In this case, the atom shared between the two rings is called a "spiro atom," and depending on the number of spiro atoms contained in a compound, these are called "monospiro-," "dicepiro-," and "trispiro-" compounds, respectively.
[0067] As used herein, the terms "fluorenyl group", "fluorenylene group", and "fluorenetriyl group" mean, unless otherwise stated, a monovalent, divalent, or trivalent functional group in which R, R', R", and R'" in the following structures are all hydrogen, and a "substituted fluorenyl group", a "substituted fluorenylene group", or a "substituted fluorenetriyl group" means that at least one of the substituents R, R', R", and R'" is a substituent other than hydrogen, and includes a case where R and R' are bonded to each other to form a spiro compound together with the carbon to which they are bonded. In the present specification, regardless of the valence such as monovalent, divalent, or trivalent, a fluorenyl group, a fluorenylene group, and a fluorenetriyl group may all be referred to as a fluorene group.
[0068]
[0069] In addition, the R, R', R" and R'" can each independently be an alkyl group having 1 to 20 carbon atoms, an alkenyl group having 1 to 20 carbon atoms, an aryl group having 6 to 30 carbon atoms, or a heterocyclic group having 2 to 30 carbon atoms, for example, the aryl group can be phenyl, biphenyl, naphthalene, anthracene or phenanthrene, and the heterocyclic group can be pyrrole, furan, thiophene, pyrazole, imidazole, triazole, pyridine, pyrimidine, pyridazine, pyrazine, triazine, indole, benzofuran, quinazoline or quinoxaline. For example, the substituted fluorenyl group and fluorenylene group may be a monovalent functional group or a divalent functional group of 9,9-dimethylfluorene, 9,9-diphenylfluorene, and 9,9'-spirobi[9H-fluorene], respectively.
[0070] The term "heterocyclic group" used in this application includes not only aromatic rings such as "heteroaryl group" or "heteroarylene group" but also non-aromatic rings, and unless otherwise stated means a ring having 2 to 60 carbon atoms each containing one or more heteroatoms, but is not limited thereto. The term "heteroatom" used in this application represents N, O, S, P or Si unless otherwise stated, and the heterocyclic group means a monocyclic ring, ring aggregate, fused multiple ring system, spiro compound, etc. containing a heteroatom.
[0071] For example, “heterocyclic group” may also include compounds that contain heteroatom groups such as SO2, P=O, etc. instead of ring-forming carbon, as in the following compounds.
[0072]
[0073] The term "ring" as used in this application includes monocyclic and polycyclic rings, and includes hydrocarbon rings as well as heterocyclic rings containing at least one heteroatom, and includes aromatic and non-aromatic rings.
[0074] The term "polycyclic" as used in this application includes ring assemblies such as biphenyls, terphenyls, etc., fused multiple ring systems and spiro compounds, including aromatic as well as non-aromatic, and including hydrocarbon rings as well as heterocycles containing at least one heteroatom.
[0075] The term "aliphatic ring" used in this application refers to a cyclic hydrocarbon other than an aromatic hydrocarbon, and includes a single ring, a ring aggregate, a fused multiple ring system, a spiro compound, etc., and unless otherwise specified, refers to a ring having 3 to 60 carbon atoms, but is not limited thereto. For example, even if an aromatic ring, benzene, and a non-aromatic ring, cyclohexane, are fused, it is considered an aliphatic ring.
[0076] Also, when prefixes are named consecutively, it means that the substituents are listed in the order they were first written. For example, in the case of an arylalkoxy group, it means an alkoxy group substituted with an aryl group, in the case of an alkoxycarbonyl group, it means a carbonyl group substituted with an alkoxy group, and in the case of an arylcarbonylalkenyl group, it means an alkenyl group substituted with an arylcarbonyl group, where the arylcarbonyl group is a carbonyl group substituted with an aryl group.
[0077] Also, unless explicitly stated otherwise, the term "substituted" in the term "substituted or unsubstituted" used in this application means deuterium, halogen, amino group, nitrile group, nitro group, C1~C 30 Alkyl group of C1~C 30 Alkoxy group, C1~C 30 Alkylamine group of C1~C 30 Alkylthiophene group, C6~C 30 Arylthiophene group, C2~C 30 Alkenyl group, C2~C 30 Alkyne group, C3~C 30 Cycloalkyl group, C6~C 30 Aryl group of C6~C substituted with deuterium 30 Aryl group of C8~C 30 C2~C containing at least one heteroatom selected from the group consisting of arylalkenyl group, silane group, boron group, germanium group, and O, N, S, Si and P 30 It means that it is substituted with one or more substituents selected from the group consisting of heterocyclic groups, but is not limited to these substituents.
[0078] In this application, the 'functional group name' corresponding to the aryl group, arylene group, heterocyclic group, etc., which are exemplified as examples of each symbol and its substituent, may be described as the 'name of the functional group reflecting the valence', but may also be described as the 'name of the parent compound'. For example, in the case of 'phenanthrene', which is a type of aryl group, the name of the group may be described by distinguishing the valence, such as 'phenanthryl (group)' for the monovalent 'group' and 'phenantrylene (group)' for the divalent group, but the name of the parent compound, 'phenanthrene', may also be described regardless of the valence.
[0079] Similarly, in the case of pyrimidine, regardless of the valence, it can be written as 'pyrimidine', or in the case of monovalent, it can be written as pyrimidinyl (group), in the case of divalent, it can be written as the 'group name' of the corresponding valence, such as pyrimidinylene (group). Accordingly, in the present application, when the type of substituent is written as the name of the parent compound, it can mean an n-valent 'group' formed by the elimination of a hydrogen atom bonded to a carbon atom and / or heteroatom of the parent compound.
[0080] In addition, in this specification, numbers or alphabets indicating positions may be omitted when describing compound names or substituent names. For example, pyrido[4,3-d]pyrimidine may be described as pyridopyrimidine, benzofuro[2,3-d]pyrimidine as benzofuropyrimidine, 9,9-dimethyl-9H-fluorene as dimethylfluorene, etc. Accordingly, both benzo[g]quinoxaline and benzo[f]quinoxaline may be described as benzoquinoxaline.
[0081] Additionally, unless explicitly stated otherwise, the chemical formulas used in this application are applied in the same manner as the substituent definitions by the index definitions of the chemical formulas below.
[0082]
[0083] Here, if a is an integer of 0, the substituent R 1means that it is absent, that is, when a is 0, it means that all the carbons forming the benzene ring are bonded with hydrogen, and in this case, the indication of hydrogen bonded to carbon can be omitted and the chemical formula or compound can be described. In addition, when a is an integer of 1, one substituent R 1 It binds to one of the carbons forming the benzene ring, and when a is an integer of 2 or 3, it can bind as follows, for example, and when a is an integer of 4 to 6, it binds to the carbon of the benzene ring in a similar manner, and when a is an integer of 2 or more, R 1 may be the same or different.
[0084]
[0085] Unless otherwise stated in this application, forming a ring means that adjacent groups are bonded to each other to form a single ring or a fused multiple ring, and the single ring and the formed fused multiple ring include a hydrocarbon ring as well as a heterocycle containing at least one heteroatom, and may include aromatic and non-aromatic rings.
[0086] Additionally, unless otherwise stated herein, when indicating a condensed ring, the number in the expression "number-condensed ring" indicates the number of condensed rings. For example, a form in which three rings are condensed together, such as anthracene, phenanthrene, and benzoquinazoline, can be expressed as a 3-condensed ring.
[0087] Meanwhile, the term "bridged bicyclic compound" used in this application, unless otherwise specified, refers to a compound in which two rings share three or more atoms to form a ring. The shared atoms may include carbon or heteroatoms.
[0088] In the present application, the organic electric element may mean a component(s) between an anode and a cathode, or may mean an organic light-emitting diode including an anode and a cathode and a component(s) positioned therebetween.
[0089] In addition, in some cases, the display device in the present application may mean an organic electroluminescent element, an organic light-emitting diode, and a panel including the same, or may mean an electronic device including a panel and a circuit. Here, for example, the electronic device may include a lighting device, a solar cell, a portable or mobile terminal (e.g., a smart phone, a tablet, a PDA, an electronic dictionary, a PMP, etc.), a navigation terminal, a game machine, various TVs, various computer monitors, etc., and is not limited thereto, and may be any type of device as long as it includes the above-mentioned component(s).
[0090] Hereinafter, embodiments of the present invention will be described in detail. However, these are presented as examples and are not intended to limit the present invention. The present invention is defined solely by the scope of the claims set forth below.
[0091] A photosensitive resin composition according to one embodiment of the present invention comprises an alkali-soluble resin, a reactive unsaturated compound, a photoinitiator, and a solvent, and may further comprise a colorant in addition to the above components.
[0092] Each component is described in detail below.
[0093] (1) Alkali-soluble resin
[0094] A photosensitive resin composition according to one embodiment of the present invention comprises a copolymer resin including a repeating unit represented by the following chemical formula (10) and a repeating unit represented by the following chemical formula (12) as an alkali-soluble resin.
[0095] Chemical formula (10) Chemical formula (12)
[0096]
[0097] In the above chemical formula (10) and chemical formula (12),
[0098] 1) * indicates the part where the combination is connected as a repeating unit,
[0099] 2) R 1 and R 2 are independently hydrogen or C1~C 30 is an alkyl group,
[0100] 3) L 1 and L 2 are independently a single bond, fluorenylene group, C1~C 30 alkylene, C6~C 30 Arylene, C2~C 30 Heterocyclic ring or C1~C 30 is an alkoxylene,
[0101] 4) a and b are integers from 0 to 500, independently of each other.
[0102] 5) X 1 C2~C containing oxygen atoms 30 is a heterocycle,
[0103] 6) X 2 is the following chemical formula (12-1) or chemical formula (12-2),
[0104] Chemical Formula (12-1) Chemical Formula (12-2)
[0105]
[0106] In the above chemical formulas (12-1) and (12-2),
[0107] 6-1) * indicates the binding position,
[0108] 6-2) L 20 is a single bond or C1~C 30 is alkylene,
[0109] 6-3) R 4 is hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group,
[0110] 6-4) n is an integer from 1 to 10,
[0111] 7) The above R 1 , R 2 , R 4 , X 1 , X 2 , L 1 , L 2 and L 20 are respectively deuterium; halogen; C1~C 30 Alkyl group or C6~C 30 Silane group substituted or unsubstituted with an aryl group; siloxane group; boron group; germanium group; cyano group; amino group; nitro group; C1~C 30 Alkylthio group of; C1~C 30 Alkoxy group of; C6~C 30 Aryl alkoxy group of; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkyne group of; C6~C 30 Aryl group of; C6~C substituted with deuterium 30 Aryl group of; Fluorenyl group; C2~C containing at least one heteroatom selected from the group consisting of O, N, S, Si and P 30 Heterocyclic group of; C3~C 30 Aliphatic ring group; C7~C 30 Arylalkyl group of; C8~C 30 and combinations thereof, and may be further substituted with one or more substituents selected from the group consisting of arylalkenyl groups, and adjacent substituents may form a ring.
[0112] The above R 4 If it is an aryl group, preferably C6~C 30 Aryl group of, more preferably C6~C 18 The aryl group may be, for example, phenyl, biphenyl, naphthyl, terphenyl, etc.
[0113] Above X 1 , R 4 and L 1 ~L 2 In this case, it is preferably C2~C 30 A heterocyclic group, more preferably C2~C 18 The heterocyclic group may be, for example, dibenzofuran, dibenzothiophene, naphthobenzothiophene, naphthobenzofuran, etc.
[0114] The above R 4 When it is a fluorenyl group, it may preferably be 9,9-dimethyl-9H-fluorene, 9,9-diphenyl-9H-fluorenyl, 9,9'-spirobifluorene, etc.
[0115] Above L 1 ~L 2 If it is an arylene group, preferably C6~C 30 Arylene group, more preferably C6~C 18 It may be an arylene group, such as phenyl, biphenyl, naphthyl, terphenyl, etc.
[0116] The above R 1 ~R 2 and R 4 If it is an alkyl group, preferably C1~C 20 An alkyl group, more preferably C1~C 10 It can be an alkyl group, for example, methyl, t-butyl, etc.
[0117] The above R 4 If it is an alkoxyl group, preferably C1~C 20 Alkoxyl group of, more preferably C1~C 10 It may be an alkoxyl group, such as methoxy, t-butoxy, etc.
[0118] The above R 1 , R 2 , R 4 , X 1 , X 2 , L 1 , L 2 and L 20 The ring formed by the bonding of adjacent groups is C6~C 30 Aromatic ring group; Fluorenyl group; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; or C3~C 30 It may be an aliphatic ring group, for example, when adjacent groups are bonded to each other to form an aromatic ring, preferably C6~C 20 An aromatic ring, more preferably C6~C 14 It can form aromatic rings such as benzene, naphthalene, phenanthrene, etc.
[0119] Among the repeating unit structures represented by the above chemical formula (10), X 1 It is preferable that the structure includes an epoxide or oxetane moiety, and it is preferably one of the structures represented by the following chemical formulas (10-1) to (10-3).
[0120] Chemical Formula (10-1) Chemical Formula (10-2) Chemical Formula (10-3)
[0121]
[0122] Among the repeating unit structures represented by the above chemical formula (10), X 1 When the structure is one of the chemical formulas (10-1) to (10-3), cross-linking is formed between the resins during the post-heat treatment process during the photopatterning process, thereby increasing the stability of the pattern and improving the developability and resolution.
[0123] In the repeating unit structure represented by the above chemical formula (10) and the repeating unit structure represented by the chemical formula (12), R 1 and R2 It is preferred that they are independently hydrogen or methyl, with methyl being most preferred.
[0124] The above copolymer resin may further include a repeating unit represented by chemical formula (13) and a repeating unit represented by chemical formula (14) in addition to the repeating unit represented by chemical formula (10) and the repeating unit represented by chemical formula (12).
[0125] Chemical formula (13) Chemical formula (14)
[0126]
[0127] In the above chemical formula (13) and chemical formula (14),
[0128] 1) R 5 and R 6 are independently hydrogen or C1~C 20 is an alkyl group,
[0129] 2) L 3 is a single bond, fluorenylene group, C1~C 30 alkylene, C6~C 30 Arylene, C2~C 30 Heterocyclic ring or C1~C 30 is an alkoxylene,
[0130] 3) Ar 1 Silver C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 20 Alkyl group of; C3~C 30 Cycloalkyl group of; C2~C 20 Alkenyl group of; C2~C 20 Alkynyl group of; C1~C 20 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 20 is an alkoxycarbonyl group,
[0131] 4) c and d are independent integers from 1 to 500.
[0132] Among the repeating unit structures represented by the above chemical formula (13), Ar 1 Silver C6~C 30 Cycloalkyl group or C6~C 30 It is preferable that it is an aryl group, more preferably a structure represented by chemical formula (13-1) or chemical formula (13-2), and most preferably a structure represented by chemical formula (13-1).
[0133] Chemical formula (13-1) Chemical formula (13-2)
[0134]
[0135] The above Ar 1 When the structure is represented by this chemical formula (13-1) or chemical formula (13-2), the Tg of the copolymer resin has a value suitable for use as a composition for forming a color filter, pixel separation part, and flat layer of an organic light-emitting display device and an insulating film of a touch panel.
[0136] In particular, Ar 1 In the case of a structure represented by this chemical formula (13-1), it is unstable as a leaving group, so the bond between the ester moiety and the cyclohexyl moiety among the repeating units represented by chemical formula (13) is stable and not easily broken.
[0137] In the repeating unit structure represented by the above chemical formula (13) and the repeating unit structure represented by the chemical formula (14), R 5 and R 6 It is preferred that it is hydrogen or methyl independently of each other, and methyl is most preferred.
[0138] When the above copolymer resin includes all of the repeating units represented by chemical formulas (10) to (14), when the total repeating units of the copolymer resin are assumed to be 100 mol%, it is preferable that the repeating unit represented by chemical formula (10) is 5 to 20 mol%; the repeating unit represented by chemical formula (12) is 5 to 20 mol%; the repeating unit represented by chemical formula (13) is 20 to 50 mol%; and the repeating unit represented by chemical formula (14) is 20 to 50 mol%.
[0139] When a photopatterning process is performed using a photosensitive resin composition including a copolymer resin in which repeating units represented by the chemical formulas (10) to (14) are included in the above ratios, sufficient photocuring is performed in the exposure process, so that a high-resolution primary pattern is formed without residue or pattern tearing in the development process, and even if the post-heat treatment process is performed at 100°C or lower, thermal curing of the primary pattern is performed, so that a final pattern with high stability and improved resolution can be obtained.
[0140] The weight average molecular weight of the copolymer resin may be 1,000 to 100,000 g / mol, preferably 1,000 to 50,000 g / mol, and more preferably 1,000 to 30,000 g / mol. When the weight average molecular weight of the copolymer resin is within the above range, a pattern is formed well without residue during the manufacture of a pattern layer, and there is no loss of film thickness during development, and a good pattern can be obtained.
[0141] The total amount of the above copolymer resin may be comprised in an amount of 3 to 70 wt%, more preferably 10 to 40 wt%, based on the total amount of the photosensitive resin composition. When the above copolymer resin is comprised within the above range, excellent sensitivity, developability, and adhesiveness (adhesion) can be obtained.
[0142] A photosensitive resin composition according to one embodiment of the present invention may further include a copolymer resin as a first alkali-soluble resin, and a resin including a repeating unit represented by the following chemical formula (2) as a second alkali-soluble resin.
[0143] Chemical formula (2)
[0144]
[0145] In the above chemical formula (2),
[0146] 1) * indicates the part where the combination is connected as a repeating unit,
[0147] 2) n is an integer from 2 to 200,000,
[0148] 3) R 1 and R 2 are independently hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group,
[0149] 4) R 1 and R 2 Each adjacent tile can form a ring,
[0150] 5) a and b are independent integers from 0 to 4,
[0151] 6) X 1 is a single bond, O, CO, SO2, CR'R", SiR'R", chemical formula (A) or chemical formula (B),
[0152] 6-1) R' and R" are independently hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group,
[0153] 6-2) R' and R" can each form a ring with an adjacent tile, and examples of R' and R" combining with each other to form a ring are as follows.
[0154]
[0155] Chemical formula (A)
[0156]
[0157] Chemical formula (B)
[0158]
[0159] In the above chemical formula (A) and chemical formula (B),
[0160] 6-3) * indicates the binding position,
[0161] 6-4) X 3 is O, S, SO2 or NR',
[0162] 6-5) R' is hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group,
[0163] 6-6) R 3 ~R 6 are independently hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group,
[0164] 6-7) R 3 ~R 6 Each adjacent tile can form a ring,
[0165] 6-8) c~f are integers from 0 to 4, independently of each other,
[0166] 7) X 2 is a fluorenyl group; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 aryloxy group; or a combination thereof,
[0167] 8) A 1 and A 2 are independently of each other chemical formula (C) or chemical formula (D),
[0168] Chemical formula (C)
[0169]
[0170] Chemical formula (D)
[0171]
[0172] In the above chemical formula (C) and chemical formula (D),
[0173] 8-1) * indicates the binding position,
[0174] 8-2) R 7 ~R 10 are independently hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group,
[0175] 8-3) Y 1 and Y 2 are independently of each other chemical formula (E) or chemical formula (F),
[0176] Chemical formula (E)
[0177]
[0178] Chemical formula (F)
[0179]
[0180] 8-3-1) * indicates the bonding position,
[0181] 8-3-2) R 11 ~R 15 are independently hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group,
[0182] 8-3-3) L 1 ~L 3 are independently a single bond, fluorenylene group, C1~C 30 alkylene, C6~C 30 Arylene, C2~C 30 Heterocyclic ring or C1~C 30 is an alkoxylene,
[0183] 8-3-4) g and h are independent integers from 0 to 3; provided that g+h=3,
[0184] 9) In a resin containing a repeating unit represented by chemical formula (2), the ratio of chemical formula (C) and chemical formula (D) is 1:9 to 9:1,
[0185] 10) The above R 1 ~R 15 , R', R", X 2 and L 1 ~L 3 And the rings formed by combining adjacent groups are each composed of deuterium; halogen; C1~C 30 Alkyl group or C6~C 30Silane group substituted or unsubstituted with an aryl group; siloxane group; boron group; germanium group; cyano group; amino group; nitro group; C1~C 30 Alkylthio group of; C1~C 30 Alkoxy group of; C6~C 30 Aryl alkoxy group of; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkyne group of; C6~C 30 Aryl group of; C6~C substituted with deuterium 30 Aryl group of; Fluorenyl group; C2~C containing at least one heteroatom selected from the group consisting of O, N, S, Si and P 30 Heterocyclic group of; C3~C 30 Aliphatic ring group; C7~C 30 Arylalkyl group of; C8~C 30 and combinations thereof, and adjacent substituents may form a ring.
[0186] The above R 1 ~R 15 , R', R" and X 2 If it is an aryl group, preferably C6~C 30 Aryl group of, more preferably C6~C 18 The aryl group may be, for example, phenyl, biphenyl, naphthyl, terphenyl, etc.
[0187] The above R 1 ~R 15 , R', R" and X 2 If it is a heterocyclic group, preferably C2~C 30 A heterocyclic group, more preferably C2~C 18 The heterocyclic group may be, for example, dibenzofuran, dibenzothiophene, naphthobenzothiophene, naphthobenzofuran, etc.
[0188] The above R 1 ~R 15 , R', R" and X 2When it is a fluorenyl group, it may preferably be 9,9-dimethyl-9H-fluorene, 9,9-diphenyl-9H-fluorenyl, 9,9'-spirobifluorene, etc.
[0189] Above L 1 ~L 3 If it is an arylene group, preferably C6~C 30 Arylene group, more preferably C6~C 18 It may be an arylene group, such as phenyl, biphenyl, naphthyl, terphenyl, etc.
[0190] The above R 1 ~R 15 , when R' and R" are alkyl groups, preferably C1~C 20 An alkyl group, more preferably C1~C 10 It can be an alkyl group, for example, methyl, t-butyl, etc.
[0191] The above R 1 ~R 15 , when R' and R" are alkoxyl groups, preferably C1~C 20 Alkoxyl group of, more preferably C1~C 10 It may be an alkoxyl group, such as methoxy, t-butoxy, etc.
[0192] The above R 1 ~R 15 , R', R", X 2 and L 1 ~L 3 The ring formed by the bonding of adjacent groups is C6~C 30 Aromatic ring group; Fluorenyl group; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; or C3~C 30 It may be an aliphatic ring group, for example, when adjacent groups are bonded to each other to form an aromatic ring, preferably C6~C 20 An aromatic ring, more preferably C6~C 14It can form aromatic rings such as benzene, naphthalene, phenanthrene, etc.
[0193] When the main chain of the resin including the repeating unit represented by the above chemical formula (2) contains the structure represented by the chemical formula (C) and the structure represented by the chemical formula (D) in a ratio of 1:9 to 9:1, it has a relatively network structure compared to a resin including only one of the structures represented by the chemical formula (C) and the structure represented by the chemical formula (D), and due to its structural characteristics, it effectively forms intermolecular bonds with surrounding compounds, thereby improving the resolution of the pattern and reducing the amount of outgas generated.
[0194] The ratio of chemical formula (E) and chemical formula (F) within the polymer chain of the resin including the repeating unit represented by the above chemical formula (2) is preferably 2:0 to 1:1, and most preferably 1.5:0.5. If the ratio of chemical formula (F) is higher than that of chemical formula (E), residue may be generated due to excessively high adhesion, and the amount of outgassing may also increase significantly. When the ratio of chemical formula (E) and chemical formula (F) is 1.5:0.5, the resolution of the pattern is the best and the amount of outgassing is also satisfactory.
[0195] The weight average molecular weight of the resin including the repeating unit represented by the above chemical formula (2) may be 1,000 to 100,000 g / mol, preferably 1,000 to 50,000 g / mol, and more preferably 1,000 to 30,000 g / mol. When the weight average molecular weight of the resin is within the above range, the pattern is formed well without residue during the manufacture of the pattern layer, there is no loss of film thickness during development, and a good pattern can be obtained.
[0196] When the photosensitive resin composition includes a first alkali-soluble resin and a second alkali-soluble resin, the total amount of the first alkali-soluble resin and the second alkali-soluble resin may be included in an amount of 3 to 70 wt%, more preferably 10 to 40 wt%, based on the total amount of the photosensitive composition. When the resin is included within the above range, excellent sensitivity, developability, and adhesiveness (adhesion) can be obtained.
[0197] In addition, it is preferable that the weight ratio of the first alkali-soluble resin and the second alkali-soluble resin in the photosensitive resin composition is 7:3 to 3:7. When the two types of resins are included in the above ratio, the photosensitive composition undergoes thermal curing at a low temperature, and outgassing is reduced, showing a tendency for the accuracy and stability of the pattern to be improved.
[0198] The photosensitive resin composition of the present invention may further include an acrylic resin in addition to the first alkaline-soluble resin and the second alkaline-soluble resin. The acrylic resin is a copolymer of a first ethylenically unsaturated monomer and a second ethylenically unsaturated monomer copolymerizable therewith, and is a resin including one or more acrylic repeating units. The acrylic resin may be a copolymer of ethylenically unsaturated monomers including 2 to 10 kinds of acrylates and / or methacrylates, and may have a weight average molecular weight of 5,000 to 30,000 g / mol.
[0199] (2) Reactive unsaturated compounds
[0200] A photosensitive resin composition according to one embodiment of the present invention comprises a reactive unsaturated compound capable of being crosslinked by radicals in an exposure step.
[0201] The above reactive unsaturated compound has an ethylenically unsaturated double bond, and thus can sufficiently polymerize upon exposure to light in a pattern forming process to form a pattern with excellent heat resistance, light resistance, and chemical resistance.
[0202] Specific examples of the above reactive unsaturated compounds include ethylene glycol diacrylate, ethylene glycol dimethacrylate, diethylene glycol diacrylate, triethylene glycol diacrylate, triethylene glycol dimethacrylate, 1,6-hexanediol diacrylate, 1,6-hexanediol dimethacrylate, pentaerythritol triacrylate, dipentaerythritol pentaacrylate, dipentaerythritol hexaacrylate, bisphenol A epoxyacrylate, ethylene glycol monomethyl ether acrylate, trimethylolpropane triacrylate, tripentaerythritol octaacrylate, and the like.
[0203] Examples of commercially available products of the above reactive unsaturated compounds are as follows.
[0204] Examples of the bifunctional ester of the above (meth)acrylic acid include Aronix M-210, M-240, M-6200, etc. from Toagosei Chemical Industry Co., Ltd.; KAYARAD HDDA, HX-220, R-604, etc. from Nihon Kayaku Industry Co., Ltd.; and V-260, V-312, V-335 HP, etc. from Osaka Yuki Chemical Industry Co., Ltd.
[0205] Examples of the trifunctional ester of the above (meth)acrylic acid include Aronix M-309, M-400, M-405, M-450, M-7100, M-8030, M-8060, etc. from Toagosei Chemical Industry Co., Ltd.; KAYARAD TMPTA, DPCA-20, DPCA-60, DPCA-120, etc. from Nihon Kayaku Industry Co., Ltd.; and V-295, V-300, V-360, etc. from Osaka Yuki Kayaku Industry Co., Ltd.
[0206] The above products can be used alone or in combination of two or more.
[0207] The above reactive unsaturated compound may be used after being treated with an acid anhydride to provide better developability. The reactive unsaturated compound may be included in an amount of 1 to 50 wt%, for example, 5 to 30 wt%, based on the total amount of the photosensitive resin composition. When the reactive unsaturated compound is included within the above range, sufficient curing occurs upon exposure in the pattern forming process, resulting in excellent reliability. The pattern has excellent heat resistance, light resistance, and chemical resistance, and also excellent resolution and adhesion.
[0208] (3) Photoinitiator
[0209] A photosensitive resin composition according to one embodiment of the present invention may include the following photoinitiator, and an oxime ester compound may be used alone or in combination of two or more types as the photoinitiator.
[0210] The photoinitiator that can be used in combination with the above oxime ester compound is a photoinitiator used in a photosensitive resin composition, and examples thereof include acetophenone compounds, benzophenone compounds, thioxanthone compounds, benzoin compounds, and triazine compounds.
[0211] Examples of the above oxime compounds include 2-(o-benzoyloxime)-1-[4-(phenylthio)phenyl]-1,2-octanedione, 1-(o-acetyloxime)-1-[9-ethyl-6-(2-methylbenzoyl)-9H-carbazol-3-yl]ethanone, O-ethoxycarbonyl-α-oxyamino-1-phenylpropan-1-one, 2-dimethylamino-2-(4-methylbenzyl)-1-(4-morpholin-4-yl-phenyl)-butan-1-one, 1-(4-phenylsulfanylphenyl)-butane-1,2-dione2-oxime-O-benzoate, 1-(4-phenylsulfanylphenyl)-octane-1,2-dione2-oxime-O-benzoate, Examples thereof include 1-(4-phenylsulfanylphenyl)-octane-1-one oxime-O-acetate and 1-(4-phenylsulfanylphenyl)-butane-1-one oxime-O-acetate, 1-(4-methylsulfanyl-phenyl)-butane-1-one oxime-O-acetate, hydroxyimino-(4-methylsulfanyl-phenyl)-acetic acid ethyl ester-O-acetate, and hydroxyimino-(4-methylsulfanyl-phenyl)-acetic acid ethyl ester-O-benzoate.
[0212] Examples of the above acetophenone compounds include 2,2'-diethoxy acetophenone, 2,2'-dibutoxy acetophenone, 2-hydroxy-2-methylpropiophenone, pt-butyltrichloro acetophenone, pt-butyldichloro acetophenone, 4-chloro acetophenone, 2,2'-dichloro-4-phenoxy acetophenone, 2-methyl-1-(4-(methylthio)phenyl)-2-morpholinopropan-1-one, 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-butan-1-one, etc.
[0213] Examples of the above benzophenone compounds include benzophenone, benzoyl benzoate, methyl benzoyl benzoate, 4-phenyl benzophenone, hydroxy benzophenone, acrylated benzophenone, 4,4'-bis(dimethylamino)benzophenone, 4,4'-bis(diethylamino)benzophenone, 4,4'-dimethylaminobenzophenone, 4,4'-dichlorobenzophenone, 3,3'-dimethyl-2-methoxybenzophenone, etc.
[0214] Examples of the above thioxanthone compounds include thioxanthone, 2-chlorothioxanthone, 2-methylthioxanthone, isopropyl thioxanthone, 2,4-diethyl thioxanthone, 2,4-diisopropyl thioxanthone, 2-chlorothioxanthone, etc.
[0215] Examples of the above benzoin compounds include benzoin, benzoin methyl ether, benzoin ethyl ether, benzoin isopropyl ether, benzoin isobutyl ether, benzyldimethyl ketal, etc.
[0216] Examples of the above triazine compounds include 2,4,6-trichloro-s-triazine, 2-phenyl 4,6-bis(trichloromethyl)-s-triazine, 2-(3',4'-dimethoxystyryl)-4,6-bis(trichloromethyl)-s-triazine, 2-(4'-methoxynaphthyl)-4,6-bis(trichloromethyl)-s-triazine, 2-(p-methoxyphenyl)-4,6-bis(trichloromethyl)-s-triazine, 2-(p-tolyl)-4,6-bis(trichloromethyl)-s-triazine, 2-biphenyl 4,6-bis(trichloromethyl)-s-triazine, bis(trichloromethyl)-6-styryl-s-triazine, Examples include 2-(naphtho-1-yl)-4,6-bis(trichloromethyl)-s-triazine, 2-(4-methoxynaphtho-1-yl)-4,6-s(trichloromethyl)-s-triazine, 2-4-trichloromethyl(piperonyl)-6-triazine, and 2-4-trichloromethyl(4'-methoxystyryl)-6-triazine.
[0217] In addition to the above compound, the above photoinitiator may also include a carbazole compound, a diketone compound, a sulfonium borate compound, a diazo compound, an imidazole compound, a biimidazole compound, etc.
[0218] The above photoinitiator may be a radical polymerization initiator, such as a peroxide-based compound or an azobis-based compound.
[0219] Examples of the above photoperoxide compounds include ketone peroxides such as methyl ethyl ketone peroxide, methyl isobutyl ketone peroxide, cyclohexanone peroxide, methylcyclohexanone peroxide, and acetylacetone peroxide; diacyl peroxides such as isobutyryl peroxide, 2,4-dichlorobenzoyl peroxide, o-methylbenzoyl peroxide, and bis-3,5,5-trimethylhexanoyl peroxide; hydroperoxides such as 2,4,4,-trimethylpentyl-2-hydroperoxide, diisopropylbenzene hydroperoxide, cumene hydroperoxide, and t-butyl hydroperoxide; Dialkyl peroxides such as dicumyl peroxide, 2,5-dimethyl-2,5-di(t-butylperoxy)hexane, 1,3-bis(t-butyloxyisopropyl)benzene, and t-butylperoxyvaleric acid n-butyl ester; alkyl peresters such as 2,4,4-trimethylpentyl peroxyphenoxyacetate, α-cumyl peroxyneodecanoate, t-butyl peroxybenzoate, and di-t-butyl peroxytrimethyl adipate; Examples include percarbonates such as di-3-methoxybutyl peroxydicarbonate, di-2-ethylhexyl peroxydicarbonate, bis-4-t-butylcyclohexyl peroxydicarbonate, diisopropyl peroxydicarbonate, acetylcyclohexylsulfonyl peroxide, and t-butyl peroxyaryl carbonate.
[0220] Examples of the above azobis compounds include 1,1'-azobiscyclohexane-1-carbonitrile, 2,2'-azobis(2,4-dimethylvaleronitrile), 2,2, -azobis(methylisobutyrate), 2,2'-azobis(4-methoxy-2,4-dimethylvaleronitrile), α,α'-azobis(isobutylnitrile), and 4,4'-azobis(4-cyanovaleic acid).
[0221] The above photoinitiator may also be used together with a photosensitizer that causes a chemical reaction by absorbing light, becoming excited, and then transferring the energy. Examples of the photosensitizer include tetraethylene glycol bis-3-mercaptopropionate, pentaerythritol tetrakis-3-mercaptopropionate, and dipentaerythritol tetrakis-3-mercaptopropionate.
[0222] The photoinitiator may be included in an amount of 0.01 to 10 wt%, for example, 0.1 to 5 wt%, based on the total amount of the photosensitive resin composition. When the initiator is included within the above range, sufficient curing occurs upon exposure in the pattern forming process, thereby obtaining excellent reliability, and the pattern has excellent heat resistance, light resistance, and chemical resistance, and also excellent resolution and adhesion, and can prevent a decrease in transmittance due to unreacted initiator.
[0223] (4) Reactive dyes
[0224] A reactive dye according to one embodiment of the present invention is a chromophore-protecting group dye, which comprises a chromophore having a structure represented by the following chemical formula (3) and a protecting group surrounding the chromophore and having a structure represented by the following chemical formula (4).
[0225] Chemical formula (3)
[0226]
[0227] In the above chemical formula (3),
[0228] 1) L 1 ~L 4 are independently a single bond; fluorenylene group; C1~C 30 alkylene; C3~C 30 Cycloalkylene group of; C1~C 30 Alkoxylene group of; C2~C 30 Polyethyleneoxy group of; C6~C 30 Arylene group of; C2~C 30 a heterocycle; or a combination thereof,
[0229] 2) X 1 ~X 4 are independently hydrogen; deuterium; fluorenyl group; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group of; C3~C 30 cycloalkyl group of; or chemical formula (4-A),
[0230] 3) X 1 ~X 4 At least one of which is of chemical formula (4-A),
[0231] Chemical formula (4-A)
[0232]
[0233] 3-1) * is L 1 ~L 4 Or the part that is combined with N,
[0234] 3-2) p is an integer from 0 to 1,
[0235] 3-3) When chemical formula (4-A) is directly bonded to N, p is 0,
[0236] 3-4) R 13 and R 14 are independently hydrogen or methyl groups,
[0237] 4) X 5 ~X 12 are independently hydrogen; deuterium; halogen; fluorenyl group; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group of; C3~C 30 Cycloalkyl group of; or C1~C 30 is an alkylamine group,
[0238] 5) X 5 ~X 12 can combine with each other to form rings,
[0239] Chemical formula (4)
[0240]
[0241] In the above chemical formula (4),
[0242] 6) Z 1 and Z 2 are independently carbon atoms or nitrogen atoms,
[0243] 7) Y 1 ~Y 14 are independently hydrogen; deuterium; halogen; fluorenyl group; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group of; C3~C 30 Cycloalkyl group of; or C1~C 30 is an alkylamine group,
[0244] 8) Y 1 ~Y 14 can combine with each other to form rings,
[0245] 9) Above X1 ~X 14 , Y 1 ~X 14 , and L 1 ~L 4 are respectively deuterium; halogen; C1~C 30 Alkyl group or C6~C 30 Silane group substituted or unsubstituted with an aryl group; siloxane group; boron group; germanium group; cyano group; amino group; nitro group; C1~C 30 Alkylthio group of; C1~C 30 Alkoxy group of; C6~C 30 Aryl alkoxy group of; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkyne group of; C6~C 30 Aryl group of; C6~C substituted with deuterium 30 Aryl group of; Fluorenyl group; C2~C containing at least one heteroatom selected from the group consisting of O, N, S, Si and P 30 Heterocyclic group of; C3~C 30 Aliphatic ring group; C7~C 30 Arylalkyl group of; C8~C 30 and combinations thereof, and may be further substituted with one or more substituents selected from the group consisting of arylalkenyl groups, and adjacent substituents may form a ring.
[0246] In the structure represented by the above chemical formula (3), L 1 ~L 4 When the polyethyleneoxy group is a polyethyleneoxy group, the polyethyleneoxy group is preferably any group selected from the group consisting of a monoethyleneoxy group, a diethyleneoxy group, a triethyleneoxy group, a tetraethyleneoxy group, a pentaethyleneoxy group, a hexaethyleneoxy group, a heptaethyleneoxy group, an octaethyleneoxy group, a nonaethyleneoxy group, a decaethyleneoxy group, an undecaethyleneoxy group, a dodecaethyleneoxy group, a tridecaethyleneoxy group, a tetradecaethyleneoxy group, and a pentadecaethyleneoxy group.
[0247] In the structure represented by the above chemical formula (3), the above X 1 and X 2 At least one of them is of chemical formula (4-A), and X 3 and X 4 It is preferable that at least one of them is of chemical formula (4-A). More specifically, the above X 1 Inland X 4 In the middle chemical formula (4-A), the unsubstituted remainder is preferably one independently selected from the group consisting of an aryl group, an alkyl group, and a cycloalkyl group, and more preferably an aryl group. Most preferably, an alkyl group is substituted on the aryl group. The chromophore-protecting group dye of the present invention represented by the structure as described above can secure excellent light resistance.
[0248] The chromophore-protecting group dye according to one embodiment is preferable because it can secure the chemical resistance of the photosensitive composition including the chromophore-protecting group by introducing a bifunctional acrylate group at both terminals of the squalene dye. More specifically, it can secure compatibility and coloring power with other components of the photosensitive composition, i.e., an alkali-soluble resin and a reactive unsaturated compound described below, and can prevent precipitation of the chromophore-protecting group dye. That is, the chromophore-protecting group dye of the present invention has excellent light resistance and chemical resistance and exhibits characteristics suitable for a red or green dye of a color filter.
[0249] In the above chromophore-protecting group dye, the chromophore comprising the structure represented by the chemical formula (3) has three resonance structures as shown in Scheme 1 below. However, in the present specification, for convenience, the chromophore structure is represented by only one resonance structure. That is, the chromophore comprising the structure represented by the chemical formula (3) can be represented by any one of the three resonance structures below.
[0250] <Scheme 1>
[0251]
[0252] The chromophore comprising a structure represented by the above chemical formula (3) may have a maximum absorption peak at a wavelength of 520 nm to 680 nm. By using the chromophore-protecting group dye comprising the chromophore having the above spectral characteristics as a green or red dye, a photosensitive composition for a color filter having high brightness and excellent light resistance can be obtained.
[0253] A chromophore-protecting group dye according to one embodiment of the present invention has a structure comprising a chromophore and a protecting group surrounding the chromophore. The protecting group includes a structure represented by chemical formula (4). Specifically, the protecting group may be a macrocyclic compound, and the protecting group may form a coating layer by surrounding a chromophore including a structure represented by chemical formula (3).
[0254] In one embodiment, the protecting group corresponding to the macrocyclic compound has a structure surrounding a chromophore having a structure represented by the chemical formula (6), i.e., a structure in which a compound represented by the chemical formula (3) exists inside the macrocyclic compound, thereby improving the durability of the chromophore-protecting group dye, and thus, a color filter having excellent light resistance and chemical resistance can be implemented.
[0255] The cage width of the protecting group including the structure represented by the above chemical formula (4) may be 6.5 Å to 7.5 Å, and the volume of the protecting group may be 10 Å to 16 Å. In the present specification, the cage width refers to the internal length of the protecting group, and means the distance between the phenylene group 1 and the phenylene group 2 in the following schematic diagram 2 (see schematic diagram 2). When the protecting group has a cage width within the above range, a chromophore-protecting group dye having a structure surrounding a chromophore including the structure represented by the above chemical formula (3) can be obtained, and accordingly, when the chromophore-protecting group dye is added to a photosensitive composition, a color filter having excellent durability and high brightness can be implemented.
[0256] <Scheme 2>
[0257]
[0258] The above chromophore-protecting group dye may contain a chromophore having a structure represented by the above chemical formula (3) and a protecting group having a structure represented by the above chemical formula (4) in a molar ratio of 1:1. When the chromophore and the protecting group are present in the above molar ratio, a coating layer (protecting group) surrounding the chromophore can be well formed. The form in which the protecting group having a structure represented by the above chemical formula (4) surrounds the chromophore having a structure represented by the above chemical formula (3) is as shown in the following schematic diagram 3, and is a form in which a rod-shaped chromophore penetrates a ring-shaped protecting group.
[0259] <Diagram 3>
[0260]
[0261] The above chromophore-protecting group dye may be used alone as a red or green dye, or may be used in combination with a colorant dye, quantum dot, or pigment.
[0262] Examples of the above-mentioned coloring dyes include triarylmethane dyes, anthraquinone dyes, benzylidene dyes, cyanine dyes, phthalocyanine dyes, azaporphyrin dyes, indigo dyes, xanthene dyes, and pyridone azo dyes.
[0263] The photosensitive composition may contain the chromophore-protecting group dye in an amount of 0.1 wt% to 50 wt% based on the solid content excluding the solvent. For example, it may contain 0.1 wt% to 40 wt%, and preferably 0.5 wt% to 30 wt%. When the chromophore-protecting group dye is used within the above range, high brightness and contrast ratio can be exhibited at a desired color coordinate.
[0264] (5) Quantum dots
[0265] Additionally, the above chromophore-protecting group dye can be used in combination with quantum dots.
[0266] Quantum dots may have a core / shell structure, which is a multilayer structure comprising a core and a shell surrounding the core. Furthermore, quantum dots may have a core / multi-shell structure with two or more shells. For example, a core / shell / shell structure may be formed with a core and a double shell.
[0267] The core and shell of the quantum dot may be composed of a group II-VI compound, a group II-V compound, a group III-V compound, a group III-IV compound, a group III-VI compound, a group IV-VI compound, a group III-VI compound, a group I-III-VI compound, or a mixture thereof, and a dopant may be doped or alloyed into the core or shell of the quantum dot, and the compound constituting the core and the compound constituting the shell may be different from each other.
[0268] The above core may include one or more ternary compounds selected from InZnN, InZnP, InZnAs, InZnSb, InZnBi, GaZnN, GaZnP, GaZnAs, GaZnSb, GaZnBi, AlZnN, AlZnP, AlZnAs, AlZnSb, AlZnTi, CuGaS and AgGaS.
[0269] Additionally, the core may include one or more four-element compounds selected from InGaZnN, InGaZnP, InGaZnAs, InGaZnSb, InGaZnBi, InAlZnN, InAlZnP, InAlZnAs, InAlZnSb, InAlZnBi, GaAlZnN, GaAlZnP, GaAlZnAs, GaAlZnSb, GaAlZnBi, CuInGaS, and AgInGaS.
[0270] The above shell may be one or more selected from CdS, CdSe, CdTe, ZnS, ZnSe, ZnTe, ZnSeS, PbS, PbSe, PbSeS, PbTe, GaAs, GaP, InP, InGaP, InZnP, InAs, CuS, InN, GaN, InGaN, AlP, AlAs, InAs, GaAs, GaSb, InSb, AlSb, HgS, HgTe, HgCdTe, ZnCdS, ZnCdSe, CdSeTe, CuInSe2, CuInS2, AgInS2, SnTe, GaS and AgGaS.
[0271] The core / shell or core / multi-shell may further include a cluster molecule as a seed. The cluster molecule is a compound that acts as a seed during the process of manufacturing the core / shell or core / multi-shell, and the core / shell or core / multi-shell may be formed by precursors of compounds constituting the core / shell or core / multi-shell growing on the cluster molecule.
[0272] The above quantum dots may be a single layer rather than a multilayer structure (core / shell structure), and may be composed of only II-VI group compounds, for example.
[0273] The particle size of the quantum dots is preferably 1 nm to 30 nm, and most preferably 5 nm to 15 nm.
[0274] In addition, the quantum dot may additionally include a ligand. For example, the quantum dot may include an amine compound having an alkyl or alkenyl group having 6 to 30 carbon atoms, a (poly)ethyleneoxy group, an aryl group, a thiol compound, or a carboxylic acid compound as the ligand. Examples of amine compounds having an alkyl group include hexadecylamine or octylamine.
[0275] Other examples of the above ligands include phosphine compounds including trioctylphosphine, triphenolphosphine, t-butylphosphine, etc.; phosphine oxides such as trioctylphosphine oxide; pyridine or thiophene, etc.
[0276] The types of the above ligands are not limited to those exemplified above.
[0277] The ligand of the core-shell-ligand complex can prevent adjacent cores / shells or cores / multishells from aggregating and quenching with each other. The ligand binds to the core / shell or core / multishell and can have hydrophobic properties.
[0278] When the above chromophore-protecting group dye and quantum dots are mixed and used, they can be mixed and used in a weight ratio of 1:9 to 9:1, specifically, in a weight ratio of 3:7 to 7:3. When mixed in the above weight ratio range, high brightness and contrast ratio can be achieved while maintaining color characteristics.
[0279] (6) Colorant
[0280] The above chromophore-protecting group dye can also be used in combination with a pigment.
[0281] A photosensitive composition according to one embodiment of the present invention may include a pigment dispersion liquid including a pigment, a dispersant, and a dispersing binder resin.
[0282] The above pigments can be used as both organic and inorganic pigments.
[0283] The above pigments include red pigment, green pigment, blue pigment, yellow pigment, black pigment, etc.
[0284] The above pigments may be used alone or in combination of two or more, and are not limited to these examples.
[0285] Examples of the above red pigments include CI Red Pigment 254, CI Red Pigment 255, CI Red Pigment 264, CI Red Pigment 270, CI Red Pigment 272, CI Red Pigment 177, CI Red Pigment 89, etc.
[0286] Examples of the above green pigments include halogen-substituted copper phthalocyanine pigments such as CI Green Pigment 36, CI Green Pigment 7, etc.
[0287] Examples of the above blue pigments include copper phthalocyanine pigments such as CI blue pigment 15:6, CI blue pigment 15, CI blue pigment 15:1, CI blue pigment 15:2, CI blue pigment 15:3, CI blue pigment 15:4, CI blue pigment 15:5, CI blue pigment 16, etc.
[0288] Examples of the above yellow pigments include isoindoline pigments such as CI Yellow Pigment 139, quinophthalone pigments such as CI Yellow Pigment 138, and nickel complex pigments such as CI Yellow Pigment 150.
[0289] Examples of the above black pigments include benzofuranone black, lactam black, aniline black, perylene black, titanium black, carbon black, etc.
[0290] The above pigment may also be used after being pretreated with a water-soluble inorganic salt and a wetting agent. When the pigment is used after being pretreated as described above, the primary particle size of the pigment can be refined. The pretreatment may be performed through a step of kneading the pigment with a water-soluble inorganic salt and a wetting agent, and a step of filtering and washing the pigment obtained in the kneading step. The kneading may be performed at a temperature of 40°C to 100°C, and the filtration and washing may be performed by washing the inorganic salt with water or the like, followed by filtration.
[0291] Examples of the above water-soluble inorganic salts include, but are not limited to, sodium chloride and potassium chloride.
[0292] The above wetting agent acts as a medium that allows the pigment and the water-soluble inorganic salt to be uniformly mixed and the pigment to be easily pulverized, and examples thereof include alkylene glycol monoalkyl ethers such as ethylene glycol monoethyl ether, propylene glycol monomethyl ether, and diethylene glycol monomethyl ether; alcohols such as ethanol, isopropanol, butanol, hexanol, cyclohexanol, ethylene glycol, diethylene glycol, polyethylene glycol, and glycerin polyethylene glycol, and these may be used alone or in combination of two or more.
[0293] The pigment that has undergone the above-described kneading step may have an average particle diameter of 20 nm to 110 nm. When the average particle diameter of the pigment is within the above range, it can effectively form fine patterns while exhibiting excellent heat and light resistance.
[0294] The pigment that has gone through the above-mentioned kneading step can have an acid group introduced to the surface that can bind the dispersant through acid treatment.
[0295] The above dispersant interacts with the pigment and dispersion binder in the pigment dispersion liquid to connect the pigment and dispersion binder resin, thereby ensuring that the pigment dispersion is stably maintained.
[0296] The above dispersant is preferably a nonionic dispersant, which is preferable because it can suppress defects in the electrode when a composition pattern including the nonionic dispersant is formed in contact with the electrode of an organic light-emitting display device. In addition, nonionic dispersants have the advantage of excellent pattern stability due to low outgassing.
[0297] It is preferable that the above dispersant is a dispersant having a structure represented by the following chemical formula (21).
[0298] Chemical formula (21)
[0299]
[0300] In the above chemical formula (21),
[0301] 1) Ar 21 Silver C3~C 30 Aliphatic ring group; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; or a combination thereof,
[0302] 2) R 21 Silver C5~C 30 is an ethylene glycol chain group,
[0303] 3) R 22 and R 23 are independently of each other, hydrogen; deuterium; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C3~C 30 Aliphatic ring group; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; C1~C 30 an alkoxycarbonyl group; or a combination thereof,
[0304] 4) R 24 ~ R 26 are independently of each other, hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C3~C 30 Aliphatic ring group; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; C1~C 30 an alkoxycarbonyl group; or a combination thereof,
[0305] 5) L 21 , L 24 and L 25 are independently a single bond; fluorenylene group; C1~C 30 alkylene; C6~C 30 Arylene of; C2~C 30 Heterocyclic ring of; C1~C 30 an alkoxylene; or a combination thereof,
[0306] 6) d is an integer of 1 or 2,
[0307] 7) With respect to the total 100 mol% of the total repeating units included in the compound represented by the above chemical formula (21), a is 10 to 30 mol%, b is 40 to 60 mol%, and c is 20 to 40 mol%.
[0308] 8) The above Ar 21 , R 21 ~R 26 , L 21 , L 24 and L 25 are respectively deuterium; halogen; C1~C 30 Alkyl group or C6~C 30 Silane group substituted or unsubstituted with an aryl group; siloxane group; boron group; germanium group; cyano group; amino group; nitro group; C1~C 30 Alkylthio group of; C1~C 30 Alkoxy group of; C6~C 30 Aryl alkoxy group of; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkyne group of; C6~C 30 Aryl group of; C6~C substituted with deuterium 30Aryl group of; Fluorenyl group; C2~C containing at least one heteroatom selected from the group consisting of O, N, S, Si and P 30 Heterocyclic group of; C3~C 30 Aliphatic ring group; C7~C 30 Arylalkyl group of; C8~C 30 and combinations thereof, and adjacent substituents may form a ring.
[0309] The dispersant represented by the above chemical formula (21) is preferably represented by the following chemical formula (23) or chemical formula (24), and chemical formula (24) is more preferable.
[0310] The dispersant of the present invention containing a diamine side chain is preferable because it can more effectively finely disperse the pigment by forming strong ð-orbital stacking or hydrogen bonding with the acid group of the dispersion binder resin and the acid group of the acid-treated pigment.
[0311] Chemical formula (23)
[0312]
[0313] Chemical formula (24)
[0314]
[0315] In the above chemical formula (23) and chemical formula (24),
[0316] 1) Ar 21 , R 21 ~R 26 , L 21 , L 24 , L 25 and a~c are the same as defined in the above chemical formula (21),
[0317] 2) R 27 and R 28 are independently of each other, hydrogen; deuterium; halogen; C6~C 30Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C3~C 30 Aliphatic ring group; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; C1~C 30 an alkoxycarbonyl group; or a combination thereof.
[0318] In addition, in the compound represented by the above chemical formula (21), it is preferable that the amine side chain includes a urea moiety linking group. When the amine side chain of the dispersant including the structure represented by the above chemical formula (21) includes a urea moiety, the dispersibility of the pigment is improved due to the structural characteristics of the urea moiety. In addition, the group linked to the urea moiety is not broken during the post-heat treatment process, and thus, less outgassing is generated, which has the effect of improving the stability of the pattern.
[0319] It is preferable that a is 10 to 30 mol%, b is 40 to 60 mol%, and c is 20 to 40 mol%, based on 100 mol% of the total repeating units included in the compound represented by the above chemical formula (21). When a, b, and c are included in the above ratios, it is preferable because it exhibits high developability and heat resistance, while at the same time generating little outgassing and effectively dispersing pigments.
[0320] In the above chemical formula (21), Ar 21It is preferable that the compound represented by the chemical formula (21) contains 40 to 60 mol% of the repeating unit including the phenyl group based on 100 mol% of the total repeating units included in the compound represented by the chemical formula (21), high heat resistance and Tg can be secured, and the pigment dispersion can be prevented from exhibiting sticky characteristics like an adhesive due to the low Tg.
[0321] In the above chemical formula (21), R 21 It is preferable that the chain is an ethylene glycol group, and the ethylene glycol group means a chain-like substituent extended with an ethylene glycol moiety. If the chain is an ethylene glycol group having less than 5 carbon atoms, there is a problem of reduced developability, and if the chain is an ethylene glycol group having more than 20 carbon atoms, there is a problem of susceptibility to outgassing, so an ethylene glycol chain group having 5 to 20 carbon atoms is more preferable.
[0322] In the above chemical formula (21), the repeating unit containing a urea moiety and an amine group can increase pigment dispersibility as the content increases, but has the disadvantage of decreasing heat resistance due to the low Tg and increasing the amount of outgassing generated during the post-heat treatment process. Therefore, in the case of the repeating unit containing the urea moiety and an amine group, it is preferable to include 20 to 40 mol% based on the total 100 mol% of repeating units included in the compound represented by the above chemical formula (21), as described above.
[0323] It is preferable that the amine value of the dispersant including the structure represented by the above chemical formula (21) is 30 to 150 mgKOH / g.
[0324] The dispersant of the present invention represented by the above chemical formula (21) can effectively disperse pigments in an average particle size (D50) range of 90 nm to 110 nm, and is highly desirable because it produces less outgassing compared to the amount of dispersant used. In addition, the dispersant of the present invention represented by the above chemical formula (21) has the advantage of being able to produce high-resolution patterns by strongly binding to the acid group of the dispersant binder and being developed together with the dispersant binder resin during the developing process, and generating less residue compared to existing dispersants.
[0325] The dispersion binder resin connected to the pigment via the above dispersant creates a steric hindrance effect between the pigment particles, allowing the pigment particles to be dispersed at regular intervals. The dispersion binder resin may be an acrylic resin containing a carboxyl group, which is preferable because it can not only improve the stability of the pigment dispersion but also improve the developability and resolution of the pattern.
[0326] The pigment dispersion may further include a pigment, a binder resin, and a solvent in addition to a dispersant having a structure represented by the chemical formula (21), and it is preferable that the pigment dispersion include, for 100 parts by weight of the pigment dispersion, 1 to 30 parts by weight of the pigment; 1 to 10 parts by weight of the dispersant binder resin; 1 to 10 parts by weight of the dispersant having a structure represented by the chemical formula (21); and 20 to 80 parts by weight of the solvent.
[0327] When the above chromophore-protecting dye and the above pigment are mixed and used, they can be mixed and used in a weight ratio of 1:9 to 9:1, specifically, in a weight ratio of 3:7 to 7:3. In addition, when the above chromophore-protecting dye and the coloring dye are mixed and used, they can be mixed and used in a weight ratio of 1:9 to 9:1, specifically, in a weight ratio of 3:7 to 7:3, and when mixed in the above weight ratio range, it is possible to have high brightness and contrast ratio while maintaining color characteristics.
[0328] The above pigment dispersion may be included in an amount of 5 to 40 wt%, more specifically 8 to 30 wt%, based on the total amount of the photosensitive resin composition. When the pigment dispersion is included within the above range, the pattern has excellent curability and adhesion, and can sufficiently express a color according to the intended purpose.
[0329] The average particle size range (D50) of the pigment particles in the photosensitive resin composition is preferably 80 nm to 220 nm, and preferably 90 nm to 110 nm. When the average particle size range of the pigment particles in the photosensitive resin composition is within the range of 90 nm to 110 nm, the resolution of the pattern is excellent and the generation of residue is suppressed, which is preferable.
[0330] The half-width of the pigment particles represents the width from the highest point (n) of the particle size distribution graph to point n / 2. The smaller the value, the more uniform the pigment size and the more advantageous it is for pattern formation. The half-width range is 70 nm to 170 nm, and preferably 75 nm to 95 nm.
[0331] (7) Reactive silica particles
[0332] The above reactive silica particles are prepared by reacting a silane monomer having a functional group capable of reacting with a conventional silica particle and a photosensitive composition.
[0333] The above reactive silica particles can be manufactured by the following method. A method of first synthesizing silica particles with high mechanical strength and then introducing a certain amount of reactive functional groups onto the silica surface is a useful method for maintaining the advantages of silica particles while increasing compatibility with other reactive resins. There is a method of reacting a copolymer having a reactive functional group with a siloxane oligomer having a molecular weight of several hundred to several thousand to increase the particle size to several tens to several hundred nm, or a method of manufacturing particles by mixing a reactive functional group silane, a reactive organic substance, and a silane for silica production. However, there are problems in that the density of the silica particles themselves may decrease, which may lower the mechanical strength, and the reactive functional groups may not exist only on the silica surface, which may lower the reaction efficiency.
[0334] When manufacturing silica particles having the above reactive functional group introduced, the silica particles can be manufactured using commercially available products (Dupont's colloidal silica series) or by reacting silane raw materials such as water glass and alkoxy silane in an aqueous solution using a base catalyst, as in a conventional method. By adding a silane monomer having a reactive group to a solution in which the silica particles are dispersed, a condensation reaction with the hydroxyl group remaining on the surface of the silica particles can be carried out, thereby treating the surface of the particles with a reactive group. This is shown in the following reaction scheme 1.
[0335] <Reaction Scheme 1>
[0336]
[0337] After the above condensation reaction, a method of replacing the solvent with another solvent and reacting it using a method such as solvent replacement can be used as needed.
[0338] Examples of the solvent that can be used include alcohols such as methanol, ethanol, n-propanol, isopropanol, ethylene glycol, and propylene glycol; ketones such as acetone, methyl ethyl ketone, cyclohexanone, and n-methyl-2-pyrrolidone; aromatic hydrocarbons such as toluene, xylene, and tetramethylbenzene; glycol ethers such as cellosolve, methyl cellosolve, ethyl cellosolve, propylene glycol monomethyl ether, propylene glycol ethyl ether, dipropylene glycol monomethyl ether, and dipropylene glycol ethyl ether; acetates such as ethyl acetate, butyl acetate, methoxybutyl acetate, cellosolve acetate, ethyl cellosolve acetate, butyl cellosolve acetate, propylene glycol monomethyl ether acetate, and propylene glycol ethyl ether acetate;
[0339] When the surface of the above particles is treated with a reactor, more catalysts can be used.
[0340] The above catalyst is not particularly limited as long as it is an acid catalyst, and may be used inorganic acids such as hydrochloric acid, nitric acid, sulfuric acid, and phosphoric acid; monoacids such as formic acid and acetic acid; and organic acids including diacids such as oxalic acid, malonic acid, and succinic acid.
[0341] When the surface treatment reaction of the above silica particles does not have sufficient reactive hydroxyl groups on the surface of the silica particles, more water may be used.
[0342] There is no significant limitation on the amount of water used, but it can be used in an amount of 0.1 to 1 part by weight based on the weight of the silane monomer that undergoes surface treatment reaction.
[0343] After the above reaction is completed, any remaining water can be removed.
[0344] As a method for removing the above water, a conventional water removal method can be applied, and a method using a rotary evaporation device or an ultrafiltration membrane can be used.
[0345] The above silica particles preferably have an average particle size of 1 to 300 nm, more preferably 5 to 200 nm. In the case of the above average particle size, not only is compatibility with the photosensitive composition excellent, resulting in improved developability, but the formed film also has excellent transparency, excellent dispersibility of the silica particles, and is also economical in terms of cost.
[0346] It is preferable that the above silica particles exist in a stable state under acidic conditions of pH 7 or lower. If the above silica particles are unstable at pH 7 or lower and must be maintained above pH 7, there is a problem in that they react with acrylic acid in a typical photosensitive composition to form a salt, thereby reducing the acid value of the photosensitive composition and lowering the developability.
[0347] The above silane monomer is for treating the silica surface, and a silane monomer having a photocurable functional group and a silane monomer having a thermosetting functional group can be used.
[0348] The silane monomer having the above-mentioned photocurable functional group is not particularly limited as long as it is a silane monomer having an unsaturated functional group, and trimethoxysilylpropyl acrylate, triethoxysilylpropyl acrylate, trimethoxysilylpropyl methacrylate, triethoxysilylpropyl methacrylate, vinyltrimethoxysilane, vinyltriethoxysilane, allyltrimethoxysilane, or allyltriethoxysilane can be used.
[0349] The silane monomer having the above thermosetting functional group is a monomer having an epoxy isocyanate functional group, and examples thereof include, but are not limited to, glycidyloxypropyltrimethoxysilane, glycidyloxypropyltriethoxysilane, trimethoxysilylpropylisocyanate, or triethoxysilylpropylisocyanate.
[0350] The above silane monomer may include, but is not limited to, functional groups such as epoxy, (meth)acrylic, thiol, isocyanate, and amine groups.
[0351] The above reactive silane monomer is preferably used in an amount of 0.01 to 0.2 moles per mole of Si atoms in the silica particles. When used in the above amount, the functional groups are sufficient, resulting in excellent reactivity and developability with the resin and an effect of improving mechanical properties.
[0352] The above reactive silane monomer may not react during the surface treatment reaction of silica particles and may remain in an unreacted state. If the unreacted silane monomer compound exists in excess, problems such as deterioration of developability and mechanical properties may occur, and therefore it is preferable to remove it using an ultrafiltration membrane.
[0353] The reactive silica particles are preferably included in an amount of 0.1 to 20 wt% based on the total amount of the photosensitive composition, and when included in the above amount, the photosensitivity of the photosensitive composition is improved, the developability is excellent, and the mechanical properties are excellent. When the reactive silica particles are included in an amount of less than 0.1 wt% based on the total amount of the photosensitive composition, the effect of sufficiently increasing photosensitivity does not occur, and when the reactive silica particles are included in an amount of 20 wt% or more based on the total amount of the photosensitive composition, excessively high sensitivity may cause residue to be generated or resolution to be lowered during exposure of the photosensitive composition, which may be undesirable.
[0354] The above reactive silica particles can be contained solely in a photosensitive composition and reacted with a resin in the photosensitive composition during a photopatterning process, and can also be used as a copolymer by polymerizing with an alkali-soluble resin, which is a reactive resin of the photosensitive composition, in advance before the photopatterning process.
[0355] The above reactive silica particles may be added to the photosensitive composition after being mixed with the colorant, dispersant, resin, and organic solvent, or may be prepared as a dispersion alone and added to the photosensitive composition.
[0356] It is preferable that the reactive silica particles according to one embodiment of the present invention include a structure represented by chemical formula (1) on the surface.
[0357] Chemical formula (1)
[0358]
[0359] In the above chemical formula (1),
[0360] 1) R 21 is a single bond, fluorenylene group, C1~C 30 alkylene, C6~C 30 Arylene, C2~C 30 Heterocyclic ring or C1~C 30 is an alkoxylene,
[0361] 2) R 22 is C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group,
[0362] 3) n 1 is an integer from 1 to 3; n 2 is an integer from 0 to 2; n 1 + n 2 = 3,
[0363] 4) * is the part that connects to the silica particles,
[0364] 5) X 3 is one of the following chemical formulas a to e,
[0365] Chemical formula a Chemical formula b Chemical formula c Chemical formula d Chemical formula e
[0366]
[0367] 6) ** is Si or R 21 It is the part that connects to ,
[0368] 7) R 23 is hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group,
[0369] 8) The above R 21 ~R 23 and X 3 are respectively deuterium; halogen; C1~C 30 Alkyl group or C6~C 30 Silane group substituted or unsubstituted with an aryl group; siloxane group; boron group; germanium group; cyano group; amino group; nitro group; C1~C 30 Alkylthio group of; C1~C 30 Alkoxy group of; C6~C 30 Aryl alkoxy group of; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkyne group of; C6~C 30 Aryl group of; C6~C substituted with deuterium 30Aryl group of; Fluorenyl group; C2~C containing at least one heteroatom selected from the group consisting of O, N, S, Si and P 30 Heterocyclic group of; C3~C 30 Aliphatic ring group; C7~C 30 Arylalkyl group of; C8~C 30 and combinations thereof, and may be further substituted with one or more substituents selected from the group consisting of arylalkenyl groups, and adjacent substituents may form a ring.
[0370] When a structure represented by chemical formula (1) is substituted on the surface of reactive silica particles, the reactivity and developability with resin are excellent, and there is an effect of improving mechanical properties.
[0371] In addition, during the exposure step of the photopatterning process, the light incident on the photosensitive composition is scattered by the reactive silica particles, thereby further activating the photoinitiator. The photoinitiator further activated by the reactive silica particles increases the resolution and curing degree of the pattern, and also has the effect of reducing the amount of unreacted photoinitiator in the photosensitive composition, thereby reducing the amount of outgassing caused by the unreacted initiator. In addition, the photoinitiator exhibits a high curing rate even during thermal curing, thereby improving the reliability of the pattern.
[0372] As mentioned above, the photosensitive resin composition of the present invention preferably uses a reactive silica containing a structure represented by chemical formula (1) on the particle surface and an alkali-soluble resin containing a repeating unit of a structure represented by chemical formula (2). In this case, the reactive silica containing a structure represented by chemical formula (1) on the particle surface preferably contains a reactive functional group represented by chemical formulas a to e.
[0373] When the reactive silica containing the structure represented by the above chemical formula (1) on the particle surface includes a reactive functional group represented by the above chemical formula a or chemical formula b, the exposure sensitivity is improved in the photopatterning process (photolithography fixation) for forming a pattern, thereby improving the degree of curing, and since sufficient curing is performed in the exposure process, there is an advantage in that the stability of the pattern can be secured even if the subsequent post-heat treatment process is performed at a low temperature (100°C or less).
[0374] This effectively activates the photoinitiator by scattering the light incident on the inside of the photosensitive composition during the exposure process by silica particles, and the unsaturated double bond included in the reactive silica effectively forms a bond with the unsaturated double bond of the alkali-soluble resin and the reactive unsaturated compound including the repeating unit represented by the chemical formula (2).
[0375] When the reactive silica including the structure represented by the above chemical formula (1) on the particle surface includes the reactive functional group represented by the above chemical formulas c to e, the reactive functional group represented by the above chemical formulas c to e does not form a bond in the exposure process of the photopatterning process, and in the subsequent post-heat treatment process performed at a low temperature (100°C or less), the reactive functional group represented by the chemical formulas c to e of the reactive silica reacts with the carboxylic acid group of the alkali-soluble resin including the repeating unit of the structure represented by the above chemical formula (2) to form a cross-linking bond.
[0376] Therefore, even if the post-heat treatment process is carried out at a low temperature of 100°C or less, cross-linking is formed between the reactive silica and the alkali-soluble resin, thereby improving the degree of curing of the photosensitive composition and enhancing the stability of the pattern.
[0377] The structure represented by the chemical formula (1) substituted on the surface of the reactive silica particle may include a reactive functional group represented by the chemical formulas a to e, and one or more types of reactive functional groups may be included in one reactive silica particle. For example, the structure of the chemical formula (1) including the chemical formula a and the structure of the chemical formula (1) including the chemical formula c may be included simultaneously on the surface of one reactive silica particle, and the type of the reactive functional group included in the structure of the chemical formula (1) may also be selected in various ways depending on the type of alkali-soluble resin, pigment, reactive unsaturated compound, etc. used in the photosensitive composition.
[0378] (8) Solvent
[0379] The solvent may be a material that is compatible with, but does not react with, the alkali-soluble resin, the reactive unsaturated compound, the pigment, and the initiator.
[0380] Examples of the solvent include alcohols such as methanol and ethanol; ethers such as dichloroethyl ether, n-butyl ether, diisoamyl ether, methylphenyl ether, and tetrahydrofuran; glycol ethers such as ethylene glycol monomethyl ether and ethylene glycol monoethyl ether; cellosolve acetates such as methyl cellosolve acetate, ethyl cellosolve acetate, and diethyl cellosolve acetate; carbitols such as methylethyl carbitol, diethyl carbitol, diethylene glycol monomethyl ether, diethylene glycol monoethyl ether, diethylene glycol dimethyl ether, diethylene glycol methylethyl ether, and diethylene glycol diethyl ether; propylene glycol alkyl ether acetates such as propylene glycol methyl ether acetate and propylene glycol propyl ether acetate; aromatic hydrocarbons such as toluene and xylene; Ketones such as methyl ethyl ketone, cyclohexanone, 4-hydroxy-4-methyl-2-pentanone, methyl-n-propyl ketone, methyl-n-butyl ketone, methyl-n-amyl ketone, and 2-heptanone; Saturated aliphatic monocarboxylic acid alkyl esters such as ethyl acetate, n-butyl acetate, and isobutyl acetate; Lactic acid esters such as methyl lactate and ethyl lactate; Oxyacetic acid alkyl esters such as methyl oxyacetate, ethyl oxyacetate, and butyl oxyacetate; Alkoxyacetic acid alkyl esters such as methyl methoxyacetate, ethyl methoxyacetate, butyl methoxyacetate, methyl ethoxyacetate, and ethyl ethoxyacetate; 3-oxypropionic acid alkyl esters such as methyl 3-oxypropionate and ethyl 3-oxypropionate; 3-alkoxypropionic acid alkyl esters such as methyl 3-methoxypropionate, ethyl 3-methoxypropionate, ethyl 3-ethoxypropionate, and methyl 3-ethoxypropionate; 2-oxypropionic acid alkyl esters such as methyl 2-oxypropionate, ethyl 2-oxypropionate, and propyl 2-oxypropionate; 2-alkoxypropionic acid alkyl esters such as methyl 2-methoxypropionate, ethyl 2-methoxypropionate, ethyl 2-ethoxypropionate, and methyl 2-ethoxypropionate;2-oxy-2-methyl propionic acid esters such as methyl 2-oxy-2-methyl propionic acid, ethyl 2-oxy-2-methyl propionic acid, etc.; monooxy monocarboxylic acid alkyl esters of 2-alkoxy-2-methyl propionic acid alkyls such as methyl 2-methoxy-2-methyl propionic acid, ethyl 2-ethoxy-2-methyl propionic acid; esters such as ethyl 2-hydroxypropionic acid, ethyl 2-hydroxy-2-methyl propionic acid, ethyl hydroxyacetate, methyl 2-hydroxy-3-methyl butanoate; ketone acid esters such as ethyl pyruvate, etc.;
[0381] In addition, high boiling point solvents such as N-methylformamide, N,N-dimethylformamide, N-methylformanilide, N-methylacetamide, N,N-dimethylacetamide, N-methylpyrrolidone, dimethyl sulfoxide, benzyl ethyl ether, dihexyl ether, acetnylacetone, isophorone, caproic acid, caprylic acid, 1-octanol, 1-nonanol, benzyl alcohol, benzyl acetate, ethyl benzoate, diethyl oxalate, diethyl maleate, γ-butyrolactone, ethylene carbonate, propylene carbonate, and phenyl cellosolve acetate can also be used.
[0382] Among the above solvents, taking compatibility and reactivity into consideration, glycol ethers such as ethylene glycol monoethyl ether; ethylene glycol alkyl ether acetates such as ethyl cellosolve acetate; esters such as 2-hydroxypropionate ethyl; carbitols such as diethylene glycol monomethyl ether; and propylene glycol alkyl ether acetates such as propylene glycol methyl ether acetate and propylene glycol propyl ether acetate can be used.
[0383] The solvent may be included as a remainder based on the total amount of the photosensitive resin composition, and specifically, may be included at 50 to 90 wt%. When the solvent is included within the above range, the photosensitive resin composition has an appropriate viscosity, thereby providing excellent processability in the manufacture of a pattern layer.
[0384] (9) Other additives
[0385] The above photosensitive composition may further include additives such as malonic acid; 3-amino-1,2-propanediol; a silane coupling agent containing a vinyl group or a (meth)acryloxy group; a leveling agent; a fluorinated surfactant; and a radical polymerization initiator to prevent stains or spots during application, improve leveling performance, and prevent the formation of residues due to non-development.
[0386] For example, the photosensitive resin composition may further include a silane coupling agent having a reactive substituent such as a vinyl group, a carboxyl group, a methacryloxy group, an isocyanate group, or an epoxy group to improve adhesion to a substrate, etc.
[0387] Examples of the above silane coupling agent include trimethoxysilyl benzoic acid, γ-methacryl oxypropyl trimethoxysilane, vinyl triacetoxysilane, vinyl trimethoxysilane, γ-isocyanate propyl triethoxysilane, γ-glycidoxy propyl trimethoxy silane, β-epoxy cyclohexyl ethyl trimethoxysilane, etc., and these may be used alone or in combination of two or more.
[0388] The above silane coupling agent may be included in an amount of 0.01 to 10 parts by weight based on 100 parts by weight of the photosensitive resin composition. When the silane coupling agent is included within the above range, adhesion, storability, etc. are excellent.
[0389] In addition, the photosensitive resin composition may further include a surfactant, such as a fluorinated surfactant, to improve coating properties and prevent defects, if necessary.
[0390] As the above fluorinated surfactant, BM Chemie's BM-1000 ® , BM-1100 ® Mecha Pack F 142D by Dai Nippon Inki Kagaku Kogyo Co., Ltd. ® , East F 172 ® , East F 173 ® , East F 183® Back; Prorad FC-135 from Sumitomo 3M Co., Ltd. ® , East FC-170C ® , East FC-430 ® , East FC-431 ® Saffron S-112 from Asahi Glass Co., Ltd. ® , East S-113 ® , East S-131 ® , East S-141 ® , East S145 ® SH-28PA from Toray Silicone Co., Ltd. ® , East-190 ® , East-193 ® , SZ-6032 ® , SF-8428 ® Fluorinated surfactants sold under the names of etc. can be used.
[0391] The above surfactant may be used in an amount of 0.001 to 5 parts by weight per 100 parts by weight of the photosensitive resin composition. When the surfactant is included within the above range, coating uniformity is ensured, staining does not occur, and wetting on a glass substrate is excellent. In addition, other additives such as antioxidants and stabilizers may be added in a certain amount to the photosensitive resin composition within a range that does not impair the physical properties.
[0392] Another embodiment of the present invention provides a color filter manufactured using the photosensitive composition described above. The method for manufacturing the color filter is as follows.
[0393] <Color filter formation process>
[0394] The photosensitive resin composition described above is applied to a glass substrate that is not coated with anything, or to a glass substrate on which a protective film, SiNx, is applied to a thickness of 500 Å to 1500 Å, using an appropriate method such as spin coating or slit coating, to a thickness of 3.1 µm to 3.4 µm. After coating, light is irradiated to form a pattern required for the color filter. After irradiating with light, the coated layer is treated with an alkaline developer, so that the unirradiated portion of the coated layer is dissolved and the pattern required for the color filter is formed. By repeating this process according to the number of required R, G, and B colors, a color filter having a desired pattern can be obtained. In the above process, the image pattern obtained by development can be further improved by heating it again or curing it by irradiating it with active rays, etc., to further improve crack resistance, solvent resistance, etc.
[0395] Another embodiment of the present invention can provide an organic light-emitting display device.
[0396] Hereinafter, referring to FIG. 1, an organic light-emitting display device will be described. An organic light-emitting display device according to an embodiment of the present invention includes a substrate (1), a TFT layer (2) on the substrate, a flattening layer (3) on the TFT layer, an organic light-emitting element layer on the flattening layer, a sealing layer (8) disposed on the organic light-emitting element layer, a touch panel (9) disposed on the sealing layer, and a color filter disposed on the touch panel, wherein at least one of the flattening layer, the organic light-emitting element layer, the sealing layer, the touch panel, and the color filter includes a pattern or film formed from the photosensitive resin composition of the present invention.
[0397] The above pattern or film is formed of a photosensitive composition containing, as essential components, reactive silica particles having a structure represented by the above chemical formula (1) on the particle surface, a resin having a repeating unit represented by the above chemical formula (2) as a main component, and the above chromophore-protecting group dye including a chromophore having a structure represented by the above chemical formula (3) and a protecting group having a structure represented by the above chemical formula (4).
[0398] The above substrate (1) may be a flexible substrate. The substrate may be made of a plastic having excellent heat resistance and durability, such as polyimide (PI), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polycarbonate (PC), polyarylate (PAR), polyetherimide (PEI), and polyethersulfone (PES).
[0399] However, the present invention is not limited thereto, and various flexible materials such as metal foil or thin glass may be used. Meanwhile, the substrate may be a rigid substrate, and in this case, the substrate may be made of a glass material with SiO2 as its main component.
[0400] In the case of a bottom emission type in which an image is implemented in the direction of the substrate, the substrate must be formed of a transparent material. However, in the case of a top emission type in which an image is implemented in the opposite direction of the substrate, the substrate does not necessarily need to be formed of a transparent material. In this case, the substrate may be formed of a metal. In the case of forming the substrate of a metal, the substrate may include, but is not limited to, one or more selected from the group consisting of carbon, iron, chromium, manganese, nickel, titanium, molybdenum, and stainless steel (SUS).
[0401] A TFT layer (2) may be arranged on the above substrate. The term TFT layer mentioned in this specification refers to a thin film transistor (TFT) array for driving an organic light-emitting element, and means a driving part for displaying an image. In Fig. 1, only an organic light-emitting element and a driving thin film transistor for driving the organic light-emitting element are illustrated, but this is only for the convenience of explanation, and the present invention is not limited to what is illustrated, and it is obvious to those skilled in the art that a plurality of thin film transistors, storage capacitors, and various types of wiring may be further included.
[0402] The TFT layer may be covered and protected by a planarization layer (3). The planarization layer may include an inorganic insulating film and / or an organic insulating film. Examples of inorganic insulating films that may be used in the planarization layer include silicon oxide (SiO2), silicon nitride (SiN). x ), silicon oxynitride (SiON), aluminum oxide (Al2O3), titanium oxide (TiO2), tantalum oxide (Ta2O5), hafnium oxide (HfO2), zirconium oxide (ZrO2), barium strontium titanate (BST), lead zirconate-titanate (PZT), etc.
[0403] In addition, examples of organic insulating films that can be used in the flat layer may include general-purpose polymers (PMMA, PS), polymer derivatives having phenolic groups, acrylic polymers, imide polymers, aryl ether polymers, amide polymers, fluorinated polymers, p-xylene polymers, vinyl alcohol polymers, and blends thereof.
[0404] Meanwhile, the flattening layer may have a composite laminated structure of an inorganic insulating film and an organic insulating film. Furthermore, the flattening layer may include the photosensitive composition of the present invention. Details regarding the photosensitive composition of the present invention are identical to those described in the aforementioned embodiment of the present invention, and therefore will be omitted.
[0405] When a flat layer is formed using the photosensitive composition of the present invention, the insulating performance can be improved by the reactive silica particles included in the photosensitive composition of the present invention, and a high taper angle of 43° or more can be formed to protect the TFT layer and easily form a pixel electrode connected to the TFT.
[0406] An organic light-emitting element layer may be formed on the above-mentioned flat layer. The organic light-emitting element layer may include a pixel electrode (4) formed on the flat layer, a counter electrode (7) arranged to face the pixel electrode, and an organic layer (6) interposed therebetween. When a voltage is applied between the pixel electrode and the counter electrode, the organic layer may emit light. The organic layer may emit red light, green light, blue light, or white light. In order to express a color image when the organic layer emits white light, or in order to increase color purity and light efficiency when the organic layer emits red light, green light, or blue light, the organic light-emitting display device may further include blue, green, and red color filters.
[0407] Organic light-emitting displays can be classified into bottom emission types, top emission types, and dual emission types depending on the light-emitting direction. In a bottom emission type organic light-emitting display, the pixel electrode is provided as a light-transmitting electrode and the opposite electrode is provided as a reflective electrode. In a top emission type organic light-emitting display, the pixel electrode is provided as a reflective electrode and the opposite electrode is provided as a transflective electrode. In the present invention, the top emission type in which the organic light-emitting element emits light in the direction of the sealing layer is described as the basis.
[0408] The pixel electrode may be a reflective electrode. The pixel electrode may include a laminated structure of a reflective layer and a transparent or semitransparent electrode layer having a high work function. The reflective layer may include Ag, Mg, Al, Pt, Pd, Au, Ni, Nd, Ir, Cr or an alloy thereof. The transparent or semitransparent electrode layer may include at least one material selected from transparent conductive oxide materials such as indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO), indium oxide (In2O3), indium gallium oxide (IGO), and aluminum zinc oxide (AZO).
[0409] The pixel electrode can be patterned and formed in an island shape corresponding to each pixel.
[0410] Additionally, the pixel electrode can function as an anode electrode.
[0411] Meanwhile, a pixel definition film (5) may be disposed on the pixel electrode, which includes a predetermined opening that covers the edge of the pixel electrode and exposes the center of the pixel electrode. An organic layer including an organic light-emitting layer that emits light may be disposed on the area defined by the opening. The area where the organic layer is disposed may be defined as a light-emitting area.
[0412] Meanwhile, when forming a light-emitting region within the opening of the pixel-defining film, a region protruding by the pixel-defining film is arranged between the light-emitting regions, and since no organic light-emitting layer is formed in this protruding region, it can be defined as a non-light-emitting region. The pixel-defining film may include the photosensitive composition of the present invention. Since the details regarding the photosensitive composition of the present invention are the same as those according to the above-described embodiment of the present invention, they will be omitted.
[0413] When a pixel defining film is formed using the photosensitive composition of the present invention, the resolution of the pixel defining film pattern is improved and outgassing is reduced.
[0414] In addition, the photosensitive composition of the present invention may include a black pigment or dye, and when a pixel definition film is formed with the photosensitive composition of the present invention including a black pigment or dye, there is an effect of improving the visibility of the organic light-emitting display device by absorbing light incident from the outside.
[0415] The counter electrode may be formed as a transparent electrode. The counter electrode may be a semi-permeable film formed by forming a thin film of a metal having a low work function, such as Li, Ca, LiF / Ca, LiF / Al, Al, Mg, or Ag. To compensate for the high resistance problem of the thin metal semi-permeable film, a transparent conductive film made of a transparent conductive oxide may be laminated on the metal semi-permeable film. The counter electrode may be formed over the entire surface of the substrate in the form of a common electrode. In addition, such a counter electrode may function as a cathode electrode.
[0416] The polarities of the pixel electrode and the counter electrode as described above may be opposite to each other.
[0417] The organic layer includes an organic light-emitting layer that emits light, and the organic light-emitting layer may use a low-molecular organic material or a high-molecular organic material. When the organic light-emitting layer is a low-molecular organic layer formed of a low-molecular organic material, a hole transport layer (HTL) and a hole injection layer (HIL) may be arranged in the direction of the pixel electrode with the organic light-emitting layer as the center, and an electron transport layer (ETL) and an electron injection layer (EIL) may be arranged in the direction of the opposite electrode. Of course, other functional layers may be stacked in addition to the hole injection layer, hole transport layer, electron transport layer, and electron injection layer.
[0418] A sealing layer (8) may be disposed on the organic light-emitting element layer to cover the organic light-emitting element layer. The organic light-emitting element included in the organic light-emitting element layer is composed of organic materials and can be easily deteriorated by external moisture or oxygen. Therefore, the organic light-emitting element layer must be sealed to protect the organic light-emitting element. The sealing layer may have a structure in which a plurality of inorganic films and a plurality of organic films are alternately laminated as a means for sealing the organic light-emitting element layer.
[0419] In the organic light-emitting display device of the present embodiment, it is preferable to form a sealing layer by using a thin film in which a plurality of inorganic films and a plurality of organic films are alternately laminated rather than a sealing substrate, and by using a thin film as a sealing means, it is possible to easily implement flexibility and thinning of the organic light-emitting display device.
[0420] The sealing layer may include a plurality of inorganic films and a plurality of organic films. The inorganic films and the organic films may be alternately laminated.
[0421] The inorganic films may be formed of metal oxides, metal nitrides, metal carbides, or combinations thereof. For example, the inorganic films may be formed of aluminum oxide, silicon oxide, or silicon nitride. In another example, the inorganic films may include a laminated structure of multiple inorganic insulating layers. The inorganic films may function to inhibit external moisture and / or oxygen from penetrating into the organic light-emitting element layer.
[0422] The organic films may be polymeric organic compounds. For example, the organic films may include any one of epoxy, acrylate, or urethane acrylate. The organic films may function to relieve internal stress in the inorganic films, or to compensate for defects and smooth the inorganic films.
[0423] The order of lamination of the inorganic and organic films constituting the above sealing layer is not limited, and an organic film or an inorganic film may be laminated on the organic light-emitting element layer, and the uppermost layer of the sealing layer may also be an organic film or an inorganic film.
[0424] A touch panel (9) may be formed on the sealing layer. The touch panel may include a first touch electrode formed on the sealing layer, a second touch electrode positioned opposite thereto, and an insulating layer interposed therebetween.
[0425] The first touch electrode and the second touch electrode may be formed in a grid pattern or a specific pattern shape. The first touch electrode may be formed in contact with the upper portion of the sealing layer, and an inorganic layer may be additionally provided between the sealing layer and the first touch electrode.
[0426] The above first touch electrode and second touch electrode may be formed of ITO or a metal mesh, and are preferably formed of a metal mesh.
[0427] Metal mesh is an electrode manufactured by printing opaque metals (copper, silver, gold, aluminum, etc.) in a grid shape with a thickness of 1 to 7 ㎛. Since it uses highly conductive metal, it has a very low resistance value, which allows for a fast touch response speed, facilitates implementation of large screens, and has the advantage of being cheaper than ITO film. In addition, metal mesh electrodes have superior durability against repeated bending compared to ITO electrodes, making them suitable for use as touch panel electrodes for foldable displays.
[0428] The above insulating layer can be formed using the photosensitive composition of the present invention. Details regarding the photosensitive composition of the present invention are the same as those described above in accordance with one embodiment of the present invention, and therefore will be omitted.
[0429] When an insulating layer is formed using the photosensitive composition of the present invention, an insulating layer having a very low dielectric constant is formed by the reactive silica particles included in the photosensitive composition, so that a touch panel with improved response speed and accuracy can be manufactured.
[0430] In addition, since the photosensitive composition of the present invention is subjected to a post-heat treatment process at 100°C or lower during the photopatterning process, it is possible to form an insulating layer of a touch panel without causing heat damage to the organic material layer of the organic light-emitting element layer.
[0431] It is preferable that the above touch panel be a capacitive touch panel that uses the capacitance of the human body when a user touches it to recognize a part where the amount of current has changed, calculate the size, and detect the location.
[0432] It is obvious to those skilled in the art that the organic light-emitting display device of the present invention is not limited to what is shown, and may further include a Control IC that converts an analog signal transmitted from a touch panel into a digital signal and controls coordinate values necessary for determining the coordinates of a touch area, an optically transparent adhesive, a flexible printed circuit board (FPCB) on which conductive and signal line patterns are formed to transmit various signals to electronic components, and other various electronic components and various wirings.
[0433] A color filter may be formed on the touch panel. The color filter may be positioned on the upper portion of the touch panel and may include a color portion (10) aligned vertically with the light-emitting region of the organic light-emitting element layer and a color separation portion (11) aligned vertically with the non-light-emitting region and separating the color portion.
[0434] The photosensitive composition of the present invention can be included in the color portion to narrow the wavelength range of light emitted from the light-emitting region, thereby improving the color purity of the organic light-emitting display device.
[0435] In addition, the photosensitive composition of the present invention can be included in a color separation unit to absorb and block external light incident on an organic light-emitting display device, thereby improving outdoor visibility.
[0436] The photosensitive composition of the present invention can form a red color portion aligned in a vertical direction with a red light-emitting region by containing the chromophore-protecting group dye alone or by containing the chromophore-protecting group dye and a red pigment or red dye together.
[0437] The photosensitive composition of the present invention can form a green color portion aligned in a vertical direction with a green light-emitting region by containing the chromophore-protecting dye alone or by containing the chromophore-protecting dye together with a green pigment or green dye.
[0438] The photosensitive composition of the present invention can form a blue color portion aligned in a vertical direction with a blue light-emitting region by containing the chromophore-protecting group dye alone or by containing the chromophore-protecting group dye together with a blue pigment or blue dye.
[0439] The photosensitive composition of the present invention can form a color separation portion aligned in a vertical direction with the pixel defining film by containing the chromophore-protecting group dye alone or by containing the chromophore-protecting group dye and a black pigment or a black dye together, and carbon black is preferable as the black pigment.
[0440] When the photosensitive composition of the present invention is used to form a color portion of a color filter, particularly a red color portion or a green color portion, the color purity is excellent and the light resistance to sunlight is also improved, which is highly desirable. In addition, when the photosensitive composition of the present invention is used to form a color separation portion of a color filter, not only light resistance to sunlight can be secured, but also chemical resistance essential for solution processing can be secured, which is highly desirable.
[0441] When the photosensitive composition of the present invention is used to form a color portion or a color separation portion of a color filter, a color filter having a low amount of outgassing and a fine-sized pattern can be formed, thereby enabling the manufacture of a high-resolution color filter.
[0442] In addition, since the photosensitive composition of the present invention has sufficient photosensitivity in the exposure process during the photopatterning process and the post-heat treatment process is performed at 100°C or lower, the color filter formation process can be performed without causing heat damage to the organic material layer of the organic light-emitting element layer.
[0443] It is obvious to those skilled in the art that the positions of each layer in the structure of the organic light-emitting display device described above are not limited, and that multiple functional layers with specific purposes and functions can be additionally arranged between each layer, and the organic light-emitting display device of the present invention is not limited to the structure and drawings described above.
[0444] Hereinafter, synthetic examples and examples according to the present invention are specifically described, but the synthetic examples and examples of the present invention are not limited thereto.
[0445] Synthesis example (synthesis of the first binder resin)
[0446] Synthesis Examples 1-1 to 1-5
[0447] (Synthesis of Binder 1-1 to 1-5)
[0448] All raw materials except Karenz BEI were added to a 500 ml 3-neck round bottom flask equipped with a distillation column according to Table 1 below, the temperature was raised to 80°C and reacted for 4 hours, then the temperature was lowered to 25°C and allowed to stand for 4 hours, then the temperature was raised again to 50°C, Karenz BEI was added, and stirred for 4 hours to obtain polymer solutions of Binder 1-1 to 1-5.
[0449] Synthesis Example 1-1 (Binder 1-1) Synthesis Example 1-2 (Binder 1-2) Synthesis Example 1-3 (Binder 1-3) Synthesis Example 1-4 (Binder 1-4) Synthesis Example 1-5 (Binder 1-5) Methacrylic acid (Sigma aldrich) 20 g (0.232 mol) 20 g (0.232 mol) 20 g (0.232 mol) 20 g (0.232 mol) 20 g (0.232 mol) 2-Hydroxyethyl methacrylate (Sigma aldrich) 10 g (0.077 mol) 10 g (0.077 mol) 10 g (0.077 mol) 10 g (0.077 mol) 10 g (0.077 mol) Benzyl methacrylate (Sigma aldrich) 55 g (0.312 mol) 55 g (0.312 mol) 55 g (0.312 mol) - - Cyclohexylmethyl methacrylate (Chemieliva) - - - 56.9 g (0.312 mol) 56.9 g (0.312 mol) Glycidyl methacrylate (Sigma aldrich) 15 g (0.106 mol) - 15 g (0.106 mol) - - (3-ethyloxetan-3-yl)methyl methacrylate (Eternal) - 15 g (0.081 mol) - 15 g (0.081 mol) - (7-oxabicyclo[4.1.0]heptan-3-yl)methyl methacrylate (Cyclomer M100, Daicel) - - 15 g (0.076 mol) - - Karenz BEI (Showa denko) 19.5 g (0.087 mol) 19.5 g (0.087 mol) 19.5 g (0.087 mol) 19.5 g (0.087 mol) 19.5 g (0.087 mol) AIBN (radical initiator) (Sigma aldrich) 7 g (0.043 mol) 7 g (0.043 mol) 7 g (0.043 mol) 7 g (0.043 mol) 7 g (0.043 mol)PGMEA (solvent)(Daicel)233g233g233g233g233gSolid content31 %31 %31 %31 %31 %Weight average molecular weight11,000 g / mol10,700 g / mol11,100 g / mol11,300 g / mol11,400 g / mol.
[0450] (Binder 1-1)
[0451]
[0452] In Binder 1-1, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 43 mol%; j is 14 mol%; k is 32 mol%; and l is 11 mol%.
[0453] (Binder 1-2)
[0454]
[0455] In Binder 1-2, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 44 mol%; j is 12 mol%; k is 33 mol%; and l is 11 mol%.
[0456] (Binder 1-3)
[0457]
[0458] In Binder 1-3, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 45 mol%; j is 11 mol%; k is 33 mol%; and l is 11 mol%.
[0459] (Binder 1-4)
[0460]
[0461] In Binder 1-4, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 43 mol%; j is 14 mol%; k is 32 mol%; and l is 11 mol%.
[0462] (Binder 1-5)
[0463]
[0464] In Binder 1-5, i, j, k, and l represent each repeating unit. Assuming the total to be 100 mol%, i is 44 mol%; j is 12 mol%; k is 33 mol%; and l is 11 mol%.
[0465] Synthesis Examples 1-6 to 1-10
[0466] (Synthesis of Binder 1-6 to 1-10)
[0467] All raw materials except Karenz AOI were added to a 500 ml 3-neck round bottom flask equipped with a distillation column according to Table 2 below, the temperature was raised to 80°C and reacted for 4 hours, then the temperature was lowered to 25°C and allowed to stand for 4 hours, then the temperature was raised again to 50°C, Karenz AOI was added, and stirred for 4 hours to obtain a polymer solution of Binder 1-6 to 1-10.
[0468] Synthesis Examples 1-6 (Binder 1-6) Synthesis Example 1-7 (Binder 1-7) Synthesis Example 1-8 (Binder 1-8) Synthesis Example 1-9 (Binder 1-9) Synthesis Example 1-10 (Binder 1-10) Methacrylic acid (Sigma aldrich) 20 g (0.232 mol) 20 g (0.232 mol) 20 g (0.232 mol) 20 g (0.232 mol) 20 g (0.232 mol) 2-Hydroxyethyl methacrylate (Sigma aldrich) 10 g (0.077 mol) 10 g (0.077 mol) 10 g (0.077 mol) 10 g (0.077 mol) 10 g (0.077 mol) Benzyl methacrylate (Sigma aldrich) 55 g (0.312 mol) 55 g (0.312 mol) 55 g (0.312 mol) - - Cyclohexylmethyl methacrylate (Chemieliva) - - - 56.9 g (0.312 mol) 56.9 g (0.312 mol) Glycidyl methacrylate (Sigma aldrich) 15 g (0.106 mol) - 15 g (0.106 mol) - - (3-ethyloxetan-3-yl)methyl methacrylate (Eternal) - 15 g (0.081 mol) - 15 g (0.081 mol) - (7-oxabicyclo[4.1.0]heptan-3-yl)methyl methacrylate (Cyclomer M100, Daicel) - - 15 g (0.076 mol) - - Karenz AOI (Showa denko) 10.8 g (0.077 mol) 10.8 g (0.077 mol) 10.8 g (0.077 mol) 10.8 g (0.077 mol) 10.8 g (0.077 mol) AIBN (radical initiator) (Sigma aldrich) 7 g (0.043 mol) 7 g (0.043 mol) 7 g (0.043 mol) 7 g (0.043 mol) 7 g (0.043 mol)PGMEA (solvent)(Daicel)233g233g233g233g233gSolid content31 %31 %31 %31 %31 %Weight average molecular weight (g / mol)10,500 g / mol10,400 g / mol10,800 g / mol11,000 g / mol11,070 g / mol.
[0469] (Binder 1-6)
[0470]
[0471] In Binder 1-6, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 43 mol%; j is 14 mol%; k is 32 mol%; and l is 11 mol%.
[0472] (Binder 1-7)
[0473]
[0474] In Binder 1-7, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 44 mol%; j is 12 mol%; k is 33 mol%; and l is 11 mol%.
[0475] (Binder 1-8)
[0476]
[0477] In Binder 1-8, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 45 mol%; j is 11 mol%; k is 33 mol%; and l is 11 mol%.
[0478] (Binder 1-9)
[0479]
[0480] In Binder 1-9, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 43 mol%; j is 14 mol%; k is 32 mol%; and l is 11 mol%.
[0481] (Binder 1-10)
[0482]
[0483] In Binder 1-10, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 44 mol%; j is 12 mol%; k is 33 mol%; and l is 11 mol%.
[0484] Synthesis Examples 1-11 to 1-13
[0485] (Synthesis of Binder 1-11 to 1-13)
[0486] Binder 1-12 and 1-13 were synthesized by adding all raw materials according to Table 3 below to a 500 ml 3-neck round bottom flask equipped with a distillation column, heating to 80℃, and reacting for 4 hours to obtain Binder 1-12 and Binder 1-13. Binder 1-11 was synthesized by adding all raw materials except Karenz AOI, heating to 80℃, reacting for 4 hours, then lowering the temperature to 25℃, waiting for 4 hours, then heating again to 50℃, adding Karenz AOI, and stirring for 4 hours.
[0487] Synthesis Example 1-11 (Binder 1-11) Synthesis Example 1-12 (Binder 1-12) Synthesis Example 1-13 (Binder 1-13) Methacrylic acid (Sigma aldrich) 20g (0.232 mol) 20g (0.232 mol) 20g (0.232 mol) 2-Hydroxyethyl methacrylate (Sigma aldrich company) 10g (0.077 mol) 10g (0.077 mol) 10g (0.077 mol) Benzyl methacrylate (Sigma aldrich company) 70g (0.397 mol) - 70g (0.397 mol) Cyclohexylmethyl methacrylate (Chemieliva company) - 56.9g (0.312 mol)-Glycidyl methacrylate-15g(0.106 mol)-Karenz AOI (Showa denko) 10.8g (0.077 mol)--AIBN (radical initiator) (Sigma aldrich) 7g (0.043 mol) 7g (0.043 mol) 7g (0.043 mol) PGMEA (solvent) (Daicel) 233g 233g 233g Solids 31% 30% 30% Weight average molecular weight (g / mol) 11,100 g / mol 10,100 g / mol 10,200 g / mol
[0488] (Binder 1-11)
[0489]
[0490] In Binder 1-11, i, j, and k represent each repeating unit, and assuming the total to be 100 mol%, i is 56 mol%; j is 11 mol%; and k is 33 mol%.
[0491] (Binder 1-12)
[0492]
[0493] In Binder 1-12, i, j, k, and l represent each repeating unit, and assuming the total to be 100 mol%, i is 43 mol%; j is 14 mol%; k is 32 mol%; and l is 11 mol%.
[0494] (Binder 1-13)
[0495]
[0496] In Binder 1-13, i, j, and k represent each repeating unit, and assuming the total to be 100 mol%, i is 56 mol%; j is 11 mol%; and k is 33 mol%.
[0497] Synthesis Example 2 (Synthesis of the Second Binder Resin)
[0498] Synthesis Example 2-1
[0499] (Preparation of compound 1-1)
[0500] 9,9'-Bisphenol fluorene 80 g (0.228 mol, Sigma Aldrich Co.), glycidyl chloride 42.67 g (0.461 mol, Sigma Aldrich Co.), and anhydrous potassium carbonate 191 g (1.38 mol) were placed in a 1500 ml 3-neck round-bottom flask equipped with a distillation column together with 600 ml of dimethylformamide, heated to 80°C, and reacted for 4 hours. After lowering the temperature to 25°C, the reaction solution was filtered, and the filtrate was added dropwise to 1000 ml of water with stirring, and the precipitated powder was filtered, washed with water, and dried under reduced pressure at 40°C to obtain 100 g (216 mmol) of compound 1-1. The obtained powder showed a purity of 98% as a result of HPLC purity analysis.
[0501] (Compound 1-1)
[0502]
[0503] Synthesis Example 2-2
[0504] (Synthesis of monomer 1-1 to monomer 1-3)
[0505] 25 g (54 mmol) of compound 1-1 obtained in Synthetic Example 2-1, 7.9 g (0.11 mol, Daejung Chemicals & Metals Co., Ltd.), 0.03 g (0.16 mmol, Daejung Chemicals & Metals Co., Ltd.) of acrylic acid, 0.03 g (0.16 mmol, Daejung Chemicals & Metals Co., Ltd.) of benzyltriethylammonium chloride, and 0.01 g (0.05 mmol, Daejung Chemicals & Metals Co., Ltd.) of hydroquinone were placed in a 300 ml 3-neck round-bottom flask equipped with a distillation column, along with 52 g of toluene (Sigma Aldrich Co., Ltd.), and stirred at 110°C for 6 hours. After the reaction was completed, toluene was removed by distillation under reduced pressure to obtain the product. After filling 500 g of silica gel 60 (230-400 mesh, Merck) into a glass column with a diameter of 220 mm, 20 g of the product was filled, and separation was performed using 10 L of a solvent containing a mixture of hexane and ethyl acetate in a volume ratio of 4:1, to separate monomers 1-1 to 1-3.
[0506] (monomer 1-1)
[0507]
[0508] (monomer 1-2)
[0509]
[0510] (monomer 1-3)
[0511]
[0512] Synthesis Examples 2-3 to 2-9
[0513] (Synthesis of Polymer 1-1 to 1-7)
[0514] Monomer 1-1, monomer 1-2 and monomer 1-3 obtained in Synthesis Example 2-2 were each placed in a 50 ml 3-neck round-bottom flask equipped with a distillation column so that the total amount was 5 g (8.2 mmol), as shown in Table 4 below, and 0.005 g (0.03 mmol, Daejung Chemicals & Metals Co., Ltd.) of Benzyltriethyl ammonium chloride, 0.001 g (0.01 mmol, Daejung Chemicals & Metals Co., Ltd.) of hydroquinone and 14 g (Sigma Aldrich Co., Ltd.) of propylene glycol methyl ether acetate were placed in the 3-neck round-bottom flask equipped with a distillation column, and 1.21 g (4 mmol, Mitsubishi Gas Co., Ltd.) of biphenyltetracarboxylic dianhydride and 0.38 g (2 mmol, Sigma Aldrich Co., Ltd.) of tetrahydrophthalic acid were added, and then stirred at 110°C for 6 hours. After the reaction was completed, the reaction solution was recovered to obtain polymers 1-1 to 1-7 containing repeating units of monomers 1-1, 1-2, and 1-3 in the form of a solution with a solid content of 45%. The molecular weight of the synthesized polymers was analyzed using gel permeation chromatography (Agilent).
[0515] Synthesis Example 2-3 (Polymer 1-1) Synthesis Example 2-4 (Polymer 1-2) Synthesis Example 2-5 (Polymer 1-3) Synthesis Example 2-6 (Polymer 1-4) Synthesis Example 2-7 (Polymer 1-5) Synthesis Example 2-8 (Polymer 1-6) Synthesis Example 2-9 (Polymer 1-7) Monomer 1-13 g (4.95 mmol) 1 g (1.65 mmol) 1 g (1.65 mmol) 4.25 g (7.01 mmol) 0.25 g (0.41 mmol) 5 g (8.24 mmol) 0 g Monomer 1-21 g (1.65 mmol) 3 g (4.95 mmol) 1 g (1.65 mmol) 0.25 g (0.41 mmol) 4.25 g (7.01 mmol) 0 g 5 g (8.24 mmol) Monomer 1-31 g(1.65 mmol)1 g(1.65 mmol)3 g(4.95 mmol)0.5 g(0.83 mmol)0.5 g(0.83 mmol)0 g0 gWeight Average molecular weight4,800 g / mol4,200 g / mol4,600 g / mol4,400 g / mol4,100 g / mol5,200 g / mol3,300 g / mol
[0516] Synthesis Example 2-10
[0517] (Synthesis of Compound 2-1)
[0518] In a 3-neck round-bottom flask equipped with a distillation column connected to cooling water, 20 g (0.147 mol) of trichloro silane (Gelest) and 17.51 g (0.147 mol) of 6-chloro-1-hexene (Aldrich) are dissolved in 200 ml of ethyl acetate, 0.02 g of platinum(0)-1,3-divinyl-1,1,3,3-tetramethyldisiloxane complex solution (2 wt% in xylene / Aldrich) is added, nitrogen is added, the temperature is raised to 75°C, and the reaction is carried out for 5 hours. After the solution is filtered with a 0.1 μm Teflon membrane, the platinum catalyst is removed. After that, 15.6 g (0.487 mol) of methanol was added dropwise at room temperature for 30 minutes, and then the temperature was raised to 50℃ and reacted for an additional 2 hours. The reaction solution was distilled under reduced pressure to remove the solvent. 24 g (0.1 mol) of 6-Chlorohexyltrimethoxysilane thus obtained, 8 g (0.15 mol) of sodium methoxide (Aldrich), 187 ml (0.15 mol) of hydrogen sulfide THF solution (0.8 M concentration), and 100 ml of methanol were placed in an autoclave and the reaction was carried out at 100℃ for 2 hours. After cooling the reaction solution, 100 ml of hydrogen chloride in methanol (1.25 M concentration) was added dropwise at room temperature for 30 minutes, and the generated salt was filtered off and distilled under reduced pressure to obtain 23 g of compound 2-1.
[0519] (Compound 2-1)
[0520]
[0521] Synthesis Example 2-11
[0522] (Synthesis of compound 2-2)
[0523] The same procedure was followed as in Synthesis Example 2-10, except that 9-Chloro-1-nonene (AK Scientific) 23.7 (0.147 mol) was used instead of 6-chloro-1-hexene.
[0524] (Compound 2-2)
[0525]
[0526] Synthesis Example 2-12
[0527] (Synthesis of compounds 2-3)
[0528] The same procedure was followed as in Synthesis Example 2-10, except that 30 g (0.147 mol) of 12-Chloro-1-dodecene (Atomax Chemicals) was used instead of 6-chloro-1-hexene.
[0529] (Compound 2-3)
[0530]
[0531] Synthesis Example 2-13
[0532] (Synthesis of compounds 2-4)
[0533] After removing platinum from Synthesis Example 2-10, the same procedure was followed, except that 22.4 g (0.487 mol) of ethanol (Aldrich) was used instead of the introduced methanol.
[0534] (Compound 2-4)
[0535]
[0536] Synthesis Example 2-14
[0537] (Synthesis of compounds 2-5)
[0538] After removing platinum from Synthesis Example 2-10, the same procedure was followed, except that 36 g (0.487 mol) of 1-butanol (Aldrich) was used instead of the introduced methanol.
[0539] (Compound 2-5)
[0540]
[0541] Synthesis Example 2-15
[0542] (Synthesis of compounds 2-6)
[0543] The same procedure was followed as in Synthesis Example 2-10, except that 18 g (0.147 mol) of dichloromethylsilane was used instead of trichlorosilane.
[0544] (Compound 2-6)
[0545]
[0546] Synthesis Example 2-16
[0547] (Synthesis of Binder 2-1)
[0548] In 360 g of the solution of Polymer 1-1 manufactured in Synthesis Example 2-3, 6.36 g (34 mmol) of KBM 803 (3-(Trimethoxysilyl)-1-propanethiol (Shinetsu Co.), the same as compound 2-7, was added, the temperature was raised to 60°C, and the mixture was stirred for 4 hours to obtain binder 2-1, a cardo-based binder resin with a silane group substituted like compound 2-7.
[0549] (Compound 2-7)
[0550]
[0551] Synthesis Examples 2-17 to 2-22
[0552] (Synthesis of Binder 2-2 to Binder 2-7)
[0553] Except that Polymer 1-2 to Polymer 1-7 described in Table 5 below were used instead of the solution of Polymer 1-1 in Synthesis Example 2-16, silane group-substituted cardo-based binder resins Binder 2-2 to Binder 2-7 were prepared in the same manner as in Synthesis Example 2-16.
[0554] Synthesis Example 2-16 (Binder 2-1) Synthesis Example 2-17 (Binder 2-2) Synthesis Example 2-18 (Binder 2-3) Synthesis Example 2-19 (Binder 2-4) Synthesis Example 2-20 (Binder 2-5) Synthesis Example 2-21 (Binder 2-6) Synthesis Example 2-22 (Binder 2-7) Polymer backbone Polymer 1-1 Polymer 1-2 Polymer 1-3 Polymer 1-4 Polymer 1-5 Polymer 1-6 Polymer 1-7 Silane group Compound 2-7 Compound 2-7 Compound 2-7 Compound 2-7 Compound 2-7 Compound 2-7 Solid content 34 % 34 % 34 % 34 % 34 % 34 % Weight Average molecular weight 4,880 g / mol 4,250 g / mol 4,680 g / mol 4,430 g / mol 4,140 g / mol 5,270 g / mol 3,320 g / mol
[0555] Synthesis Example 2-23
[0556] (Manufacturing of Binder 2-8)
[0557] 8.1 g (34 mmol) of 6-(Trimethoxysilyl)-1-hexanethiol (compound 2-1) was added to 360 g of the solution of Polymer 1-1 manufactured in Synthesis Example 2-3, and the temperature was raised to 60°C, followed by stirring for 4 hours to obtain Binder 2-8, a cardo-based binder resin substituted with a silane group similar to that of compound 2-1.
[0558] Synthesis Examples 2-24 to 2-29
[0559] (Manufacture of Binder 2-9 to Binder 2-14)
[0560] Except that Polymer 1-2 to Polymer 1-7 described in Table 6 below were used instead of the solution of Polymer 1-1 in Synthesis Example 2-23, cardo-based binder resins Binder 2-9 to Binder 2-14 having a substituted silane group were manufactured in the same manner as in Synthesis Example 2-23.
[0561] Synthesis Example 2-23 (Binder 2-8) Synthesis Example 2-24 (Binder 2-9) Synthesis Example 2-25 (Binder 2-10) Synthesis Example 2-26 (Binder 2-11) Synthesis Example 2-27 (Binder 2-12) Synthesis Example 2-28 (Binder 2-13) Synthesis Example 2-29 (Binder 2-14) Polymer backbonePolymer 1-1Polymer 1-2Polymer 1-3Polymer 1-4Polymer 1-5Polymer 1-6Polymer 1-7Silane groupCompound 2-1Compound 2-1Compound 2-1Compound 2-1Compound 2-1Compound 2-1Solid content34 %34 %34 %34 %34 %34 %34 %Weight Average molecular weight 4,900 g / mol 4,280 g / mol 4,690 g / mol 4,470 g / mol 4,160 g / mol 5,290 g / mol 3,360 g / mol
[0562] Synthesis Example 2-30
[0563] (Manufacturing of Binder 2-15)
[0564] 9.53 g (34 mmol) of 6-(Triethoxysilyl)-1-hexanethiol (compound 2-4) was added to 360 g of the solution of Polymer 1-1 manufactured in Synthesis Example 2-3, and the temperature was raised to 60°C, followed by stirring for 4 hours to obtain Binder 2-15, a cardo-based binder resin substituted with a silane group like compound 2-4.
[0565] Synthesis Examples 2-31 to 2-36
[0566] (Manufacture of Binder 2-16 to Binder 2-21)
[0567] Silane group-substituted cardo-based binder resins Binder 2-16 to Binder 2-21 were prepared in the same manner as in Synthesis Example 2-30, except that Polymer 1-2 to Polymer 1-7 described in Table 7 below were used instead of the solution of Polymer 1-1 in Synthesis Example 2-30.
[0568] Synthesis Example 2-30 (Binder 2-15) Synthesis Example 2-31 (Binder 2-16) Synthesis Example 2-32 (Binder 2-17) Synthesis Example 2-33 (Binder 2-18) Synthesis Example 2-34 (Binder 2-19) Synthesis Example 2-35 (Binder 2-20) Synthesis Example 2-36 (Binder 2-21) Polymer backbonePolymer 1-1Polymer 1-2Polymer 1-3Polymer 1-4Polymer 1-5Polymer 1-6Polymer 1-7Silane groupCompound 2-4Compound 2-4Compound 2-4Compound 2-4Compound 2-4Compound 2-4Solid content34 %34 %34 %34 %34 %34 %34 %Weight average molecular weight4,900 g / mol4,290 g / mol4,690 g / mol4,480 g / mol4,180 g / mol5,290 g / mol3,380 g / mol
[0569] Synthesis Example 3 (Synthesis of reactive silica)
[0570] Synthesis Example 3-1
[0571] (Synthesis of reactive silica 1)
[0572] In a 1000 ml 3-necked round-bottom flask equipped with a distillation column, 20 g of Ludox® TM40 colloidal silica suspension (particle size: 33 nm / 40 wt% in water, Sigma Aldrich) was added 180 g of purified water and stirred. 8 g of KBM-503 (compound (A), Shinetsu) was dispersed in 400 g of purified water, and the dispersion was added dropwise to the 3-necked round-bottom flask over 2 hours. Upon completion of the addition, the temperature was increased to 100°C, and the reaction was carried out with stirring for 18 hours. After completion of the reaction, the mixture was cooled to room temperature, and the silica having the compound (A) substituted on the surface was separated using a centrifuge. Thereafter, the mixture was washed with 300 g of purified water to obtain 8.9 g of reactive silica 1 (particle size: 54 nm) having the compound (A) substituted on the surface.
[0573] Compound (A)
[0574]
[0575] Synthesis Example 3-2
[0576] (Synthesis of reactive silica 2)
[0577] Synthesis was carried out in the same manner as in Synthesis Example 3-1, except that 8 g of KBM-503 was changed to 8 g of KBM-1403 (compound (B), Shinetsu Co.), thereby obtaining 8.7 g of reactive silica 2 (particle size: 54 nm) having compound (B) substituted on the surface.
[0578] Compound (B)
[0579]
[0580] Synthesis Example 3-3
[0581] (Synthesis of reactive silica 3)
[0582] Except that 8 g of KBM-503 in Synthesis Example 3-1 was changed to 8 g of KBM-303 (compound (C), Shinetsu Co.), the synthesis was carried out in the same manner as Synthesis Example 3-1, thereby obtaining 8.9 g of reactive silica 3 (particle size: 54 nm) having compound (C) substituted on the surface.
[0583] Compound (C)
[0584]
[0585] Synthesis Example 3-4
[0586] (Synthesis of reactive silica 4)
[0587] Except that 8 g of KBM-503 in Synthesis Example 3-1 was changed to 8 g of KBM-403 (compound (D), Shinetsu Co.), synthesis was carried out in the same manner as in Synthesis Example 3-1, thereby obtaining 8.8 g of reactive silica 4 (particle size: 54 nm) having compound (D) substituted on the surface.
[0588] Compound (D)
[0589]
[0590] Synthesis Example 3-5
[0591] (Synthesis of reactive silica 5)
[0592] Synthesis was carried out in the same manner as in Synthesis Example 3-1, except that 8 g of KBM-503 was changed to 4 g of KBM-403 and 4 g of KBM-503, thereby obtaining 8.9 g of reactive silica 5 (particle size: 54 nm) having compound (A) and compound (D) substituted on the surface.
[0593] Synthesis Example 3-6
[0594] (Synthesis of reactive silica 6)
[0595] Except that 80 g of NanoXact Silica Nanospheres (particle size: 500 nm / 10 wt% in water, nanoComposix) and 100 g of purified water were used instead of the Ludox® TM40 colloidal silica suspension in Synthesis Example 3-1, synthesis was performed in the same manner as in Synthesis Example 3-1, and 8.7 g of reactive silica 6 (particle size: 520 nm) having compound (A) substituted on the surface was obtained.
[0596] Synthesis Example 3-7
[0597] (Synthesis of non-reactive silica 1)
[0598] Except that 8 g of KBM-503 in Synthesis Example 3-1 was changed to 8 g of hexyktrimethoxysilane (compound (E), TCI Corporation), the synthesis was carried out in the same manner as in Synthesis Example 3-1, thereby obtaining 8.6 g of non-reactive silica 1 (particle size: 54 nm) having compound (E) substituted on the surface.
[0599] compound (E)
[0600]
[0601] [Synthesis of chromophore-protecting group dyes (Squarylium dyes)]
[0602] Synthesis Example 41 (Synthesis of Squarylium dye 1)
[0603] Synthesis Example 41-1
[0604] In a 1000 ml reactor equipped with a reflux device, 100 g (473.3 mmol, Alchem), 86 g (475 mmol, TCI), 11.5 g (479.2 mmol, Sigma Aldrich) of 2,4,6-Trimethyl-N-phenylaniline, and 500 g of N,N-Dimethyl formamide were placed, the temperature was increased to 80°C, and the mixture was stirred for 18 hours. After the reaction, the mixture was extracted with 500 ml of diethyl ether (Sigma Aldrich) and 1000 ml of water, distilled under reduced pressure, and separated by column chromatography to obtain 130 g of an intermediate such as the following compound D-1.
[0605] Compound D-1
[0606]
[0607] Synthesis Example 41-2
[0608] In a 2000 ml reactor equipped with a reflux and Dean-Stark apparatus, 125 g (401.3 mmol) of compound D-1, 23 g (201.6 mmol, Sigma Aldrich) of 3,4-Dihydroxy-3-cyclobutene-1,2-dione, and 800 g of chlorobenzene (Sigma Aldrich) were placed, the temperature was increased to 120°C, and the mixture was stirred for 18 hours. After completion of the reaction, the solvent was distilled off under reduced pressure, and the residue was separated by column chromatography to obtain 90 g of an intermediate such as compound D-2 below.
[0609] Compound D-2
[0610]
[0611] Synthesis Example 41-3
[0612] In a 1000 ml reactor equipped with a reflux unit, 70 g (99.9 mmol) of compound D-2, 48 g (200.7 mmol, Showa denko Co., Ltd.) of Karenz BEI, and 400 g of chloroform (Sigma Aldrich Co., Ltd.) were added, the temperature was raised to 40°C, and the mixture was stirred for 18 hours to obtain an intermediate such as compound D-3. Subsequently, after cooling to room temperature, 61 g (300.5 mmol, Sigma Aldrich Co., Ltd.) of isophthaloyl chloride and 41 g (301.1 mmol, Sigma Aldrich Co., Ltd.) of p-xylylenediamine were added dropwise over 3 hours, and the mixture was stirred for 18 hours. After completion of the reaction, the solvent was distilled off under reduced pressure, and the product was separated by column chromatography to obtain 80 g of the following squarylium dye 1.
[0613] Compound D-3
[0614]
[0615] <squarylium dye 1>
[0616]
[0617] Synthesis Example 42 (Synthesis of Squarylium dye 2)
[0618] Synthesis Example 42-1
[0619] Except that 98 g (473.2 mmol, Chemenu) of (4-(Bromomethyl)cyclohexyl)methanol was used instead of 86 g (475 mmol, TCI) of 6-Bromo-1-hexanol in Synthesis Example 41-1, the remaining process was carried out in the same manner. Through this, 135 g of an intermediate such as compound E-1 was obtained.
[0620] <Chemical Formula E-1>
[0621]
[0622] Synthesis Example 42-2
[0623] Synthesis was performed using the same process as in Synthesis Example 41-2, except that 135 g (400 mmol) of compound E-1 was used instead of 125 g (401.3 mmol) of compound D-1 in Synthesis Example 41-2. Through this, 120 g of an intermediate such as compound E-2 could be obtained.
[0624] Compound E-2
[0625]
[0626] Synthesis Example 42-3
[0627] Synthesis was performed using the same process as in Synthesis Example 41-3, except that 75 g (99.6 mmol) of compound E-2 was used instead of 70 g (99.9 mmol) of compound D-2 in Synthesis Example 41-3. Through this, 100 g of squarylium dye 2 was obtained.
[0628] <squarylium dye 2>
[0629]
[0630] Synthesis Example 43 (Synthesis of Squarylium dye 3)
[0631] Synthesis Example 43-1
[0632] Except that 95 g (472.5 mmol, Apollo Scientific) of 4-(Bromomethyl)benzyl alcohol was used instead of 86 g (475 mmol, TCI) of 6-Bromo-1-hexanol in Synthesis Example 41-1, the remaining process was carried out in the same manner. Through this, 140 g of an intermediate such as compound F-1 was obtained.
[0633] Compound F-1
[0634]
[0635] Synthesis Example 43-2
[0636] Synthesis was performed using the same process as in Synthesis Example 41-2, except that 133 g (401.3 mmol) of compound F-1 was used instead of 125 g (401.3 mmol) of compound D-1 in Synthesis Example 41-2. Through this, 125 g of an intermediate such as compound F-2 could be obtained.
[0637] Compound F-2
[0638]
[0639] Synthesis Example 43-3
[0640] Synthesis was performed using the same process as in Synthesis Example 41-3, except that 74 g (99.9 mmol) of compound F-2 was used instead of 70 g (99.9 mmol) of compound D-2 in Synthesis Example 41-3. Through this, 105 g of squarylium dye 3 was obtained.
[0641] <squarylium dye 3>
[0642]
[0643] Synthesis Example 44 (Synthesis of Squarylium dye 4)
[0644] A synthesis was performed using the same process as in Synthesis Example 41-3, except that 61 g of 2,6-pyridinedicarbonyl dichloride (299 mmol, Sigma Aldrich) was used instead of 61 g of isophthaloyl chloride (300.5 mmol, Sigma Aldrich). Through this, 110 g of squarylium dye 4 was obtained.
[0645] <squarylium dye 4>
[0646]
[0647] Synthesis Example 45 (Synthesis of Squarylium dye 5)
[0648] Synthesis Example 45-1
[0649] Except that 114 g (476.5 mmol, Showa denko) of Karenz BEI was used instead of 86 g (475 mmol, TCI) of 6-Bromo-1-hexanol in Synthesis Example 41-1, the remaining process was carried out in the same manner. Through this, 190 g of an intermediate such as compound H-1 was obtained.
[0650] Compound H-1
[0651]
[0652] Synthesis Example 45-2
[0653] Except that 180 g (399.5 mmol) of compound H-1 of Synthesis Example 45-1 was used instead of 125 g (401.3 mmol) of compound D-1 in Synthesis Example 41-2, the remaining process was carried out in the same manner. Through this, 170 g of an intermediate such as compound H-2 could be obtained.
[0654] Compound H-2
[0655]
[0656] Synthesis Example 45-3
[0657] In a 1000 ml reactor equipped with a reflux device, 97 g (99.1 mmol) of compound H-2 and 300 g of chloroform (Sigma Aldrich) were placed, and at room temperature, 61 g (300.5 mmol, Sigma Aldrich) of isophthaloyl chloride and 41 g (301.1 mmol, Sigma Aldrich) of p-xylylenediamine were added dropwise over 3 hours, followed by stirring for 18 hours. After completion of the reaction, the solvent was distilled off under reduced pressure, and separated by column chromatography to obtain 75 g of the following squarylium dye 5.
[0658] <squarylium dye 5>
[0659]
[0660] Synthesis Example 52 (Synthesis of Dispersant)
[0661] Synthesis Example 52-1
[0662] (Manufacture of Polymer 52-1)
[0663] In a 500 ml 3-neck round-bottom flask with a distiller, 50 g (0.284 mol, Sigma Aldrich Co.), 30 g (0.193 mol, TCI Co.), 20 g (0.072 mol, TCI Co.) of Benzyl methacrylate, 233 g (Daicel Co.) of PGMEA, and 4 g (0.024 mol, TCI Co.) of AIBN were added, and the mixture was stirred at 80°C for 4 hours to obtain Polymer 52-1 (solid content 30.86%, weight average molecular weight 20,400 g / mol).
[0664] Polymer 52-1
[0665]
[0666] In Polymer 52-1, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 13.1 mol%; b is 51.7 mol%; and c is 35.2 mol%.
[0667] Synthesis Example 52-2
[0668] (Manufacture of Polymer 52-2)
[0669] Except that 20 g (0.086 mol, TCI) of Triethylene glycol methyl ether methacrylate was used instead of Tetraethylene glycol methyl ether methacrylate in the above Synthesis Example 52-1, synthesis was carried out in the same manner to obtain Polymer 52-2 (solid content 30.87%, weight average molecular weight 20,310 g / mol).
[0670] Polymer 52-2
[0671]
[0672] In Polymer 52-2, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 15.3 mol%; b is 50.4 mol%; and c is 34.3 mol%.
[0673] Synthesis Example 52-3
[0674] (Manufacture of Polymer 52-3)
[0675] Except that 20 g (0.106 mol, TCI) of Diethylene Glycol Monomethyl Ether Methacrylate was used instead of Tetraethylene glycol methyl ether methacrylate in the above Synthesis Example 52-1, synthesis was carried out in the same manner to obtain Polymer 52-3 (solid content 30.86%, weight average molecular weight 20,220 g / mol).
[0676] Polymer 52-3
[0677]
[0678] In Polymer 52-3, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 18.2 mol%; b is 48.7 mol%; and c is 33.1 mol%.
[0679] Synthesis Example 52-4
[0680] (Manufacture of dispersant 51-1)
[0681] In a 300 ml 3-neck round bottom flask with a distiller, 100 g of the Polymer 52-1 solution prepared in Synthesis Example 52-1, 6.58 g (0.06 mol, TCI) of N,N-Dimethyl-1,3-propanediamine, and 0.2 g (0.32 mmol, Sigma Aldrich) of dibutyltin dilaurylate were added, and stirred at 50°C for 4 hours to obtain a dispersant 51-1 (solid content 33.3%, weight average molecular weight 20,830 g / mol).
[0682] Dispersant 51-1
[0683]
[0684] In Dispersant 51-1, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 13.1 mol%; b is 51.7 mol%; and c is 35.2 mol%.
[0685] Synthesis Example 52-5
[0686] (Manufacture of dispersant 51-2)
[0687] Dispersant 51-2 (solid content 35.9%, weight average molecular weight 20,870 g / mol) was obtained by carrying out the synthesis in the same manner as in Synthesis Example 52-4, except that 9.43 g (0.06 mol, Azepine Product) of [3-(2-aminoethoxy)propyl]dimethylamine was used instead of N,N-Dimethyl-1,3-propanediamine.
[0688] Dispersant 51-2
[0689]
[0690] In dispersant 51-2, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 13.1 mol%; b is 51.7 mol%; and c is 35.2 mol%.
[0691] Synthesis Example 52-6
[0692] (Manufacture of dispersant 51-3)
[0693] Dispersant 1-3 (solid content 40.32%, weight average molecular weight 20,860 g / mol) was obtained by proceeding with the same synthesis method, except that 13.82 g (0.06 mol, Aurora Building Co.) of (11-aminoundecyl)dimethylamine was used instead of N,N-Dimethyl-1,3-propanediamine in the above synthesis example 52-4.
[0694] Dispersant 51-3
[0695]
[0696] In dispersant 51-3, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 13.1 mol%; b is 51.7 mol%; and c is 35.2 mol%.
[0697] Synthesis Example 52-7
[0698] (Manufacture of dispersant 51-4)
[0699] Except that 10.27 g (0.06 mol, Azepine Product Co.) of [4-amino-1-(dimethylamino)butan-2-yl]dimethylamine was used instead of N,N-Dimethyl-1,3-propanediamine in the above Synthesis Example 52-4, the synthesis was carried out in the same manner to obtain dispersant 51-4 (solid content 36.7%, weight average molecular weight 20,890 g / mol).
[0700] Dispersant 51-4
[0701]
[0702] In dispersant 51-4, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 13.1 mol%; b is 51.7 mol%; and c is 35.2 mol%.
[0703] Synthesis Example 52-8
[0704] (Manufacture of dispersant 51-5)
[0705] In a 300 ml 3-neck round bottom flask with a distiller, 100 g of the Polymer 52-2 solution prepared in Synthesis Example 52-2, 10.27 g (0.06 mol, Azepine Product Co.) of [4-amino-1-(dimethylamino)butan-2-yl]dimethylamine, and 0.2 g (0.32 mmol, Sigma Aldrich Co.) of dibutyltin dilaurylate were added, and stirred at 50°C for 4 hours to obtain Dispersant 51-5 (solid content 36.97%, weight average molecular weight 20,780 g / mol).
[0706] Dispersant 51-5
[0707]
[0708] In dispersant 51-5, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 15.3 mol%; b is 50.4 mol%; and c is 34.3 mol%.
[0709] Synthesis Example 52-9
[0710] (Manufacture of dispersant 51-6)
[0711] In a 300 ml 3-neck round bottom flask with a distiller, 100 g of the Polymer 52-3 solution prepared in Synthesis Example 52-3, 10.27 g (0.06 mol, Azepine Product Co.) of [4-amino-1-(dimethylamino)butan-2-yl]dimethylamine, and 0.2 g (0.32 mmol, Sigma Aldrich Co.) of dibutyltin dilaurylate were added, and stirred at 50°C for 4 hours to obtain a dispersant 51-6 (solid content 36.97%, weight average molecular weight 20,630 g / mol).
[0712] Dispersant 51-6
[0713]
[0714] In dispersant 51-6, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 18.2 mol%; b is 48.7 mol%; and c is 33.1 mol%.
[0715] Synthesis Example 52-10
[0716] (Manufacture of comparative dispersants)
[0717] In a 300 ml 3-neck round bottom flask with a distiller, 100 g of the Polymer 52-1 solution prepared in Synthesis Example 52-1, 6.65 g (0.06 mol, TCI) of 3-(Dimethylamino)-1-propanol, and 0.2 g (0.32 mmol, Sigma Aldrich) of dibutyltin dilaurylate were added, and stirred at 50° C. for 4 hours to obtain comparative dispersant 51 (solid content 36.81%, weight average molecular weight 20,810 g / mol).
[0718] Comparative Dispersant 51
[0719]
[0720] In Comparative Dispersant 51, a, b, and c represent each repeating unit, and assuming the total to be 100 mol%, a is 13.1 mol%; b is 51.7 mol%; and c is 35.2 mol%.
[0721] Manufacturing Example 1 (Manufacture of Comparative Pigment Dispersion)
[0722] A comparative pigment dispersion was obtained by dispersing 17 g of Irgaphor Red BT-CF (red pigment / BASF), 3.05 g of a comparative dispersant, and 2.85 g of SR-3613 (SMS), 75.1 g of propylene glycol methyl ether acetate, and 100 g of zirconia beads with a diameter of 0.5 mm (Toray) for 10 hours using a paint shaker (Asada).
[0723] Manufacturing Examples 2-1 to 2-6 (Manufacturing of pigment dispersions 1 to 6)
[0724] Pigment dispersions 1 to 6 were prepared in the same manner as in Manufacturing Example 1, except that 3.05 g of dispersants 51-1 to 51-6 of the present invention were used instead of the comparative dispersant, and the reactive dye of the present invention was additionally used as shown in Table 8 below. (Average particle size D50 = 97.4 nm, half width = 76.3 nm)
[0725] Manufacturing Example 2-1 (Pigment Dispersion 1) Manufacturing Example 2-2 (Pigment Dispersion 2) Manufacturing Example 2-3 (Pigment Dispersion 3) Manufacturing Example 2-4 (Pigment Dispersion 4) Manufacturing Example 2-5 (Pigment Dispersion 5) Manufacturing Example 2-6 (Pigment Dispersion 6) Manufacturing Example 1 (Comparative Pigment Dispersion) Squarylium dye 1 solution 2g----7g-Squarylium dye 2 solution-3g-----Squarylium dye 3 solution--4g----Squarylium dye 4 solution---5g---Squarylium dye 5 solution----6g--Irgaphor Red BT-CF 15g14g13g12g11g10g17gComparative Dispersant------3.05gDispersant 1-13.05gDispersant 1-23.05g dispersant 1-33.05g dispersant 1-43.05g dispersant 1-53.05g dispersant 1-63.05g
[0726] Manufacturing Example 3 (Manufacture of the composition of the present invention and the comparative composition)
[0727] Compositions 1-1 to 1-6 containing the pigment dispersion of the present invention and the alkali-soluble resin of the present invention were prepared with the compositions (weight %) shown in Table 9 below.
[0728] Manufacturing Example 3-1 (Composition 1-1) Manufacturing Example 3-2 (Composition 1-2) Manufacturing Example 3-3 (Composition 1-3) Manufacturing Example 3-4 (Composition 1-4) Manufacturing Example 3-5 (Composition 1-5) Manufacturing Example 3-6 (Composition 1-6) Manufacturing Example 3-7 (Composition 1-7) Manufacturing Example 3-1 (Composition 1-8) Manufacturing Example 3-1 (Composition 1-9) Pigment Dispersion 130------3030 Pigment Dispersion 2-30-------Pigment Dispersion 3--30------Pigment Dispersion 4---30-----Pigment Dispersion 5----30----Pigment Dispersion 6-----30---Comparative Pigment Dispersion------30--M600 (Miwon Commercial) 888888888OXE-02 (BASF) 0.50.50.50.50.50.50.50.50.50.5 Binder 1-17--4--4-4 Binder 1-6-7--4---- Binder 1-11--7--4--- Binder 2-1---3--3 73 Binder 2-8----3---- Binder 2-15-----3--- Reactive silica particles 13-------- Reactive silica particles 2-3------- Reactive silica particles 3--3--3--- Reactive silica particles 4---3--3-- Reactive silica particles 5----3--3- Non-reactive silica particles 13 Propylene glycol methyl ether acetate (Daicel)51.551.551.551.551.551.551.551.551.551.5
[0729] The method for manufacturing a pattern using the composition of Table 9 above is as follows (photolithography step).
[0730] (1) Application and film formation stage
[0731] Each composition in Table 9 was applied to a washed 5 cm x 5 cm stainless steel substrate using a spin coater to a thickness of 3 ㎛, and then heated at a temperature of 100°C for 1 minute to remove the solvent, thereby forming a coating film.
[0732] (2) Exposure stage
[0733] In order to form the required pattern on the obtained film, an open mask of a predetermined shape was inserted, and then an active line of 190 nm to 500 nm was irradiated. The exposure device used was MA-6, and the exposure dose was 100 mJ / cm 2 was investigated.
[0734] (3) Phenomenon stage
[0735] Following the above exposure step, the film was developed by dipping in AZEM AX 300 MIF developer at 25°C for 1 minute, and then washed with water.
[0736] (4) Post-processing stage
[0737] After the film obtained by the above phenomenon was post-baked in an oven at 100°C for 60 minutes, a pattern formed with the composition of Table 5 was obtained.
[0738] Examples (pattern resolution, residue, outgas)
[0739] The resolution, residue, and outgassing of the pattern of the composition of Table 5 manufactured by the above photolithography step were evaluated by the following method.
[0740] [Example 1]
[0741] The resolution, outgas generation amount, and chemical resistance of the pattern formed with the above composition 1-1 were evaluated using the following methods, and the results are shown in Table 6 below.
[0742] 1. Resolution evaluation (measuring the minimum pattern size on the substrate)
[0743] The minimum pattern size on the substrate of the pattern of the composition 1-1 obtained through the above photolithography step was measured using an optical microscope (ECLIPSE LV100POL Model, Nikon).
[0744] 2. Residue evaluation (observation of presence or absence of residue)
[0745] The pattern of the composition 1-1 obtained through the above photolithography step was checked for residue level using an optical microscope (ECLIPSE LV100POL Model, Nikon), and the results are shown in Table 7.
[0746] 3. Outgas assessment (measuring the amount of outgas generated)
[0747] A pattern of the composition 1-1 was formed on a glass substrate through the photolithography step. The patterned glass substrate was cut into a size of 1 cm x 3 cm to produce a total of six specimens. The outgassing of the specimens was captured at 250°C for 30 minutes using JTD-505² from JAI. A calibration curve was created after measuring toluene black samples (100, 500, 1,000 ppm) using QP2020 GC / MS from Shimadzu, and the outgassing amount of the captured samples was measured.
[0748] [Examples 2 to 6; Comparative Examples 1 to 3]
[0749] In the above Example 1, a pattern was formed in the same manner as in Example 1 using Compositions 1-2 to 1-9 instead of Composition 1-1. The resolution, outgassing amount, and presence of residue of the formed pattern were evaluated in the same manner as in Example 1, and the results are shown in Table 10 below.
[0750] Pattern composition Minimum pattern size (㎛) Presence of residue (O, △, X) Outgassing amount (ppm) Pigment particle size distribution Average particle size D50 (nm) Half width (nm) Example 1 Composition 1-13.8O3.295.679.4 Example 2 Composition 1-23.3O2.892.474.5 Example 3 Composition 1-33.5O2.693.775.1 Example 4 Composition 1-43.6O2.394.375.8 Example 5 Composition 1-53.5O2.693.775.1 Example 6 Composition 1-63.7O2.494.776.3 Comparative Example 1 Composition 1-713.0X16.8119.9102.2Comparative Example 2 Composition 1-810.1△5.495.679.4Comparative Example 3 Composition 1-911.2△5.895.679.4
[0751] Comparing Examples 1 to 6 and Comparative Examples 1 to 3 in Table 10 above, it can be seen that the binder resin, pigment dispersion, and reactive silica particles among the components of the composition forming the pattern were used differently.
[0752] In contrast, the binders used in Examples 1 to 6 are polymerized from three monomers with different structures, resulting in a relatively network-like structure. Therefore, due to their structural characteristics, they effectively form intermolecular bonds with surrounding compounds, making them more suitable for photolithography processes. Consequently, they exhibit high pattern resolution, low outgassing, and excellent chemical resistance.
[0753] In Table 10 above, it can be confirmed that the example including both the reactive silica and the alkali-soluble resin of the present invention is superior to the comparative example in terms of resolution, outgassing amount, and chemical resistance.
[0754] In addition, it can be seen that Examples 1 to 6 including pigment dispersions containing the tertiary amine dispersant of the present invention show excellent results in resolution, outgassing amount, and residue evaluation, and in particular, in the case of Example 4 using the tertiary amine dispersant containing a diamine substituent, it was confirmed that the pigment was effectively dispersed, so that the average particle size D50 and the half maximum width were small and the pattern resolution was very excellent.
[0755] Looking at Example 1 using the tertiary amine dispersant of the present invention including a urea moiety linking group in the pigment dispersion in Table 10 above, it can be confirmed that Example 1 including both the tertiary amine dispersant of the present invention and the alkali-soluble resin is superior to Comparative Example 1 in terms of resolution, outgassing amount, and residue evaluation.
[0756] In particular, a large difference was observed in the amount of outgas generated. This is believed to be because, in the case of Comparative Example 1, the bond of the carbamate linkage of the tertiary amine dispersant was broken in the post-heat treatment process, resulting in a high amount of outgas generated, whereas, in the case of Example 1, the urea linkage of the tertiary amine dispersant was not broken in the post-heat treatment process and the bond was stably maintained.
[0757] Meanwhile, in the case of Comparative Example 1 using a comparative dispersant and an acrylic binder, it was confirmed that the resolution and the outgassing amount were much lower and higher than those of the examples using a tertiary amine dispersant and the alkali-soluble resin of the present invention, and that there was a large difference in the residue evaluation.
[0758] In summary of the above evaluation results, when comparing Examples 1 to 6, which evaluated a composition including the dye of the present invention, the reactive silica, and the alkali-soluble resin of the present invention in Table 10, with Comparative Example 1, which does not include the dye of the present invention and the dispersant, it can be confirmed that the average particle size D50 and the half maximum width of Examples 1 to 6 are small, effectively dispersing pigment particles. In addition, it can be seen that Examples 1 to 6 are sufficiently cured in the exposure process or the post-treatment process performed at 100°C or lower, so that the minimum pattern size on the substrate is small, resulting in excellent resolution, and not only is the amount of outgassing small, but the generation of residue is also suppressed. It is believed that this is because when the dye, dispersant, reactive silica, and alkali-soluble resin of the present invention are used together, an unpredictable effect occurs due to the structural characteristics of the materials.
[0759] Examples 7 to 12; Comparative Examples 4 to 6 (evaluation of light resistance and chemical resistance of films)
[0760] The light resistance and chemical resistance of the composition film of Table 9 manufactured by the above photolithography step were evaluated by the following methods.
[0761] [Example 7]
[0762] The light resistance and chemical resistance of the film formed from the above composition 1-1 were evaluated using the following methods, and the results are shown in Tables 11 and 12 below.
[0763] 1. Lightfastness evaluation (△Eab* measurement)
[0764] The Eab* of the film of the composition 1-1 manufactured by the above photolithography step was measured with MCPD (Otsuka) before and after 100 hours on a Q-SUN XE-1 (Q-LAB) light resistance tester, and the change was shown in Table 11 below.
[0765] 2. Chemical resistance evaluation (measurement of permeability change before and after solvent immersion)
[0766] The transmittance of the film of the composition 1-1 obtained through the above photolithography step was measured using UV-2600 (Shimadzu), and after immersing in propyl glycol methyl ether acetate at 50°C for 5 minutes, the transmittance of the film was measured and the change in thickness was observed to determine chemical resistance. The wavelength and measurement results for transmittance are as shown in Table 12 below.
[0767] [Examples 8 to 12; Comparative Examples 4 to 6]
[0768] In Example 7, a film was formed in the same manner as in Example 1, using Compositions 1-2 to 1-9 instead of Composition 1-1. The light resistance and chemical resistance of the formed film were evaluated in the same manner as in Example 7, and the results are shown in Tables 11 and 12.
[0769] Example 7 Example 8 Example 9 Example 10 Example 11 Example 12 Comparative Example 4 Comparative Example 5 Comparative Example 6 Film Composition Composition 1-1 Composition 1-2 Composition 1-3 Composition 1-4 Composition 1-5 Composition 1-6 Composition 1-7 Composition 1-8 Composition 1-9 Changes in light properties before and after light resistance test (△Eab*) 3.20 3.15 2.96 2.93 2.97 2.90 12.31 11.30 11.30
[0770] Film composition Wavelength-specific transmittance before solvent immersion (%) Wavelength-specific transmittance after solvent immersion (%) (Propylene glycol methyl ether acetate, 50°C, 5 min) Wavelength-specific transmittance difference before and after solvent immersion (%) Wavelength (nm) -450 530 620 450 530 620 450 530 620 Example 7 Composition 1-10.0 78 1.10.0 40.1 88 2.40.2 50.1 1.3 0.2 1 Example 8 Composition 1-20.0 78 0.9 0.0 40.1 88 2.6 0.1 30.1 1.7 0.0 9 Example 9 Composition 1-30.0 58 1.30.0 50.1 68 3.10.2 70.1 1.8 0.2 2 Example 10 Composition 1-40.0780.20.040.1281.90.140.051.70.1Composition of Example 11 1-50.0680.70.040.1481.70.160.0810.12Composition of Example 12 1-60.0681.10.050.1182.60.090.051.50.04Comparative Example 4 Composition 1-70.3972.60.550.5271.90.590.150.30.07Composition of Comparative Example 5 1-80.4172.10.750.6772.610.90.260.510.15Composition of Comparative Example 6 1-90.4172.10.750.6772.610.90.260.510.15
[0771] From Table 11 above, it can be confirmed that in the case of Examples 7 to 12 including the chromophore-protecting group dye and dispersant of the present invention, the light resistance is improved compared to the case of Comparative Example 4 including an acrylic binder different from the alkali-soluble resin of the present invention and not including the chromophore-protecting group dye and dispersant of the present invention.
[0772] From Table 12 above, in the case of Examples 7 to 12 including the chromophore-protecting group dye and dispersant of the present invention, the difference in transmittance before and after solvent immersion was reduced compared to the case of Comparative Example 4 not including the chromophore-protecting group dye and dispersant of the present invention, and accordingly, it can be confirmed that the chemical resistance is improved in the case of Examples 7 to 12 including the chromophore-protecting group dye and dispersant of the present invention.
[0773] From Table 11 above, it can be confirmed that in the case of Examples 7 to 12 including the alkali-soluble resin of the present invention, the light resistance is improved compared to the case of Comparative Example 5 which does not include a binder different from the alkali-soluble resin of the present invention.
[0774] From Table 12 above, in the case of Examples 7 to 12 including the alkali-soluble resin of the present invention, the difference in permeability before and after solvent immersion was reduced compared to the case of Comparative Example 5 not including the alkali-soluble resin of the present invention, and accordingly, it can be confirmed that the chemical resistance is improved in the case of Examples 7 to 12 including the alkali-soluble resin of the present invention.
[0775] From Table 11 above, it can be confirmed that in the case of Examples 7 to 12 including the reactive silica particles of the present invention, the light resistance is improved compared to the case of Comparative Example 6 not including the reactive silica particles of the present invention.
[0776] From Table 12 above, in the case of Examples 7 to 12 including the reactive silica particles of the present invention, the difference in transmittance before and after solvent immersion was reduced compared to the case of Comparative Example 6 not including the reactive silica particles of the present invention, and accordingly, it can be confirmed that the chemical resistance is improved in the case of Examples 7 to 12 including the reactive silica particles of the present invention.
[0777] The present invention is not limited to the above embodiments and can be manufactured in various different forms.
[0778] The above description is merely an example of the present invention, and those skilled in the art will appreciate that various modifications may be made without departing from the essential characteristics of the present invention.
[0779] Accordingly, the embodiments disclosed herein are intended to illustrate, rather than limit, the present invention, and the spirit and scope of the present invention are not limited by these embodiments. The scope of protection of the present invention should be interpreted by the claims, and all techniques within the scope equivalent thereto should be interpreted as being included within the scope of the present invention.
[0780] (Explanation of symbols)
[0781] 1: Substrate 2: TFT layer
[0782] 3: Flat layer 4: Pixel electrode
[0783] 5: Pixel defining film 6: Organic layer
[0784] 7: Counter electrode 8: Sealing layer
[0785] 9: Touch panel 10: Color section
[0786] 11: Color separation section
[0787] The present invention relates to a photosensitive resin composition, a pattern or film formed from the photosensitive composition, and an organic light-emitting display device using the pattern or film.
Claims
1. A photosensitive composition comprising: an alkali-soluble resin; a reactive unsaturated compound; a photoinitiator; a reactive dye comprising a chromophore of the following chemical formula (3) and a protecting group of the following chemical formula (4); a solvent; and reactive silica particles comprising a structure represented by the following chemical formula (1): Chemical formula (1) In the above chemical formula (1), 1) R 21 is a single bond, fluorenylene group, C1~C 30 alkylene, C6~C 30 Arylene, C2~C 30 Heterocyclic ring or C1~C 30 is an alkoxylene, 2) R 22 is C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group, 3) n 1 is an integer from 1 to 3; n 2 is an integer from 0 to 2; n 1 + n 2 = 3, 4) * is the part that connects to the silica particles, 5) X 3 is one of the following chemical formulas a to e, Chemical formula a Chemical formula b Chemical formula c Chemical formula d Chemical formula e 6) ** is Si or R 21 It is the part that connects to , 7) R 23 is hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group, 8) The above R 21 ~R 23 and X 3 are respectively deuterium; halogen; C1~C 30 Alkyl group or C6~C 30 Silane group substituted or unsubstituted with an aryl group; siloxane group; boron group; germanium group; cyano group; amino group; nitro group; C1~C 30 Alkylthio group of; C1~C 30 Alkoxy group of; C6~C 30 Aryl alkoxy group of; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkyne group of; C6~C 30 Aryl group of; C6~C substituted with deuterium 30 Aryl group of; Fluorenyl group; C2~C containing at least one heteroatom selected from the group consisting of O, N, S, Si and P 30 Heterocyclic group of; C3~C 30 Aliphatic ring group; C7~C 30 Arylalkyl group of; C8~C 30 and may be further substituted with one or more substituents selected from the group consisting of an arylalkenyl group; and combinations thereof, and adjacent substituents may form a ring, Chemical formula (3) In the above chemical formula (3), 1) L 1 ~L 4 are independently a single bond; fluorenylene group; C1~C 30 alkylene; C3~C 30 Cycloalkylene group of; C1~C 30 Alkoxylene group of; C2~C 30 Polyethyleneoxy group of; C6~C 30 Arylene group of; C2~C 30 a heterocycle; or a combination thereof, 2) X 1 ~X 4 are independently hydrogen; deuterium; fluorenyl group; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group of; C3~C 30 cycloalkyl group of; or chemical formula (4-A), 3) X 1 ~X 4 At least one of which is of chemical formula (4-A), Chemical formula (4-A) 3-1) * is L 1 ~L 4 Or the part that is combined with N, 3-2) p is an integer from 0 to 1, 3-3) When chemical formula (4-A) is directly bonded to N, p is 0, 3-4) R 13 and R 14 are independently hydrogen or methyl groups, 4) X 5 ~X 12 are independently hydrogen; deuterium; halogen; fluorenyl group; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group of; C3~C 30 Cycloalkyl group of; or C1~C 30 is an alkylamine group, 5) X 5 ~X 12 can combine with each other to form rings, Chemical formula (4) In the above chemical formula (4), 6) Z 1 and Z 2 are independently carbon atoms or nitrogen atoms, 7) Y 1 ~Y 14 are independently hydrogen; deuterium; halogen; fluorenyl group; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group of; C3~C 30 Cycloalkyl group of; or C1~C 30 is an alkylamine group, 8) Y 1 ~Y 14 can combine with each other to form rings, 9) Above X 1 ~X 14 , Y 1 ~Y 14 , and L 1 ~L 4 are respectively deuterium; halogen; C1~C 30 Alkyl group or C6~C 30 Silane group substituted or unsubstituted with an aryl group; siloxane group; boron group; germanium group; cyano group; amino group; nitro group; C1~C 30 Alkylthio group of; C1~C 30 Alkoxy group of; C6~C 30 Aryl alkoxy group of; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkyne group of; C6~C 30 Aryl group of; C6~C substituted with deuterium 30 Aryl group of; Fluorenyl group; C2~C containing at least one heteroatom selected from the group consisting of O, N, S, Si and P 30 Heterocyclic group of; C3~C 30 Aliphatic ring group; C7~C 30 Arylalkyl group of; C8~C 30 and combinations thereof, and may be further substituted with one or more substituents selected from the group consisting of arylalkenyl groups, and adjacent substituents may form a ring.
2. A photosensitive composition according to claim 1, characterized in that the average particle diameter of the reactive silica particles is 1 nm to 300 nm.
3. A photosensitive composition according to claim 1, characterized in that the reactive silica particles are contained in an amount of 0.1 wt% to 20 wt% based on the solid content excluding the solvent.
4. In the first paragraph, X in the chemical formula (3) 1 and X 2 At least one of them is of chemical formula (4-A), and X 3 and X 4 A photosensitive composition characterized in that at least one of the compounds has the chemical formula (4-A).
5. In the fourth paragraph, X in the chemical formula (3) 1 Inland X 4 The remaining unsubstituted compounds in the chemical formula (4-A) are independently C6~C 30 Aryl group of; C1~C 30 alkyl group of; or C3~C 30 A photosensitive composition characterized by a cycloalkyl group of; or a combination thereof.
6. A photosensitive composition characterized in that the chromophore comprising a structure represented by the chemical formula (3) in the first paragraph has a maximum absorption peak at a wavelength of 520 nm to 680 nm.
7. A photosensitive composition characterized in that, in the first paragraph, the cage width of the protecting group including the structure represented by the chemical formula (4) is 6.5 Å to 7.5 Å, and the volume of the protecting group is 10 Å to 16 Å.
8. A photosensitive composition characterized in that it comprises a chromophore comprising a structure represented by the chemical formula (3) and a protecting group comprising a structure represented by the chemical formula (4) in a molar ratio of 1:1 in the first paragraph.
9. A photosensitive composition according to claim 1, characterized in that the dye is contained in an amount of 0.1 wt% to 50 wt% based on the solid content excluding the solvent.
10. A photosensitive composition according to claim 1, characterized in that the alkali-soluble resin comprises a repeating unit represented by the following chemical formula (10) and a repeating unit represented by the following chemical formula (12): Chemical formula (10) Chemical formula (12) In the above chemical formula (10) and chemical formula (12), 1) * indicates the part where the combination is connected as a repeating unit, 2) R 1 and R 2 are independently hydrogen or C1~C 30 is an alkyl group, 3) L 1 and L 2 are independently a single bond, fluorenylene group, C1~C 30 alkylene, C6~C 30 Arylene, C2~C 30 Heterocyclic ring or C1~C 30 is an alkoxylene, 4) a and b are integers from 0 to 500, independently of each other. 5) X 1 C2~C containing oxygen atoms 30 is a heterocycle, 6) X 2 is the following chemical formula (12-1) or chemical formula (12-2), Chemical Formula (12-1) Chemical Formula (12-2) In the above chemical formulas (12-1) and (12-2), 6-1) * indicates the binding position, 6-2) L 20 is a single bond or C1~C 30 is alkylene, 6-3) R 4 is hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; or C1~C 30 is an alkoxycarbonyl group, 6-4) n is an integer from 1 to 10, 7) The above R 1 , R 2 , R 4 , X 1 , X 2 , L 1 , L 2 and L 20 are respectively deuterium; halogen; C1~C 30 Alkyl group or C6~C 30 Silane group substituted or unsubstituted with an aryl group; siloxane group; boron group; germanium group; cyano group; amino group; nitro group; C1~C 30 Alkylthio group of; C1~C 30 Alkoxy group of; C6~C 30 Aryl alkoxy group of; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkyne group of; C6~C 30 Aryl group of; C6~C substituted with deuterium 30 Aryl group of; Fluorenyl group; C2~C containing at least one heteroatom selected from the group consisting of O, N, S, Si and P 30 Heterocyclic group of; C3~C 30 Aliphatic ring group; C7~C 30 Arylalkyl group of; C8~C 30 and combinations thereof, and may be further substituted with one or more substituents selected from the group consisting of arylalkenyl groups, and adjacent substituents may form a ring.
11. In the 10th paragraph, X in the repeating unit structure represented by the chemical formula (10) 1 A photosensitive composition characterized by having any one of the structures represented by the following chemical formulas (10-1) to (10-3): Chemical Formula (10-1) Chemical Formula (10-2) Chemical Formula (10-3) 12. A photosensitive composition according to claim 10, characterized in that the copolymer resin further comprises at least one of a repeating unit represented by chemical formula (13) and a repeating unit represented by chemical formula (14): Chemical formula (13) Chemical formula (14) In the above chemical formula (13) and chemical formula (14), 1) R 5 and R 6 are independently hydrogen or C1~C 30 is an alkyl group, 2) L 3 is a single bond, fluorenylene group, C1~C 30 alkylene, C6~C 30 Arylene, C2~C 30 Heterocyclic ring or C1~C 30 is an alkoxylene, 3) Ar 1 Silver C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C1~C 30 Alkyl group of; C3~C 30 Cycloalkyl group of; C2~C 30 Alkenyl group of; C2~C30 alkynyl group; C1~C30 alkoxy group; C6~C 30 An aryloxy group; a fluorenyl group; a carbonyl group; an ether group; or a C1~C30 alkoxycarbonyl group, 4) c and d are independent integers from 1 to 500.
13. A photosensitive composition according to claim 1, characterized in that the total amount of the alkaline-soluble resin is 1 to 50 wt% based on the total amount of the photosensitive composition.
14. A photosensitive composition characterized in that it further comprises a dispersant having a structure represented by the following chemical formula (21) in the first paragraph: Chemical formula (21) In the above chemical formula (21), 1) Ar 21 Silver C3~C 30 Aliphatic ring group; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; or a combination thereof, 2) R 21 Silver C5~C 30 is an ethylene glycol chain group, 3) R 22 and R 23 are independently of each other, hydrogen; deuterium; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C3~C 30 Aliphatic ring group; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; C1~C 30 an alkoxycarbonyl group; or a combination thereof, 4) R 24 ~ R 26 are independently of each other, hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C3~C 30 Aliphatic ring group; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; C1~C 30 an alkoxycarbonyl group; or a combination thereof, 5) L 21 , L 24 and L 25 are independently a single bond; fluorenylene group; C1~C 30 alkylene; C6~C 30 Arylene of; C2~C 30 Heterocyclic ring of; C1~C 30 an alkoxylene; or a combination thereof, 6) d is an integer of 1 or 2, 7) With respect to the total 100 mol% of the total repeating units included in the compound represented by the above chemical formula (21), a is 10 to 30 mol%, b is 40 to 60 mol%, and c is 20 to 40 mol%. 8) The above Ar 21 , R 21 ~R 26 , L 21 , L 24 and L 25 are respectively deuterium; halogen; C1~C 30 Alkyl group or C6~C 30 Silane group substituted or unsubstituted with an aryl group; siloxane group; boron group; germanium group; cyano group; amino group; nitro group; C1~C 30 Alkylthio group of; C1~C 30 Alkoxy group of; C6~C 30 Aryl alkoxy group of; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkyne group of; C6~C 30 Aryl group of; C6~C substituted with deuterium 30 Aryl group of; Fluorenyl group; C2~C containing at least one heteroatom selected from the group consisting of O, N, S, Si and P 30 Heterocyclic group of; C3~C 30 Aliphatic ring group; C7~C 30 Arylalkyl group of; C8~C 30 and combinations thereof, and may be further substituted with one or more substituents selected from the group consisting of arylalkenyl groups, and adjacent substituents may form a ring.
15. In the 14th paragraph, a photosensitive composition characterized in that the chemical formula (21) is represented by the following chemical formula (23) or chemical formula (24): Chemical formula (23) Chemical formula (24) In the above chemical formula (23) and chemical formula (24), 1) Ar 21 , R 21 ~R 26 , L 21 , L 24 , L 25 and a~c are the same as defined in chemical formula (21) of the first paragraph above, 2) R 27 and R 28 are independently of each other, hydrogen; deuterium; halogen; C6~C 30 Aryl group of; C2~C containing at least one heteroatom among O, N, S, Si and P 30 Heterocyclic group of; C6~C 30 A fused ring group of an aliphatic ring and an aromatic ring; C3~C 30 Aliphatic ring group; C1~C 30 Alkyl group of; C2~C 30 Alkenyl group of; C2~C 30 Alkynyl group of; C1~C 30 Alkoxy group of; C6~C 30 Aryloxy group; fluorenyl group; carbonyl group; ether group; C1~C 30 an alkoxycarbonyl group; or a combination thereof.
16. A photosensitive composition characterized in that the weight average molecular weight of the dispersant comprising the structure represented by the chemical formula (21) in the 14th paragraph is 3,000 to 30,000 g / mol.
17. A photosensitive composition characterized in that the amine value of the dispersant containing the structure represented by the chemical formula (21) in the 14th paragraph is 30 to 150 mgKOH / g.
18. A photosensitive composition according to claim 1, characterized in that the reactive unsaturated compound is 1 to 50 wt% based on the total amount of the photosensitive composition.
19. A photosensitive composition according to claim 1, characterized in that the photoinitiator is 0.01 to 10 wt% based on the total amount of the photosensitive composition.
20. A pattern or film formed with a photosensitive composition according to paragraph 1.
Citation Information
Patent Citations
Colored curable resin composition
JP2016117858A
Novel compound, core-shell dye, photosensitive resin composition including the same, and color filter
KR1020180024290A
System for providing cloth fitting information of purchaser in connection with fitting room and system for intermediat using the same
KR1020190069353A
Aqueous graviure ink for shirink film and method for production of the same
KR1020240081867A
Bidirectional following cart
KR102171934B1