Chip and manufacturing method therefor, and electronic device

By using the electroless gold plating method in the chip to form a seed layer and an electroplated gold layer on the nickel-containing adhesive layer, the problem of difference in the thickness of the conductive plating layer is solved, the chip performance is improved and the cost is reduced.

WO2024244702A1PCT designated stage expired Publication Date: 2024-12-05HUAWEI TECH CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/086818
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-26
Filing Date
2024-04-09
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

In existing chips, the thickness of the conductive plating layer on the back of the substrate varies greatly between the inside and outside of the through holes, resulting in uneven performance and affecting chip performance.

Method used

The seed layer and electroplating layer are formed on the nickel-containing adhesive layer by electroless gold. The replacement reaction between nickel and gold is used to increase the seed layer thickness in the through hole, reduce the thickness difference between inside and outside the through hole, and control the adhesive layer. and the thickness of the electroless gold plating layer ensures uniformity of the conductive plating layer.

Benefits of technology

It effectively reduces the thickness difference between the conductive plating layer inside and outside the through hole, avoids the phenomenon of clamping, improves the uniformity and chip performance of the conductive plating layer, and reduces the amount of gold used and production cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024086818_05122024_PF_FP_ABST
    Figure CN2024086818_05122024_PF_FP_ABST
Patent Text Reader

Abstract

The present application provides a chip and a manufacturing method therefor, and an electronic device. When a chemical gold-plated layer is manufactured on a nickel-containing adhesion layer by using a chemical gold plating method, due to no influence from an electric field or a magnetic field, gold cannot be affected by an incident angle and therefore can easily enter a through hole; gold is deposited on the surface of the adhesion layer by using a replacement reaction between nickel and gold, and the thickness of the chemical gold-plated layer inside the through hole can be increased by means of gold entering the through hole, thereby reducing the thickness difference of the chemical gold-plated layer inside and outside the through hole, reducing the thickness difference of a conductive coating inside and outside the through hole, avoiding parting lines, improving the uniformity of the conductive coating inside and outside the through hole, and improving the performance of the conductive coating and even the chip. In addition, since the adhesion layer is a nickel-containing film layer, gold can be deposited on the surface of the adhesion layer, and gold cannot be deposited at other positions without the adhesion layer, thereby reducing the consumption of gold, and reducing the manufacturing costs of the chip.
Need to check novelty before this filing date? Find Prior Art

Description

Chip, manufacturing method thereof and electronic device

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims priority to the Chinese patent application filed with the State Intellectual Property Office of China on May 26, 2023, with application number 202310610896.4 and application name “A chip, its manufacturing method and electronic device”, the entire contents of which are incorporated by reference into this application. Technical Field

[0003] The present application relates to the field of semiconductor technology, and in particular to a chip, a manufacturing method thereof, and an electronic device. Background Art

[0004] A chip includes a substrate and semiconductor devices, such as transistors and capacitors, disposed on the substrate. The surface on which the semiconductor devices are disposed is referred to as the front side of the substrate, and the other surface is referred to as the back side of the substrate. When a through-hole is provided in the substrate, the power supply or ground terminal of the semiconductor device can cover the through-hole. Furthermore, when a conductive coating is formed on the back side of the substrate, the conductive coating not only covers the back side but also the sidewalls of the through-hole and the surface of the power supply or ground terminal exposed by the through-hole. This allows heat generated by the semiconductor device during operation to be conducted away from the back side, improving the chip's heat dissipation capacity. It also simplifies the complexity of the substrate's front side structure, allowing the power supply or ground terminal of the semiconductor device to be integrated into the back side of the substrate.

[0005] However, in current technology, the thickness of the conductive coating produced on the back side of the substrate varies greatly inside and outside the through-hole, which is prone to clamping. This will lead to uneven performance of the conductive coating inside and outside the through-hole, and then lead to a decrease in the performance of the conductive coating, thereby affecting the performance of the chip.

[0006] Summary of the Invention

[0007] The present application provides a chip, a manufacturing method thereof, and an electronic device, which can reduce the thickness difference of the conductive plating layer inside and outside the through hole, and improve the performance of the conductive plating layer and even the chip.

[0008] In a first aspect, an embodiment of the present application provides a chip, which may include a substrate and a conductive structure, wherein the substrate has: a first surface and a second surface arranged relative to each other, and a through hole extending through the first surface and the second surface, the number of the through hole may be one, two, three or more, and may be set according to actual needs and is not limited here. The conductive structure may be provided on the first surface, the number of the conductive structures may be one, two or more, and the function of each conductive structure may include but is not limited to: transmitting power signals, ground signals or other signals, and the functions of each conductive structure may be the same, partially the same or different, and may be set according to actual needs. However, no matter how many conductive structures are provided and how the functions of each conductive structure are set, as long as there is a conductive structure covering the through hole, the number of through holes covered by the conductive structure is not limited here.

[0009] The chip may further include a conductive plating layer, which may be formed on the second surface, the side walls of the through hole and the surface of the conductive structure exposed by the through hole, wherein the portion of the second surface other than the through hole may be referred to as an outer hole area, the side walls of the through hole may be referred to as simply hole walls, and the surface of the conductive structure exposed by the through hole may be regarded as a hole bottom, so that the outer hole area, the hole walls and the hole bottom are all provided with a conductive plating layer, and the conductive plating layer is connected to the conductive structure, so that the heat in the conductive structure can be conducted to the second surface through the conductive plating layer and dissipated through the second surface, and the signal transmitted by the conductive structure can also be transmitted to the conductive plating layer.

[0010] Wherein, the conductive plating layer may include: an adhesion layer formed in the hole outer area, the hole wall and the hole bottom, a chemical gold plating layer formed on the adhesion layer, and an electroplated gold layer formed on the chemical gold plating layer, so that the adhesion layer, the chemical gold plating layer and the electroplated gold layer are stacked in sequence along the direction from the first surface to the second surface. In this way, when the chemical gold plating method is used to make the chemical gold plating layer (also referred to as the seed layer) on the nickel-containing adhesion layer, since the chemical plating is not affected by the electric field or the magnetic field, there is no problem of the incident angle of the particles, and thus the gold is not affected by the incident angle and can more easily enter the through hole, and the substitution reaction of nickel and gold is used to deposit gold on the surface of the adhesion layer, and the gold entering the through hole can increase the thickness of the seed layer in the through hole, reduce the thickness difference of the seed layer inside and outside the through hole, and then reduce the thickness difference of the electroplated gold layer inside and outside the through hole, thereby reducing the thickness difference of the conductive plating layer inside and outside the through hole, avoiding the pinching phenomenon, improving the uniformity of the conductive plating layer inside and outside the through hole, and improving the performance of the conductive plating layer and even the chip. Moreover, since the adhesion layer is a nickel-containing film layer, a seed layer can be produced on the surface of the adhesion layer, and gold will not be deposited in other locations without the adhesion layer. This solves the problem of gold waste caused by most of the gold being deposited on the inner wall of the equipment cavity in the physical vapor deposition (PVD) method, reduces the amount of gold used, and thus reduces the cost of chip production.

[0011] In some embodiments, for the chemical gold-plated layer, the ratio of the first thickness located at any point in the through-hole to the second thickness located at any point on the second surface can be set to be greater than or equal to 0.5, indicating that the thickness difference of the seed layer inside and outside the through-hole is small, which effectively reduces the resistance of the seed layer in the through-hole. Therefore, when the gold-plated layer is produced by electroplating on the seed layer, the gold-plated layer in the through-hole can be made thicker, further reducing the thickness difference inside and outside the through-hole during gold plating, further improving the thickness uniformity of the conductive plating layer, and at the same time reducing the time for gold plating, thereby not only saving the amount of gold used, but also improving the production efficiency of the conductive plating layer and even the chip.

[0012] Exemplarily, any location within the through hole mentioned in the above content may include a location at one-third to two-thirds of the depth of the through hole. Exemplarily, for example, it includes a location at one-half the depth of the through hole. The thickness of the chemically plated gold layer at these locations is relatively close to the average thickness of the chemically plated gold layer at each location in the through hole. Selecting the thickness of the chemically plated gold layer at these locations as the first thickness can relatively easily achieve a ratio of the first thickness to the second thickness greater than or equal to 0.5, thereby helping to reduce the thickness difference of the electroplated gold layer inside and outside the through hole and reducing the time for electroplating gold.

[0013] Furthermore, the second thickness can be set to be greater than or equal to 300 nm. This helps ensure that the electroless gold-plated layer in the through-hole has a certain thickness, avoiding the electroless gold-plated layer in the through-hole being too thin and resulting in excessive resistance, thereby helping to reduce the thickness difference between the electroless gold-plated layer inside and outside the through-hole, and reducing the thickness difference between the conductive plating layer inside and outside the through-hole. In particular, when the ratio of the first thickness to the second thickness is greater than or equal to 0.5, the thickness difference between the conductive plating layer inside and outside the through-hole can be further reduced. Furthermore, when the second thickness is greater than or equal to 300 nm, the internal stress of the electroless gold-plated layer can be reduced, preventing the electroless gold-plated layer from warping, thereby helping to reduce the thickness difference between the conductive plating layer inside and outside the through-hole, and improving the performance of the conductive plating layer and even the chip.

[0014] In some embodiments, the atomic content of nickel in the adhesion layer can be set to be greater than or equal to 80%, and the atomic content of other elements can be set to be no greater than 20%. This allows the adhesion layer to contain more nickel. Since chemical gold plating can be directly performed on the surface of the nickel-containing film layer without the use of any catalyst, and the nickel content in the adhesion layer has a certain influence on the gold plating effect, the higher the nickel content, the easier the gold plating will be, and the lower the nickel content, the lower the ease of gold plating. Therefore, a higher nickel content in the adhesion layer can promote and accelerate the deposition of gold, allowing gold to be more easily deposited on the surface of the adhesion layer, thereby improving the production efficiency of the chemical gold plating layer.

[0015] Furthermore, the adhesion layer can be made of at least one of elemental nickel and a nickel-containing inorganic material, and can have a single-layer or multi-layer structure. When the adhesion layer has a multi-layer structure, the materials of each layer can be the same or different, and can be set according to actual needs. Among them, when selecting the nickel-containing inorganic material, at least one can be selected from nickel-vanadium alloy, nickel phosphide, nickel nitride, nickel boride, nickel-tungsten alloy, nickel-aluminum alloy, nickel-titanium alloy, nickel-thallium alloy, and nickel-chromium alloy, etc., allowing for a wide range of material choices to meet the needs of various application scenarios.

[0016] In addition, when making the adhesion layer, the PVD method can be used, and the thickness of the adhesion layer can be controlled to be 0.1μm to 0.5μm. This can avoid affecting the gold plating effect during chemical gold plating when the adhesion layer is too thin, making it easier to form the chemical gold plating layer on the adhesion layer. It can also avoid unnecessary waste when the adhesion layer is too thick, which is beneficial to reducing the production cost on the basis of reducing the thickness difference of the chemical gold plating layer inside and outside the through hole.

[0017] In some embodiments, the substrate may be made of a Group III or Group V compound material, such as, but not limited to, GaP, GaAs, AlAs, AlP, AlSb, InP, InSb, InAs, GaInAs, GaInP, GaAlP, and GaAlAs. The conductive structure may be made of a conductive material, such as, but not limited to, conductive metals, conductive metal oxides, conductive metal alloys, and conductive organic materials.

[0018] In a second aspect, an embodiment of the present application provides a method for manufacturing a chip, which may include: forming a conductive structure on a substrate, the substrate having a first surface and a second surface relatively arranged, and a through hole passing through the first surface and the second surface, the conductive structure being located on the first surface and covering the through hole; forming an adhesion layer on the second surface, the sidewall of the through hole and the surface of the conductive structure exposed by the through hole, the adhesion layer including nickel element; forming a chemical gold plating layer on the adhesion layer; and forming an electroplated gold layer on the chemical gold plating layer.

[0019] Thus, when a chemical gold plating method is used to make a chemical gold-plated layer (also referred to as a seed layer) on a nickel-containing adhesion layer, since chemical plating is not affected by an electric field or a magnetic field, there is no problem of the incident angle of the particles, and thus gold will not be affected by the incident angle and can more easily enter the through-hole. The gold is deposited on the surface of the adhesion layer by the substitution reaction of nickel and gold, and the gold entering the through-hole can increase the thickness of the seed layer in the through-hole, reduce the thickness difference of the seed layer inside and outside the through-hole, and thus reduce the thickness difference of the electroplated gold layer inside and outside the through-hole, thereby reducing the thickness difference of the conductive plating layer inside and outside the through-hole, avoiding the occurrence of a pinching phenomenon, improving the uniformity of the conductive plating layer inside and outside the through-hole, and improving the performance of the conductive plating layer and even the chip. Moreover, since the adhesion layer is a nickel-containing film layer, a seed layer can be made on the surface of the adhesion layer, and gold will not be deposited at other locations without the adhesion layer. This solves the problem of gold waste caused by most of the gold being deposited on the inner wall of the equipment cavity in the PVD method, reduces the amount of gold used, and thus reduces the production cost of the chip.

[0020] Since the principle of solving the problem by this manufacturing method is similar to the principle of solving the problem by the aforementioned chip, the embodiments and technical effects of this manufacturing method can refer to the embodiments and technical effects of the aforementioned chip, and the repeated parts will not be repeated.

[0021] In a third aspect, embodiments of the present application provide an electronic device, which may include: a circuit board and a chip as described in the first aspect, the chip being disposed on the circuit board. Because the uniformity of the thickness of the conductive plating layer inside and outside the through-hole is improved, the performance of the conductive plating layer and, consequently, the chip, is improved, while manufacturing costs and efficiency of the conductive plating layer are reduced. Thus, electronic devices fabricated using this chip can similarly achieve the goals of improved performance, reduced costs, and improved efficiency.

[0022] Since the principle of solving the problem by the electronic device is similar to the principle of solving the problem by the aforementioned chip, the embodiments and technical effects of the electronic device can refer to the embodiments and technical effects of the aforementioned chip, and the repeated parts will be omitted. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] FIG1 is a schematic structural diagram of an electronic device provided in an embodiment of the present application;

[0024] FIG2 is a schematic diagram of the structure of a chip provided in an embodiment of the present application;

[0025] FIG3 is a schematic diagram of a chip manufacturing process provided in an embodiment of the present application;

[0026] FIG4 is a cross-sectional view of an adhesion layer and a chemical gold plating layer provided in an embodiment of the present application;

[0027] FIG5 is a cross-sectional view of an adhesion layer and a gold layer in the prior art;

[0028] FIG6 is a cross-sectional view of an electroplated gold layer formed on a chemically plated gold layer;

[0029] FIG7 is a cross-sectional view of an electroplated gold layer formed on a gold layer formed by PVD.

[0030] Reference numerals: 10 - substrate, 11 - through hole, 20 - conductive structure, 30 - conductive plating layer, 31 - adhesion layer, 32 - chemical gold plating layer, 33 - electroplated gold layer, 100 - housing, 200 - circuit board, 300 - chip, b1 - first surface, b2 - second surface, b3 - hole wall. DETAILED DESCRIPTION

[0031] In order to make the purpose, technical solutions and advantages of this application clearer, this application will be further described in detail below with reference to the accompanying drawings.

[0032] It should be noted that the same reference numerals in the drawings of this application represent the same or similar structures, and thus their repeated description will be omitted. The words expressing positions and directions described in this application are all explained using the drawings as examples, but they can be modified as needed, and such modifications are included in the scope of protection of this application. The drawings of this application are only for illustrating relative positional relationships and do not represent true proportions.

[0033] In order to facilitate understanding of the technical solutions provided in the embodiments of the present application, the application scenario is first explained.

[0034] The chips provided in the embodiments of the present application can be widely used in various electronic devices, which may include various terminal devices and electronic components. Terminal devices may include, but are not limited to, smartphones, smart TVs, smart TV set-top boxes, smart watches, personal computers (PCs), wearable devices, smart broadband devices, and the like. Electronic components may include, but are not limited to, telecommunications equipment such as wireless networks, fixed networks, and servers, as well as chip modules, memory devices, and the like, which are not listed here one by one.

[0035] FIG1 exemplarily shows a schematic diagram of the structure of a chip when it is used in an electronic device. Referring to FIG1 , the electronic device includes a housing 100 and a circuit board 200 disposed within the housing 100, with a chip 300 disposed on the circuit board 200. The chip 300 may include a substrate and a semiconductor device disposed on the substrate, such as a transistor or capacitor. The surface of the substrate on which the semiconductor device is disposed may be referred to as the front side of the substrate, and the other surface may be referred to as the back side of the substrate. A through hole is provided in the substrate, and the power supply terminal or ground terminal of the semiconductor device may cover the through hole. Furthermore, when a conductive coating is formed on the back side of the substrate, the conductive coating not only covers the back side of the substrate, but also covers the sidewalls of the through hole and the surface of the power supply terminal or ground terminal exposed by the through hole, so that the conductive coating is connected to the power supply terminal or ground terminal. This allows heat generated by the semiconductor device during operation to be conducted away from the back side of the substrate, improving the heat dissipation capability of the chip 300. It also simplifies the structural complexity of the front side of the substrate, allowing the back side space of the substrate to be used to integrate the power line or ground line required in the circuit.

[0036] Currently, when making a conductive coating on the back side of a substrate, a titanium layer or titanium-tungsten layer can be first sputtered as an adhesion layer on the back side of the substrate, the sidewalls of the through-hole, and the surface of the power supply terminal or ground terminal exposed by the through-hole using the PVD method. A layer of gold can then be sputtered as a seed layer on the surface of the adhesion layer using the PVD method. Finally, gold is plated on the surface of the seed layer using electroplating to increase the thickness of the conductive coating. Since the PVD method cannot control the incident angle of the particles, particles with large angles find it difficult to enter the through-hole, resulting in a larger thickness of the seed layer outside the through-hole and a smaller thickness of the seed layer inside the through-hole. Based on the principle that the greater the thickness, the lower the resistance, and the smaller the thickness, the greater the resistance, when gold is electroplated, the thickness of the gold inside the through-hole will be much smaller than the thickness of the gold outside the through-hole, resulting in a large difference in the thickness of the conductive coating inside and outside the hole, ultimately leading to poor performance of the conductive coating.

[0037] Based on this, the embodiments of the present application provide a chip, a manufacturing method thereof, and an electronic device, which can reduce the thickness difference of the conductive coating inside and outside the through hole, avoid the clamping phenomenon, improve the uniformity of the conductive coating inside and outside the through hole, and improve the performance of the conductive coating and even the chip.

[0038] FIG2 exemplarily shows a schematic structural diagram of a chip provided in an embodiment of the present application. Referring to FIG2 , the chip may include a substrate 10 and a conductive structure 20, wherein the substrate 10 has: a first surface b1 and a second surface b2 arranged opposite to each other, and a through hole 11 passing through the first surface b1 and the second surface b2. The number of through holes 11 may be one, two, three or more, and may be set according to actual needs and is not limited here. The conductive structure 20 may be provided on the first surface b1, and the number of conductive structures 20 may be one, two or more, and the function of each conductive structure 20 includes but is not limited to transmitting power signals, ground signals or other signals, and the functions of each conductive structure 20 may be the same, partially the same or different, and may be set according to actual needs. However, no matter how many conductive structures 20 are provided or how the functions of each conductive structure 20 are set, as long as there is a conductive structure 20 covering the through hole 11, the number of through holes 11 covered by the conductive structure 20 is not limited here.

[0039] Continuing with reference to Figure 2, the chip may further include a conductive plating 30, which may be formed on the second surface b2, the side walls of the through hole 11 and the surface of the conductive structure 20 exposed by the through hole 11, wherein the portion of the second surface b2 other than the through hole 11 may be referred to as an outer hole area, the side walls of the through hole 11 may be referred to as hole walls b3, and the surface of the conductive structure 20 exposed by the through hole 11 may be regarded as a hole bottom, so that the outer hole area, the hole walls b3 and the hole bottom are all provided with a conductive plating 30, and the conductive plating 30 is connected to the conductive structure 20, so that the heat in the conductive structure 20 can be conducted to the second surface b2 through the conductive plating 30 and dissipated through the second surface b2, and the signal transmitted by the conductive structure 20 can also be transmitted to the conductive plating 30.

[0040] The conductive coating 30 may include: an adhesion layer 31 formed in the hole outer area, the hole wall b3 and the hole bottom, a chemical gold plating layer 32 formed on the adhesion layer 31, and an electroplated gold layer 33 formed on the chemical gold plating layer 32, so that the adhesion layer 31, the chemical gold plating layer 32 and the electroplated gold layer 33 are stacked in sequence along the direction from the first surface b1 to the second surface b2 (i.e., the F1 direction in Figure 2). The preparation material of the adhesion layer 31 includes nickel element. For example, the adhesion layer 31 can be made of at least one of elemental nickel and a nickel-containing inorganic material. When selecting the nickel-containing inorganic material, at least one can be selected from, but is not limited to, nickel-vanadium alloy, nickel phosphide, nickel nitride, nickel boride, nickel-tungsten alloy, nickel-aluminum alloy, nickel-titanium alloy, nickel-thallium alloy and nickel-chromium alloy, etc., so that the material selection has a wide range to meet the needs of various application scenarios. In addition, the adhesive layer 31 may be a single-layer structure or a multi-layer structure. When the adhesive layer 31 is a multi-layer structure, the materials of each layer may be the same or different, and the specific configuration may be based on actual needs.

[0041] In this way, when a chemical gold plating method is used to make a chemical gold-plated layer (also called a seed layer) 32 on the nickel-containing adhesion layer 31, since chemical plating is not affected by electric fields or magnetic fields, there is no problem of the incident angle of the particles, and gold will not be affected by the incident angle and can easily enter the through hole 11. The gold is deposited on the surface of the adhesion layer 31 by utilizing the substitution reaction between nickel and gold, and the gold that enters the through hole 11 can increase the thickness of the seed layer in the through hole 11, reduce the thickness difference of the seed layer inside and outside the through hole 11, and then reduce the thickness difference of the electroplated gold layer 33 inside and outside the through hole 11, thereby reducing the thickness difference of the conductive plating layer 30 inside and outside the through hole 11, avoiding the clamping phenomenon, improving the uniformity of the conductive plating layer 30 inside and outside the through hole 11, and improving the performance of the conductive plating layer 30 and even the chip.

[0042] For example, the adhesion layer 31 can be formed using a PVD method, so that the produced adhesion layer 31 can be a nickel-containing film layer. This allows the substitution reaction between nickel and gold to be used, and a gold layer can be formed on the surface of the adhesion layer 31 using a chemical gold plating method to form a seed layer. Gold will not be deposited in other areas without the adhesion layer 31. This solves the problem of gold waste caused by the PVD method where most of the gold is deposited on the inner wall of the device cavity, thereby reducing gold usage and lowering chip production costs.

[0043] It should be understood that the chemical gold plating method is a method based on the principle of redox, which utilizes chemical reactions to deposit gold on the adhesion layer 31. This method does not require external current. The electroplating gold method is a method in which gold ions are discharged under the action of external current to form a gold layer.

[0044] As shown in Figure 2, for the chemical gold-plated layer 32, the ratio of the first thickness d1 located at any point in the through-hole 11 to the second thickness d2 located at any point on the second surface b2 can be greater than or equal to 0.5, indicating that the thickness difference of the seed layer inside and outside the through-hole 11 is small, which effectively reduces the resistance of the seed layer inside the through-hole 11. Therefore, when the gold-plated layer 33 is produced by the gold-plating method on the seed layer, the gold-plated layer 33 inside the through-hole 11 can be made thicker, further reducing the thickness difference inside and outside the through-hole 11 during gold-plating, further improving the thickness uniformity of the conductive plating layer 30, and at the same time reducing the time for gold plating, thereby not only saving the amount of gold used, but also improving the production efficiency of the conductive plating layer 30 and even the chip.

[0045] As shown in Figure 2, for the chemical gold-plated layer 32, the second thickness d2 located at any point on the second surface b2 can be set to be greater than or equal to 300 nm, which is conducive to ensuring that the chemical gold-plated layer 32 in the through hole 11 has a certain thickness, avoiding the thickness of the chemical gold-plated layer 32 in the through hole 11 being too thin and resulting in too large resistance, thereby helping to reduce the thickness difference of the electroplated gold layer 33 inside and outside the through hole 11, and reduce the thickness difference of the conductive plating layer 30 inside and outside the through hole 11, especially when the ratio of the first thickness d1 to the second thickness d2 is greater than or equal to 0.5, the thickness difference of the conductive plating layer 30 inside and outside the through hole 11 can be further reduced.

[0046] FIG3 exemplarily shows a flow chart of a chip manufacturing method provided in an embodiment of the present application. Referring to FIG3 , the method may include the following steps:

[0047] Step 1: As shown in FIG. 3( a ), in a substrate 10 having a first surface b1 and a second surface b2 opposite to each other, a through hole 11 is formed that penetrates the first surface b1 and the second surface b2 ;

[0048] As shown in (a) of FIG3 , the first surface b1 and the second surface b2 of the substrate 10 are arranged relative to each other along the thickness direction of the substrate 10, and the through hole 11 extends along the thickness direction of the substrate 10 and penetrates the first surface b1 and the second surface b2. The size and shape of the through hole 11 can be set according to actual needs. For example, but not limited to, the cross-sectional shape of the through hole 11 parallel to the first surface b1 can be elliptical, circular, or irregular. Taking the elliptical shape as an example, the shortest diameter can be, but not limited to, 30 μm, and the longest diameter can be, but not limited to, 60 μm. In addition, when forming the through hole 11, the through hole 11 can be etched into the substrate 10 by, but not limited to, plasma etching.

[0049] Step 2: As shown in FIG3( b ), a conductive structure 20 covering the through hole 11 is formed on the first surface b1 ;

[0050] As shown in (b) of Figure 3, the figure takes a conductive structure 20 covering a through hole 11 as an example. If the structure in Figure (b) is turned upside down, the surface of the conductive structure 20 exposed by the through hole 11 can be regarded as the bottom of the through hole 11.

[0051] Step 3: Form a conductive plating layer 30 on the second surface b2, the sidewalls of the through hole 11, and the surface of the conductive structure 20 exposed by the through hole 11; wherein the conductive plating layer 30 includes: an adhesion layer 31, a chemical gold plating layer 32, and an electroplated gold plating layer 33 stacked in sequence along a direction from the first surface b1 to the second surface b2, wherein the adhesion layer 31 includes nickel element.

[0052] The following is a detailed description of the manufacturing process of the conductive plating layer 30, which may specifically include the following steps:

[0053] Step 3.1: As shown in (c) of FIG3 , based on the PVD method, a material containing nickel is used to form an adhesion layer 31 on the second surface b2, the hole wall b3 and the hole bottom. The thickness d3 of the adhesion layer 31 can be controlled to be 0.1 μm to 0.5 μm.

[0054] Step 3.2: Cleaning the chip with the adhesion layer 31 formed thereon.

[0055] Exemplarily, a plasma with a certain power (for example, but not limited to 400W) is used, an inert gas (for example, but not limited to argon) is introduced, and the chip with the adhesion layer 31 formed thereon is cleaned for a period of time (for example, but not limited to 90s), and then the cleaned chip is kept in a vacuum for a certain period of time (for example, but not limited to 5min) to remove organic pollutants on the surface of the chip; thereafter, a sulfuric acid solution with a certain concentration (for example, but not limited to 5%) is used to clean the chip at room temperature to remove the oxide film on the surface of the chip.

[0056] Step 3.3: As shown in FIG3( d ), a chemical gold plating layer 32 is formed on the adhesion layer 31 by using a chemical gold plating method.

[0057] Among them, the specific production process of the chemical gold plating layer 32 can include the following two steps: the first step is to use a displacement gold plating solution to cause a replacement reaction between nickel and gold on the surface of the adhesion layer 31, so that the surface of the adhesion layer 31 contains gold (which can be called a displacement gold layer); the second step is to use a chemical gold plating solution to continue gold plating on the surface of the displacement gold layer to thicken the thickness of the gold layer to obtain a chemical gold plating layer 32, so that the thickness of the chemical gold plating layer 32 at any point on the second surface b2 is greater than or equal to 300nm, and the ratio of the thickness of the chemical gold plating layer 32 at one-half of the through hole 11 to the thickness of the chemical gold plating layer 32 at any point on the second surface b2 is greater than or equal to 0.5.

[0058] Exemplarily, the replacement gold plating solution generally includes multiple components. A certain volume of each component is measured and mixed together, and the volume is supplemented to the target volume (for example, but not limited to 1L) to obtain a mixed solution A. The pH of the mixed solution A is adjusted to a preset value (for example, but not limited to 7.2). After the temperature of the mixed solution A is increased to a preset temperature (for example, but not limited to 74°C), the chip treated in step 3.2 is placed in the heated mixed solution A, so that the nickel and gold on the surface of the adhesion layer 31 undergo a replacement reaction. After the reaction has lasted for a period of time (for example, but not limited to 12 minutes), the chip is taken out and cleaned to obtain a chip containing a replacement gold layer on the surface of the adhesion layer 31.

[0059] Exemplarily, the chemical gold plating solution also generally includes multiple components. A certain volume of each component is measured and mixed together, and the volume is supplemented to the target volume (for example, but not limited to 1L) to obtain a mixed solution B. The pH of the mixed solution B is adjusted to a preset value (for example, but not limited to 7.2). After the temperature of the mixed solution B is increased to a preset temperature (for example, but not limited to 50°C), the chip with the replacement gold layer is placed in the heated mixed solution B, so that the gold in the chemical gold plating solution undergoes a reduction reaction and forms a reduced gold layer on the surface of the replacement gold layer, increasing the thickness of the gold layer. After reacting for a period of time (for example, but not limited to 3 minutes), the chip is taken out and cleaned to obtain a chip with a chemical gold plating layer 32, wherein the chemical gold plating layer 32 includes a replacement gold layer and a reduced gold layer.

[0060] Of course, when manufacturing the chemical gold plating layer 32 , the method is not limited to the two-step method mentioned above. Other methods for obtaining the chemical gold plating layer 32 may also be used, which are not limited here.

[0061] Step 3.4: Cleaning the chip with the chemical gold plating layer 32 formed thereon.

[0062] For the specific cleaning process, please refer to the cleaning process described in step 3.2 above.

[0063] Step 3.5: As shown in FIG. 3( e ), an electroplated gold layer 33 is formed on the chemically plated gold layer 32 .

[0064] When forming the electroplated gold layer 33, the chip processed in step 3.4 can first be fixed on the substrate with the chemical gold plating layer 32 facing upward, and then the substrate with the chip fixed can be transferred to the electroplating machine fixture, and electroplating can be performed step by step using electroplating gold liquid. After the electroplating is completed, it can be washed and dried with deionized water to obtain the electroplated gold layer 33.

[0065] Exemplarily, the current used in each electroplating step can be different during step-by-step electroplating, and the current size used in each electroplating step can be increased in sequence according to the electroplating order. For example, taking two-step electroplating as an example, the current used in the first step of electroplating is less than the current used in the second step of electroplating. The advantage of such an arrangement is that by adopting a smaller current in the previous electroplating step, the thickness of the gold in the through hole 11 can be thickened, and the thickness difference of the gold inside and outside the through hole 11 can be reduced. By adopting a larger current in the subsequent step, the thickness of the gold can be increased to reach the designed thickness of the electroplated gold layer 33, so that the thickness difference of the electroplated gold layer 33 inside and outside the through hole 11 can be smaller, and production efficiency can also be improved. Of course, step-by-step electroplating can be, but is not limited to, two-step electroplating, and can be specifically determined according to actual conditions and is not limited here.

[0066] The following introduces the conductive coating through specific test results.

[0067] Example: Referring to Figures 4 and 5, Figure 4 is a cross-sectional view of the adhesion layer and the chemically plated gold layer provided in the embodiment of the present application at different positions and different magnifications, and Figure 5 is a cross-sectional view of the adhesion layer and the gold layer in the prior art at different positions and different magnifications, wherein the adhesion layer in the prior art is made by PVD and the material is titanium metal, and the gold layer in the prior art is made by PVD. Moreover, in Figures 4 and 5, the magnification of Figure (a) is greater than that of Figure (b), and the magnification of Figure (b) is greater than that of Figure (c). By comparing the structures shown in Figures 4 and 5, it is found that:

[0068] 1. The second thickness d2 of the electroless gold-plated layer provided in the embodiment of the present application on the second surface is approximately 592 nm to 620 nm, as shown in FIG4(b). The first thickness d1 of the electroless gold-plated layer corresponding to half the depth of the through-hole is approximately 324 nm to 374 nm, as shown in FIG4(c). The ratio of the first thickness d1 to the second thickness d2 is greater than 0.5. Therefore, the electroless gold-plated layer provided in the embodiment of the present application has a relatively large thickness and a smooth surface (as shown in FIG4(a)).

[0069] 2. In the prior art, the second thickness d2 of the gold layer on the second surface is approximately 128 nm to 256 nm, as shown in FIG5(b). The first thickness d1 of the gold layer, corresponding to half the depth of the through-hole, is approximately 31 nm to 40 nm. As shown in FIG5(c), the ratio of the first thickness d1 to the second thickness d2 is less than 0.3. Therefore, the prior art gold layer is relatively thin, island-shaped, and has an uneven surface (as shown in FIG5(a)).

[0070] After analyzing the reasons, it was found that compared with the gold layer produced by the PVD method, the gold layer deposited by the chemical gold plating method has greater internal stress. Increasing the thickness of the gold layer may cause the gold layer to warp and the adhesion layer to separate, and even cause the wafer to tear. Therefore, the resulting gold layer is island-shaped and has an uneven surface. In addition, most of the gold in the PVD method is deposited on the inner wall of the device cavity, which limits the gold deposited on the adhesion layer, resulting in a thinner gold layer. The gold layer produced by the chemical gold plating method (i.e., the chemical gold plating layer) can avoid the above problems, so that the produced chemical gold plating layer has a flat surface and a larger thickness.

[0071] Example: As shown in Figures 6 and 7, Figure 6 is a cross-sectional view of an electroplated gold layer produced on a chemically plated gold layer at different positions and different magnifications, and Figure 7 is a cross-sectional view of an electroplated gold layer produced on a gold layer produced by a PVD method at different positions and different magnifications. Among them, in Figures 6 and 7, the magnification of Figure (a) is greater than the magnification of Figure (b), and the magnification of Figure (b) is greater than the magnification of Figure (c). By comparing the structures shown in Figures 6 and 7, it is found that:

[0072] 1. The electroplated gold layer made on the gold layer made by the PVD method has a thicker thickness outside the hole and a thinner thickness at the bottom of the hole, resulting in a pinching phenomenon, as shown in the solid coil in (a) of Figure 7. This is because when the PVD method is used to make the gold layer, due to the incident angle of the particles, it is difficult for the gold to be effectively sputtered into the through-hole, resulting in a thinner thickness and a larger resistance of the gold layer in the through-hole. Therefore, during the electroplating process, the current in the through-hole is small, and the thickness of the electroplated gold layer is thin, especially at the bottom of the hole. Since the thickness difference of the chemically plated gold layer inside and outside the through-hole is small, the resistance of the chemically plated gold layer in the through-hole is small, resulting in a larger current in the through-hole during the electroplating process, which increases the thickness of the electroplated gold layer in the through-hole and avoids the pinching phenomenon, as shown in the solid coil in (a) of Figure 6.

[0073] 2. For the electroplated gold layer formed on top of the gold layer produced by the PVD method: the thickness d4 of the electroplated gold layer in the area outside the hole is approximately 8.51μm, as shown in Figure 7(b), and the thickness d5 of the electroplated gold layer at the bottom of the hole is approximately 3.90μm. As shown in Figure 7(c), the ratio of thickness d5 to thickness d4 is 45.9%. For the electroplated gold layer formed on top of the chemically plated gold layer: the thickness d4 of the electroplated gold layer in the area outside the hole is approximately 7.63μm, as shown in Figure 6(b), and the thickness d5 of the electroplated gold layer at the bottom of the hole is approximately 4.64μm. As shown in Figure 6(c), the ratio of thickness d4 to thickness d5 is 60.8%. This shows that the electroplated gold layer formed on top of the chemically plated gold layer has a smaller thickness difference between the inside and outside of the through-hole, and the thickness of the electroplated gold layer inside the through-hole is greater. If the thickness of the electroplated gold layer at the bottom of the hole is required to be 4μm, according to the above ratio, when the electroplated gold layer is made on the gold layer made by the PVD method, the electroplated gold layer in the area outside the hole needs to be plated to 8.87μm, while when the electroplated gold layer is made on the chemical gold layer, the electroplated gold layer in the area outside the hole only needs to be plated to 6.58μm. In comparison, making the electroplated gold layer on the chemical gold layer can save 30% of the electroplated gold, which can effectively save the amount of gold used and reduce the production cost. From another perspective, when the electroplated gold layer is made on the chemical gold layer, it has better filling ability for the through hole.

[0074] It should be understood that during gold electroplating, the gold in the through-hole is consumed quickly and cannot be replenished in time, so the thickness of the electroplated gold layer inside and outside the through-hole cannot be equal under the two processes.

[0075] Obviously, those skilled in the art may make various changes and modifications to the embodiments of the present application without departing from the spirit and scope of the embodiments of the present application. Thus, if these modifications and variations of the embodiments of the present application fall within the scope of the claims of the present application and their equivalents, the present application also intends to include such modifications and variations.

Claims

1. A chip, characterized in that: include: A substrate having a first surface and a second surface arranged opposite to each other, and a through hole penetrating the first surface and the second surface; a conductive structure, the conductive structure being located on the first surface and covering the through hole; A conductive plating layer, wherein the conductive plating layer is formed on the second surface, the sidewall of the through hole and the surface of the conductive structure exposed by the through hole; wherein the conductive plating layer comprises: an adhesion layer, a chemical gold plating layer and an electroplated gold plating layer, which are sequentially stacked in a direction from the first surface to the second surface, and the adhesion layer comprises nickel element.

2. The chip according to claim 1, characterized in that: The chemical gold-plated layer at any location in the through hole has a first thickness, and the chemical gold-plated layer at any location on the second surface has a second thickness, and a ratio of the first thickness to the second thickness is greater than or equal to 0.

5.

3. The chip according to claim 2, characterized in that: Any location within the through hole includes a location at one-half the depth of the through hole.

4. The chip according to any one of claims 1 to 3, characterized in that: The thickness of the chemically plated gold layer located at any location of the second surface is greater than or equal to 300 nm.

5. The chip according to any one of claims 1 to 4, characterized in that: The atomic content of the nickel element included in the adhesion layer is greater than or equal to 80%.

6. The chip according to any one of claims 1 to 5, characterized in that: The adhesion layer includes at least one of elemental nickel and a nickel-containing inorganic substance.

7. The chip according to any one of claims 1 to 6, characterized in that: The thickness of the adhesive layer is 0.1 μm to 0.5 μm.

8. A method for manufacturing a chip, characterized in that: include: Forming a conductive structure on a substrate, wherein the substrate has a first surface and a second surface that are opposite to each other, and a through hole that penetrates the first surface and the second surface, and the conductive structure is located on the first surface and covers the through hole; forming an adhesion layer on the second surface, the sidewall of the through hole and the surface of the conductive structure exposed by the through hole, wherein the adhesion layer includes nickel element; forming a chemical gold plating layer on the adhesion layer; An electroplated gold layer is formed on the chemically plated gold layer.

9. The method of claim 8, wherein: Forming an adhesion layer, comprising: The adhesion layer is formed by a physical vapor deposition method.

10. The production method according to claim 8 or 9, characterized in that: The chemical gold-plated layer formed at any location in the through hole has a first thickness, the chemical gold-plated layer formed at any location on the second surface has a second thickness, and a ratio of the first thickness to the second thickness is greater than or equal to 0.

5.

11. The production method according to any one of claims 8 to 10, characterized in that: The thickness of the chemical gold plating layer formed at any location of the second surface is greater than or equal to 300 nm.

12. An electronic device, characterized in that: include: A circuit board and a chip as claimed in any one of claims 1 to 7, wherein the chip is arranged on the circuit board.

Citation Information

Patent Citations

  • Via-hole and its formation

    JP1995193214A

  • Semiconductor device and method of manufacturing same

    JP2007157883A

  • Semiconductor device, stacked package semiconductor device and semiconductor device manufacturing method

    JP2012146784A