Device for in-situ test of Bi-system superconducting flat wire and use method
The non-destructive test of Bi-system superconducting flat wire is realized through the pressure electrode connection device, which solves the problem of uneven current-carrying performance, improves the accuracy and efficiency of the test, and simplifies the process of process improvement determination.
Patent Information
- Application Number
- CN202411306925.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-19
- Publication Date
- 2024-11-15
AI Technical Summary
The preparation process of Bi-type superconducting flat wires is complicated, resulting in uneven current-carrying performance. The existing test methods require multiple sample methods to obtain accurate results, which increases the workload and the difficulty of promoting the development of superconducting wire strips.
Using a pressure electrode connection device, the current and potential pressure electrodes on the insulating plate are connected to the Bi-system superconducting flat wire to achieve lossless and pollution-free critical current testing, avoiding the impact of solder on process improvement, and directly conducting samples at the same position. Modification and testing.
Accurately determine the impact of process improvements on current-carrying performance, reduce sample number and experimental time, improve the accuracy and efficiency of testing, and avoid solder contamination and ceramic core damage.
Smart Images

Figure CN118962227A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of in-situ testing of Bi-based superconducting flat wires, and in particular relates to a device and a method for in-situ testing of Bi-based superconducting flat wires. Background Art
[0002] Bi-based superconducting flat wires have broad application prospects and have been demonstrated in superconducting cables, superconducting transformers, fault current limiters, etc. However, to truly achieve large-scale applications, it is necessary to greatly improve the current-carrying performance of superconducting wire strips, or reduce the cost of superconducting tapes without reducing the current-carrying performance. Therefore, modifying superconducting wire strips to improve the current-carrying performance or reduce the cost of Bi-based superconducting flat wires is the most important task in product research and development. In order to determine whether the current-carrying performance of superconducting wire strips has changed before and after process improvements, the standard four-lead method is used to test the superconducting critical current of samples before and after the improvement, and the difference in critical current is compared to determine the effectiveness of the process improvement.
[0003] The general test process is: solder two current leads and two potential leads to the superconducting wire strip respectively with solder, energize the superconducting wire strip through the current leads, and detect the potential of the current on the Bi-based superconducting flat wire through the potential leads. According to the magnitude of the potential, it is determined whether the sample is in a superconducting or non-superconducting state, and finally the magnitude of the critical superconducting current is obtained. Because solder will remain on the surface of the sample after the test (the current lead and the potential lead need to be soldered), the residual solder will affect the process improvement of the superconducting wire strip. Therefore, generally, sample one is taken at position one for critical current test, and then sample two is taken at the adjacent position for process improvement, and then the improved sample is tested for critical current, and then compared to finally obtain the corresponding results.
[0004] But we encountered a problem during the process: Bi-based superconducting flat wire is a complex composite material composed of multiple ceramic superconducting cores wrapped with metallic silver, and its preparation process is complicated, which can easily cause uneven distribution of superconducting wire strips. The difference in current carrying performance between adjacent positions is even more than 20%. When the current carrying performance of superconducting wire strips changes by less than 20%, it will lead to misjudgment of process optimization. We often solve this problem through the multi-sample method, but the number of samples must reach dozens to obtain more accurate results (the results obtained from five samples are still unreliable), which greatly increases the workload of the experiment and is extremely unfavorable to the development of superconducting wire strips.
[0005] Therefore, a device and method for in-situ testing of Bi-based superconducting flat wires are needed. Summary of the invention
[0006] The technical problem to be solved by the present invention is to provide a device for in-situ testing of Bi-based superconducting flat wires in view of the deficiencies of the above-mentioned prior art. The device uses pressure electrodes to realize the connection between the current lead and the potential lead and the Bi-based superconducting flat wire, avoiding the influence of solder on the subsequent modification of the Bi-based superconducting flat wire, completing the critical current test, and directly modifying the Bi-based superconducting flat wire. After the modification is completed, the critical current test is directly performed, and the same sample is used for the improvement and the modified, avoiding the problem of misjudgment of process optimization caused by fluctuations in superconducting wire strips.
[0007] In order to solve the above technical problems, the technical solution adopted by the present invention is: a device for in-situ testing of Bi-based superconducting flat wires, characterized in that the device includes an insulating plate, on which a first current pressure electrode, a first potential pressure electrode, a second potential pressure electrode and a second current pressure electrode with the same structure are arranged in a straight line in sequence, the first current pressure electrode includes a pressure bolt threadedly connected to the insulating plate, the pressure bolt is sleeved with an electrode pressing plate for squeezing the Bi-based superconducting flat wire, the pressure bolt is also sleeved with a pressure control spring that enables the electrode pressing plate to press the Bi-based superconducting flat wire, the electrode pressing plate is provided with a lead terminal, and the insulating plate is also provided with a limit block for limiting the position of the Bi-based superconducting flat wire.
[0008] The above-mentioned device for in-situ testing of Bi-based superconducting flat wire is characterized in that the stiffness coefficient of the pressure control spring in the first current pressure electrode and the second current pressure electrode is 5N / mm to 10N / mm.
[0009] The above-mentioned device for in-situ testing of Bi-based superconducting flat wire is characterized in that the types of the pressure bolts in the first current pressure electrode and the second current pressure electrode are M10-M12.
[0010] The above-mentioned device for in-situ testing of Bi-based superconducting flat wire is characterized in that the width of the electrode pressing sheet in the first current pressure electrode and the second current pressure electrode is 1.5 to 3 times the width of the Bi-based superconducting flat wire, the length is 3 to 5 times the width of the Bi-based superconducting flat wire, the thickness is 2 mm to 3 mm, and the material is annealed brass plate.
[0011] The above-mentioned device for in-situ testing of Bi-based superconducting flat wire is characterized in that the stiffness coefficient of the pressure control spring in the first potential pressure electrode and the second potential pressure electrode is 2N / mm to 5N / mm.
[0012] The above-mentioned device for in-situ testing of Bi-based superconducting flat wire is characterized in that the types of the pressure bolts in the first potential pressure electrode and the second potential pressure electrode are M5-M7.
[0013] The above-mentioned device for in-situ testing of Bi-based superconducting flat wire is characterized in that the width of the potential pressure plate in the first potential pressure electrode and the second potential pressure electrode is 0.5 to 1 times the width of the Bi-based superconducting flat wire, the length is 3 to 5 times the width of the Bi-based superconducting flat wire, the thickness is 2 mm to 3 mm, and the material is annealed brass plate.
[0014] The above-mentioned device for in-situ testing of Bi-based superconducting flat wire is characterized in that the lead terminal on the first current pressure electrode is the positive electrode terminal of the power supply, the lead terminal on the second current pressure electrode is the negative electrode terminal of the power supply, the positive electrode terminal and the negative electrode terminal of the power supply are respectively connected to the positive and negative electrodes of the power supply through wires, the lead terminal on the first potential pressure electrode is the positive electrode terminal of the nanovoltmeter, the lead terminal on the second potential pressure electrode is the negative electrode terminal of the nanovoltmeter, the positive electrode terminal and the negative electrode terminal of the nanovoltmeter are respectively connected to the positive and negative electrodes of the nanovoltmeter through wires.
[0015] The above-mentioned device for in-situ testing of Bi-based superconducting flat wires is characterized in that a head shape mark is provided on the limit block, and a tail shape mark is provided on the end of the insulating plate away from the limit block.
[0016] In addition, the present invention also provides a method for using the in-situ testing device for Bi-based superconducting flat wires, characterized in that the method comprises the following steps:
[0017] Step 1, respectively loosen the pressure bolts in the first current pressure electrode, the first potential pressure electrode, the second potential pressure electrode and the second current pressure electrode, so that the pressure control spring is in an uncompressed state, and at the same time make the gap between the pressure bolt and the pressure control spring larger than the thickness of the Bi-based superconducting flat wire, to obtain a device to be loaded with samples;
[0018] Step 2: Place the Bi-based superconducting flat wire on the insulating plate of the device to be loaded, and align the head with the limit block, then move the Bi-based superconducting flat wire to the lower part of the electrode pressing plate of the first current pressure electrode, the first potential pressure electrode, the second potential pressure electrode and the second current pressure electrode, respectively tighten the pressure bolts in the first current pressure electrode, the first potential pressure electrode, the second potential pressure electrode and the second current pressure electrode, so that the compression length of the pressure control spring is 1 mm to 2 mm, and obtain the loading device;
[0019] Step 3: placing the sample loading device obtained in step 2 into a liquid nitrogen tank, then supplying power to the Bi-based superconducting flat wire, and detecting the potential of the Bi-based superconducting flat wire by a nanovoltmeter to obtain the critical current of the Bi-based superconducting flat wire;
[0020] Step 4: improve the process of the Bi-based superconducting flat wire after the critical current is obtained in step 3, and then repeat steps 1 to 3 to obtain the critical current of the Bi-based superconducting flat wire after the process improvement;
[0021] Step 5: By comparing the critical current of the Bi-based superconducting flat wire obtained in step 3 with the critical current of the Bi-based superconducting flat wire after process improvement obtained in step 4, the effect of the process improvement is determined.
[0022] The present invention ensures that the pressure is 5 to 20N by controlling the compression length of the pressure control spring in the first current pressure electrode and the second current pressure electrode to 1mm to 2mm, and ensures that the pressure is 2N to 10N by controlling the compression length of the pressure control spring in the first potential pressure electrode and the second potential pressure electrode to 1mm to 2mm.
[0023] Compared with the prior art, the present invention has the following advantages:
[0024] 1. The present invention provides a first current pressure electrode and a second current pressure electrode to energize the Bi-based superconducting flat wire while clamping the Bi-based superconducting flat wire, and provides a first potential pressure electrode and a second potential pressure electrode to detect the potential of the Bi-based superconducting flat wire while clamping the Bi-based superconducting flat wire, thereby achieving non-destructive and pollution-free testing of the critical current of the Bi-based superconducting flat wire.
[0025] 2. The device for in-situ testing of Bi-based superconducting flat wires of the present invention performs in-situ testing (same sample, same position) on the same Bi-based superconducting flat wire before and after improvement, thereby accurately determining the impact of process improvement on the current-carrying performance of the Bi-based superconducting flat wire. This method effectively solves the problem of inaccurate judgment of the effectiveness of process improvement caused by uneven performance of superconducting samples in the research and development stage. Only one sample and one experiment are needed to judge the effectiveness of the process improvement. Compared with the large-sample averaging method, this method is more efficient and accurate.
[0026] 3. The present invention adopts a non-destructive and non-polluting contact pressure electrode to replace the solder welding electrode, thereby avoiding the problem of sample failure due to solder contamination and preventing the serious influence of solder on heat treatment or surface modification tests.
[0027] 4. The present invention accurately controls the pressure through the pressure control spring, which not only achieves full contact between the pressure electrode and the Bi-based superconducting flat wire, but also avoids the problem of the ceramic core in the Bi-based superconducting flat wire being crushed due to excessive pressure.
[0028] 5. The device design of the present invention is concise and efficient, and provides a test device and solution for quickly and accurately obtaining the improvement effect for the process improvement of Bi-based superconducting flat wire.
[0029] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic structural diagram of a device for in-situ testing of Bi-based superconducting flat wires according to the present invention.
[0031] Figure 2 It is a schematic diagram of the connection relationship between the device for in-situ testing of Bi-based superconducting flat wires and the Bi-based superconducting flat wires of the present invention.
[0032] Figure 3 It is a schematic structural diagram of the first current pressure electrode in the device for in-situ testing of Bi-based superconducting flat wires of the present invention.
[0033] Description of reference numerals:
[0034] 1—insulating plate; 2—first current pressure electrode; 3—first potential pressure electrode;
[0035] 4—second potential pressure electrode; 5—second current pressure electrode; 6—pressure bolt;
[0036] 7—electrode pressing piece; 8—pressure control spring; 9—limiting block;
[0037] 10—Bi-based superconducting flat wire; 11—positive power terminal; 12—negative power terminal;
[0038] 13—Nanovoltmeter positive terminal; 14—Nanovoltmeter negative terminal; 15—Head shape mark;
[0039] 16—tail shape mark; 17—sample placement area. DETAILED DESCRIPTION
[0040] The device for in-situ testing of Bi-based superconducting flat wires of the present invention is described in detail through Example 1.
[0041] Example 1
[0042] like Figure 1 , Figure 2 and Figure 3As shown, a device for in-situ testing of Bi-based superconducting flat wires in this embodiment includes an insulating plate 1, on which a first current pressure electrode 2, a first potential pressure electrode 3, a second potential pressure electrode 4 and a second current pressure electrode 5 with the same structure are arranged in a straight line in sequence, the first current pressure electrode 2 includes a pressure bolt 6 threadedly connected to the insulating plate 1, the pressure bolt 6 is sleeved with an electrode pressing plate 7 for squeezing the Bi-based superconducting flat wire 10, the pressure bolt 6 is also sleeved with a pressure control spring 8 for pressing the electrode pressing plate 7 to press the Bi-based superconducting flat wire 10, the electrode pressing plate 7 is provided with a lead terminal, and the insulating plate 1 is also provided with a limit block 9 for limiting the Bi-based superconducting flat wire 10.
[0043] It should be noted that, by providing the insulating plate 1, it is convenient to install the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4, the second current pressure electrode 5 and the Bi-based superconducting flat wire 10; by providing the first current pressure electrode 2 and the second current pressure electrode 5, the Bi-based superconducting flat wire 10 is energized while the Bi-based superconducting flat wire 10 is clamped; by providing the first potential pressure electrode 3 and the second potential pressure electrode 4, the electric potential of the Bi-based superconducting flat wire 10 is detected while the Bi-based superconducting flat wire 10 is clamped, thereby realizing non-destructive and pollution-free testing of the critical current of the Bi-based superconducting flat wire 10.
[0044] It should be noted that by setting a pressure bolt 6 and a pressure control spring 8, and by adjusting the pressure bolt 6 to adjust the pressure of the pressure control spring 8, the electrode pressing sheet 7 can better clamp the Bi-based superconducting flat wire 10, and ensure that the Bi-based superconducting flat wire 10 is not crushed. By setting lead terminals, it is convenient to connect the wires, so that the first current pressure electrode 2, the second current pressure electrode 5 and the first potential pressure electrode 3, the second potential pressure electrode 4 are connected to the power supply and the nanovoltmeter respectively. The Bi-based superconducting flat wire 10 is limited by setting a limit block 9, and the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5 are clamped.
[0045] It should be noted that the intervals between the first current pressure electrode 2 , the first potential pressure electrode 3 , the second potential pressure electrode 4 and the second current pressure electrode 5 are equal.
[0046] It should be noted that a sample placement area 17 is provided on the insulating plate 1. During testing, the Bi-based superconducting flat wire 10 is first placed on the sample placement area 17 and then pushed flatly under the pressure electrode, which is easy to operate.
[0047] In this embodiment, the spring constant of the pressure control spring 8 in the first current pressure electrode 2 and the second current pressure electrode 5 is 5N / mm-10N / mm. By controlling the spring constant, there is enough pressure to make the electrode pressing sheet 7 fully contact with the Bi-based superconducting flat wire 10, and the current can pass through the interface between the electrode pressing sheet 7 and the Bi-based superconducting flat wire 10 to finally form a closed loop. On the other hand, it is avoided that the ceramic superconducting core inside the Bi-based superconducting flat wire 10 is crushed due to excessive pressure.
[0048] In this embodiment, the type of the pressure bolts 6 in the first current pressure electrode 2 and the second current pressure electrode 5 is M10-M12. The pressure of the pressure control spring 8 can be easily controlled by controlling the type of the bolts.
[0049] In this embodiment, the width of the electrode pressing sheet 7 in the first current pressure electrode 2 and the second current pressure electrode 5 is 1.5 to 3 times the width of the Bi-based superconducting flat wire 10, the length is 3 to 5 times the width of the Bi-based superconducting flat wire 10, the thickness is 2 mm to 3 mm, and the material is an annealed brass plate. By using a larger electrode pressing sheet 7, the electrode pressing sheet 7 is ensured to be in full contact with the Bi-based superconducting flat wire 10, which is convenient for the transmission of current. By using an annealed brass plate, it is not easy to oxidize, which ensures the advantage of full contact between the electrode pressing sheet 7 and the Bi-based superconducting flat wire 10. In addition, the hardness of the annealed brass plate is relatively small, which avoids damage to the Bi-based superconducting flat wire 10 caused by excessive hardness.
[0050] In this embodiment, the spring constant of the pressure control spring 8 in the first potential pressure electrode 3 and the second potential pressure electrode 4 is 2N / mm-5N / mm. By controlling the spring constant, there is enough pressure to make the electrode pressing sheet 7 fully contact with the Bi-based superconducting flat wire 10, and the current can pass through the interface between the electrode pressing sheet 7 and the Bi-based superconducting flat wire 10, and finally form a closed loop, while avoiding the problem that the ceramic superconducting core inside the Bi-based superconducting flat wire 10 is crushed due to excessive pressure.
[0051] In this embodiment, the types of the pressure bolts 6 in the first potential pressure electrode 3 and the second potential pressure electrode 4 are M5 to M7. The pressure of the pressure spring 8 can be easily controlled by controlling the type of the bolts.
[0052] In this embodiment, the width of the potential pressure piece in the first potential pressure electrode 3 and the second potential pressure electrode 4 is 0.5 to 1 times the width of the Bi-based superconducting flat wire 10, the length is 3 to 5 times the width of the Bi-based superconducting flat wire 10, the thickness is 2 mm to 3 mm, and the material is annealed brass plate. The smaller electrode pressure piece 7 is used because the first potential pressure electrode 3 and the second potential pressure are used to test weak current signals, and the smaller electrode pressure piece 7 has a small contact point, and the data obtained by the test is accurate.
[0053] like Figure 1As shown, in this embodiment, the lead terminal on the first current pressure electrode 2 is the positive terminal 11 of the power supply, and the lead terminal on the second current pressure electrode 5 is the negative terminal 12 of the power supply. The positive terminal 11 and the negative terminal 12 of the power supply are respectively connected to the positive and negative electrodes of the power supply through wires. The lead terminal on the first potential pressure electrode 3 is the positive terminal 13 of the nanovoltmeter, and the lead terminal on the second potential pressure electrode 4 is the negative terminal 14 of the nanovoltmeter. The positive terminal 13 and the negative terminal 14 of the nanovoltmeter are respectively connected to the positive and negative electrodes of the nanovoltmeter through wires. By respectively setting the positive terminal 11 and the negative terminal 12 of the power supply, the positive terminal 13 and the negative terminal 14 of the nanovoltmeter, and respectively connecting the power supply and the nanovoltmeter, the four-lead method is implemented to measure the critical current of the Bi-based superconducting flat wire 10.
[0054] like Figure 1 As shown, in this embodiment, a head shape mark 15 is provided on the stop block 9, and a tail shape mark 16 is provided on the end of the insulating plate 1 away from the stop block 9. By providing the head shape mark 15 and the tail shape mark 16, it is convenient to point the heads of the Bi-based superconducting flat wire 10 and the Bi-based superconducting flat wire 10 after process improvement to the same direction in two tests, thereby avoiding the problem of inaccurate data caused by confusion between the head and the tail of the Bi-based superconducting flat wire 10.
[0055] The method for using the device for in-situ testing of Bi-based superconducting flat wires of the present invention is described in detail through Examples 2 to 4.
[0056] Example 2
[0057] This embodiment includes the following steps:
[0058] Step 1, loosen the pressure bolts 6 in the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5 respectively, so that the pressure control spring 8 is in a non-compressed state, and at the same time make the gap between the pressure bolt 6 and the pressure control spring 8 larger than the thickness of the Bi-based superconducting flat wire 10, to obtain a device to be loaded with samples;
[0059] Step 2: Place the Bi-based superconducting flat wire 10 on the insulating plate 1 of the sample loading device, and align the head with the limit block 9, then move the Bi-based superconducting flat wire 10 to the lower part of the electrode pressing plate 7 of the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5, respectively tighten the pressure bolts 6 in the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5, so that the compression length of the pressure control spring 8 is 2 mm, and the sample loading device is obtained;
[0060] Step 3: Place the sample loading device obtained in step 2 into a liquid nitrogen tank, then supply power to the Bi-based superconducting flat wire 10, and detect the potential of the Bi-based superconducting flat wire 10 by a nanovoltmeter, and calculate that the critical current of the Bi-based superconducting flat wire 10 is 50A;
[0061] Step 4: Improve the process of the Bi-based superconducting flat wire 10 after obtaining the critical current in step 3, and then repeat steps 1 to 3 to obtain a critical current of 50A for the Bi-based superconducting flat wire 10 after the process improvement; the process improvement is an electrochemical Ag reduction treatment, specifically, removing 30 μm of Ag from the surface of the Bi-based superconducting flat wire 10, reducing the Ag content by 48%, and substantially reducing the cost of the superconducting tape by 45%;
[0062] Step 5: By comparing the critical current of the Bi-based superconducting flat wire 10 obtained in step 3 with the critical current of the Bi-based superconducting flat wire 10 after process improvement obtained in step 4, the current carrying performance of the Bi-based superconducting flat wire 10 is not reduced, indicating that the process improvement is an effective improvement.
[0063] Comparative Example 1
[0064] This comparative example comprises the following steps:
[0065] Step 1: Take three samples from the Bi-based superconducting flat wire 10 and name them as sample 1, sample 2, and sample 3 respectively;
[0066] Step 2: solder the lead wire of sample 1 obtained in step 1 with solder, and test to obtain a critical current of 45A;
[0067] Step 3: Electrochemically reduce the Ag content of the sample 2 obtained in step 1, specifically, remove 30 μm of Ag from the surface of the Bi-based superconducting flat wire 10, reduce the Ag content by 48%, and basically reduce the cost of the superconducting tape by 45%. Then, solder the lead wires, and test to obtain a critical current of 56 A.
[0068] Step 4: Electrochemically reduce the Ag content of sample 3 obtained in step 1, specifically, remove 30 μm of Ag from the surface of Bi-based superconducting flat wire 10, reduce the Ag content by 48%, and basically reduce the cost of superconducting tape by 45%. Then, solder the lead wires, and test to obtain a critical current of 39 A.
[0069] Step 5. By comparing the critical currents obtained in Step 2, Step 3, and Step 4, the performance of some samples increased, while the performance of some samples decreased. Therefore, in the case of a small number of samples, the effectiveness of the process improvement cannot be determined by the test method of soldering leads.
[0070] By comparing Comparative Example 1 with Example 1, it can be seen that when there are few samples, the testing method of soldering leads cannot determine the effectiveness of process improvement. However, by using the device and method for in-situ critical current of the present invention, only one sample is tested twice: once before and after the improvement of the Bi-based superconducting flat wire, and the accurate process modification effect can be obtained.
[0071] Comparative Example 2
[0072] This comparative example comprises the following steps:
[0073] Step 1, taking 8 samples from the Bi-based superconducting flat wire 10, and naming them as sample 1, sample 2, sample 3, ..., sample 8 respectively;
[0074] Step 2: solder the leads of samples 1 to 4 obtained in step 1 with solder, and test to obtain an average critical current of 42A;
[0075] Step 3: Perform electrochemical Ag reduction treatment on samples 5 to 8 obtained in step 1, specifically, remove 30 μm of Ag from the surface of the Bi-based superconducting flat wire 10, reduce the Ag content by 48%, and basically reduce the cost of the superconducting tape by 45%. Then, solder the leads, and the average critical current value is 48A after testing.
[0076] Step 4: By comparing the critical currents obtained in step 2 and step 3, it can be seen that since only the surface Ag is removed, it is impossible to improve the superconducting current carrying performance of the Bi-based superconducting flat wire 10. Therefore, when using more samples, the test method of soldering the leads cannot determine the effectiveness of the process improvement.
[0077] By comparing Comparative Example 2 with Example 1, it can be seen that no reliable results can be obtained by testing 8 samples using the solder welding lead testing method. However, by using the in-situ critical current device and method of the present invention, only one sample is tested twice: the Bi-based superconducting flat wire 10 is tested once before and after the improvement, respectively, and the accurate process modification effect can be obtained.
[0078] Example 3
[0079] This embodiment includes the following steps:
[0080] Step 1, loosen the pressure bolts 6 in the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5 respectively, so that the pressure control spring 8 is in a non-compressed state, and at the same time make the gap between the pressure bolt 6 and the pressure control spring 8 larger than the thickness of the Bi-based superconducting flat wire 10, to obtain a device to be loaded with samples;
[0081] Step 2: Place the Bi-based superconducting flat wire 10 on the insulating plate 1 of the sample loading device, and align the head with the limit block 9, then move the Bi-based superconducting flat wire 10 to the lower part of the electrode pressing plate 7 of the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5, respectively tighten the pressure bolts 6 in the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5, so that the compression length of the pressure control spring 8 is 1.5 mm, and the sample loading device is obtained;
[0082] Step 3: Place the sample loading device obtained in step 2 into a liquid nitrogen tank, then supply power to the Bi-based superconducting flat wire 10, and detect the potential of the Bi-based superconducting flat wire 10 by a nanovoltmeter, and calculate that the critical current of the Bi-based superconducting flat wire 10 is 50A;
[0083] Step 4: Improve the process of the Bi-based superconducting flat wire 10 after obtaining the critical current in step 3, and then repeat steps 1 to 3 to obtain a critical current of 50A for the Bi-based superconducting flat wire 10 after the process improvement; the process improvement is an electrochemical Ag reduction treatment, specifically, removing 30 μm of Ag from the surface of the Bi-based superconducting flat wire 10, reducing the Ag content by 48%, and substantially reducing the cost of the superconducting tape by 45%;
[0084] Step 5: By comparing the critical current of the Bi-based superconducting flat wire 10 obtained in step 3 with the critical current of the Bi-based superconducting flat wire 10 after process improvement obtained in step 4, the current carrying performance of the Bi-based superconducting flat wire 10 is not reduced, indicating that the process improvement is an effective improvement.
[0085] Example 4
[0086] This embodiment includes the following steps:
[0087] Step 1, loosen the pressure bolts 6 in the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5 respectively, so that the pressure control spring 8 is in a non-compressed state, and at the same time make the gap between the pressure bolt 6 and the pressure control spring 8 larger than the thickness of the Bi-based superconducting flat wire 10, to obtain a device to be loaded with samples;
[0088] Step 2: Place the Bi-based superconducting flat wire 10 on the insulating plate 1 of the sample loading device, and align the head with the limit block 9, then move the Bi-based superconducting flat wire 10 to the lower part of the electrode pressing plate 7 of the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5, respectively tighten the pressure bolts 6 in the first current pressure electrode 2, the first potential pressure electrode 3, the second potential pressure electrode 4 and the second current pressure electrode 5, so that the compression length of the pressure control spring 8 is 1 mm, and the sample loading device is obtained;
[0089] Step 3: Place the sample loading device obtained in step 2 into a liquid nitrogen tank, then supply power to the Bi-based superconducting flat wire 10, and detect the potential of the Bi-based superconducting flat wire 10 by a nanovoltmeter, and calculate that the critical current of the Bi-based superconducting flat wire 10 is 50A;
[0090] Step 4: Improve the process of the Bi-based superconducting flat wire 10 after obtaining the critical current in step 3, and then repeat steps 1 to 3 to obtain a critical current of 50A for the Bi-based superconducting flat wire 10 after the process improvement; the process improvement is an electrochemical Ag reduction treatment, specifically, removing 30 μm of Ag from the surface of the Bi-based superconducting flat wire 10, reducing the Ag content by 48%, and substantially reducing the cost of the superconducting tape by 45%;
[0091] Step 5: By comparing the critical current of the Bi-based superconducting flat wire 10 obtained in step 3 with the critical current of the Bi-based superconducting flat wire 10 after process improvement obtained in step 4, the current carrying performance of the Bi-based superconducting flat wire 10 is not reduced, indicating that the process improvement is an effective improvement.
[0092] The above is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any simple modification, change and equivalent change made to the above embodiment according to the technical essence of the present invention still falls within the protection scope of the technical solution of the present invention.
Claims
1. A device for in-situ testing of Bi-based superconducting flat wires, It is characterized in that The device comprises an insulating plate (1), on which a first current pressure electrode (2), a first potential pressure electrode (3), a second potential pressure electrode (4) and a second current pressure electrode (5) having the same structure are arranged in a straight line in sequence, the first current pressure electrode (2) comprising a pressure bolt (6) threadedly connected to the insulating plate (1), an electrode pressing sheet (7) for pressing a Bi-based superconducting flat wire (10) being sleeved on the pressure bolt (6), a pressure control spring (8) for causing the electrode pressing sheet (7) to press the Bi-based superconducting flat wire (10) being sleeved on the pressure bolt (6), a lead terminal being arranged on the electrode pressing sheet (7), and a limit block (9) for limiting the position of the Bi-based superconducting flat wire (10) being arranged on the insulating plate (1).
2. The device for in-situ testing of Bi-based superconducting flat wire according to claim 1, It is characterized in that The stiffness coefficient of the control pressure spring (8) in the first current pressure electrode (2) and the second current pressure electrode (5) is 5N / mm to 10N / mm.
3. The device for in-situ testing of Bi-based superconducting flat wire according to claim 1, It is characterized in that The models of the pressure bolts (6) in the first current pressure electrode (2) and the second current pressure electrode (5) are M10-M12.
4. The device for in-situ testing of Bi-based superconducting flat wire according to claim 1, It is characterized in that The electrode pressing sheet (7) in the first current pressure electrode (2) and the second current pressure electrode (5) has a width of 1.5 to 3 times the width of the Bi-based superconducting flat wire (10), a length of 3 to 5 times the width of the Bi-based superconducting flat wire (10), a thickness of 2 mm to 3 mm, and is made of annealed brass plate.
5. The device for in-situ testing of Bi-based superconducting flat wire according to claim 1, It is characterized in that The stiffness coefficient of the pressure control spring (8) in the first potential pressure electrode (3) and the second potential pressure electrode (4) is 2N / mm to 5N / mm.
6. The device for in-situ testing of Bi-based superconducting flat wire according to claim 1, It is characterized in that The models of the pressure bolts (6) in the first potential pressure electrode (3) and the second potential pressure electrode (4) are M5-M7.
7. The device for in-situ testing of Bi-based superconducting flat wire according to claim 1, It is characterized in that The potential pressure plates in the first potential pressure electrode (3) and the second potential pressure electrode (4) have a width of 0.5 to 1 times the width of the Bi-based superconducting flat wire (10), a length of 3 to 5 times the width of the Bi-based superconducting flat wire (10), a thickness of 2 mm to 3 mm, and are made of annealed brass plates.
8. The device for in-situ testing of Bi-based superconducting flat wire according to claim 1, It is characterized in that The lead terminal on the first current pressure electrode (2) is a positive power terminal (11), and the lead terminal on the second current pressure electrode (5) is a negative power terminal (12). The positive power terminal (11) and the negative power terminal (12) are respectively connected to the positive and negative poles of the power supply through wires. The lead terminal on the first potential pressure electrode (3) is a positive nanovoltmeter terminal (13), and the lead terminal on the second potential pressure electrode (4) is a negative nanovoltmeter terminal (14). The positive nanovoltmeter terminal (13) and the negative nanovoltmeter terminal (14) are respectively connected to the positive and negative poles of the nanovoltmeter through wires.
9. The device for in-situ testing of Bi-based superconducting flat wire according to claim 1, It is characterized in that The limit block (9) is provided with a head shape mark (15), and the end of the insulating plate (1) away from the limit block (9) is provided with a tail shape mark (16).
10. A method for using the device for in-situ testing of Bi-based superconducting flat wire (10) as claimed in any one of claims 1 to 9, It is characterized in that The method comprises the following steps: Step 1: loosen the pressure bolts (6) in the first current pressure electrode (2), the first potential pressure electrode (3), the second potential pressure electrode (4) and the second current pressure electrode (5) respectively, so that the pressure control spring (8) is in a non-compressed state, and at the same time, make the gap between the pressure bolts (6) and the pressure control spring (8) larger than the thickness of the Bi-based superconducting flat wire (10), so as to obtain a device to be loaded with samples; Step 2: Place the Bi-based superconducting flat wire (10) on the insulating plate (1) of the sample loading device, with the head aligned with the limit block (9), then move the Bi-based superconducting flat wire (10) to the lower part of the electrode pressing plate (7) of the first current pressure electrode (2), the first potential pressure electrode (3), the second potential pressure electrode (4) and the second current pressure electrode (5), respectively tighten the pressure bolts (6) in the first current pressure electrode (2), the first potential pressure electrode (3), the second potential pressure electrode (4) and the second current pressure electrode (5) so that the compression length of the pressure control spring (8) is 1 mm to 2 mm, and obtain the sample loading device; Step 3: placing the sample loading device obtained in step 2 into a liquid nitrogen tank, then supplying power to the Bi-based superconducting flat wire (10), detecting the potential of the Bi-based superconducting flat wire (10) by a nanovoltmeter, and obtaining the critical current of the Bi-based superconducting flat wire (10) by calculation; Step 4, performing process improvement on the Bi-based superconducting flat wire (10) after obtaining the critical current in step 3, and then repeating steps 1 to 3 to obtain the critical current of the Bi-based superconducting flat wire (10) after the process improvement; Step 5: By comparing the critical current of the Bi-based superconducting flat wire (10) obtained in step 3 with the critical current of the Bi-based superconducting flat wire (10) after process improvement obtained in step 4, the effect of process improvement is determined.