Structure and processing device

WO2024241732A1PCT designated stage expired Publication Date: 2024-11-28USHIO INC +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/014266
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-24
Filing Date
2024-04-08
Publication Date
2024-11-28

Smart Images

  • Figure JP2024014266_28112024_PF_FP_ABST
    Figure JP2024014266_28112024_PF_FP_ABST
Patent Text Reader

Abstract

A structure according to one embodiment of the present invention comprises a main body part, a first moisture-proof layer, and a second moisture-proof layer. The main body part is constituted by stacking a plurality of sheet-like members that are mainly composed of carbon fibers, and has a first main surface and a second main surface, which are opposite to each other in the stacking direction of the plurality of sheet-like members. The first moisture-proof layer is superposed on the first main surface, and at least a part of the surface thereof on the reverse side from the surface that is superposed on the first main surface is composed of a ceramic material. The second moisture-proof layer is superposed on the second main surface, and is composed of a material that is different from the ceramic material.
Need to check novelty before this filing date? Find Prior Art

Description

Structure and processing device

[0001] The present invention relates to a structure containing carbon fibers and a processing device in which the structure is used.

[0002] Conventionally, various processing devices such as exposure devices and laser processing devices have been used. These processing devices often adopt a design in which components constituting the device are supported by a frame. For example, in the case of an exposure device, components such as a light emitting unit, a mask stage, a projection optical system, and a workpiece stage are supported by a frame. In the case of a laser processing device, components such as a laser emitting unit and a workpiece stage are supported by a frame. Examples of the workpiece include a substrate.

[0003] In such processing equipment, if the frame expands or contracts due to thermal expansion caused by changes in the ambient temperature or heat generated by the equipment itself, the positions of the components supported by the frame may change, which may result in a decrease in processing accuracy. Therefore, it is desirable to use a material with as low a coefficient of thermal expansion as possible for the material of the processing equipment frame.

[0004] The frame of the processing device also needs to have high rigidity (elastic modulus). For example, consider a case where a work stage is supported by the frame. The work stage frequently moves sequentially, for example, in step-and-repeat processes that expose divided areas of a substrate, or in drilling processes that form multiple through-holes in a substrate. As a result, the time spent moving the stage is often longer than the time spent actually performing the exposure process.

[0005] Therefore, if the work stage is supported by a frame with low rigidity, the frame will vibrate significantly with each successive movement of the work stage, and it will take a long time for the frame vibration to stop, i.e., the time until the next exposure or processing can be performed. As a result, the workpiece processing time will be longer, and the productivity of the device will decrease. Furthermore, if the frame's rigidity is low, it will be vulnerable to external vibrations and will be prone to shaking. This can also cause poor processing accuracy.

[0006] Another important requirement for frame components is low density, so that even large equipment can be relatively lightweight. To shorten the stage's movement time and increase its speed, the stage must be accelerated and decelerated at high speeds, but this is limited if the stage is heavy. For this reason, it is desirable for the moving parts to be as light as possible. Another option is to use a large drive motor, but this increases the weight, which in turn increases the cost of the equipment, requiring the floor of the factory where the equipment is installed to be reinforced.

[0007] Thus, it is desirable for the frame of a processing device to have characteristics such as high rigidity (elastic modulus) and low thermal expansion coefficient (thermal expansion coefficient) and density. Note that the conditions of high rigidity and low density can also be said to be the conditions of high specific rigidity (rigidity / specific gravity).

[0008] Properties that satisfy these conditions are often effective not only for frames, but also for the components that make up processing equipment. For example, a work stage on which a substrate or the like is placed must have a high degree of flatness in order to perform high-precision positioning. Furthermore, in order to perform high-precision positioning in a short time, it must be highly rigid and lightweight, i.e., have a high specific rigidity. Furthermore, it must not undergo dimensional deformation due to temperature changes, so a low coefficient of thermal expansion is required. Naturally, properties that satisfy these conditions are often effective for components other than work stages as well.

[0009] A material that has high rigidity, a small coefficient of thermal expansion, and a small density can be exemplified by carbon fiber reinforced plastic (CFRP).

[0010] CFRP is a composite material made by reinforcing resin with carbon fiber. To use the analogy of reinforced concrete, which is also made of composite materials, the resin corresponds to the concrete and the carbon fiber to the rebar. CFRP is made by impregnating carbon fiber with resin and turning it into a plate-shaped (sheet-like) component called prepreg. Multiple sheets of this prepreg are stacked in a mold, taking into consideration the fiber orientation, and then heated and pressed in an autoclave to harden and form the material.

[0011] Thermosetting resins such as epoxy resins are often used as the matrix (base material). CFRP is lightweight and has high strength, so it is used in a variety of applications, including golf clubs, fishing rods, aircraft, and automobiles.

[0012] CFRP has the property of absorbing moisture in the environment, expanding and causing dimensional deformation. Furthermore, since moisture penetrates and diffuses slowly into CFRP, the distribution of moisture concentration within CFRP is uneven and the state changes gradually. This can lead to problems such as deterioration of surface roughness and torsional deformation, which can cause various complex deformations.

[0013] Countermeasures against moisture absorption by CFRP are described in the following Patent Documents 1 and 2. Patent Document 1 describes a structure in which ceramic members are bonded to both sides of a CFRP member in a sandwiched manner, in particular, a method of coating the CFRP member with an inorganic material such as metal or ceramic.

[0014] Patent Document 2 describes bonding aluminum or ceramics to the end faces of a member in which CFRP is laminated.

[0015] JP 2009-248398 A JP 2017-80899 A

[0016] In exposure devices, laser processing devices, and the like, improving exposure accuracy and laser processing accuracy are important issues. Of course, improving processing accuracy is also important in other processing devices. As mentioned above, in order to achieve high accuracy in processing devices, it is effective to improve the characteristics of the frame, components, etc.

[0017] In view of the above circumstances, an object of the present invention is to provide a structure that exhibits characteristics that are effective in improving processing accuracy when used in the frame, components, etc. of a processing device, and a processing device using said structure.

[0018] To achieve the above object, one aspect of the present invention provides a structure comprising a main body, a first moisture-proof layer, and a second moisture-proof layer. The main body is formed by stacking a plurality of sheet-like members whose main component is carbon fiber, and has a first main surface and a second main surface that face each other in the stacking direction of the plurality of sheet-like members. The first moisture-proof layer is stacked on the first main surface, and at least a portion of the surface opposite to the side where it is stacked on the first main surface is made of a ceramic material. The second moisture-proof layer is stacked on the second main surface, and is made of a material different from the ceramic material.

[0019] In this structure, a first moisture-proof layer, at least a portion of whose surface is made of a ceramic material, is laminated on a first main surface of a main body formed by laminating multiple sheet-like members whose main component is carbon fiber. A second moisture-proof layer, made of a material different from the ceramic material, is laminated on a second main surface of the main body. By applying this structure to the frame or components of a processing device, it is possible to demonstrate properties that are effective in improving processing accuracy.

[0020] The entire surface of the first moisture-proof layer may be made of a ceramic material.

[0021] Each of the plurality of sheet-like members may be a prepreg made of carbon fiber impregnated with resin, and in this case, the main body may be a carbon fiber reinforced plastic member formed by laminating the prepregs.

[0022] The first moisture-proof layer may be made of low thermal expansion glass.

[0023] The first moisture-proof layer has a thermal expansion coefficient of −1×10 at temperatures of 20° C. to 130° C. in a direction parallel to the surface on the side laminated to the first main surface. -6 / °C or greater than 1 × 10 -6 / °C.

[0024] The first moisture proof layer may include a low thermal expansion glass that forms the surface, and an intermediate member that is disposed between the low thermal expansion glass and the first main surface.

[0025] The intermediate member may be made of a metal foil.

[0026] The second moisture-proof layer may be made of any one of a metal foil, a rubber tape on which the metal foil is formed, and a resin film on which a moisture-proof film is formed.

[0027] At least one of the first moisture-proof layer and the second moisture-proof layer may be bonded to the main body portion via an adhesive that hardens at low temperatures or an adhesive layer that exhibits adhesive strength at low temperatures.

[0028] The second moisture-proof layer may be configured by adhering the metal foil to the second main surface with an adhesive that hardens at a low temperature.

[0029] The first moisture-proof layer may be made of a material that causes a thermal residual stress of 6 MPa or less, which is caused by a step of bonding the first moisture-proof layer to the main body portion.

[0030] The thermal expansion coefficient of the first moisture-proof layer in a direction parallel to the surface of the first moisture-proof layer laminated on the first main surface at temperatures of 20°C to 130°C is -1×10 -6 / °C or greater than 1 × 10 -6 / °C.

[0031] The difference in thermal expansion coefficient between the first moisture-proof layer and the main body is 1×10 -6 / °C.

[0032] The first moisture-proof layer may be laminated over the entire first main surface, and in this case, the second moisture-proof layer may be laminated over the entire second main surface.

[0033] The first moisture-proof layer may be configured such that the surface made of a ceramic material serves as a processing surface to be processed.

[0034] The surface to be processed may be a surface to be subjected to flattening.

[0035] The main body may have a side surface between the first main surface and the second main surface. In this case, the structure may further include a third moisture-proof layer laminated on the side surface.

[0036] The third moisture-proof layer may be made of any one of a metal foil, a metal thin plate, and a rubber tape on which the metal foil is formed.

[0037] The third moisture-proof layer may be bonded to the side surface via an adhesive that hardens at low temperatures or a pressure-sensitive adhesive layer that exhibits adhesive strength at low temperatures.

[0038] The third moisture-proof layer may be configured by adhering the metal foil or the metal thin plate to the side surface with an adhesive that hardens at a low temperature.

[0039] A structure according to another aspect of the present invention includes a main body, a first moisture-proof layer, a second moisture-proof layer, and a third moisture-proof layer. The main body is formed by stacking a plurality of sheet-like members whose main component is carbon fiber, and has a first main surface and a second main surface that face each other in the stacking direction of the plurality of sheet-like members, and a side surface between the first main surface and the second main surface. The first moisture-proof layer is stacked on the first main surface. The second moisture-proof layer is stacked on the second main surface. The third moisture-proof layer is stacked on the side surface. At least one of the first moisture-proof layer and the second moisture-proof layer is made of a material other than a ceramic material.

[0040] In this structure, a first moisture-proof layer is laminated on a first main surface of a main body formed by stacking multiple sheet-like members primarily composed of carbon fiber, and a second moisture-proof layer is laminated on a second main surface. A third moisture-proof layer is also laminated on a side surface of the main body. At least one of the first and second moisture-proof layers is made of a material other than ceramic material. This allows the structure to exhibit properties that are effective in improving processing accuracy when applied to frames, components, etc. of processing equipment.

[0041] A structure according to another aspect of the present invention includes a main body, a first moisture-proof layer, and a second moisture-proof layer. The main body is composed of a plurality of sheet-like members primarily composed of carbon fiber, and has first and second principal surfaces facing each other. The first moisture-proof layer is laminated on the first principal surface, and at least a portion of the surface opposite the side laminated on the first principal surface is made of a ceramic material. The second moisture-proof layer is laminated on the second principal surface, and is made of a material different from the ceramic material. This structure configuration can also be applied to the frame or components of a processing device, thereby exhibiting properties that are effective in improving processing accuracy.

[0042] A structure according to another aspect of the present invention includes a main body, a first moisture-proof layer, a second moisture-proof layer, and a third moisture-proof layer. The main body is composed of a plurality of sheet-like members primarily composed of carbon fiber, and has first and second principal surfaces facing each other and a side surface between the first and second principal surfaces. The first moisture-proof layer is laminated on the first principal surface. The second moisture-proof layer is laminated on the second principal surface. The third moisture-proof layer is laminated on the side surface. At least one of the first moisture-proof layer and the second moisture-proof layer is composed of a material other than a ceramic material. This structure configuration can also exhibit properties effective for improving processing accuracy by applying it to the frame or components of a processing device.

[0043] A method for manufacturing a structure according to one embodiment of the present invention includes the following steps: a lamination step of stacking a plurality of sheet-like members composed primarily of carbon fiber; a joining step of joining the plurality of sheet-like members to each other: a first moisture-proof layer laminated on a first main surface, which is one main surface in the stacking direction of the plurality of sheet-like members; and a second moisture-proof layer laminated on a second main surface opposite to the first main surface. Furthermore, at least a portion of the surface of the first moisture-proof layer opposite to the side laminated on the first main surface is made of a ceramic material. Furthermore, the second moisture-proof layer is made of a material different from the ceramic material.

[0044] The joining process may include a process of integrally joining the plurality of sheet-like members, the first moisture-proof layer, and the second moisture-proof layer by heat-pressing, or a process of joining each of the first moisture-proof layer and the second moisture-proof layer to a main body portion in which the plurality of sheet-like members are joined to each other by heat-pressing.

[0045] A method for manufacturing a structure according to another aspect of the present invention includes the following steps: a lamination step of laminating a plurality of sheet-like members whose main component is carbon fiber; a first joining step of joining the plurality of sheet-like members to each other: a first moisture-proof layer laminated on a first main surface, which is one main surface in the lamination direction of the plurality of sheet-like members; and a second moisture-proof layer laminated on a second main surface opposite to the first main surface. A second joining step of joining a third moisture-proof layer to a side surface between the first and second main surfaces of the plurality of sheet-like members. Furthermore, at least one of the first moisture-proof layer and the second moisture-proof layer is made of a material other than a ceramic material.

[0046] A method for manufacturing a structure according to another aspect of the present invention includes the following steps: a molding step of forming a main body having a first main surface and the second main surface from a plurality of sheet-like members whose main component is carbon fiber; a first joining step of joining a first moisture-proof layer to the first main surface; and a second joining step of joining a second moisture-proof layer to the second main surface. At least a portion of the surface of the first moisture-proof layer opposite to the side where it is laminated on the first main surface is made of a ceramic material. The second moisture-proof layer is made of a material different from the ceramic material.

[0047] A method for manufacturing a structure according to another aspect of the present invention includes the following steps: a molding step of molding a main body portion having a first main surface, a second main surface, and a side surface between the first main surface and the second main surface using a plurality of sheet-like members whose main component is carbon fiber; a first joining step of joining a first moisture-proof layer to the first main surface; a second joining step of joining a second moisture-proof layer to the second main surface; and a third joining step of joining a third moisture-proof layer to the third main surface. Furthermore, at least one of the first moisture-proof layer and the second moisture-proof layer is made of a material other than a ceramic material.

[0048] A processing device according to one embodiment of the present invention is a processing device for processing a workpiece, and is configured using the structure described above.

[0049] The structure may be used as a work stage that holds the workpiece.

[0050] The processing apparatus may be configured as an exposure apparatus.

[0051] As described above, according to the present invention, it is possible to provide a structure that exhibits characteristics effective in improving processing accuracy when used in the frame or components of a processing device, a method for manufacturing the structure, and a processing device using the structure. Note that the effects described here are not necessarily limited, and may be any of the effects described in this disclosure.

[0052] 1 is a schematic diagram (side view) showing an example of the basic configuration of a structure according to a first embodiment; FIG. 2 is a schematic diagram (perspective view) showing an example of the basic configuration of a structure according to a first embodiment; FIG. 3 is a schematic diagram (exploded perspective view) showing an example of the basic configuration of a structure according to a first embodiment; FIG. 4 is a graph showing the results of an accelerated moisture absorption test verifying the presence or absence of moisture-proof layers on the first and second main surfaces of a CFRP member and the change in moisture-absorption expansion strain over time; FIG. 5 is a graph showing the change in the change in moisture-absorption expansion strain over time in Examples 1 to 8; FIG. 6 is a table showing the moisture-absorption expansion strain and reference ratios in Examples 1 to 8; FIG. 7 is a schematic diagram (perspective view) showing an example of the basic configuration of a structure according to a second embodiment; FIG. 8 is a graph showing the change in the change in moisture-absorption expansion strain over time in Examples 9 to 20; Fig. 15 is a schematic diagram showing a schematic configuration of a laser processing device which is an example of a processing device. Fig. 16 is a schematic diagram showing a configuration example of a structure according to another embodiment. Fig. 17 is a schematic diagram showing a configuration example of a CFRP member according to another embodiment. Fig. 18 is a schematic diagram showing an internal structure of the CFRP member shown in Fig. 14.

[0053] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0054] 1 to 3 are schematic diagrams showing a basic configuration example of a structure according to a first embodiment of the present invention. Fig. 1 is a side view of the structure 1 as seen from the side. Fig. 2 is a perspective view of the structure 1 as seen from an oblique angle. Fig. 3 is an exploded perspective view showing the components of the structure 1 in an exploded form.

[0055] In this embodiment, the structure 1 is a CFRP structure containing carbon fiber reinforced plastic (CFRP).

[0056] Hereinafter, for ease of understanding of the explanation, the left-right direction, front-rear direction, and up-down direction will be defined for convenience with respect to the structure 1. Specifically, the X direction in the drawing is the left-right direction (the positive side of the X axis is the right side, and the negative side is the left side), the Y direction in the drawing is the front-rear direction (the positive side of the Y axis is the rear side, and the negative side is the front side), and the Z direction in the drawing is the up-down direction (the positive side of the Z axis is the upper side, and the negative side is the lower side).

[0057] Of course, the application of this technology does not limit the orientation of the structure 1, nor does it limit which part of the structure 1 is the front side part and which part is the side side part.

[0058] 3 is a diagram created to facilitate understanding of the configuration of the structure 1. It does not necessarily mean that the structure 1 has a configuration in which each component can be clearly disassembled as shown in FIG. 3 (although such a configuration is of course also included).

[0059] As shown in FIGS. 1 to 3, the structure 1 has a CFRP member 2 , a first moisture-proof layer 3 , and a second moisture-proof layer 4 .

[0060] The CFRP member 2 is formed by laminating a plurality of prepregs 5. The prepregs 5 are sheet-like members whose main component is carbon fiber. Specifically, the prepregs 5 are sheet-like members in which carbon fibers are impregnated with resin while maintaining the fiber directionality.

[0061] In this embodiment, multiple prepregs 5 are stacked in the vertical direction (Z direction) and integrated by heat and pressure bonding. Specifically, the CFRP member 2 is formed by heating to approximately 120°C to 130°C under reduced pressure and then pressurizing (press bonding) the prepregs to harden them.

[0062] 1 to 3, the vertical direction (Z direction) is the stacking direction of the multiple prepregs 5. Conversely, Figures 1 to 3 can also be said to be drawings in which the stacking direction of the multiple prepregs 5 with respect to the structure 1 is defined as the vertical direction (Z direction).

[0063] The matrix resin constituting the prepreg 5 is, for example, a thermosetting epoxy resin. Alternatively, other thermosetting resins such as unsaturated polyester, vinyl ester, phenol, cyanate ester, and polyimide can also be used as the matrix resin.

[0064] The CFRP member 2 is a high-strength material while having a lower density (i.e., lighter weight) than metal materials such as iron and aluminum. It is also possible to use standard CFRP plates of standard dimensions (standard dimensions) that can be stocked inexpensively (for example, 5 mm UD (Uni-Directional) material) as the multiple sheet-like members whose main component is carbon fiber.

[0065] In the structure 1 according to this embodiment, the first moisture proof layer 3 and the second moisture proof layer 4 can be integrally formed when the CFRP member 2 is formed. Of course, it is also possible to join the first moisture proof layer 3 and the second moisture proof layer 4 to the formed CFRP member 2. In other words, in applying the present technology, any method can be used as a joining method for joining the first moisture proof layer 3 and the second moisture proof layer 4 to the CFRP member 2.

[0066] The method of integrally molding the first moisture barrier layer 3 and the second moisture barrier layer 4 when molding the CFRP member 2 is advantageous in shortening the time and reducing the cost required to manufacture the structure 1. On the other hand, when the first moisture barrier layer 3 and the second moisture barrier layer 4 are adhesively bonded to the molded CFRP member 2, thermal residual stress can be reduced, which is advantageous in reducing the risk of deformation due to long-term relaxation of thermal residual stress. Thermal residual stress will be described in detail later.

[0067] As shown in Fig. 3, the CFRP member 2 has an approximate external shape of a rectangular parallelepiped. The CFRP member 2 has a first main surface 6 and a second main surface 7 that face each other in the stacking direction of the multiple prepregs 5, i.e., the vertical direction (Z direction). In this embodiment, the upper surface of the upper side of the CFRP member 2 is the first main surface 6, and the lower surface of the lower side is the second main surface 7. However, without being limited thereto, it is also possible to practice the present technology with the lower surface of the CFRP member 2 as the first main surface and the upper surface as the second main surface.

[0068] The CFRP member 2 also has side surfaces 8 between the first main surface 6 and the second main surface 7. In this embodiment, the side surfaces 8 are four surfaces: a left side surface 8 a, a right side surface 8 b, a front side surface 8 c, and a rear side surface 8 d.

[0069] The first main surface 6 and the second main surface 7 of the CFRP member 2 are also called flatwise surfaces of the CFRP member 2. The side surface 8 of the CFRP member 2 is also called edgewise surfaces of the CFRP member 2.

[0070] In this embodiment, the CFRP member 2 corresponds to an embodiment of a main body according to the present invention.

[0071] The first moisture proof layer 3 is laminated on the first main surface 6 of the CFRP member 2. As shown in FIGS. 1 to 3 , the first moisture proof layer 3 is laminated on the entire first main surface 6. Furthermore, at least a portion of a surface 9 of the first moisture proof layer 3 opposite to the side where the first moisture proof layer 3 is laminated on the first main surface 6 is made of a ceramic material. In this embodiment, the surface 9 corresponds to the upper surface of the upper side of the first moisture proof layer 3. Furthermore, in this embodiment, the entire surface 9 of the first moisture proof layer 3 is made of a ceramic material.

[0072] The second moisture-proof layer 4 is laminated on the second main surface 7. As shown in Figures 1 to 3, the second moisture-proof layer 4 is laminated on the entire second main surface 7. The second moisture-proof layer 4 is made of a material other than a ceramic material.

[0073] A method for manufacturing the structure 1 according to this embodiment includes joining (including integral molding) a CFRP member 2 having a desired size in terms of left-right width (size in the left-right direction) and front-to-back width (size in the front-to-back direction) when viewed from above to a moisture barrier layer (first moisture barrier layer 3 / second moisture barrier layer 4).

[0074] Without being limited to this, a method may be used in which the CFRP member 2 and the moisture-proof layer (first moisture-proof layer 3 / second moisture-proof layer 4) are joined (including integral molding) together in a state in which the left-right width and top-bottom width when viewed from above are larger than the desired size, and then cutting is performed so that the left-right width and top-bottom width are the desired size.

[0075] The CFRP is molded so that the left-right and up-down widths when viewed from above are larger than the desired size. The CFRP member 2 is then produced by cutting out the left-right and up-down widths to the desired size. The first moisture barrier layer 3 and the second moisture barrier layer 4 are bonded to the first main surface 6 and the second main surface 7 of the produced CFRP member 2. This method can also be used.

[0076] In the following description, the process of cutting out the CFRP member 2 (plurality of prepregs 5) having the desired left-right and vertical widths will be omitted in some cases. That is, the structure 1 will be mainly described in terms of joining together the CFRP member 2 (plurality of prepregs 5) having the desired left-right and vertical widths, the first moisture barrier layer 3, and the second moisture barrier layer 4.

[0077] Of course, the various technical matters described below can be implemented in appropriate combination with the process of cutting out the CFRP member 2 so that the left-right width and the top-bottom width are the desired sizes. For example, the content of the following description of creating a CFRP member 2 by heat-pressing a plurality of prepregs 5 can be applied not only to a state in which the left-right width and the front-to-back width are the same size as desired, but also to a state in which the left-right width and the front-to-back width are larger than the desired size.

[0078] In the following explanation, the content of manufacturing the structure 1 by integral molding by heat-pressing a plurality of prepregs 5 and moisture-proof layers (first moisture-proof layer 3 / second moisture-proof layer 4) can be applied not only to a state in which the left-right width and front-to-back width are the desired size, but also to a state in which the left-right width and front-to-back width are larger than the desired size.

[0079] Of course, if integral molding or joining of parts is performed when the left-right width and front-to-back width are larger than the desired size, a cutting process can be performed at an appropriate time thereafter so that the left-right width and top-to-bottom width are the desired size.

[0080] [CFRP Member] The CFRP member 2 is integrally molded by applying pressure and heat curing a plurality of prepregs 5. Examples of prepregs 5 include pitch-based prepregs that are characterized by high elasticity and high vibration damping, and PAN-based prepregs that are characterized by high strength.

[0081] The pitch-based carbon fiber (CF) that makes up the pitch-based prepreg has a high elastic modulus. Therefore, even if the matrix resin thermally expands, the change can be suppressed, making it possible to reduce the coefficient of thermal expansion (linear expansion coefficient). Furthermore, even if the matrix resin (e.g., epoxy resin) tries to expand due to moisture absorption, the pitch-based carbon fiber can suppress the change.

[0082] Therefore, pitch-based prepregs can be made smaller in terms of moisture-absorbing expansion (deformation) than PAN-based prepregs. Whether the cause of the expansion (deformation) is thermal expansion or moisture-absorbing expansion, the basic behavior (expansion mode) is the same. Furthermore, pitch-based prepregs, which have high vibration damping properties, are advantageous for the application of the present invention.

[0083] [Moisture-proof layer] The first moisture-proof layer 3 and the second moisture-proof layer 4 have moisture-proof performance for suppressing moisture absorption (adsorption of moisture) of the CFRP member 2. The moisture-proof performance can be evaluated using, for example, the water vapor transmission rate (WVTR).

[0084] In this embodiment, the moisture-proof performance of the first moisture-proof layer 3 and the second moisture-proof layer 4 is such that the water vapor permeability at 40°C and 90% RH is 1.0 g / (m 2 The water vapor permeability is 1×10 -1 g / (m 2 The moisture-proof performance of the first moisture-proof layer 3 and the second moisture-proof layer 4 is called high barrier property. -2 g / (m 2 It is preferred that the moisture-proof performance be such that the moisture-proof performance is equal to or less than 1 / 2 day. Of course, the smaller the water vapor permeability, the higher the moisture-proof performance.

[0085] [First Moisture Proof Layer] The first moisture proof layer 3 having the surface 9 made of a ceramic material can be realized, for example, by laminating a ceramic member made of a ceramic material on the first main surface 6 of the CFRP member 2.

[0086] As the ceramic member, for example, low thermal expansion glass can be used. Low thermal expansion glass is glass with a small linear expansion coefficient, and includes crystallized glass, synthetic quartz glass, borosilicate glass, etc. Among these, crystallized glass is glass that has both crystallinity and transparency, and for example, heat-resistant crystallized glass "Neoceram" manufactured by Nippon Electric Glass Co., Ltd. (NEG) can be used. Of course, ceramic members other than low thermal expansion glass may also be used.

[0087] In the present disclosure, "low thermal expansion glass" refers to a glass having a thermal expansion coefficient (linear expansion coefficient) of ±1×10 at temperatures of 20°C to 130°C in a direction parallel to the joining surface. -6 / °C. The notation " / °C" may be omitted in some cases.

[0088] The coefficient of thermal expansion (CTE) is a value that indicates the change in length or volume of an object caused by a rise in temperature, expressed as the rate of change per 1 K (1 °C). For example, it can be measured and evaluated using a method that uses optical interference in accordance with JIS R3251 (1995). Alternatively, it can be evaluated by measuring the displacement on the surface or inside the CFRP using a strain gauge.

[0089] When measuring the thermal expansion coefficients of the CFRP member 2 (plurality of prepregs 5), the first moisture barrier layer 3, and the second moisture barrier layer 4, it is preferable to measure them before joining them to other members. In this case, the thermal expansion coefficients of each member are measured in directions parallel to the surfaces that can become the joining surfaces. Of course, this is not limited to this. In this embodiment, the directions parallel to the joining surfaces are the left-right direction (X direction) and the front-back direction (Y direction).

[0090] Furthermore, for a non-isotropic member such as the CFRP member 2, when the thermal expansion coefficient in the direction parallel to the joining surface at 20°C to 130°C is viewed microscopically, it may not be uniform in the thickness direction of the member. In this case, the present technology can be applied by using the average value of the thermal expansion coefficients measured as different values ​​in the thickness direction as the thermal expansion coefficient parallel to the joining surface of the member.

[0091] In the following description, when indicating the coefficient of thermal expansion, the condition "at temperatures of 20°C to 130°C in a direction parallel to the joining surface" may be omitted.

[0092] The first moisture-proof layer 3 may be configured to include a ceramic member disposed on the surface 9 and an intermediate member disposed between the ceramic member and the first main surface 6. The ceramic member may be, for example, low-thermal expansion glass. The intermediate member may be, for example, a metal foil containing a metal as its main component. For example, a metal foil made of copper (Cu), aluminum (Al), titanium (Ti), stainless steel (SUS), Super Invar, or the like may be used.

[0093] In this way, a moisture-proof layer having a multilayer structure made of low-thermal expansion glass and metal foil can be used as the first moisture-proof layer 3. By disposing the low-thermal expansion glass on the surface 9 side, the first moisture-proof layer 3 having the surface 9 made of a ceramic member is realized. Of course, a ceramic member other than low-thermal expansion glass may be used. Furthermore, a member other than metal foil may be used as the intermediate member. Furthermore, the intermediate member itself may have a multilayer structure.

[0094] [Second Moisture Barrier Layer] Any member having moisture barrier properties and a structure other than a ceramic material can be used as the second moisture barrier layer 4. That is, the second moisture barrier layer 4 can be realized by laminating a member having moisture barrier properties and a structure other than a ceramic material on the second main surface 7 of the CFRP member 2.

[0095] For example, the second moisture-proof layer 4 can be made of a metal foil, a rubber tape on which a metal foil is formed (laminated), or a resin film on which a moisture-proof film is formed.

[0096] The metal foil may be made of, for example, copper (Cu), aluminum (Al), titanium (Ti), stainless steel (SUS), super invar, etc. The rubber tape on which the metal foil is formed may be, for example, a butyl tape with an Al foil.

[0097] The resin film on which the moisture-proof coating is formed can be, for example, a high-barrier film in which a moisture-proof coating of alumina, silica, or the like is coated on a PET (polyethylene terephthalate) film or the like by PVD, CVD, etc. Note that the resin film on which the moisture-proof coating is formed can also be called a moisture-proof coated film.

[0098] When using a resin film on which a moisture-proof membrane is formed as the second moisture-proof layer 4, it is effective to laminate the film so that the moisture-proof membrane faces the CFRP member 2. This is because it is possible to eliminate the influence of water vapor transmission through the base film itself, such as PET, and because the base film acts as a protective layer, improvements in performance and reliability can be expected.

[0099] In particular, metal foil does not allow water vapor to pass through, so the water vapor permeability is zero, making it possible to demonstrate extremely high moisture-proofing performance.

[0100] [Method for Manufacturing Structure 1] The method for manufacturing the structure 1 can include the following steps: a lamination step of stacking a plurality of sheet-like members (a plurality of prepregs 5) composed primarily of carbon fiber; and a joining step of joining the plurality of sheet-like members to each other: a first moisture-proof layer 3 laminated on a first main surface 6, which is one main surface in the lamination direction of the plurality of sheet-like members; and a second moisture-proof layer 4 laminated on a second main surface 7 opposite the first main surface 6. As described above, at least a portion of the surface 9 of the first moisture-proof layer 3 opposite the side laminated on the first main surface 6 (in this embodiment, the entire surface 9) is made of a ceramic material. The second moisture-proof layer 4 is made of a material other than the ceramic material.

[0101] [Method of joining first moisture proof layer 3 / second moisture proof layer 4] In the joining step, any method can be used to join the moisture proof layers (first moisture proof layer 3 / second moisture proof layer 4) to the CFRP member 2. For example, as a method of joining the moisture proof layers, a method can be used in which the moisture proof layers are directly and integrally molded when the CFRP member 2 is molded (hereinafter, this may be referred to as an integral molding method).

[0102] As a method for joining the moisture-proof layer, it is also possible to adopt a method in which the moisture-proof layer is bonded to the molded CFRP member 2 using an adhesive (hereinafter, this may be referred to as an adhesive bonding method).

[0103] Another method for joining the moisture-proof layer is to use an adhesive tape such as double-sided tape that has excellent moisture-proof properties to bond the moisture-proof layer (hereinafter, this may be referred to as the tape bonding method).

[0104] Furthermore, when a rubber tape or the like on which a metal foil is formed is used as the moisture-proof layer, an adhesive layer is formed on the moisture-proof layer, and this adhesive layer bonds the moisture-proof layer to the CFRP member 2. In this way, a method can also be employed in which the adhesive layer in the moisture-proof layer bonds the moisture-proof layer to the CFRP member 2 (hereinafter, this method may be referred to as an adhesive layer bonding method).

[0105] It is also possible to employ a method that combines the integral molding method and the adhesive lamination method using a sheet-like adhesive. For example, multiple prepregs 5 are stacked, and moisture-proof layers (first moisture-proof layer 3 / second moisture-proof layer 4) are placed on both end surfaces in the stacking direction (surfaces that will become the first main surface 6 and second main surface 7 of the CFRP member 2) with a sheet-like adhesive sandwiched between them. The moisture-proof layers are then integrally bonded during molding of the CFRP member 2 (hereinafter, this bonding method may be referred to as the adhesive-integrated molding method).

[0106] Note that sheet-like adhesives are available in thermoplastic and thermosetting types, and a type (model) that can adhere at the curing temperature (e.g., 120°C to 130°C) during molding of the CFRP member 2 is selected. This makes it possible to bond the moisture-proof layer to the CFRP member 2 by sandwiching the sheet-like adhesive between the moisture-proof layer and the prepreg 5 and laminating and curing it.

[0107] For example, a thermoplastic adhesive film known as a hot-melt adhesive film (sheet) can be used as a sheet-like adhesive. When heated, the film melts and generates adhesive strength, and when returned to room temperature, it hardens again, maintaining stable adhesive strength. Film-like adhesives with a consistent thickness are available, making them easy to work with and easily reducing in-plane thickness variations. Furthermore, since there are many types available, it is possible to select the appropriate type and grade depending on the materials to be bonded and the heat bonding temperature. For example, olefin-based and polyester-based hot-melt adhesives have good heat resistance and thermal stability, making them suitable materials for manufacturing the structure 1 according to the present technology.

[0108] Thermosetting adhesive films can also be used as sheet adhesives, and epoxy-based thermosetting resin adhesive films are also available. When epoxy resin is used as the matrix resin, the prepreg 5 and the film are made of the same material, which is effective in increasing compatibility due to similar properties, including thermal expansion coefficients. Furthermore, thermosetting resin adhesive films provide stable adhesive strength even at relatively high temperatures, which is advantageous in terms of long-term reliability.

[0109] Furthermore, because it is in film form, it is just as easy to work with as thermoplastic adhesive films, and by selecting the appropriate type and grade, it is also possible to mold prepreg laminates, adhesive films, and various moisture-proof layers all at once.

[0110] The adhesive integral molding method using a sheet-like adhesive can improve the adhesive strength between the prepreg 5 and the moisture-proof layer compared to the integral molding method. On the other hand, the integral molding method not using a sheet-like adhesive can reduce the cost of parts.

[0111] It should be noted that the state (bonding aspect) after bonding of the moisture-proof layer to the CFRP member 2 using the adhesive bonding method, tape bonding method, pressure-sensitive adhesive layer bonding method, and adhesive integral molding method does not necessarily exhibit clearly different characteristics. Depending on the materials and configurations of the adhesive, tape, and pressure-sensitive adhesive layer, the bonded states may be very similar.

[0112] The above-described integral molding method and adhesive integral molding method correspond to embodiments of the process of the present invention for integrally joining a plurality of sheet-like members, a first moisture-proof layer, and a second moisture-proof layer by thermocompression bonding. The adhesive bonding method, tape bonding method, and adhesive layer bonding method correspond to embodiments of the process of the present invention for bonding each of the first moisture-proof layer and the second moisture-proof layer to a main body portion formed by thermocompression bonding of a plurality of sheet-like members.

[0113] [Specific Example of Integral Molding Method] A specific example of an integral molding method will be described. First, a plurality of prepregs 5 are prepared. The prepregs 5 are stacked, and low thermal expansion glass that will become the first moisture-proof layer 3 is laminated on the upper surfaces in the stacking direction (the surfaces that will become the first main surfaces 6 of the CFRP member 2). Furthermore, metal foil is laminated on the lower surfaces of the prepregs 5 (the surfaces that will become the second main surfaces 7 of the CFRP member 2).

[0114] A laminate consisting of metal foil, multiple prepregs 5, and low-thermal expansion glass laminated in this order is sandwiched between two bagging films in the vertical direction (Z direction), and the edges of the two bagging films are sealed with sealing tape, thereby encasing the laminate in a sealed space.

[0115] The inside of the sealed space is depressurized by drawing a vacuum, and then pressurized by the external atmospheric pressure, and the temperature is raised to 120°C to 130°C over 1 to 2 hours. This hardens the prepreg 5, bonds the low thermal expansion glass to the first main surface 6, and bonds the metal foil to the second main surface 7.

[0116] Hereinafter, the method of housing the structure in a sealed space, evacuating the inside and pressurizing it with atmospheric pressure will be referred to as “bagging adsorption pressurization.” Note that conditions such as temperature and time can be set appropriately.

[0117] After the bagging and pressure application, a post-baking (PB) is carried out at a high temperature (for example, 145°C) for 2 hours to improve the degree of hardening and eliminate distortion during molding. Note that this PB step is not essential.

[0118] Such thermocompression bonding makes it possible to manufacture the structure 1 by integral molding. In addition to the above-mentioned bagging adsorption and pressure method, an autoclave method in which the temperature is raised and cured under pressure can also be used. When the autoclave method is adopted, the cost is high in terms of equipment, etc., but stable manufacturing is possible.

[0119] When a metal foil is used as the second moisture-proof layer 4, a protective layer can be formed on the surface of the metal foil opposite to the bonding surface with the CFRP member 2 to prevent oxidation, contamination, and generation of wear powder. The protective layer can be made of a plastic film such as PET, PEN (polyethylene naphthalate), or PI (polyimide). Nickel plating or tin plating can also be used as the protective layer.

[0120] [Thermal Residual Stress Applied to the CFRP Member 2] For example, when the CFRP member 2 and the moisture barrier layer (first moisture barrier layer 3 / second moisture barrier layer 4) are integrally molded by the above-described integral molding method, the interface between the CFRP member 2 and the moisture barrier layer becomes stress-free at a temperature of, for example, 120°C to 130°C. When the structure 1 is then returned to room temperature (usage temperature), high thermal residual stress is applied between the CFRP member 2 and the moisture barrier layer, causing deformation such as warping. Furthermore, if the thermal residual stress is gradually alleviated over a long period of time at the usage temperature, there is a risk that the structure 1 will gradually deform.

[0121] Long-term changes and deformations are a major concern when realizing a high-precision CFRP structure 1. Therefore, in order to realize a high-precision structure 1, it is important to reduce the thermal residual stress caused by the process of bonding the moisture barrier layers (first moisture barrier layer 3 / second moisture barrier layer 4) to the CFRP member 2. This also applies when a bonding method other than the integral molding method is used.

[0122] In addition, when the matrix resin of the CFRP member 2 itself is an epoxy resin, the stress relaxation is not zero, but the effect can be reduced by using a highly elastic CF.

[0123] The thermal residual stress can be evaluated, for example, by multiplying the difference in the thermal expansion coefficients of both members by the temperature difference (the temperature difference ΔT from the stress-free temperature to the operating temperature). When the value obtained by such a calculation is used, it is effective to use a material for the moisture barrier layer that causes a thermal residual stress of 6 MPa or less, which is caused by the process of bonding the moisture barrier layer to the CFRP member 2.

[0124] Furthermore, the following two measures can be cited as effective measures for reducing thermal residual stress.

[0125] (1) The moisture-proof layers (first moisture-proof layer 3 / second moisture-proof layer 4) are made of materials with a small difference in thermal expansion coefficient from the CFRP member 2. (2) The process of joining the moisture-proof layers (first moisture-proof layer 3 / second moisture-proof layer 4) to the CFRP member 2 is carried out at a low temperature (for example, at an operating temperature such as room temperature or a temperature close to the operating temperature). This reduces the temperature difference ΔT.

[0126] Regarding countermeasure (1), for example, the thermal expansion coefficient of pitch-based prepreg cross-ply laminates (CP (Cross-Ply) material) and quasi-isotropic plates (QI (Quasi-Isotropic) material) is -5 × 10 -7 On the other hand, low thermal expansion glass, especially "Neoceram", has a low thermal expansion coefficient of -2 × 10 over a wide temperature range above room temperature. -7The thermal expansion coefficients of both materials are approximately the same in the temperature range of the CFRP hardening molding process, so it is possible to greatly reduce the thermal residual stress between the two materials.

[0127] For example, the first moisture-proof layer 3 has a thermal expansion coefficient of −1×10 at temperatures of 20° C. to 130° C. in a direction parallel to the surface on the side laminated to the first main surface 6. -6 / °C or greater than 1 × 10 -6 / °C. This makes it possible to maintain a small difference in the thermal expansion coefficient during the molding process from when the CFRP hardens at high temperature until it is returned to room temperature, thereby suppressing thermal residual stress.

[0128] Furthermore, the thermal expansion coefficient of the first moisture-proof layer 3 in a direction parallel to the surface on the side laminated to the first main surface 6 at temperatures of 20°C to 130°C is -1 x 10 -6 / °C or greater than 1 × 10 -7 / °C. This further reduces the difference in thermal expansion coefficient, making it possible to further suppress thermal residual stress.

[0129] The thermal expansion coefficient of "Neoceram" manufactured by NEG at temperatures of 20°C to 130°C in a direction parallel to the surface on the side laminated to the first main surface 6 is -1 x 10 -6 / °C or greater than 1 × 10 -7 This corresponds to low thermal expansion glass in the range of less than 1 / °C.

[0130] Of course, even when a ceramic material other than low thermal expansion glass is used, the thermal expansion coefficient at temperatures of 20°C to 130°C in a direction parallel to the surface of the first moisture-proof layer 3 that is laminated on the first main surface 6 of the first moisture-proof layer 3 should be less than -1 x 10 -6 / °C or greater than 1 × 10 -6 / °C, it is possible to suppress thermal residual stress. In particular, the thermal expansion coefficient of the first moisture-proof layer 3 at temperatures of 20°C to 130°C in a direction parallel to the surface on the side laminated to the first main surface 6 is set to be within a range of -1×10 -6 / °C or greater than 1 × 10 -7By configuring the temperature to be within a range smaller than 1 / °C, it is possible to further suppress the thermal residual stress.

[0131] The difference in thermal expansion coefficient between the first moisture-proof layer 3 and the CFRP member 2 is 1×10 -6 The ceramic material (low thermal expansion glass, etc.) has a thermal expansion coefficient of less than 1 / °C. This makes it possible to suppress thermal residual stress.

[0132] For example, a pitch-based CFRP structure in which pitch-based prepregs are laminated and integrated is adopted as the CFRP member 2. Furthermore, as the first moisture-proof layer 3, a material such as "Neoceram" manufactured by NEG, which has a thermal expansion coefficient of -1×10 at temperatures of 20°C to 130°C in a direction parallel to the surface laminated on the first main surface 6, is used. -6 / °C or greater than 1 × 10 -7 / °C is bonded to the first main surface 6 of the CFRP member 2.

[0133] The difference in thermal expansion coefficient between such low thermal expansion glass and the CFRP member 2 having a pitch-based CFRP structure is 1×10 -6 / °C. Furthermore, the thermal residual stress resulting from the step of bonding the first moisture proof layer 3 to the CFRP member 2 is 6 MPa or less, and the effect of suppressing the thermal residual stress is extremely high.

[0134] Furthermore, when a material with a very small thickness (size in the vertical direction (Z direction)), such as metal foil, is used as the moisture-proof layer, the metal foil itself undergoes elastic and plastic deformation, making it possible to design the CFRP member 2 to have a significantly small residual stress. Therefore, even if a multilayer structure of a ceramic member (low thermal expansion glass) and metal foil is adopted as the first moisture-proof layer 3, the suppression of thermal residual stress is maintained.

[0135] For example, the first moisture-proof layer 3 may be made of a material such as "Neoceram" manufactured by NEG, which has a thermal expansion coefficient of -1×10 at temperatures of 20° C. to 130° C. in a direction parallel to the surface that is laminated on the first main surface 6. -6 / °C or greater than 1 × 10 -7A multilayer structure of low-thermal expansion glass with a thermal expansion coefficient in the range smaller than 1 / °C and metal foil is adopted. A pitch-based CFRP structure is adopted as the CFRP member 2. In this case, metal foil is disposed between the CFRP member 2 having a pitch-based CFRP structure and the low-thermal expansion glass. As a result, it is possible to shift the thermal expansion coefficient of the CFRP member 2 to the positive side, further reducing the difference in thermal expansion coefficient with the low-thermal expansion glass. It is expected that the effect of reducing the difference in thermal expansion coefficient can be improved by appropriately adjusting the thickness of the metal foil.

[0136] The second moisture-proof layer 4 is also made of a material that has a small difference in thermal expansion coefficient from the CFRP member 2. This makes it possible to reduce the thermal residual stress acting on the CFRP member 2. It is also effective to use a metal foil as the second moisture-proof layer 4, which can suppress the thermal residual stress through elastic deformation and plastic deformation.

[0137] The second moisture-proof layer 4 can be made of a rubber tape with a metal foil, such as an aluminum foil-attached butyl tape. The adhesive layer of the rubber tape is made of a rubber such as butyl rubber, which has a low elastic modulus, and this can further reduce the thermal residual stress. The second moisture-proof layer 4 can also be made of a resin film with a moisture-proof coating, such as a high-barrier film, which can also reduce the thermal residual stress.

[0138] Even when an adhesive lamination method is used in which a moisture-proof layer is bonded to the CFRP member 2 via an adhesive, if there is a difference in the thermal expansion coefficient between the two members, thermal residual stress will occur due to the difference in the amount of contraction when the members are returned to the operating temperature.

[0139] Furthermore, the state of this thermal residual stress changes over time. Adhesives are typically made of resin, which has viscoelastic properties, and creep deformation occurs over time if stress remains applied. Therefore, the change (deformation) in the direction of relieving the thermal residual stress progresses very slowly.

[0140] Regarding countermeasure (2), the moisture-proof layers (first moisture-proof layer 3 / second moisture-proof layer 4) are bonded to the CFRP member 2 via an adhesive that hardens at low temperatures (low-temperature adhesive) or an adhesive layer that exerts adhesive strength at low temperatures. This makes it possible to reduce the temperature difference ΔT and suppress thermal residual stress.

[0141] In the adhesive lamination method, by using a low-temperature adhesive, it is possible to reduce the temperature difference ΔT and suppress thermal residual stress. Also, in the tape lamination method and adhesive layer bonding method, by forming an adhesive layer that hardens at a low temperature, it is possible to reduce the temperature difference ΔT and suppress thermal residual stress.

[0142] In the present disclosure, "low temperature" refers to a range of temperatures equal to or lower than the higher of room temperature (the temperature at which the structure 1 is used) and 70° C. Typically, temperatures equal to or lower than 70° C. are considered to fall under the "low temperature" in the present disclosure.

[0143] Epoxy resin (epoxy adhesive) can be used as a low-temperature adhesive. In addition to two-component mixture types that use a curing agent that can initiate a curing reaction with the epoxy base at low temperatures, it is also possible to use "latent curing agents" that initiate curing when triggered by an external stimulus such as heat or light.

[0144] In addition to heat, there are methods (types) of using light, pressure, etc. as stimulus triggers for hardening low-temperature adhesives. For example, there are types that decompose when exposed to light to generate cations, and types that undergo structural changes when exposed to light to generate anions. There is also a method in which the curing agent is microencapsulated and dispersed in the epoxy resin. These methods can initiate and progress the reaction between the epoxy base and curing agent without using heat, making it possible to harden at low temperatures.

[0145] Of course, countermeasure (2) can also be achieved by appropriately using a tape or film on which an adhesive layer (a layer made of adhesive) using a "latent curing agent" is formed, making it possible to suppress thermal residual stress.

[0146] The effect of suppressing thermal residual stress is also achieved when only one of the first moisture-proof layer 3 and the second moisture-proof layer 4 is bonded via an adhesive that hardens at low temperatures or an adhesive layer that exhibits adhesive strength at low temperatures.

[0147] The following method can also be used to bond the moisture barrier layers (first moisture barrier layer 3 / second moisture barrier layer 4) to the CFRP member 2. First, metal foil is bonded to each of the first main surface 6 and the second main surface 7. Then, thermal expansion glass is bonded to the metal foil bonded to the first main surface 6 via an adhesive or the like. In this configuration, the first moisture barrier layer 3 has a multilayer structure of metal foil and low thermal expansion glass.

[0148] By first laminating metal foil on the first main surface 6 and the second main surface 7, moisture-proofing properties are realized for the first main surface 6 and the second main surface 7. Therefore, there is a high degree of freedom in the selection of materials for the adhesive used to laminate low-thermal expansion glass to the metal foil in the next step. For example, a low-temperature adhesive can be used. It is also possible to use an adhesive that does not have high rigidity. It is also possible to use a material that functions as a stress relief layer. Furthermore, there is a high degree of freedom in the selection of the thickness of the adhesive, etc.

[0149] In other words, even if there is a difference in the thermal expansion coefficient between the multiple prepregs 5 and the low-thermal expansion glass, the adhesive that bonds the metal foil and the low-thermal expansion glass can exert a stress-relieving function, thereby making it possible to sufficiently suppress deformation such as warping at the top and bottom of the completed structure 1.

[0150] [Study on improving the properties of CFRP structures] The inventors have conducted extensive research into CFRP structures that can exhibit properties that are effective in improving the processing accuracy of processing equipment, particularly CFRP structures that can be applied to components that require high flatness accuracy, such as suction plates on which workpieces are placed in workpiece stages of exposure equipment, etc.

[0151] For example, suppose an adsorption plate or the like is constructed using only the CFRP member 2. In this case, it is difficult to process the first main surface 6 and the second main surface 7 of the CFRP member 2 with high precision, and high flatness accuracy cannot be ensured (hereinafter, this may be referred to as a flatness problem). Furthermore, the CFRP member 2 alone poses problems such as deformation due to expansion caused by moisture absorption and changes in shape over time (hereinafter, this may be referred to as a moisture absorption deformation problem).

[0152] Figure 4 is a graph showing the results of an accelerated moisture absorption test verifying the presence or absence of a moisture-proof layer on the first principal surface 6 and the second principal surface 7 of the CFRP member 2 and the change in moisture-absorption expansion strain over time. The horizontal axis of Figure 4 represents elapsed time (Hr), and the vertical axis represents the change in moisture-absorption expansion strain (με). The "both sides" in Figure 4 correspond to the first principal surface 6 and the second principal surface 7, which are the flatwise surfaces of the CFRP member 2. The strain change was measured by placing a strain gauge in the center layer during CFRP lamination molding and embedding it inside by hardening molding.

[0153] Fig. 4 shows the change over time in moisture absorption expansion strain of a reference sample, which is a CFRP member 2 alone that does not have a moisture barrier layer formed on either the first main surface 6 or the second main surface 7. Fig. 4 also shows a graph of a sample in which glass is bonded as a moisture barrier layer to the entire surface of either the first main surface 6 or the second main surface 7 of the CFRP member 2. Fig. 4 also shows a graph of a sample in which low-thermal expansion glass is bonded to the first main surface 6 of the CFRP member 2 and Al foil is bonded to the second main surface 7 (corresponding to an embodiment of the present structure 1).

[0154] As shown in Figure 4, it was confirmed that the reference sample (without a moisture-proof layer) experienced a very large moisture absorption expansion in the accelerated moisture absorption test. It was also confirmed that the sample in which a glass layer was integrally formed on one of the flatwise surfaces of the CFRP member 2 experienced a large moisture absorption expansion in the accelerated moisture absorption test.

[0155] On the other hand, it was confirmed that a sample in which low-thermal expansion glass was laminated on the first main surface 6 of the CFRP member 2 and Al foil was laminated on the second main surface 7 showed almost no moisture absorption expansion. In other words, it was found that for moisture absorption of the CFRP member 2, it is very important to use moisture-proof layers on both flatwise surfaces, i.e., on both the first main surface 6 and the second main surface 7.

[0156] In the structure 1 according to this embodiment shown in Figures 1 to 3, a first moisture barrier layer 3 is laminated on a first main surface 6 of a CFRP member 2, and a second moisture barrier layer 4 is laminated on a second main surface 7. This provides a very effective configuration against the problem of deformation due to moisture absorption.

[0157] Furthermore, in the structure 1 according to this embodiment, the first moisture proof layer 3, whose surface 9 is made of a ceramic material, is laminated on the first main surface 6 of the CFRP member 2. This allows for highly accurate processing of the surface 9 made of a ceramic material, making it possible to achieve high flatness accuracy. In other words, the structure 1 according to this embodiment has a configuration that is extremely effective in addressing flatness issues.

[0158] The layer made of a ceramic material formed on the surface 9 side of the first moisture-proof layer 3 can also be considered a processing-sacrificial layer. When the first moisture-proof layer 3 is made of low-thermal expansion glass, the entire first moisture-proof layer 3 can be considered a processing-sacrificial layer.

[0159] Furthermore, in the structure 1 according to this embodiment, a second moisture proof layer 4 made of a material other than the ceramic material is laminated on the second main surface 7 of the CFRP member 2. This is extremely advantageous in reducing the weight of the structure 1.

[0160] For example, suppose that moisture-proof layers made of a ceramic material (e.g., low-thermal expansion glass) are laminated on both the first main surface 6 and the second main surface 7 of the CFRP member 2. In this case, taking into account the density and thickness of the ceramic material, the weight increases considerably, significantly compromising the benefit of reducing the weight of the CFRP structure 1.

[0161] For example, the second moisture-proof layer 4 has a density of 2.5 g / cm 3When a low thermal expansion glass having a thickness of 3 mm and a size of 600 mm square is used, the weight increases by about 2.7 kg. On the other hand, when a low thermal expansion glass having a density of 2.7 g / cm3 is used as the second moisture-proof layer 4, the weight increases by about 2.7 kg. 3 When an Al foil having a thickness of 20 μm and a size of 600 mm square is used, the weight is 19 g, which is about 1 / 140 of the weight.

[0162] The first moisture-proof layer 3, which is the target of flattening, needs to function both as a processing sacrificial layer and as a moisture-proof layer. On the other hand, the second moisture-proof layer 4, which is bonded to the opposite second main surface 7, only needs to function as a moisture-proof layer. Therefore, a lightweight structure, such as a very thin metal foil, is adopted as the second moisture-proof layer 4. Furthermore, grinding is the main method for thinning ceramic materials, which increases processing costs. Furthermore, ceramic materials themselves are expensive, so material costs are also an issue.

[0163] The present inventors have devised a new configuration for the structure 1 illustrated in Figures 1 to 3. This configuration makes it possible to realize a structure 1 that can exhibit characteristics that are effective in improving the processing accuracy of a processing device.

[0164] When the structure 1 according to the present technology is applied to a work stage (suction plate), high-precision positioning can be achieved due to high flatness accuracy. Furthermore, high-precision positioning can be performed in a short time. Furthermore, dimensional deformation due to temperature changes and moisture absorption can be sufficiently suppressed.

[0165] For example, in the case of an apparatus that performs high-precision exposure by frequently moving the stage position, such as a step-and-repeat exposure apparatus (division projection exposure apparatus), there are significant benefits to applying the structure 1 according to the present technology to the work stage (adsorption plate).

[0166] This structure 1 can be made lightweight while maintaining high rigidity and dimensional stability, making it possible to shorten the time it takes to move the stage. This is because, according to the relationship F = ma, the smaller the mass m, the higher the acceleration a that can be obtained with the same driving force F. Being able to accelerate and decelerate at high acceleration shortens the time required to move a given distance, making it possible to shorten the takt time of the device.

[0167] Furthermore, when moving with the same acceleration a, a smaller driving force F is required, which allows a smaller driving motor to be used, making the entire device smaller and lighter.Furthermore, it is possible to reduce the reaction force, which in turn reduces the vibration of the entire device.

[0168] Furthermore, it is possible to achieve high vibration damping characteristics, and even when accelerating or decelerating at high acceleration, vibrations converge in a short time, allowing the exposure process to proceed. Normally, the settling time until the vibrations converge accounts for a significant proportion of the overall takt time. Therefore, by shortening the settling time, it is possible to significantly improve the processing speed performance of the exposure device.

[0169] Of course, the present structure 1 can be applied not only to exposure devices but also to work stages and the like of other processing devices such as laser processing devices, etc. Also, the present structure 1 can be applied to components other than the work stage, or to frames that support components.

[0170] In particular, the structure 1 can be configured so that the surface 9 of the first moisture barrier layer 3 made of a ceramic material serves as the surface to be machined. Therefore, the structure 1 is effective for components or frames that have surfaces that need to be machined.

[0171] In an example in which the structure 1 is applied to a work stage (adsorption surface), the surface 9 of the first moisture-proof layer 3 is configured as a surface to be processed into a flat surface. Of course, this is not limited to this, and the surface 9 of the first moisture-proof layer 3 may be configured as a surface to be processed for various other processes, such as processes to form a surface with a predetermined shape such as a tapered surface or a concave / convex portion.

[0172] [Evaluation of Examples] The inventors created a number of examples of the structure 1 according to the present technology and the manufacturing method thereof, and evaluated the moisture-proof performance by an accelerated moisture absorption test. This will be described in detail below.

[0173] (Reference Sample) A mirror-symmetric eight-layer structure made of PAN-based CP material was used as the CFRP member 2 used as the reference sample. In practice, pitch-based prepregs with a high elastic modulus are often used, but in order to make it easier to measure changes in moisture absorption and expansion, PAN-based prepregs with a lower elastic modulus than pitch-based prepregs were used for evaluation. Note that both pitch-based prepregs and PAN-based prepregs exhibit similar moisture-proof properties when epoxy resin is used as the matrix resin, so the evaluation results are the same.

[0174] When producing the CFRP member 2 as the reference sample, curing and molding were carried out under the recommended curing conditions for PAN-based prepreg, namely, at 120°C for 2 hours (curing under bagging adsorption pressure), followed by PB at 145°C for 2 hours.

[0175] (Moisture absorption test conditions) Evaluation was carried out at high temperatures and high humidity of 80°C and 95% or more. In terms of the diffusion coefficient of water vapor, the 80°C temperature condition is an accelerated condition that is approximately 32 times faster than room temperature of 20°C. Since moisture absorption by the CFRP member 2 increases in proportion to the difference between the internal moisture concentration and the environmental relative humidity, a moisture absorption test at 95% relative humidity can be said to be a stricter accelerated condition than evaluation in a normal environment (e.g., 50% relative humidity).

[0176] (Evaluation and Measurement Method) A strain gauge was placed at the center of the central layer of the prepreg laminate and integrally molded for measurement. After the prepreg was cured and PB was performed, the strain change was measured based on the strain level at the time when the constant conditions of 80°C and 95% relative humidity were reached.

[0177] Figure 5 is a graph showing the change in moisture-induced swelling strain over time for each example described below. Figure 6 is a table showing the moisture-induced swelling strain and reference ratio for each example at the time when the moisture-induced swelling of the reference sample was saturated after 60 hours.

[0178] (Example 1) First moisture-proof layer (integrally molded low thermal expansion glass) / second moisture-proof layer (integrally molded Al foil) First moisture-proof layer...NEOCERAM manufactured by NEG (thickness 3 mm) Second moisture-proof layer...Al foil (thickness 20 μm) Laminated in a configuration of low thermal expansion glass / 8 layers of PAN-based prepreg CP arrangement / Al foil, and integrally molded by hot pressing using bagging adsorption pressure. After 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain of Structure 1 of Example 1 was 0.8 με, which was suppressed to 0.9% compared to the reference.

[0179] (Example 2) First moisture-proof layer (integrally molded low thermal expansion glass) / second moisture-proof layer (integrally molded electrolytic copper foil) First moisture-proof layer...NEOCERAM manufactured by NEG (thickness 3 mm) Second moisture-proof layer...copper foil (thickness 20 μm) Laminated in a configuration of low thermal expansion glass / 8 layers of PAN-based prepreg CP arrangement / copper foil, and integrally molded by hot pressing using bagging adsorption pressure. After 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain of Structure 1 of Example 2 was 0.8 με, which was suppressed to 0.9% compared to the reference.

[0180] (Example 3) First moisture-proof layer (integrally molded low-thermal expansion glass) / Second moisture-proof layer (electrolytic copper foil bonded with low-temperature adhesive) First moisture-proof layer... NEG's "Neoceram" (thickness 3 mm) Second moisture-proof layer... Copper foil (thickness 20 μm) A configuration of 8 layers of low-thermal expansion glass / PAN-based prepreg CP arrangement was laminated and integrally molded by hot pressing using bagging adsorption pressure. After PB, copper foil was bonded to the second main surface 7 of the roughened CFRP member 2 using a low-temperature adhesive. After 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain of the structure 1 of Example 3 was 4.5 με, which was suppressed to 4.8% compared to the reference.

[0181] In all of the structures 1 of Examples 1 to 3, the second moisture-proof layer 4 was made of a thin (small-thickness) metal foil, and it was possible to sufficiently suppress the thermal residual stress in the CFRP member 2.

[0182] (Example 4) First moisture-proof layer (low thermal expansion glass integrally molded via adhesive film) / second moisture-proof layer (Al foil integrally molded) First moisture-proof layer...NEOCERAM manufactured by NEG (thickness 3 mm) Second moisture-proof layer...Al foil (thickness 20 μm) Laminated in a configuration of low thermal expansion glass / adhesive film / 8 layers of PAN-based prepreg CP arrangement / Al foil, and integrally molded by hot pressing using bagging adsorption pressure. After 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain of Structure 1 of Example 4 was 1.5 με, which was suppressed to 1.6% compared to the reference.

[0183] (Example 5) First moisture-proof layer (low thermal expansion glass bonded with low-temperature adhesive) / second moisture-proof layer (integrally molded Al foil) First moisture-proof layer...NEOCERAM manufactured by NEG (thickness 3 mm) Second moisture-proof layer...Al foil (thickness 20 μm) A configuration of 8 layers of PAN-based prepreg CP arrangement / Al foil was laminated and integrally molded by hot pressing using bagging adsorption pressure. After PB was performed, low thermal expansion glass was bonded to the first main surface 6 of the CFRP member 2 using a low-temperature adhesive. After 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain of the structure 1 of Example 5 was 3.5 με, which was suppressed to 3.7% compared to the reference.

[0184] Example 6 First moisture-proof layer (multilayer structure of low thermal expansion glass and copper foil) / second moisture-proof layer (integrally molded copper foil) First moisture-proof layer...NEOCERAM (3 mm thick) manufactured by NEG / copper foil (20 μm thick) Second moisture-proof layer...copper foil (20 μm thick) Copper foil / 8-layer PAN-based prepreg CP arrangement / copper foil structure was laminated and integrally molded by hot pressing using bagging adsorption pressure. After PB, low thermal expansion glass was bonded to the copper foil formed on the first main surface 6 of the CFRP member 2 using a low-temperature adhesive. After 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain of the structure 1 of Example 6 was 2.5 με, suppressed to 2.7% compared to the reference.

[0185] In Example 6, copper foil is first bonded to both flatwise surfaces (first main surface 6 and second main surface 7) of the CFRP member 2 by integral molding. For example, with copper foil bonded to both surfaces as the basic configuration, when a surface to be processed is required, low thermal expansion glass is bonded to the copper foil bonded to the first main surface 6. By employing such a manufacturing method, it is possible to improve the workability in manufacturing the structure 1 and to increase efficiency.

[0186] (Example 7) First moisture-proof layer (integrally molded low thermal expansion glass) / second moisture-proof layer (integrally molded resin film with moisture-proof membrane) First moisture-proof layer... NEG's "Neoceram" (thickness 3 mm) Second moisture-proof layer... High barrier film (structure in which moisture-proof layer is laminated on film by CVD) (thickness 38 μm) A configuration of low thermal expansion glass / PAN-based prepreg CP arrangement 8 layers / high barrier film was laminated, and integrally molded by thermocompression bonding using bagging adsorption pressure, followed by PB. After 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain of Structure 1 of Example 7 was 3.7 με, suppressed to 3.9% compared to the reference.

[0187] In Example 7, the high barrier film is based on a resin film such as a PET film, and therefore has a low modulus of elasticity, and even when laminated, almost no residual thermal stress is applied to the CFRP member 2. In addition, the barrier layer formed by CVD is made of SiO X Thin films of materials such as silicon dioxide and silicon oxynitride are often used, which are highly flexible and have a multi-layer structure that provides high water vapor barrier properties.

[0188] Also, a barrier film having a barrier layer of alumina or the like formed by PVD (sputtering) can be used. As mentioned above, when a resin film having a moisture-proof film formed thereon is used as the second moisture-proof layer 4, the water vapor permeability should be 1×10 -1 g / (m 2 It is desirable to have a so-called high barrier property of 1×10 -2 g / (m 2 It is preferable that the moisture-proof performance is less than 1 / 2 day.

[0189] Example 8: First moisture-proof layer (integrally molded low-thermal expansion glass) / Second moisture-proof layer (rubber tape with metal foil attached) First moisture-proof layer... NEG's "Neoceram" (thickness 3 mm) Second moisture-proof layer... Butyl tape with Al foil (Al foil thickness 7 μm) Low-thermal expansion glass / PAN-based prepreg CP arrangement 8 layers were laminated, integrally molded by hot pressing with bagging adsorption pressure, and then PB was performed. After 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain of Structure 1 of Example 8 was 5.5 με, suppressed to 5.9% compared to the reference. In Example 8, the metal foil was very thin and the thick rubber layer functioned as a buffer material, making it possible to suppress thermal residual stress to a very low level.

[0190] As described above, each example exhibited high moisture-proofing performance, and it was possible to significantly reduce moisture-absorbing expansion. When the examples are listed in order of increasing moisture-proofing performance, i.e., decreasing moisture-absorbing expansion, the order is (Example 1), (Example 2), (Example 4), (Example 6), (Example 5), (Example 7), (Example 3), and (Example 8).

[0191] 5 and 6, when the CFRP member 2, the first moisture barrier layer 3, and the second moisture barrier layer 4 are all integrally molded, the moisture barrier performance is slightly higher than when the first moisture barrier layer 3 and the second moisture barrier layer 4 are bonded to the molded CFRP member 2 using an adhesive or the like. However, the difference is very small, and is not considered to be significant when measurement errors and other factors are taken into account. It is also believed that the moisture barrier performance can be further improved by devising the bonding conditions.

[0192] As described above, in the structure 1 according to this embodiment, a first moisture barrier layer 3 having at least a portion of its surface 9 (in this embodiment, the entire surface 9) made of a ceramic material is laminated on a first main surface 6 of a CFRP member 2 formed by laminating a plurality of prepregs 5 whose main component is carbon fiber. In addition, a second moisture barrier layer 4 made of a material different from the ceramic material is laminated on a second main surface 7 of the CFRP member 2. As a result, by applying this structure 1 to the frame or components of a processing device, it becomes possible to exhibit properties that are effective in improving processing accuracy.

[0193] By implementing this technology, it is possible to realize a structure 1 that exhibits less dimensional deformation due to humidity changes than CFRP alone, is more rigid than metal, has low density and high specific rigidity, and is capable of achieving surface precision.

[0194] Second Embodiment A structure according to a second embodiment of the present invention will be described below. In the following description, the description of parts having the same configuration and function as those of the structure 1 described in the above embodiment will be omitted or simplified.

[0195] [Formation of Moisture Proof Layer on Side Surfaces] Figure 7 is a schematic diagram showing an example of the basic configuration of a structure according to the second embodiment. In the structure 12 according to this embodiment, moisture proof layers are further laminated on the side surfaces 8 (left side surface 8a, right side surface 8b, front side surface 8c, and rear side surface 8d), which are edgewise surfaces of the CFRP member 2. Please also refer to Figures 1 to 3 for illustrations of each part such as the side surfaces 8 (left side surface 8a, right side surface 8b, front side surface 8c, and rear side surface 8d).

[0196] Hereinafter, the moisture-proof layer laminated on the side surface 8 will be referred to as the third moisture-proof layer 13. In the structure 12 shown in Fig. 7, a third moisture-proof layer 13a (not shown) is laminated on the entire surface of the left side surface 8a, and a third moisture-proof layer 13b is laminated on the entire surface of the right side surface 8b. In the structure 12, a third moisture-proof layer 13c is laminated on the entire surface of the front side surface 8c, and a third moisture-proof layer 13d (not shown) is laminated on the entire surface of the rear side surface 8d.

[0197] As explained in the first embodiment, the moisture barrier layers (first moisture barrier layer 3 / second moisture barrier layer 4) are bonded to the flatwise surfaces of the CFRP member 2, i.e., the first main surface 6 and the second main surface 7. This makes it possible to exhibit high moisture barrier performance and solve the problem of moisture absorption deformation of the CFRP structure.

[0198] In order to further improve the moisture-proof performance, the inventors have conducted extensive research into the formation of a third moisture-proof layer 13 on the side surface 8 as shown in FIG.

[0199] In order to fully prevent the problem of deformation due to moisture absorption and to achieve high dimensional accuracy and long-term stability, it is important to improve moisture-proof performance. In the structure 1 shown in Figures 1 to 3, preventing moisture absorption from the side surface 8 of the CFRP member 2 is thought to be effective in further improving moisture-proof performance.

[0200] It is considered that the diffusion rate of moisture is slow inside the CFRP member 2, and the effect of moisture absorption on the central portion is small. Therefore, it is considered that the effect of moisture absorption is large on the flatwise surfaces (first main surface 6 / second main surface 7) which have a large area and a small thickness dimension (dimension in the Z direction).

[0201] On the other hand, the edgewise surface (side surface 8) is considered to be less affected by moisture absorption than the flatwise surface, and therefore the required moisture barrier performance may be slightly lower. However, the formation of the third moisture barrier layer 13 is considered to improve the moisture barrier performance.

[0202] The CFRP member 2 is formed by laminating a plurality of prepregs 5 and then subjecting them to heat and pressure bonding. As described above, when molding the CFRP member 2, it is possible to integrally mold the first moisture barrier layer 3 and the second moisture barrier layer 4 onto the first main surface 6 and the second main surface 7 of the CFRP member 2. However, when molding the CFRP member 2, excess matrix resin is pushed out from the side surface 8, making it difficult to simultaneously integrally mold the third moisture barrier layer 13 onto the side surface 8 of the CFRP member 2.

[0203] The third moisture barrier layer 13 must be laminated after a precise edgewise surface is formed by cutting and edge trimming the molded CFRP member 2. Therefore, the bonding of the third moisture barrier layer 13 to the side surface 8 of the CFRP member 2 must be performed in a separate process from the process of bonding the first moisture barrier layer 3 and the second moisture barrier layer 4 to the flatwise surface (first main surface 6 / second main surface 7).

[0204] The thermal expansion coefficient in the stacking direction (Z direction) of the plurality of prepregs 5 on the edgewise surface (side surface 8) is large because there is no constraint by the CF constituting the prepreg 5. Although it depends on the type of prepreg 5 and molding conditions, for example, at around room temperature, -6 / °C or more, and the thermal expansion coefficient is even greater in higher temperature regions.

[0205] Therefore, suppose the third moisture barrier layer 13 is bonded and integrated to the edgewise surface (side surface 8) using a high-temperature thermosetting adhesive or the like. In this case, the large difference in thermal expansion coefficients during the process of returning to room temperature (usage temperature) after bonding at high temperature could result in large thermal residual stresses being generated in the edgewise surface (side surface 8). This could result in deformation around the edgewise surface (side surface 8) or peeling of the third moisture barrier layer 13. As a result, problems such as a decrease in moisture barrier performance could occur, increasing the risk of not being able to ensure high dimensional accuracy.

[0206] The inventors have studied the selection of a material for the third moisture barrier layer 13 to be laminated on the side surface 8 of the CFRP member 2 that can suppress the thermal residual stress caused by the temperature difference between the temperature at the time of joining and the temperature at which the third moisture barrier layer 13 is used, and have also studied the reduction of the temperature difference between the time of joining and the time of normal use. As a result, the following effective countermeasures have been newly discovered.

[0207] (1) By using metal foil as the third moisture-proof layer 13 as a base, it is possible to achieve both high (or complete) moisture-proof performance and suppression of stress on the CFRP member 2. Because the metal foil is very thin, it is possible to suppress thermal residual stress even if a temperature difference occurs when bonding to the side surface 8. In addition, the adhesive layer or bonding layer used to bond the metal foil to the side surface 8 functions as a buffer material, making it possible to further suppress thermal residual stress.

[0208] (2) The temperature at which the third moisture barrier layer 13 is bonded to the side surface 8 of the CFRP member 2 is set to a low temperature (a temperature equal to or lower than the higher of the operating temperature of the structure 12 and 70°C), thereby reducing the thermal residual stress during bonding. If the third moisture barrier layer 13 can be bonded at the operating temperature, it is possible to reduce the thermal residual stress to almost zero. For example, it is very effective to bond the third moisture barrier layer 13 to the side surface 8 via an adhesive that hardens at low temperatures or an adhesive layer that exhibits adhesive strength at low temperatures.

[0209] The inventors have newly discovered the following effective examples of the configuration and bonding method of the third moisture-proof layer 13 that satisfy these conditions: Attaching metal foil with a low-temperature adhesive; Attaching metal foil with a UV-curable adhesive; Attaching at room temperature with the adhesive layer of butyl tape (such as butyl tape with aluminum foil) laminated with metal foil; Attaching thin metal or metal foil at room temperature using double-sided butyl tape; Attaching at room temperature with the adhesive layer of aluminum tape.

[0210] [Evaluation of Each Example] The inventors evaluated the moisture barrier performance of each example of the third moisture barrier layer 13 made based on metal foil by an accelerated moisture absorption test.

[0211] Furthermore, if a strain gauge is placed between the edgewise surface (side surface 8) and the third moisture-proof layer 13 to measure the change in moisture-absorption expansion strain, the accuracy of the measurement may be questionable due to the influence of moisture absorption by the strain gauge itself and the influence of stress generated at the interface between the third moisture-proof layer 13 and the edgewise surface (side surface 8).

[0212] Therefore, first, in order to measure the basic moisture-proof performance of the material and joining method used for the third moisture-proof layer 13, a moisture-proof layer was formed on the flatwise surface (first main surface 6 and second main surface 7) of the CFRP member 2 using the material and joining method used for the third moisture-proof layer 13, and then the moisture-proof performance was evaluated in an accelerated moisture absorption test.

[0213] (Reference Sample) A 10-layer structure of pitch-based UD material with mirror symmetry on the top and bottom was used for the CFRP member 2 used as the reference sample. When creating the CFRP member 2 of the reference sample, curing molding was carried out at 120°C for 2 hours (curing under bagging adsorption pressure), which is the recommended curing condition for pitch-based prepreg. Then, PB was carried out at 145°C for 2 hours.

[0214] (Moisture absorption test conditions) Evaluation was carried out at a temperature of 45°C and a relative humidity of 95% or higher. Evaluation in the 90° direction relative to the CF fiber of the UD material mainly involves the moisture absorption expansion of the matrix resin (epoxy resin), resulting in a large change in moisture absorption expansion strain. Therefore, the evaluation was carried out at a temperature condition with a low acceleration factor of 45°C. In terms of the diffusion coefficient of water vapor, a temperature condition of 45°C is an acceleration condition that is approximately four times that of room temperature of 25°C.

[0215] (Evaluation and Measurement Method) A strain gauge was placed at the center of the central layer of the prepreg laminate and integrally molded for measurement. After the prepreg was cured and PB was performed, the strain change was measured based on the strain level at the time when the temperature reached 45°C and the relative humidity reached 95%.

[0216] Figure 8 is a graph showing the change in moisture expansion strain over time for each example described below. Figure 9 is a table showing the moisture expansion strain and reference ratio for each example after 135 hours at 45°C and 95% relative humidity.

[0217] Example 9: Al foil was bonded to the first and second main surfaces 6 and 7 with a low-temperature adhesive (Al foil thickness: 20 μm). The roughened first and second main surfaces 6 and 7 were cured using the low-temperature adhesive at temperatures of 40°C to 60°C for 2 to 8 hours (curing under bagging adsorption pressure). After 135 hours at 45°C and a relative humidity of 95%, the moisture absorption expansion strain was 18 με and the reference ratio was 2.8%, confirming sufficient moisture-proof performance of the third moisture-proof layer 13.

[0218] Example 10: Electrodeposited copper foil was bonded to the first and second main surfaces 6 and 7 with a low-temperature adhesive (electrodeposited copper foil thickness: 20 μm). The low-temperature adhesive was used on each of the roughened first and second main surfaces 6 and 7, and cured at a temperature of 40°C to 60°C for 2 to 8 hours (curing under bagging adsorption pressure). After 135 hours at 45°C and a relative humidity of 95%, the moisture absorption expansion strain was 15 με and the reference ratio was 2.2%, confirming sufficient moisture barrier properties for the third moisture barrier layer 13.

[0219] In Examples 9 and 10, even when the curing temperature was changed within the range of 40°C to 60°C, there was no effect on moisture-proofing by ensuring sufficient curing time corresponding to each temperature. Low-temperature adhesives can be cured over time, even at room temperature. Furthermore, there was no effect on moisture-proofing performance when pressure was applied by weight instead of bagging. There was almost no difference in moisture-proofing performance between Al foil and electrolytic copper foil, confirming high moisture-proofing performance.

[0220] (Example 11) Al foil was bonded to the first principal surface 6 and the second principal surface 7 with a UV-curable adhesive (Al foil thickness: 20 μm). The UV-curable adhesive used was an epoxy-type tape-like adhesive that begins to harden rapidly when exposed to UV light. A surface roughening treatment was performed on each of the first principal surface 6 and the second principal surface 7. The tape-like adhesive was applied to the Al foil in advance, and after UV irradiation, it was attached to the CFRP member 2 by applying pressure under weight. After 135 hours at 45°C and a relative humidity of 95%, the moisture absorption expansion strain was 64 με and the reference ratio was 9.5%, confirming sufficient moisture-proof performance of the third moisture-proof layer 13.

[0221] Example 12: Electrodeposited copper foil was bonded to the first main surface 6 and the second main surface 7 with a UV-curable adhesive (electrodeposited copper foil thickness: 20 μm). The UV-curable adhesive used was an epoxy-type tape-like adhesive that begins to cure rapidly upon UV irradiation. A surface roughening treatment was performed on each of the first main surface 6 and the second main surface 7. The tape-like adhesive was attached to the electrodeposited copper foil in advance, and after UV irradiation, the foil was attached to the CFRP member 2 by applying pressure under weight. After 135 hours at 45°C and a relative humidity of 95%, the moisture absorption expansion strain was 54 με and the reference ratio was 8.0%, confirming sufficient moisture-proofing performance of the third moisture-proof layer 13.

[0222] In Examples 11 and 12, there was almost no difference in moisture-proof performance between the Al foil and the electrolytic copper foil, and high moisture-proof performance was confirmed.

[0223] (Examples 13) to 15) Aluminum foil-attached butyl tape was bonded to the first and second principal surfaces 6 and 7 under pressure at room temperature (usage temperature). Three different aluminum foil-attached butyl tapes were used for Examples 13 to 15. Each of the first and second principal surfaces 6 and 7 was roughened. After 135 hours at 45°C and 95% relative humidity, Example 13 exhibited a moisture-absorption expansion strain of 47 με (relative to the reference strain) and a reference strain of 7.0%. Example 14 exhibited a moisture-absorption expansion strain of 71 με (relative to the reference strain) and a reference strain of 10.6%. Example 15 exhibited a moisture-absorption expansion strain of 62 με (relative to the reference strain) and a reference strain of 9.2%. While there were slight differences between the products, all exhibited high moisture-proof performance as the third moisture-proof layer 13. Furthermore, favorable results were obtained, showing a tendency for moisture-absorption expansion to saturate over time.

[0224] (Example 16) Al foil (20 μm thick) was bonded to the first and second principal surfaces 6 and 7 using double-sided butyl tape under pressure at room temperature (usage temperature). Each of the first and second principal surfaces 6 and 7 was roughened. After 135 hours at 45°C and 95% relative humidity, the moisture-absorption expansion strain was 76 με and the reference ratio was 11.3%, confirming sufficient moisture-proof performance for the third moisture-proof layer 13. The use of double-sided butyl tape allows for greater freedom in metal foil selection. This means that various metal foils can be used as the third moisture-proof layer 13. Since thin metal plates can be used in addition to metal foils, attaching an Al channel (with a U-shaped cross section) to the side of the CFRP structure 12 can also function as a protective guard member.

[0225] Example 17: Aluminum tape was adhered to the first principal surface 6 and the second principal surface 7 at room temperature (usage temperature). The aluminum tape used had an adhesive layer made of a synthetic resin. A surface roughening treatment was performed on each of the first principal surface 6 and the second principal surface 7. After 135 hours at 45°C and a relative humidity of 95%, the moisture absorption expansion strain was 98 με and the reference ratio was 14.6%, confirming that the moisture barrier performance of the third moisture barrier layer 13 was sufficient.

[0226] Example 18: Aluminum tape was adhered to the first principal surface 6 and the second principal surface 7 at room temperature (usage temperature). The aluminum tape used was an airtight, waterproof aluminum tape with an acrylic adhesive layer. A surface roughening treatment was performed on each of the first principal surface 6 and the second principal surface 7. After 135 hours at 45°C and a relative humidity of 95%, the moisture absorption expansion strain was 288 με and the reference ratio was 42.6%, which is a slightly lower characteristic for the moisture barrier performance of the third moisture barrier layer 13. However, compared to a reference sample without the third moisture barrier layer 13, the moisture barrier effect was still evident.

[0227] When the Al tapes of Examples 17 and 18 were used, the moisture-proofing performance and reproducibility were slightly lower. This is presumably due to differences in the condition of the substrate (unevenness) and the finish at the time of application. The butyl tapes of Examples 13 to 16 were less susceptible to the condition of the substrate and produced stable results, likely due to factors such as the thick adhesive layer and the very low water vapor permeability of butyl rubber.

[0228] In contrast, it was recognized that the moisture-proofing performance of Al tape may be reduced depending on the conditions of the substrate and the bonding. However, under the appropriate conditions, it is believed that a considerable moisture-proofing performance can be obtained, and the effect is demonstrated when compared with an untreated edgewise product (reference sample).

[0229] (Example 19) Butyl tape without metal foil was attached to the first principal surface 6 and the second principal surface 7 by pressure bonding at room temperature (usage temperature). Each of the first principal surface 6 and the second principal surface 7 was subjected to a surface roughening treatment. After 135 hours at 45°C and a relative humidity of 95%, the moisture absorption expansion strain was 550 με, and the reference ratio was 81.8%.

[0230] (Example 20) An airtight waterproof tape was adhered to the first principal surface 6 and the second principal surface 7 by applying pressure at room temperature (usage temperature). A surface roughening treatment was performed on each of the first principal surface 6 and the second principal surface 7. After 135 hours at 45°C and a relative humidity of 95%, the moisture absorption expansion strain was 603 με, and the reference ratio was 89.7%.

[0231] High moisture-proof performance was not obtained with the third moisture-proof layer 13 not using a metal foil in Examples 19 and 20. However, compared with the reference sample not forming the third moisture-proof layer 13, a moisture-proof effect was exhibited.

[0232] The examples are listed in order of increasing moisture-proofing performance, i.e., decreasing moisture absorption expansion, as follows: (Example 10), (Example 9), (Example 13), (Example 12), (Example 15), (Example 11), (Example 14), (Example 16), (Example 17), (Example 18), (Example 19), and (Example 20).

[0233] In order to confirm whether the moisture-proofing performance results of Examples 9 to 20 obtained by the accelerated moisture absorption test described above are consistent with actual moisture absorption conditions, the inventors measured the long-term change in weight gain due to water immersion using the moisture-proof layers of Examples 14, 15, and 20 as representative samples.

[0234] (Reference Sample) A reference sample was prepared by bonding the Al foil-attached butyl tape used in Example 15 to the flatwise surfaces (first main surface 6 / second main surface 7) of a CFRP member 2 made of eight mirror-symmetric layers of PAN-based CP material. As shown in Figures 8 and 9, the Al foil-attached butyl tape used in Example 15 was confirmed to have a high moisture-proof effect.

[0235] (Representative Samples 1 to 3) Representative samples 1 to 3 were prepared by joining the third moisture-proof layer 13 to the edgewise surface (side surface 8) of the reference sample using the materials and joining methods of Examples 14, 15 and 20.

[0236] (Measurement of Weight Increase Due to Water Immersion) Each sample was immersed in a water tank, taken out at a predetermined time, and the weight was measured after natural drying for 45 minutes.

[0237] FIG. 10 is a graph showing the change over time in the weight gain rate of each sample due to immersion in water.

[0238] As shown in Figure 10, it was confirmed that by joining the third moisture-proof layer 13 to the edgewise surface (side surface 8) of the CFRP member 2, it is possible to suppress weight increase due to moisture absorption and to exhibit a moisture-proof effect.

[0239] Furthermore, the effect of suppressing weight gain was observed to have a similar tendency to the effect of suppressing moisture-absorption expansion strain in the moisture absorption accelerated test shown in Figures 8 and 9. That is, the order of Representative Sample 2 (Example 15), Representative Sample 1 (Example 14), and Representative Sample 3 (Example 20), which is the order of the highest moisture-absorption expansion strain suppression effect in the moisture absorption accelerated test shown in Figures 8 and 9, also corresponds to the order of the highest weight gain suppression effect due to water immersion. From these results, it is recognized that the moisture-proof performance results from the moisture absorption accelerated test shown in Figures 8 and 9 are consistent with the actual moisture absorption state.

[0240] Furthermore, by improving the moisture-proof performance of each of the first moisture-proof layer 3 laminated on the first main surface 6 and the second moisture-proof layer 4 laminated on the second main surface 7, the weight increase due to water immersion shown in Figure 10 can be further suppressed.

[0241] 8 to 10 confirm that the moisture barrier performance is improved by bonding the third moisture barrier layer 13 to the side surface 8 of the CFRP member 2. It was also found that this effect is widely exhibited without limiting the material or bonding method of the moisture barrier layer (first moisture barrier layer 3 / second moisture barrier layer 4) bonded to the flatwise surfaces (first main surface 6 and second main surface 7) of the CFRP member 2.

[0242] That is, any material and any joining method may be adopted as the material and joining method for the moisture barrier layers (first moisture barrier layer 3 / second moisture barrier layer 4) joined to the flatwise surfaces (first main surface 6 and second main surface 7) of the CFRP member 2. Regardless of the material and joining method selected, when comparing a configuration in which the third moisture barrier layer 13 is not formed on the edgewise surfaces (side surfaces 8) of the CFRP member 2 with a configuration in which the third moisture barrier layer 13 is formed on the edgewise surfaces (side surfaces 8), the configuration in which the third moisture barrier layer 13 is formed will exhibit higher moisture barrier performance.

[0243] The present inventor has newly discovered the following configuration for a structure in which the first moisture-proof layer 3, the second moisture-proof layer 4, and the third moisture-proof layer 13 are formed, which configuration can exhibit characteristics that are effective in improving the processing accuracy of a processing device.

[0244] (Configuration 1) A structure comprising: a main body portion formed by stacking a plurality of sheet-like members whose main component is carbon fiber, the main body portion having a first main surface and a second main surface that face each other in the stacking direction of the plurality of sheet-like members, and a side surface between the first main surface and the second main surface; a first moisture-proof layer stacked on the first main surface; a second moisture-proof layer stacked on the second main surface; and a third moisture-proof layer stacked on the side surface, wherein at least one of the first moisture-proof layer and the second moisture-proof layer is made of a material different from a ceramic material.

[0245] In a structure having this configuration, a first moisture-proof layer 3 is laminated on a first main surface 6 of a CFRP member 2 formed by laminating multiple prepregs 5 whose main component is carbon fiber, and a second moisture-proof layer 4 is laminated on a second main surface 7. In addition, a third moisture-proof layer 13 is laminated on a side surface 8 of the CFRP member 2. This provides high moisture-proof performance.

[0246] In the structure having (Configuration 1), at least one of the first moisture barrier layer 3 and the second moisture barrier layer 4 is made of a material other than a ceramic material, which makes it possible to reduce the weight of the structure and also to reduce processing costs and material costs.

[0247] As a result, by applying the structure having (Configuration 1) to the frame or components of a processing device, it becomes possible to exhibit properties that are effective in improving processing accuracy.

[0248] For example, a structure in which the first moisture barrier layer 3, at least a portion of which surface 9 is made of a ceramic material as described in the first embodiment, and the second moisture barrier layer 4, which is made of a material other than the ceramic material, are joined to the flatwise surfaces (first main surface 6 / second main surface 7), and a third moisture barrier layer 13 is joined to the side surface 8, is included in the structure having the above-mentioned (Configuration 1). Note that this structure corresponds to the configuration of structure 12 shown in FIG. 7.

[0249] Without being limited thereto, a structure having the above-mentioned (Configuration 1) also includes a structure in which both the first moisture barrier layer 3 and the second moisture barrier layer 4 are made of a material other than a ceramic material and a third moisture barrier layer 13 is bonded to the side surface 8. For example, a structure having the above-mentioned (Configuration 1) includes a structure in which various moisture barrier layers given as examples of the second moisture barrier layer 4 in the first embodiment are bonded to both flatwise surfaces (first main surface 6 / second main surface 7) of the CFRP member 2 and a third moisture barrier layer 13 is bonded to the side surface 8.

[0250] For example, a structure having the above-mentioned (Configuration 1) includes a structure in which metal foil is bonded to both flatwise surfaces (first main surface 6 / second main surface 7) of the CFRP member 2 and a third moisture barrier layer 13 is bonded to the side surface 8. Also, a structure having the above-mentioned (Configuration 1) includes a structure in which rubber tape having metal foil formed thereon is bonded to both flatwise surfaces (first main surface 6 / second main surface 7) of the CFRP member 2 and a third moisture barrier layer 13 is bonded to the side surface 8. Also, a structure having the above-mentioned (Configuration 1) includes a structure in which resin films having moisture barrier membranes are bonded to both flatwise surfaces (first main surface 6 / second main surface 7) of the CFRP member 2 and a third moisture barrier layer 13 is bonded to the side surface 8.

[0251] Furthermore, the inventors have newly devised a structure having the following configuration, which is a further ingenious addition to the structure having the configuration of (Configuration 1).

[0252] (Configuration 2) The structure according to (Configuration 1), wherein the third moisture-proof layer is made of a material other than a ceramic material. This (Configuration 2) makes it possible to reduce the weight of the structure 1.

[0253] (Configuration 3) The structure according to (Configuration 1), wherein the third moisture-proof layer is formed of any one of a metal foil, a thin metal plate, and a rubber tape having the metal foil formed thereon.

[0254] (Configuration 4) The structure according to (Configuration 1), wherein the third moisture-proof layer is bonded to the side surface via an adhesive that hardens at low temperatures or an adhesive layer that exhibits adhesive strength at low temperatures.

[0255] (Configuration 5) The structure according to (Configuration 3), wherein the third moisture-proof layer is formed by adhering the metal foil or the metal thin plate to the side surface with an adhesive that hardens at a low temperature.

[0256] (Configuration 6) The structure according to (Configuration 1), wherein at least a portion of the surface of the first moisture-proof layer opposite to the side where it is laminated on the first main surface is made of a ceramic material, and the second moisture-proof layer is made of a material different from the ceramic material. This (Configuration 6) makes it possible to achieve the effects of Structure 1 described in the first embodiment.

[0257] (Configuration 7) The structure according to (Configuration 6), wherein the first moisture-proof layer has an entire surface made of a ceramic material.

[0258] (Configuration 8) The structure according to (Configuration 1), wherein each of the first moisture barrier layer and the second moisture barrier layer is made of a material other than a ceramic material.

[0259] (Configuration 9) The structure according to (Configuration 1), wherein the first moisture-proof layer is formed of any one of a metal foil, a rubber tape on which the metal foil is formed, and a resin film on which a moisture-proof film is formed; and the second moisture-proof layer is formed of any one of a metal foil, a rubber tape on which the metal foil is formed, and a resin film on which a moisture-proof film is formed.

[0260] [Method for manufacturing a structure having (Configuration 1)] A method for manufacturing a structure having (Configuration 1) can include the following steps: a lamination step of stacking a plurality of sheet-like members (a plurality of prepregs 5) composed primarily of carbon fiber; a first joining step of joining the plurality of sheet-like members, a first moisture barrier layer 3 laminated on a first main surface 6, which is one main surface in the lamination direction of the plurality of sheet-like members, and a second moisture barrier layer 4 laminated on a second main surface 7 opposite to the first main surface 6; and a second joining step of joining a third moisture barrier layer 13 to a side surface 8 between the first main surface 6 and the second main surface 7 of the plurality of sheet-like members. As described above, at least one of the first moisture barrier layer 3 and the second moisture barrier layer 4 is made of a material other than a ceramic material.

[0261] In the second joining step, the third moisture-proof layer 13 is bonded to the side surface 8 with an adhesive that hardens at a low temperature, thereby making it possible to suppress thermal residual stress.

[0262] [Processing Apparatus] An example of a processing apparatus to which the structure according to the present technology can be applied will be described. The structure according to the present technology can be used in any processing apparatus that processes a workpiece such as a substrate.

[0263] 11 is a schematic diagram showing the general configuration of an exposure apparatus, which is an example of a processing apparatus. The exposure apparatus 15 is a projection exposure apparatus that exposes a workpiece W. Here, the workpiece W is a silicon workpiece, a printed circuit board, a glass substrate for a liquid crystal panel, or the like, and is a workpiece with a resist film applied to its surface.

[0264] The exposure apparatus 15 includes a light emitting unit 16 , a mask stage 17 , a projection optical system 18 , a workpiece stage 19 , and a frame 20 .

[0265] The light emitting unit 16 emits the exposure light EL. For example, a short arc type mercury lamp is used as the light emitting unit 16. The mercury lamp emits ultraviolet light having wavelengths of, for example, 365 nm (i-line), 405 nm (h-line), and 436 nm (g-line). Of course, the configuration is not limited to this, and a lamp that emits light in a wavelength band other than ultraviolet light may be used. Alternatively, a solid-state light source such as an LED (Light Emitting Diode) or an LD (Laser Diode) may be used.

[0266] The mask stage 17 is disposed below the light emitting part 16. The mask stage 17 holds an exposure mask M. A predetermined mask pattern is formed on the mask M. Furthermore, alignment marks (mask marks) are formed on the mask M.

[0267] The projection optical system 18 irradiates the workpiece W held on the workpiece stage 19 with the exposure light EL that is emitted from the light emitting unit 16 and transmitted through the mask M. As a result, an image of the mask pattern formed on the mask M is projected onto the workpiece W. The projection optical system 18 is configured as an imaging optical system having a projection lens.

[0268] The workpiece stage 19 holds the workpiece W. The workpiece stage 19 has a suction plate to which the workpiece W is attached. A plurality of vacuum suction holes are formed in the suction plate, and the workpiece W is held by vacuum suction.

[0269] The frame 20 supports components that make up the exposure apparatus 15, such as the light emitting unit 16, the mask stage 17, the projection optical system 18, and the workpiece stage 19. These components are held in predetermined positions by the frame 20.

[0270] Note that components such as the mask stage 17 and the workpiece stage 19 may be movably supported by the frame 20. For example, the components may be supported by the frame 20 so as to be able to move linearly in two mutually perpendicular directions along the horizontal direction, move linearly along the optical axis direction of the exposure light EL (up and down direction), or move rotationally around the optical axis direction of the exposure light EL (up and down direction) as the rotation axis. Of course, a portion of the frame 20 that supports the components may be configured to be movable.

[0271] For example, it is possible to realize a moving mechanism for moving components or a frame using any moving mechanism such as a linear stage using a stepping motor, or any rotating mechanism using a gear mechanism.

[0272] In the exposure device 15, once the alignment of the mask M and the workpiece W and focus control are completed, the exposure process for the workpiece W begins, and the exposure light EL is emitted from the light emitting unit 16. The exposure light EL emitted from the light emitting unit 16 is irradiated onto the workpiece W via the mask M on which a mask pattern is formed and the projection optical system 18. As a result, the mask pattern is projected onto the workpiece W and exposed.

[0273] 11, the structure according to the present technology is applied to components such as a frame 20 and a work stage (suction plate) 19. This makes it possible to exert characteristics that are effective in improving exposure accuracy, and high exposure accuracy is achieved.

[0274] 12 is a schematic diagram showing the general configuration of a laser processing apparatus 22, which is an example of a processing apparatus. The laser processing apparatus 22 has a laser emission unit 23, a workpiece stage 24, and a frame 25.

[0275] The laser emission unit 23 emits a laser beam L. The laser beam L emitted from the laser emission unit 23 is irradiated onto a workpiece W held on a workpiece stage 24, and processing such as cutting and drilling of the workpiece W is performed.

[0276] The frame 25 supports components that make up the laser processing device 22, such as the laser emission unit 23 and the workpiece stage 24. These components are held in predetermined positions by the frame 25. Note that the frame 25 may movably support components such as the workpiece stage 24. Of course, a portion of the frame 25 that supports the components may be configured to be movable.

[0277] 12, the structure according to the present technology is applied to components such as a frame 25 and a work stage 24. This makes it possible to exert characteristics that are effective in improving laser processing accuracy, and high laser processing accuracy is realized.

[0278] In addition, the structure according to the present technology can be applied to various processing devices. For example, the structure according to the present technology can be used as a component for semiconductor device manufacturing devices. The structure according to the present technology is also suitable as a stage component used for precision positioning in steppers, inspection devices, etc. In addition, the structure according to the present technology can be applied to position measurement mirrors, wafer chucks, position adjustment components, precision measurement jigs, etc., making it possible to improve processing accuracy.

[0279] <Other Embodiments> The present invention is not limited to the above-described embodiment, and various other embodiments can be realized.

[0280] Fig. 13 is a schematic diagram showing an example of the configuration of a structure according to another embodiment. The structure 27 shown in Fig. 13 is an embodiment in which the first moisture proof layer 3 has a multilayer structure including a ceramic member 28 and an intermediate member 29, as described in Example 6.

[0281] 13 , a metal foil is bonded to the entire first main surface 6 of the CFRP member 2 as an intermediate member 29. A ceramic member 28 is bonded to the surface (top surface) of the intermediate member 29. As the second moisture-proof layer 4, for example, the same metal foil as the intermediate member 29 is bonded.

[0282] The shape and size of the ceramic member 28 to be joined to the intermediate member 29 when viewed from above can be designed arbitrarily. That is, the ceramic member 28 can be designed to have a size smaller than the entire first main surface 6 (the entire surface of the intermediate member 29) when viewed from above.

[0283] A metal foil is bonded to the entire surface of the first main surface 6 as an intermediate member 29. This provides moisture protection to the first main surface 6. This allows the ceramic member 28 bonded to the metal foil to be smaller than the entire surface of the metal foil. This allows the structure 1 to be made smaller and lighter. It also allows the material cost of the ceramic member 28 to be reduced.

[0284] 13 , the surface 9 of the first moisture proof layer 3 opposite to the side that is laminated on the first main surface 6 includes the upper surface 30 of the ceramic member 28 and the upper surface 31 of the portion of the intermediate member 29 on which the ceramic member 28 is not laminated. Thus, the first moisture proof layer 3 of the structure 27 is laminated over the entire first main surface 6, and only a portion of the surface 9 opposite to the side that is laminated on the first main surface 6 is made of a ceramic material. Even with this configuration, the effects unique to the present invention described above can be achieved.

[0285] For example, when the structure 27 is applied to a work stage (suction plate), the ceramic member 28 can be designed in a shape and size required to hold the work. Of course, even when various processes other than flat processing are performed, the ceramic member 28 can be designed in a required shape and size.

[0286] In addition, a multilayer structure may be adopted for the second moisture-proof layer 4 laminated on the second main surface 7 of the CFRP member 2 and the third moisture-proof layer 13 bonded to the side surface 5.

[0287] [Another Configuration Example of CFRP Member] Fig. 14 is a schematic diagram showing a configuration example of a CFRP member according to another embodiment. Fig. 15 is a schematic diagram showing the internal structure of the CFRP member shown in Fig. 14.

[0288] In the above embodiment, a plurality of prepregs, which are sheet-like members primarily composed of carbon fiber, are laminated to form the CFRP member 2. The above-described bonding of the first moisture barrier layer 3, the second moisture barrier layer 4, and the third moisture barrier layer 13 according to the present invention can also be applied to CFRP members having other configurations.

[0289] 14 has an approximate rectangular parallelepiped outer shape and has a first main surface 6 and a second main surface 7 that are large flatwise surfaces. The CFRP member 32 also has side surfaces 8 (a left side surface 8a, a right side surface 8b, a front side surface 8c, and a rear side surface 8d) that are small edgewise surfaces.

[0290] The structure 33 also has an upper skin member 34, a lower skin member 35, side skin members 36 (left skin member 36a, right skin member 36b, front skin member 36c, rear skin member 36d), and an internal structure 37.

[0291] The upper skin member 34 is joined to the upper side of the internal structure 37 and constitutes the first main surface 6. The lower skin member 35 is joined to the lower side of the internal structure 37 and constitutes the second main surface 7.

[0292] The side skin portions 36 are joined to the sides of the internal structure 37 to form the side surfaces 8. As shown in Figures 14 and 15 , the left side surface 8a is formed by a left skin member 36a joined to the left side of the internal structure 37. The right side surface 8b is formed by a right skin member 36b joined to the right side of the internal structure 37. The front side surface 8c is formed by a front skin member 36c joined to the front side of the internal structure 37. The rear side surface 8d is formed by a rear skin member 36d joined to the rear side of the internal structure 37.

[0293] The upper skin member 34, the lower skin member 35, and the side skin member 36 are made of carbon fiber reinforced plastic members formed by laminating prepregs made of carbon fiber impregnated with resin. Note that the upper skin member 34, the lower skin member 35, and the side skin member 36 may each be made of a single sheet of prepreg. There are no specific restrictions on the material of the prepreg.

[0294] 15, the internal structure 37 is formed by assembling a plurality of plate-like members 39. The plate-like members 39 are formed of carbon fiber reinforced plastic members molded by laminating prepregs made of carbon fibers impregnated with resin. Note that the plate-like member 39 may be formed of a single sheet of prepreg. There are no specific limitations on the material of the prepreg.

[0295] In this embodiment, four rectangular plate-like members 39a of the same shape are arranged at equal intervals in the front-rear direction (Y direction) so as to extend in the left-right direction (X direction). Four plate-like members 39b of the same shape as the plate-like members 39a are arranged so as to intersect with the four plate-like members 39a.

[0296] 15, the four plate-like members 39b are arranged at equal intervals in the left-right direction (X direction) so as to extend in the front-rear direction (Y direction). Slits (not shown) are formed at the intersections of the plate-like members 39a and 39b, and the slits fit together.

[0297] As shown in FIG. 15, the plate-like members 39a and 39b are assembled so that both ends of each member are positioned on the periphery of a predetermined rectangle when viewed from above.

[0298] In addition to the plate-shaped members 39a and 39b, six plate-shaped members 39c, whose widthwise size is equal to that of the plate-shaped members 39a and 39b and whose lengthwise size is appropriately adjusted, are arranged so as to intersect with the plate-shaped members 39a and 39b.

[0299] The six plate-like members 39c are arranged at equal intervals along a direction perpendicular to the left-right direction (X direction) and the front-rear direction (Y direction) (the left-right direction in FIG. 15 ) at 45 degrees to each other. The six plate-like members 39c are also arranged so as to intersect at the midpoints between adjacent plate-like members 39a and between adjacent plate-like members 39b. Slits (not shown) are formed at the intersections, and the slits fit together.

[0300] The longitudinal size of the six plate-like members 39c is adjusted appropriately so that the positions of both ends are positioned on the periphery of a predetermined rectangle where both ends of the plate-like members 39a and 39b are located.

[0301] As shown in FIG. 15, when the internal structure 37 is viewed from above, it has a configuration in which hexagonal gaps 40 and triangular gaps 41 are arranged periodically.

[0302] When viewed from above, an upper skin member 34 having a rectangular shape that fits along both ends of the plate-like members 39a to 39c is joined to the upper side of the internal structure 37 to form the first main surface 6. A lower skin member 35 having substantially the same shape as the upper skin member 34 is joined to the lower side of the internal structure 37 to form the second main surface 7. Side skin members 36 (36a to 36d) are joined to the sides of the internal structure 37 to form side surfaces 8 (8a to 8d).

[0303] It is possible to apply the bonding of the first moisture barrier layer 3, the second moisture barrier layer 4, and the third moisture barrier layer 13 according to the present invention described above to such a CFRP member 37, thereby achieving the effects unique to the present invention described above.

[0304] Of course, the present invention can also be applied to a CFRP member having a different configuration from the structure 37 shown in Figures 14 and 15. That is, when applying the present invention, various configurations can be adopted as the internal structure 37 that constitutes the CFRP member.

[0305] For example, an internal structure may be employed in which, when viewed from above, gaps of a predetermined shape, such as a triangle, a rectangle, a regular hexagon, or another polygon, are regularly arranged. For example, an internal structure having a honeycomb structure may be employed. The structures shown in Figures 14 and 15 can also be broadly considered to be internal structures having a honeycomb structure.

[0306] The internal structure may also be formed using corrugated members made of carbon fiber reinforced plastic members, or may be formed by randomly assembling members made of carbon fiber reinforced plastic members.

[0307] The first moisture barrier layer 3 and the second moisture barrier layer 4 described in the first embodiment are bonded to a CFRP member 2 of any configuration having a first main surface 6, a second main surface 7, and a side surface 8. A structure constructed in this manner is included in the following (Structure A).

[0308] (Structure A) A structure comprising: a main body portion formed of a plurality of sheet-like members whose main component is carbon fiber and having a first main surface and a second main surface opposing each other; a first moisture-proof layer laminated on the first main surface, at least a portion of the surface opposite to the side laminated on the first main surface being made of a ceramic material; and a second moisture-proof layer laminated on the second main surface, being made of a material different from the ceramic material.

[0309] Of course, the structure 1 shown in FIG. 1 and the structure 33 shown in FIG. 14 are also included in (structure A).

[0310] As a method for manufacturing such a (Structure A), a manufacturing method including the following steps can be adopted.

[0311] a molding process for forming a main body having a first main surface and the second main surface from a plurality of sheet-like members whose main component is carbon fiber; a first joining process for joining a first moisture-proof layer to the first main surface; and a second joining process for joining a second moisture-proof layer to the second main surface. Note that at least a portion of the surface of the first moisture-proof layer opposite to the side laminated on the first main surface is made of a ceramic material. Furthermore, the second moisture-proof layer is made of a material different from the ceramic material.

[0312] The molding step, the first bonding step, and the second bonding step may be performed in separate steps, or may be performed integrally in the same step. Also, any combination of the molding step, the first bonding step, and the second bonding step may be performed integrally in the same step.

[0313] The first bonding step includes bonding the first moisture-proof layer to a sheet-like member (which can be called a first sheet-like member) that constitutes the first main surface before the molding step, and the second bonding step includes bonding the second moisture-proof layer to a sheet-like member (which can be called a second sheet-like member) that constitutes the second main surface before the molding step.

[0314] 14 and 15 , the molding process of the inner structure 37 and the process of joining the skin members to the inner structure 37 may be performed in separate processes, or may be performed integrally in the same process. Furthermore, the molding process of the CFRP member 33 and the process of joining each moisture-proof layer may be performed in separate processes, or may be performed integrally in the same process.

[0315] Alternatively, the step of joining the upper skin member 34 and the internal structure 37 (i.e., the step of forming the CFRP member 33) may be performed after the first moisture proof layer 3 is joined to the upper skin member 34. Alternatively, the step of joining the lower skin member 35 and the internal structure 37 (i.e., the step of forming the CFRP member 33) may be performed after the second moisture proof layer 4 is joined to the lower skin member 35.

[0316] Furthermore, the above-described (Configuration 1) is applied to a CFRP member 2 having any configuration, including a first main surface 6, a second main surface 7, and a side surface 8. A structure configured in this manner is included in the following (Structure B).

[0317] (Structure B) A structure comprising: a main body portion formed of a plurality of sheet-like members whose main component is carbon fiber, the main body portion having first and second main surfaces opposing each other and side surfaces between the first and second main surfaces; a first moisture-proof layer laminated on the first main surface; a second moisture-proof layer laminated on the second main surface; and a third moisture-proof layer laminated on the side surfaces, wherein at least one of the first moisture-proof layer and the second moisture-proof layer is made of a material other than a ceramic material.

[0318] As a method for manufacturing such a (Structure B), a manufacturing method including the following steps can be adopted.

[0319] a molding process for molding a main body having a first main surface, a second main surface, and a side surface between the first main surface and the second main surface using a plurality of sheet-like members whose main component is carbon fiber; a first joining process for joining a first moisture-proof layer to the first main surface; a second joining process for joining a second moisture-proof layer to the second main surface; and a third joining process for joining a third moisture-proof layer to the third main surface. At least one of the first moisture-proof layer and the second moisture-proof layer is made of a material other than a ceramic material.

[0320] The molding step, the first bonding step, the second bonding step, and the third bonding step may be performed separately or integrally in the same step. Also, any combination of the molding step, the first bonding step, the second bonding step, and the third bonding step may be performed integrally in the same step.

[0321] The first joining step includes joining the first moisture-proof layer to a sheet-like member (which can be called a first sheet-like member) that constitutes the first main surface before the molding step. The second joining step includes joining a second moisture-proof layer to a sheet-like member (which can be called a second sheet-like member) that constitutes the second main surface before the molding step. The third joining step includes joining a third moisture-proof layer to a sheet-like member (which can be called a third sheet-like member) that constitutes the side surface before the molding step.

[0322] 14 and 15 , the molding process of the inner structure 37 and the process of joining the skin members to the inner structure 37 may be performed in separate processes, or may be performed integrally in the same process. Furthermore, the molding process of the CFRP member 33 and the process of joining each moisture-proof layer may be performed in separate processes, or may be performed integrally in the same process.

[0323] Furthermore, the step of joining the upper skin member 34 and the internal structure 37 (i.e., the step of forming the CFRP member 33) may be performed after the first moisture proof layer 3 is joined to the upper skin member 34. Furthermore, the step of joining the lower skin member 35 and the internal structure 37 (i.e., the step of forming the CFRP member 33) may be performed after the second moisture proof layer 4 is joined to the lower skin member 35. Furthermore, the step of joining the side skin member 36 and the internal structure 37 (i.e., the step of forming the CFRP member 33) may be performed after the third moisture proof layer 13 is joined to the side skin member 36.

[0324] In the above embodiment, the first moisture barrier layer 3, at least a portion of which surface 9 is made of a ceramic material, the second moisture barrier layer 4, which is made of a material other than a ceramic material, and the third moisture barrier layer 13, which is basically made of metal foil, have been described. For example, the third moisture barrier layer 13 can be realized using the configuration and bonding method described for the second moisture barrier layer 4, which is made of a material other than a ceramic material. Also, the second moisture barrier layer 13 can be realized using the configuration and bonding method described for the third moisture barrier layer 13, which is basically made of metal foil.

[0325] Furthermore, the configuration and bonding method described for the second moisture barrier layer 4 made of a material other than ceramic material may be used to realize an intermediate member for the first moisture barrier layer 3 that forms a multilayer structure with a ceramic member. Furthermore, the configuration and bonding method described for the third moisture barrier layer 13 that is basically made of metal foil may be used to realize an intermediate member for the first moisture barrier layer 3 that forms a multilayer structure with a ceramic member.

[0326] In the present disclosure, the metal foil is configured to have a thickness of 200 μm or less. For example, the metal foil according to the present invention can be formed so as to have a thickness of 1 μm or more and 200 μm or less.

[0327] If the thickness of the metal foil is too small, through holes may be formed, which may reduce the function of the moisture-proof layer. Therefore, in order to achieve a high moisture-proof function, it is preferable to use a metal foil having a thickness of 5 μm or more.

[0328] Furthermore, as described above, the metal foil undergoes elastic and plastic deformation, thereby making it possible to reduce the thermal residual stress applied to the CFRP member 2. The thinner the metal foil is, the greater the effect of suppressing the thermal residual stress due to elastic and plastic deformation.

[0329] Therefore, by reducing the upper limit of the thickness of the metal foil, for example, to 200 μm or less, 175 μm or less, 150 μm or less, 125 μm or less, 100 μm or less, 75 μm or less, 50 μm or less, or 25 μm or less, it is possible to realize a metal foil that is highly effective in suppressing thermal residual stress due to elastic deformation and plastic deformation.

[0330] Considering both the moisture-proof function and the effect of suppressing thermal residual stress, the thinner the metal foil is, within the range of 5 μm or more, the more preferable the configuration. Of course, even when a metal foil with a thickness of 200 μm is used, the moisture-proof function and the effect of suppressing thermal residual stress are exhibited.

[0331] For example, in the structure 1 of Example 6 described above, the copper foil serving as the intermediate member of the first moisture-proof layer 3 and the copper foil serving as the second moisture-proof layer 4 were both changed to 20 μm-thick Al foil. In this case, no deformation due to thermal residual stress was observed. Furthermore, the results of the accelerated moisture absorption test showed that after 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain was 2.5 με, which was suppressed to 2.7% compared to the reference. This result is equivalent to that when a 20 μm-thick copper foil was used in Example 6.

[0332] In addition, in the structure 1 of Example 6, the copper foil serving as the intermediate member of the first moisture barrier layer 3 and the copper foil serving as the second moisture barrier layer 4 were both replaced with Al foils having a thickness of 50 μm. Even in this configuration, no deformation or the like caused by thermal residual stress was observed. Furthermore, the results of the accelerated moisture absorption test showed that after 60 hours, when the moisture absorption expansion of the reference sample was saturated, the moisture absorption expansion strain was 2.0 με, which was suppressed to 2.1% compared to the reference.

[0333] That is, in the structure 1 of Example 6, three types of samples were tested as the metal foil that serves as the intermediate member of the first moisture-proof layer 3 and the metal foil that serves as the second moisture-proof layer 4: copper foil with a thickness of 20 μm, Al foil with a thickness of 20 μm, and Al foil with a thickness of 50 μm. As a result, no deformation due to thermal residual stress was observed in any of the structures 1, and the results of the accelerated moisture absorption test were also good, at almost the same level.

[0334] Various components can be manufactured using the processing apparatus according to the present invention. For example, by performing exposure using the exposure apparatus according to the present invention, various substrates on which predetermined patterns are formed can be manufactured as components. For example, components can be manufactured such as electrical circuit elements, optical elements, MEMS, recording elements, sensors, or molds. Examples of electrical circuit elements include volatile or non-volatile semiconductor memories such as DRAM, SRAM, flash memory, and MRAM, as well as semiconductor elements such as LSIs, CCDs, image sensors, and FPGAs. Examples of molds include molds for imprinting.

[0335] The respective configurations of the structure, CFRP member, first moisture-proof layer, second moisture-proof layer, third moisture-proof layer, processing device, exposure device, laser processing device, etc., as well as the method for manufacturing the structure, the method for bonding the first moisture-proof layer, the method for bonding the second moisture-proof layer, the method for bonding the third moisture-proof layer, the method for integrally molding a plurality of prepregs, the exposure method, the laser processing method, etc., described with reference to the respective drawings are merely one embodiment and can be arbitrarily modified without departing from the spirit of the present invention. In other words, any other configurations, processing flows, algorithms, etc. for implementing the present invention may be adopted.

[0336] In the present disclosure, terms such as "generally," "almost," and "approximately" are used as appropriate to facilitate understanding of the description. However, there is no clear difference between using and not using terms such as "generally," "almost," and "approximately." That is, in the present disclosure, concepts defining shape, size, positional relationship, state, and the like, such as "center," "central," "uniform," "equal," "same," "orthogonal," "parallel," "symmetrical," "extended," "axial direction," "cylindrical," "cylindrical," "ring-shaped," and "annular," are concepts that include "substantially center," "substantially central," "substantially uniform," "substantially equal," "substantially the same," "substantially orthogonal," "substantially parallel," "substantially symmetrical," "substantially extended," "substantially axial," "substantially cylindrical," "substantially cylindrical," "substantially ring-shaped," and "substantially annular," and the like. For example, states within a predetermined range (e.g., a range of ±10%) based on "completely centered," "completely central," "completely uniform," "completely equal," "completely the same," "completely orthogonal," "completely parallel," "completely symmetrical," "completely extended," "completely axial direction," "completely cylindrical," "completely cylindrical," "completely ring-shaped," "completely annular," and the like are also included. Therefore, even if the words "roughly," "almost," "approximately," etc. are not added, the concept expressed by adding "roughly," "almost," "approximately," etc. may be included. Conversely, a state expressed by adding "roughly," "almost," "approximately," etc. does not necessarily exclude a complete state.

[0337] In the present disclosure, expressions using "than", such as "greater than A" and "smaller than A", are expressions that comprehensively include both concepts that include the case where it is equivalent to A and concepts that do not include the case where it is equivalent to A. For example, "greater than A" is not limited to cases that do not include equivalent to A, but also includes "A or greater". Furthermore, "smaller than A" is not limited to "less than A" but also includes "A or less". When implementing the present technology, specific settings and the like can be appropriately adopted from the concepts included in "greater than A" and "smaller than A" so that the effects described above can be achieved.

[0338] It is also possible to combine at least two of the features of the present technology described above. That is, the various features described in each embodiment may be arbitrarily combined without distinguishing between the embodiments. Furthermore, the various effects described above are merely examples and are not intended to be limiting, and other effects may also be achieved.

[0339] DESCRIPTION OF SYMBOLS 1, 12...Structure (CFRP structure) 2...CFRP member 3...First moisture-proof layer 4...Second moisture-proof layer 5...Prepreg 6...First main surface 7...Second main surface 8 (8a to 8d)...Side surface 9...Surface of first moisture-proof layer 13 (13a to 13d)...Third moisture-proof layer 15...Exposure device 19, 24...Work stage 20, 25...Frame 22...Laser processing device

Claims

1. A structure comprising: a main body formed by laminating a plurality of sheet-like members whose main component is carbon fiber, the main body having a first main surface and a second main surface which face each other in the lamination direction of the plurality of sheet-like members; a first moisture-proof layer laminated on the first main surface, at least a portion of the surface opposite to the side laminated on the first main surface being made of a ceramic material; and a second moisture-proof layer laminated on the second main surface, the second moisture-proof layer being made of a material different from the ceramic material.

2. A structure according to claim 1, wherein the first moisture-proof layer has an entire surface made of a ceramic material.

3. A structure as claimed in claim 1, wherein each of the plurality of sheet-like members is a prepreg made of carbon fibre impregnated with resin, and the main body is a carbon fibre reinforced plastic member formed by laminating the prepregs.

4. A structure according to claim 1, wherein the first moisture-proof layer is made of low thermal expansion glass.

5. The structure according to claim 1, wherein the first moisture-proof layer has a thermal expansion coefficient of -1×10 at temperatures of 20° C. to 130° C. in a direction parallel to the surface laminated on the first main surface. -6 / °C or more than 1×10 -6 A structure made of a low thermal expansion glass having a thermal expansion coefficient in the range of less than 1 / °C.

6. A structure according to claim 1, wherein the first moisture-proof layer includes a low thermal expansion glass constituting the surface, and an intermediate member disposed between the low thermal expansion glass and the first main surface.

7. A structure according to claim 6, wherein the intermediate member is made of a metal foil.

8. A structure according to claim 1, wherein the second moisture-proof layer is composed of any one of a metal foil, a rubber tape on which the metal foil is formed, and a resin film on which a moisture-proof film is formed.

9. A structure according to claim 1, wherein at least one of the first moisture barrier layer and the second moisture barrier layer is bonded to the main body via an adhesive that hardens at low temperatures or an adhesive layer that exerts adhesive strength at low temperatures.

10. A structure according to claim 1, wherein the second moisture-proof layer is formed by adhering the metal foil to the second main surface with an adhesive that hardens at a low temperature.

11. A structure as described in claim 1, wherein the first moisture-proof layer is made of a material in which the thermal residual stress resulting from the process of bonding the first moisture-proof layer to the main body is 6 MPa or less.

12. The structure according to claim 1, wherein the thermal expansion coefficient of the first moisture-proof layer in a direction parallel to the surface of the first main surface at temperatures of 20°C to 130°C is -1×10 -6 / °C or more than 1×10 -6 / °C.

13. The structure according to claim 1, wherein the difference in thermal expansion coefficient between the first moisture-proof layer and the main body is 1×10 -6 A structure made of a ceramic material having a temperature of less than 100°C.

14. A structure according to claim 1, wherein the first moisture-proof layer is laminated over the entire surface of the first main surface, and the second moisture-proof layer is laminated over the entire surface of the second main surface.

15. A structure according to claim 1, wherein the surface of the first moisture-proof layer, which is made of a ceramic material, is configured as a processing surface that is to be processed.

16. A structure according to claim 15, wherein the surface to be machined is a surface to be machined into a flat surface.

17. A structure as described in claim 1, wherein the main body portion has a side surface between the first main surface and the second main surface, and the structure further comprises a third moisture barrier layer laminated to the side surface.

18. The structure according to claim 17, wherein the third moisture-proof layer is formed of any one of a metal foil, a metal sheet, and a rubber tape on which the metal foil is formed.

19. A structure according to claim 17, wherein the third moisture-proof layer is bonded to the side surface via an adhesive that hardens at low temperatures or an adhesive layer that exerts adhesive strength at low temperatures.

20. A structure according to claim 17, wherein the third moisture-proof layer is formed by adhering the metal foil or the metal sheet to the side surface with an adhesive that hardens at a low temperature.

21. A structure comprising: a main body portion formed by stacking a plurality of sheet-like members whose main component is carbon fiber, the main body portion having a first main surface and a second main surface opposing each other in the stacking direction of the plurality of sheet-like members, and a side surface between the first main surface and the second main surface; a first moisture barrier layer laminated on the first main surface, a second moisture barrier layer laminated on the second main surface, and a third moisture barrier layer laminated on the side surface, at least one of the first moisture barrier layer and the second moisture barrier layer being made of a material other than a ceramic material.

22. A structure comprising: a main body composed of multiple sheet-like members whose main component is carbon fiber and having a first main surface and a second main surface opposing each other; a first moisture-proof layer laminated on the first main surface, at least a portion of the surface opposite to the side laminated on the first main surface being made of a ceramic material; and a second moisture-proof layer laminated on the second main surface and made of a material different from the ceramic material.

23. A structure comprising: a main body formed of multiple sheet-like members whose main component is carbon fiber, the main body having first and second main surfaces opposing each other and a side surface between the first and second main surfaces; a first moisture barrier layer laminated on the first main surface; a second moisture barrier layer laminated on the second main surface; and a third moisture barrier layer laminated on the side surface, wherein at least one of the first moisture barrier layer and the second moisture barrier layer is made of a material other than a ceramic material.

24. A processing device for processing a workpiece, the processing device being configured using the structure according to claim 1, 21, 22 or 23.

25. A processing device according to claim 24, wherein the structure is used as a work stage that holds the work.

26. The processing apparatus according to claim 24, configured as an exposure apparatus.

Citation Information

Patent Citations

  • Structure containing ceramic and carbon fiber reinforced plastic

    JP2009248398A

  • High flatness structure

    JP2017080899A

  • Method for producing carbon fiber-reinforced plastic

    JP2018076502A

  • Carbon fiber-reinforced plastic structure and processing device

    JP2019051653A

  • Structure, method for manufacturing the same and processing apparatus

    JP2019136889A