Temperature control method for solar cell sintering furnace and solar cell sintering furnace
By monitoring the empty furnace state in the solar cell sintering furnace and raising the sintering zone temperature when the cell enters, the inadequate sintering and cloud black problems caused by temperature fluctuations in the early stage of recombination production are solved, and stable temperature control is achieved.
Patent Information
- Application Number
- CN202410995850.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-08
AI Technical Summary
In the early stages of the production of solar cell sintering furnace re-machine, the furnace temperature fluctuations caused the battery cell to be insufficient sintered, the contact resistance increased, and frequent cloud-black quality problems.
By monitoring whether the sintering furnace is in the empty furnace state, when the solar cell is detected, the temperature of the high-temperature sintering zone is raised to a compensation temperature higher than the process temperature, and after the battery passes, it will be restored to the process temperature to ensure the temperature in the furnace. Stablize.
It effectively avoids temperature fluctuations in the early stage of re-machine production, ensures that the temperature experienced by the battery cells in each temperature zone is consistent with continuous production, and solves the problems of insufficient sintering and cloud blacking.
Smart Images

Figure CN118912927A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a temperature control method, in particular to a method for controlling the furnace temperature of a sintering furnace for sintering solar cell sheets and a solar cell sheet sintering furnace. Background Art
[0002] At present, crystalline silicon solar cells use sintering furnaces to form metal contacts at high temperatures. The main functional areas of the sintering furnace from feeding to discharging include: feeding-low temperature drying area-medium temperature pre-firing area-high temperature sintering area-cooling area-discharging. During the sintering process of crystalline silicon cells, organic matter volatilization, glass material dissolution, electrode formation, etc. occur, and the temperature has a greater impact on the quality of the cell.
[0003] In the case of replacing or wiping the screen, etc., which prevents continuous production, the sintering furnace needs to be restarted after the furnace is empty. At present, in the initial stage of re-restarting production, the furnace temperature of the sintering furnace in the empty furnace state first reaches the set temperature, the heater stops working, and the battery cells entering the furnace of the sintering furnace quickly absorb a large amount of heat, causing the temperature in the furnace to quickly drop below the set temperature, resulting in insufficient sintering of the battery cells entering the roller sintering furnace in the initial stage of re-starting production, increased contact resistance, and frequent cloud black quality problems. Summary of the invention
[0004] In order to avoid or at least reduce the temperature fluctuation in the furnace of the sintering furnace in the initial stage of the re-production, the present invention provides a temperature control method for a solar cell sintering furnace, wherein the sintering furnace includes a low-temperature drying zone, a medium-temperature sintering zone, a high-temperature sintering zone and a temperature reduction cooling zone, and the method includes:
[0005] S1. Monitor whether the sintering furnace is in an empty furnace state;
[0006] S2, when it is monitored that the sintering furnace is in an empty furnace state, in response to detecting that the solar cell enters the feed port of the sintering furnace, the set temperature in the high temperature sintering zone of the sintering furnace is increased to a compensation temperature (T0) and maintained for a predetermined compensation time period, and the compensation temperature (T0) is higher than the process temperature (T1) of the high temperature sintering zone;
[0007] S3, restoring the set temperature in the high temperature sintering zone of the sintering furnace to the process temperature (T1);
[0008] S4. Repeat steps S1 to S3.
[0009] In some embodiments, monitoring whether the sintering furnace is in an empty furnace state includes: monitoring a slice-in count and a slice-out count of the sintering furnace, and determining that the sintering furnace is in an empty furnace state in response to the slice-out count being equal to the slice-in count for a predetermined waiting period of time.
[0010] In some embodiments, the predetermined waiting period is determined according to the following formula:
[0011] t0≥L / v×1.5
[0012] Wherein, t0 is a predetermined waiting time period, L is a distance between a feed port and a discharge port of the sintering furnace, and v is a moving speed of the solar cell in the sintering furnace.
[0013] In some embodiments, the compensation temperature (T0) is in a range of 13 to 17°C higher than the process temperature (T1).
[0014] In some embodiments, the predetermined compensation time period is determined according to the following formula:
[0015] L / v+80s≥t1≥L / v+40s
[0016] Wherein, t1 is a predetermined compensation time period, L is a distance between a feed port and a discharge port of the sintering furnace, and v is a moving speed of the solar cell in the sintering furnace.
[0017] Another aspect of the present invention provides a solar cell sintering furnace, which includes a furnace, a plurality of rollers arranged in the furnace, and a plurality of temperature zones. The plurality of temperature zones include a low-temperature drying zone, a medium-temperature sintering zone, a high-temperature sintering zone, and a temperature reduction cooling zone arranged in sequence in the furnace. Each temperature zone includes a heater. The furnace has a feed port and a discharge port.
[0018] The sintering furnace further includes a control system, which includes a feed sensor arranged at the feed port, a discharge sensor arranged at the discharge port, and a controller communicatively connected to the feed sensor, the discharge sensor and the heater.
[0019] The controller is configured to perform the following steps:
[0020] S1, monitoring whether the sintering furnace is in an empty furnace state;
[0021] S2, when it is monitored that the sintering furnace is in an empty furnace state, in response to detecting that the solar cell enters the feed port of the sintering furnace, the set temperature in the high temperature sintering zone of the sintering furnace is increased to a compensation temperature (T0) and maintained for a predetermined compensation time period, wherein the compensation temperature (T0) is higher than the process temperature (T1) of the high temperature sintering zone;
[0022] S3, restoring the set temperature in the high temperature sintering zone of the sintering furnace to the process temperature (T1);
[0023] S4. Repeat steps S1 to S3.
[0024] In some embodiments, the feed sensor is configured to sense the sheet input count of the sintering furnace, the discharge sensor is configured to sense the sheet output count of the sintering furnace, and the controller is configured such that when the sheet output count is equal to the sheet input count and lasts for a predetermined waiting period of time, the sintering furnace is in an empty furnace state.
[0025] In some embodiments, each temperature zone includes an upper temperature zone and a lower temperature zone which are arranged above and below the roller conveyor opposite to each other, and a heater is respectively disposed in the upper temperature zone and the lower temperature zone.
[0026] The temperature control method provided by the present invention detects that the sintering furnace is in an empty furnace state, and raises the temperature in the high-temperature sintering zone to a compensation temperature higher than the process temperature when the solar cell enters the feed port of the sintering furnace, thereby solving the problem of black cloud on the solar cell in the early stage of sintering furnace production. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 Schematic diagram of temperature zone distribution of a solar cell sintering furnace according to the present invention;
[0028] Figure 2 It is a comparison diagram of the temperature distribution curve of the empty furnace re-production using the temperature control method for the solar cell sintering furnace of the present invention, the temperature distribution curve of the empty furnace re-production without using the temperature control method for the solar cell sintering furnace of the present invention, and the temperature distribution curve of continuous production;
[0029] Figure 3 The figure is a flow chart of a temperature control method for a solar cell sintering furnace according to the present invention. DETAILED DESCRIPTION
[0030] The temperature control method for a solar cell sintering furnace and the solar cell sintering furnace disclosed in the present invention are further described in detail below in conjunction with the accompanying drawings and specific embodiments. The advantages and features of the present invention will become clearer according to the following detailed description and claims. It should be noted that the accompanying drawings are in a very simplified form and use non-precise ratios, which are only used for the purpose of conveniently and clearly assisting in explaining the embodiments of the present invention.
[0031] Reference Figure 1 An exemplary solar cell sintering furnace according to the first aspect of the present invention is described, for example, a roller type sintering furnace. The sintering furnace comprises a furnace, a plurality of rollers 22 arranged in the furnace, and a plurality of temperature zones. The furnace has a feed port and a discharge port.
[0032] A plurality of rollers 22 are arranged parallel to each other in the furnace, which can carry the battery sheet 21 and drive the battery sheet 21 to move thereon. The rollers 22 can be implemented as ceramic rollers, for example, which move the battery sheet 21 from the feed port to the discharge port at a preferably constant rate.
[0033] The multiple temperature zones, such as Figure 1 The temperature zones 1-18 shown in the figure are arranged adjacent to each other in sequence from the feed port to the discharge port, and include a low-temperature drying zone, a medium-temperature sintering zone, a high-temperature sintering zone and a temperature reduction cooling zone from the feed port to the discharge port, and each temperature zone includes a heater 23.
[0034] Further, each temperature zone may include an upper temperature zone and a lower temperature zone which are arranged above and below the roller 22 opposite to each other, and each of the upper temperature zone and the lower temperature zone is provided with a heater 23, such as an infrared lamp.
[0035] In the attached Figure 1 In the embodiment shown, the sintering furnace has 18 upper temperature zones and 18 lower temperature zones. Figure 2 , temperature zones 1 to 6 and 1 to 6 correspond to low-temperature drying zones, temperature zones 7 to 12 and 7 to 12 correspond to medium-temperature sintering zones, temperature zones 13 to 15 and 13 to 15 correspond to high-temperature sintering zones (600-800°C), and temperature zones 16 to 18 and 16 to 18 correspond to cooling zones. Among them, the temperature in the low-temperature drying zone is less than 400°C, in which the evaporation and combustion of the slurry organic solvent and organic binder mainly occur; the temperature in the medium-temperature sintering zone is between 400-600°C, in which the glass begins to melt and the silver particles begin to aggregate; the temperature in the high-temperature sintering zone is between 600-800°C, in which silver, silicon, and glass begin to react to form a silver-silicon alloy; in the cooling zone, the silver particles crystallize and grow on the surface of the silicon wafer.
[0036] The sintering furnace also includes a control system, which includes a feed sensor 19 arranged at the feed port, a discharge sensor 20 arranged at the discharge port, and a controller 24 connected to the feed sensor 19, the discharge sensor 20 and each heater 23 in communication. The controller 24 can be implemented as a PLC, a single-chip microcomputer, a microprocessor, a microcontroller, etc. The controller 24 can be configured to perform mathematical operations and other calculation functions. The controller 24 receives counting signals from the feed sensor 19 and the discharge sensor 20, and individually controls the heating operation of each heater 23 and thereby controls the temperature of each temperature zone.
[0037] The control system may further include a plurality of temperature sensors arranged in the furnace, preferably a plurality of temperature sensors arranged in each temperature zone, which sense the temperature in the corresponding temperature zone. More particularly, the control system includes a plurality of temperature sensors arranged in each upper temperature zone and lower temperature zone.
[0038] The feed sensor 19 is configured to monitor the count of the battery cells 21 passing through the feed port to obtain the feed count; the discharge sensor 20 is configured to monitor the count of the battery cells 21 passing through the discharge port to obtain the discharge count. The feed sensor 19 and the discharge sensor 20 are preferably configured to communicate with the controller 24 in real time.
[0039] The controller 24 receives the sheet-in counting information from the feed sensor 19 and the sheet-out counting information from the sheet-out sensor 20 , and can determine the number of battery cells 21 in the furnace by subtracting the sheet-out counting from the sheet-in counting.
[0040] According to another aspect of the present disclosure, a temperature control method for a solar cell sintering furnace is provided to avoid or at least reduce temperature fluctuations in the furnace of the sintering furnace in the early stage of re-production. The temperature control method can be implemented by the solar cell sintering furnace according to the first aspect of the present invention.
[0041] Reference Figure 3 A temperature control method for a solar cell sintering furnace according to the present invention is described.
[0042] The temperature control method may include the following steps:
[0043] S1. Monitor whether the sintering furnace is in an empty furnace state.
[0044] The empty furnace state means that there is no battery cell 21 in the furnace. In particular, monitoring whether the sintering furnace is in the empty furnace state includes monitoring the cell entry count and cell exit count of the sintering furnace via the feed sensor 19 and the discharge sensor 20, and determining that the sintering furnace is in the empty furnace state in response to the cell exit count being equal to the cell entry count for a predetermined waiting period of time.
[0045] Specifically, when the sheet-in count is equal to the sheet-out count and continues for a predetermined waiting period of time, it is determined that the sintering furnace is in an empty furnace state.
[0046] The predetermined waiting time period can be determined according to the following formula:
[0047] t0≥L / v×1.5
[0048] Among them, t0 is the predetermined waiting time period, L is the distance between the feed port and the discharge port of the sintering furnace (i.e., the length of the furnace), v is the moving speed of the solar cell in the sintering furnace, and 1.5 is the waiting coefficient.
[0049] That is, if the battery cell 21 is not detected in the sintering furnace within a period of time greater than or equal to 1.5 times, preferably equal to 1.5 times, the time taken for the battery cell 21 to pass through the sintering furnace, the sintering furnace is determined to be in an empty furnace state.
[0050] For example, the distance L between the feed port and the discharge port of the sintering furnace can be 19.7 m, the roller 22 carries the solar cell 21 in the sintering furnace at a moving speed of 15 m / min, the cell 21 takes about 80 s to move from the inlet to the outlet, and t0 is greater than or equal to about 120 s.
[0051] The step of monitoring whether the sintering furnace is in an empty furnace state can be implemented by the control system. The controller 24 determines the number of battery cells 21 present in the furnace by calculating the difference between the incoming cell count and the outgoing cell count. When the outgoing cell count is equal to the incoming cell count, that is, the difference is zero, and continues for the above-mentioned predetermined waiting time period, the controller 24 can determine that there are no battery cells in the furnace, that is, the sintering furnace is in an empty furnace state.
[0052] S2. When it is monitored that the sintering furnace is in an empty furnace state, in response to detecting that the solar cell sheet enters the feed port of the sintering furnace, the set temperature in the high-temperature sintering zone of the sintering furnace is increased to a compensation temperature (T0) and maintained for a predetermined compensation time period, and the compensation temperature (T0) is higher than the process temperature (T1) of the high-temperature sintering zone.
[0053] Reference Figure 2 , which respectively show the temperature distribution of the furnace of the sintering furnace after the battery cell 21 passes through the continuous production and empty furnace restart. It is worth noting that when the battery cell 21 passes through the high-temperature sintering zone (upper 13 / upper 14 / upper 15, lower 13 / lower 14 / lower 15 temperature zone), the temperature of the high-temperature sintering zone is affected by the heat absorption of the battery cell 21 and quickly drops to a temperature lower than that in the continuous production case.
[0054] In order to compensate for the temperature drop of the high-temperature sintering zone caused by the heat absorption of the battery cell 21, the temperature of the high-temperature sintering zone is set to a compensation temperature (T0) higher than the process temperature (T1), so that after the battery cell 21 passes through the high-temperature sintering zone and absorbs heat, the temperature of the high-temperature sintering zone is reduced to the process temperature (T1) due to the heat absorption of the battery cell 21. This can solve the problem that the battery cell 21 entering the furnace of the sintering furnace in the initial stage of the empty furnace restart quickly absorbs a large amount of heat, causing the temperature in the furnace to quickly drop to below the set temperature; thereby eliminating the quality problems of insufficient sintering of the battery cell 21 entering the roller sintering furnace, increased contact resistance, and frequent occurrence of black clouds.
[0055] When the sintering furnace is detected to be in an empty furnace state, the controller 24 continuously receives the feeding counting signal of the feeding sensor 19. When the feeding sensor 19 senses the battery cell 21, it transmits the feeding counting signal to the controller 24. The controller 24 controls the set temperature of the high-temperature sintering zone to be raised to the compensation temperature (T0) higher than the process temperature (T1). The heater 23 of the high-temperature sintering zone raises the temperature of the high-temperature sintering zone to the compensation temperature (T0). When the battery cell 21 undergoes this high-temperature sintering, it takes away part of the heat, causing the temperature of the high-temperature sintering zone to drop, especially to the process temperature (T1).
[0056] Reference Figure 2 , through the temperature curve process evaluation, it is verified that the compensation temperature (T0) value required for the high-temperature sintering zone is obtained. In particular, the temperature of the high-temperature sintering zone can be reduced by up to 15°C due to the heat absorption of the battery cell 21. Accordingly, the compensation temperature (T0) can be set to be 13 to 17°C higher than the process temperature (T1), especially 15°C, so that when the battery cell 21 passes through the high-temperature sintering zone, it takes away part of the heat, causing the temperature of the high-temperature sintering zone to drop by 15°C to close to the process temperature (T1), preferably to the process temperature (T1). At this time, the temperature experienced by the battery cell 21 entering the sintering furnace at the beginning of production after the production line is shut down is consistent with that in the continuous production case, such as Figure 2 As shown, the problem of black clouding of battery cells in the early stage of sintering furnace production is eliminated.
[0057] Alternatively, the predetermined compensation time period may be determined according to the following formula:
[0058] L / v+80s≥t1≥L / v+40s
[0059] In particular,
[0060] t1=L / v+60s
[0061] Wherein, t1 is a predetermined compensation time period, L is a distance between a feed port and a discharge port of the sintering furnace, and v is a moving speed of the solar cell in the sintering furnace.
[0062] For example, the distance L between the inlet and outlet of the sintering furnace may be 19.7 m, the roller 22 carries the solar cell 21 in the sintering furnace at a moving speed of 15 m / min, the solar cell 21 takes about 80 seconds to move from the inlet to the outlet, and t1 is in the range of about 120 s to about 160 s. In particular, t1 is 140 s.
[0063] S3. Restoring the set temperature in the high temperature sintering zone of the sintering furnace to the process temperature (T1).
[0064] After the cell 21 enters the sintering furnace, the sintering furnace leaves the empty furnace state and enters the continuous production state. During the continuous production, the heater 23 of the high temperature sintering zone continues to work, and the heat absorption of the cell 21 entering the high temperature sintering zone will not cause a significant drop in the temperature in the high temperature sintering zone. Therefore, after step S2, the set temperature in the high temperature sintering zone of the sintering furnace is restored from the compensation temperature (T0) to the process temperature (T1) via the controller 24.
[0065] S4. Repeat steps S1 to S3.
[0066] The actual operation process of the temperature control method for a solar cell sintering furnace according to the present invention is described below.
[0067] Taking the sintering furnace shown as an example, the length of the sintering furnace is 19.7 m, the roller 22 carries the solar cell 21 and moves at a speed of 15 m / min in the sintering furnace, and it takes about 80 s for the first solar cell 21 to move from the feed port to the discharge port.
[0068] The feed sensor 19 senses the feeding of the cell 21, transmits the feeding count to the controller 24, and transports the cell 21 through the roller 22. The discharge sensor 20 senses the discharge of the cell 21, and transmits the discharge count to the controller 24. The controller 24 calculates the number of cells 21 in the sintering furnace based on the feeding count and the discharge count. If the feeding count and the discharge count are equal and last for a predetermined waiting time period greater than or equal to about 120 seconds, it means that the sintering furnace is in an empty furnace state.
[0069] When the sintering furnace is empty, the feed sensor 19 senses that the battery cell 21 enters the sintering furnace and transmits a feed signal to the controller 24. The controller 24 controls the heater 23 in the high-temperature sintering zone to increase its set temperature (for example, 13-17°C, especially 15°C) to the compensation temperature. When the battery cell 21 passes through the high-temperature sintering zone, it takes away some heat, causing the temperature in the furnace to drop by 15°C to close to the process temperature.
[0070] After a predetermined compensation period of 40s to 80s, preferably 60s, after the discharge sensor 20 senses the discharge of the battery cell 21, the high temperature sintering zone of the sintering furnace returns to the process temperature, and the total heating time is about 120s to 160s.
[0071] During the whole process, the temperature in the sintering furnace is kept near the set temperature, especially not lower than the set temperature, in order to reduce the quality problems such as insufficient sintering of the battery cell 21, increased contact resistance, and clouding caused by the temperature reduction in the high-temperature sintering zone.
[0072] In the description of the present invention, it should be noted that the terms "center", "up", "down", "left", "right", "vertical", "horizontal", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction. Therefore, they should not be understood as limitations on the present invention.
[0073] In addition, the technical features involved in the different embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0074] As used in this disclosure and the appended claims, the singular forms "a", "an", "said", and "the" are intended to include the plural forms as well, unless the context clearly indicates otherwise. It should also be understood that the term "and / or" as used herein refers to and encompasses any and all possible combinations of one or more of the associated listed items.
[0075] Obviously, those skilled in the art can make various changes and modifications to the temperature control method for solar cell sintering furnace and solar cell sintering furnace disclosed in the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A temperature control method for a solar cell sintering furnace, wherein the sintering furnace comprises a low-temperature drying zone, a medium-temperature sintering zone, a high-temperature sintering zone and a cooling zone in sequence, It is characterized in that The following steps are involved: S1, monitoring whether the sintering furnace is in an empty furnace state; S2, when it is monitored that the sintering furnace is in an empty furnace state, in response to detecting that the solar cell enters the feed port of the sintering furnace, raising the set temperature in the high temperature sintering zone of the sintering furnace to a compensation temperature and continuing for a predetermined compensation time period, wherein the compensation temperature is higher than the process temperature of the high temperature sintering zone; S3, restoring the set temperature in the high temperature sintering zone of the sintering furnace to the process temperature; S4. Repeat steps S1 to S3.
2. The temperature control method according to claim 1, It is characterized in that The monitoring of whether the sintering furnace is in an empty furnace state comprises: The sheet-in count and the sheet-out count of the sintering furnace are monitored, and in response to the sheet-out count being equal to the sheet-in count for a predetermined waiting period of time, it is determined that the sintering furnace is in an empty furnace state.
3. The temperature control method according to claim 2, It is characterized in that The predetermined waiting time period is determined according to the following formula: t 0 ≥L / v×1.5 Among them, t 0 is the predetermined waiting time period, L is the distance between the feed port and the discharge port of the sintering furnace, and v is the moving speed of the solar cell in the sintering furnace.
4. The temperature control method according to claim 1, It is characterized in that The compensation temperature is in the range of 13 to 17° C. higher than the process temperature.
5. The temperature control method according to claim 1, It is characterized in that The predetermined compensation time period is determined according to the following formula: L / v+80s≥t 1 ≥L / v+40s Among them, t 1 is the predetermined compensation time period, L is the distance between the feed port and the discharge port of the sintering furnace, and v is the moving speed of the solar cell in the sintering furnace.
6. A solar cell sintering furnace, It is characterized in that The sintering furnace comprises a furnace, a plurality of rollers arranged in the furnace, and a plurality of temperature zones, wherein the plurality of temperature zones comprise a low-temperature drying zone, a medium-temperature sintering zone, a high-temperature sintering zone, and a temperature reduction cooling zone sequentially arranged in the furnace, each temperature zone comprises a heater, and the furnace has a feed port and a discharge port; The sintering furnace further includes a control system, the control system including a feed sensor disposed at the feed port, a discharge sensor disposed at the discharge port, and a controller communicatively connected to the feed sensor, the discharge sensor and the heater; The controller is configured to perform the following steps: S1, monitoring whether the sintering furnace is in an empty furnace state; S2, when it is monitored that the sintering furnace is in an empty furnace state, in response to detecting that the solar cell enters the feed port of the sintering furnace, raising the set temperature in the high temperature sintering zone of the sintering furnace to a compensation temperature and continuing for a predetermined compensation time period, wherein the compensation temperature is higher than the process temperature of the high temperature sintering zone; S3, restoring the set temperature in the high temperature sintering zone of the sintering furnace to the process temperature; S4. Repeat steps S1 to S3.
7. The solar cell sintering furnace according to claim 6, It is characterized in that The feed sensor is configured to sense a sheet feed count of the sintering furnace, the discharge sensor is configured to sense a sheet discharge count of the sintering furnace, and the controller is configured to determine that the sintering furnace is in an empty furnace state when the sheet discharge count is equal to the sheet feed count and lasts for a predetermined waiting period of time.
8. The solar cell sintering furnace according to claim 7, It is characterized in that The predetermined waiting time period is determined according to the following formula: t 0 ≥L / v×1.5 Among them, t 0 is the predetermined waiting time period, L is the distance between the feed port and the discharge port of the sintering furnace, and v is the moving speed of the solar cell in the sintering furnace.
9. The solar cell sintering furnace according to claim 6, It is characterized in that The compensation temperature is in the range of 13 to 17° C. higher than the process temperature.
10. The solar cell sintering furnace according to claim 6, It is characterized in that Each of the temperature zones includes an upper temperature zone and a lower temperature zone which are arranged above and below the roller table opposite to each other, and each of the upper temperature zone and the lower temperature zone is provided with the heater.
Citation Information
Cited By
Temperature control method of silk screen sintering furnace
CN119937674A
Solar cell sintering furnace, preparation method of solar cell and solar cell
CN121185055A
Solar cell sintering furnace, solar cell manufacturing method, and solar cell
CN121185055B
High-purity fused quartz crucible sintering furnace control system and method
CN122062485A
A control system and method for a high-purity fused silica crucible sintering furnace
CN122062485B