Method for measuring easily extrudable PCR resin and PCR resin composition

The capillary rheometer device method addresses the classification challenges of PCR resin by measuring pressure and dimensions to assess extrudability, ensuring efficient processing and improved physical properties, thus overcoming the difficulties in recycling polyethylene PCR resin.

WO2024253500A1PCT designated stage expired Publication Date: 2024-12-12SK INNOVATION CO LTD +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2024/095673
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-06-07
Filing Date
2024-04-04
Publication Date
2024-12-12

AI Technical Summary

Technical Problem

The classification of polyethylene post-consumer recycled (PCR) resin into recyclable grade A and non-recyclable grade C is challenging due to deteriorated physical properties and foreign matter content, making continuous processing difficult, and existing analysis methods are costly and inefficient.

Method used

A method using a capillary rheometer device to determine the extrudability of PCR resin by measuring the initial and final pressure, piston and capillary diameters, sieve mesh size, and wire diameter, allowing for the classification of PCR resin based on foreign matter content and optimal mixing with new materials for improved processability.

Benefits of technology

Enables the easy classification of continuously extrudable PCR resin with low foreign matter content, ensuring excellent physical properties and efficient processing, reducing the need for costly analysis and preventing blockages during extrusion.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2024095673_12122024_PF_FP_ABST
    Figure KR2024095673_12122024_PF_FP_ABST
Patent Text Reader

Abstract

Provided is a method for measuring an easily extrudable extrusion-moldable PCR resin. Specifically, a method for distinguishing a post-consumer recycled (PCR) resin in a new manner which may distinguish a high grade PCR resin by adding the PCR resin to a capillary rheometer and quantifying a volume value measured when a pressure is increased to a certain level, which is a method for providing determination information of the easily extrudable extrusion-moldable PCR resin.
Need to check novelty before this filing date? Find Prior Art

Description

METHOD FOR MEASURING EASILY EXTRUDABLE PCR RESIN AND PCR RESIN COMPOSITION

[0001] The present disclosure relates to a method for measuring easily extrudable PCR resin and PCR resin composition

[0002] A post-consumer recycled (PCR) resin refers to a recycled resin, and a study for recycling it is currently in progress. The PCR resin is a polymer resin, such as polyethylene (PE), polyethylene terephthalate (PET), polypropylene (PP), poly (vinyl chloride) (PVC), and polystyrene (PS), and the polymer resin is mainly used in clothing, carpets, bottles, plastic lumber, pipes, floor tiles, packaging, fibers, and the like, and thus, the content of a discharged PCR resin is increasing every year.

[0003] Among the PCR resin materials, in the case of stretch wrap used to package large supermarket items of a polyethylene (PE) resin, resin having a large volume and the same properties may be secured in a large amount, and thus, a study for recycling the resin continues.

[0004] However, since a polyethylene PCR resin usually has deteriorated physical properties and processability as compared with a new material polymer resin, it is difficult to use the polyethylene PCR resin again. In particular, the physical properties are greatly deteriorated due to foreign matter inside the resin of the polyethylene PCR resin after processing, and in particular, even when a foreign matter removal filter is separately provided during extrusion, , the filter in an extruder is eventually blocked by excessive foreign matter during processing so that continuous processing is very difficult.

[0005] Accordingly, the collected polyethylene PCR resin materials should be differentiated and classified into recyclable grade A resins, non-recyclable C grade resins, and the like, but it is difficult to classify the grade A PCR resin and the grade C PCR resin by visual inspection, ICP elemental analysis, TGA pyrolysis analysis, and the like, and the cost of the analysis is also high.

[0006] An embodiment of the present invention is directed to providing a method for determining an easily extrudable PCR resin which enables easy classification of a PCR resin having a foreign matter content at or below a certain level by using a capillary rheometer device of a grade A PCR resin material having a low content of foreign matter.

[0007] Another embodiment of the present invention is directed to providing a PCR resin composition which is easily processed by mixing even a low-grade PCR resin with a new material at an optimal content, since a composition of a mixture of a PCR resin and a new material is measured using a capillary rheometer device.

[0008] In one general aspect, a method for measuring an easily extrudable post-consumer recycled (PCR) resin which is a method for providing determination information of the easily extrudable PCR resin is provided, wherein the PCR resin includes a polyolefin resin, a total capacity of a resin at which an initial pressure (P0) becomes doubled (Pt) when the PCR resin passes through a capillary rheometer satisfies the following Equation 1, a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, and a sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3:

[0009] [Equation 1]

[0010] ((Vt-Va)) / Vt<0.8

[0011] wherein Vtis an initial volume (cm3) of the PCR resin entering the capillary rheometer, and Vais a volume (cm3) of a resin filtered by the mesh in the capillary rheometer at which the initial pressure becomes doubled,

[0012] [Equation 2]

[0013] 0.05 ≤ M2 / M1≤0.2

[0014] wherein M1is a piston diameter, and M2is a capillary diameter,

[0015] [Equation 3]

[0016] 0.65≤ WD / SM ≤ 0.73

[0017] wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).

[0018] In an exemplary embodiment, the PCR resin may include a polyethylene resin.

[0019] In an exemplary embodiment, the mesh included in the capillary rheometer may be 50 to 200 meshes.

[0020] In an exemplary embodiment, the mesh may have a total permeation area ratio of 30 to 50%.

[0021] In an exemplary embodiment, a pressure applied to the capillary rheometer may be 10 to 1,000 bar.

[0022] In an exemplary embodiment, a cylinder internal temperature of the capillary rheometer may satisfy the following Equation 4:

[0023] [Equation 4]

[0024] PT1+50°C < T1< PT1+150°C

[0025] wherein PT1is a melting temperature of the PCR resin, and T1is the cylinder internal temperature of the capillary rheometer.

[0026] In an exemplary embodiment, the capillary rheometer may have the piston diameter of 10 to 30 mm and the capillary diameter of 1 to 5 mm.

[0027] In another general aspect, a method for measuring an easily extrudable post-consumer recycled (PCR) resin which is a method for providing determination information of an easily extrudable PCR resin composition is provided, wherein the PCR resin includes a polyolefin resin, the following Equation 5 is satisfied when the PCR resin passes through a capillary rheometer, a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, and a sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3:

[0028] [Equation 5]

[0029] (ln(PL / P0)) / V < 0.16

[0030] [Equation 2]

[0031] 0.05 ≤ M2 / M1≤ 0.2

[0032] wherein M1is a piston diameter, and M2is a capillary diameter,

[0033] [Equation 3]

[0034] 0.65 ≤ WD / SM ≤ 0.73

[0035] wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).

[0036] P0is an initial internal pressure of the capillary rheometer when the PCR resin is added and a pressure was applied at a volume of 1 cc, and PLis a pressure finally applied to the capillary rheometer. In addition, V is an internal volume of the capillary rheometer decreased by additional pressure from P0, and V refers to a volume until a PLvalue becomes twice a P0value. When the PLvalue is more than twice the P0value, V is measured with PLbeing limited to twice P0. In addition, when PLis less than twice P0, V is set as a final measured volume.

[0037] In an exemplary embodiment, the PCR resin may include a new material.

[0038] In an exemplary embodiment, the mesh included in the capillary rheometer may be 50 to 200 meshes.

[0039] In an exemplary embodiment, the mesh may have a total permeation area ratio of 35 to 50%.

[0040] In an exemplary embodiment, a cylinder internal temperature of the capillary rheometer satisfies the following Equation 4:

[0041] [Equation 4]

[0042] PT1+50°C < T1< PT1+150°C

[0043] wherein PT1is a melting temperature of the PCR resin, and T1is the cylinder internal temperature of the capillary rheometer.

[0044] In an exemplary embodiment, the capillary rheometer may have the piston diameter of 10 to 30 mm and the capillary diameter of 1 to 5 mm.

[0045] In another general aspect, an excellently melt-extrudable post-consumer recycled (PCR) resin is provided, wherein a total capacity of a resin at which an initial pressure (P0) becomes doubled (Pt) when the PCR resin passes through a capillary rheometer satisfies the following Equation 1, a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, and a sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3:

[0046] [Equation 1]

[0047] ((Vt-Va)) / Vt< 0.8

[0048] wherein Vtis an initial volume (cm3) of the PCR resin entering the capillary rheometer, and Vais a volume (cm3) of a resin filtered by the mesh in the capillary rheometer at which the initial pressure becomes doubled,

[0049] [Equation 2]

[0050] 0.05 ≤ M2 / M1≤ 0.2

[0051] wherein M1is a piston diameter, and M2is a capillary diameter,

[0052] [Equation 3]

[0053] 0.6 5≤ WD / SM ≤ 0.73

[0054] wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).

[0055] In still another general aspect, a post-consumer recycled (PCR) resin composition is provided, wherein the PCR resin includes a polyolefin resin, the following Equation 5 is satisfied when the PCR resin passes through a capillary rheometer, a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, and a sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3:

[0056] [Equation 5]

[0057] (ln(PL / P0)) / V < 0.16

[0058] [Equation 2]

[0059] 0.05 ≤ M2 / M1≤ 0.2

[0060] wherein M1 is a piston diameter, and M2 is a capillary diameter,

[0061] [Equation 3]

[0062] 0.65 ≤ WD / SM ≤ 0.73

[0063] wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).

[0064] P0is an initial internal pressure of the capillary rheometer when the PCR resin is added and a pressure was applied at a volume of 1 cc, and PLis a pressure finally applied to the capillary rheometer. In addition, V is an internal volume of the capillary rheometer decreased by additional pressure from P0, and V refers to a volume until a PLvalue becomes twice a P0value. When the PLvalue is more than twice the P0value, V is measured with PLbeing limited to twice P0. In addition, when PLis less than twice P0, V is set as a final measured volume.

[0065] In an exemplary embodiment, the PCR resin composition may include a new material.

[0066] Other features and aspects will be apparent from the following detailed description, the drawings, and the claims.

[0067] The method for measuring a PCR resin of the present disclosure may easily determine a continuously extrudable PCR resin material by deriving a correlation between a foreign matter and an extrusion pressure of the PCR resin using a capillary rheometer device.

[0068] In addition, the present disclosure may provide a PCR resin composition which is easily processed by mixing even a low-grade PCR resin with a new material at an optimal content, since a composition of a mixture of a low-grade PCR resin and a new material is measured using a capillary rheometer device.

[0069] FIG. 1 is a rough schematic diagram of a capillary rheometer device.

[0070] FIG. 2 is a graph in which a PCR resin volume to reach an optional pressure using the capillary rheometer device is schematized.

[0071] FIG. 3 is a graph of measuring a pressure state occurring when a piston is pressed at a constant speed in the capillary rheometer device.

[0072] FIG. 4 is a graph showing a value depending on a PCR resin content in a PCR resin composition using the capillary rheometer device.

[0073] Hereinafter, the present disclosure will be described in more detail with reference to specific examples and exemplary embodiments including the accompanying drawings. However, the following specific examples and exemplary embodiments are only a reference for describing the present disclosure in detail, and the present disclosure is not limited thereto and may be implemented in various forms.

[0074] In addition, unless otherwise defined, all technical terms and scientific terms have the same meanings as those commonly understood by one of those skilled in the art to which the present disclosure pertains. The terms used herein are only for effectively describing a certain specific example, and are not intended to limit the present disclosure.

[0075] In addition, the singular form used in the specification and claims appended thereto may be intended to include a plural form also, unless otherwise indicated in the context.

[0076] In addition, unless particularly described to the contrary, “”any elements will be understood to imply further inclusion of other elements rather than the exclusion of any other elements.

[0077] Conventionally collected polyethylene PCR resin materials should be differentiated and classified into recyclable grade A resins, non-recyclable C grade resins, and the like, but it is difficult to classify the grade A PCR resin and the grade C PCR resin materials by visual inspection, ICP elemental analysis, TGA pyrolysis analysis, and the like, and the cost of the analysis is also high.

[0078] Accordingly, the present disclosure provides a method for measuring an easily extrudable post-consumer recycled (PCR) resin which is a method for providing determination information of the easily extrudable grade A PCR resin is provided, wherein the PCR resin includes a polyolefin resin, a total capacity of a resin at which an initial pressure (P0) becomes doubled (Pt) when the PCR resin passes through a capillary rheometer satisfies the following Equation 1, a ratio between the piston diameter and the capillary diameter in the capillary rheometer satisfies the following Equation 2, and a sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3.

[0079] In addition, the polyolefin resin may be any one or more polyolefin resins selected from polyethylene, polypropylene, polyketone, polypropylene copolymer, polymethylpentene, polystyrene, and polyvinyl chloride, specifically, may be any one or more polyolefin resins selected from polyethylene, polypropylene, and polystyrene, and specifically, may be a polyethylene resin, but is not limited thereto.

[0080] According to an exemplary embodiment of the present disclosure, the polyethylene resin may be any one or more polyethylene resins selected from low density polyethylene (LDPE), linear low-density polyethylene (LLDPE), crosslinked high-density polyethylene (XLPE), and high-density polyethylene, but is not limited thereto:

[0081] [Equation 1]

[0082] ((Vt-Va)) / Vt<0.8

[0083] wherein Vtis an initial volume (cm3) of the PCR resin entering the capillary rheometer, Va is a volume (cm3) of a resin filtered by the mesh from the capillary rheometer at which the initial pressure becomes doubled, and when all resin inside the capillary rheometer is discharged without reaching twice the pressure, a Vavalue is set as a Vt,

[0084] [Equation 2]

[0085] 0.05 ≤ M2 / M1≤ 0.2

[0086] wherein M1is a piston diameter, and M2is a capillary diameter,

[0087] [Equation 3]

[0088] 0.65 ≤ WD / SM ≤ 0.73

[0089] wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).

[0090] A high-quality continuously extrudable PCR resin material may be easily determined without particular analysis and device in the collected PCR resin, by the method for measuring an easily extrudable PCR resin.

[0091] Now, the method of measuring an easily extrudable PCR resin will be described using FIG. 1 as an example. However, FIG. 1 is only an example for describing the capillary rheometer of the present disclosure in detail, and the present disclosure is not limited to FIG. 1.

[0092] The capillary rheometer device 1,000 includes a cylinder body 100, a piston 200, a pressure gauge 300, a mesh 400, and a capillary die 500, but the constituents may be further added, if necessary.

[0093] A PCR resin material is added to the capillary rheometer device 1000, the cylinder body 100 is heated until the PCR resin material is melted, and then the piston 200 is pressed at a certain speed to discharge a melted PCR resin through the capillary of the capillary die 500.

[0094] The certain speed of the piston may be 0.01 to 0.5 mmsec-1, 0.05 to 0.3 mmsec-1, or 0.08 to 0.2 mmsec-1but is not limited thereto.

[0095] Since the mesh 400 is installed in a lower portion of the cylinder body 100, when the melted PCR resin is discharged, foreign matter inside the PCR resin blocks the hole of the mesh and the internal pressure of the cylinder body 100 is increased. Herein, as the foreign matter content is high, the pressure is rapidly increased even when the piston 200 is pressed a little, and when the pressure is excessively applied, the mesh may burst.

[0096] That is, in the present disclosure, a continuously extrudable PCR resin may be distinguished by calculating a time taken to reach a certain pressure or a PCR resin volume inside the cylinder body, depending on the content of foreign matter.

[0097] When the PCR resin satisfying the following Equation 1 of the present disclosure is used, it is continuously extrudable and a PCR resin having excellent physical properties may be distinguished. Specifically, in the case of a PCR resin having a value depending on a pressure in the following Equation 1 of 0.8 or more, a mesh for filtering foreign matter in extrusion in an extruder may be broken due to excessive pressure, and even when a film is manufactured by extrusion, the physical properties of the film may be greatly deteriorated due to excessive foreign matter. However, in the case of a PCR resin having a value depending on the pressure in the following Equation 1 of less than 0.8, extrusion is well performed, and when a film is manufactured, film manufacture by excessive foreign matter due to an excessive amount is suppressed, and thus, mechanical properties such as tensile strength are excellent. The following Equation 1 may be less than 0.8, specifically, the upper limit may be 0.7 or less, 0.6 or less, 0.5 or less, 0.4 or less, 0.3 or less, 0.2 or less, or 0.1 or less and the lower limit may be 0.0 or more, 0.001 or more, and specifically, 0.0 or more and less than 0.8, specifically 0.001 or more and less than 0.8, and specifically 0.01 to 0.7, but the present disclosure is not limited thereto.

[0098] As the following Equation 1 is close to 0, the foreign matter content is almost 0, and when the following Vt value and the Va value are the same, it may have equivalent quality to a new material having almost no foreign matter:

[0099] [Equation 1]

[0100] ((Vt-Va)) / Vt<0.8

[0101] wherein Vtis an initial volume (cm3) of the PCR resin entering the capillary rheometer, Vais a volume (cm3) of a resin filtered by the mesh from the capillary rheometer at which the initial pressure becomes doubled, and when all resin inside the capillary rheometer is filtered without reaching twice the pressure, a Vavalue is set as a Vt.

[0102] A standard of the capillary rheometer device 1000 from which Equation 1 is derived may be a device satisfying the following Equations 2 and 3:

[0103] [Equation 2]

[0104] 0.05 ≤ M2 / M1≤ 0.2

[0105] wherein M1is a piston diameter, and M2is a capillary diameter,

[0106] [Equation 3]

[0107] 0.65 ≤ WD / SM ≤ 0.73

[0108] wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).

[0109] A PCR resin satisfying Equation 1 using the capillary rheometer device 1000 in which a piston diameter and a capillary diameter of the capillary rheometer device 1000 satisfy Equation 2 and a wire diameter of the mesh 400 and a sieve mesh size are based on Equation 3 has excellent continuous extrudability and when it is processed into a film, its physical properties are also excellent.

[0110] According to an exemplary embodiment of the present disclosure, the PCR resin may include a polyethylene resin, and since the polyethylene resin PCR resin which is distinguished as a PCR resin satisfying Equation 1 using the capillary rheometer device 1000 satisfying Equations 2 and 3 is extrudable, a polyethylene PCR resin product which has excellent physical properties and is continuously extrudable without blockage may be provided.

[0111] According to an exemplary embodiment of the present disclosure, the mesh included in the capillary rheometer may have an upper limit of 200 meshes or less and a lower limit of 50 meshes or more, specifically 50 to 200 meshes, but is not limited thereto.

[0112] According to an exemplary embodiment of the present disclosure, the mesh may have a total permeation area ratio of 30 to 50%, specifically 50% or less, 48% or less, 45% or less, 43% or less, 42% or less, 41% or less, or 40% or less as an upper limit and 30% or more, 33% or more, 36% or more, 37% or more, 38% or more, or 39% or more as a lower limit, specifically 37 to 48%, specifically 38 to 40%, but is not limited thereto.

[0113] According to an exemplary embodiment of the present disclosure, a pressure applied to the capillary rheometer may be 10 to 1,000 bar, specifically 10 to 500 bar, and specifically 30 to 100 bar, but is not limited thereto.

[0114] According to an exemplary embodiment of the present disclosure, a cylinder internal temperature of the capillary rheometer may satisfy the following Equation 4, but it is not limited thereto as long as it is in a melting temperature range of a polymer, and as an example, may be 300°C or lower, 250°C or lower, or 200°C or lower as an upper limit and may be 50°C or higher, 100°C or higher, or 150°C or higher as a lower limit, and specifically, 50 to 300°C, specifically 100 to 300°C, specifically 150 to 300°C, specifically 150 to 250°C, and specifically 150 to 230°C, but is not limited thereto:

[0115] [Equation 4]

[0116] PT1+50°C < T1< PT1+150°C

[0117] wherein PT1is a melting temperature of the PCR resin, and T1is the cylinder internal temperature of the capillary rheometer.

[0118] According to an exemplary embodiment of the present disclosure, the piston diameter of the capillary rheometer may be 10 to 30 mm, specifically 12 to 25 mm and the capillary diameter may be 1 to 5 mm, specifically 1.5 to 3 mm, but the present disclosure is not limited thereto.

[0119] The present disclosure may separate and provide an excellently melt-extrudable post-consumer recycled (PCR) resin is provided, wherein a total capacity of a resin at which an initial pressure (P0) becomes doubled (Pt) when the PCR resin passes through a capillary rheometer satisfies the following Equation 1, a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, and a sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3. Since the PCR resin having excellent melt extrudability satisfies the following Equation 1, a recycled film having excellent physical properties and also excellent processability may be provided. Since the capillary rheometer is described in detail above, the description thereof will be omitted here:

[0120] [Equation 1]

[0121] ((Vt-Va)) / Vt<0.8

[0122] wherein Vtis an initial volume (cm3) of the PCR resin entering the capillary rheometer, and Vais a volume (cm3) of a resin filtered by the mesh in the capillary rheometer at which the initial pressure becomes doubled,

[0123] [Equation 2]

[0124] 0.05 ≤ M2 / M1≤ 0.2

[0125] wherein M1is a piston diameter, and M2is a capillary diameter,

[0126] [Equation 3]

[0127] 0.65 ≤ WD / SM ≤ 0.73

[0128] wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).

[0129] Since Equations 1 to 3 are described in detail above, the description thereof will be omitted here.

[0130] According to an exemplary embodiment of the present disclosure, the PCR resin may include a polyethylene resin, but since it is also described above, the description thereof will be omitted here.

[0131] According to an exemplary embodiment of the present disclosure, the mesh included in the capillary rheometer may be 50 to 200 meshes, but since it is also described above, the description thereof will be omitted here.

[0132] According to an exemplary embodiment of the present disclosure, the mesh may have a total permeation area ratio of 35 to 50%, but since it is also described above, the description thereof will be omitted here.

[0133] According to an exemplary embodiment of the present disclosure, a pressure applied to the capillary rheometer may be 10 to 1,000 bar, but since it is also described above, the description thereof will be omitted here.

[0134] According to an exemplary embodiment of the present disclosure, a cylinder internal temperature of the capillary rheometer may satisfy the following Equation 4, but since it is also described above, the description thereof will be omitted here:

[0135] [Equation 4]

[0136] PT1+50°C < T1< PT1+150°C

[0137] wherein PT1is a melting temperature of the PCR resin, and T1is the cylinder internal temperature of the capillary rheometer.

[0138] According to an exemplary embodiment of the present disclosure, the capillary rheometer may have the piston diameter of 10 to 30 mm and the capillary diameter of 1 to 5 mm, but since it is also described above, the description thereof will be omitted here.

[0139] The PCR resin having excellent melt extrudability may be used alone by melt extrusion, or may be used with a new material further mixed with the PCR resin.

[0140] The new material may be the polyolefin-based resin described above, but is not limited thereto.

[0141] According to another exemplary embodiment of the present disclosure, an easily extrudable post-consumer recycled (PCR) resin composition may be provided, wherein the PCR resin includes a polyolefin resin, the following Equation 5 is satisfied when the PCR resin passes through a capillary rheometer, a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, and a sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3:

[0142] [Equation 5]

[0143] (ln(PL / P0)) / V < 0.16

[0144] [Equation 2]

[0145] 0.05 ≤ M2 / M1≤ 0.2

[0146] wherein M1is a piston diameter, and M2is a capillary diameter,

[0147] [Equation 3]

[0148] 0.65 ≤ WD / SM ≤ 0.73

[0149] wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).

[0150] P0is an initial internal pressure of the capillary rheometer when the PCR resin is added and a pressure was applied at a volume of 1 cc, and PLis a pressure finally applied to the capillary rheometer. In addition, V is an internal volume of the capillary rheometer decreased by additional pressure from P0, and V refers to a volume until a PLvalue becomes twice a P0value. When the PLvalue is more than twice the P0value, V is measured with PLbeing limited to twice P0. In addition, when PLis less than twice P0, V is set as a final measured volume.

[0151] Since Equations 2, 3, and 5 are described in detail above, the description thereof will be omitted here.

[0152] According to an exemplary embodiment of the present disclosure, the PCR resin may include a polyethylene resin, but since it is also described above, the description thereof will be omitted here.

[0153] According to an exemplary embodiment of the present disclosure, the mesh included in the capillary rheometer may be 50 to 200 meshes, but since it is also described above, the description thereof will be omitted here.

[0154] According to an exemplary embodiment of the present disclosure, the mesh may have a total permeation area ratio of 35 to 50%, but since it is also described above, the description thereof will be omitted here.

[0155] According to an exemplary embodiment of the present disclosure, a pressure applied to the capillary rheometer may be 10 to 1,000 bar, but since it is also described above, the description thereof will be omitted here.

[0156] According to an exemplary embodiment of the present disclosure, a cylinder internal temperature of the capillary rheometer may satisfy the following Equation 4, but since it is also described above, the description thereof will be omitted here:

[0157] [Equation 4]

[0158] PT1+50°C < T1< PT1+150°C

[0159] wherein PT1is a melting temperature of the PCR resin, and T1is the cylinder internal temperature of the capillary rheometer.

[0160] According to an exemplary embodiment of the present disclosure, the capillary rheometer may have the piston diameter of 10 to 30 mm and the capillary diameter of 1 to 5 mm, but since it is also described above, the description thereof will be omitted here.

[0161] Hereinafter, the examples of the present disclosure will be further described with reference to the specific experimental examples. It is apparent to those skilled in the art that the examples and the comparative examples included in the experimental examples only illustrate the present disclosure and do not limit the appended claims, and various modifications and alterations of the examples may be made within the range of the scope and spirit of the present invention, and these modifications and alterations will fall within the appended claims.

[0162]

[0163] [Examples and Comparative Examples]

[0164] An increased pressure occurring in a sample and a flow rate of a sample which passed through a capillary rheometer die were measured using a capillary rheometer (RHEOGRAPH 25, Gottfert).

[0165] The measurement was performed using a capillary die having a diameter of 2.0 mm and a length of 25 mm. In addition, the diameter of the piston of the rheometer device was 15 mm and a length of 250 mm, and a 120 mesh filter having a sieve size of 0.13 mm, a wire diameter of 0.08 mm, and an opening ratio of 38.3% was mounted on the upper portion of the capillary die.

[0166] A capillary die on which a 120 mesh filter is attached was mounted on the lower end of the barrel of the rheometer device and the temperature was maintained at a die test temperature of 190°C. When a PCR resin sample was loaded in a barrel area of the rheometer, air trapped in the sample was all removed so that a volume of 40 cm3or more was loaded, and then the sample was extruded at a selected piston descending speed of 0.1 mmsec-1 through a capillary die in a barrel. When the sample was processed by passing through a capillary die in the barrel, the pressure applied to the sample and the amount of the sample filtered through the capillary die on which the mesh was mounted were recorded over time to confirm a pressure increase tendency by foreign matter. The results are listed in the following Table 1:

[0167] Example 1Example 2Example 3Example 4Example 5Comparative Example 1Type of resinPCR A-1PCR A-2PCR A-3PCR A-4PCR A-5PCR CVolume (cm3)1.5 times the initial pressure13.1319.2012.2613.40 402.50Later volume / initial volume0.6720.520.6940.66500.9382.0 times the initial pressure18.8835.4324.6220.57 404.48Later volume / initial volume0.5280.1140.3850.48600.888

[0168] The resins in Table 1 and FIG. 1 are those collected by each company, and as a result of extruding the PCR resin under the capillary rheometer conditions of the present disclosure, all except Comparative Example 1 satisfied the conditions of Equation 1. In addition, in FIG. 2 also, it was confirmed that in Comparative Example 1, when the PCR resin was pushed out at a certain speed, the pressure was rapidly increased.

[0169] In addition, for the PCR resin composition, a mixed composition of new material polyethylene resin with the PCR resin of the comparative example was added to a capillary rheometer and then the measurement was performed in the same manner as in the comparative example. Content ranges of the new material in the PCR resin are shown in Table 1 and FIG. 4:

[0170] PCR resin: PCR CPCR resin content10 wt%15 wt%25 wt%50 wt%75 wt%100 wt%a value0.012950.023650.043550.072030.114850.1598

[0171] Each measurement was performed with the capillary rheometer device in a range of 10 to 100 wt% of the PCR resin content in the PCR resin composition, and measurements were substituted into Equation 5 to derive the value. As shown in Table 2 and FIG. 4, it is confirmed that the value is linearly related to the PCR resin content ratio, and extrusion processing is performed well from the PCR resin content of 75 wt% or less. Thus, it is shown that when a resin is processed, specifically a thin film and the like are manufactured, a PCR resin mixing ratio may be identified in advance through Equation 5.

[0172] As a result, in the present disclosure, it was identified that extrusion processing is not performed well due to the foreign matter in a PCR resin and a method for separating a PCR resin which is extrusion-processed well, which may identify it in advance, is described, and in particular, even for a low grade PCR resin or a composition mixed with a new material, a method for separating a PCR resin composition which may identify a critical point of a PCR resin content at which extrusion processing is well performed in advance is described.

[0173] Hereinabove, although the present disclosure has been described by specific matters, limited implementations, and drawings, they have been provided only for assisting the entire understanding of the present disclosure, and the present disclosure is not limited to the implementations, and various modifications and changes may be made by those skilled in the art to which the present disclosure pertains from the description.

[0174] Therefore, the spirit of the present disclosure should not be limited to the above-described exemplary embodiments, and the following claims as well as all modified equally or equivalently to the claims are intended to fall within the scope and spirit of the disclosure.

[0175]

[0176] [Detailed Description of Main Elements]

[0177] 1000: Capillary rheometer device

[0178] 100: Cylinder body

[0179] 200: Piston

[0180] 300: Pressure gauge

[0181] 400: Mesh

[0182] 500: Capillary die

Claims

1.A method for measuring an easily extrudable post-consumer recycled (PCR) resin which is a method for providing determination information of the easily extrudable PCR resin,wherein the PCR resin includes a polyolefin resin,a total capacity of a resin at which an initial pressure (P0) becomes doubled (Pt) when the PCR resin passes through a capillary rheometer satisfies the following Equation 1,a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, and a sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3:[Equation 1]((Vt-Va)) / Vt<0.8wherein Vtis an initial volume (cm3) of the PCR resin entering the capillary rheometer, and Vais a volume (cm3) of a resin filtered by the mesh in the capillary rheometer at which the initial pressure becomes doubled,[Equation 2]0.05 ≤ M2 / M1≤0.2wherein M1is a piston diameter, and M2is a capillary diameter,[Equation 3]0.65 ≤ WD / SM ≤ 0.73wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).2.The method for measuring an easily extrudable PCR resin of claim 1, wherein the PCR resin includes a polyethylene resin.3.The method for measuring an easily extrudable PCR resin of claim 1, wherein the mesh included in the capillary rheometer is 50 to 200 meshes.4.The method for measuring an easily extrudable PCR resin of claim 3, wherein the mesh has a total permeation area ratio of 30 to 50%.5.The method for measuring an easily extrudable PCR resin of claim 1, wherein a pressure applied to the capillary rheometer is 10 to 1,000 bar.6.The method for measuring an easily extrudable PCR resin of claim 1, wherein a cylinder internal temperature of the capillary rheometer satisfies the following Equation 4:[Equation 4]PT1+50°C < T1< PT1+150°Cwherein PT1is a melting temperature of the PCR resin, and T1is the cylinder internal temperature of the capillary rheometer.7.The method for measuring an easily extrudable PCR resin of claim 1, wherein the capillary rheometer has the piston diameter of 10 to 30 mm and the capillary diameter of 1 to 5 mm.8.A method for measuring an easily extrudable post-consumer recycled (PCR) resin which is a method for providing determination information of an easily extrusion-moldable PCR resin composition,wherein the PCR resin includes a polyolefin resin,the following Equation 5 is satisfied when the PCR resin passes through a capillary rheometer,a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, anda sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3:[Equation 2]0.05 ≤ M2 / M1≤0.2wherein M1is a piston diameter, and M2is a capillary diameter,[Equation 3]0.65 ≤ WD / SM ≤ 0.73wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm),[Equation 5](ln(PL / P0)) / V < 0.16wherein P0is an initial internal pressure of the capillary rheometer when the PCR resin is added and a pressure was applied at a volume of 1 cc, PLis a pressure finally applied to the capillary rheometer, and V is an internal volume of the capillary rheometer decreased by additional pressure from P0, refers to a volume until a PLvalue becomes twice a P0value, is measured with PLbeing limited to twice P0when the PLvalue is more than twice the P0value, and is set as a final measured volume when PLis less than twice P0.9.The method for measuring an easily extrudable PCR resin of claim 8, wherein the PCR resin includes a new material.10.The method for measuring an easily extrudable PCR resin of claim 8, wherein the mesh included in the capillary rheometer is 50 to 200 meshes.11.The method for measuring an easily extrudable PCR resin of claim 8, wherein the mesh has a total permeation area ratio of 35 to 50%.12.The method for measuring an easily extrudable PCR resin of claim 8, wherein a cylinder internal temperature of the capillary rheometer satisfies the following Equation 4:[Equation 4]PT1+50°C < T1< PT1+150°Cwherein PT1is a melting temperature of the PCR resin, and T1is the cylinder internal temperature of the capillary rheometer.13.The method for measuring an easily extrudable PCR resin of claim 8, wherein the capillary rheometer has the piston diameter of 10 to 30 mm and the capillary diameter of 1 to 5 mm.14.An excellently melt-extrudable post-consumer recycled (PCR) resin,wherein a total capacity of a resin at which an initial pressure (P0) becomes doubled (Pt) when the PCR resin passes through a capillary rheometer satisfies the following Equation 1,a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, anda sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3:[Equation 1]((Vt-Va)) / Vt<0.8wherein Vtis an initial volume (cm3) of the PCR resin entering the capillary rheometer, and Vais a volume (cm3) of a resin filtered by the mesh in the capillary rheometer at which the initial pressure becomes doubled,[Equation 2]0.05 ≤ M2 / M1≤ 0.2wherein M1is a piston diameter, and M2is a capillary diameter,[Equation 3]0.65 ≤ WD / SM ≤ 0.73wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm).15.An easily extrudable post-consumer recycled (PCR) resin composition,wherein the PCR resin includes a polyolefin resin,the following Equation 5 is satisfied when the PCR resin passes through a capillary rheometer,a ratio between a piston diameter and a capillary diameter in the capillary rheometer satisfies the following Equation 2, anda sieve mesh size and a wire diameter of a mesh included in the capillary rheometer satisfy the following Equation 3:[Equation 2]0.05 ≤ M2 / M1≤0.2wherein M1is a barrel diameter, and M2is a capillary diameter,[Equation 3]0.65 ≤ WD / SM ≤ 0.73wherein WD is a wire diameter (mm), and SM is a sieve mesh size (mm),[Equation 5](ln(PL / P0)) / V < 0.16wherein P0is an initial internal pressure of the capillary rheometer when the PCR resin is added and a pressure was applied at a volume of 1 cc, PLis a pressure finally applied to the capillary rheometer, and V is an internal volume of the capillary rheometer decreased by additional pressure from P0, refers to a volume until a PLvalue becomes twice a P0value, is measured with PLbeing limited to twice P0when the PLvalue is more than twice the P0value, and is set as a final measured volume when PLis less than twice P0.16.The easily extrudable PCR resin composition of claim 15, wherein the PCR resin composition includes a new material.

Citation Information

Patent Citations

  • Polypropylene resin composition polypropylene resin foamed material and process for procucing the same

    KR100338843B1

  • Insert-molded product

    KR101728926B1

  • Recyclable polyarylene sulfide and preparation method threrof

    KR101781607B1

  • Method and apparatus for determining driving speed using pedestrian intention estimation

    KR1020240044888A

  • Polyethylene resin composition and Method of producing the same

    KR102395347B1