Cage-shaped nano-carrier for targeted delivery of siRNA as well as preparation method and application of cage-shaped nano-carrier

By transforming the negatively charged inner cavity of ferritin into a positively charged one and combining it with functional peptides, a cage-shaped nanocarrier for targeted delivery of siRNA was constructed, which solved the problems of siRNA stability and targeting in the body and achieved efficient cellular uptake and lysis. The body escapes and the treatment effect is improved.

CN118767165APending Publication Date: 2024-10-15INSTITUTE OF BIOPHYSICS CHINESE ACADEMY OF SCIENCES
View PDF 0 Cites 3 Cited by

Patent Information

Application Number
CN202410739532.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-07
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing siRNA has poor stability in the body, low cellular uptake efficiency, lack of targeting and lysosomal escape ability, which limits its application in treatment.

Method used

Through genetic engineering, the negatively charged inner cavity of ferritin was transformed into a positively charged one, and combined with E-helix truncation and functional peptides, a cage-like nanocarrier for targeted delivery of siRNA was constructed to achieve electrostatic adsorption and lysosomal escape.

Benefits of technology

It significantly improves the delivery stability, cellular uptake efficiency and targeted therapy efficacy of siRNA in vivo and in vitro, realizes lysosomal escape function, and is widely used in anti-tumor and genetic disease treatment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118767165A_ABST
    Figure CN118767165A_ABST
Patent Text Reader

Abstract

The invention discloses a cage-shaped nano-carrier for targeted delivery of siRNA as well as a preparation method and application thereof. The preparation method comprises the following steps: (A) mutating negatively charged or uncharged amino acid on the inner surface of ferritin into positively charged amino acid; and any one or more of the following steps: (B) coupling a functional peptide with nucleic acid affinity to the N end of the ferritin; (C) coupling the N end of the ferritin with a functional peptide for promoting lysosome escape; (D) truncating an E helix at the C end of the ferritin; (E) coupling the C end of the ferritin with a functional peptide with nucleic acid affinity; and (F) coupling the C end of the ferritin with a functional peptide for promoting lysosome escape. According to the preparation method, a negative electricity inner cavity of ferritin is transformed into positive electricity, a novel nucleic acid protein-loaded nanocage carrier is constructed, the electronegative siRNA can be efficiently loaded into the ferritin nanocage through the electrostatic adsorption effect, and the in-vivo and in-vitro delivery stability, the lysosome escape function and the targeted treatment effect of the siRNA are remarkably improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a ferritin bionano material, in particular to a cage-shaped nanocarrier for targeted delivery of siRNA, and a preparation method and application thereof. Background Art

[0002] Nucleic acid drugs can specifically target pathogenic genes and precisely target and regulate diseases at the gene level. Due to their safety, high specificity, high efficiency, and low production cost, nucleic acid drugs have received widespread attention in the field of precision and personalized treatment in recent years. In 1998, the RNA interference phenomenon was first discovered. RNAi forms an RNA-induced silencing complex in the cytoplasm by introducing double-stranded RNA (i.e., small interfering RNA, siRNA) with the same sequence as the endogenous target gene, and pairs with its homologous mRNA to degrade it, thereby achieving post-transcriptional gene silencing. This method is relatively safe, and siRNA will not be integrated into the genome. After taking effect, it can be degraded by enzymes and will not affect gene transcription and protein expression in other normal cells. However, there are huge challenges in the current field. Free siRNA has the problems of poor stability and easy to cause immunity in the application. First of all, as a short nucleotide sequence, siRNA is easily degraded by nucleases after entering the blood circulation, and is easily cleared through the kidneys, with a short half-life in the body. At the same time, it is immunogenic and easily causes an immune response in the human body. In addition, siRNA is a negatively charged hydrophilic molecule with low cellular uptake efficiency. Free siRNA is also not targeted and cannot achieve precise delivery. In addition, after entering the cell, siRNA cannot escape the lysosome and then function in the cytoplasm. siRNA cannot effectively target tumors, which also limits their application in vivo. In order to overcome these difficulties, researchers have designed a variety of carriers, such as lipid nanoparticles (LNPs), GalNAc-based nanocarriers, cationic polymers, micelles, etc. These carriers have solved the problems of poor stability and low delivery efficiency of siRNA to a certain extent. However, due to the lack of tumor targeting ability, the therapeutic effect is not ideal. Therefore, in order to achieve the goal of safe, efficient and precisely targeted nucleic acid therapy, it is urgent to develop a safe and efficient siRNA drug in vivo delivery carrier.

[0003] Among the numerous nucleic acid delivery systems, caged proteins have attracted extensive attention in the field of drug carriers due to their unique water solubility, high dispersibility, symmetry and uniformity. Ferritin is a representative natural caged protein. Mammalian ferritin has 24 subunits and can form a hollow spherical nanoprotein cage with an inner diameter of 8nm and an outer diameter of 12nm through a reversible self-assembly process. Ferritin has many advantages as a drug carrier, including: 1. Uniform nanometer size and hollow cage structure; 2. High stability, low immunogenicity and high biocompatibility; 3. Reversible self-assembly properties, which can simply mediate the disassembly and self-assembly of the protein cage by adjusting the pH of the buffer or adding a denaturant, thereby achieving drug loading in the lumen; 4. It is easy to modify its properties and functions through methods such as genetic engineering or chemical modification; 5. Ferritin has transferrin receptor 1 (TfR1)-mediated endocytosis and inherent tumor targeting. At present, ferritin has been used in many studies to deliver drugs, but further research is still needed in siRNA delivery. Summary of the invention

[0004] In response to the problems of siRNA lysosomal escape, loading and lack of tumor targeting, the present invention provides a caged nanocarrier for targeted delivery of siRNA, a preparation method and application thereof, which can efficiently and stably load siRNA into the inner cavity of the caged protein and achieve lysosomal escape.

[0005] In order to achieve the above object, the present invention provides a method for preparing a caged nanocarrier for targeted delivery of siRNA, the preparation method comprising:

[0006] (A), mutating the negatively charged or uncharged amino acids spatially distributed on the inner surface of ferritin into positively charged amino acids; and any one or more of the following steps:

[0007] (B), coupling the N-terminus of the ferritin to a functional peptide having nucleic acid affinity;

[0008] (C), coupling the N-terminus of the ferritin to a functional peptide that promotes lysosomal escape;

[0009] (D), truncating the E helix at the C-terminus of the ferritin;

[0010] (E), coupling the C-terminus of the ferritin to a functional peptide having nucleic acid affinity;

[0011] (F) The C-terminus of the ferritin is coupled to a functional peptide that promotes lysosomal escape.

[0012] Ferritin "HFn" refers to any ferritin that can form a cage-like structure, which can be ferritin of natural origin, or recombinantly expressed ferritin, or a mutant thereof, which can be derived from prokaryotes, protists, fungi, plants or animals, such as bacteria, fungi, insects, reptiles, birds, amphibians, fish, mammals, such as rodents, ruminants, non-human primates or humans, such as mice, rats, guinea pigs, dogs, cats, cattle, horses, sheep, monkeys, gorillas, humans. From bacteria to humans, although the amino acid sequences of ferritin in different organisms are very different, their structures are similar and can form a protein shell structure.

[0013] In certain embodiments, the ferritin is human heavy chain ferritin HFn, whose amino acid sequence is SEQ ID NO.1.

[0014] The present invention transforms the negatively charged inner cavity of ferritin into a positively charged one by means of genetic engineering, constructs a novel nucleic acid-carrying protein nanocage carrier, and through electrostatic adsorption, negatively charged siRNA can be efficiently loaded into the ferritin nanocage, significantly improving the in vitro and in vivo delivery stability, cellular uptake efficiency and targeted therapeutic efficacy of siRNA, while achieving lysosomal escape function (such as Fig.15 shown).

[0015] Specifically, in step (A), the mutation sites of the ferritin are Glu61, Glu64, Glu140, Glu147, D177, D179 and E181.

[0016] Preferably, in step (A), the positively charged amino acid is selected from any one of arginine, lysine and histidine.

[0017] Specifically, step (B) is any of the following:

[0018] (B1) coupling the N-terminus of the ferritin with a functional motif having a nucleic acid binding peptide;

[0019] (B2) coupling the N-terminus of the ferritin with a functional motif having a positively charged peptide;

[0020] Step (C) is: coupling the N-terminus of the ferritin with a functional motif having a cell-penetrating peptide;

[0021] Step (E) is any of the following:

[0022] (E1) coupling the C-terminus of the ferritin with a functional motif having a nucleic acid binding peptide;

[0023] (E2) coupling a functional motif with a positively charged peptide to the C-terminus of the ferritin;

[0024] Step (F) is: coupling the C-terminus of the ferritin with a functional motif of a cell-penetrating peptide.

[0025] Preferably, in step (B1) and step (E1), the functional motif sequence with nucleic acid binding peptide is as shown in SEQ ID NO.9;

[0026] In step (B2) and step (E2), the functional motif sequence with positively charged peptide is shown as SEQ ID NO.10-15;

[0027] In step (C) and step (F), the functional motif sequence with the cell penetrating peptide is shown as SEQ ID NO.16-31.

[0028] The second aspect of the present invention provides a caged nanocarrier for targeted delivery of siRNA prepared by the preparation method described in the first aspect of the present invention, wherein the inner cavity of the ferritin cage nanocarrier is positively charged.

[0029] In certain embodiments, the ferritin cage nanocarrier contains mutation sites of Glu61, Glu64, Glu140, Glu147, D177, D179 and E181.

[0030] In certain embodiments, the ferritin cage nanocarrier is truncated to varying degrees at the C-terminus, and the final sequence is SEQ ID NO. 5-8.

[0031] In certain embodiments, the ferritin cage nanocarrier comprises the amino acid sequence of SEQ ID NO.9-31.

[0032] In certain embodiments, the amino acid sequence of the ferritin cage nanocarrier is any one or more of SEQ ID NO.1-8.

[0033] In certain embodiments, the siRNA loading capacity of the ferritin cage nanocarrier is 2-3 nucleic acid molecules per protein cage.

[0034] The third aspect of the present invention provides a siRNA delivery system, which comprises siRNA and the caged nanocarrier for targeted siRNA delivery according to the second aspect of the present invention.

[0035] In certain embodiments, the molar mass ratio of the ferritin cage nanocarrier to the siRNA is 1:(1-5), preferably 1:2.

[0036] The fourth aspect of the present invention provides a method for encapsulating siRNA using the siRNA delivery system described in the third aspect, the method comprising the following steps:

[0037] S1. Preparation and purification of ferritin cage nanocarriers for siRNA delivery system;

[0038] S2, dissolve siRNA in DEPC water and dilute to a certain concentration;

[0039] S3, adding the ferritin nanocage carrier obtained in step S1 to an acidic buffer solution of pH 1-3, and incubating at 4° C. for 20-30 minutes to obtain an acid depolymerization system;

[0040] S4, adding the siRNA solution prepared in step S2 to an alkaline buffer solution of pH 9-11, mixing evenly, adding the acid depolymerization system obtained in step S3, and incubating at 4° C. for 2-3 hours to reassemble the ferritin nanocage with the siRNA loaded in the inner cavity.

[0041] In certain embodiments, the acidic buffer solution in step S3 is an HCl solution, preferably an HCl solution with a pH of 1.5-1.6.

[0042] In certain embodiments, the alkaline buffer described in step S4 includes but is not limited to Na2CO3 / NaHCO3, Na2CO3, NaHCO3, Tris, NaOH solution, etc. Preferably, the alkaline buffer is a Na2CO3 / NaHCO3 solution with a pH of 9-10.

[0043] In certain embodiments, the molar mass ratio of the protein cage nanocarrier to the siRNA in step S4 is 1:1-1:5, preferably 1:2.

[0044] The fifth aspect of the present invention provides the caged nanocarrier for targeted delivery of siRNA described in the second aspect of the present invention, and use of the siRNA delivery system described in the third aspect of the present invention in siRNA delivery.

[0045] The sixth aspect of the present invention provides the caged nanocarrier for targeted delivery of siRNA described in the second aspect of the present invention, and the use of the siRNA delivery system described in the third aspect of the present invention in the preparation of drugs for the treatment of anti-tumor or anti-viral and related genetic diseases.

[0046] Through the above technical solution, the present invention achieves the following beneficial effects:

[0047] The present invention transforms the negatively charged inner cavity of ferritin into a positively charged one by means of genetic engineering, and constructs a novel nucleic acid-carrying protein nanocage carrier. Through electrostatic adsorption, negatively charged siRNA can be efficiently loaded into the interior of the ferritin nanocage, combined with measures such as E-helix truncation and the addition of lysosomal escape peptides, significantly improving the in vivo and in vitro delivery stability, cell uptake efficiency and targeted therapeutic efficacy of siRNA, while achieving lysosomal escape function. The ferritin cage nanocarrier constructed by the present invention can be used as a universal siRNA loading platform to achieve lysosomal escape, and is widely used in anti-tumor, anti-viral and related gene disease treatment. BRIEF DESCRIPTION OF THE DRAWINGS

[0048] Figure 1 Schematic diagram of the construction and characterization of the inner cavity positively charged mutant and C-terminal truncated protein cage nanocarrier in Example 2 of the present invention, wherein (A) is the size exclusion chromatography analysis of the wild-type HFn and a series of mutant tHFn(+) proteins, (B) is the 15% SDS-PAGE analysis of the purified wild-type HFn and a series of mutant tHFn(+) proteins, (C) is the Native-PAGE analysis of the purified wild-type HFn and a series of mutant tHFn(+) proteins, (D) is the Zeta potential analysis of the wild-type HFn and a series of mutant tHFn(+) proteins, (E) is the characterization of the particle size of the wild-type HFn and a series of mutant tHFn(+) proteins by DLS, and (F) is the TEM characterization of the wild-type HFn and a series of mutant tHFn(+) proteins;

[0049] Figure 2 It is the evaluation of the lysosomal escape function of tHFn(+) in Example 3 of the present invention, wherein (AB) is the CLSM analysis of the localization of HFn, tHFn(+) and endosomal in U87MG cells, (C) is the Pearson correlation coefficient quantitative analysis of the localization of HFn, tHFn(+) and endosomal in U87MG cells (DE) is the CLSM analysis of the localization of HFn, tHFn(+) and lysosome in U87MG cells, (F) is the Pearson correlation coefficient quantitative analysis of the localization of HFn, tHFn(+) and lysosome in U87MG cells;

[0050] Figure 3 The figure is the characterization of siRNA@tHFn(+) in Example 4 of the present invention, wherein (A) is the comparison of siRNA loading capacity between the protein mutant and HFn, (B) is the protein recovery rate of siRNA loaded by the protein mutant, (C) is the particle size measurement of siRNA@tHFn(+), and (D) is the transmission electron microscopy characterization of siRNA@tHFn(+);

[0051] Figure 4This is the evaluation of the cellular uptake efficiency of siRNA@tHFn(+) in Example 5 of the present invention, wherein (A) is the CLSM analysis of siRNA uptake in U87MG cells, and (BC) is the FCM analysis and quantification of siRNA uptake in U87MG cells;

[0052] Figure 5 It is the evaluation of the knockdown ability of siRNA@tHFn(+) at the cellular level in Example 6 of the present invention, (AB) is the situation and gray value analysis of TERT knockdown in U87MG cells by siTERT@tHFn(+), and (CD) is the situation and gray value analysis of EGFR knockdown in U87MG cells by siEGFR@tHFn(+);

[0053] Figure 6 This is the evaluation of the tumor targeting ability of siRNA@tHFn(+) in Example 7 of the present invention, (A) is the binding ability of the protein to the TfR1 receptor, and (B) is the tumor targeting situation of siRNA@tHFn(+) in mice;

[0054] Figure 7 is the anti-tumor efficacy of siTERT@tHFn(+) on mouse brain glioma in Example 8 of the present invention, (AB) is the bioluminescence intensity and quantification of brain tumor, and (C) is the weight of mouse;

[0055] Figure 8 is the anti-tumor efficacy of siEGFR@tHFn(+) on mouse brain glioma in Example 8 of the present invention, (AB) is the bioluminescence intensity and quantification of brain tumor, and (C) is the weight of mouse;

[0056] Fig. 9 DLS (A) and TEM characterization (B) of the purified nucleic acid-binding peptide-modified ferritin in Example 9 of the present invention;

[0057] Fig.10 is a comparison of the siRNA loading capacity of the nucleic acid-binding peptide-modified ferritin and HFn in Example 10 of the present invention;

[0058] Fig.11 Native-PAGE (A) analysis and TEM characterization (B) of the purified positively charged peptide-modified ferritin in Example 11 of the present invention;

[0059] Fig.12 The CLSM analysis of the localization of positively charged peptide-modified ferritin mutants and lysosomes in U87MG cells in Example 12 of the present invention;

[0060] Fig.13 is the TEM characterization of the purified cell-penetrating peptide-modified ferritin in Example 13 of the present invention;

[0061] Fig.14 The CLSM analysis of the localization of the cell-penetrating peptide-modified ferritin mutant and lysosomes in U87MG cells in Example 14 of the present invention;

[0062] Fig.15 It is a schematic diagram of the present invention in which ferritin is modified and loaded with siRNA. DETAILED DESCRIPTION

[0063] The embodiments of the technical solution of the present invention are described in detail below. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and are therefore only used as examples, and cannot be used to limit the scope of protection of the present invention. It should be noted that, unless otherwise specified, the technical terms or scientific terms used in this application should be the usual meanings understood by those skilled in the art to which the present invention belongs.

[0064] Example 1 Construction of recombinant plasmids of ferritin cage nanocarriers with positive internal charge mutation and C-terminal truncated ferritin cage

[0065] The design was based on amino acid mutations on the inner surface of the protein cage and truncation of the C-terminus of ferritin: point mutations were made to the negatively charged amino acids located on the inner surface of HFn (SEQ ID NO.1) by genetic engineering means, that is, positively charged lysine and arginine were used to specifically replace glutamic acid at positions 61, 64, 140, 147, and 181 and aspartic acid at positions 177 and 179 of the HFn subunit (SEQ ID NO.2-4, HFn (4+), HFn (5+), HFn (7+)), and the specific mutations were E61K / E64R / E140K / E147K / E181K / D177K / D179K. At the same time, the C-terminus of ferritin was truncated to different degrees (the C-terminus was truncated to positions 179, 174, 162, and 159). The cDNA sequence of tHFn(+) was designed according to its amino acid sequence (SEQ ID NO.5-8), and cloned into the E. coli expression vector pET30a plasmid with NdeI and BamHI restriction enzyme cutting sites. The sequence was confirmed to be correct by DNA sequencing.

[0066] Example 2 Expression, purification and characterization of intracavity positively charged mutant and C-terminally truncated protein cage nanocarriers

[0067] tHFn(+) protein expression: The plasmids obtained in Example 1 were transformed into the expression strain BL21(DE3), respectively, and grown and amplified in LB medium containing 100 mg / L kanamycin or ampicillin, and IPTG was added at a final concentration of 0.5 mM, and cultured at 25°C, 200 rpm for 12 h for protein induced expression.

[0068] Purification of tHFn(+) protein: Collect bacterial liquid, centrifuge at 4000g to collect bacterial cells, and resuspend the bacterial cells in 20mM Tris-HCl (pH8.0) buffer. After high-pressure homogenization, centrifuge at 12000g to remove E. coli debris, collect the supernatant and heat it in a 60℃ water bath for 10 minutes to denature and precipitate most of the impurities. Centrifuge at 12000g to collect the supernatant. The mutant supernatant was first purified by hydrophobic chromatography column Phenyl sepharose, and then further purified by Superdex 200 molecular sieve.

[0069] The protein concentrations of wild-type HFn and mutant tHFn(+) were determined by the BCA method, the purity of HFn and tHFn(+) was identified by 15% SDS-PAGE electrophoresis, the 24-mer assembly of mutant tHFn(+) was identified by Native-PAGE electrophoresis, and the morphology and particle size of tHFn(+) were further characterized by transmission electron microscopy (TEM) and dynamic light scattering (DLS).

[0070] Analyze the experimental results, such as Figure 1 As shown, size exclusion chromatography analysis showed that the mutant tHFn(+) 1-179 、tHFn(+) 1-174 、tHFn(+) 1-162 、tHFn(+) 1-159 The peak position is basically consistent with WT. SDS-PAGE results show that the protein bands of the tHFn(+) series mutants with different degrees of C-terminal truncation appear at a molecular weight of 17-21kDa, which is consistent with the theoretical value. On Native-PAGE gel, the protein bands of the series of mutants HFn(+) and wild-type HFn are in similar positions, indicating that the lumen modification and C-terminal truncation do not affect the assembly ability of ferritin, and the tHFn(+) subunits can smoothly self-assemble to form 24-mers. TEM and DLS analysis showed that the series of mutants tHFn(+) with positively charged amino acid mutations in the lumen and C-terminal truncation had a nanocage structure with a diameter of about 13nm. Zeta potential analysis showed that the external surface properties of the tHFn(+) series were basically consistent with WT.

[0071] Example 3 Verification of the Lysosomal Escape Function of tHFn(+) Nanocarriers

[0072] Select the protein mutant tHFn(+) with the largest degree of truncation in Example 2 1-159 Subsequent exploration was carried out (SEQ ID NO. 8), which is hereinafter referred to as tHFn(+).

[0073] Endosomal colocalization: U87MG was plated onto a confocal dish, and Cy5.5-HFn and Cy5.5-tHFn(+) were added, respectively, with the concentration of Cy5.5 being 1 μM. After 15 and 30 min of co-incubation, the cells were taken out, endosomes were stained with EEA1, cell nuclei were stained with DAPI, and different fluorescence inside U87MG cells was observed by CLSM to characterize the localization of drugs and endosomes.

[0074] Lysosome colocalization: U87MG was spread on a confocal dish, and Cy5.5-HFn and Cy5.5-tHFn(+) were added, respectively, where the concentration of Cy5.5 was 1μM. After 15, 30, 60, and 120 minutes of co-incubation, the cells were taken out, lysosomes were stained with LAMP-1, cell nuclei were stained with DAPI, and different fluorescence inside U87MG cells was observed by CLSM to characterize the localization of drugs and lysosomes.

[0075] The experimental results were analyzed and the results were as follows Figure 2 As shown in the figure, from the CLSM results and Pearson correlation coefficient analysis, it can be seen that HFn first enters the endosome and then accumulates in the lysosome, while tHFn(+) first enters the early endosome and then escapes without entering the lysosome, indicating that tHFn(+) nanocarriers can achieve escape function in tumor cells.

[0076] Example 4 Method for loading siRNA into protein cage nanocarrier

[0077] siRNA is an oligonucleotide with a double-stranded RNA structure. The following is a detailed description of the method for siRNA encapsulation based on protein cage nanocarriers: add an equal volume of 10 mg / mL protein cage nanocarrier tHFn(+) solution to HCl solution (pH 1-3), mix thoroughly, and incubate at 4°C for 20-30 minutes to mediate protein cage depolymerization in a strong acid environment. Take the siRNA solution and premix it with Na2CO3 / NaHCO3 solution (pH 9-11), then add it to the acid depolymerization system of the protein cage and mix thoroughly, neutralize the system to neutrality (pH 6.5-7.5), and incubate at 4°C for 2-3 hours. After taking it out, ultrafilter the sample solution to remove free siRNA. Finally, use the Qubit 4Fluorometer microRNA kit to quantify the concentration of siRNA, use the BCA kit to quantify the concentration of protein, and calculate the siRNA loading rate, protein recovery rate, and siRNA utilization rate of tHFn(+).

[0078] The experimental results were analyzed and the results were as follows Figure 3As shown in the figure, as the degree of C-terminal truncation gradually increases, the siRNA rate and siRNA utilization rate also increase successively. Compared with HFn, the nucleic acid loading capacity of tHFn(+) has been greatly improved. At the same time, the inner cavity modification does not affect the stability of the ferritin cage itself, and the protein recovery rate of tHFn(+) is basically consistent with that of wild-type HFn. TEM and DLS analysis showed that siRNA@tHFn(+) can be assembled into a protein cage structure with a diameter of about 13.7nm, which is consistent with the structure of tHFn(+) without siRNA loading.

[0079] Example 5 Promotion of siRNA Cellular Uptake by tHFn(+) Nanocarriers (In Vitro Cell Verification)

[0080] (1) Evaluation by fluorescence confocal microscopy (CLSM): U87MG was plated on a confocal dish, and Free Cy5-siRNA and Cy5-siRNA@tHFn(+) were added to the control group and the experimental group, respectively, where the concentration of Cy5-siRNA was 1μM. After 2 hours of co-incubation, the cells were taken out, the cell nuclei were stained with DAPI, and the Cy5-siRNA fluorescence inside the U87MG cells was observed by CLSM to characterize the cell uptake. (2) Evaluation by flow cytometry: U87MG was plated on a 6-well plate, and co-incubated with Free Cy5-siRNA and siRNA@tHFn(+) at 37℃ for 2 hours and 4 hours, and then the cells in each group were collected, and the Cy5-siRNA fluorescence was detected by flow cytometry and quantitative analysis was performed.

[0081] The experimental results were analyzed and the results were as follows Figure 4 As shown in the figure, the results of CLSM and flow cytometry analysis show that free siRNA is difficult to be taken up by cells through the cytoplasmic membrane due to its hydrophilicity. Flow cytometry quantitative analysis shows that the siRNA uptake of siRNA@tHFn(+) in U87MG cells is much higher than that of free siRNA. In the U87MG cells of the free siRNA group, almost no fluorescence of Cy5-siRNA was observed, while in the siRNA@tHFn(+) experimental group, the cellular internalization efficiency of siRNA can be significantly improved by means of the cellular endocytosis process mediated by tHFn(+).

[0082] Example 6 Verification of the knockdown function of target protein by siRNA@tHFn(+) nanocarrier

[0083] U87MG was plated on a 6-well plate, and tHFn(+), free siRNA, siNC@tHFn(+), siRNA@LNP, and siRNA@tHFn(+) were added respectively. After incubation for 48 hours, the cells were harvested, and the proteins were separated in 10% SDS-PAGE, then transferred to a PVDF membrane, blocked with blocking solution for 1 hour, incubated with TERT / EGFR primary antibody and Tubulin primary antibody at 4°C overnight, incubated with secondary antibody for 1 hour, and exposed. The protein bands were analyzed by gray value to characterize the expression of TERT / EGFR protein.

[0084] The experimental results were analyzed and the results were as follows Figure 5 As shown in the figure, from the WB results and gray value analysis, it can be seen that free siEGFR has no knockdown effect, while siRNA@LNP and siRNA@tHFn(+) can achieve knockdown of the target protein at the cellular level, indicating that tHFn(+) is an effective siRNA delivery carrier.

[0085] Example 7 Tumor Targeting Ability of tHFn(+) Protein Cage Nanocarrier

[0086] Protein affinity for TfR1 receptor (ELISA method): HFn and tHFn(+) protein samples were graded diluted with carbonate buffer (pH 9.4), added to the ELISA plate, and incubated at 37°C for 2 hours. Then, 0.5% BSA solution was incubated at 37°C for 1 hour. Subsequently, the plate was incubated with TfR1, TfR1 antibody, and anti-mouse IgG (H+L) for 1 hour. Finally, TMB substrate was added to the plate and read at OD 652nm using a microplate reader.

[0087] Evaluation of tumor targeting ability in mice: 1×10 6 U87MG-luc-mCherry cells were used to construct a brain tumor model. Cy5-labeled siRNA and siRNA@tHFn(+) were intravenously injected, and the final concentration of Cy5 was 15μM. Living Image was used for in vivo imaging 6, 12, and 24 hours after administration.

[0088] Analyze the experimental results, such as Figure 6 As shown, according to the ELISA results and calculated K D Value, K of HFn and tHFn(+) DThe values ​​were 26.59nM and 1.44nM, respectively, which indicates that tHFn(+) increases the affinity of protein to TfR1, which is beneficial for the vector to target tumor cells. According to in vivo imaging of mice, free siRNA mainly enters the kidneys and cannot be enriched in brain tumors, while siRNA delivered by tHFn(+) can cross the blood-brain barrier and target brain tumors.

[0089] Example 8 Anti-tumor function of siRNA delivered by tHFn(+) protein cage nanocarrier (in vivo efficacy verification)

[0090] Evaluation of antitumor efficacy (orthotopic brain glioma model): 1×10 6 U87MG-luc-mCherry cells were used to construct a brain tumor model. For TERT-target-based treatment, tumor-bearing mice were randomly divided into groups and intravenously administered with PBS, tHFn(+), siTERT, siNC@tHFn(+), siTERT@LNP, and siEGFR@tHFn(+), respectively, with a siTERT dose of 1 mg / kg. The drug was injected every other day, and the weight of the mice was detected and recorded. The mice were imaged by IVIS Lumina3 every two days, and the bioluminescence intensity was analyzed to record the tumor size. For EGFR-target-based treatment, the mice were divided into four groups: PBS, siEGFR, tHFn(+), and siEGFR@tHFn(+). Body weight and tumor volume were recorded according to the experimental design.

[0091] Analyze the experimental results, such as Figure 7 and Figure 8 As shown in the figure, the in vivo antitumor efficacy results showed that free siRNA and siRNA@LNP could not inhibit tumor growth. The tHFn(+) carrier itself did not have antitumor effects, but by delivering siTERT or siEGFR, it showed antitumor effects on orthotopic brain glioma. In addition, the ferritin cage nanocarrier tHFn(+) and siRNA@tHFn(+) had good in vivo safety and did not cause side effects such as weight loss.

[0092] Example 9 Construction, expression, purification and characterization of the recombinant plasmid of the ferritin cage nanocarrier modified with nucleic acid binding peptide functional motif

[0093] Design based on the functional motif of modified nucleic acid binding peptide at the N-terminus or C-terminus of ferritin: The wild-type ferritin (SEQ ID NO.1) and the inner cavity positive point electrogenic mutant ferritin (SEQ ID NO.2) obtained in Example 1 were truncated at the C-terminus and coupled with the functional motif of nucleic acid binding peptide by genetic engineering means. The cDNA sequence of the ferritin mutant was designed based on the amino acid sequence of Dps16 (SEQ ID NO.9), cloned into the E. coli expression vector pET22b plasmid with NdeI and BamHI restriction enzyme cutting sites, and the sequence was confirmed to be correct by DNA sequencing.

[0094] Protein expression: The plasmids obtained above were transformed into the expression strain BL21 (DE3), and grown in LB medium containing 100 mg / L kanamycin or ampicillin. IPTG was added at a final concentration of 0.5 mM and cultured at 25°C, 200 rpm for 12 h for protein induced expression.

[0095] Protein purification: Collect bacterial liquid, centrifuge at 4000g to collect bacterial cells, and resuspend the bacterial cells in 20mM Tris-HCl (pH 8.0) buffer. After high-pressure homogenization to break the bacteria, centrifuge at 12000g to remove E. coli debris, collect the supernatant and heat it in a 60℃ water bath for 10 minutes to denature and precipitate most of the impurities. Centrifuge at 12000g to collect the supernatant. The mutant supernatant is first purified by an anion exchange column Q-Sepharose Fast Flow, and then further purified by Superdex 200 molecular sieve.

[0096] Protein characterization: DLS and TEM were used to characterize the particle size and nanocage assembly of the ferritin mutant modified with the nucleic acid-binding peptide functional motif.

[0097] Analyze the experimental results, such as Fig. 9 As shown, the DLS and TEM results indicate that ferritin can be successfully self-assembled to form nanocages with a diameter of about 13 nm after being modified with nucleic acid-binding peptides.

[0098] Example 10 Verification of the loading level of ferritin cage nanocarrier modified with nucleic acid binding peptide functional motif

[0099] Add an equal volume of 10 mg / mL Dps16-modified protein cage nanocarrier solution to HCl solution (pH 1-3), mix thoroughly, and incubate at 4°C for 20-30 minutes to mediate protein cage disaggregation in a strong acid environment. Premix the siRNA solution with Na2CO3 / NaHCO3 solution (pH 9-11), then add it to the acid depolymerization system of the protein cage and mix thoroughly, neutralize the system to neutrality (pH 6.5-7.5), and incubate at 4°C for 2-3 hours. After taking out, ultrafilter the sample solution to remove free siRNA. Use the Qubit4Fluorometer microRNA kit to quantify the concentration of siRNA, use the BCA kit to quantify the concentration of protein, and calculate the siRNA loading rate of the protein. The experimental results were analyzed, and the results are as follows: Fig.10 As shown, the nucleic acid loading capacity of HFn(+)-Dps16 was improved compared with HFn.

[0100] Example 11 Construction, expression, purification and characterization of the recombinant plasmid of the ferritin cage nanocarrier modified with positively charged peptide functional motif

[0101] Design based on the modification of positively charged peptide functional motifs at the N-terminus or C-terminus of ferritin: The C-terminus of the wild-type ferritin and the positively charged mutant ferritin HFn(4+) constructed in Example 1 was truncated by genetic engineering and coupled with a functional motif with a positively charged peptide (SEQ ID NO.10-15). The cDNA sequence of the ferritin mutants connected with the amino acid sequence (SEQ ID NO.10-15) was designed and cloned into the E. coli expression vector pET22b plasmid with NdeI and BamHI restriction enzyme cutting sites, and the sequence was confirmed to be correct by DNA sequencing.

[0102] Protein expression: The plasmids obtained above were transformed into the expression strain BL21 (DE3), and grown in LB medium containing 100 mg / L kanamycin or ampicillin. IPTG was added at a final concentration of 0.5 mM and cultured at 25°C, 200 rpm for 12 h for protein induced expression.

[0103] Protein purification: Collect bacterial liquid, centrifuge at 4000g to collect bacterial cells, and resuspend the bacterial cells in 20mM Tris-HCl (pH 8.0) buffer. After high-pressure homogenization to break the bacteria, centrifuge at 12000g to remove E. coli debris, collect the supernatant and heat it in a 60℃ water bath for 10 minutes to denature and precipitate most of the impurities. Centrifuge at 12000g to collect the supernatant. The mutant supernatant is first purified by an anion exchange column Q-Sepharose Fast Flow, and then further purified by Superdex 200 molecular sieve.

[0104] Protein characterization: Native-PAGE electrophoresis and TEM were used to characterize the 24-mer assembly and protein cage morphology of the positively charged peptide functional motif-modified ferritin mutant, respectively.

[0105] Analyze the experimental results, such as Fig.11 As shown in the figure, on the Native-PAGE gel, the protein bands of the positively charged peptide functional motif-modified ferritin mutant and wild-type HFn are in similar positions, indicating that ferritin can smoothly self-assemble into 24-mers after modification with positively charged peptides. TEM analysis showed that the ferritin mutant modified with the positively charged peptide in the inner cavity has a good nanocage structure.

[0106] Example 12 Verification of the lysosomal escape function of ferritin nanocarriers modified with positively charged peptide functional motifs

[0107] U87MG was plated on a confocal dish, and Cy5-labeled HFn+(LR)3(SEQ ID NO.13), HFn+(LR)4(SEQ ID NO.14), and HFn+(LR)5(SEQ ID NO.15) were added, respectively, where the concentration of Cy5 was 1 μM. After 15, 30, and 120 min of co-incubation, the cells were taken out, lysosomes were stained with LAMP-1, cell nuclei were stained with DAPI, and different fluorescence inside U87MG cells was observed by CLSM to characterize the localization of drugs and lysosomes.

[0108] The experimental results were analyzed and the results were as follows Fig.12 As shown in the figure, the CLSM results show that HFn+(LR)3, HFn+(LR)4, and HFn+(LR)5 modified with cell-penetrating peptide functional motifs are not co-localized with lysosomes, indicating that after disassembly of this series of ferritin mutants in lysosomes, they can achieve lysosomal escape through the membrane-breaking effect of positively charged peptides.

[0109] Example 13 Construction, expression, purification and characterization of the cell-penetrating peptide functional motif-modified ferritin cage nanocarrier recombinant plasmid

[0110] Design based on the modification of the cell-penetrating peptide functional motif at the N-terminus or C-terminus of ferritin: by genetic engineering means, the N-terminus of some of the positive electrogenic mutant ferritins HFn(4+) in Example 1 was coupled with a functional motif of a cell-penetrating peptide, the C-terminus of some HFn(4+) was truncated and coupled with a functional motif of a cell-penetrating peptide, and the C-terminus of some other HFn(4+) was truncated and coupled with a functional motif of a cell-penetrating peptide at the N-terminus. The cDNA sequence of the ferritin mutants connected with the amino acid sequence (SEQID NO.16-31) was designed, cloned into the E. coli expression vector pET22b plasmid with NdeI and BamHI restriction enzyme cutting sites, and the sequence was confirmed to be correct by DNA sequencing.

[0111] Protein expression: The plasmids obtained above were transformed into the expression strain BL21 (DE3), and grown in LB medium containing 100 mg / L kanamycin or ampicillin. IPTG was added at a final concentration of 0.5 mM and cultured at 25°C, 200 rpm for 12 h for protein induced expression.

[0112] Protein purification: Collect bacterial liquid, centrifuge at 4000g to collect bacterial cells, and resuspend the bacterial cells in 20mM Tris-HCl (pH 8.0) buffer. After high-pressure homogenization, centrifuge at 12000g to remove E. coli debris, collect the supernatant and heat it in a 60℃ water bath for 10 minutes to denature and precipitate most of the impurities. Centrifuge at 12000g to collect the supernatant.

[0113] The supernatants of some mutants were initially purified by anion exchange column Q-Sepharose Fast Flow and then further purified by Superdex 200 molecular sieve.

[0114] The supernatants of some mutants were initially purified by Phenyl sepharose, a hydrophobic chromatography column, and then further purified by Superdex 200 molecular sieve.

[0115] The supernatants of some mutants were initially purified by nickel column and then further purified by Superdex 200 molecular sieve.

[0116] Protein characterization: TEM was used to characterize the 24-mer assembly and morphology of the ferritin mutant modified with the positively charged peptide functional motif.

[0117] The experimental results were analyzed and TEM showed that the series of mutants modified with cell-penetrating peptides (SEQ ID NO.16-31) all had good nanocage structures ( Fig.13Part of the cell penetrating peptide functional motif results are shown, with GALA6 at the C-terminus and H5WY at the N-terminus).

[0118] Example 14 Verification of the lysosomal escape function of ferritin nanocarriers modified with cell-penetrating peptide functional motifs

[0119] U87MG was plated on a confocal dish, and Cy5-labeled HFn(+)-GALA6 (SEQ ID NO.19) and H5WY-HFn(+) (SEQ ID NO.22) were added, respectively, where the concentration of Cy5 was 1 μM. After 15, 30, and 120 min of co-incubation, the cells were taken out, lysosomes were stained with LAMP-1, cell nuclei were stained with DAPI, and different fluorescence inside U87MG cells was observed by CLSM to characterize the localization of drugs and lysosomes.

[0120] The experimental results were analyzed and the results were as follows Fig.14 As shown in the figure, the CLSM results show that HFn(+)-GALA6 and H5WYG-HFn(+) modified with the cell-penetrating peptide functional motif do not co-localize with lysosomes, indicating that after disassembly of this series of ferritin mutants in lysosomes, the cell-penetrating peptide can penetrate the lysosomal membrane and achieve lysosomal escape function.

[0121] The sequence described in the present invention is as follows:

[0122] SEQ ID NO.1 Human heavy chain recombinant ferritin HFn

[0123] TTASTSQVRQNYHQDSEAAINRQINLELYASYVYLSMSYYFDDRDDVALKNFAKY

[0124] FLHQSHEEREHAEKLMKLQNQRGGRIFLQDIKKPDCDDWESGLNAMECALHLEKNV

[0125] NQSLLELHKLATDKNDPHLCDFIETHYLNEQVKAIKELGDHVTNLRKMGAPESGLAEY

[0126] LFDKHTLGDSDNES

[0127] SEQ ID NO.2-4 Inner surface amino acid residue mutation

[0128] HFn(4+)

[0129] TTASTSQVRQNYHQDSEAAINRQINLELYASYVYLSMSYYFDRDDVALKNFAKYFLHQSHKERRHAEKLMKLQNQRGGRIFLQDIKKPDCDDWESGLNAMECALHLEKNVNQSLLELHKLATDKNDPHLCDFIETHYLNKQVKAIKKLGDHVTNLRKMGAPESGLAEYLFDKHTLGDSDNES

[0130] HFn(5+)

[0131] TTASTSQVRQNYHQDSEAAINRQINLELYASYVYLSMSYYFDRDDVALKNFAKYFLHQSHKERRHAEKLMKLQNQRGGRIFLQDIKKPDCDDWESGLNAMECALHLEKNVNQSLLELHKLATDKNDPHLCDFIETHYLNKQVKAIKKLGDHVTNLRKMGAPESGLAEYLFDKHTLGDSDNKS

[0132] HFn(7+)

[0133] TTASTSQVRQNYHQDSEAAINRQINLELYASYVYLSMSYYFDRDDVALKNFAKYFLHQSHKERRHAEKLMKLQNQRGGRIFLQDIKKPDCDDWESGLNAMECALHLEKNVNQSLLELHKLATDKNDPHLCDFIETHYLNKQVKAIKKLGDHVTNLRKMGAPESGLAEYLFDKHTLGKSKNKS

[0134] The inner surface amino acid residues of SEQ ID NO.5-8 are mutated and the C-terminus is truncated to positions 179, 174, 162, and 159

[0135] tHFn(+) 1-179

[0136] TTASTSQVRQNYHQDSEAAINRQINLELYASYVYLSMSYYFDRDDVALKNFAKYFLHQSHKERRHAEKLMKLQNQRGGRIFLQDIKKPDCDDWESGLNAMECALHLEKNVNQSLLELHKLATDKNDPHLCDFIETHYLNKQVKAIKKLGDHVTNLRKMGAPESGLAEYLFDKHTLGDSD

[0137] tHFn(+) 1-174

[0138] TTASTSQVRQNYHQDSEAAINRQINLELYASYVYLSMSYYFDRDDVALKNFAKYFLHQSHKERRHAEKLMKLQNQRGGRIFLQDIKKPDCDDWESGLNAMECALHLEKNVNQSLLELHKLATDKNDPHLCDFIETHYLNKQVKAIKKLGDHVTNLRKMGAPESGLAEYLFDKHT

[0139] tHFn(+) 1-162

[0140] TTASTSQVRQNYHQDSEAAINRQINLELYASYVYLSMSYYFDRDDVALKNFAKYFLHQSHKERRHAEKLMKLQNQRGGRIFLQDIKKPDCDDWESGLNAMECALHLEKNVNQSLLELHKLATDKNDPHLCDFIETHYLNKQVKAIKKLGDHVTNLRKMGAPE

[0141] tHFn(+) 1-159

[0142] TTASTSQVRQNYHQDSEAAINRQINLELYASYVYLSMSYYFDRDDVALKNFAKYFLHQSHKERRHAEKLMKLQNQRGGRIFLQDIKKPDCDDWESGLNAMECALHLEKNVNQSLLELHKLATDKNDPHLCDFIETHYLNKQVKAIKKLGDHVTNLRKMG

[0143] SEQ ID NO.9 Nucleic Acid-Binding Functional Peptide Dps16

[0144] QSTEKGAADKARRKSA

[0145] SEQ ID NO.10-15 Positively Charged Peptides

[0146] (LR)1: LRLR

[0147] (LR)2: LRLRGGLRLR

[0148] (LR)3: LRLRGGLRLRGGLRLR

[0149] (LR)4: LRLRGGLRLRGGLRLRGGLRLR

[0150] (LR)5: LRLRGGLRLRGGLRLRGGLRLRGGLRLR

[0151] (LR)6: LRLRGGLRLRGGLRLRGGLRLRGGLRLRGGLRLR

[0152] SEQ ID NO.16 - 25 Cell - penetrating peptides

[0153] GALA: WEAALAEALAEALAEHLAEALAEALEALAA

[0154] GALA4: LAEALAEHLAEALAE

[0155] GALA5: LAEALAEHLAEALAEALAE

[0156] GALA6: LAEALAEHLAEALAEALAEALAE

[0157] GALA7: LAEALAEHLAEALAEALAEALAEALAE

[0158] H5WYG: GLFHAIAHFIHGGWHGLIHGWY

[0159] H5WY: HHHHHWY

[0160] YWH5: YWHHHHH

[0161] H5: HHHHH

[0162] H(GH3)4: HHHHHGHHHGHHHGHHHG

[0163] SEQ ID NO.26 - 31 Positively charged cell - penetrating peptides

[0164] TAT: GRKKRRQRRR

[0165] Penetratin: RQIKIWFQNRRMKWKK

[0166] CADY: GLWRALWRLLRSLWRLLWRA

[0167] (KH3)4: KHHHKHHHKHHHKHHH

[0168] H(KH3)3: HHHHHKHHHKHHHK

[0169] Mu:MRRAHHRRRRASHRRMRGG

[0170] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. These modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the present invention, and they should all be included in the scope of the claims and specification of the present invention.

Claims

1. A method for preparing a caged nanocarrier for targeted delivery of siRNA, characterized in that: include: (A) Mutating negatively or uncharged amino acids spatially distributed on the inner surface of ferritin into positively charged amino acids; And any one or more of the following steps: (B), coupling the N-terminus of the ferritin to a functional peptide having nucleic acid affinity; (C), coupling the N-terminus of the ferritin to a functional peptide that promotes lysosomal escape; (D), truncating the E helix at the C-terminus of the ferritin; (E), coupling the C-terminus of the ferritin to a functional peptide having nucleic acid affinity; (F) The C-terminus of the ferritin is coupled to a functional peptide that promotes lysosomal escape.

2. The preparation method according to claim 1, characterized in that: In step (A), the mutation sites of the ferritin are Glu61, Glu64, Glu140, Glu147, D177, D179 and E181.

3. The preparation method according to claim 1, characterized in that: In step (A), the positively charged amino acid is selected from any one of arginine, lysine and histidine.

4. The preparation method according to claim 1, characterized in that: Step (B) is any of the following: (B1) coupling the N-terminus of the ferritin with a functional motif having a nucleic acid binding peptide; (B2) coupling the N-terminus of the ferritin with a functional motif having a positively charged peptide; Step (C) is: coupling the N-terminus of the ferritin with a functional motif having a cell-penetrating peptide; Step (E) is any of the following: (E1) coupling the C-terminus of the ferritin with a functional motif having a nucleic acid binding peptide; (E2) coupling a functional motif with a positively charged peptide to the C-terminus of the ferritin; Step (F) is: coupling the C-terminus of the ferritin with a functional motif of a cell-penetrating peptide.

5. The preparation method according to claim 4, characterized in that: In step (B1) and step (E1), the functional motif sequence of the nucleic acid binding peptide is as shown in SEQ ID NO.9; In step (B2) and step (E2), the functional motif sequence with positively charged peptide is shown as SEQ ID NO.10-15; In step (C) and step (F), the functional motif sequence with the cell penetrating peptide is shown as SEQ ID NO.16-31.

6. A ferritin cage nanocarrier for targeted delivery of siRNA prepared by the preparation method according to any one of claims 1 to 5.

7. The ferritin cage nanocarrier according to claim 6, characterized in that: The siRNA loading capacity of the ferritin cage nanocarrier is 2-3 nucleic acid molecules per protein cage.

8. A siRNA delivery system, characterized in that The invention comprises siRNA and the ferritin cage nanocarrier for targeted delivery of siRNA according to claim 6 or 7.

9. The siRNA delivery system according to claim 8, characterized in that The molar mass ratio of the ferritin cage nanocarrier to the siRNA is 1:(1-5).

10. A method for encapsulating siRNA using the siRNA delivery system according to claim 8 or 9, characterized in that: The following steps are involved: S1. Preparation and purification of ferritin cage nanocarriers for siRNA delivery system; S2, dissolve siRNA in DEPC water; S3, adding the ferritin nanocage carrier obtained in step S1 to an acidic buffer solution of pH 1-3, and incubating at 4° C. for 20-30 minutes to obtain an acid depolymerization system; S4, adding the siRNA solution prepared in step S2 to an alkaline buffer solution of pH 9-11, mixing evenly, adding the acid depolymerization system obtained in step S3, and incubating at 4° C. for 2-3 hours to reassemble the ferritin nanocage with the siRNA loaded in the inner cavity.

11. Use of the caged nanocarrier for targeted siRNA delivery according to claim 6 or 7, or the siRNA delivery system according to claim 8 or 9 in siRNA delivery.

12. Use of the ferritin cage nanocarrier for targeted siRNA delivery according to claim 6 or 7, and the siRNA delivery system according to claim 8 or 9 in the preparation of drugs for treating tumors, viral infections, central nervous system diseases, and cardiovascular diseases.

Citation Information

Cited By

  • Assembly type protein nano-carrier CABRi for targeted delivery of small interfering nucleic acid as well as preparation method and application of assembly type protein nano-carrier CABRi

    CN119700704A

  • An assembled protein nanocarrier CABRi for targeted delivery of small interfering nucleic acids, its preparation method and applications

    CN119700704B

  • Cage-like nanocarrier for targeted delivery of sirna, and preparation method therefor and use thereof

    WO2025251574A1