Cross color suppression method and system for multi-color 3D printing
By establishing a steady-state operating benchmark in multicolor 3D printing, executing pre-switching retraction actions and new material injection, reconstructing the flow and path coordination relationship, and implementing dynamic pressure balance control, the problem of color mixing during material switching was solved, achieving clear color boundaries and stable mechanical properties.
Patent Information
- Application Number
- CN202610298976.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-03-12
- Publication Date
- 2026-05-15
AI Technical Summary
In multicolor 3D printing, color bleeding occurs when switching materials, resulting in blurred color boundaries and the penetration of impurities, which affects the appearance accuracy and interlayer bonding strength.
By establishing a steady-state operating benchmark before material switching, executing a pre-switching retraction action, guiding the new material to be smoothly injected into the melting chamber and fused with the residual melt, reconstructing the synergistic relationship between the extrusion flow rate and the nozzle movement path, implementing dynamic pressure balance control, generating local path fine-tuning instructions adapted to the characteristics of the new material, executing a gradual flow rate ramp-up, and completing post-switching status verification.
It effectively suppresses color bleeding in multicolor 3D printing, ensures clear and sharp color boundaries, uniform and stable mechanical properties in transition areas, avoids material waste and time delays, and improves the appearance quality and structural reliability of multicolor printed parts.
Smart Images

Figure CN122034336A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of 3D printing technology, specifically to a method and system for suppressing color bleeding in multi-color 3D printing. Background Technology
[0002] In the field of multicolor 3D printing technology, when a printing task requires switching between filaments of different colors or materials, traditional methods typically employ a simple stop-retract-refill strategy. Specifically, existing technologies often completely stop extrusion at the material switching point, perform a fixed-distance filament retraction to remove residual material from the molten chamber, then inject new material and perform a pre-extrusion period until clean, new material is observed flowing out before resuming printing. Some improvements introduce basic pressure monitoring or fixed-time delay mechanisms to attempt to ensure that the old material is completely expelled.
[0003] However, these methods have significant drawbacks: at the material switching interface, color bleeding inevitably occurs due to factors such as pressure fluctuations within the melt chamber, differences in the physical properties of the new and old materials, and instability of the flow front. This results in blurred transitions and color penetration at the color boundaries of the printed product, severely affecting the appearance accuracy. At the same time, uneven material mixing at the interface weakens the interlayer bonding strength, leading to a decrease in structural reliability. Summary of the Invention
[0004] This invention aims to provide a method and system for suppressing color bleeding in multi-color 3D printing, which effectively suppresses color bleeding in multi-color 3D printing, makes the color boundaries clear and sharp, and ensures uniform and stable mechanical properties in the transition area. At the same time, it avoids the material waste and time delay caused by excessive pre-extrusion in traditional methods.
[0005] To achieve the above objectives, the technical solution adopted by this invention is: a method for suppressing color bleeding in multi-color 3D printing, comprising: Establish a steady-state operating baseline before material switching, and obtain the current material's extrusion flow rate, melt chamber pressure, nozzle position, and direction of movement; Based on the steady-state operating benchmark, a pre-switching retraction action is performed to reduce the residual pressure in the melting chamber. In response to the pre-switching retraction result, the new material is smoothly injected into the melting chamber and fused with the residual melt. Based on the injection state of the new material, the synergistic relationship between the extrusion flow rate and the nozzle movement path is reconstructed. Combined with the reconstructed synergistic relationship, dynamic pressure balance control is implemented to stabilize the pressure in the melt chamber. Under stable pressure, a local path fine-tuning command is generated to adapt to the properties of the new material. Using the fine-tuned path, a gradual flow ramp is executed to make the extrusion flow reach the target value. Based on the traffic surge results, complete the post-switch status verification and return to normal printing.
[0006] Preferably, establishing a steady-state operating baseline before material switching includes: Monitor the current continuous extrusion rate of the material; While the monitored extrusion rate remains constant, the pressure balance level inside the melt chamber is measured. Record the current position and direction vector of the nozzle, and determine the spatial coordinates of the material switching trigger point based on the recorded vector.
[0007] Preferably, the pre-switch rollback action includes: The total pullback amount is set based on the steady-state flow rate; The retraction speed curve is dynamically adjusted based on the pressure balance level inside the melting chamber. By utilizing the nozzle's current position and direction of motion vector, a retraction action is initiated when approaching the switching point, responding to a dynamically adjusted retraction speed curve, and monitoring the pressure drop trend during the retraction process.
[0008] Preferably, the method of guiding the smooth injection of new material into the molten cavity includes: Initiate the pre-feeding of the new material to establish initial contact, and gradually increase the heating power according to the pre-feeding state and the characteristics of the new material; Under conditions of increased heating power, control the degree of shear mixing at the interface between the old and new melts; Based on the results of shear mixing control, micro-extrusion was performed to verify melt continuity.
[0009] Preferably, the reconstructed coordination relationship between the extrusion flow rate and the nozzle movement path includes: Initialize the target extrusion flow rate based on the properties of the new material; By utilizing the initial target extrusion flow rate and melt chamber pressure, viscosity shifts caused by temperature changes are dynamically compensated. Based on the compensated viscosity shift, the nozzle movement speed is adjusted synchronously to maintain linewidth consistency; The first segment of printing is performed along the optimized transition path, based on the adjusted printhead movement speed.
[0010] Preferably, the implementation of dynamic pressure balance control includes: Establish a monitoring window for the rate of pressure change in the molten zone; Adjust the propulsion output based on the monitored rate of pressure change; The heating compensation strategy is optimized by combining the adjusted propulsion output and temperature field distribution; Based on the optimized heating compensation strategy and pressure change trend, the pressure is determined to be stable and the transition control is allowed to be discontinued.
[0011] Preferably, the method for generating local path fine-tuning instructions adapted to the properties of the new material includes: Extract the morphological characteristics of the initial extrusion section of the new material; Based on the extracted morphological features, the source of path deviation is identified by comparing the design value with the measured value; Based on the identified path deviation sources, a local path offset vector is constructed to compensate for flow lag; Update the short-term path cache in the motion controller according to the constructed local path offset vector.
[0012] Preferably, the implementation of progressive traffic ramping includes: Set the total traffic ramp-up time and segment intervals; Based on the set total duration, an S-shaped curve is used to plan the flow increment sequence; By utilizing the planned flow increment sequence, the heating power is adjusted synchronously to match the flow growth rate; By adjusting the heating power, the actual flow response is monitored and the ramp-up curve is dynamically corrected.
[0013] Preferably, the post-switching status verification includes: Acquire the first image of the formed quality after the switching is completed; Based on the acquired images, image texture features are analyzed to evaluate the fusion quality; In response to the evaluation of fusion quality, reset all temporary control parameters to their default settings; Based on the reset parameter status, record the entire switching process log and grant permission for the next trigger.
[0014] On the other hand, this invention proposes a color crosstalk suppression system for multicolor 3D printing, comprising: The material switching control module is used to establish a steady-state operating baseline before material switching and to obtain the current material's extrusion flow rate, melt chamber pressure, nozzle position, and direction of movement. The injection guidance module is used to perform a pre-switching retraction action based on the steady-state operating benchmark, reduce the residual pressure in the melting chamber, respond to the pre-switching retraction result, and guide the new material to be smoothly injected into the melting chamber and fuse with the residual melt. The dynamic balancing module is used to reconstruct the synergistic relationship between the extrusion flow rate and the nozzle movement path by referring to the injection state of the new material. Based on the reconstructed synergistic relationship, dynamic pressure balance control is implemented to stabilize the pressure in the melt chamber. The path fine-tuning module is used to generate local path fine-tuning instructions to adapt to the properties of new materials under stable pressure. Using the fine-tuned path, a gradual flow ramp is executed to make the extrusion flow reach the target value. The normal regression module is used to verify the status after the switch based on the traffic crawling results, and print the normal regression status.
[0015] Compared with the prior art, the beneficial effects of the present invention are as follows: This invention achieves precise control of the material switching process by establishing a steady-state operating benchmark before material switching, executing a pre-switching retraction action, guiding the smooth injection of new material and its fusion with the residual melt, reconstructing the synergistic relationship between extrusion flow rate and nozzle movement path, implementing dynamic pressure balance control, generating local path fine-tuning instructions adapted to material characteristics, executing progressive flow rate ramp-up, and completing post-switching state verification. This systematic approach effectively suppresses color bleeding in multi-color 3D printing, resulting in clear and sharp color boundaries and uniform and stable mechanical properties in transition areas. It also avoids material waste and time delays caused by excessive pre-extrusion in traditional methods, significantly improving the appearance quality and structural reliability of multi-color printed parts. Attached Figure Description
[0016] Figure 1 A flowchart of the color mixing suppression method for multicolor 3D printing according to the present invention; Figure 2 This is a flowchart of the color mixing suppression system for multicolor 3D printing according to the present invention. Detailed Implementation
[0017] The following description is intended to disclose the invention and enable those skilled in the art to implement it. The preferred embodiments described below are merely examples, and other obvious variations will occur to those skilled in the art.
[0018] like Figure 1 As shown, this embodiment provides a method for suppressing color bleeding in multi-color 3D printing. This method achieves a fast, clean, and continuous transition between different colors / materials by coordinating and controlling the extrusion flow rate, dynamic response of the cavity pressure, and nozzle path planning during material switching. Specifically, it includes the following steps: Establish a steady-state operating baseline before material switching, and obtain the current material extrusion flow rate, melt chamber pressure, nozzle position and movement direction; specifically including: monitoring the current material continuous extrusion rate; when the monitored extrusion rate remains constant, measuring the pressure balance level inside the melt chamber; recording the current nozzle position and movement direction vector, and determining the spatial coordinates of the material switching trigger point based on the recorded vector.
[0019] By establishing a stable operating baseline before material switching, key parameters of the system under normal operating conditions can be accurately grasped, providing a reliable reference for subsequent switching operations. This technology ensures the accuracy and timing of switching decisions, effectively avoiding premature or late switching due to system fluctuations or positioning deviations, thereby reducing flow instability in the transition area, improving the uniformity and continuity of the material interface, and reducing the risk of color bleeding and material breakage.
[0020] Based on the steady-state operating baseline, a pre-switching retraction action is performed to reduce the residual pressure in the melting chamber. Specifically, this includes: setting the total retraction amount based on the steady-state flow rate; dynamically adjusting the retraction speed curve by referring to the pressure balance level inside the melting chamber; and initiating the retraction action when approaching the switching point by using the nozzle's current position and movement direction vector, responding to the dynamically adjusted retraction speed curve, and monitoring the pressure drop trend during the retraction process.
[0021] By controlling the total amount, speed, and timing of the retraction action, residual pressure within the molten chamber is effectively released, reducing the amount of old material residue and the risk of backflow. This technology avoids material leakage caused by insufficient retraction or vacuum suction imbalance caused by excessive retraction, ensuring stable retraction of the melt at the switching front face, creating favorable conditions for the clean injection of new material, significantly reducing the probability of color bleeding and improving interface clarity.
[0022] In response to the pre-switch retraction result, the new material is guided to be smoothly injected into the melting cavity and fused with the residual melt. Specifically, this includes: initiating the pre-feeding of the new material to establish initial contact; gradually increasing the heating power according to the pre-feeding state and the characteristics of the new material; controlling the degree of shear mixing at the interface between the new and old melts while the heating power is increased; and performing micro-extrusion operation to verify the continuity of the melt based on the control result of the degree of shear mixing.
[0023] By guiding the injection of new materials in an orderly manner and controlling their fusion process with the residual melt, flow blockage and pressure surges caused by cold material impact or differences in thermal inertia are effectively avoided. This technology achieves a gradual connection between new and old materials at the molecular level, suppresses eddies and entrapment at the interface, ensures smooth advancement of the melt front, significantly reduces color penetration and cavitation defects, and improves the density and visual purity of the transition region.
[0024] Based on the injection state of the new material, the coordination relationship between the extrusion flow rate and the nozzle movement path is reconstructed. Specifically, this includes: initializing the target extrusion flow rate according to the characteristics of the new material; dynamically compensating for viscosity shifts caused by temperature changes using the initialized target extrusion flow rate and melt chamber pressure; synchronously adjusting the nozzle movement speed to maintain linewidth consistency based on the compensated viscosity shift; and performing the first segment printing along the optimized transition path according to the adjusted nozzle movement speed.
[0025] By matching the rheological properties of the new material with the nozzle motion parameters in real time, the problem of flow mismatch and path deviation caused by material switching is effectively eliminated. This technology ensures the continuity and stability of the extruded melt in terms of geometry, avoids the under-extrusion, over-extrusion, or edge burrs commonly seen in the first stage of printing, significantly improves the dimensional accuracy and surface uniformity of the transition area, and ensures that the printed lines after color switching are straight, full, and have clear boundaries.
[0026] By combining the reconstructed synergistic relationship, dynamic pressure balance control is implemented to stabilize the pressure in the melting chamber. Specifically, this includes: establishing a monitoring window for the rate of change of pressure in the melting zone; adjusting the propulsion output based on the monitored rate of change of pressure; optimizing the heating compensation strategy based on the adjusted propulsion output and temperature field distribution; and determining the pressure stabilization state and allowing the exit from transition control based on the optimized heating compensation strategy and pressure change trend.
[0027] By monitoring pressure dynamics in real time and coordinating the adjustment of propulsion and heating strategies, pressure oscillations caused by flow inertia and thermal response lag during the initial material switching phase are effectively suppressed. This technology achieves rapid stabilization of the force field within the molten cavity, avoiding overflow caused by sudden pressure increases or flow interruptions caused by sudden pressure drops. It significantly enhances the continuity and uniformity of melt delivery, providing a stable kinetic basis for forming a dense, defect-free transition interface.
[0028] Under stable pressure, local path fine-tuning instructions adapted to the characteristics of the new material are generated. Specifically, these instructions include: extracting the morphological features of the initial extrusion section of the new material; identifying path deviation sources by comparing the design values with the measured values based on the extracted morphological features; constructing a local path offset vector to compensate for flow hysteresis based on the identified path deviation sources; and updating the short-term path cache in the motion controller according to the constructed local path offset vector.
[0029] By dynamically correcting the printing path based on feedback from the actual extrusion morphology, the flow lag and corner accumulation problems caused by the viscoelasticity differences of the new material are effectively compensated. This technology improves the forming accuracy of complex geometric contours, avoids line offset, edge blurring, or dimensional distortion in transition areas, ensures that the initial trajectory after color switching closely matches the design model, and significantly improves the detail reproduction and surface consistency of multi-color components.
[0030] Using the fine-tuned path, a gradual flow ramp-up is executed to bring the extruded flow rate to the target value. Specifically, this includes: setting the total flow ramp-up time and segmented intervals; using an S-curve to plan the flow increment sequence based on the set total time; adjusting the heating power synchronously to match the flow growth rate using the planned flow increment sequence; and monitoring the actual flow response and dynamically correcting the ramp-up curve by adjusting the heating power.
[0031] By smoothly and gradually increasing the flow rate and coordinating the adjustment of heat input, jetting or stringing phenomena caused by sudden changes in flow rate during the startup phase of new materials are avoided. This technology achieves a seamless transition from the extrusion rate transition state to stable printing, effectively preventing melt fracture, bubble entrapment, and weakening of interlayer bonding. It significantly improves the density and geometric continuity of the initial deposition section after color switching, ensuring a smooth recovery of the printing process to full power operation.
[0032] Based on the traffic surge results, complete the post-switch status verification and return to normal printing; specifically, this includes: acquiring the first image of the formed quality after the switch is completed; analyzing the image texture features based on the acquired image to evaluate the fusion quality; in response to the evaluated fusion quality, resetting all temporary control parameters to default settings; and recording the entire switch process log based on the reset parameter status and granting permission for the next trigger.
[0033] By automatically evaluating the switching results and resetting the system status through visual feedback, the verifiability of material transition quality and the timely zeroing of control parameters are ensured. This technology effectively avoids interference from residual control strategies in subsequent printing stages, guarantees a seamless switch from transition mode to normal mode during the printing process, and enables operation traceability and improves system reliability through log recording, ensuring the stability and consistency of long-term multicolor printing operation.
[0034] On the other hand, this invention proposes a color crosstalk suppression system for multi-color 3D printing, such as... Figure 2 As shown, it includes: The material switching control module is used to establish a steady-state operating baseline before material switching and to obtain the current material's extrusion flow rate, melt chamber pressure, nozzle position, and direction of movement. The injection guidance module is used to perform a pre-switching retraction action based on the steady-state operating benchmark, reduce the residual pressure in the melting chamber, respond to the pre-switching retraction result, and guide the new material to be smoothly injected into the melting chamber and fuse with the residual melt. The dynamic balancing module is used to reconstruct the synergistic relationship between the extrusion flow rate and the nozzle movement path by referring to the injection state of the new material. Based on the reconstructed synergistic relationship, dynamic pressure balance control is implemented to stabilize the pressure in the melt chamber. The path fine-tuning module is used to generate local path fine-tuning instructions to adapt to the properties of new materials under stable pressure. Using the fine-tuned path, a gradual flow ramp is executed to make the extrusion flow reach the target value. The normal regression module is used to verify the status after the switch based on the traffic crawling results, and print the normal regression status.
[0035] In addition, the modules described above are also used to implement other steps of the aforementioned method for suppressing color bleeding in multi-color 3D printing, as follows: Step 1: Establish steady-state operating baseline before material switching Before initiating any material switching operation, it must first be confirmed that the material currently in use is in a stable conveying state. The goal of this stage is to acquire and record the key operating characteristic values of the material that is about to be phased out under normal operating conditions, as a reference for subsequent adjustments.
[0036] Step 1.1: Monitor the continuous extrusion rate of the current material. While the nozzle moves along a predetermined trajectory, the volumetric output of the material per unit time from the inlet at the heated end to the outlet of the nozzle is continuously collected. This value is calculated by measuring the drive wheel speed using a rotary encoder mounted on the feeding mechanism, combining it with the known pitch diameter of the feeding gear to obtain the instantaneous feed length, and then multiplying it by the cross-sectional area of the material to obtain the volumetric flow rate. ; in, For the radius of the material wire, This represents the measured feed rate. The formula reflects the principle of volume conservation; under no-slip conditions, the volume of material input into the melt chamber should equal the theoretical extrusion volume. In practice, due to compression deformation and back pressure, there is a certain lag; therefore, the raw data needs to be low-pass filtered to extract the smoothed representative values.
[0037] Step 1.2: Determine the pressure balance level inside the melting cavity. The static pressure value in the molten pool region inside the heating block is detected using an embedded miniature pressure sensor. This pressure is formed by the accumulation of material after it softens due to heat under the action of propulsion force, and its magnitude is directly related to the melt's fluidity and resistance to backflow. When the extrusion rate remains constant, if the pressure reading fluctuates less than a preset threshold within three consecutive sampling periods... If the pressure is within ±5 kPa, the system is considered to have entered a pressure equilibrium state. This state means that the melt is evenly distributed within the cavity, the shear stress tends to be stable, and there will be no sudden release due to local pressure buildup, thus providing reliable initial conditions for subsequent active control.
[0038] Step 1.3: Record the current position and direction vector of the nozzle. With the help of the device's built-in motion control system, the three-dimensional spatial position of the nozzle in the coordinate system of the construction platform can be read in real time. and its current movement direction unit vector , among which angle These represent the angles between the direction of motion and the X, Y, and Z axes, respectively. This information is not only used for trajectory tracking, but more importantly, it prepares the basis for predicting the geometric characteristics near the switching point. Especially in path segments with high curvature, where the direction changes drastically, failure to identify this in advance may lead to inappropriate switching timing, causing material buildup or stringing.
[0039] Step 1.4: Determine the spatial coordinates of the material switching trigger point. Based on the boundary outline of the color area that is about to be completed, and combined with the current position and direction of travel obtained in step 1.3, the optimal starting position for material switching is calculated. The selection of this point follows two principles: first, it must be located at the end of the current color-filled area but before entering the next color area; second, it should be situated on a straight segment or at a location with minimal curvature to reduce disturbances caused by acceleration and deceleration. Specifically, this is achieved by analyzing the curvature of the next path segment. Choose to satisfy The nearest feasible point as The switching point determined in this way not only ensures the accuracy of color zoning, but also reserves sufficient response time window for subsequent dynamic adjustment.
[0040] By comprehensively understanding the current material's flow rate, pressure, location, and path characteristics, the system can establish a quantifiable operating baseline. This baseline not only determines when to initiate a switchover but also provides a reference standard for subsequent parameter adjustments in each stage. In particular, the acquired data... and This value will be used in the next phase to set pullback targets and ensure the transition process is controllable.
[0041] Step 2: Perform a pre-switchback to reduce residual pressure. Once it is confirmed that the current material is in a stable operating state and the switching point location has been identified, the next step is to enter the active intervention phase. The core task of this phase is to reach... Previously, the amount of material and its internal pressure in the melting chamber were reduced in a controlled manner to prevent excessive melt from being passively extruded after the material was interrupted, which would cause color tailing. This process was not simply about quickly pulling back the wire, but rather about designing a gradual withdrawal curve based on the data collected in the early stages, taking into account both pressure release efficiency and avoiding the risk of air being sucked into the vacuum.
[0042] Step 2.1: Set the total pullback amount based on steady-state flow. Based on the measurements in step 1.1 Calculate the volume of melt to be removed. Considering the compressibility and viscoelasticity of the molten material, complete emptying is neither realistic nor necessary. The goal is to remove the excess material accumulated in the cavity, reducing the remaining pressure below the critical overflow threshold. The retraction volume is set to be proportional to the original flow rate. ; in, This is an empirical coefficient (taken as 0.6-0.8), reflecting the material's shrinkage efficiency at high temperatures; The expected material residence time, i.e., the time interval from when the feed stops to when the new material arrives at the nozzle, can be estimated using historical data. The significance of this formula is that the energy accumulated after high-flow operation is greater, requiring a larger retraction to offset the inertial effect; otherwise, even if the feed is stopped, the residual pressure will still push the melt to continue flowing out.
[0043] Step 2.2: Dynamically adjust the retraction speed curve based on the melting pressure. Unlike the fixed-speed withdrawal method, a variable-speed strategy is used here, and its rate of change over time follows an exponential decay law: ; in, The initial pullback speed is determined by the material type and temperature. The decay rate constant is the same as the value measured in step 1.2. The higher the related stress, The smaller the value, the faster the initial pullback, allowing for rapid pressure release. The advantage of this non-linear design is that the initial high-speed pull can quickly break the melt bridging structure, reducing the risk of blockage; the subsequent deceleration avoids air being sucked into the nozzle due to excessive negative pressure, forming bubbles or interrupting subsequent material supply.
[0044] Step 2.3: Initiate the pullback action when approaching the switching point. The retraction operation does not begin at any arbitrary position, but rather at the distance from the nozzle. There are also specific itineraries The movement is initiated at a certain time. This distance is determined by both the material response delay time and the current moving speed. ; in, This represents the current movement speed of the nozzle. The time delay from issuing the retraction command to the actual effective displacement includes factors such as motor response and elimination of transmission backlash. Using the motion direction information provided in step 1.3, the system can predict the nozzle trajectory and issue the retraction command at the appropriate time, ensuring that the nozzle arrives at its destination safely. At this point, the pullback has been completed by about 70%-80%. The pressure has decreased significantly, but some melt connection is still maintained, which is conducive to the subsequent delivery of new materials.
[0045] Step 2.4: Monitor the downward pressure trend during the pullback. Throughout the entire pullback, pressure sensor signals were continuously read and plotted. The curve showing the change over time. Ideally, the pressure should exhibit a monotonically decreasing trend and approach a safe lower limit at the end of the retracement. (e.g., 10 kPa). If the pressure drops slowly or rebounds, it indicates insufficient retracement, and the retracement time may need to be extended or the magnitude increased; conversely, if the pressure drops sharply to a negative value, it indicates excessive retracement, which may introduce air.
[0046] Through the above operations, a shift from passive waiting to proactive control is achieved. Retreat is no longer an isolated action, but a dynamic response process closely linked to the previous operational state. The set... and All data are derived from real-world measurements, enhancing adaptability. Furthermore, path prediction allows for precise control of the pullback initiation timing, preventing uncontrolled pressure due to inappropriate timing.
[0047] Step 3: Guide the new material to be injected smoothly and fuse with the residual melt. After the old material has completed its phased withdrawal, the new material introduction phase begins. The key to this phase is how to ensure that the new color / material smoothly enters the melting chamber with the help of the wire switching device, and achieves a smooth transition with the remaining material in the chamber, without creating voids or breaks, or causing mixing and contamination due to forced extrusion.
[0048] Step 3.1: Initiate the pre-feeding of the new material to establish initial contact. After confirming that the retraction action has reduced the melt chamber pressure to the target range, the new material feeding mechanism is activated at a low speed, below the normal printing speed. Push the wire forward. This speed is generally set to 30%-50% of the normal extrusion speed. The purpose is to allow the tip of the new material to slowly approach the heating zone, avoiding pressure shock caused by sudden acceleration. Pre-feed distance. According to the distance from the nozzle to the melting zone Sure: ; in, For an additional extension (approximately 1-2 mm), ensure the wire tip actually enters the heat-affected zone and begins to soften. Complete melting is not the goal at this stage; the aim is simply to create a malleable tip to prepare for subsequent fusion. Feeding at full speed too early may cause the high-temperature area to cool due to the sudden influx of cold material, affecting flowability.
[0049] Step 3.2: Gradually increase the heating power to match the melting requirements of the new material. Because wires of different colors or materials have varying glass transition temperatures, heat capacities, and thermal conductivity, existing heating settings may not be suitable for new materials. Therefore, during pre-feeding, the corresponding temperature control curve is retrieved based on the material identification information, and the heating block temperature is gradually increased to the target value. The heating process employs a segmented ramp method: ; in, The current temperature. This is the thermal response time constant, which depends on the heating element power and the heat dissipation environment. Slow heating prevents the outer layer from overheating and carbonizing while the inner core remains uncooked, ensuring consistent melting. The temperature rises to... When the level reaches 90%, further increases should be paused, and the final adjustments should be made after signs of recovery from the squeeze are observed.
[0050] Step 3.3: Controlling the degree of shear mixing at the interface between the old and new melts As the new material gradually melts and comes into contact with the remaining old material, a transition interface is formed between the two. To prevent color mixing caused by vigorous stirring, the propulsion acceleration of the screw or piston is limited to no more than [a certain value]. This causes the shear rate to Maintain at a low level: ; in, To accelerate, This represents the effective spacing between interfaces. By maintaining a small... This allows two melts to superimpose in a laminar flow manner, naturally merging through diffusion rather than turbulent mixing.
[0051] Step 3.4: Verify melt continuity and confirm flow status through micro-extrusion. After the new material has fully entered the molten zone, a short, micro-extrusion operation is performed, outputting a very small amount of melt (approximately 0.01 mL) to a non-forming area (such as a waste trough or support edge). This is to check whether the melt channel is unobstructed and whether there is any air resistance or cold material blockage. If the melt can be discharged stably, it indicates that a continuous melt path has been formed, and the system can enter the formal extrusion stage; if intermittent or no material occurs, the pre-feeding should be repeated and the temperature appropriately increased.
[0052] Step 4: Reconstruct the synergistic relationship between extrusion flow rate and nozzle path Once the new material has been injected and its flow is confirmed to be unobstructed, the system enters the final forming stage. The task of this stage is to re-establish a stable extrusion output and match the nozzle movement trajectory with the material supply rhythm, ensuring that a complete and uniform line can be formed on the first segment of the path after the switch, and eliminating the phenomenon of weak or accumulated lines at the beginning.
[0053] Step 4.1: Initialize the target extrusion flow rate based on the new material properties Refer to the settings in step 3.2 Given the material type, refer to the table to obtain the recommended extrusion flow rate for that material under standard conditions. This value is determined by parameters such as wire diameter, layer thickness, and printing speed, and its basic expression is as follows: ; in, To the expected extrusion linewidth, For floor height, This represents the printing speed for the current path segment. Since the new material has just entered the system, the actual flow rate may be lower than this target value; therefore, an initial setting slightly lower than this is used. startup traffic It then climbs at a predetermined rate to avoid drive malfunction or pressure fluctuations caused by excessive instantaneous demand.
[0054] Step 4.2: Dynamically compensate for viscosity shift caused by temperature changes Although the heating block has been adjusted to However, the actual melt temperature may still exhibit a gradient distribution, affecting fluidity. Therefore, a real-time viscosity correction factor is introduced. Its value is derived by inversely from the pressure sensor reading. According to Poiseuille's law, in circular pipe flow, the pressure drop... With viscosity Proportional: ; in, The length of the flow channel. Where is the pipe radius. When... and When known, it can be monitored Estimation And compared with the ideal value, we obtain .like This indicates that the melt is too thick and needs to be increased appropriately. Alternatively, the insulation time can be extended; conversely, the target flow rate can be reduced to prevent over-squeezing. This compensation mechanism allows flow control to adapt to the actual rheological state of the material.
[0055] Step 4.3: Synchronously adjust the nozzle movement speed to maintain consistent line width. If the nozzle continues to travel at its original speed before the flow rate has fully stabilized, it can easily lead to insufficient or excessive extrusion. Therefore, the nozzle speed should be adjusted within the initial few millimeters of the path after switching. Reduced proportionally: ; in, This represents the current measured traffic volume. As... Approaching step by step It also subsequently rebounded to the nominal value.
[0056] Step 4.4: Perform the first segment printing along the optimized transition path. Considering the possibility of slight height differences or surface unevenness near the switching point, printing directly along the original path might affect the adhesion. Therefore, after switching, the previous... Perform local path corrections on each path point (such as the first 5) to slightly raise their elevation. (Approximately 0.02 mm), and extend the dwell time at the first point. (Approximately 50ms) to enhance the initial layer adhesion. This corrected path is applied only to the transition section, after which the original design trajectory is immediately restored. In this way, the initial connection is ensured to be robust without affecting the overall geometric accuracy. By reconstructing the flow reference, compensating for rheological deviations, coordinating the motion rhythm, and optimizing the initial path, the system successfully achieved a return from the transition state to stable printing.
[0057] Step 5: Implement dynamic pressure balance control across material interfaces After the new material begins to participate in the forming process, although the extrusion flow rate and nozzle movement have been initially coordinated, the system is still in a transitional state due to the differences in the physical properties of the old and new materials and the residual substances that have not been completely discharged from the melt cavity. If the system directly enters the full-power printing mode at this time, microcracks, delamination, or color penetration may easily occur at the interface due to uneven internal stress release or unstable flow front. Therefore, a pressure regulation mechanism based on real-time feedback needs to be introduced to actively intervene in the force field distribution in the melt cavity in the initial stage after the switch, so that it gradually approaches the target steady state.
[0058] Step 5.1: Establish a monitoring window for the rate of change of pressure in the molten zone. From the moment the new material first contacts the construction surface, a period of time is initiated. The pressure monitoring cycle is typically 0.8-1.5 seconds. During this period, embedded sensor data is read at a higher sampling frequency than usual to obtain the pressure value. The sequence of changes over time, and its instantaneous rate of change: ; This derivative reflects the system's sensitivity to external disturbances. If An excessively large value indicates drastic fluctuations in the flow process; if it remains close to zero for an extended period but with frequent sign alternation, it suggests the system is on the verge of oscillation. This can be addressed by setting a dynamic threshold. This allows the system to determine whether the system has entered a relatively stable range. The existence of this monitoring window enables the control system to detect microscopic pressure fluctuations invisible to the naked eye, providing a basis for subsequent adjustments.
[0059] Step 5.2: Adjust the thrust output according to the pressure gradient trend When detected When the force deviates significantly from the ideal range, the drive mechanism immediately corrects the axial thrust applied to the wire. Specifically, if the pressure rises too quickly ( This indicates that the melt buildup rate exceeds the discharge capacity. In this case, the thrust should be appropriately reduced to prevent overpressure from causing the melt to overflow from the nozzle edge and contaminate the surrounding area; conversely, if the pressure drops rapidly ( If the output is insufficient, it indicates that the thrust needs to be increased to maintain continuous flow. Thrust adjustment amount. It is directly proportional to the degree of deviation: ; in, This is the proportional gain coefficient, determined by material stiffness and transmission efficiency; The historical average rate of change represents the baseline level under normal operating conditions.
[0060] Step 5.3: Optimize heating compensation strategy based on temperature field distribution Pressure fluctuations stem not only from mechanical pushing but also from the non-uniformity of heat conduction. Particularly during multi-material switching, the entry of cold material into the high-temperature zone causes localized cooling, forming "cold spots" and increasing flow resistance. To mitigate this effect, while performing step 5.2, differentiated power allocation is implemented for different areas of the heating block based on the surface temperature spectrum provided by the infrared thermography module. For sectors with lower temperatures, the local heating intensity is temporarily increased. : ; in, This is a thermal compensation factor, which is related to the material's specific heat capacity and thermal diffusivity. The measured temperature is for the corresponding location. This zoned temperature control method can effectively shorten the thermal equilibrium time and avoid abnormal shear thinning caused by temperature differences, thereby stabilizing the pressure output.
[0061] Step 5.4: Determine if the pressure has stabilized and allow the transitional control to be discontinued. The system is considered to have stabilized when multiple consecutive sampling points meet the following conditions: (1) Current pressure Fall into the preset working area ; (2) The absolute value of the pressure change rate is lower than And the duration exceeds (e.g., 300ms); (3) Thrust correction Approaching zero.
[0062] Once all three indicators are met simultaneously, the dynamic pressure control mode is shut down, active intervention ceases, and the system switches to the regular printing process. This decision-making logic ensures that the protection mechanism only terminates after true mechanical equilibrium is achieved, preventing premature exit and secondary disturbances.
[0063] By precisely sensing and responding to pressure change trends, the system can achieve a smooth transition at the molecular flow level. In particular, the coupled regulation of mechanical thrust and thermal input breaks through the limitations of single-dimensional control and improves overall stability.
[0064] Step Six: Generate local path fine-tuning instructions adapted to material properties Even if the melt output stabilizes, the original path followed by the nozzle may no longer be entirely suitable for the actual flow behavior of the current material. Because wires of different colors or materials differ in viscoelasticity, cooling rate, and adhesion characteristics, using a uniform path may lead to problems such as edge burrs, corner buildup, or surface distortion. Therefore, after pressure balancing, the initial trajectory needs to be adaptively modified to better conform to the forming characteristics of the new material, thereby improving the geometric accuracy and surface quality of the transition region.
[0065] Step 6.1: Extract the morphological characteristics of the initial extrusion section of the new material. As the nozzle begins to move along the new area path, a high-speed imaging device installed near the nozzle captures real-time images of the extrusion line. The line width within the first 10-20mm length is analyzed in detail. Edge sharpness and center offset These parameters are extracted using image processing algorithms, such as using edge detection operators to locate the contour boundary and then calculating the distance between two points to obtain the actual width. The resulting data is used to evaluate the degree of matching between the current path and material behavior.
[0066] Step 6.2: Identify the source of path deviation by comparing design values with measured values. The information obtained in step 6.1 Compared with theoretical design value Compare, if the relative error If the deviation exceeds the allowable range (e.g., ±8%), further investigation is needed to determine the source of the deviation. If a significant center offset is also observed, the problem may be due to misalignment of the path or nozzle blockage; if only the line width is abnormal but the position is accurate, it is more likely due to a mismatch between flow rate and speed.
[0067] Step 6.3: Construct local path offset vectors to compensate for flow hysteresis For path segments with large curvature (such as inner rounded corners and acute angle transitions), material inertia often leads to excessive extrusion on the outer side and insufficient extrusion on the inner side, creating a "banana effect." To counteract this deformation, based on the current direction of movement... and radius of curvature Calculate a compensation vector perpendicular to the trajectory. : ; in, This is a material flow correction factor, calibrated from previous tests; Current printing speed; This is the path normal unit vector (pointing to the center of curvature). This vector is superimposed on the original path point coordinates to form a new trajectory. By making a slight pre-offset, the melt front edge is made closer to the ideal profile, reducing the need for subsequent adjustments.
[0068] Step 6.4: Update the short-term path cache in the motion controller The revised path data is written to the temporary buffer of the motion control unit, replacing the original planned path. Path points ( The scope of the correction is determined, generally 15-30 points. The update operation is completed without stopping the printhead movement, ensuring continuity of action. The new path is only effective during this transition phase and automatically becomes invalid after the printing extends to a safe distance, restoring the global path planning.
[0069] Step 7: Perform a gradual traffic ramp-up with multiple parameters linked. Although the system has achieved pressure balance in step five and completed path adaptation in step six, the extrusion rate has not yet reached the final target value. Immediately switching to full output would still cause a transient shock, disrupting the newly established stable state. Therefore, a smooth flow rate growth curve must be designed to gradually increase the supply rate of the new material to the design level.
[0070] Step 7.1: Set the total traffic ramp-up time and segment intervals. Determine the initial flow rate based on the material type and layer thickness parameters. Rise to target traffic Total time required This duration is determined by the transport delay of the melt from the inlet to the outlet. and thermal activation time Joint decision: ; in, This is a safety margin factor (taken as 1.3-1.7) used to cope with sudden disturbances. Divided into several equal-length time periods An incremental traffic update is performed once per time period, forming a step-like upward process. The number of segments should not be too few (to avoid excessively large jumps) nor too many (to prevent response lag), generally 6-10 segments are appropriate.
[0071] Step 7.2: Plan the flow increment sequence using an S-curve To reduce mechanical shock, flow rate growth is not linear, but rather an S-shaped (sigmoid) curve is used as a template: ; in, The steepness of the control curve's ascent, This represents the midpoint. The function is characterized by a slow initial growth rate, accelerated growth in the middle stage, and a slowdown again at the end, consistent with the thermodynamic response characteristics of most materials—slow molecular chain rearrangement in the initial stage, followed by increased fluidity, and then stabilization near saturation. The resulting flow command is more natural, which is beneficial for extending equipment life and improving forming consistency.
[0072] Step 7.3: Synchronously adjust the heating power to match the flow rate increase rhythm. As the extrusion rate increases, the volume of material to be melted per unit time increases, leading to a rise in heat demand. If the heating power remains constant, the molten pool temperature may drop, increasing the risk of blockage. Therefore, the heating output should be increased proportionally with each increase in flow rate. : ; in, Based on heating power, The heat compensation per unit flow rate is derived from the material's specific heat capacity and latent heat of fusion. This linkage ensures a dynamic balance between energy input and material throughput, maintaining a constant melting efficiency.
[0073] Step 7.4: Monitor actual flow response and dynamically adjust the ramp curve. During the flow ramp-up process, the measured extrusion volume was continuously collected. and the theoretical curve Compare. If found If the performance consistently falls short of expectations and the deviation exceeds a threshold, the time interval for subsequent stages should be appropriately extended to allow for greater responsiveness; if Reaching the target ahead of schedule allows for the compression of the remaining time period and accelerates the process. This closed-loop correction mechanism enhances resistance to external disturbances (such as voltage fluctuations and changes in ambient temperature), ensuring that the final output accurately meets the target.
[0074] Step 8: Complete post-switch status verification and system return to normal. Even after the extrusion flow rate of the new material successfully climbs to the target value and remains there for a period of time, the switchover process is not yet completely finished. A comprehensive status check must be conducted to confirm that all key parameters have returned to normal ranges and that no potential problems remain. Only after multiple verifications have been passed can the switchover be considered successfully completed, and control be returned to the main printing cycle to resume normal operation.
[0075] Step 8.1: Acquire the first segment forming quality image after the switching is completed. After the printhead completes its transition path and enters the stable zone, the imaging system is triggered to capture a high-resolution photograph of the printed line, approximately 20-30mm in length. Key areas of focus include the starting connection point, the first bend, and the middle straight section. The image must clearly show the integrity of the line edges, surface smoothness, and the presence of defects such as bubbles, discontinuities, or color mixing. This visual record is not only used for this verification but can also be archived for subsequent batch comparison analysis.
[0076] Step 8.2: Analyze image texture features to evaluate fusion quality The acquired image is converted to grayscale and filtered, and the standard deviation of the brightness distribution is extracted. and texture entropy As an evaluation indicator. If Too high a height indicates uneven surface roughness; if An abnormally high value may indicate the presence of micropores or delamination within the sample. These values are compared with the data of qualified samples in the standard sample library. If the deviation is within the allowable range, the fusion is considered good; otherwise, it is marked as abnormal, triggering an alarm.
[0077] Step 8.3: Reset all temporary adjustment parameters to default settings. After confirming that the status is normal, sequentially disable the previously enabled transition-specific functions, including dynamic pressure compensation, path fine-tuning buffer, flow ramp controller, and zone heating mode. Simultaneously, restore the configuration of the drivers, heating modules, and sensors to the universal print parameter set. This reset operation ensures that residual settings will not affect the next switchover or other print jobs, maintaining a consistent operating environment.
[0078] Step 8.4: Record the entire switching process log and grant permission for the next trigger. All key events of this material switchover were compiled into a structured log in chronological order, covering: the start time of the switchover, the execution status of each stage, parameter adjustment trajectory, anomaly detection results, and final conclusions. This log is stored locally and accessible to a remote monitoring platform via a network interface. After archiving, the interlock mechanism is released, allowing the system to respond to the next material switchover request, thus completing a closed-loop management cycle.
[0079] Visual verification ensures the reliability of the results, parameter resetting guarantees system cleanliness, and logging supports traceability and analysis. The final log generation and permission release mark the completion of this switchover task.
[0080] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the claimed invention. The scope of protection claimed by the appended claims and their equivalents is defined.
Claims
1. A method for suppressing color bleeding in multi-color 3D printing, characterized in that, include: Establish a steady-state operating baseline before material switching, and obtain the current material's extrusion flow rate, melt chamber pressure, nozzle position, and direction of movement; Based on the steady-state operating benchmark, a pre-switching retraction action is performed to reduce the residual pressure in the melting chamber. In response to the pre-switching retraction result, the new material is smoothly injected into the melting chamber and fused with the residual melt. Based on the injection state of the new material, the synergistic relationship between the extrusion flow rate and the nozzle movement path is reconstructed. Combined with the reconstructed synergistic relationship, dynamic pressure balance control is implemented to stabilize the pressure in the melt chamber. Under stable pressure, a local path fine-tuning command is generated to adapt to the properties of the new material. Using the fine-tuned path, a gradual flow ramp is executed to make the extrusion flow reach the target value. Based on the traffic surge results, complete the post-switch status verification and return to normal printing.
2. The method for suppressing color bleeding in multi-color 3D printing according to claim 1, characterized in that, The establishment of a steady-state operating baseline before material switching includes: Monitor the current continuous extrusion rate of the material; While the monitored extrusion rate remains constant, the pressure balance level inside the melt chamber is measured. Record the current position and direction vector of the nozzle, and determine the spatial coordinates of the material switching trigger point based on the recorded vector.
3. The method for suppressing color bleeding in multi-color 3D printing according to claim 1, characterized in that, The execution of the pre-switch rollback action includes: The total pullback amount is set based on the steady-state flow rate; The retraction speed curve is dynamically adjusted based on the pressure balance level inside the melting chamber. By utilizing the nozzle's current position and direction of motion vector, a retraction action is initiated when approaching the switching point, responding to a dynamically adjusted retraction speed curve, and monitoring the pressure drop trend during the retraction process.
4. The method for suppressing color bleeding in multi-color 3D printing according to claim 1, characterized in that, The method of guiding the smooth injection of new material into the melting cavity includes: Initiate the pre-feeding of the new material to establish initial contact, and gradually increase the heating power according to the pre-feeding state and the characteristics of the new material; Under conditions of increased heating power, control the degree of shear mixing at the interface between the old and new melts; Based on the results of shear mixing control, micro-extrusion was performed to verify melt continuity.
5. The method for suppressing color bleeding in multi-color 3D printing according to claim 1, characterized in that, The reconstructed coordination relationship between extrusion flow rate and nozzle movement path includes: Initialize the target extrusion flow rate based on the properties of the new material; By utilizing the initial target extrusion flow rate and melt chamber pressure, viscosity shifts caused by temperature changes are dynamically compensated. Based on the compensated viscosity shift, the nozzle movement speed is adjusted synchronously to maintain linewidth consistency; The first segment of printing is performed along the optimized transition path, based on the adjusted printhead movement speed.
6. The method for suppressing color bleeding in multi-color 3D printing according to claim 1, characterized in that, The implementation of dynamic pressure balance control includes: Establish a monitoring window for the rate of pressure change in the molten zone; Adjust the propulsion output based on the monitored rate of pressure change; The heating compensation strategy is optimized by combining the adjusted propulsion output and temperature field distribution; Based on the optimized heating compensation strategy and pressure change trend, the pressure is determined to be stable and the transition control is allowed to be discontinued.
7. The method for suppressing color bleeding in multi-color 3D printing according to claim 1, characterized in that, The generated local path fine-tuning instructions adapted to the properties of the new material include: Extract the morphological characteristics of the initial extrusion section of the new material; Based on the extracted morphological features, the source of path deviation is identified by comparing the design value with the measured value; Based on the identified path deviation sources, a local path offset vector is constructed to compensate for flow lag; Update the short-term path cache in the motion controller according to the constructed local path offset vector.
8. The method for suppressing color bleeding in multi-color 3D printing according to claim 1, characterized in that, The implementation of gradual traffic ramping includes: Set the total traffic ramp-up time and segment intervals; Based on the set total duration, an S-shaped curve is used to plan the flow increment sequence; By utilizing the planned flow increment sequence, the heating power is adjusted synchronously to match the flow growth rate; By adjusting the heating power, the actual flow response is monitored and the ramp-up curve is dynamically corrected.
9. The method for suppressing color bleeding in multi-color 3D printing according to claim 1, characterized in that, The post-switching status verification includes: Acquire the first image of the formed quality after the switching is completed; Based on the acquired images, image texture features are analyzed to evaluate the fusion quality; In response to the evaluation of fusion quality, reset all temporary control parameters to their default settings; Based on the reset parameter status, record the entire switching process log and grant permission for the next trigger.
10. A color crosstalk suppression system for implementing the method of any one of claims 1-9 in multicolor 3D printing, characterized in that, include: The material switching control module is used to establish a steady-state operating baseline before material switching and to obtain the current material's extrusion flow rate, melt chamber pressure, nozzle position, and direction of movement. The injection guidance module is used to perform a pre-switching retraction action based on the steady-state operating benchmark, reduce the residual pressure in the melting chamber, respond to the pre-switching retraction result, and guide the new material to be smoothly injected into the melting chamber and fuse with the residual melt. The dynamic balancing module is used to reconstruct the synergistic relationship between the extrusion flow rate and the nozzle movement path by referring to the injection state of the new material. Based on the reconstructed synergistic relationship, dynamic pressure balance control is implemented to stabilize the pressure in the melt chamber. The path fine-tuning module is used to generate local path fine-tuning instructions to adapt to the properties of new materials under stable pressure. Using the fine-tuned path, a gradual flow ramp is executed to make the extrusion flow reach the target value. The normal regression module is used to verify the status after the switch based on the traffic crawling results, and print the normal regression status.