Secondary battery and method for manufacturing secondary battery
The anti-corrosion coating layer with a fluorescent material and fire extinguishing agent addresses corrosion at welded joints in secondary batteries, ensuring durability and safety by allowing precise inspection and fire suppression.
Patent Information
- Application Number
- PCT/KR2026/095897
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-09
- Filing Date
- 2026-04-14
- Publication Date
- 2026-11-12
AI Technical Summary
Secondary batteries face issues with corrosion at the welded joints of the case and vent plate due to exposure during laser welding, which can lead to structural degradation and potential safety hazards.
Application of an anti-corrosion coating layer containing a fluorescent material and a fire extinguishing agent, which is cured using UV light, allowing for precise inspection of uniformity and presence through luminescence reactions, and includes a heat-reactive nanocapsule to suppress fires at high temperatures.
The anti-corrosion coating effectively prevents corrosion and enhances the durability of secondary batteries by ensuring uniform application and rapid curing, while also providing fire suppression capabilities.
Smart Images

Figure KR2026095897_12112026_PF_FP_ABST
Abstract
Description
Secondary battery and method for manufacturing a secondary battery
[0001] The present disclosure relates to a secondary battery and a method for manufacturing a secondary battery.
[0002] Unlike primary batteries, which cannot be recharged, secondary batteries are batteries capable of both charging and discharging. Low-capacity secondary batteries are used in small portable electronic devices such as smartphones, feature phones, laptop computers, digital cameras, and camcorders, while high-capacity secondary batteries are widely used as power sources for motor drive systems and power storage batteries in hybrid and electric vehicles. Such secondary batteries include an electrode assembly consisting of a positive electrode and a negative electrode, a case housing the assembly, and electrode terminals connected to the electrode assembly.
[0003] The information described above disclosed in the background technology of this invention is intended only to enhance understanding of the background of the present invention and may therefore include information that does not constitute prior art.
[0004] The present invention provides a secondary battery capable of uniformly applying an anti-corrosion coating layer to the surface of a secondary battery case, and a method for manufacturing the secondary battery.
[0005] In addition, the present invention provides a secondary battery and a method for manufacturing a secondary battery capable of inspecting the uniformity of the application of a rust-preventive coating layer by applying a multi-inspection method utilizing the transparency of the rust-preventive coating layer and the fluorescent reaction of a fire extinguishing agent.
[0006] However, the technical problems that the present invention aims to solve are not limited to those described above, and other unmentioned problems can be clearly understood by those skilled in the art from the description of the invention below.
[0007] An exemplary secondary battery according to one embodiment of the present invention for solving the above technical problem may include a case having an inner space for accommodating an electrode assembly, a vent plate for sealing the case, and an anti-corrosion coating layer containing a fluorescent material on the outer side of at least one of the case and the vent plate.
[0008] In some examples, the anti-corrosion coating layer may include a UV-curable acrylic resin.
[0009] In some examples, the UV-curable acrylic resin may include at least one of epoxy acrylate resin, urethane acrylate resin, and polyester acrylate resin.
[0010] In some examples, the thickness of the anti-corrosion coating layer may be 10㎛ or more and 30㎛ or less.
[0011] In some examples, the anti-corrosion coating layer may contain a fluorescent material in a range of 0.3% to 0.7% relative to the total weight of the anti-corrosion coating liquid.
[0012] In some examples, the anti-corrosion coating layer may include a fluorescent material that emits light when irradiated with ultraviolet (UV) light.
[0013] In some examples, the presence and uniformity of the anti-corrosion coating layer can be inspected based on an image in which a fluorescent material emits light in response to ultraviolet irradiation.
[0014] In some examples, the anti-corrosion coating layer may contain a fire extinguishing agent.
[0015] In some examples, the fire extinguishing agent may include a fluorescent marker having a different luminescence color from the fluorescent material of the anti-corrosion coating layer.
[0016] In some examples, the anti-corrosion coating layer may include a fire extinguishing agent in capsule form.
[0017] In some examples, the fire extinguishing agent may be included in a range of 0.5% to 2% relative to the total weight of the anti-corrosion coating liquid.
[0018] In some examples, the fire extinguishing agent is composed of a heat-reactive nanocapsule and can be released at a temperature of 150°C or higher to suppress the fire.
[0019] An exemplary method for manufacturing a secondary battery according to one embodiment of the present invention for solving the above technical problem may include the steps of: providing a case having an inner space for accommodating an electrode assembly; applying an anti-corrosion coating solution containing a fluorescent material to at least one of the outer side of the case and the outer side of a vent plate welded to the case; curing the anti-corrosion coating layer by irradiating the anti-corrosion coating solution with ultraviolet (UV) light; and inspecting the coating state of the anti-corrosion coating layer by irradiating with ultraviolet light.
[0020] In some examples, the anti-corrosion coating solution may include a UV-curable acrylic resin.
[0021] In some examples, the UV-curable acrylic resin may include at least one of epoxy acrylate resin, urethane acrylate resin, and polyester acrylate resin.
[0022] In some examples, the step of applying the anti-corrosion coating liquid can uniformly apply the anti-corrosion coating liquid to the outer surfaces of the case and the vent plate.
[0023] In some examples, the step of inspecting the application state of the anti-corrosion coating layer can be performed using a vision inspection unit based on the transparency of the anti-corrosion coating layer upon ultraviolet (UV) irradiation.
[0024] In some examples, the anti-corrosion coating solution contains a fire extinguishing agent and can be applied and cured in a single process.
[0025] In some examples, the fire extinguishing agent is included in the form of nano-sized capsules, and the application status of the fire extinguishing agent can be inspected through a luminescence color different from the fluorescent material of the anti-corrosion coating solution upon UV irradiation after curing.
[0026] In some examples, the step of inspecting the application state of the anti-corrosion coating layer may include a first inspection step of inspecting the application state of the anti-corrosion coating layer based on the transparency of the anti-corrosion coating layer and a second inspection step of inspecting the application state of the anti-corrosion coating layer based on the uniformity of the distribution of the fire extinguishing agent.
[0027] In some examples, the anti-corrosion coating layer may contain a fire extinguishing agent in a range of 0.5% to 2% relative to the total weight of the anti-corrosion coating liquid.
[0028] In some examples, the fire extinguishing agent is composed of a heat-reactive nanocapsule and can be released at a temperature of 150°C or higher to suppress the fire.
[0029] According to the present invention, since an anti-corrosion coating layer containing a fluorescent material and a fire extinguishing agent can be uniformly applied to the surface of a secondary battery case, the occurrence of corrosion of the secondary battery can be effectively prevented.
[0030] In addition, by applying a multi-inspection method utilizing the transparency of the anti-corrosion coating layer and the fluorescent reaction of the fire extinguishing agent, the uniformity of the anti-corrosion coating layer can be precisely inspected.
[0031] In addition, by using UV-curable acrylic resin, rapid curing and application stability of the anti-corrosion coating layer can be ensured, thereby improving the reliability and productivity of the manufacturing process.
[0032] However, the effects obtainable through the present invention are not limited to those described above, and other unmentioned technical effects will be clearly understood by those skilled in the art from the description of the invention below.
[0033] The following drawings attached to this specification illustrate preferred embodiments of the present invention and serve to further enhance understanding of the technical concept of the present invention together with the detailed description of the invention provided below; therefore, the present invention should not be interpreted as being limited only to the matters described in such drawings.
[0034] FIG. 1 is a cross-sectional view of a secondary battery according to one embodiment of the present invention.
[0035] FIG. 2 is a perspective view of a secondary battery according to one embodiment of the present invention.
[0036] FIG. 3 is a bottom view illustrating the state before an anti-corrosion coating layer is formed on a vent plate according to one embodiment of the present invention.
[0037] FIG. 4 is a bottom view illustrating a state in which an anti-corrosion coating layer is formed on a vent plate according to one embodiment of the present invention.
[0038] FIG. 5 is a schematic diagram illustrating the composition of an anti-corrosion coating layer according to one embodiment of the present invention.
[0039] FIG. 6 is a bottom view illustrating an area in which a fire extinguishing agent is unevenly distributed in an anti-corrosion coating layer according to one embodiment of the present invention.
[0040] FIG. 7 is a bottom view showing an area in which the transparency of the anti-corrosion coating layer according to one embodiment of the present invention is unevenly distributed.
[0041] FIG. 8 is a front view illustrating a device for inspecting whether a rust-preventive coating layer is properly applied according to one embodiment of the present invention.
[0042] FIG. 9 is a front view illustrating the state in which a fire extinguishing agent is discharged from the bottom of a secondary battery according to one embodiment of the present invention.
[0043] FIG. 10 is a flowchart of a method for manufacturing a secondary battery according to one embodiment of the present invention.
[0044] FIGS. 11 and FIGS. 12 are perspective views illustrating a battery pack including an exemplary secondary battery according to the present invention.
[0045] FIGS. 13 and FIGS. 14 are a perspective view and a side view illustrating an automobile including an exemplary battery pack according to the present invention.
[0046] Preferred embodiments of the present invention will be described in detail below with reference to the attached drawings. Prior to this, terms and words used in this specification and claims should not be interpreted as being limited to their ordinary or dictionary meanings. Instead, based on the principle that the inventor can appropriately define the concepts of terms to best describe their invention, they should be interpreted in a meaning and concept consistent with the technical spirit of the present invention. Therefore, the embodiments described in this specification and the configurations illustrated in the drawings are merely some of the most preferred embodiments of the present invention and do not represent all of the technical spirit of the present invention. It should be understood that various equivalents and modifications capable of replacing them may exist at the time of filing this application.
[0047] Additionally, as used herein, “comprise, include” and / or “comprising, including” specify the presence of the mentioned features, numbers, steps, actions, parts, elements, and / or groups thereof, and do not exclude the presence or addition of one or more other features, numbers, actions, parts, elements, and / or groups.
[0048] Additionally, to aid in understanding the invention, the attached drawings are not drawn to actual scale, and the dimensions of some components may be exaggerated. Furthermore, the same reference numerals may be assigned to identical components in different embodiments.
[0049] The statement that two subjects of comparison are 'identical' means that they are 'substantially identical.' Therefore, substantial identity may include deviations considered low in the industry, for example, deviations within 5%. Additionally, the statement that a parameter is uniform in a given area may mean that it is uniform from an average perspective.
[0050] Although terms such as "first," "second," etc., are used to describe various components, it goes without saying that these components are not limited by these terms. These terms are used merely to distinguish one component from another, and unless specifically stated otherwise, the first component may also be the second component.
[0051] Throughout the specification, unless specifically stated otherwise, each component may be singular or plural.
[0052] The fact that any configuration is placed on the “upper (or lower)” of a component or on the “upper (or lower)” of a component may mean not only that any configuration is placed in contact with the upper (or lower) surface of said component, but also that another configuration may be interposed between said component and any configuration placed on (or below) said component.
[0053] Furthermore, where it is stated that one component is “connected,” “coupled,” or “joined” to another component, it should be understood that while said components may be directly connected or joined to each other, another component may be “interposed” between each component, or that each component may be “connected,” “coupled,” or “joined” through another component. Additionally, when it is stated that a part is electrically coupled with another part, this includes not only cases where they are directly connected but also cases where they are connected with an intermediate element in between.
[0054] Throughout the specification, “and / or B” means A, B, or A and B unless specifically stated otherwise. That is, “and / or” includes any combination or any combination of the enumerated items. “Up to D” means C or more and D or less, unless specifically stated otherwise.
[0055] The terms used in this specification are intended to describe embodiments of the present disclosure and are not intended to limit the present disclosure.
[0056] FIG. 1 is a cross-sectional view of a secondary battery (1) according to one embodiment of the present invention, and FIG. 2 is a perspective view of a secondary battery (1) according to one embodiment of the present invention. As shown in FIG. 1 and FIG. 2, a secondary battery (1) according to one embodiment of the present invention may include a case (10), an electrode assembly (20), a vent plate (50), and an anti-corrosion coating layer (100). Additionally, the secondary battery (1) may further include a rivet terminal (40), a gasket (60), and an insulating member (70).
[0057] The present invention relates to a circular secondary battery (1) with a beadingless structure. The secondary battery (1) is manufactured by sealing the cap plate and the case (10) through external laser welding without the conventional beading and crimping methods.
[0058] However, the nickel coating layer of the case (10) and the vent plate (50) may be damaged during the laser welding process, and as a result, the metal surface of the welded part is exposed, raising concerns about corrosion occurring in a room temperature environment.
[0059] To prevent such problems, an anti-corrosion coating liquid (110) containing a fluorescent material (115) and a fire extinguishing agent (120), which will be described later, can be applied to the outside of the weld, and the anti-corrosion coating layer (100) can be cured by irradiating ultraviolet (UV) light. The coating state of the anti-corrosion coating layer (100) can be inspected based on the luminescence reaction and transparency of the fluorescent material (115) within the anti-corrosion coating layer (100).
[0060] The anti-corrosion coating solution (110) contains a UV-curing acrylic resin solution and may contain a small amount of fluorescent material (115). During a general visual inspection, the anti-corrosion coating layer (100) is transparent, making it difficult to directly determine whether it has been applied. However, when ultraviolet (UV) irradiation (365 nm) is performed, it emits light in a set color such as blue, allowing the application status of the anti-corrosion coating layer (100) to be clearly confirmed.
[0061] Additionally, the anti-corrosion coating layer (100) may include a fire extinguishing agent (120) and may be configured in the form of a nano-sized capsule. When the fire extinguishing agent (120) is irradiated with ultraviolet light, it emits a color different from the fluorescent material (115) of the anti-corrosion coating layer (100), so that the uniformity of the distribution of the fire extinguishing agent (120) and the coating state of the anti-corrosion coating layer (100) can be visually confirmed.
[0062] In particular, since the welded portion of the cap plate and the case (10) has structural characteristics that make it difficult to apply the anti-corrosion coating liquid (110) uniformly, a first inspection is performed based on the transparency of the anti-corrosion coating layer (100), and a second cross inspection is performed based on the uniformity of light emission of the fire extinguishing agent (120), thereby allowing for precise determination of the defective coating area.
[0063] Through such technology, the present invention can strengthen the durability of the secondary battery (1) and maximize the corrosion prevention effect.
[0064] A case (10) according to one embodiment of the present invention has an inner space for accommodating an electrode assembly (20). The case (10) may be formed with a structure having one side open and may be modified into various shapes as needed. In some examples, the case (10) may include a cover portion (11) and a side wall portion (12).
[0065] The cover portion (11) may be formed in the shape of a disc, and a terminal hole (15) for installing a rivet terminal (40) is formed in the center. A cylindrical side wall portion (12) extending a certain length downward from the cover portion (11) is provided. The cover portion (11) and the side wall portion (12) of the case (10) may be formed as a single unit.
[0066] The cover portion (11) may have a flat circular plate shape and may be provided with a terminal hole (15) penetrating the center. A rivet terminal (40) may be inserted into the terminal hole (15) of the cover portion (11) and joined.
[0067] In the manufacturing process of the secondary battery (1), the upper or lower part of the cylindrical case (10) may be open. Accordingly, after inserting the electrode assembly (20) into the case (10) together with the electrolyte, the case (10) can be sealed by attaching a vent plate (50) to the end of the open case (10).
[0068] In some examples, when the case (10) is inverted, the cover portion (11) is located at the bottom, and a vent plate (50) can be attached to the top of the case (10).
[0069] In some examples, the cylindrical case (10) may comprise steel, steel alloy, nickel-plated steel, stainless steel, aluminum, or aluminum alloy. Additionally, in some examples, the case (10) may be referred to as a can, housing, or casing.
[0070] The vent plate (50) is a member welded to the case (10) to seal the open end of the case (10), and various variations are possible. The vent plate (50) is coupled to the case (10) to seal one side of the case (10) and may include a notch (vent) that ruptures at a set pressure.
[0071] The vent plate (50) may be formed of a circular metal plate and may be attached to the bottom of the case (10). In some examples, the lower surface of the vent plate (50) may be exposed to the outside.
[0072] The electrical connection method may vary depending on the material of the vent plate (50). A vent plate (50) made of steel has a negative polarity and can be electrically connected to the case (10). On the other hand, a vent plate (50) made of aluminum can have its electrical connection to the case (10) cut off so that it does not have a negative polarity. Aluminum can provide accurate venting pressure maintenance and excellent machinability, and can reduce the operating pressure error of the vent.
[0073] The vent plate (50) may be formed as a circular plate corresponding to the lower surface of the electrode assembly (20). In some examples, the vent plate (50) may be directly connected to the second electrode plate (22) of the electrode assembly (20), or may be electrically connected to the second electrode plate (22) through a negative current collector. The upper surface of the vent plate (50) may be in contact with the lower surface of the electrode assembly (20). In some examples, the upper surface of the vent plate (50) may be fixed and electrically connected to the second electrode plate (22) exposed to the lower part of the electrode assembly (20) by welding while in contact with the lower surface of the electrode assembly (20).
[0074] The electrode assembly (20) may be referred to as an electrode group, an electrode body, or a jelly roll. An electrode assembly (20) according to one embodiment of the present invention may include a first electrode plate (21), a second electrode plate (22), and a separator (23).
[0075] The electrode assembly (20) may be formed into a cylindrical shape by stacking and winding a first electrode plate (21), a second electrode plate (22), and a separator (23). In some embodiments, the electrode assembly (20) may include a core which is a hollow space in the center.
[0076] In some examples, the first electrode plate (21) may be referred to as the positive electrode plate, and the second electrode plate (22) may be referred to as the negative electrode plate. The opposite configuration is also possible.
[0077] A first electrode plate (21) according to one embodiment of the present invention may include a first substrate and a first active material layer. In some examples, the first active material may be composed of a transition metal oxide (e.g., LiCoO₂, LiNiO₂, LiMn₂O₄, etc.) and may be coated on the first substrate to form the first active material layer. The first substrate may be made of an aluminum (Al) foil.
[0078] The first electrode plate (21) can be electrically connected to the rivet terminal (40) through the positive electrode collector plate (30), and the second electrode plate (22) can be electrically connected to the case (10) through the vent plate (50) or the negative electrode collector plate.
[0079] A second electrode plate (22) according to one embodiment of the present invention may include a second substrate and a second active material layer. In some examples, the second active material may be composed of a negative electrode active material such as graphite or carbon, and may be coated on the second substrate to form a second active material layer. The second substrate may be made of copper (Cu) or nickel (Ni) foil.
[0080] The separator (23) may be positioned between the first electrode plate (21) and the second electrode plate (22) to prevent an electrical short circuit and to allow only lithium ions to move. In some examples, the separator (23) may be positioned on the inner or outer side of the first electrode plate (21). In some examples, the first electrode plate (21), the separator (23), and the second electrode plate (22) may be stacked and wound into a cylindrical shape. The separator (23) may be formed of polyethylene (PE) or polypropylene (PP).
[0081] The positive current collector plate (30) may be formed as a circular metal plate having a shape corresponding to the upper surface of the electrode assembly (20). The area or size of the positive current collector plate (30) may be formed to be the same as or smaller than the area or size of the upper surface of the electrode assembly (20).
[0082] The positive current collector plate (30) may be made of aluminum (Al). The positive current collector plate (30) may be fixed and electrically connected to the first electrode plate (21) exposed to the upper part of the electrode assembly (20) by welding while the lower surface of the positive current collector plate (30) is in contact with the upper surface of the electrode assembly (20).
[0083] Additionally, the upper surface of the positive current collector plate (30) can be fixed and electrically connected to the rivet terminal (40) by welding while in contact with the lower surface of the rivet terminal (40). The positive current collector plate (30) can serve as a current flow path between the first electrode plate (21) of the electrode assembly (20) and the rivet terminal (40).
[0084] The rivet terminal (40) can be inserted into a terminal hole (15) formed in the cover portion (11) of the case (10) and electrically connected to the positive current collector plate (30). The rivet terminal (40) can be configured as a positive terminal, and the rivet terminal (40) and the case (10) can have different polarities. The rivet terminal (40) can be formed of the same or similar material as the positive current collector plate (30) and the first electrode plate (21).
[0085] The rivet terminal (40) may have an upper diameter exposed to the outside of the case (10) and a diameter located inside the case (10) that is larger than the diameter of the terminal hole (15).
[0086] The rivet terminal (40) may include a head (41) exposed to the top of the case (10) and a fastening part (42) located inside the case (10) and coupled with the positive current collector plate (30). The rivet terminal (40) may be coupled from the outside of the terminal hole (15) toward the inside. At this time, the head (41) may be located outside the case (10). Additionally, the fastening part (42) may be compressed by riveting (compressive molding) and pressed into the lower part of the cover part (11) with an insulating member interposed therein. The fastening part (42) may have a larger diameter as it extends from the terminal hole (15) toward the inside of the case (10). In other words, the diameter of the lower part of the fastening part (42) may be larger than the diameter of the upper part. Here, the upper part of the fastening part (42) may refer to the part connected to the head (41). The diameter of the lower portion of the fastening portion (42) may be larger than the diameter of the terminal hole (15), and the diameter of the terminal hole (15) may be larger than the diameter of the upper portion of the fastening portion (42). Additionally, the head (41) may be in close contact with the upper part of the cover portion (11) with a gasket (60) interposed therein. The rivet terminal (40) may be electrically connected to the first electrode plate (21) of the electrode assembly (20) through the positive current collector plate (30).
[0087] The rivet terminal (40) may further include a welding groove (43) having a certain depth from the upper surface of the head (41) toward the fastening part (42). That is, the welding groove (43) penetrates the center of the head (41) and can form a groove from the upper to the lower direction of the fastening part (42). By this welding groove (43), the thickness of the fastening part (42) is reduced, so that welding between the fastening part (42) and the anode current collector plate (30) can be easily performed from the outside of the case (10).
[0088] A gasket (60) is positioned between the rivet terminal (40) and the terminal hole (15) to provide electrical insulation between the rivet terminal (40) and the case (10). An insulating member (70) is positioned between the positive current collector plate (30) and the cover portion (11) of the case (10) to electrically insulate between the positive current collector plate (30) and the case (10).
[0089] The gasket (60) and the insulating member (70) can be formed from a resin material such as polyethylene (PE), polypropylene (PP), or polyethylene terephthalate (PET).
[0090] In some embodiments, the head (41) of the rivet terminal (40) is located on the upper part of the cover portion (11) of the case (10), and a gasket (60) may be interposed in the area where the head (41) and the cover portion (11) overlap in a planar manner. In this case, the gasket (60) may serve to block electrical contact between the rivet terminal (40) and the case (10).
[0091] The diameter of the gasket (60) may be larger than the diameter of the head (41), and the outer circumference of the gasket (60) may extend outward from the head (41) and be exposed to the outside.
[0092] The insulating member (70) can be installed in a plate shape between the cover part (11) and the positive current collector plate (30) in a shape that wraps around the outer perimeter of the fastening part (42).
[0093] Various modifications are possible within the technical concept of preventing rust by applying a rust-preventing coating liquid (110) containing a fluorescent material (115) to at least one of the outer surfaces of the case (10) and the vent plate (50).
[0094] The anti-corrosion coating layer (100) can be formed not only on the outer side of the vent plate (50) but also on the area where the vent plate (50) and the case (10) are welded. In some embodiments, the anti-corrosion coating layer (100) can be formed over the entire outer side of the case (10) and the vent plate (50), and, if necessary, a variation is also possible in which the anti-corrosion coating layer (100) is selectively formed around the weld area.
[0095] For example, the thickness of the anti-corrosion coating layer (100) may be 10㎛ or more and 30㎛ or less. If the thickness of the anti-corrosion coating layer (100) is less than 10㎛, the anti-corrosion performance may be reduced, and if the thickness of the anti-corrosion coating layer (100) exceeds 30㎛, it may be difficult to apply the anti-corrosion coating layer (100) uniformly.
[0096] The anti-corrosion coating layer (100) can be formed using an anti-corrosion coating solution (110) containing a UV-curing acrylic resin, and may include a fluorescent material (115) to check the uniformity of the application of the anti-corrosion coating layer (100). The anti-corrosion coating layer (100) containing the fluorescent material (115) can be inspected for the presence and uniformity of the application of the anti-corrosion coating layer (100) by utilizing a luminescence reaction upon UV irradiation.
[0097] FIG. 3 is a bottom view illustrating the state before the anti-corrosion coating layer (100) is formed on the vent plate (50) according to one embodiment of the present invention. FIG. 3 is a bottom view of a secondary battery (1) illustrating the state before the anti-corrosion coating layer (100) is formed on the vent plate (50).
[0098] In FIG. 3, the vent plate (50) is depicted as a disc shape for clarity of explanation, but in reality, it may include a deformed structure in which a vent is formed or a curve is formed. The vent plate (50) is shown fixed to the case (10) by welding.
[0099] FIG. 4 is a bottom view illustrating a state in which an anti-corrosion coating layer (100) is formed on a vent plate (50) according to one embodiment of the present invention. As shown in FIG. 4, an anti-corrosion coating layer (100) is formed on the outer surface of the vent plate (50) and the case (10), so that corrosion of the vent plate (50) and the case (10) can be effectively prevented.
[0100] FIG. 5 is a schematic diagram illustrating the configuration of an anti-corrosion coating layer (100) according to an embodiment of the present invention. As shown in FIG. 5, the anti-corrosion coating layer (100) is a layer formed to prevent rust by applying it to at least one of the outer surfaces of the case (10) and the vent plate (50). The anti-corrosion coating layer (100) may include an anti-corrosion coating liquid (110) and a fire extinguishing agent (120). The anti-corrosion coating liquid (110) can serve as a medium to evenly disperse the fluorescent material (115) and the fire extinguishing agent (120) while providing an anti-corrosion function. As the anti-corrosion coating liquid (110) hardens, an anti-corrosion coating layer (100) containing the fluorescent material (115) and the fire extinguishing agent (120) can be formed.
[0101] The anti-corrosion coating liquid (110) included in the anti-corrosion coating layer (100) may include a UV-curable acrylic resin. In some examples, the UV-curable acrylic resin may include at least one of an epoxy acrylate resin, a urethane acrylate resin, and a polyester acrylate resin.
[0102] Epoxy acrylate resin exhibits excellent chemical resistance and adhesion, which can improve adhesion to metal surfaces. Urethane acrylate resin offers excellent flexibility and impact resistance, making it effective in preventing cracking in the coating layer. Polyester acrylate resin offers excellent curing speed and heat resistance, which can improve production efficiency and provide stability in high-temperature environments.
[0103] The anti-corrosion coating layer (100) may contain a fluorescent material (115) in a range of 0.3% to 0.7% relative to the total weight of the anti-corrosion coating liquid (110). The fluorescent material (115) has the characteristic of emitting light when irradiated with ultraviolet (UV) light, and the presence or absence and uniformity of the anti-corrosion coating layer (100) can be inspected based on the image of the fluorescent material (115) emitting light in response to UV light irradiation. Additionally, it can be used to inspect the coating state and thickness of the anti-corrosion coating layer (100) based on the image of the fluorescent material (115) emitting light in response to UV light irradiation.
[0104] The fluorescent material (115) may be composed of an organic fluorescent dye or an inorganic fluorescent material.
[0105] Organic fluorescent dyes may include arylamines, coumarins, quinolines, luminescent dyes, etc. These organic fluorescent dyes have high luminescence intensity and can produce various luminescence colors.
[0106] Inorganic phosphors may include zinc sulfate (ZnS), yttrium vanadate (YVO4:Eu), aluminum oxide, etc. Inorganic phosphors have excellent durability and can have stable properties even in high temperature and ultraviolet environments.
[0107] The fluorescent material (115) can emit light through electron transitions when irradiated with ultraviolet (UV) light. When irradiated with ultraviolet light, electrons within the fluorescent material (115) become excited to a high energy level, and then emit light energy as they return to a stable state.
[0108] A fluorescent material (115) can be used to inspect the coating state and the thickness of the anti-corrosion coating layer (100). In some embodiments, blue light emission or green light emission may indicate that the anti-corrosion coating layer (100) is applied normally. Additionally, changes in the thickness of the anti-corrosion coating layer (100) can be visually determined based on the difference in the light emission intensity of the fluorescent material (115).
[0109] The anti-corrosion coating layer (100) may include a fire extinguishing agent (120). The fire extinguishing agent (120) may be formed in the form of nano-sized capsules. For example, the fire extinguishing agent (120) may include a light-emitting marker having a different light-emitting color from the fluorescent material (115) of the anti-corrosion coating layer (100).
[0110] The fire extinguishing agent (120) is released by its thermal reactive properties when a fire occurs, and the released fire extinguishing agent (120) can suppress the fire through the release of non-combustible gas and a heat-blocking effect. In some examples, the anti-corrosion coating layer (100) may include a fire extinguishing agent (120) in the form of a capsule.
[0111] In some examples, the anti-corrosion coating layer (100) may contain a fire extinguishing agent (120) in a range of 0.5% to 2% relative to the total weight of the anti-corrosion coating liquid (110). This range may be set to ensure both anti-corrosion performance and fire suppression performance of the anti-corrosion coating layer (100) simultaneously.
[0112] If the inclusion ratio of the fire extinguishing agent (120) is less than 0.5% relative to the total weight of the anti-corrosion coating liquid (110), the amount of fire extinguishing agent (120) included in the anti-corrosion coating layer (100) is insufficient, and thus the fire extinguishing performance may be reduced in the event of a fire. Additionally, the concentration of the luminescent marker included in the fire extinguishing agent (120) is low, making it difficult to visually inspect the coating state and distribution uniformity of the fire extinguishing agent (120).
[0113] On the other hand, if the inclusion ratio of the fire extinguishing agent (120) exceeds 2% of the total weight of the anti-corrosion coating liquid (110), the anti-corrosion performance may be reduced due to the dilution of the anti-corrosion component in the anti-corrosion coating liquid (110). In addition, excessive use of the fire extinguishing agent (120) may cause an increase in the coating thickness of the anti-corrosion coating layer (100), making it difficult to maintain uniformity of coating.
[0114] Accordingly, it may be preferable for the anti-corrosion coating layer (100) to contain 0.5% or more and 2% or less of a fire extinguishing agent (120) so as to maintain anti-corrosion function while also exhibiting efficient fire suppression performance.
[0115] In some examples, the fire extinguishing agent (120) is configured in the form of a heat-reactive nanocapsule and can be released at a temperature of 150°C or higher to suppress a fire. The reason the fire extinguishing agent (120) does not operate at a temperature below 150°C is that under normal operating conditions, the extinguishing agent is not released and only the anti-corrosion function is performed. Additionally, the fire extinguishing agent (120) can be activated in a high-temperature environment of 150°C or higher to release the extinguishing agent and thus suppress a fire.
[0116] The fire extinguishing agent (120) may include a compound that performs non-combustible gas release and heat blocking functions to maximize fire suppression performance. In some embodiments, the fire extinguishing agent (120) may include one or more of a trihalomethane compound, a powder fire extinguishing agent, a halogenated fire extinguishing agent, and a metal oxide-based fire extinguishing agent.
[0117] Trihalomethane compounds may include carbon tetrafluoride (CF₄) and hexafluoroethane (C₂F₆), and these compounds decompose at high temperatures to release non-combustible gases, thereby suppressing combustion in the event of a fire.
[0118] Powdered fire extinguishers, such as sodium bicarbonate (NaHCO₃) and potassium carbonate (K₂CO₃), decompose upon heating to release carbon dioxide and can suppress combustion reactions.
[0119] Halogenated fire extinguishing agents are carbon halogenated compounds such as Halon 1301 (Bromotrifluoromethane) and Halon 1211 (Bromochlorodifluoromethane), which can provide non-flammable gas release and cooling effects.
[0120] Metal oxide-based fire extinguishers, such as high-temperature stable materials like magnesium oxide (MgO) and aluminum oxide (Al₂O₃), can perform the function of absorbing heat and blocking oxygen.
[0121] The fire extinguishing agent (120) can be manufactured in the form of a nanometer-sized capsule, which ensures uniform distribution of the extinguishing agent and allows it to be activated only at a specific temperature above that of a fire. The nano capsule may consist of a core extinguishing agent and an outer capsule wall surrounding it. The core extinguishing agent is a extinguishing agent released by heat, which can be released at high temperatures to suppress the fire. The outer capsule wall may be formed from a polymer material such as polyurethane or silica, and may be configured to protect the extinguishing agent (120) and be destroyed only at a temperature above that of the set temperature.
[0122] The fire extinguishing agent (120) may include a light-emitting marker that is distinct from the fluorescent material (115) contained in the anti-corrosion coating liquid (110). The fluorescent material (115) of the anti-corrosion coating liquid (110) may emit blue light, and the light-emitting marker of the fire extinguishing agent (120) may emit green light.
[0123] Since the fire extinguishing agent (120) has a different luminescence color than the fluorescent material (115) of the anti-corrosion coating liquid (110), it can be used to check the application state of the fire extinguishing agent (120). When ultraviolet light is irradiated, it can be inspected by imaging whether the fire extinguishing agent (120) has been uniformly applied based on the luminescence reaction.
[0124] In addition, a fire extinguishing agent (120) having a different luminescent color can be used to evaluate the uniformity of the application of the anti-corrosion coating layer (100). By comparing the luminescent color of the blue fluorescent material (115) included in the anti-corrosion coating liquid (110) with the green luminescent marker of the fire extinguishing agent (120), the uniformity of the application of the anti-corrosion coating layer (100) can be verified more accurately.
[0125] FIG. 6 is a bottom view illustrating the distribution state of a fire extinguishing agent (120) within a rust-preventive coating layer (100) according to an embodiment of the present invention. As shown in FIG. 6, the fire extinguishing agent (120) within the rust-preventive coating layer (100) may be distributed in the form of capsules. At this time, an area where the fire extinguishing agent (120) is unevenly distributed may be defined as a first poorly coated area (170), and an area where the fire extinguishing agent (120) is uniformly distributed may be defined as a first normal area (175). The first poorly coated area (170) may refer to an area where the capsules of the fire extinguishing agent (120) are excessively dense or insufficient. On the other hand, an area where the fire extinguishing agent (120) is evenly distributed and can sufficiently perform the function of the rust-preventive coating layer (100) may be defined as a first normal area (175).
[0126] By irradiating ultraviolet rays to obtain a luminescence image of the fire extinguishing agent (120) in the anti-corrosion coating layer (100) and analyzing the image, the existence of a first coating defect area (170) can be inspected. The method of inspecting the distribution of the fire extinguishing agent (120) is based on the intensity and uniformity of the luminescence marker of the fire extinguishing agent (120), and the defect can be determined based on areas where the luminescence intensity of the fire extinguishing agent (120) is abnormally high or low.
[0127] FIG. 7 is a bottom view illustrating the non-uniformity of transparency of a rust-preventive coating layer (100) according to an embodiment of the present invention. As shown in FIG. 7, when the thickness of the rust-preventive coating layer (100) is formed non-uniformly, a clear change in transparency may occur. At this time, the area where the thickness of the rust-preventive coating layer (100) is applied normally may be defined as a second normal area, and the area where the thickness of the rust-preventive coating layer (100) is excessively thin or thick may be defined as a second poorly applied area (180).
[0128] The second coating defect area (180) can be visually distinguished as an area that is excessively brighter or darker than the set normal brightness when irradiated with ultraviolet light. When ultraviolet light is irradiated, the transparency of the second coating defect area (180) and the transparency of the second normal area (185) appear differently. For example, the brightness of the second coating defect area (180) may be lower than that of the second normal area (185).
[0129] The second normal area (185) and the second coating defect area (180) are determined based on the reflected light of the fluorescent material (115) included in the anti-corrosion coating solution.
[0130] The thickness and transparency of the anti-corrosion coating layer (100) may have an inverse relationship. As the thickness of the anti-corrosion coating layer (100) becomes thinner, the transparency may increase, and as the thickness of the anti-corrosion coating layer (100) becomes thicker, the transparency may decrease. For example, if the thickness of the anti-corrosion coating layer (100) is 100 µm, the transparency is defined as 0%. And if the thickness of the anti-corrosion coating layer (100) is 50 µm, the transparency is defined as 20%. And if the thickness of the anti-corrosion coating layer (100) is 30 µm, the transparency is defined as 50%. And if the thickness of the anti-corrosion coating layer (100) is 20 µm, the transparency is defined as 80%.
[0131] The suitability of the coating state can be determined by setting a standard for the normal thickness of the anti-corrosion coating layer (100) in advance. For example, if the normal thickness of the anti-corrosion coating layer (100) is set to 30㎛, the normal area can be determined based on 50% transparency at that thickness.
[0132] For example, the second normal area can be set to a transparency of 50% ± tolerance range (e.g., ±10%), and the second coating defect area (180) can be set to a transparency that is excessively high or low compared to the 50% standard.
[0133] If the transparency of the anti-corrosion coating layer (100) is 80% or more, the thickness of the anti-corrosion coating layer (100) may be excessively thin, and the anti-corrosion performance may be reduced. Also, if the transparency of the anti-corrosion coating layer (100) is 20% or less, the thickness of the anti-corrosion coating layer (100) may be excessively thick, and the uniformity of the coating layer may be reduced.
[0134] FIG. 8 is a front view illustrating a device for inspecting whether a rust-preventive coating layer (100) is properly applied according to an embodiment of the present invention. As shown in FIG. 8, an ultraviolet irradiation unit (130), a vision inspection unit, a control unit (150), and a notification unit (160) may be installed on the outside of a secondary battery (1) to inspect the application state of the rust-preventive coating layer (100). The device may be configured to quickly and accurately inspect the uniformity and normality of the application of the rust-preventive coating layer (100).
[0135] The ultraviolet irradiation unit (130) is installed in the logistics transfer line of the secondary battery (1) and can simultaneously perform inspection and curing of the anti-corrosion coating layer (100). The ultraviolet irradiation unit (130) irradiates ultraviolet light onto the anti-corrosion coating layer (100) to induce a fluorescent reaction and can visually inspect the coating state and thickness of the anti-corrosion coating layer (100).
[0136] The ultraviolet irradiation unit (130) can also perform the function of curing the anti-corrosion coating layer (100). If the anti-corrosion coating layer (100) contains an ultraviolet-curing acrylic resin, the anti-corrosion coating layer (100) can be cured by irradiation of the ultraviolet irradiation unit (130). Through this, the adhesion and durability of the anti-corrosion coating layer (100) can be improved.
[0137] The method of ultraviolet irradiation of the ultraviolet irradiation unit (130) can be modified in various ways. In some embodiments, ultraviolet light can be irradiated only to the welded portion of the vent plate (50) and the case (10), and in other embodiments, ultraviolet light can be irradiated to the entire front surface of the vent plate (50) to inspect the entire area of the anti-corrosion coating layer (100).
[0138] The vision inspection unit is a device that captures and collects images of the anti-corrosion coating layer (100) that emits light through ultraviolet irradiation by the ultraviolet irradiation unit (130). The vision inspection unit may include a high-speed camera or an image sensor, and the captured images may be transmitted to the control unit (150).
[0139] The vision inspection unit can collect images based on the luminescence intensity and uniformity of the anti-corrosion coating layer (100) generated by ultraviolet irradiation, and can measure the thickness change and coating state of the anti-corrosion coating layer (100) in real time.
[0140] The control unit (150) can determine the coating status of the anti-corrosion coating layer (100) by analyzing an image received from the vision inspection unit. The control unit (150) can determine whether the coating is normal based on luminescence intensity and transparency, and can determine it as defective if the thickness of the coating or the uniformity of luminescence deviates from the set criteria.
[0141] In some embodiments, the judgment criteria of the control unit (150) may be set to normal coating and defective coating. Normal coating is when the fluorescence reaction is uniform and the transparency is within a preset range. Defective coating is when the fluorescence reaction is abnormally strong or weak and the transparency deviates from the preset criteria.
[0142] The notification unit (160) is a device that visually or audibly informs the operator whether the anti-corrosion coating layer (100) is normal or defective based on the inspection results of the control unit (150). The notification unit (160) may be configured to provide intuitive delivery of the inspection results, and in some embodiments, the normality of the anti-corrosion coating layer (100) may be indicated through green and red traffic lights.
[0143] FIG. 9 is a front view illustrating a state in which a fire extinguishing agent (120) is discharged from the lower part of a secondary battery (1) according to an embodiment of the present invention. As shown in FIG. 9, a plurality of secondary batteries (1) can be mounted on a module frame (190) to form a battery module (200).
[0144] The module frame (190) can be configured as a structure for stably supporting multiple secondary batteries (1) and for electrical connection and mechanical fixation.
[0145] The battery module (200) can provide a desired power output by adjusting the voltage and current through a series or parallel connection of secondary batteries (1), and can be used in various applications such as electric vehicles and energy storage devices (ESS).
[0146] In the event that a fire occurs outside the secondary battery (1), the fire extinguishing agent (120) within the anti-corrosion coating layer (100) mounted on the bottom of the secondary battery (1) is configured in the form of a heat-reactive capsule, so that the fire extinguishing agent (120) can be automatically released when the temperature reaches 150°C or higher. The released fire extinguishing agent (120) can quickly suppress the initial fire by releasing non-combustible gas or by cooling and oxygen blocking action.
[0147] FIG. 10 is a flowchart of a method for manufacturing a secondary battery (1) according to an embodiment of the present invention. As shown in FIG. 10, the method for manufacturing an exemplary secondary battery (1) according to an embodiment of the present invention has the step of providing a case (10) having an inner space for accommodating an electrode assembly (20). (S10) The method may proceed to the step of forming an anti-corrosion coating layer (100) with a vent plate (50) welded to the case (10).
[0148] The method has a step of applying an anti-corrosion coating liquid (110) containing a fluorescent material (115) to at least one of the outer side of the case (10) and the outer side of the vent plate (50) welded to the case (10). (S20)
[0149] In one embodiment, the step of applying the anti-corrosion coating liquid (110) may involve uniformly applying the anti-corrosion coating liquid (110) to the outer surface of the case (10) and the vent plate (50). The anti-corrosion coating liquid (110) may include a fire extinguishing agent (120) and may be cured to form an anti-corrosion coating layer (100) after application of the anti-corrosion coating liquid (110).
[0150] The method of applying the anti-corrosion coating liquid (110) can be modified in various ways. In one embodiment, the anti-corrosion coating liquid (110) can be applied by a spray coating method, in which case the anti-corrosion coating liquid (110) can be uniformly applied by spraying it onto the outer surface of the case (10) and the vent plate (50).
[0151] In another embodiment, an immersion coating method may be used, and the rust-preventive coating layer (100) may be formed by directly immersing the case (10) in the rust-preventive coating liquid (110).
[0152] In another embodiment, a roll coating method may be applied, and the anti-corrosion coating liquid (110) can be applied uniformly to a certain thickness using a roller.
[0153] As such, the application method of the anti-corrosion coating liquid (110) can be applied in various ways, such as spray coating, immersion coating, and roll coating, and each method can be selected to maximize the uniformity of the coating layer and the application efficiency.
[0154] The method has a step of curing the anti-corrosion coating layer (100) by irradiating the anti-corrosion coating liquid (110) with ultraviolet (UV) light (S30). If the anti-corrosion coating liquid (110) contains an ultraviolet-curing acrylic resin, it can be cured quickly by ultraviolet irradiation, and as a result, the durability and anti-corrosion effect of the anti-corrosion coating layer (100) can be enhanced.
[0155] UV irradiation can be performed in a localized curing method or a full curing method depending on the application area and inspection purpose of the anti-corrosion coating layer (100). In the localized curing method, the anti-corrosion coating layer (100) can be selectively cured by irradiating UV rays only to specific areas, such as the welded parts of the vent plate (50) and the case (10). In the full curing method, the entire area of the anti-corrosion coating layer (100) can be uniformly cured by irradiating UV rays to the entire area where the anti-corrosion coating liquid (110) is applied. Thus, the UV curing method can be modified into a localized curing method and a full curing method, and can be selectively applied depending on the application method and protection area of the anti-corrosion coating layer (100).
[0156] The method includes a step of inspecting the coating state of the anti-corrosion coating layer (100) by ultraviolet irradiation (S40). The step of inspecting the coating state of the anti-corrosion coating layer (100) can be performed by using a vision inspection unit (140) to inspect the transparency of the anti-corrosion coating layer (100) when irradiated with ultraviolet (UV) light.
[0157] The fire extinguishing agent (120) is included in the form of a nano-sized capsule, and the coating state of the fire extinguishing agent (120) can be inspected through a different luminescence color from the fluorescent material (115) of the anti-corrosion coating liquid (110) when irradiated with ultraviolet light after curing.
[0158] In some embodiments, the step of inspecting the coating state of the anti-corrosion coating layer (100) may be divided into a first inspection step and a second inspection step.
[0159] In the first inspection stage, the normality of the coating state can be inspected based on the transparency of the anti-corrosion coating layer (100). Since the thickness and transparency of the anti-corrosion coating layer (100) have an inverse relationship, if the transparency deviates from the set standard range, it can be determined that the coating thickness is uneven.
[0160] In the second inspection stage, the coating state of the anti-corrosion coating layer (100) can be inspected based on the uniformity of the distribution of the fire extinguishing agent (120). The fire extinguishing agent (120) may be included in the anti-corrosion coating layer (100) in the form of nano-sized capsules and may include a luminescent marker that is distinguishable from the fluorescent material (115) of the anti-corrosion coating liquid (110) when irradiated with ultraviolet light. In the second inspection stage, if the fire extinguishing agent (120) is locally excessively dense or insufficient, the area may be determined to have an uneven coating state.
[0161] If both the first and second inspection stages are passed, the anti-corrosion coating layer (100) can be judged to be in a normal coating state, and if it deviates from the standard in even one stage, it can be judged to be in a defective coating state. In this way, by combining the first transparency inspection and the second uniformity inspection of the fire extinguishing agent (120), the coating quality of the anti-corrosion coating layer (100) can be inspected more precisely.
[0162] The electrode assembly (20) of the present invention will be described in more detail.
[0163] In some examples, a compound capable of reversible intercalation and deintercalation of lithium (a lithated intercalation compound) may be used as the positive electrode active material. Specifically, one or more composite oxides of lithium and a metal selected from cobalt, manganese, nickel, and combinations thereof may be used.
[0164] The above composite oxide may be a lithium transition metal composite oxide, and specific examples include a lithium nickel-based oxide, a lithium cobalt-based oxide, a lithium manganese-based oxide, a lithium iron phosphate-based compound, a cobalt-free nickel-manganese-based oxide, or a combination thereof.
[0165] As an example, a compound represented by any one of the following chemical formulas may be used.
[0166] Li a A 1-b X b O 2-c D c (0.90≤a≤1.8, 0≤b≤0.5, 0≤c≤0.05); Li a Mn 2-b X b O 4-c D c (0.90≤a≤1.8, 0≤b≤0.5, 0≤c≤0.05); Li a Ni 1-b-c Co b X c O 2-α D α(0.90≤a≤1.8, 0≤b≤0.5, 0≤c≤0.5, 0<α<2); Li a Ni 1-b-c Mn b X c O 2-α D α (0.90≤a≤1.8, 0≤b≤0.5, 0≤c≤0.5, 0<α<2); Li a Ni b Co c L 1 d G e O2(0.90≤a≤1.8, 0≤b≤0.9, 0≤c≤0.5, 0≤d≤0.5, 0≤e≤0.1); Li a NiG b O2(0.90≤a≤1.8, 0.001≤b≤0.1); Li a CoG b O2(0.90≤a≤1.8, 0.001≤b≤0.1); Li a Mn 1-b G b O2(0.90≤a≤1.8, 0.001≤b≤0.1); Li a Mn2G b O4(0.90≤a≤1.8, 0.001≤b≤0.1); Li a Mn 1-g G g PO4(0.90≤a≤1.8, 0≤g≤0.5); Li (3-f) Fe2(PO4)3(0≤f≤2); Li a FePO4(0.90≤a≤1.8).
[0167] In the above chemical formula, A is Ni, Co, Mn, or a combination thereof; X is Al, Ni, Co, Mn, Cr, Fe, Mg, Sr, V, a rare earth element, or a combination thereof; D is O, F, S, P, or a combination thereof; G is Al, Cr, Mn, Fe, Mg, La, Ce, Sr, V, or a combination thereof; L 1 is Mn, Al, or a combination thereof.
[0168] A positive electrode for a lithium secondary battery may include a current collector (e.g., a first substrate) and a positive electrode active material layer formed on the current collector. The positive electrode active material layer may include a positive electrode active material and may further include a binder and / or a conductive material.
[0169] The content of the positive active material is 90% to 99.5% by weight with respect to 100% by weight of the positive active material layer, and the content of the binder and the conductive material may each be 0.5% to 5% by weight with respect to 100% by weight of the positive active material layer.
[0170] Aluminum may be used as the current collector mentioned above, but is not limited thereto.
[0171] The negative electrode active material includes a material capable of reversibly intercalating / deintercalating lithium ions, lithium metal, an alloy of lithium metal, a material capable of doping and dedoping lithium, or a transition metal oxide.
[0172] A material capable of reversibly intercalating / deintercalating the above lithium ions may be a carbon-based negative electrode active material, such as crystalline carbon, amorphous carbon, or a combination thereof. Examples of the crystalline carbon include graphite, such as natural graphite or artificial graphite, and examples of the amorphous carbon include soft carbon or hard carbon, mesophase pitch carbide, calcined coke, etc.
[0173] As a material capable of doping and undoping the above lithium, a Si-based negative electrode active material or a Sn-based negative electrode active material may be used. The above Si-based negative electrode active material may be silicon, a silicon-carbon composite, SiOx (0 < x < 2), a Si-based alloy, or a combination thereof.
[0174] The silicon-carbon composite may be a composite of silicon and amorphous carbon. According to one embodiment, the silicon-carbon composite may be in the form of silicon particles and amorphous carbon coated on the surface of the silicon particles.
[0175] The silicon-carbon composite may further include crystalline carbon. For example, the silicon-carbon composite may include a core comprising crystalline carbon and silicon particles and an amorphous carbon coating layer located on the surface of the core.
[0176] A negative electrode for a lithium secondary battery may include a current collector (e.g., a second substrate) and a negative electrode active material layer formed on the current collector. The negative electrode active material layer may include a negative electrode active material and may further include a binder and / or a conductive material.
[0177] For example, the negative electrode active material layer may comprise 90% to 99% by weight of negative electrode active material, 0.5% to 5% by weight of binder, and 0% to 5% by weight of conductive material.
[0178] As the binder, a non-aqueous binder, an aqueous binder, a dry binder, or a combination thereof may be used. When an aqueous binder is used as the cathode binder, a cellulose-based compound capable of imparting viscosity may be further included.
[0179] As the current collector mentioned above, a material selected from copper foil, nickel foil, stainless steel foil, titanium foil, nickel foam, copper foam, a polymer substrate coated with a conductive metal, and combinations thereof may be used.
[0180] The electrolyte for a lithium secondary battery may include a non-aqueous organic solvent and a lithium salt.
[0181] The above-mentioned non-aqueous organic solvent serves as a medium through which ions involved in the electrochemical reaction of the battery can move.
[0182] The above-mentioned non-aqueous organic solvent may be a carbonate-based, ester-based, ether-based, ketone-based, or alcohol-based solvent, a non-protic solvent, or a combination thereof, and may be used alone or in a mixture of two or more types.
[0183] In addition, when using carbonate-based solvents, cyclic carbonates and chain carbonates can be mixed and used.
[0184] As described above, a separator may be present between the positive and negative electrodes of a lithium secondary battery. As such a separator, polyethylene, polypropylene, polyvinylidene fluoride, or a multilayer film of two or more layers thereof may be used.
[0185] The above separator may include a porous substrate and a coating layer comprising an organic material, an inorganic material, or a combination thereof located on one or both sides of the porous substrate.
[0186] The above organic material may include a polyvinylidene fluoride-based polymer or a (meth)acrylic-based polymer.
[0187] The above inorganic materials are Al2O3, SiO2, TiO2, SnO2, CeO2, MgO, NiO, CaO, GaO, ZnO, ZrO2, Y2O3, It may include, but is not limited to, inorganic particles selected from SrTiO3, BaTiO3, Mg(OH)2, boehmite, and combinations thereof.
[0188] The above organic and inorganic materials may exist mixed in a single coating layer, or may exist in a stacked form with a coating layer containing organic materials and a coating layer containing inorganic materials.
[0189] The battery according to the above-described embodiment can be used to manufacture a battery pack.
[0190] FIGS. 11 and 12 are perspective views illustrating a battery pack including an exemplary secondary battery according to the present invention. Referring to FIGS. 11 and 12, the battery pack (300) may include a plurality of battery modules (200) and a housing (310) for accommodating the plurality of battery modules (200). For example, the housing (310) may include first and second housings (311, 312) that are coupled in a direction facing each other with the plurality of battery modules (200) interposed therebetween. The plurality of battery modules (200) may be electrically connected to each other using a bus bar (251), and the plurality of battery modules (200) may be electrically connected to each other in a series / parallel or mixed series / parallel manner to obtain the required electrical output. In the drawings, for convenience of illustration, components such as a bus bar for electrical connection of battery cells, a cooling unit, and external terminals are omitted. In some examples, the battery pack (300) may be mounted in a vehicle. The vehicle may be, for example, an electric vehicle, a hybrid vehicle, or a plug-in hybrid vehicle. The vehicle may include a four-wheeled vehicle or a two-wheeled vehicle.
[0191] FIGS. 13 and FIGS. 14 are a perspective view and a side view illustrating an automobile including an exemplary battery pack according to the present invention. In FIG. 13, the battery pack (300) may include a battery pack cover (311) (which may correspond to the first housing) which is part of the vehicle under body (410) and a pack frame (312) (which may correspond to the second housing) disposed at the bottom of the vehicle under body (410). The battery pack cover (311) and the pack frame (312) may be structures formed integrally with the vehicle floor portion (420). The vehicle under body (410) separates the interior and exterior of the vehicle, and the pack frame (312) may be disposed on the exterior of the vehicle.
[0192] As illustrated in FIG. 14, the vehicle may be formed by combining additional parts, such as a hood (510) at the front of the vehicle and fenders (520) located at the front and rear of the vehicle, respectively, with the vehicle body (400). The vehicle includes a battery pack (300) comprising a battery pack cover (311) and a pack frame (312), and the battery pack (300) may be combined with the vehicle body part (400).
[0193] Although the present invention has been described above by limited embodiments and drawings, the present invention is not limited thereto, and it is obvious that various modifications and variations are possible within the scope of the technical spirit of the present invention and the equivalent scope of the claims described below by those skilled in the art to which the present invention belongs.
Claims
1. A case having an inner space for accommodating an electrode assembly; A vent plate for sealing the above case; and A secondary battery comprising: a corrosion-preventive coating layer containing a fluorescent material on the outer side of at least one of the above case and the above vent plate.
2. In Paragraph 1, A secondary battery characterized in that the above-mentioned anti-corrosion coating layer comprises a UV-curing acrylic resin.
3. In Paragraph 2, A secondary battery characterized by the above-mentioned UV-curing acrylic resin comprising at least one of epoxy acrylate resin, urethane acrylate resin, and polyester acrylate resin.
4. In Paragraph 1, A secondary battery characterized by the thickness of the above-mentioned anti-corrosion coating layer being 10㎛ or more and 30㎛ or less.
5. In Paragraph 1, A secondary battery characterized in that the above-mentioned anti-corrosion coating layer contains a fluorescent material in a range of 0.3% to 0.7% relative to the total weight of the anti-corrosion coating liquid.
6. In Paragraph 1, The above anti-corrosion coating layer includes a fluorescent material that emits light when irradiated with ultraviolet (UV) light, and A secondary battery characterized by inspecting the presence and uniformity of the anti-corrosion coating layer based on an image in which the fluorescent material emits light in response to ultraviolet irradiation.
7. In Paragraph 6, The above anti-corrosion coating layer contains a fire extinguishing agent, and A secondary battery characterized in that the above-mentioned fire extinguishing agent includes a luminescent marker having a different luminescent color from the fluorescent material of the anti-corrosion coating layer.
8. In Paragraph 1, A secondary battery characterized by the above-mentioned anti-corrosion coating layer containing a capsule-shaped fire extinguishing agent.
9. In Paragraph 8, A secondary battery characterized by the above-mentioned fire extinguishing agent being included in a range of 0.5% or more and 2% or less relative to the total weight of the anti-corrosion coating liquid.
10. In Paragraph 9, A secondary battery characterized by the above-mentioned fire extinguishing agent being configured in the form of a thermally reactive nanocapsule and configured to be released at a temperature of 150°C or higher to suppress a fire.
11. A step of providing a case having an inner space for accommodating an electrode assembly; A step of applying an anti-corrosion coating solution containing a fluorescent material to at least one of the outer side of the above case and the outer side of the vent plate welded to the above case; A step of curing the anti-corrosion coating layer by irradiating the above anti-corrosion coating solution with ultraviolet (UV) light; and A method for manufacturing a secondary battery comprising the step of inspecting the coating state of the anti-corrosion coating layer by ultraviolet irradiation.
12. In Paragraph 11, A method for manufacturing a secondary battery characterized in that the above-mentioned anti-corrosion coating solution comprises a UV-curing acrylic resin.
13. In Paragraph 12, A method for manufacturing a secondary battery characterized in that the above-mentioned UV-curing acrylic resin comprises at least one of epoxy acrylate resin, urethane acrylate resin, and polyester acrylate resin.
14. In Paragraph 11, A method for manufacturing a secondary battery, characterized in that the step of applying the anti-corrosion coating liquid involves uniformly applying the anti-corrosion coating liquid to the outer surface of the case and the vent plate.
15. In Paragraph 11, A method for manufacturing a secondary battery, characterized in that the step of inspecting the coating state of the above-mentioned anti-corrosion coating layer is to inspect based on the transparency of the anti-corrosion coating layer when irradiated with ultraviolet (UV) light using a vision inspection unit.
16. In Paragraph 11, A method for manufacturing a secondary battery characterized in that the above-mentioned anti-corrosion coating liquid includes a fire extinguishing agent and is applied and cured in a single process.
17. In Paragraph 16, The above-mentioned fire extinguishing agent is included in the form of nano-sized capsules, and A method for manufacturing a secondary battery characterized by being configured to inspect the coating state of the fire extinguishing agent through a different luminescence color from the fluorescent material of the anti-corrosion coating liquid when irradiated with ultraviolet light after curing.
18. In Paragraph 16, The step of inspecting the application state of the above-mentioned anti-corrosion coating layer is, A first inspection step for inspecting the application state of the anti-corrosion coating layer based on the transparency of the anti-corrosion coating layer; and A method for manufacturing a secondary battery comprising: a second inspection step of inspecting the coating state of the anti-corrosion coating layer based on the uniformity of distribution of the fire extinguishing agent.
19. In Paragraph 16, A method for manufacturing a secondary battery, characterized in that the above-mentioned anti-corrosion coating layer contains a fire extinguishing agent in a range of 0.5% or more and 2% or less relative to the total weight of the above-mentioned anti-corrosion coating liquid.
20. In Paragraph 16, A method for manufacturing a secondary battery, characterized in that the fire extinguishing agent is configured in the form of a heat-reactive nanocapsule and is configured to be released at a temperature of 150°C or higher to suppress a fire.