Substrate processing method and substrate processing system
The substrate processing method and system address the inefficiencies in conventional edge trim processes by forming specific peripheral modified regions for precise edge removal, ensuring effective bonding and device layer protection, thus enhancing the semiconductor manufacturing process.
Patent Information
- Application Number
- PCT/JP2024/012409
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-23
- Filing Date
- 2024-03-27
- Publication Date
- 2024-11-28
AI Technical Summary
Conventional substrate processing systems fail to effectively remove the peripheral edge of bonded substrates during the edge trim process, as they do not consider the optimal formation position of the modified surface, leading to inefficiencies in bonding force reduction and edge removal.
A substrate processing method and system that form specific peripheral modified regions within the first substrate, allowing for precise removal of the upper and lower peripheral edges using laser irradiation and a wedge-shaped blade, ensuring the modified regions do not intersect inside the substrate after thinning, thereby controlling the stress and preventing damage to the device layer.
This approach enables efficient and precise removal of the peripheral edges, maintaining the bonding integrity and preventing damage to the device layer, thereby improving the edge trim process and enhancing the yield of semiconductor devices.
Smart Images

Figure JP2024012409_28112024_PF_FP_ABST
Abstract
Description
Substrate processing method and substrate processing system
[0001] The present disclosure relates to a substrate processing method and a substrate processing system.
[0002] Each of Patent Documents 1 to 3 discloses a substrate processing system for processing a laminated substrate formed by bonding a first substrate and a second substrate. The substrate processing system includes a modified layer forming device for forming a modified layer inside the first substrate, an interface processing device for modifying the interface where the first substrate and the second substrate are bonded, and an edge removing device for removing the edge portion of the first substrate.
[0003] International Publication No. 2019 / 176589 International Publication No. 2019 / 208298 International Publication No. 2019 / 208359
[0004] The technology according to the present disclosure appropriately removes the peripheral edge portion of the first substrate to be removed in a laminated substrate in which a first substrate and a second substrate are bonded together.
[0005] One aspect of the present disclosure is a substrate processing method for processing a laminated substrate in which a first substrate and a second substrate are bonded, comprising: forming a first peripheral modified region within the first substrate along the boundary between the peripheral portion and central portion of the first substrate to be removed; forming a second peripheral modified region radially within the first substrate, at least radially outward from the first peripheral modified region; removing an upper portion of the peripheral portion from the first substrate using the first peripheral modified region and the second peripheral modified region as base points; and forming the second peripheral modified region, wherein after the first substrate from which the upper portion of the peripheral portion has been removed is thinned, the first peripheral modified region and the second peripheral modified region intersect at a position where they do not remain within the first substrate.
[0006] According to the present disclosure, in a laminated substrate in which a first substrate and a second substrate are bonded together, the peripheral edge portion of the first substrate to be removed can be appropriately removed.
[0007] 1 is an explanatory diagram of overlapping wafers to be processed; FIG. 2 is a plan view showing an outline of the configuration of a wafer processing system; FIG. 3 is a plan view showing an outline of the configuration of a laser irradiation device; FIG. 4 is a side view showing an outline of the configuration of a laser irradiation device; FIG. 5 is an explanatory diagram showing main steps of wafer processing according to a first embodiment; FIG. 6 is an explanatory diagram showing main steps of wafer processing according to a second embodiment; FIG. 7 is an explanatory diagram of a second peripheral modified region in another embodiment; FIG. 8 is an explanatory diagram of a first peripheral modified region in another embodiment; FIG. 9 is an explanatory diagram of a second peripheral modified region in another embodiment; FIG. 10 is an explanatory diagram of a third peripheral modified region in another embodiment; FIG. 11 is an explanatory diagram of a method for removing an upper peripheral portion according to another embodiment; FIG. 12 is an explanatory diagram of a method for removing an upper peripheral portion according to another embodiment; FIG. 13 is an explanatory diagram showing how a first peripheral modified region and a second peripheral modified region are formed in another embodiment.
[0008] In the manufacturing process of semiconductor devices, a first wafer, which is a semiconductor substrate (hereinafter referred to as "wafer") having a plurality of devices such as electronic circuits formed on its surface, is bonded to a second wafer to form a laminated wafer, and the first wafer is thinned. Before the thinning process of the first wafer, a process called edge trimming is performed to remove the peripheral portion of the first wafer.
[0009] The edge trimming of the first wafer is performed using a substrate processing system disclosed in, for example, Patent Documents 1 to 3. In the substrate processing system, a laser beam is irradiated along the boundary between the peripheral portion and the central portion of the first wafer to be removed, forming a modified layer inside the first wafer. Furthermore, a laser beam is irradiated at the interface where the first wafer and the second wafer are bonded to form a modified surface in the peripheral portion. Then, in a peripheral removal device, the peripheral portion of the first wafer is removed starting from the modified layer. Since a modified surface has been formed on the peripheral portion, the bonding force between the first wafer and the second wafer can be reduced, allowing the peripheral portion to be appropriately removed.
[0010] As a result of extensive research, the inventors have found that it is preferable to form the modified surface above the thinned surface when thinning the first wafer, as will be described later. However, the edge trims disclosed in Patent Documents 1 to 3 do not take into consideration the position where the modified surface is formed, and there is room for improvement in conventional edge trims.
[0011] The technology disclosed herein appropriately removes a peripheral portion of a first substrate to be removed in a laminated substrate formed by bonding a first substrate and a second substrate. Hereinafter, a wafer processing system as a substrate processing system and a wafer processing method as a substrate processing method according to the present embodiment will be described with reference to the drawings. Note that in this specification and the drawings, elements having substantially the same functional configurations are designated by the same reference numerals, and redundant description will be omitted.
[0012] 1 , a wafer processing system 1 according to this embodiment, which will be described later, processes a laminated wafer T as a laminated substrate in which a first wafer W as a first substrate and a second wafer S as a second substrate are bonded together. Hereinafter, the surface of the first wafer W that is bonded to the second wafer S will be referred to as the front surface Wa, and the surface opposite the front surface Wa will be referred to as the back surface Wb. Similarly, the surface of the second wafer S that is bonded to the first wafer W will be referred to as the front surface Sa, and the surface opposite the front surface Sa will be referred to as the back surface Sb.
[0013] The first wafer W is a semiconductor wafer such as a silicon substrate, and at least one film is laminated on the front surface Wa side. Hereinafter, the film formed on the front surface Wa side will be referred to as a "laminated film." In this embodiment, the laminated film includes a device layer Dw and a bonding film Fw. The device layer Dw includes a plurality of devices. The bonding film Fw may include, for example, an oxide film (THOX film, SiO 2A bonding film Fw, such as a TEOS film, a SiC film, a SiCN film, or an adhesive, is used. The first wafer W is bonded to the second wafer S via the bonding film Fw. The peripheral edge We of the first wafer W is chamfered, and the thickness of the cross section of the peripheral edge We decreases toward its tip. The peripheral edge We is a portion to be removed in the edge trimming process described below, and is, for example, in a range of 0.5 mm to 3 mm in the radial direction from the outer edge of the first wafer W. In the following description, the region of the first wafer W that is radially inward of the peripheral edge We to be removed may be referred to as the central portion Wc.
[0014] The second wafer S has, for example, the same configuration as the first wafer W. That is, a device layer Ds and a bonding film Fs are formed as laminated films on the surface Sa side, and the peripheral portion is chamfered. Note that the second wafer S does not necessarily have to be a device wafer on which the device layer Ds is formed, and may be, for example, a support wafer that supports the first wafer W. In such a case, the second wafer S functions as a protective material that protects the device layer Dw of the first wafer W.
[0015] 1 illustrates an example in which a device layer and a bonding film are formed as laminated films on the surfaces of the first wafer W and the second wafer S. However, the type and number of laminated films are not limited to this.
[0016] 2 , wafer processing system 1 has a configuration in which a load / unload station 2 and a processing station 3 are integrally connected. In load / unload station 2, for example, a cassette C capable of accommodating a plurality of overlapped wafers T is loaded and unloaded between the load / unload station 2 and the outside. Processing station 3 is equipped with various processing devices that perform desired processing on overlapped wafers T.
[0017] The carry-in / out station 2 is provided with a cassette mounting table 10 on which a cassette C capable of accommodating a plurality of overlapped wafers T is mounted. A wafer transfer device 20 is provided adjacent to the cassette mounting table 10 on the positive side of the X-axis of the cassette mounting table 10. The wafer transfer device 20 moves on a transfer path 21 extending in the Y-axis direction, and is configured to be able to transfer the overlapped wafers T between the cassette C on the cassette mounting table 10 and a transition device 30, which will be described later.
[0018] In the loading / unloading station 2 , a transition device 30 for transferring the overlapped wafer T between the processing station 3 and the wafer transfer device 20 is provided adjacent to the wafer transfer device 20 on the positive side of the X axis of the wafer transfer device 20 .
[0019] In the processing station 3, a wafer transfer device 40, a laser irradiation device 50, an upper peripheral edge removal device 60, a lower peripheral edge removal device 70, and a cleaning device 80 are arranged.
[0020] The wafer transfer device 40 is provided on the positive X-axis side of the transition device 30. The wafer transfer device 40 is configured to be movable on a transfer path 41 extending in the X-axis direction, and is configured to be able to transfer the overlapped wafer T to the transition device 30, the laser irradiation device 50, the upper peripheral edge removal device 60, the lower peripheral edge removal device 70, and the cleaning device 80 in the carry-in / out station 2.
[0021] The laser irradiation device 50 irradiates the inside of the first wafer W with a modifying laser beam (e.g., a YAG laser or a fiber laser) to form a peripheral modified layer that serves as a base point for peeling off the upper part of the peripheral edge We. The laser irradiation device 50 also has a control device 51, which will be described later.
[0022] As shown in FIGS. 3 and 4 , the laser irradiation device 50 includes a chuck 100 that holds the overlapped wafer T on its upper surface. The chuck 100 suction-holds the back surface Sb of the second wafer S, with the first wafer W on top and the second wafer S on the bottom. The chuck 100 is supported by a slider table 102 via an air bearing 101. A rotation mechanism 103 is provided on the underside of the slider table 102. The rotation mechanism 103 incorporates, for example, a motor as a drive source. The chuck 100 is configured to be rotatable about a vertical axis by the rotation mechanism 103 via the air bearing 101. The slider table 102 is configured to be movable on rails 106 extending in the Y-axis direction on a base 105 via a movement mechanism 104 provided on the underside of the slider table 102. The drive source of the movement mechanism 104 is not particularly limited, but may be, for example, a linear motor.
[0023] A laser head 110 is provided above the chuck 100. The laser head 110 has a lens 111. The lens 111 is a cylindrical member provided on the lower surface of the laser head 110, and irradiates the inside of the overlapped wafer T held by the chuck 100, more specifically, the inside of the first wafer W, with laser light.
[0024] The laser head 110 is supported by a support member 112. The laser head 110 is configured to be able to move up and down by an elevating mechanism 114 along rails 113 extending in the vertical direction. The laser head 110 is also configured to be able to move in the Y-axis direction by a moving mechanism 115. The elevating mechanism 114 and the moving mechanism 115 are each supported by a support column 116.
[0025] An imaging mechanism 120 is provided above the chuck 100 on the Y-axis positive side of the laser head 110. The imaging mechanism 120 includes at least one camera. An image captured by the camera is output to a control device 51 or a control device 90, which will be described later. The laser irradiation device 50 determines the position of the overlapped wafer T on the chuck 100 based on the image obtained by the imaging mechanism 120, and then aligns the overlapped wafer T and determines the irradiation position of the laser light based on this. The imaging mechanism 120 is configured to be able to move up and down freely by an elevating mechanism 121, and is further configured to be able to move freely in the Y-axis direction by a moving mechanism 122. The moving mechanism 122 is supported by a support column 116.
[0026] In the illustrated example, the chuck 100 is configured to be rotatable relative to the laser head 110 and movable horizontally by the rotation mechanism 103 and the movement mechanism 104, but the laser head 110 may be configured to be rotatable relative to the chuck 100 and movable horizontally. Alternatively, both the chuck 100 and the laser head 110 may be configured to be rotatable relative to each other and movable horizontally.
[0027] The upper peripheral edge removal device 60 shown in Figure 2 removes the upper part of the peripheral edge We of the first wafer W (hereinafter referred to as the "upper peripheral edge Wea"; see Figure 5 described below) using the peripheral modified layer formed by the laser irradiation device 50 as a base point. The method for removing the upper peripheral edge Wea can be selected arbitrarily. In one example, the upper peripheral edge removal device 60 may insert, for example, a wedge-shaped blade between the first wafer W and the second wafer S.
[0028] The lower peripheral edge removal device 70 irradiates a lower portion of the peripheral edge We (hereinafter referred to as the "lower peripheral edge Web"; see FIG. 5 described later) of the first wafer W with a removal laser beam (e.g., a UV femtosecond laser) to remove the lower peripheral edge Web by laser ablation. The lower peripheral edge removal device 70 also has a control device 71 described later.
[0029] The lower peripheral edge removal device 70 has a configuration similar to that of the laser irradiation device 50, for example. That is, the lower peripheral edge removal device 70 may include a chuck that holds the overlapped wafer T, a laser head provided above the chuck, and an imaging mechanism. The chuck is configured to be movable horizontally and rotatable about a vertical axis. The laser head is configured to be movable horizontally and movable up and down. The laser head is configured to be able to irradiate the above-mentioned removal laser light that is irradiated onto the lower peripheral edge Web, instead of the modification laser light used in the laser irradiation device 50.
[0030] In this embodiment, the upper peripheral edge removal device 60 removes the upper peripheral edge Wea, and the lower peripheral edge removal device 70 removes the lower peripheral edge Web, thereby removing the entire peripheral edge We, i.e., performing edge trimming.
[0031] The cleaning device 80 performs a cleaning process on the first wafer W and the second wafer S after the edges have been trimmed by the upper peripheral edge removal device 60 and the lower peripheral edge removal device 70, thereby removing particles from these wafers. Any cleaning method can be selected.
[0032] The above-described wafer processing system 1 is provided with a control device 51, a control device 71, and at least one control device 90. The control device 51 individually controls the operation of the laser irradiation device 50. The control device 71 individually controls the operation of the lower peripheral edge removal device 70. The control device 90 comprehensively controls a series of wafer processing operations in the wafer processing system 1.
[0033] Controller 51, controller 71, and controller 90 each process computer-executable instructions that cause laser irradiation apparatus 50, under-peripheral edge removal apparatus 70, and wafer processing system 1 to perform the various steps described herein. Controller 51, controller 71, and controller 90 can each be configured to control the elements of laser irradiation apparatus 50, under-peripheral edge removal apparatus 70, and wafer processing system 1 to perform the various steps described herein. In one embodiment, some or all of controller 51 may be included in laser irradiation apparatus 50, some or all of controller 71 may be included in under-peripheral edge removal apparatus 70, and some or all of controller 90 may be included in wafer processing system 1.
[0034] The control devices 51, 71, and 90 may each include a processing unit, a storage unit, and a communication interface. The control devices 51, 71, and 90 may each be realized by, for example, a computer. The processing unit may be configured to read a program providing logic or routines that enable various control operations from the storage unit and execute the read program to perform various control operations. This program may be stored in the storage unit in advance or may be acquired via a medium when needed. The acquired program is stored in the storage unit and read from the storage unit and executed by the processing unit. The medium may be various computer-readable storage media or a communication line connected to the communication interface. The storage medium may be temporary or non-temporary. The processing unit may be a CPU (Central Processing Unit) or one or more circuits. The storage unit may include a RAM (Random Access Memory), a ROM (Read Only Memory), a HDD (Hard Disk Drive), a SSD (Solid State Drive), or a combination thereof. The communication interface may communicate between the laser irradiation device 50, the lower peripheral edge removal device 70, and the wafer processing system 1 via a communication line such as a LAN (Local Area Network).
[0035] In this embodiment, the control devices 51 and 71 are installed separately for the laser irradiation device 50 and the lower peripheral edge removal device 70, respectively, but the control devices 51 and 71 may be configured integrally with the control device 90. In other words, the operations of the laser irradiation device 50 and the lower peripheral edge removal device 70 may be controlled by the control device 90.
[0036] Next, two embodiments (a first embodiment and a second embodiment) of wafer processing performed using the wafer processing system 1 configured as described above will be described. In the first and second embodiments, the wafer processing involves edge trimming to remove the peripheral portion We of the first wafer W. At this time, the peripheral portion We is removed in stages, divided into an upper peripheral portion Wea and a lower peripheral portion Web.
[0037] In the first and second embodiments, before being processed in the wafer processing system 1, the first wafer W and the second wafer S are bonded together outside the wafer processing system 1 to form a laminated wafer T in advance.
[0038] Furthermore, in the first and second embodiments, after processing in the wafer processing system 1, a process for thinning the central portion Wc of the first wafer W is performed outside the wafer processing system 1. The process for thinning the first wafer W is optional. FIG. 5 is an explanatory diagram showing the main steps of wafer processing, and this explanatory diagram shows a thinned surface G (a surface to be thinned) when thinning the central portion Wc of the first wafer W. Note that a thinning device for thinning the central portion Wc of the first wafer W, such as a grinding device (not shown), may be provided outside the wafer processing system 1 as in this embodiment, or may be installed in the wafer processing system 1.
[0039] Wafer processing according to the first embodiment will be described. First, a cassette C containing a plurality of overlapping wafers T is placed on a cassette mounting table 10 in a carry-in / out station 2. Next, the overlapping wafers T are removed from the cassette C by a wafer transfer device 20 and transferred to a laser irradiation device 50 via a transition device 30 and a wafer transfer device 40.
[0040] In the laser irradiation device 50, as shown in FIG. 5A, the inside of the first wafer W is irradiated with a modifying laser beam L1 to form a first peripheral modified layer M1 and a second peripheral modified layer M2.
[0041] When forming the first peripheral modified layer M1, laser light L1 is irradiated into the first wafer W along the boundary between the peripheral portion We and the central portion We of the first wafer W. The boundary between the peripheral portion We and the central portion We is, for example, a boundary extending in the thickness direction of the first wafer W. When the first peripheral modified layer M1 is formed by this laser light L1, a first crack C1 extends from the first peripheral modified layer M1 along the boundary between the peripheral portion We and the central portion We. Then, a first peripheral modified region N1 including the first peripheral modified layer M1 and the first crack C1 is formed. The first peripheral modified region N1 extends between the back surface Wb of the first wafer W and a second peripheral modified region N2, which will be described later.
[0042] When forming the second peripheral modified layer M2, laser light L1 is irradiated in a surface direction (radial direction) into the first wafer W, at least radially outward from the first peripheral modified region N1 (first peripheral modified layer M1 and first crack C1) and above the thinned surface G of the first wafer W. When the second peripheral modified layer M2 is formed above the thinned surface G by this laser light L1, the second crack C2 extends from the second peripheral modified layer M2 in the surface direction of the first wafer W. Then, a second peripheral modified region N2 including the second peripheral modified layer M2 and the second crack C2 is formed. Note that the second peripheral modified region N2 is formed so that at least a point Q where the first peripheral modified region N1 and the second peripheral modified region N2 intersect (hereinafter referred to as the "intersection Q") is located above the thinned surface G.
[0043] These first and second peripheral modified regions N1 and N2 serve as starting points for removing the upper peripheral Wea. The order of forming the first peripheral modified region N1 and the second peripheral modified region N2 is arbitrary, but it is preferable to form the first peripheral modified region N1 after forming the second peripheral modified region N2. In this case, the extension of the first crack C1 in the first peripheral modified region N1 connects to the second peripheral modified region N2, preventing the first crack C1 from extending to the device layer Dw and, as a result, preventing damage to the device layer Dw.
[0044] The overlapped wafer T, in which the first peripheral modified region N1 and the second peripheral modified region N2 have been formed inside the first wafer W, is then transferred by the wafer transfer device 40 to the upper peripheral edge removal device 60. In the upper peripheral edge removal device 60, a blade B is inserted between the first wafer W and the second wafer S, as shown in FIG. 5B, to remove the upper peripheral edge Wea from the first wafer W. At this time, the upper peripheral edge Wea is peeled and removed from the central portion Wc of the first wafer W, using the first peripheral modified region N1 and the second peripheral modified region N2 as base points. In addition, the lower peripheral edge Web remains on the peripheral edge We of the first wafer W.
[0045] The overlapped wafer T from which the upper peripheral edge Wea of the first wafer W has been removed is then transported by the wafer transport device 40 to the lower peripheral edge removal device 70. In the lower peripheral edge removal device 70, a removal laser beam L2 is irradiated onto the lower peripheral edge Web, as shown in FIG. 5(c). The lower peripheral edge Web irradiated with the laser beam L2 is removed by laser ablation. By removing the upper peripheral edge Wea and the lower peripheral edge Web in this manner, the entire peripheral edge Wea is removed, completing the edge trim. Note that when removing the lower peripheral edge Web, the bonding film Fw below the lower peripheral edge Web may also be removed.
[0046] The overlapped wafer T from which the lower peripheral edge Web of the first wafer W has been removed is then transferred by the wafer transfer device 40 to the cleaning device 80. In the cleaning device 80, the first wafer W and / or the second wafer S from which the peripheral edge We has been removed are cleaned.
[0047] Thereafter, the overlapped wafer T that has been subjected to all the processes is transferred by the wafer transfer device 20 to the cassette C on the cassette mounting table 10 via the transition device 30. In this way, a series of wafer processes in the wafer processing system 1 is completed.
[0048] Next, a description will be given of wafer processing according to the second embodiment. The second embodiment differs from the first embodiment mainly in the modification processing of the first wafer W in the laser irradiation device 50.
[0049] In the laser irradiation device 50, as shown in FIG. 6(a), a modification laser beam L1 is irradiated onto the inside of the first wafer W to form a first peripheral modified layer M1, a second peripheral modified layer M2, and a third peripheral modified layer M3.
[0050] The methods for forming the first peripheral modified layer M1 and the second peripheral modified layer M2 are similar to those for forming the first peripheral modified layer M1 and the second peripheral modified layer M2 in the first embodiment, respectively. Then, a first peripheral modified region N1 including the first peripheral modified layer M1 and the first crack C1, and a second peripheral modified region N2 including the second peripheral modified layer M2 and the second crack C2 are formed.
[0051] When forming the third peripheral modified layer M3, laser light L1 is irradiated from the radially outer side of the second peripheral modified region N2 (second peripheral modified layer M2 and second crack C2) toward the second wafer S, for example, in the thickness direction of the first wafer W. When the third peripheral modified layer M3 is formed by this laser light L1, the third crack C3 extends from the third peripheral modified layer M3 in the thickness direction of the first wafer W. Then, a third peripheral modified region N3 including the third peripheral modified layer M3 and the third crack C3 is formed. The third peripheral modified region N3 extends between the second peripheral modified region N2 and the front surface Wa of the first wafer W.
[0052] The first, second, and third peripheral modified regions N1, N2, and N3 serve as base points for removing the upper peripheral Wea. The order of forming the first, second, and third peripheral modified regions N1, N2, and N3 is arbitrary, but as in the first embodiment, it is preferable to form the second peripheral modified region N2 before forming the first peripheral modified region N1.
[0053] 6B, in the upper peripheral edge removal device 60, a blade B is inserted between the first wafer W and the second wafer S, and the upper peripheral edge Wea is removed from the first wafer W. At this time, the upper peripheral edge Wea is peeled off and removed from the central portion Wc of the first wafer W, using the first peripheral modified region N1, the second peripheral modified region N2, and the third peripheral modified region N3 as base points.
[0054] In the lower peripheral edge removal device 70, the lower peripheral edge Web is irradiated with a removal laser beam L2 as shown in FIG. 6C. The lower peripheral edge Web irradiated with the laser beam L2 is removed by laser ablation. By removing the upper peripheral edge Wea and the lower peripheral edge Web in this manner, the entire peripheral edge We is removed, completing the edge trimming.
[0055] According to the first and second embodiments described above, the upper peripheral edge Wea can be removed starting from the peripheral modified region including at least the first peripheral modified region N1 and the second peripheral modified region N2. Furthermore, the lower peripheral edge Web can be removed by laser ablation. Therefore, the peripheral edge We of the first wafer W can be appropriately removed, thereby appropriately performing edge trimming.
[0056] Furthermore, if the second peripheral modified region N2 is formed radially inward from the first peripheral modified region N1 and is formed below the thinned surface G, the peripheral portion We will be removed and a portion of the second peripheral modified region N2 will remain inside the first wafer W after further thinning.
[0057] In this regard, according to the first and second embodiments, the second peripheral modified region N2 is formed inside the first wafer W so that at least the intersection Q of the first peripheral modified region N1 and the second peripheral modified region N2 is located above the thinned surface G of the first wafer W. In this case, even if the second peripheral modified region N2 is formed radially inward from the first peripheral modified region N1, the second peripheral modified region N2 can be removed when the central portion Wc of the first wafer W is thinned.
[0058] In the first embodiment described above, the thickness of the lower peripheral edge web remaining after removing the upper peripheral edge weave is smaller than the thickness of the lower peripheral edge web in the second embodiment. In this case, the second embodiment can reduce the amount of laser light L2 applied when removing the lower peripheral edge web with the lower peripheral edge removal device 70 compared to the first embodiment.
[0059] In the first and second embodiments described above, when forming the second peripheral modified region N2, it is preferable to form the second peripheral modified layer M2 from the outside to the inside in the radial direction. For example, if the laser beam L1 is irradiated from the inside to the outside in the radial direction inside the first wafer W, the stress acting by the laser beam L1 may accumulate inside the first wafer W, which may result in the second peripheral modified layer M2 being formed in an unexpected direction. In this regard, if the laser beam L1 is irradiated from the outside to the inside in the radial direction, the stress acting by the laser beam L1 can be released from the inside to the outside in the radial direction, making it easier to appropriately control the formation position of the second peripheral modified layer M2.
[0060] In the first and second embodiments, the first peripheral modified region N1 is formed after the second peripheral modified region N2 is formed as described above, so that the first crack C1 in the first peripheral modified region N1 extends to the second peripheral modified region N2, thereby preventing the first crack C1 from extending into the device layer Dw.
[0061] In this regard, as shown in Figure 7, the second peripheral modified region N2 may extend radially inward from the first peripheral modified region N1. In the following description, the portion of the second peripheral modified region N2 that extends radially inward from the first peripheral modified region N1 is referred to as the overstroke P. To form the overstroke P, as shown in Figure 7, laser light L1 may be irradiated radially inward from the first peripheral modified region N1 to form a second peripheral modified layer M2, and a second crack C2 may be propagated from the second peripheral modified layer M2 radially outward from the first peripheral modified region N1. Alternatively, the laser beam L1 may be irradiated radially inward of the first peripheral modified region N1, and the laser beam L1 may also be irradiated radially outward of the first peripheral modified region N1, causing the second crack C2 to extend from the second peripheral modified layer M2 radially outward of the first peripheral modified region N1, thereby forming an overstroke P including the second peripheral modified layer M2 and the second crack C2. In this example, the second peripheral modified region N2 is formed as described above, and then the first peripheral modified region N1 is formed.
[0062] In this case, because the second peripheral modified region N2 extends radially inward from the first peripheral modified region N1, the extension of the first crack C1 in the first peripheral modified region N1 can be reliably connected by the second peripheral modified region N2, thereby reliably preventing the first crack C1 from extending to the device layer Dw and preventing damage to the device layer Dw.
[0063] Here, when inserting the blade B into the upper peripheral edge removal device 60, there is a risk that an unexpected crack may occur at the radially inner tip of the second peripheral modified region N2, and this crack may extend to the front surface Wa of the first wafer W, causing peeling. In this regard, in the example shown in FIG. 7 , the intersection of the first peripheral modified region N1 and the second peripheral modified region N2, which serves as the fulcrum for removing the upper peripheral edge Wea, can be offset from the radially inner tip of the second peripheral modified region N2, which serves as the peeling fulcrum. This allows stress acting on the intersection of the first peripheral modified region N1 and the second peripheral modified region N2 during insertion of the blade B to be released radially inward, thereby suppressing the occurrence of an unexpected crack at the radially inner tip of the second peripheral modified region N2 and preventing peeling. It is even more advantageous to identify a position where unexpected cracks will not occur and set the range of the overstroke P to that position.
[0064] Even if an overstroke P is formed in the second peripheral modified region N2 as shown in FIG. 7, the overstroke P can be removed when thinning the central portion Wc of the first wafer W.
[0065] In the first and second embodiments described above, the first peripheral modified region N1 is formed in the thickness direction of the first wafer W, but the direction in which the first peripheral modified region N1 is formed is not limited to this. For example, as shown in Figure 8, the first peripheral modified region N1 may be formed in an oblique direction along the crystal orientation of silicon in the first wafer W. For example, the 111 crystal orientation of silicon is in a direction of approximately 70 degrees from the vertical direction, and the first peripheral modified region N1 is formed along this 111 crystal orientation.
[0066] Here, when inserting blade B into upper peripheral edge removal device 60, if the insertion force or insertion amount of blade B is increased to properly remove the upper peripheral edge Wea, as described above, an unexpected crack may occur from the radially inner tip of second peripheral modified region N2, which may cause separation between the first wafer W and the second wafer S.
[0067] In this regard, forming the first peripheral modified region N1 along the crystal orientation as in this example makes it easy to remove the upper peripheral weave in the first peripheral modified region N1. As a result, the insertion force and insertion amount of the blade B when removing the upper peripheral weave can be reduced, thereby suppressing unexpected cracks and peeling at the radially inner tip of the second peripheral modified region N2 described above.
[0068] In the first and second embodiments described above, the second peripheral modified region N2 is formed in the in-plane direction of the first wafer W. However, the direction in which the second peripheral modified region N2 is formed is not limited to this. For example, as shown in FIG. 9 , the second peripheral modified region N2 may be formed in an oblique direction relative to the in-plane direction of the first wafer W. This second peripheral modified region N2 is preferably formed in an oblique direction that rises from the outer side toward the inner side in the radial direction. In this case, the second peripheral modified region N2 in the central portion Wc of the first wafer W can be prevented from extending to a position lower than the thinned surface G of the first wafer W.
[0069] In the second embodiment described above, the third peripheral modified region N3 is formed in the thickness direction of the first wafer W. However, the direction in which the third peripheral modified region N3 is formed is not limited to this. For example, as shown in FIG. 10 , the third peripheral modified region N3 may be formed in a direction oblique to the thickness direction of the first wafer W.
[0070] In the first and second embodiments described above, the upper peripheral edge removal device 60 removes the upper peripheral edge Wea by inserting the blade B between the first wafer W and the second wafer S in the surface direction, but the method of removing the upper peripheral edge Wea is not limited to this.
[0071] Here, if the blade B is inserted in the surface direction in the upper peripheral edge removal device 60 to apply stress in a direction that separates the bond between the first wafer W and the second wafer S, an unexpected crack may occur from the radially inner tip of the second peripheral modified region N2, as described above, and separation may occur between the first wafer W and the second wafer S. Therefore, stress may be applied in a direction different from the surface direction, for example, in the direction in which the first peripheral modified region N1 is formed. The upper peripheral edge removal device 60 that applies such stress may have any configuration.
[0072] In the upper peripheral edge removal device 60, as shown in Fig. 11, for example, a pressure unit 200 may be used to apply pressure to the upper peripheral edge Wea from above, thereby applying downward stress along the first peripheral modified region N1. In this case, the pressure unit 200 may abut against the upper peripheral edge Wea and physically press it, or the pressure unit 200 may apply an impact to the upper peripheral edge Wea by spraying air or a water jet toward the upper peripheral edge We. In the example of Fig. 11, the first peripheral modified region N1 is formed in an oblique direction, which makes it easier to remove the upper peripheral edge Wea.
[0073] Furthermore, the upper peripheral edge removal device 60 may use a clamping unit 210, as shown in FIG. 12, to clamp the upper peripheral edge Wea from above and apply downward stress along the first peripheral modified region N1. The clamping unit 210 has an upper clamping member 211 and a lower clamping member 212. The overlapped wafer T is clamped with the upper clamping member 211 abutting against the upper peripheral edge Wea and the lower clamping member 212 abutting against a chuck 213 that holds the second wafer S. Note that in the example of FIG. 12, the first peripheral modified region N1 is also formed in an oblique direction, and in this case, the upper peripheral edge Wea can be more easily removed.
[0074] In addition, in the peripheral upper portion removal device 60, for example, the blade B shown in Figure 5 (b) may be inserted between the first wafer W and the second wafer S, and the blade B may be moved upward to apply stress upward along the first peripheral modified region N1.
[0075] In the first embodiment described above, the first peripheral modified layer M1 (first peripheral modified region N1) and the second peripheral modified layer M2 (second peripheral modified region N2) were formed using the laser irradiation device 50, but these peripheral modified layers M1 and M2 may be formed using a different laser irradiation device. Also, in the second embodiment, the first peripheral modified layer M1 (first peripheral modified region N1), the second peripheral modified layer M2 (second peripheral modified region N2), and the third peripheral modified layer M3 (third peripheral modified region N3) were formed, but these peripheral modified layers M1, M2, and M3 may be formed using a different laser irradiation device.
[0076] In the above first and second embodiments, the second peripheral modified region N2 was formed so that the intersection point Q was located above the thinned surface G of the first wafer W. In contrast, if the second peripheral modified region N2 is not formed radially inward from the first peripheral modified region N1, the second peripheral modified region N2 may be formed so that the intersection point Q is located below the thinned surface G.
[0077] As a method (control) for preventing the second peripheral modified region N2 from being formed radially inward of the first peripheral modified region N1, for example, the first peripheral modified region N1 may first be formed below the thinned surface G as shown in FIG. 13( a), and then the second peripheral modified region N2 may be formed so as to be located below the thinned surface G as shown in FIG. 13( b). In this case, a crack formed between the first peripheral modified layer M1 of the first peripheral modified region N1 and the second peripheral modified region N2 is connected. Specifically, by connecting the second crack C2 extending from the second peripheral modified layer M2 formed later to the first peripheral modified layer M1 formed earlier and located below the thinned surface G, the second crack C2 is prevented from being formed radially inward of the first peripheral modified region N1. In other words, the second crack C2 does not remain inside the first wafer W after thinning.
[0078] For example, the first peripheral modified region N1 may be formed after the second peripheral modified region N2 is formed. In this case, a crack that occurs between the second peripheral modified layer M2 and the first peripheral modified region N1 is connected. Specifically, the first crack C1 extending from the first peripheral modified layer M1 formed earlier may be connected to the second peripheral modified layer M2 formed later, thereby preventing the second peripheral modified region N2 from being formed radially inward (toward the device layer Dw) of the first peripheral modified region N1.
[0079] Furthermore, the timing for connecting the first peripheral modified region N1 and the second peripheral modified region N2, i.e., the timing for connecting the cracks, may be the timing for inserting blade B between the first wafer W and the second wafer S when removing the upper peripheral edge Wea.
[0080] When the second peripheral modified region N2 is formed below the thinned surface G in this manner, the thickness of the lower peripheral web can be reduced, thereby reducing the amount of the lower peripheral web that is removed. This shortens the time required to remove the lower peripheral web. This also reduces the total energy of the laser light L2 used to remove the lower peripheral web.
[0081] As shown in FIG. 13 , the first peripheral modified region N1 may be formed so as to extend from the back surface Wb (upper side) of the first wafer W toward the front surface Wa (lower side) of the first wafer W, sloping from the inner side to the outer side in the radial direction of the first wafer W. In such a case, the angle between the top portion Wep of the upper peripheral edge Wea formed by the first peripheral modified region N1 and the second peripheral modified region N2 is an obtuse angle (90 degrees or more). In this case, when removing the upper peripheral edge Wea from the first wafer W, the load on the top portion Wep of the upper peripheral edge Wea is smaller than when the angle is a right angle. As a result, it is possible to prevent a portion of the upper peripheral edge Wea from remaining on the first wafer W, thereby preventing a portion of the upper peripheral edge Wea from chipping off and generating particles.
[0082] As shown in Figure 13, the first peripheral modified region N1 may be formed to have a curved shape that is convex downward in side view. In this case, the angle between the top portion Wep of the peripheral upper portion Wea formed by the first peripheral modified region N1 and the second peripheral modified region N2 is made obtuse, and the first peripheral modified region N1 can be prevented from extending radially inward. As a result, the radial distance of the first peripheral modified region N1 can be reduced.
[0083] 13, when the first peripheral modified region N1 is formed at an angle or curve, it is preferable to form it from bottom to top. In this case, the first crack C1 can extend upward from the first peripheral modified layer M1 at the lower end of the first peripheral modified region N1. In other words, the first crack C1 can be prevented from extending in an unexpected direction, such as toward the device layer Dw. As a result, damage to the device layer Dw can be prevented, and product yield can be improved.
[0084] In the first and second embodiments described above, the laser irradiation device 50 forms at least the first peripheral modified region N1 and the second peripheral modified region N2. However, it is also possible to form multiple divided modified regions that serve as base points for dividing the upper peripheral region Wea into small pieces. Each divided modified region extends in the thickness direction of the first wafer W, radially outward of the first peripheral modified region N1. Specifically, the laser beam L1 is irradiated in the thickness direction of the first wafer W to form a divided modified layer, and then a crack is propagated from the divided modified layer in the thickness direction of the first wafer W to form a divided modified region including the divided modified layer and the crack. By forming multiple divided modified regions in the radial direction, a line of divided modified regions extending radially outward from the first peripheral modified region N1 is formed, and multiple lines of the same line are further formed in the circumferential direction. In such a case, when the upper peripheral edge removal device 60 wears the upper peripheral edge, the upper peripheral edge wear is divided into a plurality of small pieces, starting from the divided modified regions of the plurality of lines.
[0085] The embodiments disclosed herein should be considered to be illustrative in all respects and not restrictive. The above-described embodiments may be omitted, substituted, or modified in various ways without departing from the scope and spirit of the appended claims. For example, the components of the above-described embodiments may be arbitrarily combined. Such an arbitrary combination naturally provides the functions and effects of each of the components involved in the combination, and also provides other functions and effects that are apparent to those skilled in the art from the description of this specification.
[0086] Furthermore, the effects described herein are merely descriptive or exemplary and are not limiting. In other words, the technology according to the present disclosure may achieve other effects that would be apparent to a person skilled in the art from the description of this specification, in addition to or in place of the above-described effects.
[0087] REFERENCE SIGNS LIST 1 wafer processing system 50 laser irradiation device 60 peripheral upper portion removal device 90 control device G thinned surface N1 first peripheral modified region N2 second peripheral modified region Q intersection S second wafer T overlapped wafer W first wafer Wc central portion We peripheral portion
Claims
1. A substrate processing method for processing an overlapped substrate formed by bonding a first substrate and a second substrate, comprising: forming a first peripheral modified region inside the first substrate along the boundary between a peripheral portion and a central portion of the first substrate to be removed; forming a second peripheral modified region radially inside the first substrate, at least radially outward from the first peripheral modified region; removing an upper portion of the peripheral portion from the first substrate using the first peripheral modified region and the second peripheral modified region as base points; and forming the second peripheral modified region, such that after the first substrate from which the upper portion of the peripheral portion has been removed is thinned, the first peripheral modified region and the second peripheral modified region intersect at a position where they do not remain inside the first substrate.
2. A substrate processing method as described in claim 1, wherein at least the point where the first peripheral modified region and the second peripheral modified region intersect is formed above the thinned surface when thinning the central portion of the first substrate.
3. A substrate processing method as described in claim 1, wherein at least the point where the first peripheral modified region and the second peripheral modified region intersect is formed below the thinning surface when thinning the central portion of the first substrate.
4. A substrate processing method according to any one of claims 1 to 3, further comprising forming a third peripheral modified region inside the first substrate on the second substrate side from the second peripheral modified region.
5. A substrate processing method as described in claim 1 or 2, wherein the first peripheral modified region includes a first peripheral modified layer and a first crack extending from the first peripheral modified layer, the second peripheral modified region includes a second peripheral modified layer and a second crack extending from the second peripheral modified layer, and after forming the second peripheral modified region, the first peripheral modified region is formed, and the second peripheral modified region extends radially inward from the first peripheral modified region.
6. A substrate processing method according to any one of claims 1 to 3, wherein the second peripheral modified region is formed from the radially outer side toward the inner side of the first substrate.
7. A substrate processing method according to any one of claims 1 to 3, further comprising the steps of: removing an upper portion of the peripheral edge portion; irradiating a lower portion of the peripheral edge portion with laser light; and removing the lower portion of the peripheral edge portion.
8. A substrate processing method according to any one of claims 1 to 3, wherein the first peripheral modified region is formed along a crystal orientation of the first substrate.
9. A substrate processing method according to any one of claims 1 to 3, wherein stress is applied in a direction along the first peripheral modified region when removing the upper portion of the peripheral portion.
10. A substrate processing method according to any one of claims 1 to 3, wherein the first peripheral modified region extends from above to below the first substrate, sloping from the radial inner side to the radial outer side of the first substrate.
11. A substrate processing system for processing an overlapped substrate formed by bonding a first substrate and a second substrate, comprising: a laser irradiation device that forms a first peripheral modified region inside the first substrate along a boundary between a peripheral portion and a central portion of the first substrate to be removed, and forms a second peripheral modified region radially inside the first substrate at least radially outward from the first peripheral modified region; an upper peripheral portion removal device that removes an upper portion of the peripheral portion from the first substrate based on the first peripheral modified region and the second peripheral modified region; and a control device, wherein the control device performs control to form the second peripheral modified region so that the first peripheral modified region and the second peripheral modified region intersect at a position where they do not remain inside the first substrate, after thinning the first substrate from which the upper portion of the peripheral portion has been removed.
12. The substrate processing system of claim 11, wherein the control device executes control to form at least the intersection point of the first peripheral modified region and the second peripheral modified region above a thinning surface when thinning a central portion of the first substrate.
13. The substrate processing system of claim 11, wherein the control device executes control to form at least the intersection point of the first peripheral modified region and the second peripheral modified region below a thinning surface when thinning a central portion of the first substrate.
14. A substrate processing system according to any one of claims 11 to 13, wherein the laser irradiation device forms a third peripheral modified region inside the first substrate on the second substrate side from the second peripheral modified region.
15. A substrate processing system as described in claim 11 or 12, wherein the first peripheral modified region includes a first peripheral modified layer and a first crack extending from the first peripheral modified layer, and the second peripheral modified region includes a second peripheral modified layer and a second crack extending from the second peripheral modified layer, and the control device performs the following controls: control to form the first peripheral modified region after forming the second peripheral modified region; and control to form the second peripheral modified region so as to extend radially inward from the first peripheral modified region.
16. A substrate processing system according to any one of claims 11 to 13, wherein the control device executes control to form the second peripheral modified region from the radially outer side toward the radially inner side of the first substrate.
17. A substrate processing system according to any one of claims 11 to 13, comprising a lower edge removal device that, after removing an upper portion of the peripheral edge, irradiates a lower portion of the peripheral edge with laser light to remove the lower portion of the peripheral edge.
18. The substrate processing system according to any one of claims 11 to 13, wherein the control device executes control to form the first peripheral modified region along a crystal orientation of the first substrate.
19. A substrate processing system according to any one of claims 11 to 13, wherein the peripheral upper portion removal device applies stress in a direction along the first peripheral modified region when removing the upper portion of the peripheral portion.
20. A substrate processing system according to any one of claims 11 to 13, wherein the control device performs control to form the first peripheral modified region so that it extends from above to below the first substrate, and at an incline from the radial inner side to the radial outer side of the first substrate.
Citation Information
Patent Citations
Laser processing device setting method, laser processing method, laser processing device, thinning system, and substrate processing method
JP2020136442A
Semiconductor manufacturing apparatus and manufacturing method
JP2022136755A
Laser processing apparatus and laser processing method
JP2023069018A
Substrate processing system and substrate processing method
WO2019208359A1
Substrate processing device and substrate processing method
WO2021215145A1
Cited By
Laser processing method, method for manufacturing semiconductor device, and laser processing device
WO2026163510A1