Photo-vulcanization method for preparing elastic sheet
By using photo-vulcanization, which utilizes light and natural light in a greenhouse for rubber vulcanization, the energy consumption and pollution problems caused by high-temperature vulcanization are solved, the stability of rubber sheets and product quality are improved, and an environmentally friendly and efficient vulcanization process is achieved.
Patent Information
- Application Number
- PCT/CN2025/092772
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-05-06
- Publication Date
- 2026-11-12
AI Technical Summary
Existing rubber vulcanization technology is energy-intensive and polluting. High-temperature vulcanization also leads to instability of chemical agents, affecting product quality and yield. Furthermore, rubber materials are prone to deformation when bonded to thin sheets.
The photocuring method is adopted, in which the elastic material is pre-cured and vulcanized by light irradiation. The vulcanization is carried out by sunlight and light in a greenhouse, avoiding high-temperature treatment, and the vulcanization process is controlled by combining heat-absorbing and moisture-reacting materials.
It reduces energy consumption and pollution, improves the stability of chemical agents and product yield, avoids adhesion deformation problems, and the prepared elastic sheet is soft and easy to process, meeting environmental protection requirements.
Smart Images

Figure CN2025092772_12112026_PF_FP_ABST
Abstract
Description
A photocuring method for preparing elastic sheets Technical Field
[0001] This application relates to the field of rubber technology, and particularly to a photocuring method for preparing elastic sheets. Background Technology
[0002] Rubber materials typically undergo a vulcanization process to set and mature into products. This process generally involves adding a vulcanizing agent (such as sulfur) to the rubber material and then heating it at high temperatures in a vulcanizing oven (for example, a tunnel oven, where the vulcanization temperature is approximately 150°C to 200°C) and / or pressurizing it. This causes the vulcanizing agent to undergo a cross-linking reaction with the rubber molecular chains, forming a cross-linked structure. This process achieves the desired mechanical properties and chemical stability, and improves the performance of the rubber product. Furthermore, the vulcanization reaction accelerates with increasing temperature and pressure. The vulcanization time, temperature, and pressure are adjusted according to the rubber material formulation and product requirements.
[0003] In the existing technology, the ovens used for the vulcanization process of rubber materials are not only energy-intensive (for example, a tunnel oven with a power of 2300Kw consumes about 2300Kw of energy to operate for 1 hour), but also a source of pollution (for example, a tunnel oven with a power of 2300Kw emits about 1100kg of CO2 to operate for 1 hour, as well as pollutants such as high-temperature solvent volatilization). Under the current needs and goals of environmental protection and carbon emission control, there is a lot of room for improvement.
[0004] In addition, in the existing technology, the structure of sports mats or step mats with rubber as the main material is usually made of at least two pieces of material bonded together (e.g., a sports mat is made of an elastic layer bonded to a fabric, and a step mat is made of an elastic layer bonded to a non-slip layer). The bonding method is to use adhesive or adhesive-free bonding technology (using the gas pressure generated when the foaming agent in the rubber material foams to bond the two pieces together). After the bonded two pieces are vulcanized and cured at high temperature, the elastic material often shrinks, causing the bonding deformation.
[0005] Secondly, the high-temperature vulcanization and curing process can easily cause the chemicals in rubber materials to become unstable, degrade, leach out, or even interact to produce harmful components, thus affecting product quality. Furthermore, because high-temperature vulcanization increases the instability of the chemicals in rubber materials, the proportions of these chemicals added must be precise. Even slight errors can lead to poor product quality and reduced yield. In other words, the tolerance for errors in chemical addition is very low, increasing the difficulty of manufacturing rubber products, although there are areas for improvement and progress. Summary of the Invention
[0006] To address the aforementioned technical problems, this application discloses a photocuring method for preparing elastic sheets.
[0007] To achieve the above-mentioned objective, this application provides a photocuring method for preparing elastic sheets, characterized in that the photocuring method includes at least the following steps:
[0008] Compressed sheet: compressing an elastic material into a sheet shape, wherein the elastic material contains a vulcanizing agent;
[0009] Bonding: A thin sheet is placed on one side of a sheet of elastic material and pressure is applied to bond the two together to form a semi-finished elastic sheet.
[0010] Photocuring: A light source is used to irradiate the surface of the elastic material of the semi-finished elastic sheet for a predetermined time, causing the elastic material to absorb light and heat, resulting in a polymerization reaction and promoting surface curing of the elastic material to produce the semi-finished elastic sheet.
[0011] Photocuring: After the elastic sheet semi-finished product is rolled up, it is placed under a greenhouse. The elastic sheet semi-finished product is irradiated by sunlight and / or light inside the greenhouse, so that the elastic sheet semi-finished product is vulcanized and cured into an elastic sheet.
[0012] Preferably, in the tableting step, the elastic material includes at least one of an elastomer, an elastomer mainly composed of plant-based elastic materials, and an all-plant-based elastomer.
[0013] Preferably, in the bonding step, the sheet is at least one of fabric or elastic sheet.
[0014] Preferably, the elastic material further includes a heat-absorbing material to allow the elastic material to absorb the heat generated when exposed to light, which is then used to supply the vulcanizing agent within the elastic material for reaction. This allows the semi-finished elastic sheet to vulcanize and mature at room temperature into an elastic sheet.
[0015] Preferably, the elastic material further comprises a moisture-reactive material to enable the elastic material to absorb moisture within the greenhouse. This promotes appropriate hardening of the elastic sheet semi-finished product to facilitate vulcanization and curing into an elastic sheet.
[0016] Preferably, in the photopre-curing step, the light source includes at least one of ultraviolet light, X-ray, laser light, or microwave, and the elastic material further contains a photoinitiator. When the surface of the elastic material is irradiated by light, the photoinitiator in the elastic material can absorb the light and generate a polymerization reaction, thereby promoting the surface pre-curing of the elastic material.
[0017] Preferably, the photocuring and photocuring steps further include a barrier means, wherein a tearable barrier sheet is attached to the surface of the elastic material to prevent the surfaces of the elastic material from sticking together when the semi-finished elastic sheet is rolled up.
[0018] Preferably, the barrier sheet is supplemented with a heat-conducting material to conduct the heat generated when light shines to the elastic material.
[0019] Preferably, the surface of the barrier sheet is textured. This promotes the formation of textures on the surface of the elastic sheet after vulcanization and curing.
[0020] Preferably, in the photo-sulfurization step, the greenhouse is equipped with at least one lamp that can emit light, and the power required for the lamp to operate is supplied by power generated by solar panels installed outside the greenhouse.
[0021] This application discloses a photocuring method for preparing elastic sheets, which avoids the problems of deformation when elastic materials adhere to the sheet, as well as the instability, loss, deterioration, or release of chemical agents, and even the generation of harmful components. It can improve the tolerance of error values when adding chemical agents, greatly improve the product yield, and the overall energy consumption is far lower than that of conventional ovens used to cure rubber, which can reduce production costs. Furthermore, it avoids pollution such as high-temperature solvent evaporation from ovens, making it more environmentally friendly. The resulting elastic sheets have higher softness, are easier to process, and have greater practical value. Attached Figure Description
[0022] To more clearly illustrate the photocuring method for preparing elastic sheets described in this application, the accompanying drawings required for the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.
[0023] Figure 1 is a flowchart of a preferred embodiment of this application.
[0024] Figure 2 is a flowchart of another preferred embodiment of this application. Detailed Implementation
[0025] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the scope of protection of this application.
[0026] As used herein, "an embodiment" or "an embodiment" refers to a specific feature, structure, or characteristic that may be included in at least one implementation of this application. The invention will be more readily understood by referring to the following detailed description of preferred embodiments and included examples. Unless otherwise specified, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. In case of conflict, the definitions in this specification shall prevail.
[0027] For the terms defined below, unless a different definition is given elsewhere in the claims or this specification, these definitions shall apply. All numerical values, whether or not explicitly indicated, are defined herein as being modified by the term "about". The term "about" generally refers to a range of numerical values that a person skilled in the art will consider equivalent to the stated values to produce substantially the same properties, functions, results, etc. A range of numerical values indicated by a low value and a high value is defined as including all numerical values included within the range and all subranges included within the range.
[0028] Although the numerical ranges and parameters illustrating the broad scope of the invention are approximate, the values listed in the specific examples are reported as precisely as possible. However, any numerical value inherently contains some error that is necessarily caused by the standard deviation found in their respective test measurements.
[0029] When a numerical range is disclosed herein, the range is considered continuous and includes the minimum and maximum values of the range, as well as every value between such minimum and maximum values. Further, when the range refers to an integer, it includes every integer between the minimum and maximum values of the range. Additionally, when multiple ranges are provided to describe a feature or characteristic, the ranges may be combined. In other words, unless otherwise specified, all ranges disclosed herein should be understood to include any and all subranges to which they are included. For example, a specified range from “1 to 10” should be considered to include any and all subranges between the minimum value 1 and the maximum value 10. Exemplary subranges of the range 1 to 10 include, but are not limited to, 1 to 6.1, 3.5 to 7.8, 5.5 to 10, etc.
[0030] It should be noted that the terms "first," "second," etc., in the specification, claims, and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data used can be interchanged where appropriate so that the embodiments of this application described herein can be implemented in orders other than those illustrated or described herein. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion.
[0031] The following examples illustrate a photocuring method for preparing elastic sheets provided in this application.
[0032] Example 1
[0033] Referring to Figure 1, the environmentally friendly photocuring method 100 for producing elastic sheets according to a preferred embodiment of the present invention is to produce elastic sheets using a non-high-temperature curing method.
[0034] The first step is sheet pressing 110: this involves pressing an elastic material into a sheet-like elastomer using existing equipment such as a rolling mill or flatbed press. This elastic material can include natural rubber, synthetic rubber, plastics, and / or recycled rubber or plastics, commonly used in the manufacture of elastic mats (such as floor mats, anti-slip mats, or sports mats), and is mixed with additives such as vulcanizing agents (this invention uses room temperature vulcanizing agents), accelerators, antioxidants, and phototriggers or photocurable resins. The elastic material can also be an elastomer primarily composed of plant-based elastic materials (i.e., the proportion of plant-based elastic materials used is higher than other elastic materials). Examples of plant-based elastic materials include natural rubber (which is the sap obtained from rubber trees and therefore belongs to the category of plant-based elastic materials), but this is not limited to this step. The elastic material can also be a completely plant-based elastomer, containing only natural rubber and no other elastic materials. The types of elastic materials added to the aforementioned elastic material depend on the product characteristics required for the finished elastic mat; this is prior art and will not be elaborated upon here. Vulcanizing agents and other additives are known additives used to control the vulcanization and maturation of rubber. They are also known technologies. The detailed composition of various additives and the principles of vulcanization and maturation will not be elaborated here.
[0035] The second step of this invention is lamination 120: a thin sheet is placed on one side of a sheet-like elastic material, and pressure is applied using conventional rolling mills or flat presses to bond the thin sheet and the sheet-like elastic material together to form a semi-finished elastic sheet. The thin sheet can be fabric or elastic sheet material.
[0036] The third step of this invention is photopre-curing 130: a light is used to irradiate the surface of the elastic material of the elastic sheet semi-finished product, causing the elastic material to absorb light and heat and produce a polymerization reaction, thereby promoting the surface pre-curing of the elastic material and producing the elastic sheet semi-finished product.
[0037] This causes the photoinitiator within the elastic material to absorb light and undergo a polymerization reaction, promoting proper curing and maturation of the elastic material's surface, i.e., pre-curing. The light source can be ultraviolet (UV), laser, X-ray, or microwave, but is not limited to these. This embodiment uses ultraviolet light, which is used to irradiate the surface of the elastic material of the semi-finished elastic sheet for a predetermined time (the UV light intensity is approximately 1000 mW / cm²). 2 When using common UV lamps, the irradiation time is approximately 1 to 5 minutes; this ultraviolet light has a wavelength of 365 nm and an intensity of approximately 500-1000 mW / cm². 2When using UV-LED lamp light, the irradiation time is approximately 2 to 6 minutes; the ultraviolet light has a wavelength of 200-400nm and an intensity of approximately 1000mW / cm². 2 When using mercury lamps as described above, the irradiation time is approximately 1 to 3 minutes. The polymerization reaction that occurs after the photoinitiator absorbs ultraviolet light is a known technique and will not be described in detail here. The main purpose of this invention is to utilize such techniques to properly cure and mature the surface of the elastic material.
[0038] The final step of this invention is photocuring 140: the semi-finished elastic sheet is rolled up and placed in a greenhouse, where it is continuously irradiated for several days for 24 hours by sunlight entering the greenhouse and light generated inside the greenhouse, so that the semi-finished elastic sheet matures into an elastic sheet. The method of rolling up the semi-finished elastic sheet is to place the sheet-like elastic material inside the roll, but it is not limited to this. The greenhouse is a conventional fully transparent agricultural cultivation room for growing vegetables and fruits, which allows sunlight to enter during the day. Furthermore, the outer side of the greenhouse (such as the roof or other light-receiving surface) is equipped with multiple solar panels, and the interior of the greenhouse is equipped with at least one lamp, each of which can emit ultraviolet light. The power required for its operation is supplied by the power generated by the solar panels installed outside the greenhouse, or by several batteries that store the power generated by the solar panels, so that when there is no sunlight at night, the lamps inside the greenhouse can emit ultraviolet light. Based on this, the semi-finished elastic sheet material in the greenhouse can be exposed to sunlight and the temperature inside the greenhouse during the day (room temperature 25°C, and the room temperature inside the greenhouse reaches about 60°C to 70°C in hot climates), and at night it can be exposed to ultraviolet light from various lamps. Through the continuous exposure to light and temperature inside the greenhouse day and night, the elastic material is not only continuously vulcanized at room temperature by the vulcanizing agent, but also slightly hardened by the polymerization reaction generated by the photoinitiator absorbing light. Thus, the semi-finished elastic sheet material is cured into an elastic sheet in a few days (as fast as 3 to 5 days, as slow as 2 to 3 weeks). After confirming that the elastic sheet is fully cured, the elastic sheet can be taken out of the greenhouse for subsequent processing such as cutting to make elastic sheet products with non-rigid physical properties.
[0039] The amount of vulcanizing agent used in the aforementioned elastic material depends on the required degree of vulcanization and curing of the finished elastic sheet and the vulcanization time required for the photocuring step 140. This can be varied and adjusted according to product requirements. The amount of photoinitiator used and the light irradiation time depend on the required degree of hardening and curing of the elastic material surface in the photocuring step 130 (so that the semi-finished elastic sheet can be rolled up without the surfaces of the elastic material sticking together during rolling), and the degree of hardening required for the curing of the elastic material in the photocuring step 140. This can also be varied and adjusted according to product requirements.
[0040] Furthermore, the time it takes for the semi-finished elastic sheet to mature into an elastic sheet in a greenhouse is affected by the amount of vulcanizing agent and photoinitiator used, as well as by the thickness and type of elastic material selected. These are parameters that can be adjusted according to product requirements.
[0041] Therefore, the environmentally friendly photocuring method 100 of this invention, through the steps of pressing 110, laminating 120, photocuring 130, and photocuring 140, places the semi-finished elastic sheet in a greenhouse for photocuring and curing. It can prepare an elastic sheet made of the sheet and elastic material by laminating at room temperature of 25°C to 70°C. This is different from the conventional industrial rapid manufacturing thinking of using ovens (such as tunnel ovens) for high-temperature (150°C to 200°C) vulcanization and curing of rubber products. Not only will it avoid the quality problem of elastic material shrinkage after high-temperature curing affecting the deformation of the sheet, but the chemical additives such as vulcanizing agents and photoinitiators in the elastic material have high stability. It will not have the problems of unstable chemical agents, loss, deterioration or release (for example, zinc stearate produced by the chemical reaction of zinc oxide powder and stearic acid is easy to be released from the rubber surface, and zinc oxide powder and stearic acid are used for rubber vulcanization) or even the interaction to produce new harmful components during the high-temperature curing of traditional rubber products.
[0042] Secondly, conventional ovens for curing rubber products are not only energy-intensive but also sources of pollution (solvent evaporation, CO2 emissions, etc.). In this invention, energy consumption and CO2 emissions only occur in the light pre-curing step 130 (where light irradiates the surface of the elastic material of the semi-finished elastic pad). The light vulcanization step 140 involves placing the semi-finished elastic pad in a greenhouse for light vulcanization and curing, thus eliminating energy consumption and CO2 emissions. Overall, the energy consumption is far lower than that of an oven (for example, a 2300kW tunnel oven consumes approximately 2300kW of energy per hour of operation, while a 0kW oven consumes significantly less). The energy consumption of a 0.5kW, 1 square meter UV lamp irradiating ultraviolet light for one hour is only about 0.5kW, a significant difference. CO2 emissions are also much lower than those of an oven (for example, a tunnel oven with a power of 2300kW emits about 1100kg of CO2 in one hour of operation, while a 0.5kW, 1 square meter UV lamp irradiating ultraviolet light for one hour emits only about 0.25kg of CO2, a significant difference). This can reduce production costs. Furthermore, this invention does not produce the pollution caused by the high-temperature solvent evaporation of an oven, which is in line with the requirements of environmental protection and carbon emission control.
[0043] Furthermore, the elastic sheet produced by this invention is cured in a greenhouse, resulting in a room-temperature vulcanization crosslinking structure that differs from the crosslinking structure achieved through high-temperature oven curing. This results in higher softness, making it easier to process and suitable for manufacturing leather and other products. Moreover, the chemical agents in this elastic material do not react excessively during non-high-temperature processes, exhibiting greater stability and improved tolerance for errors in chemical addition (even if the amount of added chemical agents slightly exceeds the predetermined value, it will not affect the quality and expected properties of the elastic sheet), significantly increasing the product yield of the elastic sheet. On the other hand, the greenhouse curing method of this invention prevents the composition of the elastic sheet from being damaged by high temperatures, thus facilitating recycling and reuse.
[0044] Since the photocuring step 140 of this invention is to cure the elastic sheet in a greenhouse, in order to increase the curing and curing speed of the elastic sheet, a heat-absorbing material can be added to the elastic material, such as a soot-based heat-absorbing material (e.g., graphite, iron black, iron blue, iron red, chrome green, carbon black, bituminous coal), etc., but not limited thereto, so that the elastic material can better absorb the heat generated by sunlight and light irradiation in the greenhouse, and supply the elastic material to carry out the curing reaction, so that the semi-finished elastic sheet can be cured at room temperature into an elastic sheet.
[0045] Alternatively, a moisture-reactive material, such as moisture-reactive single-component polyurethane (PU), may be added to the elastic material to enable it to absorb moisture in the greenhouse, promote proper hardening of the elastic sheet semi-finished product to facilitate vulcanization and curing into an elastic sheet, and also increase the curing speed of the elastic sheet.
[0046] Example 2
[0047] Referring to Figure 2, another preferred embodiment of the present invention illustrates an environmentally friendly photocuring method 200 for an elastic sheet. The steps are generally the same as those of the environmentally friendly photocuring method 100, except that a barrier means 210 is included between the photocuring pre-curing 130 and photocuring 140 steps. This involves attaching a peelable barrier sheet (not shown) to the surface of the elastic material. This barrier sheet can be a conventional release film, but is not limited to it. Therefore, the barrier sheet prevents the surface of the elastic material from sticking together when the semi-finished elastic sheet is rolled up, thereby reducing the energy consumption of the photocuring pre-curing 130 step in curing and maturing the surface of the elastic material (the energy of the light can be reduced, and the irradiation time can be shortened). Furthermore, the surface of the barrier sheet may be textured, so that the surface of the elastic sheet forms texture after curing. In addition, a heat-conducting material can be added to the barrier sheet so that when the semi-finished elastic sheet is rolled up and placed in a greenhouse, the heat-conducting material in the barrier sheet can conduct the heat generated by sunlight and light in the greenhouse to the elastic material, promoting the vulcanization and curing of the elastic material.
[0048] In summary, the environmentally friendly photocuring method for elastic sheets provided by this invention, consisting of a series of steps including sheeting, lamination, photocuring pre-curing, and photocuring, not only avoids the quality issues caused by shrinkage of the elastic material after high-temperature curing, which affects the deformation during lamination with the sheet, but also avoids the problems of unstable, wasted, deteriorated, or released chemicals, or even the generation of harmful components, that occur during the high-temperature curing of conventional rubber products. The chemical stability is higher, increasing the tolerance for error values during chemical addition and significantly improving the product yield of the elastic sheet. Furthermore, the overall energy consumption of this invention is far lower than that of conventional ovens used for curing rubber, reducing production costs and eliminating pollution such as high-temperature solvent evaporation from ovens, making it highly environmentally friendly. The elastic sheets produced by this invention have higher softness, are easier to process, and their overall composition is not damaged by high temperatures, making them easy to recycle and reuse. This process is unprecedented and offers multiple functional improvements.
[0049] The above-disclosed embodiments are merely preferred embodiments of this application and are not intended to limit the invention. It should be noted that any modifications made by those skilled in the art to the specific embodiments of this application do not depart from the scope of the claims. Accordingly, the scope of the claims is not limited to the foregoing specific embodiments.
Claims
1. A photocuring method for preparing elastic sheets, characterized in that, The preparation method includes at least the following steps: Compressed sheet (110): An elastic material is compressed into a sheet shape, said elastic material containing a vulcanizing agent; Adhesion (120): A thin sheet is placed on one side of a sheet-like elastic material and pressure is applied to bond the two together to form an elastic sheet semi-finished product; Photocuring (130): A light source is used to irradiate the surface of the elastic material of the elastic sheet semi-finished product for a predetermined time, causing the elastic material to absorb light and heat, thus promoting surface curing of the elastic material and producing the elastic sheet semi-finished product; and Photocuring (140): After the elastic sheet semi-finished product is rolled up, it is placed under a greenhouse and the elastic sheet semi-finished product is irradiated by sunlight and / or light inside the greenhouse to vulcanize and mature the elastic sheet semi-finished product into an elastic sheet.
2. The photocuring method for preparing an elastic sheet according to claim 1, characterized in that, In the step of tableting (110), the elastic material includes at least one of an elastomer, an elastomer mainly composed of plant-based elastic materials, and an all-plant-based elastomer.
3. The photocuring method for preparing an elastic sheet according to claim 1, characterized in that, In the bonding (120) step, the sheet is at least one of fabric or elastic sheet.
4. A method for preparing adhesive-free bonding as described in claim 1, characterized in that, The elastic material also includes a heat-absorbing material, which allows the elastic material to absorb the heat generated when exposed to light, and supply the vulcanizing agent within the elastic material to react.
5. The photocuring method for preparing an elastic sheet according to claim 1, characterized in that, The elastic material also includes a moisture-reactive material to enable the elastic material to absorb moisture in the greenhouse.
6. The photocuring method for preparing an elastic sheet according to claim 1, characterized in that, In the step of photopre-curing (130), the light source includes at least one of ultraviolet light, X-ray, laser light or microwave, and the elastic material also contains a photoinitiator. When the surface of the elastic material is irradiated by light, the photoinitiator in the elastic material can absorb the light and generate a polymerization reaction, thereby promoting the pre-curing of the surface of the elastic material.
7. The photocuring method for preparing an elastic sheet according to claim 1, characterized in that, Between the photo-pre-curing (130) and photo-curing (140) steps, there is also a barrier means (210) that attaches a tearable barrier sheet to the surface of the elastic material to prevent the surfaces of the elastic material from sticking together when the elastic sheet semi-finished product is rolled up.
8. The photocuring method for preparing an elastic sheet according to claim 7, characterized in that, The barrier sheet is equipped with a heat-conducting material to conduct the heat generated when light shines on it to the elastic material.
9. The photocuring method for preparing an elastic sheet according to claim 8, characterized in that, The surface of the barrier sheet is textured.
10. A photocuring method for preparing an elastic sheet according to any one of claims 1 or 6, characterized in that, In the photo-sulfurization (140) step, the greenhouse is equipped with at least one lamp that can emit light, and the power required for the operation of the lamp is supplied by power generated by solar panels installed outside the greenhouse.