The monitor circuit addresses inefficiencies in measuring doping position errors by electrically detecting resistance changes in silicon photonics devices, allowing for faster and more accurate evaluation of optical modulators without requiring optical measurements.

WO2024247010A1PCT designated stage expired Publication Date: 2024-12-05NT T INC
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/019798
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-26
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

Current methods for measuring doping position errors in silicon photonics optical devices are inefficient due to long measurement times and difficulty in confirming positional deviations between doped regions and waveguide regions, particularly in optical modulators, as they require optical characteristics measurement.

Method used

A monitor circuit that electrically measures doping position shifts by varying the resistance value based on the overlapping area between doped regions and waveguide layers, allowing for detection without optical characteristics measurement, with elements designed to have non-overlapping or partially overlapping structures to detect positional deviations.

Benefits of technology

Enables rapid detection of doping position shifts and improves the accuracy of optical modulator evaluation by measuring electrical characteristics, reducing the need for time-consuming optical alignment and measurement processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023019798_05122024_PF_FP_ABST
    Figure JP2023019798_05122024_PF_FP_ABST
Patent Text Reader

Abstract

An embodiment of the present disclosure provides a monitor circuit for electrically measuring a doping position deviation when doping an optical waveguide. A monitor circuit (100) comprises a plurality of elements (110, 120, 130), each element being provided with a doping region (103), a waveguide layer (105), and an electrode port (107). The relative positions between the doping regions and waveguide layers of the plurality of elements are different from one another. In at least one of the plurality of elements, the doping region and the waveguide layer do not overlap, but one long side of the doping region and one long side of the waveguide layer are formed at a same position (P) in the design.
Need to check novelty before this filing date? Find Prior Art

Description

Monitor Circuit

[0001] The present disclosure relates generally to monitor circuits, and more particularly to monitor circuits for measuring doping placement errors in the fabrication of silicon photonics optical devices.

[0002] With the rapid increase in demand for communications, vigorous research is being conducted to increase the capacity of communications networks. Regarding optical modules, there is a strong demand for broader bandwidth and higher efficiency, with the aim of improving the bit rate per unit volume of communications equipment and reducing power consumption. The bandwidth and modulation efficiency of the optical modulator in an optical module are highly sensitive to the doping position during wafer manufacturing, and are strongly affected by wafer manufacturing errors, resulting in variations. Therefore, monitoring and accurately understanding the doping position is effective for optical modulator inspection and is also effective for improving the accuracy of optical modulator evaluation.

[0003] SS Azadeh et al., “Low Vπ Silicon photonics modulators with highly linear epitaxially grown phase shifters”, Optics Express, 23, 23526-23550, 2015

[0004] A measurement method using optical response is used to monitor and accurately grasp the doping position formed in an optical modulator. However, measurement using optical response requires optical input and optical alignment time, which makes it long to measure, and it is difficult to confirm the direction of misalignment between the doping region and the waveguide region.

[0005] The present disclosure has been made in view of such problems, and an object of the present disclosure is to provide a monitor circuit that does not require measurement of optical characteristics.

[0006] To achieve this object, one embodiment of the present disclosure is a monitor circuit for electrically measuring a doping position deviation when doping an optical waveguide, the monitor circuit comprising a plurality of elements, each element including a doping region, a waveguide layer, and an electrode port, the relative positions of the doping region and the waveguide layer of the plurality of elements being different from one another, and at least one of the plurality of elements having a doping region and a waveguide layer that do not overlap, but one long side of the doping region and one long side of the waveguide layer formed in the same position by design.

[0007] The monitor circuit may be mounted on the same die as the optical waveguide or on an adjacent die, and at least one monitor circuit may be mounted within a shot area.

[0008] This makes it possible to detect doping misalignment only by measuring electrical characteristics, without needing to measure optical characteristics. Further features and advantages of the present disclosure will become apparent from the following detailed description, taken in conjunction with the accompanying drawings.

[0009] 1A and 1B are diagrams showing a monitor circuit according to an embodiment of the present invention, where (a) is a top view of the monitor circuit and (b) is a cross-sectional view of the monitor circuit. (a) is a graph showing the resistance value versus the relative position of the monitor circuit designed according to an embodiment of the present invention, and (b) is a graph showing the state of the monitor circuit when misalignment occurs and the change in resistance value versus the relative position at that time. (b) is a diagram showing the relative positions of the monitor circuit and optical modulator according to an embodiment of the present invention formed on a wafer, showing that the monitor circuit is mounted on the same die as the optical modulator. (c) is a diagram showing the relative positions of the monitor circuit and optical modulator according to an embodiment of the present invention formed on a wafer, showing that the monitor circuit is mounted on a die adjacent to the die on which the optical modulator is mounted. (d) is a diagram showing the relative positions of the monitor circuit and optical modulator according to an embodiment of the present invention formed on a wafer, showing that at least one monitor circuit is mounted in each shot area. (e) is a diagram showing a monitor circuit structure according to an embodiment of the present invention, including multiple sets of elements each having a waveguide layer and a doping region, with the same level of misalignment. (f) is a diagram showing that the monitor circuit and optical modulator according to an embodiment of the present invention are formed in the same direction.

[0010] Hereinafter, with reference to the drawings, an embodiment of a monitor circuit for measuring doping position errors in the manufacture of an optical device using silicon photonics will be described. Hereinafter, an optical device will be exemplified as an optical modulator, but the monitor circuit of the present disclosure can also be implemented in optical devices other than optical modulators, i.e., in any optical device in which doping is performed on an optical waveguide. Note that the drawings are schematic and are intended to conceptually explain functions or structures. Furthermore, the present invention is not limited to the embodiments shown below. In the drawings, the same reference numerals are used to designate the same or similar components whenever possible.

[0011] Before describing embodiments of the monitor circuit in this disclosure, we will first describe optical modulators. Optical modulators are key components for various integrated photonic functions, such as optical interconnects, on-chip clock and data distribution, and optical signal processing. Among the various technologies proposed for developing optical modulators, silicon photonics is one of the most promising because it can be mass-produced at competitive costs and enables the development of complex optical functions monolithically integrated with high-end electronics from a single silicon chip.

[0012] Silicon-based modulators are widely used for optical modulators. As is well known in the art, silicon optical modulators can be based on the use of PN junctions in ridge waveguides, for example (see Non-Patent Document 1). Such waveguides can be formed by providing a silicon waveguide core region surrounded by a slab or having a slab on one side.

[0013] The waveguide core region may be formed by a PN junction, typically formed along the direction of light propagation, or laterally of the waveguide perpendicular to the direction of light propagation, or in both directions, by doping one side of the waveguide with an N-type dopant and the other side with a P-type dopant.

[0014] The doping concentration of silicon in the waveguide core region must be weak to avoid excessive optical loss, typically less than 1×10 17 ~1×10 18 cm -3To allow good ohmic contact between the electrodes, the doping concentration near the electrodes must be high, typically in the range of 1×10 20 ~1×10 21 cm -3 In the art, there may also be one or more transition regions connecting the lightly doped and heavily doped regions on either side of this PN junction to achieve a compromise between optical loss and contact resistance.

[0015] In such a silicon optical modulator, when an external control voltage is applied to the electrodes to change the carrier density in the waveguide, the refractive index of the silicon wire waveguide changes due to the carrier plasma dispersion effect, and the phase of the light passing through it can be shifted.

[0016] Ion implantation is a commonly used method for forming PN junction structures, i.e., doped regions, in waveguide core regions. The bandwidth and modulation efficiency of optical modulators in optical modules are highly sensitive to the doping position during wafer manufacturing. However, manufacturing errors, such as wafer deformation or misalignment, during the manufacturing process can have a significant impact, resulting in variations between wafers or locations within a wafer. Therefore, monitoring and accurately determining the doping position is effective for optical modulator inspection and also contributes to improving the accuracy of optical modulator evaluation.

[0017] As described above, a method using optical response is used to measure doping misalignment due to wafer manufacturing errors in silicon photonics circuits. However, optical response measurement requires optical input and optical alignment time, which makes it difficult to confirm the direction of misalignment between the doping region and the waveguide region. Therefore, the present disclosure provides a monitor circuit that can detect doping misalignment for optical waveguides by measuring only electrical characteristics, without the need to measure optical characteristics.

[0018] (Embodiment 1) The principle of measuring the misalignment of the doped region in the monitor circuit of the present disclosure is to electrically measure the change in resistance due to the change in the area of ​​the overlapping portion between the doped region and the waveguide layer. In a structure in which the doped region and the waveguide layer do not overlap, a relatively large resistance is exhibited, whereas in a structure in which the overlapping portion increases, a smaller resistance is exhibited.

[0019] 1A and 1B are diagrams showing a monitor circuit according to one embodiment, with (a) being a top view of the monitor circuit and (b) being a cross-sectional view of the monitor circuit. The monitor circuit 100 includes two or more sets of elements (e.g., 110, 120, or 130 in FIG. 1A ) each including a doped region 103, a waveguide layer 105, and electrode ports 107 bonded to both ends of the waveguide layer 105. The relative positions of the doped region 103 and the waveguide layer 105 in different sets of elements are different. For example, in the case of the first set of elements 110, the doped region 103 and the waveguide layer 105 are formed at separate locations and do not overlap. In the second set of elements 120, the doping regions 103 and the waveguide layer 105 do not overlap, but are formed close to each other so that one long side of the doping regions 103 and one long side of the waveguide layer 105 are at the same position (P). On the other hand, in the third set of elements 130, the doping regions 103 and the waveguide layer 105 are formed to overlap in whole or in part.

[0020] (Regarding the doped region) As shown in FIG. 1, one doped region 103 is formed for each pair of elements constituting the monitor circuit 100, and the relative position of the doped region 103 differs in each pair of elements. The length (x direction) of the doped region 103 may be the same as or shorter than the waveguide layer 105 described below. The width (y direction) of the doped region 103 is preferably the same as the waveguide layer 105, but may be wider or narrower. The thickness (z direction) of the doped region 103 is set to the same level as the thickness of the doped region of the optical modulator produced during the manufacturing process, but is not limited thereto.

[0021] In manufacturing or use, only the portion of the doped region 103 that overlaps with the waveguide layer 105 is formed in the waveguide layer 105, and contributes to the operation of the monitor circuit 100. On the other hand, the portion that does not overlap with the waveguide layer 105 is doped in the buried oxide film 101 and does not affect the resistance value.

[0022] The doped region 103 is formed by a conventional doping technique such as implantation, and may be p-type doped with an impurity such as boron (B), or n-type doped with an impurity such as phosphorus (P).

[0023] (Regarding the Waveguide Layer) The waveguide layer 105 is formed in a rectangular shape extending in the x-direction on the buried oxide film 101. On both ends of the waveguide layer 105, ohmic contact regions 109 are provided, which are doped at a concentration higher than the doping concentration of the doping region 103, in order to obtain good ohmic contact with the electrode port 107, and are directly bonded to the electrode port 107.

[0024] In one non-limiting embodiment, the length (x-direction) of the waveguide layer 105 is 10 μm and the thickness (z-direction) of the waveguide layer 105 is 220 nm.

[0025] A crystalline semiconductor can be used for the waveguide layer 105. Examples of crystalline semiconductors that can be used for the waveguide layer 105 include silicon (Si), germanium (Ge), silicon germanium (SiGe), indium phosphide (InP), gallium arsenide (GaAs), and mixed crystals of these.

[0026] (Regarding the Electrode Ports) The electrode ports 107 are formed on both ends of the waveguide layer 105 to measure a change in resistance value due to a change in the area of ​​the overlapping portion between the doping region 103 and the waveguide layer 105. A conductive metal material is generally used for the electrode ports 107. According to an exemplary embodiment, the electrode ports 107 may be made of Fe, Co, Ni, Cu, Zn, Ag, Pt, Au, Al, In, Ti, Mn, Ge, Pb, or C.

[0027] (Ohmic Contact Regions) The ohmic contact regions 109 are doped at a higher concentration than the doping concentration of the doped regions 103 in order to obtain good ohmic contact between the waveguide layer 105 and the electrode port 107, and are provided on both ends of the waveguide layer 105. The ohmic contact regions 109 may be formed to have the same area as the electrode port 107, or may be formed to have a larger area.

[0028] (Method of Measuring Positional Misalignment Using a Monitor Circuit) As one embodiment, as shown in FIG. 2( a), the monitor circuit 100 is designed to have a structure in which the doping region 103 and the waveguide layer 105 do not overlap, a structure in which the doping region 103 and the waveguide layer 105 do not overlap but are formed close to each other so that one long side of the doping region 103 and one long side of the waveguide layer 105 are at the same position (P), and a structure in which the doping region 103 and the waveguide layer 105 overlap in whole or in part.

[0029] At this time, a pair of elements 110 in which the doping region 103 and the waveguide layer 105 do not overlap, and a pair of elements 120 formed close together so that one long side of the doping region 103 and one long side of the waveguide layer 105 are at the same position (P) but do not yet overlap, are detected as having high resistance values. On the other hand, a pair of elements 130 in which the doping region 103 and the waveguide layer 105 partially overlap, have a resistance value that decreases in proportion to the overlapping area. That is, as shown in the graph in Figure 2(a), the doping region 103 and the waveguide layer 105 are gradually brought closer together from a positional relationship in which they are separated, and the resistance value curve begins to bend and decrease at the point (P) when they come into contact.

[0030] If there is no misalignment of the doped region 103 during manufacturing, as shown in the graph of FIG. 2B, the resistance value begins to change at the same timing (P) as the designed resistance value curve. On the other hand, if there is a misalignment of the doped region 103 during manufacturing, the resistance value begins to change at a different timing (P') from the designed resistance value curve. Therefore, it is possible to detect the misalignment of the doped region 103 from the difference in the bending timing between the designed resistance value curve and the resistance value curve after manufacturing. Therefore, the monitor circuit 100 of the present disclosure can electrically detect the amount and direction of misalignment of the doped region in the optical modulator 303.

[0031] (Embodiment 2) This embodiment provides a monitor circuit 100 that is mounted on the same first die 301 as the optical modulator 303. Misalignment of the doping region 103 generally tends to be small in the center of the wafer 300 surface and large in the outer periphery. Therefore, if it is desired to monitor the effect of misalignment of the doping region 103 on the optical modulator 303 mounted on a certain die, it is desirable that the monitor circuit 100 be positioned close to the optical modulator 303. Furthermore, the closer the monitor circuit 100 is, the higher the monitoring accuracy will be.

[0032] 3 illustrates an exemplary embodiment of a monitor circuit 100 according to the present disclosure. The monitor circuit 100 includes two or more sets of elements as shown in the first embodiment, and each set of elements is formed so that the relative positional relationship between the respective doping regions 103 and the waveguide layers 105 is different.

[0033] The monitor circuit 100 is mounted on the same first die 301 as the optical modulator 303. In Fig. 3, the monitor circuit 100 is illustrated below (on the y-axis) the optical modulator 303, but the monitor circuit 100 is not necessarily limited to being below, and the purpose can be achieved by having the monitor circuit 100 located near the optical modulator 303 on the same die.

[0034] (Embodiment 3) Another embodiment provides a monitor circuit 100 that is mounted on a second die 302 adjacent to a first die 301 on which an optical modulator 303 is mounted. As shown in FIG. 4 , the monitor circuit 100 can still achieve the purpose of detecting misalignment of the doping region 103 even if it is formed on the second die 302 adjacent to the first die 301 on which the optical modulator 303 is mounted. Although the monitor circuit 100 is illustrated on the second die 302 above (in the y-axis) the first die 301 on which the optical modulator 303 is formed, the monitor circuit 100 is not necessarily limited to the upper second die 302, and the purpose can be achieved as long as it is on a die near the first die 301 on which the optical modulator 303 is formed. Separating the first die 301 on which the optical modulator 303 is mounted from the second die 302 on which the monitor circuit 100 is mounted has the effect of making the first die 301 smaller.

[0035] (Embodiment 4) Another embodiment provides a monitor circuit 100 that is mounted at several predetermined locations on an entire wafer 300. As shown in Figure 5, in the process of manufacturing the optical modulators 303, an exposure device is used to transfer a photomask pattern to multiple shot areas of photoresist applied to a substrate. Multiple optical modulators 303 are formed in each shot area to improve the manufacturing throughput of semiconductor devices. The shot areas are arranged in a matrix on the semiconductor substrate, taking into consideration the dimensions of the effective exposure area of ​​the semiconductor substrate and the dimensions of the shot areas, etc.

[0036] Generally, the amount of misalignment of the doping regions 103 often occurs the same within one shot area. Therefore, even if one monitor circuit 100 is mounted in one shot area (e.g., 510 in FIG. 5 ), it is possible to collectively detect misalignment of the doping regions 103 in multiple optical modulators formed within the same shot. Therefore, by reducing the number of dies on which the monitor circuits 100 are mounted, more dies can be secured for manufacturing the optical modulators 303.

[0037] The position of the die on which the monitor circuit 100 is mounted within one shot area is not limited, and the monitor circuit 100 may be mounted on any die within one shot area 510. For example, as shown in FIG. 5 , the monitor circuit 100 may be mounted in the center of one shot area 510 or at each corner.

[0038] Fifth Embodiment This embodiment provides a monitor circuit 100 characterized by connecting multiple pairs of elements having the same misalignment level in parallel to improve the measurement accuracy of resistance changes. As described above, the monitor circuit 100 of the present disclosure electrically measures the change in resistance due to the change in the area of ​​the overlap between the doping region and the waveguide layer. In this structure, the measurement accuracy of resistance changes can be improved by increasing the number of doping regions 103 and waveguide layers 105 in each pair of elements and averaging them.

[0039] (Components of the Monitor Circuit) The configuration of the monitor circuit 100 for this purpose is shown in FIG. 6. The monitor circuit 100 has multiple doping regions (e.g., a first doping region 103A and a second doping region 103B), multiple waveguide layers (e.g., a first waveguide layer 105A and a second waveguide layer 105B), and electrode ports 107 bonded to both ends of the waveguide layer 105. The relative positions of the doping regions 103 and the waveguide layers 105 in different sets of elements are different. For example, in the first set of elements 110, the doping regions 103 and the waveguide layers 105 are formed at separate locations and do not overlap. In the second set of elements 120, the doping regions 103 and the waveguide layers 105 do not overlap, but are formed close to each other so that one long side of the doping region 103 and one long side of the waveguide layer 105 are at the same position (P). On the other hand, in the case of the third set of elements 130, the doping region 103 and the waveguide layer 105 are formed to overlap in whole or in part.

[0040] (Regarding Doping Regions) As shown in FIG. 6, two or more doping regions (e.g., a first doping region 103A and a second doping region 103B) are provided in each set of elements, and are formed by a conventional doping technique such as an implantation method. They may be p-type doped with impurities such as boron (B), or n-type doped with impurities such as phosphorus (P).

[0041] As described above, the relative positions of the doped regions in different sets of elements are different, but the doped regions in the same set of elements have the same misalignment level. The length (x direction) of the doped regions 103A and 103B may be the same as or shorter than the waveguide layers 105A and 105B described below. The width (y direction) of the doped regions 103A and 103B is preferably the same as the waveguide layers 105A and 105B, but may be wider or narrower. The thickness (z direction) of the doped regions 103A and 103B is, but is not limited to, the same level as the thickness of the doped regions of the optical modulator fabricated during the manufacturing process.

[0042] For manufacturing or use, only the portions of the doped regions 103A and 103B that overlap with the waveguide layers 105A and 105B are formed in the waveguide layer 105, and contribute to the operation of the monitor circuit 100. On the other hand, the portions that do not overlap with the waveguide layer 105 are doped in the buried oxide film 101 and do not affect the resistance value.

[0043] (Regarding Waveguide Layers) Similar to the doped regions, two or more waveguide layers (e.g., a first waveguide layer 105A and a second waveguide layer 105B) are provided in each set of elements and are formed on the buried oxide film 101. The two or more waveguide layers 105A and 105B are bonded in parallel, and highly doped ohmic contact regions 109 are provided on both ends of the waveguide layers, which are directly bonded to electrode ports 107 for resistance measurement.

[0044] The waveguide layer 105A may be made of a crystalline semiconductor, such as silicon (Si), germanium (Ge), silicon germanium (SiGe), indium phosphide (InP), gallium arsenide (GaAs), or a mixed crystal thereof.

[0045] In one embodiment, the length of the waveguide layer 105A is 10 μm and the thickness of the waveguide layer 105A is 220 nm, but this is not limiting.

[0046] (Regarding the Electrode Port) The electrode port 107 is formed to measure the change in resistance due to the change in the area of ​​the overlap between the doped regions 103A and 103B and the waveguide layers 105A and 105B. It is directly bonded to the ohmic contact regions 109 provided at both ends of the waveguide layers 105A and 105B. The material of the electrode port 107 is generally a conductive metal material. According to an exemplary embodiment, the electrode port 107 can be Fe, Co, Ni, Cu, Zn, Ag, Pt, Au, Al, In, Ti, Mn, Ge, Pb, or C.

[0047] (Ohmic Contact Regions) The ohmic contact regions 109 are doped at a higher concentration than the doping concentrations of the doped regions 103A and 103B to obtain good ohmic contact between the waveguide layers 105A and 105B and the electrode port 107, and are provided on both ends of the waveguide layers 105A and 105B. The ohmic contact regions 109 may be formed to have the same area as the electrode port 107, or may be formed to have a larger area.

[0048] (Embodiment 6) Another embodiment provides a monitor circuit 100 characterized in that the waveguide direction of the waveguide layer 105 of the monitor circuit 100 and the optical modulator 303 are the same. The bandwidth and modulation efficiency of the optical modulator 303 are sensitive to the doping position. In particular, in the case of an optical modulator 303 having an elongated shape in the x direction as shown in FIG. 7, misalignment of the doping region 103 in the y direction can significantly change the characteristics of the optical modulator 303. Therefore, the monitor circuit 100 needs to be sensitive to misalignment in the y direction.

[0049] When the monitor circuit 100 in this embodiment is formed in a rectangular shape extending in the x direction, the relative positional relationship is formed to change in a specific direction (the y direction in FIG. 7 ), and positional deviation of the doping region 103 in the y direction can be detected. That is, the y direction, which is perpendicular to the length direction (x direction) of the waveguide layer 105 of the monitor circuit 100, becomes the sensitivity axis of the monitor circuit 100. Furthermore, positional deviation of the doping in the optical modulator 303 occurs mainly in the y direction, which is perpendicular to the length direction of the waveguide of the optical modulator 303. Therefore, by aligning the length direction (x direction) of the waveguide layer 105 of the monitor circuit 100 with the length direction of the waveguide of the optical modulator (303), it becomes easier to predict the characteristics of the optical modulator from the results of the monitor circuit.

[0050] Additional Considerations The foregoing description of embodiments of the present invention has been presented for purposes of illustration and is not intended to be exhaustive or to be limited to the precise form disclosed. Those skilled in the art will recognize that many modifications and variations are possible in light of the above disclosure.

[0051] Finally, the language used herein has been selected primarily for readability and instructional purposes, and may not have been selected to delineate or limit the subject matter of the invention. Accordingly, it is intended that the scope of the invention be limited not by this detailed description, but rather by the appended claims. Accordingly, the disclosure of embodiments of the invention is intended to be illustrative, but not limiting, of the scope of the invention, which is set forth in the claims.

[0052] 100 Monitor circuit 101 Buried oxide film (BOX) 103 Doped region 103A First doped region 103B Second doped region 105 Waveguide layer 105A First waveguide layer 105B Second waveguide layer 107 Electrode port 109 Ohmic contact region 110 First set of elements 120 Second set of elements 130 Third set of elements 300 Wafer 301 First die 302 Second die 303 Optical modulator 510 Shot region

Claims

1. A monitor circuit for electrically measuring a doping position deviation when doping an optical waveguide, the monitor circuit comprising: a plurality of elements, each element including a doping region, a waveguide layer, and an electrode port; the relative positions of the doping region and the waveguide layer of the plurality of elements are different from one another; and in at least one of the plurality of elements, the doping region and the waveguide layer do not overlap, but one long side of the doping region and one long side of the waveguide layer are formed in the same position by design.

2. The monitor circuit according to claim 1, wherein said monitor circuit is mounted on the same first die as said optical waveguide.

3. The monitor circuit according to claim 1, wherein said monitor circuit is mounted on a die adjacent to said optical waveguide.

4. The monitor circuit according to claim 1, wherein at least one of said monitor circuits is provided for each shot area.

5. A monitor circuit as claimed in any one of claims 1 to 4, characterized in that each of the plurality of elements has a plurality of the doping regions and a plurality of the waveguide layers, and a plurality of patterns including the doping regions having the same misalignment level are formed electrically in parallel within the plurality of elements.

6. A monitor circuit according to any one of claims 1 to 4, wherein the length direction of said waveguide layer of said monitor circuit is the same as the length direction of said optical waveguide.

Citation Information

Patent Citations

  • Semiconductor device

    JP1992085822A

  • Semiconductor device

    JP1995183351A

  • Semiconductor device and alignment evaluation method

    JP2008198634A

  • Robust modulator circuits using lateral doping junctions

    US20140112611A1

  • Method for forming a self-aligned Mach-Zehnder interferometer

    US9696604B1