Method for preparing fermentable sugar by pretreating lignocellulose with recyclable low-concentration p-toluenesulfonic acid

By using low-concentration p-toluenesulfonic acid pretreatment and ultra-high cross-linking adsorption resin recovery technology, the high cost and high energy consumption of high-concentration acid pretreatment were solved. This enabled hemicellulose degradation and acid recovery under low temperature and low pressure conditions, improved the yield of fermentable sugars, and provided a new strategy for the high-value utilization of lignocellulose.

CN121137093APending Publication Date: 2025-12-16GUANGZHOU INST OF ENERGY CONVERSION CHINESE ACAD OF SCI

Patent Information

Application Number
CN202410769779.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-14
Publication Date
2025-12-16

AI Technical Summary

Technical Problem

In existing technologies, high-concentration p-toluenesulfonic acid pretreatment of lignocellulose has problems such as carbohydrate degradation, high recycling costs, and high energy consumption. In addition, traditional pretreatment processes are cumbersome and difficult to achieve efficient and low-cost preparation of fermentable sugars.

Method used

Lignocellulose was pretreated with a low-concentration p-toluenesulfonic acid aqueous solution, and p-toluenesulfonic acid in the hemicellulose hydrolysate was recovered using an ultra-high cross-linking adsorption resin. Pretreatment was carried out under low temperature and low pressure conditions, combined with enzymatic hydrolysis, to selectively degrade hemicellulose into fermentable sugars, and the acid was recovered using an ultra-high cross-linking adsorption resin.

Benefits of technology

The efficient degradation of hemicellulose under low temperature and low pressure conditions was achieved, which significantly improved the yield of fermentable sugars, reduced the energy consumption and cost of acid recovery, and provided a low-cost and efficient lignocellulose utilization strategy that is suitable for large-scale application in biorefining.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for preparing fermentable sugar from recyclable low-concentration p-toluenesulfonic acid pretreated lignocellulose, which comprises the following steps: firstly, pretreating lignocellulose by using a low-concentration p-toluenesulfonic acid aqueous solution, and carrying out solid-liquid separation to obtain hemicellulose hydrolysate and a pretreated solid component; then saccharifying and pretreating the solid component by using cellulase to obtain hydrolysate rich in glucose, adsorbing the hemicellulose hydrolysate by using hypercrosslinked adsorption resin, carrying out solid-liquid separation to obtain hydrolysate rich in xylose, and carrying out desorption treatment on the resin by using industrial ethanol to obtain xylose; and performing rotary evaporation on the desorbed liquid to remove the industrial ethanol to obtain p-toluenesulfonic acid. According to the method, hemicellulose is efficiently degraded to obtain derived sugar of hemicellulose, meanwhile, the saccharification efficiency of cellulase is improved, p-toluenesulfonic acid is recycled through the hypercrosslinked adsorption resin, and the method has the advantages of being high in fermentable sugar yield, recyclable in acid catalyst, low in cost, environmentally friendly and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical fields:

[0001] This invention belongs to the field of biochemical technology, specifically relating to a method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid. Background technology:

[0002] Lignocellulose is characterized by its wide distribution and large yield. Hemicellulose and cellulose in lignocellulose can be degraded into fermentable sugars, functional sugars, furfural, and their derivatives. However, lignocellulose has a complex structure; cellulose is embedded in ordered fiber bundles within lignin and hemicellulose, tightly bound together by hydrogen bonds to form a network structure. This natural physical barrier makes lignocellulose difficult to degrade, thus requiring pretreatment to break down this natural degradation barrier. Hemicellulose has poor thermal stability and is easily degraded into pentose sugars such as xylose under high temperature and acidic conditions. Therefore, preferential pretreatment strategies for hemicellulose have become the mainstream process for lignocellulose utilization. Numerous pretreatment methods exist for preferential hemicellulose removal, such as high-temperature hydrothermal treatment, steam explosion, inorganic acid hydrolysis, and organic acid hydrolysis. High-temperature hydrothermal treatment and steam explosion require significant energy and sophisticated equipment, while inorganic acid pretreatment corrodes equipment, pollutes the environment, and is difficult to recycle. p-Toluenesulfonic acid, an acidic co-water solvent with strong acidity and good surface activity, has attracted widespread attention due to its mild pretreatment conditions, high component separation efficiency, and ease of recovery. Although numerous patents exist for the pretreatment of lignocellulose with p-toluenesulfonic acid, most employ high concentrations of p-toluenesulfonic acid, which easily degrades carbohydrates and significantly increases recycling costs. For example, patents with publication numbers CN112322677A and CN11304262A, while featuring mild reaction conditions and high enzymatic hydrolysis efficiency, are complex and use excessively high concentrations of p-toluenesulfonic acid solutions, resulting in enormous energy consumption for recycling. Therefore, there is a need to develop a highly efficient, low-cost, low-concentration, and recyclable p-toluenesulfonic acid pretreatment method. Summary of the Invention:

[0003] This invention provides a method for preparing fermentable sugars from lignocellulose by pretreating it with a low concentration of p-toluenesulfonic acid. The method uses a low concentration of p-toluenesulfonic acid to pretreat lignocellulose, selectively degrading hemicellulose into xylose. The pretreated lignocellulose exhibits good digestibility during enzymatic hydrolysis. Furthermore, p-toluenesulfonic acid in the hemicellulose hydrolysate is recovered using an ultra-high cross-linking adsorption resin. This method solves the problems of low profitability, high cost, and high energy consumption caused by the high concentration of p-toluenesulfonic acid used in pretreatment and the cumbersome p-toluenesulfonic acid recovery process in existing technologies.

[0004] This invention is achieved through the following technical solutions:

[0005] A method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid includes the following steps:

[0006] (1) Pretreatment of lignocellulose: Lignocellulose is pretreated with a 0.5-2.0 wt% p-toluenesulfonic acid aqueous solution at 110-170℃, preferably 130-150℃, more preferably 130-140℃ for 0.5-2.5h, preferably 1.5-2.5h. After the reaction, solid-liquid separation is performed to obtain hemicellulose hydrolysate and pretreated lignocellulose solid components.

[0007] (2) Enzymatic hydrolysis of pretreated lignocellulose: The pretreated lignocellulose solid component from step (1) and the buffer containing cellulase are placed in a reactor at a solid-liquid mass ratio of 1:10 to 1:50. The enzymatic hydrolysis reaction is carried out at 45 to 55°C under shaking conditions. After the reaction is completed, cellulose hydrolysate is obtained.

[0008] (3) Recovery of p-toluenesulfonic acid: The swollen ultra-high cross-linked adsorption resin is immersed in the hemicellulose hydrolysate from step (1) and adsorbed under shaking conditions. After adsorption, the solid and liquid are separated. The separated ultra-high cross-linked adsorption resin is immersed in industrial ethanol and desorbed under shaking conditions. After desorption, the solid and liquid are separated. The separated mixture is subjected to rotary evaporation to remove industrial ethanol and recover p-toluenesulfonic acid solution. The ultra-high cross-linked adsorption resin is prepared according to the preparation method of ultra-high cross-linked adsorption resin disclosed in Chinese Patent CN202211440528.1.

[0009] Preferably, the lignocellulose is derived from wheat straw and / or corn straw.

[0010] Preferably, in step (1), the solid-liquid ratio of the pretreatment is 1:(6-15).

[0011] Preferably, in step (2), the enzymatic hydrolysis reaction takes 6-72 hours.

[0012] Preferably, in step (3), the amount of ultra-high cross-linking adsorption resin added during the adsorption process is 2.5-20 wt%.

[0013] Preferably, in step (3), the ultra-high cross-linking adsorption resin is immersed in 5-15 times the volume of the resin added in industrial ethanol for desorption.

[0014] Preferably, in step (3), the adsorption time is 1-12 hours and the desorption time is 1-3 hours.

[0015] Preferably, in step (3), the recovered p-toluenesulfonic acid solution is used in step (1) for lignocellulose pretreatment.

[0016] Compared with the prior art, the present invention has the following advantages:

[0017] (1) This invention utilizes low-concentration p-toluenesulfonic acid to pretreat lignocellulose, thereby directionally breaking down hemicellulose under low temperature and low pressure conditions. This saves on acidic catalysts and avoids the harsh conditions of traditional pretreatment processes. Furthermore, under optimal conditions, the damage to the cellulose structure is minimal, which can significantly improve the yield of fermentable sugars, providing a new strategy for the high-value utilization of lignocellulose.

[0018] (2) This invention utilizes ultra-high cross-linking adsorption resin to recover p-toluenesulfonic acid, solving the problem of dilute acid recovery in dilute acid pretreatment. This recycling system has low energy consumption, high recovery rate, and is green and environmentally friendly, which can well meet the economic requirements of biorefining and is easy to scale up. Attached image description: Detailed implementation method:

[0019] Those skilled in the art will understand that the techniques disclosed in the following embodiments represent those discovered by the inventors that work well in the practice of this invention. However, many changes can be made to the specific embodiments disclosed, still obtaining the same or similar results without departing from the spirit and scope of the invention.

[0020] The ultra-high crosslinking adsorption resins in the following examples were prepared according to the method disclosed in Example 2 of CN115845555A.

[0021] Example 1:

[0022] A method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid includes the following steps:

[0023] (1) Lignocellulose pretreatment: 6g of dried wheat straw and a 2.0wt% p-toluenesulfonic acid solution were placed in a reactor at a solid-liquid mass ratio of 1:10. The reaction time was set to 1.5h and the reaction temperature to 170℃. After the reaction, solid-liquid separation was performed to obtain hemicellulose hydrolysate and pretreated wheat straw. HPLC and biomass composition analysis showed that the xylose yield was 7.36%.

[0024] (2) Enzymatic hydrolysis of pretreated lignocellulose: The dried wheat straw pretreated in step (1) and a buffer solution containing cellulase were loaded into a reactor at a solid-liquid mass ratio of 1:50. The reaction was carried out at 50℃ with shaking for 6 hours. After the reaction, cellulose hydrolysate was obtained. According to HPLC test and calculation ((concentration of glucose in the hydrolysate * 0.9) / (substrate mass * percentage of dextran in the substrate)), the glucose yield was 20.37%.

[0025] (3) Recovery of p-toluenesulfonic acid: 2.5 wt% of swollen ultra-high cross-linked adsorption resin was added to the hemicellulose hydrolysate from step (1) for 1 h of adsorption, with shaking maintained during the adsorption process. After adsorption, solid-liquid separation was performed to obtain resin particles rich in p-toluenesulfonic acid. The resin was then immersed in 15 times the volume of industrial ethanol for desorption, with a desorption time of 1.5 h, with shaking maintained during the desorption process. Analysis showed that the p-toluenesulfonic acid recovery rate was 22.89%.

[0026] Example 2:

[0027] A method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid includes the following steps:

[0028] (1) Lignocellulose pretreatment: 6g of dried wheat straw and a 0.5wt% p-toluenesulfonic acid solution were placed in a reaction vessel at a solid-liquid mass ratio of 1:10. The reaction time was set to 1.5h and the reaction temperature to 110℃. After the reaction, solid-liquid separation was performed to obtain hemicellulose hydrolysate and pretreated wheat straw. HPLC and biomass composition analysis showed that the xylose yield was 4.49%.

[0029] (2) Enzymatic hydrolysis of pretreated lignocellulose: The dried wheat straw pretreated in step (1) and a buffer solution containing cellulase were loaded into a reactor at a solid-liquid mass ratio of 1:50. The reaction was carried out at 50℃ with shaking for 72 hours. After the reaction, cellulose hydrolysate was obtained. According to HPLC test and calculation ((concentration of glucose in the hydrolysate * 0.9) / (substrate mass * percentage of dextran in the substrate)), the glucose yield was 68.81%.

[0030] (3) Recovery of p-toluenesulfonic acid: 20 wt% of the swollen ultra-high crosslinked adsorption resin was added to the hemicellulose hydrolysate from step (1) and adsorbed for 12 h with shaking during the adsorption process. After adsorption, solid-liquid separation was performed to obtain resin particles rich in p-toluenesulfonic acid. The resin was then immersed in 15 times the volume of industrial ethanol for desorption for 1.5 h with shaking during the desorption process. The p-toluenesulfonic acid recovery rate was calculated to be 98.23%. The preparation of the ultra-high crosslinked adsorption resin was the same as in Example 1.

[0031] Example 3:

[0032] A method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid includes the following steps:

[0033] (1) Lignocellulose pretreatment: 6g of dried wheat straw and a 1.5wt% p-toluenesulfonic acid solution were placed in a reactor at a solid-liquid mass ratio of 1:10. The reaction time was set to 0.5h and the reaction temperature to 130℃. After the reaction, solid-liquid separation was performed to obtain hemicellulose hydrolysate and pretreated wheat straw. HPLC and biomass composition analysis showed that the xylose yield was 74.59%.

[0034] (2) Enzymatic hydrolysis of pretreated lignocellulose: The dried wheat straw pretreated in step (1) and a buffer solution containing cellulase were loaded into a reactor at a solid-liquid mass ratio of 1:50. The reaction was carried out at 50℃ with shaking for 72 h. After the reaction, cellulose hydrolysate was obtained. According to HPLC test and calculation ((concentration of glucose in the hydrolysate * 0.9) / (substrate mass * percentage of dextran in the substrate)), the glucose yield was 62.40%.

[0035] (3) Recovery of p-toluenesulfonic acid: 5 wt% of the swollen ultra-high cross-linked adsorption resin was added to the hemicellulose hydrolysate from step (1) and adsorbed for 12 h with shaking during the adsorption process. After adsorption, solid-liquid separation was performed to obtain resin particles rich in p-toluenesulfonic acid. The resin was then immersed in 15 times the volume of industrial ethanol for desorption for 3 h with shaking during the desorption process. Analysis showed that the p-toluenesulfonic acid recovery rate was 41.87%. The preparation of the ultra-high cross-linked adsorption resin was the same as in Example 1.

[0036] Comparative Example 1:

[0037] Referring to Example 3, the difference is that in step (3), a macroporous adsorption resin (Zhengzhou Hecheng New Material Technology Co., Ltd., product model X-5) is used to adsorb the hemicellulose hydrolysate, and the other steps are the same as in Example 3.

[0038] Recovery of p-toluenesulfonic acid: 5 wt% of swollen macroporous adsorption resin was added to the pretreated hemicellulose hydrolysate for adsorption for 12 h, with shaking maintained during the adsorption process. After adsorption, solid-liquid separation yielded resin particles rich in p-toluenesulfonic acid. The resin was then immersed in 15 times its volume of industrial ethanol for desorption for 3 h, with shaking maintained during the desorption process. Analysis showed that the p-toluenesulfonic acid recovery rate was 16.00%.

[0039] As can be seen from Example 3 and Comparative Example 1, the present invention uses an ultra-high cross-linked adsorption resin, which achieves a recovery rate of 41.87% for toluenesulfonic acid, which is higher than the recovery rate of 16.00% of conventional commercial macroporous adsorption resin, thus solving the problem of low recovery rate of dilute acid in dilute acid pretreatment.

[0040] Example 4:

[0041] A method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid includes the following steps:

[0042] (1) Lignocellulose pretreatment: 6g of dried wheat straw and a 1.5wt% p-toluenesulfonic acid solution were placed in a reactor at a solid-liquid mass ratio of 1:10. The reaction time was set to 2.5h and the reaction temperature to 130℃. After the reaction, solid-liquid separation was performed to obtain hemicellulose hydrolysate and pretreated wheat straw. HPLC and biomass composition analysis showed that the xylose yield was 73.63%.

[0043] (2) Enzymatic hydrolysis of pretreated lignocellulose: The dried wheat straw pretreated in step (1) and a buffer solution containing cellulase were loaded into a reactor at a solid-liquid mass ratio of 1:50. The reaction was carried out at 50℃ with shaking for 6 hours. After the reaction, cellulose hydrolysate was obtained. According to HPLC and biomass composition analysis and calculation ((concentration of glucose in the hydrolysate * 0.9) / (substrate mass * percentage of dextran in the substrate)), the glucose yield was 56.80%.

[0044] (3) Recovery of p-toluenesulfonic acid: 10 wt% of the swollen ultra-high crosslinked adsorption resin was added to the hemicellulose hydrolysate from step (1) and adsorbed for 12 h with shaking during the adsorption process. After adsorption, solid-liquid separation was performed to obtain resin particles rich in p-toluenesulfonic acid. The resin was then immersed in 15 times the volume of industrial ethanol for desorption for 1.5 h with shaking during the desorption process. Analysis showed that the p-toluenesulfonic acid recovery rate was 65.45%. The preparation of the ultra-high crosslinked adsorption resin was the same as in Example 1.

[0045] Example 5:

[0046] A method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid includes the following steps:

[0047] (1) Lignocellulose pretreatment: 6g of dried corn stalks and a 1.0wt% p-toluenesulfonic acid solution were placed in a reactor at a solid-liquid mass ratio of 1:10. The reaction time was set to 1.5h and the reaction temperature to 140℃. After the reaction, solid-liquid separation was performed to obtain hemicellulose hydrolysate and pretreated corn stalks. HPLC and biomass composition analysis showed that the xylose yield was 54.79%.

[0048] (2) Enzymatic hydrolysis of pretreated lignocellulose: The pretreated corn stalks from step (1) were dried and mixed with a buffer solution containing cellulase at a solid-liquid mass ratio of 1:50 in a reactor. The reaction was carried out at 50℃ with shaking for 6 hours. After the reaction, cellulose hydrolysate was obtained. By HPLC and biomass composition analysis and calculation ((concentration of glucose in the hydrolysate * 0.9) / (substrate mass * percentage of dextran in the substrate)), the glucose yield was 74.88%.

[0049] (3) Recovery of p-toluenesulfonic acid: 15 wt% of the swollen ultra-high crosslinked adsorption resin was added to the hemicellulose hydrolysate from step (1) and adsorbed for 12 h with shaking during the adsorption process. After adsorption, solid-liquid separation was performed to obtain resin particles rich in p-toluenesulfonic acid. The resin was then immersed in 15 times the volume of industrial ethanol for desorption for 1.5 h with shaking during the desorption process. The p-toluenesulfonic acid recovery rate was calculated to be 74.65%. The preparation of the ultra-high crosslinked adsorption resin was the same as in Example 1.

[0050] Example 6:

[0051] A method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid includes the following steps:

[0052] (1) Lignocellulose pretreatment: 6g of dried wheat straw and a 1.0wt% p-toluenesulfonic acid solution were placed in a reactor at a solid-liquid mass ratio of 1:10. The reaction time was set to 1.5h and the reaction temperature to 150℃. After the reaction, solid-liquid separation was performed to obtain hemicellulose hydrolysate and pretreated wheat straw. HPLC and biomass composition analysis showed that the xylose yield was 52.63%.

[0053] (2) Enzymatic hydrolysis of pretreated lignocellulose: The dried wheat straw pretreated in step (1) and a buffer solution containing cellulase were loaded into a reactor at a solid-liquid mass ratio of 1:50. The reaction was carried out at 50℃ with shaking for 72 h. After the reaction, cellulose hydrolysate was obtained. According to HPLC and biomass composition analysis and calculation ((concentration of glucose in the hydrolysate * 0.9) / (substrate mass * percentage of dextran in the substrate)), the glucose yield was 74.61%.

[0054] (3) Recovery of p-toluenesulfonic acid: 20 wt% of the swollen ultra-high crosslinked adsorption resin was added to the hemicellulose hydrolysate from step (1) and adsorbed for 12 h with shaking during the adsorption process. After adsorption, solid-liquid separation was performed to obtain resin particles rich in p-toluenesulfonic acid. The resin was then immersed in 5 times the volume of industrial ethanol for desorption for 1.5 h with shaking during the desorption process. Analysis showed that the p-toluenesulfonic acid recovery rate was 49.77%. The preparation of the ultra-high crosslinked adsorption resin was the same as in Example 1.

[0055] Example 7:

[0056] A method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid includes the following steps:

[0057] (1) Lignocellulose pretreatment: 6g of dried wheat straw and a 1.0wt% p-toluenesulfonic acid solution were placed in a reactor at a solid-liquid mass ratio of 1:10. The reaction time was set to 1.5h and the reaction temperature to 130℃. After the reaction, solid-liquid separation was performed to obtain hemicellulose hydrolysate and pretreated wheat straw. HPLC and biomass composition analysis showed that the xylose yield was 85.61%.

[0058] (2) Enzymatic hydrolysis of pretreated lignocellulose: The dried wheat straw pretreated in step (1) and a buffer solution containing cellulase were loaded into a reactor at a solid-liquid mass ratio of 1:50. The reaction was carried out at 50℃ with shaking for 72 hours. After the reaction, cellulose hydrolysate was obtained. By HPLC and biomass composition analysis and calculation ((concentration of glucose in the hydrolysate * 0.9) / (substrate mass * percentage of dextran in the substrate)), the glucose yield was 81.55%.

[0059] (3) Recovery of p-toluenesulfonic acid: 15 wt% of the swollen ultra-high crosslinked adsorption resin was added to the hemicellulose hydrolysate from step (1) and adsorbed for 12 h with shaking during the adsorption process. After adsorption, solid-liquid separation was performed to obtain resin particles rich in p-toluenesulfonic acid. The resin was then immersed in 5 times the volume of industrial ethanol for desorption for 1.5 h with shaking during the desorption process. The p-toluenesulfonic acid recovery rate was calculated to be 74.65%. The preparation of the ultra-high crosslinked adsorption resin was the same as in Example 1.

[0060] Comparative Example 2:

[0061] Fermentable sugars were prepared by pretreating wheat straw with a high-concentration p-toluenesulfonic acid solution and then enzymatically hydrolyzing it.

[0062] Six g of dried wheat straw and an 80 wt% p-toluenesulfonic acid solution were placed in a reaction vessel at a solid-liquid mass ratio of 1:10. The reaction time was set to 20 min and the reaction temperature to 80℃. After the reaction, the dried pretreated wheat straw and a buffer solution containing cellulase were added to the reactor at a solid-liquid mass ratio of 1:50. The reaction was carried out at 50℃ with shaking for 72 h. HPLC analysis and biomass composition analysis and calculation ((concentration of glucose in the enzymatic hydrolysate * 0.9) / (substrate mass * percentage of dextran in the substrate)) showed a glucose yield of 65.94%.

[0063] As can be seen from Examples 1-7 and Comparative Example 2, compared with the traditional high-concentration p-toluenesulfonic acid pretreatment conditions, the present invention uses low-concentration p-toluenesulfonic acid to pretreat lignocellulose, which not only saves acidic catalysts but also significantly improves the yield of fermentable sugars. In Example 7, the glucose yield of enzymatic hydrolysis after wheat straw pretreatment reached 81.55%, providing a new strategy for the high-value utilization of lignocellulose.

Claims

1. A method for preparing fermentable sugars from lignocellulose pretreated with recyclable low-concentration p-toluenesulfonic acid, characterized in that, Includes the following steps: (1) Lignocellulose pretreatment: Lignocellulose was pretreated with a 0.5-2.0 wt% p-toluenesulfonic acid aqueous solution at 110-170℃ for 0.5-2.5 h. After the reaction, solid-liquid separation was performed to obtain hemicellulose hydrolysate and pretreated lignocellulose solid components. (2) Enzymatic hydrolysis of pretreated lignocellulose: The pretreated lignocellulose solid component from step (1) and the buffer containing cellulase are placed in a reactor at a solid-liquid mass ratio of 1:10 to 1:

50. The enzymatic hydrolysis reaction is carried out at 45 to 55°C under shaking conditions. After the reaction is completed, cellulose hydrolysate is obtained. (3) Recovery of p-toluenesulfonic acid: The swollen ultra-high cross-linked adsorption resin is immersed in the hemicellulose hydrolysate from step (1) and adsorbed under shaking conditions. After adsorption, the solid and liquid are separated. The separated ultra-high cross-linked adsorption resin is immersed in industrial ethanol and desorbed under shaking conditions. After desorption, the solid and liquid are separated. The separated mixture is subjected to rotary evaporation to remove industrial ethanol and recover p-toluenesulfonic acid solution. The ultra-high cross-linked adsorption resin is prepared according to the preparation method of ultra-high cross-linked adsorption resin disclosed in Chinese Patent CN202211440528.

1.

2. The method according to claim 1, characterized in that, The lignocellulose is derived from wheat straw and / or corn straw.

3. The method according to claim 1, characterized in that, In step (1), the solid-liquid mass ratio of the pretreatment is 1:(6-15).

4. The method according to claim 1, characterized in that, In step (1), the pretreatment temperature is 130-150℃ and the pretreatment time is 1.5-2.5h.

5. The method according to claim 4, characterized in that, In step (1), the pretreatment temperature is 130-140℃.

6. The method according to claim 1, characterized in that, In step (2), the enzymatic hydrolysis reaction takes 6-72 hours.

7. The method according to claim 1, characterized in that, In step (3), the amount of ultra-high cross-linked adsorption resin added during the adsorption process is 2.5-20 wt%.

8. The method according to claim 1, characterized in that, In step (3), the ultra-high cross-linking adsorption resin is immersed in 5-15 times the volume of the resin added in industrial ethanol for desorption.

9. The method according to claim 1, characterized in that, In step (3), the adsorption time is 1-12 hours and the desorption time is 1-3 hours.

10. The method according to claim 1, characterized in that, In step (3), the recovered p-toluenesulfonic acid solution is used in step (1) for lignocellulose pretreatment.

Citation Information

Patent Citations

  • Efficient pretreatment process for all-component utilization of corn stalks

    CN112322677A

  • Method for treating volatile organic compounds by adopting hypercrosslinked adsorption resin

    CN115845555A

Cited By

  • Method for coupling agricultural and forestry waste pretreatment with low organic acid under assistance of low-concentration auxiliary agent and in-situ enzyme hydrolysis

    CN122012649A

  • Lignocellulose disassembling reagent for in-situ modification of lignin, high-quality lignin, lignocellulose disassembling method and glucose preparation method

    CN122104834A