Water cooling device and single crystal furnace
By designing segmented cooling zones and non-cooling zones in the water cooling device, cooling efficiency is reduced, and the residence time of the crystals in the temperature range of 600-850°C is extended, the oxygen precipitation and stress problems caused by high nitrogen concentration are solved, and the BMD density is improved and the mass of the epitaxial layer.
Patent Information
- Application Number
- PCT/CN2023/135374
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-31
- Filing Date
- 2023-11-30
- Publication Date
- 2024-12-05
AI Technical Summary
During the process of electronic-grade large-size semiconductor crystal drawing, oxygen precipitation and stress generated by high nitrogen concentration lead to the crystal’s residence time in the high temperature range being too short, and high-density bulk micro defects (BMDs) cannot be formed, affecting the quality of the epitaxial layer.
Design a water cooling device, including a cooling zone and a water cooling sleeve arranged in segments along the axial direction, reduce cooling efficiency, extend the residence time of the crystal in the temperature range of 600-850°C, and the area through the non-cooling zone is greater than cooling zone to reduce stress and dislocation defects.
It effectively extends the residence time of the crystal in the BMD nucleation temperature range, improves the BMD density, reduces the risk of crystal cracking, and improves the quality of epitaxial silicon wafers.
Smart Images

Figure CN2023135374_05122024_PF_FP_ABST
Abstract
Description
Water cooling device and single crystal furnace
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to Chinese Patent Application No. 202310635809.0 filed in China on May 31, 2023, the entire contents of which are incorporated herein by reference. Technical Field
[0003] The present application relates to the technical field of single crystal rod production, and in particular to a water cooling device and a single crystal furnace. Background Art
[0004] In the related art, during the process of pulling large-scale electronic-grade semiconductor crystals, water cooling is typically added to the area where crystal growth has completed in order to increase crystal growth rates and control defects. Nitrogen doping is commonly used to develop ingots for epitaxial products with bulk micro defect (BMD) densities (>5E8). To meet high BMD concentrations, nitrogen doping concentrations are typically higher than 1E14 atoms / cm3. However, excessively high nitrogen concentrations can lead to the formation of large oxygen precipitates at high temperatures (1000-1200°C), resulting in significant stress and associated dislocation defects during crystal cooling. When such defects appear on the surface of the epitaxial silicon wafer substrate, they can extend into the epilayer as it grows, causing epitaxial stacking faults (EPI stacking faults). Furthermore, to achieve high BMD density, sufficient residual vacancy concentrations are required in the crystal, and the crystal must remain in the nucleation temperature range (600-850°C) for as long as possible.
[0005] Summary of the Invention
[0006] In order to solve the above technical problems, the present application provides a water cooling device and a single crystal furnace to solve the problem of how to prolong the residence time of the crystal in the temperature range of 600-850°C to pull high-density BMD crystal rods.
[0007] In order to achieve the above-mentioned object, the technical solution adopted in the embodiment of the present application is: a water cooling device is applied to a single crystal furnace, comprising a water cooling jacket, wherein along the axial direction of the water cooling jacket, the water cooling jacket comprises a first end and a second end opposite to each other, and when the water cooling jacket is located in the single crystal furnace, the second end is arranged close to the crucible in the single crystal furnace,
[0008] Along a direction from the first end to the second end, the water cooling jacket includes a first portion and a second portion, and the first portion includes a cooling area and a non-cooling area that are spaced apart.
[0009] Optionally, the non-cooling area is provided with at least one through hole.
[0010] Optionally, the area of the cooling zone is smaller than the area of the non-cooling zone.
[0011] Optionally, the area of the non-cooling zone is greater than or equal to 80% of the total area of the first part.
[0012] Optionally, in the circumferential direction of the water-cooling jacket, the circumferential length of one of the cooling zones is smaller than the circumferential length of one of the non-cooling zones.
[0013] Optionally, the inner surface of the cooling zone is provided with a first coating, and the emissivity of the first coating is less than 0.3.
[0014] Optionally, a first cooling pipe extending in the axial direction of the water cooling jacket is provided on the side wall of the cooling zone, and a second cooling pipe communicating with the first cooling pipe is provided on the side wall of the second part.
[0015] Optionally, a side wall of the second portion is hollow to form the second cooling duct.
[0016] Optionally, the inner surface of the second portion is provided with a second coating, and the emissivity of the second coating is greater than 0.8.
[0017] An embodiment of the present application also provides a single crystal furnace, comprising the above-mentioned water cooling device.
[0018] The beneficial effects of the present application are: the water-cooling jacket is segmented along its axial direction, and a cooling zone and a non-cooling zone are set on the first part, thereby reducing the cooling area of the first part, thereby reducing the cooling efficiency of the first part, and further extending the time that the crystal stays in the BMD nucleation temperature (600-850°C) region to promote the BMD nucleation density. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] FIG1 is a schematic diagram of a water cooling device according to an embodiment of the present application;
[0020] FIG2 is a schematic diagram showing the temperature distribution inside the crystal in the related art
[0021] FIG3 is a schematic diagram showing the temperature distribution inside the crystal in an embodiment of the present application;
[0022] Figure 4 shows a schematic diagram of a single crystal furnace in an embodiment of the present application. 1 First section; 2 Second section; 11 Cooling zone; 12 Non-cooling zone; 100 Crystal; 101 Position corresponding to 1200°C; 102 Position corresponding to 1000°C; 103 Position corresponding to 850°C; 104 Position corresponding to 600°C; 3 Flange; 5 Furnace body; 6 Crucible assembly; 7 Heating element; 8 Support shaft; 9 Guide tube; 10 Water cooling jacket. DETAILED DESCRIPTION
[0023] To make the purpose, technical solutions, and advantages of the embodiments of the present disclosure more clear, the technical solutions of the embodiments of the present disclosure will be clearly and completely described below in conjunction with the accompanying drawings of the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, not all of the embodiments. Based on the described embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present disclosure.
[0024] Unless otherwise defined, the technical or scientific terms used in this disclosure should have the usual meanings understood by people with ordinary skills in the field to which this disclosure belongs. The words "first", "second" and similar words used in this disclosure do not indicate any order, quantity or importance, but are only used to distinguish different components. Similarly, words such as "one", "an" or "the" do not indicate a quantity limitation, but rather indicate the existence of at least one. Words such as "include" or "comprise" mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects. Words such as "connect" or "connected" are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the object being described changes, the relative positional relationship may also change accordingly.
[0025] In recent years, with the development of miniaturization in the manufacturing process of semiconductor devices, the requirements for the required silicon wafers are getting higher and higher. Not only are the surface defects of the silicon wafers required to be few or even defect-free, but the silicon wafers are also required to have sufficient bulk micro defects (BMDs) to protect the silicon wafer area where the electronic components are set from being contaminated by heavy metal impurities. The heavy metal impurities contained in the silicon wafer have become an important factor affecting the quality of semiconductor devices. Therefore, the content of heavy metal impurities needs to be reduced as much as possible during the silicon wafer production process. At present, it is known that when enough BMDs are formed inside the silicon wafer, these BMDs have the intrinsic gettering (IG) effect of capturing heavy metal impurities, which can greatly improve the problem of poor quality of semiconductor devices caused by heavy metal impurities. In recent years, the production of silicon wafers containing BMDs with a density equal to or greater than 1×10 8 As the demand for silicon wafers with a density of 100 BMDs / cm3 increases, sufficient BMD cores need to be included in the base silicon wafer when the silicon wafers are supplied to electronic component manufacturers so that a high BMD density can be achieved.
[0026] Epitaxial silicon wafers are made by growing a single crystal layer (also known as an epitaxial layer) on a silicon wafer via a vapor deposition reaction. Due to the high crystalline integrity and near-defect nature of epitaxial layers, epitaxial silicon wafers are currently widely used as substrate materials for semiconductor devices. However, during the epitaxial growth process, the silicon wafers are exposed to high temperatures exceeding 1000°C, which eliminates smaller BMD cores. Consequently, the epitaxial silicon wafers lack sufficient BMD cores, resulting in an inability to generate a sufficient density of BMDs when manufacturing semiconductor devices using these epitaxial silicon wafers. This, in turn, results in poor quality of the resulting semiconductor devices.
[0027] 1 to 4 , this embodiment provides a water cooling device for use in a single crystal furnace, comprising a water cooling jacket. Along the axial direction of the water cooling jacket, the water cooling jacket comprises a first end and a second end opposite to each other. When the water cooling jacket is located in the single crystal furnace, the second end is disposed adjacent to the crucible in the single crystal furnace.
[0028] Along the direction from the first end to the second end, the water cooling jacket includes a first portion 1 and a second portion 2 , and the first portion 1 includes a cooling area 11 and a non-cooling area 12 that are spaced apart.
[0029] The water-cooling jacket is segmented along its axial direction, and a cooling zone and a non-cooling zone are provided on the first portion, thereby reducing the cooling area of the first portion and thus reducing the cooling efficiency of the first portion. This can extend the time that the crystal 100 stays in the BMD nucleation temperature region (600-850° C.) to promote the BMD nucleation density.
[0030] It should be noted that the setting of the non-cooling zone 11 in the first part 1 makes it possible for only the bottom of the water-cooling jacket (i.e., the second end) to have the maximum cooling effect. Compared with the traditional water-cooling jacket, it can reduce the stress generated in the crystal 100 and thus reduce the problem of cracking of the crystal 100 caused by excessive cooling.
[0031] It should be noted that the specific structural forms of the non-cooling zone 12 and the cooling zone 11 can be various, as long as the cooling area of the first portion 1 can be reduced to reduce the cooling zone efficiency of the first portion 1. The structural forms of the non-cooling zone 12 and the cooling zone 11 in this embodiment are described in detail below.
[0032] In an exemplary embodiment, the cooling area 11 and the non-cooling area 12 are arranged at intervals along the circumferential direction of the water-cooling jacket.
[0033] During the crystal ingot pulling process, the crystal ingot is located in the crystal ingot lifting area in the middle of the water-cooling jacket. The cooling zone 11 and the non-cooling zone 12 are arranged at intervals along the circumferential direction of the water-cooling jacket, which is beneficial to the uniformity of the temperature of the crystal ingot in the circumferential direction.
[0034] In order to effectively reduce the cooling efficiency of the first portion 1 , the total area of the non-cooling zone 12 is greater than the total area of the cooling zone 11 .
[0035] In a specific embodiment, in the circumferential direction of the water-cooling jacket, the circumferential length of one cooling zone 11 is smaller than the circumferential length of one non-cooling zone 12 , so that the area of each non-cooling zone 12 is larger than the area of each cooling zone 11 .
[0036] The larger the area of the non-cooling zone 12 is and the smaller the area of the cooling zone 11 is, the lower the cooling efficiency of the first part 1 is.
[0037] It should be noted that to increase the residence time of the crystal in the temperature range of 600-850°C, the length L1 of the first portion in the axial direction of the water-cooling jacket should not be too large. For example, the maximum length of L1 should not exceed 30 cm (for example, L1 can be 20 cm, 25 cm, 30 cm, etc.). At the same time, in the L1 portion, the area of the non-cooling zone should be as large as possible while ensuring the water cooling effect of the second portion. For example, the area of the non-cooling zone accounts for greater than or equal to 80%, but the invention is not limited thereto.
[0038] Exemplarily, the first part includes at least two cooling zones 11 , and the areas of the at least two cooling zones 11 are the same, thereby improving the temperature uniformity of the water cooling jacket on the crystal rod and the silicon melt.
[0039] In an exemplary embodiment, the non-cooling area 12 is provided with at least one through hole.
[0040] The provision of the through holes can effectively reduce the cooling area of the first portion 1 , thereby reducing the cooling efficiency of the first portion 1 and increasing the residence time of the crystal in the temperature range (600-850° C.) during the pulling process.
[0041] In one embodiment, the non-cooling area 12 is provided with a through hole, and the through hole completely covers the non-cooling area 12 .
[0042] It should be noted that in order to avoid affecting the axial gradient change of the crystal, the time that the crystal stays in the temperature range of 600-850°C should not be too long. Therefore, a flange 3 is provided at the first end, and a connecting area 4 is provided between the flange 3 and the first part 1, that is, the first part does not directly pass through the first end of the water-cooling jacket, but this is not limited to this.
[0043] In an exemplary embodiment, the non-cooling area 12 is provided with a plurality of through holes, which can increase the overall connection stability of the water cooling jacket compared to the provision of a single through hole.
[0044] The through holes may be distributed in various ways, for example, along the circumferential direction of the water cooling jacket, a plurality of rows of through holes may be arranged side by side and at intervals.
[0045] The length of each through hole in the axial direction of the water cooling jacket can be set according to actual needs.
[0046] The length of each through hole in the circumferential direction of the water cooling jacket can also be set according to actual needs.
[0047] In the circumferential direction of the water cooling jacket, the spacing between two adjacent rows of through holes can be set according to actual needs. For example, the spacing between two adjacent rows of through holes can be half of the width of the through holes in the circumferential direction of the water cooling jacket, but is not limited thereto.
[0048] Exemplarily, the plurality of columns of through holes include a first column of through holes and a second column of through holes that are adjacent to each other, and an orthographic projection of one through hole in the first column of through holes on the second column of through holes completely coincides with a corresponding through hole in the second column of through holes.
[0049] Exemplarily, the plurality of columns of through holes include a first column of through holes and a second column of through holes that are adjacent to each other, and an orthographic projection of a through hole in the first column of through holes on the second column of through holes partially overlaps with a corresponding through hole in the second column of through holes.
[0050] In an exemplary embodiment, the inner surface of the cooling zone 11 is provided with a first coating layer, and the emissivity of the first coating layer is less than 0.3, but the present invention is not limited thereto.
[0051] The provision of the first coating layer can reduce the amount of heat absorbed by the cooling zone 11 , thereby reducing the cooling efficiency of the cooling zone 11 .
[0052] It should be noted that the first coating is made of silicon-based ceramic material, and its emissivity can be controlled by setting the depth of its color. The darker the color, the greater the emissivity and the greater the heat absorption capacity. The lighter the color, the smaller the emissivity and the smaller the heat absorption capacity.
[0053] Illustratively, the color of the first coating layer is white, but not limited thereto.
[0054] In the related art, in order to solve the problem of reduced BMD density in epitaxial silicon wafers, nitrogen doping is usually performed during the pulling process of single crystal silicon rods to obtain a stable BMD core. When the nitrogen concentration is too high, a large number of large-sized oxygen precipitates will be formed at high temperatures (1000-1200°C), which will generate large stress and related dislocation defects during the cooling process of the crystal. When this defect appears on the surface of the epitaxial silicon wafer substrate, it will extend into the epitaxial layer as the epitaxial layer grows, causing an epitaxial stacking fault (EPI Stacking Fault). In addition, in order to form high-density BMDs, the crystal needs to stay in the nucleation temperature range (600-850°C) as long as possible.
[0055] In related technologies, the crystal pulling speed is increased to reduce the crystal's residence time in the temperature region where large-size oxygen precipitation is formed (1000-1200°C). However, this method will also reduce the crystal's time in the BMD nucleation temperature range (600-850°C), which is not conducive to the formation of a high-density BMD core.
[0056] To avoid epitaxial stacking faults when doping with high nitrogen concentrations, the crystal's residence time in the temperature range (1000-1200°C) where large oxygen precipitates form is minimized during cooling. Compared to water-cooling jackets in related art, this embodiment improves the cooling efficiency of the second portion. Specifically, this can be achieved by increasing the cooling area of the second portion, but the invention is not limited thereto.
[0057] Exemplarily, the cooling area of the second portion may be increased by increasing the length of the second portion in the axial direction of the water-cooling jacket.
[0058] It should be noted that, as the length of the second portion in the axial direction of the water-cooling jacket increases, the total length of the water-cooling jacket in its axial direction increases, and thereby the distance between the water-cooling jacket and the liquid surface of the silicon melt decreases. For example, the length of the second portion in the axial direction of the water-cooling jacket increases by 10-20 cm, but is not limited thereto.
[0059] Illustratively, in the axial direction of the water-cooling jacket, the length of the second portion is greater than or equal to 10 cm, for example, 12 cm, 15 cm, etc., but is not limited thereto.
[0060] The second portion 2 absorbs heat to fully remove the heat radiated by the melt and ensure the crystal growth rate, thereby reducing the residence time in the temperature range of 1000-1200°C.
[0061] FIG2 is a schematic diagram of the axial temperature distribution of a crystal obtained in the related art, and FIG3 is a schematic diagram of the axial temperature distribution of a crystal formed after adopting the water cooling device in the embodiment of the present application.
[0062] In FIG2 and FIG3, the area between the reference numerals 101 and 102 is a temperature range of 1000-1200°C, and the area between the reference numerals 103 and 104 is a temperature range of 600-850°C.
[0063] It can be seen from Figures 2 and 3 that after adopting the water cooling device of the embodiment of the present application, the pulling distance of the crystal in the temperature range of 1000-1200°C is reduced, and the pulling distance of the crystal in the temperature range (600-850°C) is increased. The pulling distance of the crystal at 1000-1200°C in Figure 2 is 73mm, and the pulling distance of the crystal at 1000-1200°C in Figure 3 is reduced to 59mm. The pulling distance of the crystal in the temperature range (600-850°C) in Figure 2 is 172mm, and the pulling distance of the crystal in the temperature range (600-850°C) in Figure 3 is increased to 320mm.
[0064] It should be noted that, corresponding to the axial temperature distribution of the crystal in Figure 2, the bottom end of the water-cooling jacket is 35 cm away from the silicon melt, corresponding to the axial temperature distribution of the crystal in Figure 3, the bottom end of the water-cooling jacket is 23 cm away from the silicon melt, and the length L2 of the second part in the axial direction of the water-cooling jacket is 10 cm, the length L1 of the first part in the axial direction of the water-cooling jacket is 30 cm, and a through hole is provided in the non-cooling zone, and the area of the through hole is 80% of the total area of the first part.
[0065] In an exemplary embodiment, a first cooling pipe extending in the axial direction of the water cooling jacket is provided on the side wall of the cooling zone 11 , and a second cooling pipe communicating with the first cooling pipe is provided on the side wall of the second portion 2 .
[0066] The first cooling pipe and the second cooling pipe contain a cooling medium, which may be cooling water, but is not limited thereto.
[0067] The first cooling pipes are only distributed in the cooling zone 11 , thereby reducing the cooling efficiency of the first portion 1 .
[0068] It should be noted that the larger the area of the non-cooling zone, the lower the cooling zone efficiency of the first part, and thus the longer the crystal stays in the temperature range of 600-850 degrees. However, the area of the cooling zone must ensure that sufficient cooling medium is delivered to the second part to ensure the cooling efficiency of the second part. Therefore, in some embodiments, the area of the non-cooling zone accounts for less than or equal to 80% of the total area of the first part, but is not limited to this.
[0069] Illustratively, the entire second portion 2 is a cooling zone 11, which effectively absorbs heat and ensures the growth rate of the crystal.
[0070] In order to increase the cooling efficiency of the second part 2, in an exemplary embodiment, the second part 2 is hollow as a whole, that is, the internal space of the side wall of the second part 2 serves as the second cooling pipe and is filled with cooling medium. Compared with the arrangement of laying multiple cooling pipes, the cooling area can be increased and the cost can be reduced.
[0071] In order to increase the cooling efficiency of the second portion 2 , in an exemplary embodiment, the inner surface of the second portion 2 is provided with a second coating, and the emissivity of the second coating is greater than 0.8.
[0072] Exemplarily, the second coating is made of silicon-based ceramic material, and its emissivity can be controlled by setting the depth of its color. The darker the color, the greater the emissivity and the greater the heat absorption capacity. The lighter the color, the smaller the emissivity and the smaller the heat absorption capacity.
[0073] Illustratively, the color of the second coating layer is black, but not limited thereto.
[0074] In order to increase the cooling efficiency of the second portion 2, in an exemplary embodiment, a concave-convex structure is provided on the inner wall of the second portion 2 to increase the cooling area.
[0075] It should be noted that the specific structural forms of the concave-convex structure can be various, as long as the cooling area of the second part 2 can be increased. The following introduces several specific configuration forms of the concave-convex structure in this embodiment.
[0076] In an exemplary embodiment, the concave-convex structure includes a plurality of convex portions and concave portions extending along a circumferential direction of the water-cooling jacket, such that the concave-convex structure is wavy.
[0077] In an exemplary embodiment, the concave-convex structure includes a plurality of protrusions arranged at intervals on the inner wall of the second portion 2 .
[0078] Exemplarily, the plurality of protrusions are evenly distributed on the second portion 2 .
[0079] Exemplarily, the plurality of protrusions and the side wall of the second portion 2 are an integral structure, which simplifies the manufacturing process and improves the connection stability between the plurality of protrusions and the second portion 2 .
[0080] Exemplarily, the plurality of protrusions are formed by extending inward from corresponding positions on the inner wall of the second portion 2 .
[0081] Exemplarily, there is a depression between two adjacent protrusions, that is, the plurality of protrusions are formed by depressions outwards at corresponding positions on the inner wall of the second part 2 so that the protrusions are formed at positions corresponding to the protrusions.
[0082] Exemplarily, the inner wall of the second part 2 includes a first area and a second area that are staggered, the first area extends inward to form the protrusion to form the concave-convex structure on the inner wall of the second part 2, and / or the second area is recessed outward so that the inner wall of the second part 2 forms the concave-convex structure.
[0083] For example, in order to prevent the protrusion from damaging the crystal rod, the end of the protrusion away from the inner wall of the second portion 2 is a round end.
[0084] Exemplarily, the diameter of the sidewall of the water-cooling jacket gradually decreases from the first portion 1 to the second portion 2. That is, the water-cooling jacket has a tapered structure. The closer the distance between the sidewall of the water-cooling jacket and the crystal ingot is, the higher the cooling rate is, and the farther the distance between the sidewall of the water-cooling jacket and the crystal ingot is, the lower the cooling rate is.
[0085] Exemplarily, in the radial direction of the water-cooling jacket, the thickness of the second portion 2 is greater than that of the first portion 1 , and the interior of the second portion 2 is hollow as a whole to accommodate the cooling medium, thereby increasing the capacity of the cooling medium and thus increasing the cooling rate.
[0086] Exemplarily, the outer surface of the first part 1 and the outer surface of the second part 2 are located in the same plane, the inner surface of the first part 1 and the inner surface of the second part 2 form a step structure, and the inner wall of the second part 2 is protruded inward to prevent the water cooling jacket from interfering with other components.
[0087] Exemplarily, the water cooling device further includes a lifting structure, and the lifting structure is used to control the lifting and lowering of the water cooling jacket.
[0088] The lifting structure includes a driving part and a transmission part. The transmission part includes two lifting rods. The first end of the water cooling jacket includes a flange 3. The flange 3 is connected to the lifting rods.
[0089] The driving part may be a driving motor, but is not limited thereto.
[0090] 4 , an embodiment of the present application further provides a single crystal furnace, comprising the above-mentioned water cooling device.
[0091] The single crystal furnace further includes the aforementioned water cooling device, which includes a water cooling jacket 10 and a lifting structure for controlling the lifting of the water cooling jacket 10 .
[0092] The lifting structure passes through the furnace cover to be connected to the water-cooling jacket 10 , and controls the water-cooling jacket 10 to be suspended above the silicon melt.
[0093] The single crystal furnace also includes:
[0094] Furnace body 5;
[0095] A furnace cover provided on the furnace body 5;
[0096] A crucible assembly 6 is disposed in the inner cavity of the furnace body 5, and the crucible assembly 6 includes a quartz crucible and a graphite crucible that are arranged in a sleeve, and the quartz crucible contains a silicon solution;
[0097] A guide tube 9 is sleeved on the outside of the water cooling jacket 10, with a gap between the guide tube 9 and the water cooling jacket 10;
[0098] A heating component 7 is provided around the crucible assembly and is used to heat the crucible assembly 6. The heating component is fixed to the bottom of the furnace body 5 through electrode bolts and is connected to the heating electrode at the bottom of the furnace body 5;
[0099] a heat-insulating layer 20 , provided between the heating component 7 and the side wall of the furnace body 5 , for preventing the heat of the heating component 7 from radiating to the outside of the furnace body 5 ;
[0100] The support shaft 8 is supported and connected to the bottom of the graphite crucible; the upper end of the support shaft 8 is provided with a crucible tray, and the lower end of the support shaft 8 passes through the bottom of the furnace body 5.
[0101] The following describes the process of crystal pulling using the above-mentioned single crystal furnace:
[0102] First, the crystal raw material is placed in the crucible assembly 6 and melted by the high temperature generated by the heating part 7 .
[0103] Then, the molten silicon solution is slightly cooled to produce a certain degree of supercooling.
[0104] Then, a silicon single crystal (called a seed crystal) fixed on the seed crystal axis is inserted into the melt surface. After the seed crystal and the melt are melted, the seed crystal is slowly pulled upward, and the crystal will grow at the lower end of the seed crystal.
[0105] Next, the seed crystal is controlled to grow a thin neck with a length of about 100 mm and a diameter of 3 mm to 5 mm to eliminate the dislocation of atomic arrangement caused by the strong thermal shock of the high-temperature solution on the seed crystal. This process is called seeding.
[0106] Subsequently, the crystal diameter is enlarged to the size required by the process, generally 75mm to 300mm. This process is called shouldering.
[0107] Then, suddenly increase the pulling speed to rotate the shoulder so that the shoulder is approximately at a right angle.
[0108] Then, the equal-diameter process is entered, and single crystal columns of a certain size are grown by controlling the thermal field temperature and the crystal lifting speed.
[0109] Finally, when most of the silicon solution has completed crystallization, the crystals are gradually shrunk to form a tail-shaped cone, which is called the finishing process.
[0110] In this way, the single crystal pulling process is basically completed and can be taken out after a certain period of insulation and cooling.
[0111] It is understood that the above embodiments are merely exemplary embodiments for illustrating the principles of the present application, and the present application is not limited thereto. Those skilled in the art may make various modifications and improvements without departing from the spirit and substance of the present application, and such modifications and improvements are also considered to be within the scope of protection of the present application.
Claims
1. A water cooling device, applied in a single crystal furnace, comprising a water cooling jacket, wherein along the axial direction of the water cooling jacket, the water cooling jacket comprises a first end and a second end opposite to each other, and when the water cooling jacket is located in the single crystal furnace, the second end is arranged close to the crucible in the single crystal furnace; Along a direction from the first end to the second end, the water cooling jacket includes a first portion and a second portion, and the first portion includes a cooling area and a non-cooling area that are spaced apart.
2. The water cooling device according to claim 1, wherein: The non-cooling zone is provided with at least one through hole.
3. The water cooling device according to claim 1, wherein: The area of the cooling zone is smaller than the area of the non-cooling zone.
4. The water cooling device according to claim 3, wherein: The area of the non-cooling zone is greater than or equal to 80% of the total area of the first portion.
5. The water cooling device according to claim 1, wherein: In the circumferential direction of the water-cooling jacket, the circumferential length of one of the cooling zones is smaller than the circumferential length of one of the non-cooling zones.
6. The water cooling device according to claim 1, wherein: The inner surface of the cooling zone is provided with a first coating, and the emissivity of the first coating is less than 0.
3.
7. The water cooling device according to claim 1, wherein: A first cooling pipeline extending in the axial direction of the water cooling jacket is arranged on the side wall of the cooling zone, and a second cooling pipeline communicating with the first cooling pipeline is arranged on the side wall of the second part.
8. The water cooling device according to claim 7, wherein: The side wall of the second portion is hollow to form the second cooling duct.
9. The water cooling device according to claim 1, wherein: The inner surface of the second portion is provided with a second coating, and the emissivity of the second coating is greater than 0.
8.
10. A single crystal furnace, comprising the water cooling device according to any one of claims 1 to 9.
Citation Information
Patent Citations
Heat field structure for fast increasing growth speed of czochralski silicon single crystal
CN104313682A
Cooling rate control apparatus and ingot growing apparatus including same
CN105189834A
Heat exchanger for growing silicon crystal ingot, growth furnace of silicon crystal ingot and method for preparing silicon crystal ingot
CN109537045A
Crystal growth furnace and water-cooling jacket of crystal growth furnace
CN109811400A
Novel semiconductor monocrystalline silicon furnace water jacket
CN112048762A