High-purity bismuth telluride-based semiconductor material

The hydrotreatment and grinding process produces high-purity bismuth telluride powder that can be doped for use in both p-type and n-type semiconductors, addressing impurity issues and enhancing thermoelectric performance in semiconductor materials.

WO2024239060A1PCT designated stage expired Publication Date: 2024-11-28C I CORP PTY LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/AU2024/050521
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-21
Filing Date
2024-05-21
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

Current methods for producing bismuth telluride-based semiconductor materials often result in impurities that hinder their effectiveness in thermoelectric applications, particularly in the fabrication of both p-type and n-type semiconductors.

Method used

A process involving hydrotreatment of impure bismuth telluride with hydrogen gas at elevated temperature and pressure to convert impurities into gaseous products, followed by grinding to produce high-purity bismuth telluride powder, which can be doped with conductive metals for use in both p-type and n-type semiconductor fabrication.

Benefits of technology

The process achieves high-purity bismuth telluride suitable for both p-type and n-type semiconductors, enhancing their thermoelectric performance by removing impurities and allowing for effective doping, thereby improving the efficacy of thermoelectric cells.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure AU2024050521_28112024_PF_FP_ABST
    Figure AU2024050521_28112024_PF_FP_ABST
Patent Text Reader

Abstract

A process for producing a high-purity bismuth telluride (Bi2Te3)-based semiconductor material is disclosed. The process comprises the steps of: (a) contacting an impure form of Bi2Te3 mineral with hydrogen (H2) gas at elevated temperature and / or pressure to convert impurities within the Bi2Te3 mineral to one or more gaseous products for removal therefrom; and (b) grinding / milling the obtained Bi2Te3 mineral to produce a high-purity Bi2Te3 powder suitable for use as a Bi2Te3-based semiconductor material. The high-purity Bi2Te3-based semiconductor material finds useful application in the fabrication of both p-type and n-type semiconductors, wherein the n-type semiconductor comprises Bi2Te3 doped with a conductive metal.
Need to check novelty before this filing date? Find Prior Art

Description

HIGH-PURITY BISMUTH TELLURIDE -BASED SEMICONDUCTOR MATERIALTECHNICAL FIELD

[0001] The present invention relates to a process for producing a high-purity bismuth telluride (Bi2Te3)-based semiconductor material, and a use of high-purity bismuth telluride (Bi2Tes)- based semiconductor material in the fabrication of both p-type and n-type semiconductors.BACKGROUND OF THE INVENTION

[0002] The following discussion of the prior art is provided to place the invention in an appropriate technical context and enable the advantages of it to be more fully understood. It should be appreciated, however, that any discussion of the prior art throughout the specification should not be considered as an express or implied admission that such prior art is widely known or forms part of the common general knowledge in the field.

[0003] In 1834, Peltier first described the impact of applying a voltage differential between two materials to generate a temperature difference and cause heat transfer. When an electric current is maintained in a material circuit made up of two different conductors, one junction cools and the other heats. This impact is magnified in circuitry made up of dissimilar semiconductors. For example, in a circuit consisting of a battery connected by two pieces of copper wire to a length of bismuth wire, a temperature rise occurs at the junction where the current passes from the copper wire to the bismuth wire, and a temperature decrease occurs at the junction where the current passes from the bismuth wire to the copper wire.

[0004] Essentially, the greatest efficacy of thermoelectric cells is found when an n-type semiconductor is linked with a p-type semiconductor. The electrons in n-type semiconductors have a negative charge, hence the term “n-type”. While in a p-type semiconductors, the absence of an electron creates the impression of a positive charge, hence the name “p-type”.

[0005] Bismuth Telluride (Bi2Tes) is considered to be one of the more promising thermoelectric materials. Generally, Bi2Te3 has a trigonal crystal structure, but it is known to crystallize to form several different crystal structures, depending on its stoichiometric composition. It is often shown that the n-type conducting nature of Bi2Te3 is obtained by doping the Bi2Te3 mineral with a conductive metal such as copper, while the intrinsic Bi2Te3 mineral is observed to have a p-type conducting nature.

[0006] It is an object of the present invention to overcome or ameliorate one or more the disadvantages of the prior art, or at least to provide a useful alternative.

[0007] It is an object of at least one preferred embodiment of the present invention to provide a high-purity bismuth telluride (Bi2Te3)-based semiconductor material for use in the fabrication of both p-type and n-type semiconductors for application in thermoelectric cells.SUMMARY OF THE INVENTION

[0008] According to a first aspect, the present invention provides a process for producing a high-purity bismuth telluride (Bi2Te3)-based semiconductor material, comprising the steps of: i. contacting an impure form of Bi2Te3 mineral with hydrogen (H2) gas at elevated temperature and / or pressure to convert impurities within the Bi2Te3 mineral to one or more gaseous products for removal therefrom; and ii. grinding / milling the obtained Bi2Te3 mineral to produce a high-purity Bi2Te3 powder suitable for use as a Bi2Te3-based semiconductor material.

[0009] According to a second aspect, the present invention provides a high-purity bismuth telluride (Bi2Te3)-based semiconductor material produced according to the first aspect.

[0010] According to a third aspect, the present invention provides the use of a high-purity bismuth telluride (Bi2Te3)-based semiconductor material produced according to the first aspect in the fabrication of a p-type semiconductor.

[0011] According to a fourth aspect, the present invention provides the use of a high-purity bismuth telluride (Bi2Te3)-based semiconductor material produced according to the first aspect in the fabrication of an n-type semiconductor, wherein the Bi2Te3-based semiconductor material is doped with a conductive metal via cation exchange.

[0012] The skilled person will appreciate that the present invention may provide one or more significant advantages and improvements in the field and / or in view of the prior art. For example, these advantages include:

[0013] The ability to produce bismuth telluride (Bi2Te3) in sufficiently high purity to render it suitable for use in the fabrication of both p-type and n-type semiconductorsDEFINITIONS

[0014] In describing and claiming the present invention, the following terminology will be used in accordance with the definitions set out below. It is also to be understood that the terminology used herein is for the purpose of describing particular embodiments of the invention only and is not intended to be limiting.

[0015] Unless defined otherwise, all technical and scientific terms used herein have the same meaning as commonly understood by one having ordinary skill in the art to which the invention pertains.

[0016] Unless the context clearly requires otherwise, throughout the description and the claims, the terms “comprise”, “'comprising”, and the like are to be construed in an inclusive sense as opposed to an exclusive or exhaustive sense; that is to say, in the sense of “including, but not limited to”. For example, a composition, mixture, process or method that comprises a list of elements is not necessarily limited to only those elements but may include other elements not expressly listed or inherent to such composition, mixture, process or method.

[0017] Where the applicant has defined an invention or a portion thereof with an open- ended term such as "comprising", it should be readily understood that (unless otherwise stated) the description should be interpreted to also describe such an invention using the terms "consisting essentially of" or "consisting of." In other words, with respect to the terms “comprising”, “consisting of’, and “consisting essentially of’, where one of these three terms is used herein, the presently disclosed and claimed subject matter may include the use of either of the other two terms. Thus, in some embodiments not otherwise explicitly recited, any instance of “comprising” may be replaced by “consisting of’ or, alternatively, by “consisting essentially of’.

[0018] While reference may be made in this disclosure to the invention comprising a combination of a plurality of elements, it is also understood that this invention is regarded to comprise combinations which omit or exclude one or more of such elements, even if this omission or exclusion of an element or elements is not expressly stated herein, unless it is expressly stated herein that an element is essential to the applicant' s combination and cannot be omitted. It is further understood that the related prior art may include elements from which this invention may be distinguished by negative claim limitations, even without any express statement of such negative limitations herein. It is to be understood, between the positive statements of applicant's invention expressly stated herein, and the prior art and knowledge ofthe prior art by those of ordinary skill which is incorporated herein even if not expressly reproduced here for reasons of economy, that any and all such negative claim limitations supported by the prior art are also considered to be within the scope of this disclosure and its associated claims, even absent any express statement herein about any particular negative claim limitations.

[0019] As used herein, with reference to numbers in a range of numerals, the terms "about," "approximately" and "substantially" are understood to refer to the range of -10% to +10% of the referenced number, preferably -5% to +5% of the referenced number, more preferably -1 % to + 1 % of the referenced number, most preferably -0 .1 % to +0 .1 % of the referenced number. Moreover, with reference to numerical ranges, these terms should be construed as providing support for a claim directed to any number or subset of numbers in that range. For example, a disclosure of from 1 to 10 should be construed as supporting a range of from 1 to 8, from 3 to 7, from 1 to 9, from 3.6 to 4.6, from 3.5 to 9.9, from 8 to 10, and so forth.

[0020] The terms “preferred” and “preferably” refer to embodiments of the invention that may afford certain benefits, under certain circumstances. However, other embodiments may also be preferred, under the same or other circumstances. Furthermore, the recitation of one or more preferred embodiments does not imply that other embodiments are not useful, and is not intended to exclude other embodiments from the scope of the invention.

[0021] The complete disclosures of the patents, patent documents and publications cited herein are incorporated by reference in their entirety as if each were individually incorporated.

[0022] Unless expressly stated to the contrary, "or" refers to an inclusive or and not to an exclusive or. For example, a condition A or B is satisfied by any one of the following: A is true (or present) and B is false (or not present), A is false (or not present) and B is true (or present), and both A and B are true (or present).

[0023] The term "and / or" used in the context of "X and / or Y" should be interpreted as "X," or "Y," or "X and Y." Similarly, "at least one of X or Y" should be interpreted as "X," or "Y," or "both X and Y."

[0024] The indefinite articles "a" and "an" preceding an element or component of the invention are intended to be non-restrictive regarding the number of instances (i.e., occurrences) of the element or component. Therefore "a" or "an" should be read to include oneor at least one, and the singular word form of the element or component also includes the plural unless the number is obviously meant to be singular.

[0025] As used herein, wt.% refers to the weight of a particular component relative to total weight of the referenced composition.

[0026] It will be understood that use of the term “between” herein when referring to a range of numerical values encompasses the numerical values at each endpoint of the range. For example, a temperature of between 80 °C and 150 °C is inclusive of a temperature of 80 °C and a temperature of 150 °C.

[0027] Various features of the embodiments of the invention disclosed herein are, for brevity, described in the context of a single embodiment, but may also be provided separately or in any suitable sub-combination. All combinations of the embodiments are specifically embraced by the illustrative embodiments disclosed herein just as if each and every combination was individually and explicitly disclosed. In addition, all sub-combinations listed in the embodiments describing such variables are also specifically embraced by the present compositions and are disclosed herein just as if each and every such sub-combination was individually and explicitly disclosed herein.

[0028] In the foregoing paragraphs, where various ratios of components have been disclosed. It will be appreciated that these ratios of components can be combined in any disclosed combination. For example, the ratio of A:B (which may be between about 100:1 and 1:100 or any range therein), may be combined with the ratio of C:D (which may be between about 50:1 and 1:50 or any range therein), and may be combined with the ratio of E:F (which may be between about 10:1 and about 1:10 or any range therein).BRIEF DESCRIPTION OF THE DRAWINGS

[0029] The aspects described above, as well as other apparent aspects, advantages, and objectives of the present invention are apparent from the detailed description below in combination with the drawing, in which:

[0030] Figure 1 shows a schematic representation of a process for producing a high-purity bismuth telluride (Bi2Te3)-based semiconductor material, and then using the Bi2Te3-based semiconductor material in the fabrication of p and n type semiconductors, where in n-type semiconductors, the highly purified Bi2Te3 material is doped with a conductive metal such as copper (Cu).DETAILED DESCRIPTION OF EMBODIMENTS

[0031] The skilled addressee will understand that the invention comprises the embodiments and features disclosed herein as well as all combinations and / or permutations of the disclosed embodiments and features.

[0032] The present invention is predicated includes mineral processing to eliminate impurities from the Bi2Te3 mineral.

[0033] In accordance with a preferred embodiment, the present invention provides a process for producing a high-purity bismuth telluride (Bi2Te3)-based semiconductor material.

[0034] As shown in Figure 1, the process comprises the following key steps of: i. contacting an impure form of Bi2Te3 mineral with hydrogen (H2) gas at elevated temperature and / or pressure to convert impurities within the Bi2Te3 mineral to one or more gaseous products for removal therefrom; and ii. grinding / milling the obtained Bi2Te3 mineral to produce high-purity Bi2Te3 powder suitable for use as a Bi2Te3-based semiconductor material.

[0035] Step (i) is essentially a hydrotreatment process operating at an elevated pressure (typically about 30 bar to about 100 bar) and elevated temperature (typically about 400°C to about 500 °C). Specifically, the hydrotreatment process involves contacting or subjecting the impure with hydrogen (H2) gas in a hydrogenation reactor under these elevated conditions while in the presence of a catalyst, such as nickel or cobalt. Impurities like sulfur, oxygen, and carbon are subsequently converted during this process into gaseous compounds that can be readily removed during the reaction.

[0036] To ensure that the desired level of purification is attained and that the properties of the Bi2Te3 mineral are not compromised, it is crucial to carefully control the process conditions and monitor the reaction.

[0037] In Step (ii), once the impurities have been removed, the obtained Bi2Te3 mineral is then ground or milled using a ball mill or the like to produce a fine powder of high-purity Bi2Te3 that can, in one embodiment, be subsequently moulded in a press to produce a p-type semiconductor.

[0038] Figure 1 also shows the additional steps required to produce an n-type semiconductor.

[0039] Specifically, the powdered high purity EfeTes semiconductor material is doped with a conductive metal such as copper. Copper can be doped into EfeTes by a cation exchange reaction in ethanol solution at room temperature.

[0040] Once doped, the resultant product is ground or milled again and then moulded in a press to produce an n-type semiconductor.

[0041] Although the invention has been described with reference to specific examples, it will be appreciated by those skilled in the art that the invention may be embodied in many other forms, and in particular features of any one of the various described examples may be provided in any combination in any of the other described examples. Various modifications and alterations to this invention will become apparent to those skilled in the art without departing from the scope and spirit of this invention. It should be understood that this invention is not intended to be unduly limited by the illustrative embodiments and examples set forth herein and that such examples and embodiments are presented by way of example only with the scope of the invention intended to be limited only by the claims set forth herein as follows.

Claims

CLAIMS1. A process for producing a high-purity bismuth telluride (Bi2Te3)-based semiconductor material, comprising the steps of: i. contacting an impure form of Bi2Te3 mineral with hydrogen (H2) gas at elevated temperature and / or pressure to convert impurities within the Bi2Te3 mineral to one or more gaseous products for removal therefrom; and ii. grinding / milling the obtained Bi2Te3 mineral to produce high-purity Bi2Te3 powder for use as a Bi2Te3-based semiconductor material.

2. The process according to claim 1, wherein the contacting step is conducted at an elevated pressure that falls within a range of about 30 bar to about 100 bar.

3. The process according to claim 1, wherein the contacting step is conducted at an elevated temperature that falls within a range of about 400 °C to about 500 °C.

4. The process according to claim 1, wherein the contacting step is conducted in the presence of a catalytic amount of a metal selected from nickel and cobalt.

5. A high-purity bismuth telluride (Bi2Te3)-based semiconductor material produced according to the process of any one of claims 1 to 4.

6. Use of a high-purity bismuth telluride (Bi2Te3)-based semiconductor material produced according to the process of any one of claims 1 to 4 in the fabrication of a p-type semiconductor.

7. Use of a high-purity bismuth telluride (Bi2Te3)-based semiconductor material produced according to the process of any one of claims 1 to 4 in the fabrication of an n-type semiconductor.

8. The use according to claim 7, wherein the Bi2Te3-based semiconductor material is doped with a conductive metal via cation exchange.

9. The use according to claim 8, wherein the conductive metal is copper.

Citation Information

Patent Citations

  • Method for preparing N-type Bi2Te3 based thermoelectric materials by refrigeration crystal bar processing waste

    CN103311426A

  • Preparation method of copper-doped bismuth telluride composite electrothermal material

    CN106992246A

  • Silver and copper halide doped bi2te3-as2se3 thermoelectric material

    US3258427A